AI Technical Summary
The manufacturing of dry electrodes faces challenges such as poor mechanical and electrical performance due to granulation of active materials and breakage of binder fibers during high shear mixing, leading to defects like pinholes and cracks, and issues with equipment clogging, which hinder mass production.
A method involving the stacking of unit electrode films with fibrillized binders and active materials in a way that their machine directions are antiparallel to each other, combined with high temperature low shear blending and calendaring, to minimize granulation and maximize fibrillization, resulting in improved mechanical properties and preventing channel clogging.
This approach enhances the mechanical properties of dry electrodes in both machine and transverse directions, improves productivity, and facilitates mass production by preventing agglomeration and equipment clogging, resulting in higher quality and more efficient electrode manufacturing.
Abstract
Description
TECHNICAL FIELDThe present disclosure relates to an electrode film, a dry electrode and a secondarybattery comprising the same.The present application claims priority to Korean Patent Application No. 10-2022-0032853 filed on March 16, 2022 in the Republic of Korea, the disclosures of which areincorporated herein by reference.BACKGROUND ARTDue to the increasing use of fossil fuels, there is a growing demand for the use ofalternative energy and clean energy, and in such circumstances, many studies are being madein the field of energy generation and storage using electrochemistry.Currently, a typical example of electrochemical devices using electrical andchemical energy is secondary batteries, and the range of application of secondary batteriesis gradually expanding.One of typical secondary batteries, lithium secondary batteries are used as not onlyan energy source of mobile devices but also a power source of electric vehicles and hybridelectric vehicles as an alternative to vehicles using fossil fuels such as gasoline vehicles anddiesel vehicles that are regarded as one of the main causes of air pollution, and the range ofapplication of lithium secondary batteries is expanding to an auxiliary power source througha grid.A process of manufacturing a lithium secondary battery largely includes three steps:an electrode process, an assembly process and a forming process. The electrode processincludes an active material mixing process, an electrode coating process, a drying process, arolling process, a slitting process and a winding process.The active material mixing process is a process of mixing coating materials forforming an electrode active layer in which electrochemical reaction occurs in the electrode,and specifically, an electrode active material which is the essential element of the electrodeis mixed with an additive such as a conductive material, fillers, a binder for binding powderand adhering to a current collector, and a solvent for making viscous and dispersing powerto prepare a flowable slurry.The mixture composition for forming the electrode active layer is referred to as anelectrode mixture in a broad sense.Subsequently, the electrode coating process of coating the electrode mixture on anelectrically conductive current collector and the drying process for removing a solvent fromthe electrode mixture are performed, followed by rolling, to manufacture the electrode witha predetermined thickness.Meanwhile, defects such as pinholes or cracks may occur in the already formedelectrode active layer due to evaporation of the solvent contained in the electrode mixtureduring the drying. Additionally, the active layer is not uniformly dried all over the entireregion, and due to a difference in solvent evaporation rate, some regions get dried earlier andpowder at the corresponding regions float, and some other regions get dried at a time interval,resulting in low quality of the electrode.Accordingly, recently, many studies are being made to manufacture dry electrodeswithout solvents.In general, a dry electrode is manufactured by laminating a free-standing filmcomprising an active material, a binder and a conductive material on a current collector.During the process, a high shear mixing process such as jet-milling is performed to fibrillizethe binder, and in this instance, when the high shear mixing process is applied to the fragileactive material, fine particles of small size are produced in large amounts, which maydegrade the mechanical performance or the electrical and chemical performance, and in casethat high shear mixing is too much, the produced binder fibers are broken, which makes thefree-standing film less flexible. Additionally, the constituent components are attached tothe inside of the equipment during the jet-milling and a flow of high pressure air is disturbed,resulting in clogged channels, and it is not favorable for mass production.Therefore, there is an urgent need for the development of dry electrodemanufacturing technology to solve the problem.DISCLOSURETechnical ProblemThe present disclosure is directed to providing a free-standing film with improvedmechanical properties in machine direction (MD) and transverse direction (TD)perpendicular to MD for use in dry electrodes with improved flexibility and mechanicalproperties by minimized granulation of an active material and maximized fibrillization of abinder and a method for manufacturing the same.The present disclosure is further directed to providing a dry electrode comprisingthe free-standing film with improved mechanical properties in MD and TD and a method formanufacturing the same.Technical SolutionTo solve the above-described problem, according to an aspect of the presentdisclosure, there is provided an electrode film of the following embodiments.According to a first embodiment, there is provided the electrode film comprising aunit electrode film stacked in two or more layers, the unit electrode film comprising afibrillized binder and an active material, wherein machine directions (MDs) of the unitelectrode films in contact with each other among the two or more layers of unit electrodefilms