Fabrication of a trimetallic selenide-graphene oxide electrocatalyst derived from a metal-organic framework for use in the oxygen evolution process
A trimetallic Ni.Cu.Co/GO.Se electrocatalyst addresses OER inefficiencies by optimizing proton-electron transfer and stability, achieving low overvoltage and high current density for sustainable hydrogen production.
Patent Information
- Application Number
- IR140550140003000499
- Authority / Receiving Office
- IR · IR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2026-05-02
- Publication Date
- 2026-11-04
- Estimated Expiration
- 2046-05-02
AI Technical Summary
The oxygen evolution reaction (OER) in water electrolysis is inefficient due to high overpotential, slow kinetics, and instability of existing electrocatalysts, particularly those based on noble metals like RuO₂ and IrO₂, which are costly and scarce, while cheaper alternatives suffer from structural degradation and inefficient charge transfer.
A trimetallic electrocatalyst composed of nickel, copper, and cobalt immobilized on graphene oxide with selenium modification, forming a stable, conductive structure that optimizes proton-electron co-transfer pathways and enhances active oxyhydroxide species generation, addressing the challenges of random metal distribution, stability, and charge transfer inefficiencies.
The Ni.Cu.Co/GO.Se electrocatalyst reduces overvoltage, increases current density, and ensures long-term stability, providing an economical and commercializable solution for OER with improved reaction kinetics and durability.
Smart Images

Figure 00000015_0000 
Figure 00000016_0000 
Figure 00000016_0001
Abstract
Description
Description of the invention Title of the invention Fabrication of trimetallic selenide-graphene oxide electrocatalyst derived from metal-organic framework for application in oxygen evolution process Technical background of the relevant invention This invention is in the field of electrocatalytic materials and water splitting technology, particularly in the subfield of metal-organic nanomaterials with controlled morphology and functionality tailored to rare and precious metals for the oxygen evolution reaction. Technical problem and stating the objectives of the invention With the increase in population and industrial development, the global demand for energy has increased significantly. Currently, more than 80% of the world's energy is supplied by fossil fuels, which in addition to resource limitations, has led to environmental pollution and exacerbated the phenomenon of global warming. In the meantime, hydrogen, as a clean energy carrier with very high energy density and without producing pollutants during consumption, is considered an ideal option for the future of energy. However, the main challenge is how to produce hydrogen in a sustainable and green way. Hydrogen production has various methods, one of the most attractive routes for producing green hydrogen is the electrochemical splitting of water, which we have chosen. Electrochemical water splitting is a process that involves two half-reactions: a hydrogen evolution reaction at the cathode and an oxygen evolution reaction at the anode. While the HER reaction is kinetically relatively simpler, the OER reaction is a complex four-electron process and is considered the main bottleneck of water electrolysis. Therefore, the development of efficient electrocatalysts for OER plays a crucial role in reducing energy consumption and increasing the overall system efficiency. Although noble metals such as iridium and ruthenium have high performance in OER, their high cost and limited resources hinder their widespread industrial use. Among them, carbon materials derived from metal-organic frameworks (MOFs) have received widespread attention as a new generation of electrocatalysts. Among them, our synthesized material (Ni.Cu.Co / GO.Se) is an efficient, stable and low-cost electrocatalyst for this reaction. Objectives of the invention: Provide a simple, reproducible, and relatively scalable method for preparing Ni.Cu.Co / GO.Se nanocomposites with an optimized hierarchical morphology in which the active selenide phases are uniformly distributed on a planar graphene oxide supporting framework. This structure provides effective electronic contact, increases surface roughness and porosity, and forms a continuous network for electron transport and electrolyte diffusion. Reduction of overpotential and Tafel slope in CoNiCu / GO.Se sample indicating improvement in reaction kinetics and facilitation of the rate-controlling step in OER. This result is important because it indicates that the performance improvement is not simply due to increased active surface area, but also that the reaction mechanism has been optimized. Reduction of charge transfer resistance in the CoNiCu / GO.Se sample as well as a significant increase in the mechanical and chemical stability of the structure under harsh OER reaction conditions. Providing the basis for the industrial application of CoNiCu / GO.Se electrocatalysts in the water splitting reaction with effective and economical performance. A