stacked are antiparallel to each other.According to a second embodiment, in the first embodiment, an angle between theMDs of the unit electrode films in contact with each other among the two or more layers ofunit electrode films may be more than 0° and 90° or less.According to a third embodiment, in the first or second embodiment, an anglebetween the MDs of the unit electrode films in contact with each other among the two ormore layers of unit electrode films may be 45°to 90°.According to a fourth embodiment, in any one of the first to third embodiments, anaverage thickness of the electrode film may be 50 μm to 600 μm.According to a fifth embodiment, in any one of the first to fourth embodiments,when measuring a tensile strength of the electrode film in accordance with ASTM D638, aratio of the tensile strength measured in a direction perpendicular to the MD to the tensilestrength measured in the MD of one of the two or more layers of unit electrode films stackedmay be 0.3 or more.According to a sixth embodiment, in any one of the first to fifth embodiments, whenmeasuring an elastic modulus of the electrode film in accordance with ASTM D638, a ratioof the elastic modulus measured in a direction perpendicular to the MD to the elastic modulusmeasured in the MD of one of the two or more layers of unit electrode films stacked may be0.3 or more.According to another aspect of the present disclosure, there is provided a methodfor manufacturing an electrode film of the following embodiments.According to a seventh embodiment, there is provided the method for manufacturingthe electrode film comprising mixing an active material and a binder to make a mixture;blending the mixture at high temperature low shear to make a mass of mixture; high sheargrinding the mass of mixture to make an electrode powder mixture; feeding the electrodepowder mixture in between a plurality of rolls to carry out calendaring to manufacture a unitelectrode film; stacking the unit electrode film in two or more layers such that axes of MDsof the unit electrode films in contact with each other are antiparallel to each other to obtaina film stack; and calendaring the film stack.According to an eighth embodiment, in the seventh embodiment, the stacking maycomprise stacking such that an angle between the MDs of the unit electrode films in contactwith each other among the two or more layers of unit electrode films is more than 0° and 90°or less.According to a ninth embodiment, in the seventh or eighth embodiment, an averagethickness of the electrode film may be 50 μm to 600 μm.According to another aspect of the present disclosure, there is provided an electrodeof the following embodiments.According to a tenth embodiment, there is provided the electrode comprising acurrent collector; and the electrode film according to any one of the first to sixthembodiments on at least one surface of the current collector.According to another aspect of the present disclosure, there is provided an electrodeof the following embodiments.According to an eleventh embodiment, there is provided the method formanufacturing the electrode comprising laminating the electrode film according to any oneof the first to sixth embodiments on at least one surface of a current collector.According to another aspect of the present disclosure, there is provided a secondarybattery of the following embodiments.According to a twelfth embodiment, there is provided the secondary battery in whichan electrode assembly comprising a positive electrode, a negative electrode and a separatoris included in a battery case together with a lithium containing nonaqueous electrolyte,wherein at least one of the positive electrode or the negative electrode is the electrodeaccording to the tenth embodiment.Advantageous EffectsAccording to the present disclosure, it may be possible to provide the free-standingfilm with improved mechanical properties in machine direction (MD) and a direction that isantiparallel to the MD, for use in dry electrodes, and the method for manufacturing the same.Additionally, using the above-described film, it may be possible to provide the dryelectrode with improved productivity and properties and the method for manufacturing thesame.Furthermore, according to an embodiment of the present disclosure, since hightemperature low shear blending rather than high shear mixing is performed, and grinding isperformed after the high temperature low shear blending, it may be possible to provide thedry electrode in which the granulation of the active material is minimized, the fibrillizationof the binder is maximized and the disintegration of the fibrillized binder is minimized.Further, since blending through the blender and grinding are performed without high shearjet-milling, it may be possible to prevent clogged channels due to the agglomeration of theconstituent components, and it is favorable for mass production.DESCRIPTION OF DRAWINGSFIG. 1 is a diagram showing a process of manufacturing a unit electrode filmaccording to an embodiment of the present disclosure.FIG. 2 is a diagram showing two unit electrode films stacked such that machinedirections (MD) are antiparallel to each other according to an embodiment of the presentdisclosure.FIG. 3 is a diagram showing an angle (θ) between MDs of two unit electrode filmsaccording to an embodiment of the present disclosure.BEST MODEHereinafter, the present disclosure will be described in detail.When used herein, "a MD of a unit electrode film" refers to a running direction ofthe unit electrode film in the process of manufacturing the unit electrode film.FIG. 1 is a diagram showing a process of manufacturing the unit electrode film bycalendaring a electrode powder mixture according to an embodiment of the presentdisclosure. Referring to FIG. 1, when the electrode powder mixture 10 is fed in between aplurality of rolls 1, the unit electrode film 100 is formed along a direction. In this instance,the running direction of the manufactured unit electrode film may be defined as the MD ofthe unit electrode film.The MD of the unit electrode film matches the orientation of fibers in the film, andthus may be identified through the orientation of fibers in the manufactured film. Forexample, the MD of the unit electrode film may be identified through a scanning electronmicroscopy (SEM) image of the unit electrode film. Additionally, it may be identifiedthrough a SEM image of a laminate film manufactured using the unit electrode film. Theorientation of fibers identified through the SEM image may be determined to be the MD ofeach unit electrode film.As described above, the method for manufacturing a dry electrode includes a processof manufacturing a free-standing film through a roll calendaring process. In this instance,the manufactured free-standing film has a difference between properties in MD andmechanical properties in a direction (a transverse direction (TD)) perpendicular to the MD.The inventors recognized that the difference between properties in MD and TD ofthe free-standing film may be a defect factor in the electrode manufacturing process, andfound that the electrode film manufactured by calendaring the electrode powder mixture haspoorer mechanical properties in a direction that is not parallel to the MD than the mechanicalproperties in the MD, and the present disclosure is finally completed.An electrode film according to an aspect of the present disclosure is characterizedin that a unit electrode film is stacked in two or more layers, the unit electrode filmcomprising the fibrillized binder and the active material, and the MDs of the unit electrodefilms in contact with each other among the two or more layers of unit electrode films stackedare antiparallel to each other.FIG. 2 is a diagram showing two unit electrode films 100 stacked such that the MDsare antiparallel to each other according to an embodiment of the present disclosure.Referring to FIG. 2, the electrode film according to the present disclosure comprises at leasttwo unit electrode films stacked such that the MDs are not parallel to each other.When used herein, "the MDs of the unit electrode films in contact with each otheramong the two or more layers of unit electrode films are antiparallel to each other" representsthat the MDs of the unit electrode films in contact with each other are not parallel to eachother when the two or more layers of unit electrode films are stacked.FIG. 3 is a diagram showing an angle (θ) between the MDs of the two layers of unitelectrode films stacked such that the MDs are antiparallel to each other according to anembodiment of the present disclosure.Referring to FIG. 3, the electrode film according to an aspect of the presentdisclosure comprises two or more layers of unit electrode films stacked such that the angle(θ) between the MDs of the unit electrode films in contact with each other is not 0° (or 180°).According to an embodiment of the present disclosure, the angle between the MDsof the unit electrode films in contact with each other among the two or more layers of unitelectrode films may be, for example, more than 0° and 90° or less, specifically 10° to 90°,specifically 45° to 90°, and more specifically 60° to 90°, 70° to 90°, 80° to 90°, 85° to 90°,or 90°. When the angle between the MDs of the unit electrode films in contact with eachother is in the above-described range, it may be possible to provide the electrode film havingimproved mechanical properties in an arbitrary direction.According to an embodiment of the present disclosure, the average thickness of theelectrode film has the ordinary thickness of free-standing films, and is not limited to aparticular thickness. For example, the average thickness of the electrode film may be 50μm to 600 μm, but is not limited thereto. Since the electrode film comprises two or morelayers of unit electrode films such that the MDs are antiparallel to each other, it may bepossible to improve the mechanical properties, and maintain the average thickness of theelectrode film at the ordinary level, thereby providing the electrode film having goodelectrical and chemical properties.The average thickness of the electrode film may be measured through known meansfor measuring the thickness of each component in the corresponding technical field such asthickness measurement machine, SEM imaging or the like. In an embodiment of thepresent disclosure, the thickness of the electrode film may be measured using thicknessmeasurement machine (Mitutoyo, VL-50S-B), but is not limited thereto.Each of the unit electrode films stacked in two or more layers independentlycomprises the fibrillized binder and the active material.When used herein, the 'fibrillized' binder refers to a fibril shaped binder by stretchingthe binder used to manufacture the film by a predetermined process for manufacturing theelectrode film. The fibrillized binder may play a role in binding the active material whichis the essential element of the electrode by forming a network. Additionally, the fibrillizedbinder may play a role in providing the adhesion strength of the electrode film to the currentcollector, but the shape and function of the fibrillized binder is not limited thereto.In an embodiment of the present disclosure, the fibrillized binder which binds theactive material obtained by forming a network in a fibril shape may be seen, for example,through a SEM image of the unit electrode film and / or the electrode film.According to an embodiment of the present disclosure, in addition to the fibrillizedbinder and the active material, each unit electrode film may, independently, further comprisea conductive material.In an embodiment of the present disclosure, the binder is not limited to a particulartype and may include any binder that uniformly disperses the powdery material included inthe electrode film such as the active material without causing a chemical change to thecorresponding battery.In an embodiment of the present disclosure, the binder may comprise, for example,polytetrafluoroethylene (PTFE), polyolefin, or a mixture thereof, specifically,polytetrafluoroethylene (PTFE), and more specifically, polytetrafluoroethylene (PTFE).In another embodiment of the present disclosure, in case that the binder comprisespolytetrafluoroethylene (PTFE), the PTFE may be included in an amount of 60 weight% ormore based on the total weight of the binder.In another embodiment of the present disclosure, the binder may further compriseat least one of polyethylene oxide (PEO), polyvinylidene fluoride (PVdF) or polyvinylidenefluoride-co-hexafluoropropylene (PVdF-HFP).In an embodiment of the present disclosure, the binder may be, for example,included in an amount of 0.5 to 15 parts by weight based on 100 parts by weight of the activematerial. Specifically, the binder may be included in an amount of 0.5 to 15 parts by weight,0.5 to 10 parts by weight, 1 to 5 parts by weight, or 1 to 3 parts by weight based on 100 partsby weight of the active material. When the amount of the binder satisfies the abovedescribedrange, the binder may be adequately fibrillized in the subsequent blending process,resulting in sufficient agglomeration to form a mass of mixture, thereby making it easy tomanufacture the electrode film and improving the properties of the electrode film. In anembodiment of the present disclosure, in case that the electrode film is used to manufacturea positive electrode, the active material may be a positive electrode active material.The positive electrode active material may comprise, for example, at least one oflithium transition metal oxide; lithium metal phosphate; lithium nickel-manganese-cobaltoxide; or oxide with partial substitution of other transition metal in lithium nickelmanganese-cobalt oxide, but is not limited thereto. Specifically, the positive electrodeactive material may comprise, for example, layered compounds such as lithium cobalt oxide(LiCoO2), lithium nickel oxide (LiNiO2) or compounds with one or more transition metalsubstitution; lithium manganese oxide of formula Li1+xMn2-xO4 (where x = 0 to 0.33),LiMnO3, LiMn2O3, LiMnO2; lithium copper oxide (Li2CuO2); vanadium oxide such asLiV3O8, LiV3O4, V2O5, Cu2V2O7; Ni site lithium nickel oxide represented by formula LiNi1-xMxO2 (where M = Co, Mn, Al, Cu, Fe, Mg, B or Ga, x = 0.01 to 0.3); lithium manganesecomposite oxide represented by formula LiMn2-xMxO2 (where M = Co, Ni, Fe, Cr, Zn or Taand x = 0.01 to 0.1) or Li2Mn3MO8 (where M = Fe, Co, Ni, Cu or Zn); lithium nickel cobaltmanganese aluminum oxide (NCMA) Li1+x (NiaCobMncAld)1-xO2 (x = 0 to 0.03, a = 0.3 to0.95, b = 0.01 to 0.35, c = 0.01 to 0.5, d = 0.001 ~ 0.03, a+b+c+d=1) with partial substitutionof aluminum ion for Li in formula, for example, Li[Ni0.73Co0.05Mn0.15Al0.02]O2; lithium metalphosphate LiMPO4 (where M = Fe, CO, Ni, or Mn), disulfide compounds; Fe2(MoO4)3, butis not limited thereto.In another embodiment of the present disclosure, in case that the electrode film isused to manufacture a negative electrode, the active material may be a negative electrodeactive material.The negative electrode active material may include, for example, carbon such asnongraphitizing carbon, graphite-based carbon; metal composite oxide such as LixFe2O3(0≤x≤1), LixWO2 (0≤x≤1), SnxMe1-xMe'yOz (Me: Mn, Fe, Pb, Ge; Me': Al, B, P, Si, Groups1, 2 and 3 elements in the periodic table, halogen; 0<x≤1; 1≤y≤3; 1≤z≤8); lithium metal;lithium alloys; silicon-based alloys; tin-based alloys; silicon-based oxide such as SiO, SiO / C,SiO2; metal oxide such as SnO, SnO2, PbO, PbO2, Pb2O3, Pb3O4, Sb2O3, Sb2O4, Sb2O5, GeO,GeO2, Bi2O3, Bi2O4, and Bi2O5; conductive polymer such as polyacetylene; Li-Co-Ni basedmaterials, but is not limited thereto.In an embodiment of the present disclosure, the conductive material is not limitedto a particular type and may include any material having conductive properties while notcausing any chemical change to the corresponding battery. The conductive material mayinclude, for example, graphite such as natural graphite or artificial graphite; carbon blackbasedcarbon compounds such as carbon black, acetylene black, ketjen black, channel black,furnace black, lamp black, thermal black; conductive fibers such as carbon fibers or metalfibers; metal powder such as fluorocarbon, aluminum and nickel powder; conductivewhiskers such as zinc oxide, potassium titanate; conductive metal oxide such as titaniumoxide; conductive materials such as polyphenylene derivatives. Specifically, to uniformlymix the conductive material and improve conductivity, the conductive material may includeactivated carbon, graphite, carbon black, carbon nanotubes or a mixture thereof, and morespecifically carbon black.In an embodiment of the present disclosure, each unit electrode film mayindependently comprise the active material: the conductive material: the binder at a weightratio of 80 to 99 parts by weight : 0 to 10 parts by weight : 0.5 to 10 parts by weight, andspecifically 90 to 99 parts by weight : 0 to 5 parts by weight : 0.5 to 10 parts by weight.Alternatively, the weight ratio of the active material: the conductive material: the binder maybe 80 to 99 parts by weight : 0.5 to 10 parts by weight : 0.5 to 10 parts by weight, andspecifically 90 to 99 parts by weight : 0.5 to 5 parts by weight : 0.5 to 10 parts by weight.In an embodiment of the present disclosure, each unit electrode film may furtherinclude, independently, fillers to suppress the expansion of the electrode. For example, thefillers may include, without limitation, any fibrous material that does not cause a chemicalchange to the corresponding battery, and for example, an olefin-based polymer such aspolyethylene, polypropylene, glass fibers, carbon fibers or the like.In an embodiment of the present disclosure, when the MD of one of the unitelectrode films is set as a reference direction, the electrode film may have improvedmechanical properties not only in the reference direction but also in a direction that is notparallel to the reference direction.The improved mechanical properties of the electrode film according to anembodiment of the present disclosure may include tensile strength, elastic modulus andelongation at break commonly required for the electrode film, and the mechanical propertiesare not limited to a particular type.In an embodiment of the present disclosure, when measuring the tensile strength ofthe electrode film in