description of the state of the prior art and the history of developments related to the claimed invention. In recent years, much research has been conducted on the development and improvement of electrocatalyst catalysts, especially those based on transition metals and multi-element compounds: Nickel and cobalt have been studied for their superior activities in OER reactions. Examples of these materials include nickel hydroxides and alloyed or oxide cobalt hydroxides, which have shown superior performance in water electrolysis and fuel cells. Research has shown that the addition of other elements such as copper or molybdenum can improve the activity and stability of these materials. Copper has been considered alongside nickel and cobalt due to its reactivity and low cost. Copper oxide compounds (e.g. CuO, Cu₂O) have been introduced in some cases as active catalysts for OER, although they require structural and surface modifications due to their lower stability. Multi-element compounds, including nickel-cobalt, nickel-copper alloys, and other combinations, have been able to provide improved performances in OER. These materials have attracted much attention in laboratory studies and experimental applications due to their diverse surface structures, tunability of surface properties, and desirable electrical properties. Molybdenum (Mo) has been used in multi-element compounds such as Mo, Ni, Co, and Cu for OER reactions due to its ability to tune surface structures and improve electrochemical activities. The relationship between multi-element structures and electrocatalytic activities has been extensively investigated. Graphene oxide (GO) is an attractive area of study in multicomponent structures due to its favorable viscosity, surface modification capabilities, and increased active surface area. GO, with its surface-active groups, allows for uniform dispersion and increased active surface area for catalyst placement, which leads to improved overall catalyst activity. The addition of GO plays an important role in increasing the stability and improving the electrical properties of multicomponent catalysts, which is important in reducing the activity loss over time. The presence of the graphene substrate, due to its high conductivity, helps to facilitate charge transfer processes and improve the ternary activity, which enables higher currents. In recent studies, compounds containing nickel, copper, cobalt, and molybdenum on a graphene oxide substrate have received significant research attention. Multi-element structures such as NiCuCoMo have shown excellent performance in catalyzing OER reactions due to their diverse surface structures and multi-molecular activities. These compounds are usually synthesized as nanoparticles on a GO substrate. Modifying surface structures and using conductive substrates leads to increased activity and reduced efficiency loss over time. Research has shown that adding molybdenum plays a role in regulating surface structures and preventing corrosion. New developments, including nanostructure control, surface modification, and the use of synthetic nanoprocesses to improve dispersion and activity, are currently emerging as the most important areas of research in parallel with the development of new materials. Providing a solution to an existing technical problem along with an accurate, sufficient, and integrated description of the invention The oxygen evolution reaction (OER) remains one of the most challenging steps in water electrolysis. This reaction limits the efficiency of electrolyzers due to its multistep nature of electron–proton transfer, slow kinetics, and the need for high overvoltages. Classical electrocatalysts based on RuO₂ and IrO₂, although highly efficient, are not suitable for widespread and commercial applications due to their high cost, metal scarcity, and limited stability under industrial conditions. On the other hand, many cheaper electrocatalysts based on transition metals such as Ni, Co, and Cu either undergo structural degradation at different pH environments or are unable to provide stable performance at high current densities due to the lack of stable active sites and inefficient charge transfer. In particular, three major technical problems stand out in non-low-cost, non-molecular electrocatalysts for OER: 1) Inefficient activation of transition metals due to random distribution of metal centers and lack of a regular coordination structure. 2) Limited stability at high voltages and gradual decomposition in alkaline or neutral environments. 3) Reduced electronic conductivity and surface charge transfer, especially when metals are dispersed as irregular nanoparticles or lack a uniform conductive substrate. The present invention introduces a metal-organic composite electrocatalyst with an engineered composition of Ni.Cu.Co / GO.Se that comprehensively addresses these challenges. This system utilizes the multi-metallic synergy between nickel, copper, and cobalt ions and immobilizes them on a graphene oxide (GO) substrate along with a selenium (Se) modifier to create an ordered, stable, and highly conductive structure. The presence of selenium plays a key role in improving stability, facilitating charge transfer, and modifying the electronic structure of the metal centers, such that PCET (proton-electron co-transfer) pathways are optimized and the ability to generate active oxyhydroxide species at low potential is enhanced. In this invention, Ni, Cu, and Co metals are immobilized in the form of organometallic sites coordinated to the oxygen groups present in GO and undergo favorable electronic rearrangement through the presence of selenium, leading to the formation of multimetallic active sites with suitable adsorption energy for the reactive species *OH, *O, and *OOH. The structural design of this electrocatalyst significantly reduces the activation energy for the key steps of O–O bond formation and significantly lowers the overvoltage required for OER. Another advantage of this system is the presence of the GO substrate as a two-dimensional conductive network, which ensures rapid charge transfer between metal centers, prevents metal aggregation or blocking, and maintains catalyst stability even at high current densities. As a result of this supported metal-organic-multimetallic design, the Ni.Cu.Co / GO.Se electrocatalyst is able to provide: Low overvoltage, high current density, long-term stability, and specific activity at the molecular level directly address the existing technical problem in the OER field and offer an innovative, economical, and commercializable path. 1-Synthesis method of nanocomposites and schematic of the electrocatalytic system Table 1 shows the specifications of the materials required to make the electrocatalysts used, along with their application and the name of the manufacturer. The synthesis of the electrocatalysts is discussed below. 1-1- Synthesis of graphene oxide In order to synthesize graphene oxide, the modified Hammers method was used. For this purpose, first a suitable container was placed in an ice bath and 360 ml of concentrated H₂SO₄ was poured into it. While stirring, 2 g of pure graphite was added to the container and stirred for 15 minutes. Then 6 g of KMnO₄ was slowly added to the mixture with vigorous stirring over a period of 1.5 hours, and after completion, the mixing process was continued for half an hour. Then, the bath temperature was increased to 35 degrees Celsius and after the temperature stabilized, the mixing was continued for about another hour. For dilution, 100 ml of distilled water was carefully added to the container and the stirrer was turned off. Then 300 ml of distilled water was poured into a larger container and the contents of the initial container were slowly transferred to the larger container and mixing was carried out for half an hour. At this stage, the bath temperature should not exceed 40 degrees Celsius. After diluting the mixture with distilled water, 20 ml of 30% hydrogen peroxide was slowly added to the container and mixing continued for half an hour. At this stage, the color of the solution briefly changed to light yellow.Then, the mixture was washed to remove ions and increase pH by adding 10% hydrochloric acid and distilled water to the mixture and using a stirrer (and centrifuge at 3000 rpm) for 10 minutes and in 5 steps. Then, the material was placed in an oven at 60 degrees Celsius for 12 hours, but it was not completely dried and turned into a brown paste. For this reason, it was placed in an oven again at 100 degrees Celsius for 12 hours to turn into hard lumps. The amount of the paste was 7.14 grams, but after drying it decreased to 3.5 grams. The synthesis schematic of this step is shown in part (a) of Figure 1. 2.1- Synthesis of metal-organic framework (NiCuCo MOF) The trimetallic metal–organic framework NiCuCo-MOF was synthesized using a modified method based on the method presented by Shahiner et al. For this purpose, 0.96 mmol (201.73 mg) of H₃BTC, 0.72 mmol (209.38 mg) of Ni(NO₃)₂·6H₂O, 0.48 mmol (115.97 mg) of Cu(NO₃)₂·3H₂O and 1.44 mmol (419.097 mg) of Co(NO₃)₂·6H₂O were poured into a reaction vessel. Then, 40 mL of DMF along with 4 mL of ethanol and 4 mL of distilled water were added to the reaction mixture. The resulting mixture was stirred for several minutes to evenly disperse the starting components in the reaction medium. After stirring, the color of the mixture changed to deep pink. Then, the reaction mixture was transferred into an autoclave and subjected to hydrothermal conditions at 140°C for 24 hours. After the reaction time, the autoclave was cooled naturally to ambient temperature. The resulting solution, which was observed to be liver-colored, was centrifuged at 3000 rpm to separate the solid product.The resulting precipitate was washed five times with ethanol and water to remove unreacted materials and residual impurities. Finally, the washed product was oven-dried at 60°C for 8 hours to obtain NiCuCo-MOF powder. 