accordance with ASTM D638, a value of TSTD / TSMD may be 0.3 ormore, the TSTD / TSMD being a ratio of the tensile strength (TSTD) measured in the directionperpendicular to the MD (the reference direction) to the tensile strength (TSMD) measured inthe MD of one of the two or more layers of unit electrode films stacked. For example,when the electrode film comprises a first unit electrode film and a second unit electrode filmstacked on the first unit electrode film such that the MD of the first unit electrode film andthe MD of the second unit electrode film are antiparallel to each other, the value ofTSTD / TSMD may be 0.3 or more, the TSTD / TSMD being a ratio of the tensile strength (TSTD)of the electrode film measured in the direction perpendicular to the MD of the first unitelectrode film to the tensile strength (TSMD) of the electrode film measured in the MD of thefirst unit electrode film.In an embodiment of the present disclosure, specifically, the ratio TSTD / TSMD maybe 0.3 or more, 0.4 or more, 0.5 or more, 0.6 or more, 0.7 or more, 0.8 or more, or 0.9 ormore, and 1 or less. With the increasing number of unit electrode films stacked in theelectrode film such that the MDs of the unit electrode films in contact with each other areantiparallel to each other, the mechanical properties of the electrode film may be uniformlyimproved in an arbitrary direction. Accordingly, with the increasing number of unitelectrode films stacked, the ratio TSTD / TSMD may converge to 1.In an embodiment of the present disclosure, when measuring the elastic modulus ofthe electrode film in accordance with ASTM D638, a value of MTD / MMD may be 0.3 or more,the MTD / MMD being a ratio of the elastic modulus (MTD) measured in the directionperpendicular to the MD (the reference direction) to the elastic modulus (MMD) measured inthe MD of one of the two or more layers of unit electrode films stacked. For example,when the electrode film comprises the first unit electrode film and the second unit electrodefilm stacked on the first unit electrode film such that the MD of the first unit electrode filmand the MD of the second unit electrode film are antiparallel to each other, the value ofMTD / MMD may be 0.3 or more, the MTD / MMD being a ratio of the elastic modulus (MTD) ofthe electrode film measured in the direction perpendicular to the MD of the first unitelectrode film to the elastic modulus (MMD) of the electrode film measured in the MD of thefirst unit electrode film.In an embodiment of the present disclosure, specifically, the ratio MTD / MMD may be0.3 or more, 0.4 or more, 0.5 or more, 0.6 or more, 0.7 or more, 0.8 or more, or 0.9 or more,and 1 or less. With the increasing number of unit electrode films stacked in the electrodefilm such that the MDs of the unit electrode films in contact with each other are antiparallelto each other, the mechanical properties of the electrode film may be uniformly improved inan arbitrary direction. Accordingly, with the increasing number of unit electrode filmsstacked, the ratio MTD / MMD may converge to 1.In another embodiment of the present disclosure, the number of unit electrode filmsstacked in the electrode film may be two or more, and specifically two to five, or two to four,or two to three. When the number of unit electrode films stacked satisfies the abovedescribedrange, it may be possible to properly maintain the thickness of the electrode film,thereby preventing the chipping of the active material due to high pressure applied whenmanufacturing the electrode film and improving the electrical properties and mechanicalproperties of the electrode film.An electrode according to another aspect of the present disclosure comprises acurrent collector and the above-described electrode film on at least one surface of the currentcollector.In an embodiment of the present disclosure, the current collector is not limited to aparticular type and may include those having high conductivity without causing anychemical change to the battery, and may include, for example, stainless steel, aluminum,nickel, titanium, sintered carbon, copper or aluminum or stainless steel treated with carbon,nickel, titanium or silver on the surface. The current collector may have microtexture onthe surface to increase the adhesion strength of the positive electrode active material, andmay come in various forms, for example, a film, a sheet, a foil, a net, a porous body, a foamand a nonwoven. Further, the current collector may be coated with a conductive primer inpart or in whole to reduce the resistance on the surface and improve the adhesion strength.Here, the conductive primer may comprise a conductive material and a binder, and theconductive material may include, without limitation, any material having conductiveproperties, and for example, a carbon-based material.A method for manufacturing the electrode film according to another aspect of thepresent disclosure includes the following steps of:obtaining a mixture comprising the active material and the binder,blending the mixture at a high temperature low shear rate to manufacture a mass ofmixture,high shear grinding the mass of mixture to manufacture the electrode powdermixture,feeding the electrode powder mixture in between a plurality of rolls to carry outcalendaring to manufacture the unit electrode film,stacking the unit electrode film in two or more layers such that the MDs of the unitelectrode films in contact with each other are antiparallel to each other to obtain a film stack,andcalendaring the film stack,wherein the step of obtaining the mixture comprising the active material and thebinder is a step of mixing the constituent components of the unit electrode film such as theactive material and the binder, and optionally the conductive material and the additive at apredetermined mix ratio to obtain the mixture.In the step of manufacturing the mixture, the mixing for obtaining the mixture isperformed to uniformly distribute the active material and the binder, and optionally theconductive material and the additive. Since these constituent components are mixed in aform of powder, the mixing method is not