3.1- Synthesis of graphene oxide-derived MOF To add GO to MOF, 200 mg of MOF was mixed with 0.2 mL of aminopropyltriethoxysilane (APTES or (3-Aminopropyl)Triethoxysilane) and 20 mL of 2-propanol and placed on a stirrer for 24 hours and then centrifuged carefully. The resulting material was poured into 40 mL of distilled water and dissolved, and GO solution proportional to the weight of the resulting material (2 mg / mL, 60 mL) was added to the mixture (120 mg of GO in 60 mL of distilled water). The resulting mixture was placed on a stirrer for 6 hours and then centrifuged, washed, and dried at 80°C for 12 hours. The resulting powder was named NiCuCo / GO. 4.1 Synthesis of MOF-derived selenide with graphene oxide In order to synthesize the metal-organic framework derived material, 1 mmol, equivalent to 120 mg of SeO₂ was added to 30 mL of ethylene glycol in vessel number one, and then 10 mL of hydrazine was slowly added to the vessel. Next, 100 mg of CoNiCu / GO was added to the resulting solution and the vessel was placed on a stirrer for 30 min. After the formation of a single-phase solution, the contents of vessel one were transferred into an autoclave and heated at a temperature increase rate of 5 °C / min for 10 h at 140 °C. When removing the material from the oven and autoclave, the operation should be performed under a hood, because due to the presence of hydrazine, the material has a very unpleasant odor. Next, the sample was centrifuged at 3000 rpm and washed three times with water and ethanol, and then dried in an oven for 12 hours at 60 degrees Celsius, and the resulting powder was named NiCuCo / GO.Se. 5-1- The electrocatalytic system of the water splitting cell and how the reaction is carried out Figure 2 shows the schematic of the electrocatalytic system of the water splitting cell. Electrochemical water splitting, as one of the key methods for green hydrogen production, involves two separate half-cell reactions: water oxidation reaction at the anode (OER) and proton reduction reaction at the cathode (HER). This process takes place in the presence of electrolyte, electrodes, and the application of an external potential. The overall reaction for water splitting can be described by equations (1.1) to (1.5). 1–1 In an acidic environment: 1–2 1–3 Game environment: 1–4 1–5 2- Physical-chemical properties of electrocatalysts Next, the XRD, FT-IR, FE-SEM, EDX, RAMAN, and TEM characterization analyses of the synthesized materials are examined to analyze the structure of the electrocatalysts, and the results obtained are discussed. 1-2- XRD test In Figures 3 and 4, the XRD patterns of graphene oxide and MOF composite samples were recorded in the range of 0-80°. In the X-ray diffraction (XRD) analysis of graphene oxide, an intense and sharp peak at 2θ ≈ 10.5° and a broad peak at about 27° are observed. These peaks are attributed to the graphene oxide plane and indicate an increase in the interlayer distance due to the presence of oxygenated functional groups (hydroxyl, epoxy, carboxylic), which confirms the successful synthesis of GO with a high oxidation degree and a layered structure. For example, Ni.Cu.Co.MOF, the appearance of broad and moderately intense peaks at low angles (5-15 degrees) is observed. This pattern is characteristic of the formation of the MOF framework based on the BTC ligand and indicates moderate crystallinity. Also, no peaks of free metals or oxides are observed. For example, Ni.Cu.Co / GO, a decrease in the intensity of the MOF peaks and an increase in the amorphous background are observed, which is due to the disruption of the long-range order of the structure by the amorphous GO sheets, which at this stage indicates the successful synthesis of the MOF framework and the formation of its composite with GO. For the Ni.Cu.Co.Se sample, broad and new peaks are observed in the range of 2θ ≈ 30-55°, which correspond to the selenide phases of transition metals such as (Co, Ni)Se₂. The broadness of the peaks indicates the size of the microcrystals (nanostructure) and the presence of crystal defects. In relation to the final Ni.Cu.Co / GO.Se sample, a very broad and close to amorphous diffraction pattern is observed and no distinct peaks of GO or sharp crystalline phases are observed. The selenidation process leads to the formation of nanocrystalline / semi-amorphous selenide phases, and the presence of GO enhances this microcrystallinity. 2-2- FTIR test FTIR spectroscopy was used to investigate the functional groups, the maintenance of the MOF framework, and the evaluation of chemical interactions in the synthesized samples including GO, trimetallic MOF NiCuCo, NiCuCo / GO, NiCuCo.Se, and NiCuCo / GO.Se. The FTIR spectra of these materials were recorded in the wavenumber range of 400–4000 cm⁻¹, as shown in Figure 5. The FTIR spectrum of GO shows characteristic peaks that are in good agreement with previous reports in the literature. The broad band observed around 3400 cm⁻¹ is attributed to the stretching vibration of O–H groups, which is caused by hydroxyl groups as well as water adsorbed on the GO surface. The relatively strong peak in the region 1720–1730 cm⁻¹ is assigned to the C=O stretching of carboxylic groups. In addition, the peak observed around 1610–1630 cm⁻¹ is attributed to the C=C vibration of graphene sheets. The peaks located at 1220 and 1050 cm⁻¹ are also related to the C–OH and C–O (epoxy / alkoxy) vibrations, respectively. In the FTIR spectrum of Ni.Cu.Co MOF, the broad band in the region of 3400–3500 cm⁻¹ is attributed to the presence of structural water or solvent trapped in the pores of the MOF. The characteristic peaks in the regions of 1580–1600 and 1380–1400 cm⁻¹ are related to the asymmetric and symmetric stretching vibrations of the carboxylate (COO⁻) groups of the BTC ligand, respectively. The disappearance of the characteristic peak of the free C=O around 1720 cm⁻¹ indicates that the H₃BTC ligand is completely deprotonated (converting the –COOH group to –COO⁻ and forming a coordinate bond with the metal) and is bound to the metal ions. Also, the weak bands in the range of 520–600 cm⁻¹ are attributed to the vibrations of the metal–oxygen (M–O) bond, including Ni–O, Co–O and Cu–O. The FTIR spectrum of Ni.Cu.Co / GO.Se shows a combination of the characteristics of the three components GO, MOF and Se. The bands corresponding to the carboxylate groups of MOF are still detectable, indicating the stability of the MOF framework. At the same time, the intensity of the oxygenated bands of GO is reduced compared to the Ni.Cu.Co / GO sample, which may indicate the partial reduction of GO in the presence of selenium. 3-2- RAMAN test Raman spectra analysis of the initial unactivated Ni.Cu.Co / GO.Se electrode compared to the electrode after 40 h of electrocatalytic activity showed that the main GO (D and G) and MOF (C=C and COO) peaks were mostly retained, with minor changes in peak intensity or width, indicating the stability of the composite under electrocatalytic conditions. The I_D / I_G ratio may decrease slightly, indicating partial reduction of GO (rGO) during the process, but without overall degradation. This is consistent with studies on GO-MOF composites, where hybridization with GO enhances the mechanical and chemical stability of MOF. A slight shift or attenuation of the low-band peaks (200–600 cm⁻¹) is observed, which could be due to changes in metal–Se bonds or adsorption of electrocatalytic intermediate species (such as oxides or hydroxides), without any sign of framework collapse (such as disappearance of BTC peaks). These changes are similar to FTIR, where the metal environment has changed but the structure remains stable. However, stability may decrease after long cycles (due to blockage of active sites by bubbles or precipitates), as reported for similar MOFs. 4-2- TEM test In TEM analysis, the haloing of the particles is clearly visible, and the graphene oxide sheet is also visible, and it does not show porosity compared to Ni.Cu.Co / GO.Se. 5-2- FE-SEM and EDX test FESEM images of the initial GO show that the material has a well-formed, folded sheet morphology, confirming the correct synthesis and its suitability as a structural support framework. In the pure MOF sample, a relatively compact spherical particle morphology with limited interparticle contact is observed, indicating the successful formation of the MOF framework, but at the same time indicating the absence of a continuous conductive network at the electrode scale. By adding graphene oxide to the MOF structure, a significant change in morphology is observed, such that the MOF particles are distributed on the 2D and folded GO sheets. This structure indicates that GO acts as an effective physical support framework and prevents excessive particle aggregation. In the NiCuCo.Se sample, the selenidation process causes the MOF structure to rearrange and form more active metal-selenide phases that inherently have higher electrical conductivity than the original MOF. However, FESEM images show that in the absence of GO, the selenide particles tend to aggregate and form more compact structures, which leads to a decrease in the effective porosity and a restriction of charge and mass transfer pathways at the electrode scale. In contrast, the NiCuCo / GO.Se sample exhibits an optimized hierarchical morphology in which the active selenide phases are uniformly distributed on the GO sheet support framework. This structure results in effective electronic contact, increased surface roughness and porosity, and the formation of a continuous network for electron transport and electrolyte diffusion. In order to evaluate and determine the type and distribution of the constituent elements of the materials, energy dispersive X-ray spectroscopy (EDS) and elemental mapping were used to examine the synthesized samples. In the graphene oxide sample, the presence of only carbon and oxygen elements was observed, indicating the appropriate purity and correct synthesis of this material. The presence of carbon element in MOF samples is attributed to the presence of BTC organic ligand, which indicates the successful formation of metal-organic frameworks. The presence of oxygen is also attributed to the presence of organic ligand in the structure. The presence of selenium element with uniform distribution and appropriate percentage indicates the successful formation of selenide phases. The results of EDS spectra confirm the presence of expected elements in all samples and show their uniform distribution on the surface of the materials. 