limited to a particular method and may include avariety of methods that enable simple mixing. However, since the method is used tomanufacture the dry electrode without solvents, the mixing may use a dry mixing process,and may be performed by putting these materials into a device such as a blender or asupermixer.In an embodiment of the present disclosure, the mixing may be performed in themixer at 5,000 rpm to 20,000 rpm for 30 seconds to 20 minutes, and specifically, at 10,000rpm to 15,000 rpm for 30 seconds to 5 minutes, to ensure uniformity.The step of manufacturing the mass of mixture is a step for fibrillizing the binder inthe mixture manufactured as described above, and may be, for example, referred to askneading.In an embodiment of the present disclosure, high shear mixing such as jet-millingmay be performed to fibrillize the binder, but low shear blending may be preferablyperformed to prevent granulation of the active material and breakage of the formed fibers.In this instance, the blending may be, for example, performed through a kneader,but is not limited thereto.In the blending step, the active material, the conductive material and the porouscarbon powder are held or connected together by the fibrillization of the binder, to form themass of mixture with 100% solids.Specifically, the blending for manufacturing the mass of mixture may be performedat 10 rpm to 100 rpm for 1 minute to 30 minutes, and specifically, at 25 rpm to 50 rpm for 3minutes to 7 minutes, and in this instance, the blending may be performed at the shear ratein a range between 10 / s and 500 / s for 1 minute to 30 minutes. More specifically, the shearrate may be in a range between 30 / s and 100 / s. Additionally, the blending step may beperformed at high temperatures and pressure conditions that are equal to or higher thannormal pressure, and more specifically, in the pressure conditions that are higher than normalpressure.In an embodiment of the present disclosure, in the step of manufacturing the massof mixture, the blending may be performed in a range between 70°C and 200°C, andspecifically in a range between 90°C and 180°C or between 90°C and 150°C. When theblending is performed at low temperature outside of the above-described temperature range,the binder is not fibrillized well during the blending and agglomeration by the blending ispoor, which makes it difficult to form a film during calendaring in the subsequent step, andwhen the blending is performed at too high temperature, the fibrillization of the binder takesplace quickly, and subsequently, the already formed fibers may be broken by too high shearforce.In an embodiment of the present disclosure, in the step of manufacturing the massof mixture, the blending may be performed at or above normal pressure, specifically 1 atmto 60 atm, or 1 atm to 30 atm, or 1 atm to 10 atm, or 1 atm to 3 atm, or 1.1 atm to 3 atm. Incase that the blending is performed under too high pressure outside of the above-describedpressure range, too high shear force and pressure is applied, the formed fibers may be brokenor the density of the mass of mixture may be too high.As described above, in an embodiment of the present disclosure, the blending maybe preferably performed by low shear mixing at high temperature and pressure conditionthat is equal to or higher than normal pressure, rather than high shear mixing.The step of manufacturing the electrode powder mixture from the mass of mixtureis a step of grinding the mass of mixture to obtain the electrode powder. To directly formthe mass of mixture into a film, a high pressure and high temperature process is required.The density of the film is too high or it fails to obtain a uniform film, so after the mass ofmixture is ground to obtain the electrode powder, calendaring is performed on the obtainedpowder.In an embodiment of the present disclosure, the grinding may be performed using ablender, or a grinder such as a cutter mill or a fine impact mill, but is not limited thereto, andspecifically, the grinding may be performed at 500 rpm to 20000 rpm for 30 seconds to 10minutes, and specifically at 1000 rpm to 10000 rpm for 30 seconds to 1 minute. When thegrinding is performed at too low rpm or for a short time outside of the above-described range,the grinding is not adequately performed, failing to form a powder of suitable size forforming a film, and when the grinding is performed at too high rpm or for a long time, manyfine particles may be formed from the mass of mixture.In an embodiment of the present disclosure, the method may further include sievingthe ground electrode powder before the calendaring after manufacturing the electrodepowder mixture. In the sieving step, the powder for the electrode having a predeterminedsize or more may be obtained by filtering the ground electrode powder using a mesh havingopenings of the predetermined size or less.Subsequently, the calendaring is performed using the electrode powder obtained asdescribed above, or the sieved electrode powder to manufacture the unit electrode film.The calendaring forms the electrode powder mixture into a film, and for example,may be a step of forming the electrode powder mixture into a film having the averagethickness of 50 μm to 600 μm through rolling.In this instance, the calendaring may be, for example, performed by rolls present onopposite sides, and in this instance, the roll temperature may be 25°C to 200°C, and therotational speed of the rolls may be 10 rpm to 50 rpm.When the calendaring step is performed, the film that performs the role of theelectrode mixture may be manufactured. The film is also called a free-standing film.When used herein, the electrode film manufactured through the calendaring isreferred to as the unit electrode film.After the calendaring, the step of obtaining the film stack includes stacking the unitelectrode film in two or more layers such that the MDs of the unit electrode films in contactwith each other are antiparallel to each other.According to an embodiment of the present disclosure, the stacking may beperformed such that the angle between the MDs of the unit electrode films in contact witheach other among the two or more layers of unit electrode films is more than 0° and 90°.The angle between the MDs of the unit electrode films in contact with each other among thetwo or more layers of unit electrode films may be, for example, more than 0° and 90° or less,specifically 10° to 90°, specifically 45° to 90°, and more specifically 85° to 90°, or 90°.According to an embodiment of the present disclosure, the film stack may be a stackof one to three unit electrode films in contact with each other such that the MDs areantiparallel to each other.According to an embodiment of the present disclosure, the unit electrode film maybe stacked in two or more layers, for example 2 to 5, 2 to 4 or 2 to 3 layers, but the presentdisclosure is not limited thereto.Subsequently, the film stack obtained as described above undergoes calendaring tomanufacture the electrode film.The calendaring of the film stack may include rolling the film stack to a thicknessof a single layer of electrode film. For example, the film stack may be rolled such that theaverage thickness of the manufactured electrode film is 50 μm to 300 μm.In this instance, the calendaring may be, for example, performed by the rolls presenton opposite sides, and in this instance, the roll temperature may be 25°C to 200°C, and therotational speed of the rolls may be 0.1 rpm to 50 rpm.Due to not comprising a solvent, the electrode film manufactured as described abovehas no or little flowability, and thus is easy to handle and may be formed into a desired shapefor use in the manufacture of various types of electrodes. In addition, when the electrodefilm is used to manufacture the electrode, it may be possible to eliminate the drying processfor solvent removal, thereby significantly improving the efficiency of the electrodemanufacturing process, and solving the problem raised in the manufacture of the dryelectrode, such as granulation of the active material or breakage of the fibrillized binder.In addition, the electrode film comprising the two or more layers of unit electrodefilms stacked such that the MDs are antiparallel to each other may exhibit the improvedmechanical properties in an arbitrary direction, thereby significantly reducing the defect ratewhen manufacturing the electrode.A method for manufacturing an electrode according to another aspect of the presentdisclosure includes laminating the above-described electrode film on at least one surface ofthe current collector.In an embodiment of the present disclosure, the lamination may be a step of rollingand attaching the electrode film to the current collector to the predetermined thickness. Thelamination may be also performed by lamination rolls, and in this instance, the laminationrolls may be maintained at the temperature of room temperature (25°C) to 200°C, but is notlimited thereto.According to an embodiment of the present disclosure, the electrode manufacturedby the manufacturing method includes the electrode film containing no solvent, and thusmay be referred to as a dry electrode.A secondary battery according to another aspect of the present disclosure is asecondary battery in which an electrode assembly comprising a positive electrode, a negativeelectrode and a separator is included in a battery case together with a lithium containingnonaqueous electrolyte, and the above-described electrode is used for at least one of thepositive electrode or the negative electrode.The detailed structure of the secondary battery is well known and its description isomitted.The secondary battery according to the present disclosure may be included as a unitbattery in an energy storage system, but the use of the present disclosure is not limited thereto.The detailed structure of the energy storage system is well known and its descriptionis omitted.Hereinafter, the present disclosure will be described in more detail throughexamples, but the following examples are provided to describe the present disclosure by wayof illustration, and the scope of the present disclosure is not limited thereto.[Manufacture of dry electrode]Comparative example 197g of lithium nickel cobalt manganese aluminum oxide (NCMA,Li[Ni0.73Co0.05Mn0.15Al0.02]O2) as a positive electrode active material, 1g of carbon black asa conductive material and 2g of polytetrafluoroethylene (PTFE) as a binder were put into ablender and mixed at 15,000 rpm for 1 minute to obtain a mixture.Subsequently, the temperature of a kneader (irie-shokai, PBV0.1) was stabilized to150°C, the manufactured mixture was put into the kneader to carry out kneading at 50 rpmfor 5 minutes under the pressure of 1.1 atm to obtain a mass of mixture.The mass of mixture was put into a blender (Hanil, HMF-3260s) to carry outgrinding at 10,000 rpm for 1 minute to obtain electrode powder.Subsequently, the manufactured electrode powder was put into a lab roll press (rolltemperature: 100°C, roll diameter: 160 mm, roll speed ratio 1.4) to manufacture a 90 μmthick electrode film.Example 1The electrode film manufactured in comparative example 1 was prepared as a unitelectrode film. The prepared unit electrode film was stacked in two layers such that anangle between MDs is 90° and put into a lab roll press (roll temperature: 100°C, roll diameter:160 mm, roll speed ratio 1.4) to carry out rolling again to manufacture a 90 μm thickelectrode film.Example 2The electrode film manufactured in comparative example 1 was prepared as a unitelectrode film. The prepared unit electrode film was stacked in two layers such that anangle between MDs is 45° and put into a lab roll press (roll temperature: 100°C, roll diameter:160 mm, roll speed ratio 1.4) to carry out rolling again to manufacture a 90 μm thickelectrode film.[Evaluation of properties]For each of the manufactured electrode films according to comparative example 1and examples 1 and 2, density, elastic modulus, tensile strength and elongation at break wereevaluated by the following method, and the results are shown in the following Tables 1 and2.In the following Table 1, the MD direction of comparative example 1 denotes therunning direction of the film when manufacturing the film (see FIG. 1), and the TD directiondenotes the direction perpendicular to the MD direction of the manufactured film.Additionally, the MD direction of example 1 denotes the MD direction of the lower layer,and the TD direction denotes the direction perpendicular to the MD direction of the lowerlayer.