3- Optimization of the electrocatalytic process Various parameters, including overpotential, electron charge transfer rate and reaction kinetics, charge transfer behavior and interfacial processes, and the number of active sites and stability, have a significant impact on electrocatalytic performance. Each of these factors is investigated below and their results are presented. 1-3- Investigating excess potential In oxygen evolution reaction (OER), the reduction of the overpotential required for the initiation and progression of the reaction is considered one of the most important indicators for evaluating the activity and efficiency of electrocatalysts. Based on the results of the LSV plot, the overpotential values at a current density of 15 mA cm⁻² (η₁₅) for the NiCuCo BTC-MOF, NiCuCo / GO, NiCuCo.Se and NiCuCo / GO.Se samples were 248, 602, 346 and 204 mV, respectively. These results indicate that the NiCuCo / GO.Se sample has the lowest overpotential among all the samples and consequently exhibits the highest electrocatalytic activity for the OER reaction. The significant increase in the overpotential of the NiCuCo / GO sample compared to the pure MOF can be attributed to the electronic nature of the raw graphene oxide. Although GO can improve the dispersion of MOF particles and increase the active surface area, at higher current densities it limits the charge transfer and leads to an increase in the overpotential. In contrast, the selenidation process of the MOF framework has led to a significant decrease in the overpotential, which is attributed to the formation of metal-selenide phases with higher electrical conductivity and also to the improvement of the electronic structure of the metal active centers. The best performance is related to the NiCuCo / GO.Se sample, which is the result of the synergy between the presence of the supporting graphene oxide framework, preventing the aggregation of active phases and transforming the insulating GO into a more conductive substrate after selenidation. This structure leads to an increase in the number of active sites, improved electronic contact and reduced charge transfer resistance, and ultimately creates the lowest OER overpotential. Such behavior is consistent with previous reports on the improvement of OER activity by combining multimetallic MOFs with carbon phases and converting them into chalcogenides. 2.3- Optimal electron charge transfer rate and reaction kinetics The Tafel slope is one of the key parameters in the analysis of electrocatalytic kinetics of oxygen evolution reaction, as it shows how the change in overpotential increases the logarithm of the current density and therefore quantitatively expresses the electron charge transfer rate and reaction kinetics. In fact, a lower Tafel slope means that a lower overpotential is required to increase the current density, which indicates a higher reaction rate and better catalytic efficiency. According to the data, the lowest Tafel slope among the investigated samples belongs to NiCuCo / GO.Se, which shows the fastest OER reaction kinetics among the synthesized metal-organic frameworks. This behavior can be attributed to the key role of the higher conductivity selenide phases and the presence of the carbon support framework in improving the charge transfer pathway, so that the number of active sites is increased and more pathways for electron transfer are provided. In contrast, the NiCuCo / GO sample, despite morphological modification and increased abstract active surface area, showed a higher Tafel slope, indicating slower reaction kinetics. Also, the NiCuCo sample.Se exhibits a significant decrease in the Tafel slope compared to the raw MOF, which is consistent with the formation of selenide phases with higher structural conductivity. However, the absence of a continuous carbon support framework causes the charge transfer at the electrode surface to be incomplete and non-uniform, and therefore its kinetics cannot reach the performance of the NiCuCo / GO.Se sample. 3-3- Optimization of charge transfer behavior and interfacial processes Electrochemical impedance spectroscopy is a key tool for investigating charge transfer behavior and interfacial processes in electrocatalysts for oxygen evolution reactions. This technique allows for the separation of resistive and capacitive components of the system and helps to identify the limitations of electron and ion transport in the electrolyte and electrode surface. Nyquist plots of the studied samples were recorded in a 100 kHz to 0.1 Hz frequency range and at a constant potential in 1 M KOH solution. The Nyquist curves do not appear as classical semicircles and are more quasi-linear or elongated. Lower Rct values indicate easier charge transfer at the electrode–electrolyte interface. Among the studied samples, CoNiCu / GO.Se showed the lowest effective charge transfer resistance and the most suitable impedance response. This superior performance can be attributed to the synergy between the formation of conductive selenide phases, the presence of a graphene oxide supporting framework to create a continuous charge transport network, and the increase in the electrochemically active surface area.Such a structure facilitates simultaneous electron and ion transport and minimizes the kinetic and diffusion limitations of the OER reaction. These results are in good agreement with the LSV and Tafel slope data, confirming that the improved electrocatalytic performance of the CoNiCu / GO.Se sample is due to a real reduction in electrochemical resistances and not simply surface effects. 