- Density measurement: The manufactured film was cut into 5 cm X 5 cm (horizontal dimension X verticaldimension) to prepare a sample. The density was measured by dividing the weight of thesample film by the film volume (thickness x 25 cm2).- Tensile strength measurement: The manufactured film was cut into 1 cm X 10 cm (horizontal dimension x verticaldimension) to prepare a sample. In accordance with American Society for Testing andMaterials (ASTM) D638, two ends of the prepare sample were pulled at the pre-load of 0.01kg / cm and the test speed of 50 mm / min using UTM (ZwichRoell) machine.In this instance, the tensile strength was measured by dividing the force applied tothe sample when the sample breaks by the initial cross-sectional area of the sample.- Elastic modulus measurement: The manufactured film was cut into 1 cm X 10 cm (horizontal dimension x verticaldimension) to prepare a sample. In accordance with American Society for Testing andMaterials (ASTM) D638, two ends of the prepared sample were pulled at the pre-load of0.01 kg / cm and the test speed of 50 mm / min using UTM (ZwichRoell) machine.In this instance, the elastic modulus was measured as a value obtained by dividingthe tensile strength by the strain in the linear stress-strain region.- Elongation at break: The manufactured film was cut into 1 cm X 10 cm (horizontal dimension x verticaldimension) to prepare a sample. In accordance with American Society for Testing andMaterials (ASTM) D638, the elongation at break (%) was measured using the followingequation by pulling two ends of the prepared sample at the pre-load of 0.01 kg / cm and thetest speed of 50 mm / min using UTM (ZwichRoell) machine.Elongation at break (ε) = ΔL / L0 X 100 (%)In the above equation, L0 denotes the initial length of the sample, and ΔL denotesa length change until the sample breaks.[Table 1][Table 2]As can be seen from the above results, it was confirmed that the electrode filmaccording to comparative example 1 had very poor mechanical properties in TD, while theelectrode films according to examples 1 and 2 had improved mechanical properties in MDand TD.As each of the elastic modulus, tensile strength and elongation at break is higher,the electrode film has improved stability and efficiency of the process of manufacturing theelectrode, so it was confirmed that the electrode films according to examples 1 and 2 hadhigh stability and improved efficiency of the process of manufacturing the electrode.[Description of Reference Numerals]1 - Roll10 - Electrode powder mixture100 - Unit electrode film
Claims
1. An electrode film, comprising: two or more unit electrode film stacked in two or more layers, the unit electrode film comprising a fibrillized binder and an active material, wherein machine directions (MDs) of the unit electrode films in contact with each other among the two or more stacked layers are antiparallel to each other.
2. The electrode film according to claim 1, wherein an angle between the MDs of the unit electrode films in contact with each other among the two or more layers of unit electrode films is more than 0° and 90° or less.
3. The electrode film according to claim 1, wherein an angle between the MDs of the unit electrode films in contact with each other among the two or more layers of unit electrode films is 45°to 90°.
4. The electrode film according to claim 1, wherein an average thickness of the electrode film is 50 μm to 600 μm.
5. The electrode film according to claim 1, wherein a ratio of a tensile strength measured in a direction perpendicular to the MD to a tensile strength measured in the MD of one of the two or more layers of stacked unit electrode films is 0.3 or more, wherein the tensile strength are measured in accordance with ASTM D638.
6. The electrode film according to claim 1, wherein a ratio of an elastic modulus measured in a direction perpendicular to the MD to an elastic modulus measured in the MD of one of the two or more layers of stacked unit electrode films is 0.3 or more, wherein the elastic moduli are measured in accordance with ASTM D638.
7. A method for manufacturing an electrode film, comprising: mixing an active material and a binder to make a mixture; blending the mixture at high temperature low shear conditions to make a mass of the mixture; high shear grinding the mass of the mixture to make an electrode powder mixture; feeding the electrode powder mixture in between a plurality of rolls to carry out calendaring to manufacture a unit electrode film; stacking two of more of the unit electrode film in two or more layers such that machine directions (MDs) of the unit electrode films in contact with each other are antiparallel to each other to obtain a film stack; and calendaring the film stack.
8. The method for manufacturing the electrode film according to claim 7, wherein the stacking comprises stacking such that an angle between the MDs of the unit electrode films in contact with each other among the two or more layers of unit electrode films is more than 0° and 90° or less.
9. The method for manufacturing the electrode film according to claim 7, wherein an average thickness of the electrode film is 50 μm to 600 μm.
10. An electrode, comprising: a current collector; and the electrode film according to any one of claims 1 to 6 on at least one surface of the current collector.
11. A method for manufacturing an electrode, comprising: laminating the electrode film according to any one of claims 1 to 6 on at least one surface of a current collector.
12. A secondary battery in which an electrode assembly comprising a positive electrode, a negative electrode and a separator is included in a battery case together with a lithium containing nonaqueous electrolyte, wherein at least one of the positive electrode or the negative electrode is the electrode according to claim 10.