4.3- Optimizing the number of active sites Since electrochemical reactions occur exclusively on the effective surface of the electrode, the calculation of the electrochemical active surface area (ECSA) is one of the key parameters in evaluating the performance of electrocatalysts. Increasing the ECSA usually leads to an increase in the number of available active sites, improving charge transfer, and ultimately increasing the efficiency and rate of electrochemical reactions. The CoNiCu / GO.Se sample showed the highest Cdl value and, consequently, the largest electrochemical active surface area among all the samples investigated, such that its double layer capacitance value reached 3.7 mF cm⁻². This significant increase in Cdl and ECSA indicates the provision of a larger number of active sites and better access of the electrolyte to the electrocatalyst surface. The increase in ECSA in the CoNiCu / GO.Se sample can be attributed to the synergistic effect between the addition of multiple metals, selenidation of the MOF structure, and the presence of graphene oxide. These factors lead to improved electrical conductivity, increased effective interaction between the active phase and the carbon substrate, and the creation of a porous morphology with a higher specific surface area. As a result, the increase in double layer capacity and ECSA is directly consistent with the improvement in electrocatalytic performance observed in LSV, TOEFL slope, and EIS tests, confirming the key role of this parameter in enhancing the OER activity. 5.3- Sustainability optimization Stable performance and electrochemical durability are essential requirements for the practical application of electrocatalysts in oxygen evolution reactions, as the loss of activity over time can seriously limit the efficiency of water electrolysis systems. Therefore, evaluating the stability of electrocatalysts under practical conditions and over long time periods is an integral part of electrochemical analysis. In this study, in order to investigate the electrochemical stability, two samples, CoNiCu / GO.Se as the most active electrocatalyst and CoNiCu.Se as the sample expected to improve performance, were subjected to chronoamperometric testing. This test was performed at a constant current density of 15 mA cm⁻² and for 40 hours in 1 M KOH solution. As can be seen, the CoNiCu / GO.Se electrode showed only very slight fluctuations in potential during the 40 hours of testing, indicating good electrochemical durability and stability under alkaline conditions. This behavior indicates that the electrocatalyst structure did not undergo significant degradation during the OER reaction and its active centers remained stable. In order to further investigate the stability, cyclic voltammetry (CV) testing was also performed for these electrocatalysts. As can be seen from the curves, the CoNiCu / GO.Se electrocatalyst showed very little decrease in electrocatalytic activity after 1000 consecutive sweep cycles in the OER process. Superior stability of the CoNiCu / GO sample.Se can be attributed to the synergy between selenidation of the MOF structure, increased electrical conductivity, and uniform distribution of active phases on the graphene oxide substrate. This architecture reduces local stresses on the electrode surface, improves charge transfer, and prevents structural degradation during the OER reaction. Explanation of shapes, maps and diagrams Figure 1- Schematic of the synthesis of (a) GO, (b) CoNiCu MOF, (c) CoNiCu / GO, (d) CoNiCu / GO.Se samples. Figure 2- Schematic of the electrocatalytic water splitting system Figure 3 - X-ray diffraction (XRD) spectrum of graphene oxide Figure 4- X-ray diffraction (XRD) spectra of synthesized nanocomposites Figure 5 - Fourier transform infrared (FTIR) spectra for synthesized nanocomposites Figure 6- RAMAN spectrum of the CoNiCu / GO.Se nanocomposite electrode Figure 7 - Electron microscope images of (a) GO, (b) CoNiCu MOF, (c) CoNiCu / GO, (d) CoNiCu / GO.Se Figure 8- EDX images, (a) GO, (b) CoNiCu MOF, (c) CoNiCu / GO, (d) CoNiCu / GO.Se Figure 9- TEM images, (a) GO, (b) CoNiCu MOF, (c) CoNiCu / GO, (d) CoNiCu / GO.Se Figure 10 - Results of linear scanning voltammetry curves for the OER process for metal-organic frameworks and their derivatives in the current density range of 0 to 30 mA cm⁻² Figure 11- TOEFL slope test results for metal-organic frameworks and their derivatives in the OER process in 1 M KOH solution Figure 12 - Nyquist plots of the organometallic framework and its derivatives in 1 M KOH solution and in the frequency range 0.1–10⁵ Hz. Figure 13. Effect of CV curves in the non-Faradic region at different scan rates for (a) CoNiCu MOF, (b) CoNiCu / GO, (c) CoNiCu / GO.Se and (d) CoNiCu.Se. Figure 14 - Cathodic and anodic current difference curve as a function of scan rate for the metal-organic framework and its derivatives for calculating the electrochemically active surface area (ECSA) Figure 15- Chronopotentiometry results of the CoNiCu / GO.Se sample at a current density of 15 mA cm⁻² for 40 hours in 1 M KOH solution. Figure 16 - Results of linear scan voltammetry curves for the OER process for CoNiCu / GO.Se before and after 1000 CV cycles Table 1- Chemicals used Table 2 - Comparison of similar past work done Table 3 - Double layer capacities and electrochemical active surface area of all electrocatalysts A clear and precise statement of the advantages of the claimed invention over prior inventions. 1- Trimetallic (Ni–Cu–Co) synergism mechanism with the highest efficiency In previous inventions, usually only one or two transition metals (preferably Ni or Co) were used for OER, and their performance remained at the level of conventional oxyhydroxide networks. 2- Much higher stability in industrial currents and at high voltages 3- Significant improvement in charge transfer through graphene support and Se electronic tuning, while many previous catalysts suffer from defects in electronic conductivity and ohmic drop. 4- Clear reduction in overpotential compared to previous catalysts Typical Ni-Co catalysts have overvoltages in the range of 320–380 mV to reach 10 mA / cm². 5- Specific Activity and Higher Active Site Density 6- Reduced cost of raw materials compared to Ru and Ir-based catalysts Ru and Ir catalysts are still among the most expensive OER catalysts. 7- High compatibility with alkaline electrolyzers and different pHs Previous catalysts were mainly applicable to alkaline environments with limited conditions. 8- Completely innovative metal-organic design with a stable structure Previous examples have rarely used Ni–Cu–Co-based molecular organometallic design. Description of at least one implementation method for implementing the invention 1- Implementation method for use in alkaline electrolyzers (AWE) This invention is most compatible with alkaline electrolyzers. Implementation steps include: Synthesis of Ni.Cu.Co / GO.Se electrocatalyst in powder or thin film form Preparation of ink using solvents such as isopropanol and Nafion or PVDF as binder Coating on nickel foam (Ni-foam), stainless steel or carbon paper Drying and stabilizing the layer at ambient or low temperature Electrode assembly as electrolyzer anode In this case, the catalyst has stable and suitable performance in 1–6 M KOH environment. This method is applicable for hydrogen production on an industrial scale. 2- Implementation method for use in membrane electrolyzers (AEM Electrolyzer) In this method, the electrocatalyst is immobilized on an AEM (Anion Exchange Membrane)-based substrate. Implementation steps: Preparation of Ni.Cu.Co / GO.Se catalytic ink Spraying or doctor blade on AEM specific substrates Applying a thin layer with controlled thickness (10 to 30 microns) Gentle hot press to consolidate the layer Connection to the MEA (Membrane Electrode Assembly) Advantage: Requires lower KOH concentration; reduces system cost and corrosion. Explicit mention of the industrial application of the invention Due to its exceptional stability, low cost, superior kinetic performance, and large-scale manufacturability, the Ni.Cu.Co / GO.Se electrocatalyst has practical applications in a wide range of industries, including: Industrial production of green hydrogen Alkaline and membrane electrolyzers Reversible fuel cells Flow reactors Industrial oxygen production Commercial production of coated electrodes Electrolysis-based energy storage power plants These features indicate that the present invention is fully implementable on an industrial scale and has significant economic and practical value.
Claims
Claims What is claimed: Claim 1) The synthesis method of NiCuCO / GO.Se nanostructured electrocatalysts derived from NiCuCo MOF is novel and novel and has been synthesized to participate in the oxygen evolution reaction of water splitting and green hydrogen production. The electrical current required for this process can be supplied from renewable energy sources. Claim 2) According to claim 1, NiCuCo MOF is a trimetallic MOF synthesized by a simple two-step hydrothermal method, and after adding graphene oxide, NiCuCo / GO.Se derived from it was synthesized under a simple hydrothermal system at a temperature of 140°C and a time of 10 hours. Claim 3) According to claim 2, the NiCuCo / GO.Se sample exhibits an optimized hierarchical morphology in which the active selenide phases are uniformly distributed on the GO sheet support framework. This structure results in effective electronic contact, increased surface roughness and porosity, and the formation of a continuous network for electron transport and electrolyte diffusion.