Polyurethane elastomer for biomechanical structures and its production process
A polyurethane-based nanocomposite with nanoclay, silica fume, talc, and titanium dioxide addresses discomfort and functionality issues in prosthetics, offering improved mechanical and biological properties for comfortable, durable, and aesthetically pleasing prosthetic devices.
Patent Information
- Application Number
- IR140450140003000621
- Authority / Receiving Office
- IR · IR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-04-19
- Publication Date
- 2026-11-04
- Estimated Expiration
- 2045-04-19
AI Technical Summary
Existing prosthetic devices face issues such as discomfort, limited functionality, high weight, susceptibility to wear and tear, high cost, and difficulty in integration with the user's movement patterns, along with challenges related to skin sensitivity, sweating, and bacterial growth at the connection point.
A two-component polyurethane matrix-based elastomeric nanocomposite incorporating nanoclay nanoparticles, silica fume, talc powder, and titanium dioxide coating to enhance mechanical, biological, and aesthetic properties, providing improved tensile strength, elasticity, thermal stability, and antibacterial properties suitable for direct skin contact.
The nanocomposite material offers enhanced tensile strength, reduced density, UV resistance, and antibacterial properties, ensuring comfort, durability, and a natural appearance, making it suitable for various extracorporeal prostheses.
Smart Images

Figure 00000025_0000 
Figure 00000025_0001 
Figure 00000026_0000
Abstract
Description
Description of the invention Title of the invention Polyurethane elastomer for biomechanical structures and its production process Technical background of the relevant invention This invention is in the field of interdisciplinary knowledge of mechanics, polymers, and nanotechnology, especially artificial prostheses. Technical problem and stating the objectives of the invention A prosthetic device is a device designed to replace a body part that is usually missing due to injury, disease, or congenital condition. Prostheses can be used for various parts of the body, including limbs (arms and legs), teeth, eyes, and other organs. Past prosthetic devices had disadvantages and problems that have gradually been overcome with the advancement of science. Among the disadvantages and problems of artificial limbs are the following: Early prostheses were often uncomfortable and ill-fitting, leading to skin irritation, blisters, and other complications; Many artificial limbs lacked the ability to perform complex movements, which limited their use in daily activities; Older prostheses and devices were often heavy, making them difficult to use for long periods of time; Many materials were not resistant to wear and tear, leading to frequent replacement or repairs; Past prostheses often looked unnatural, which could affect the user's self-esteem and social interactions; Many artificial limbs required significant effort to control.They are not directly responsive to the user's movements. Advanced prosthetics and devices can be very expensive and inaccessible to many people in need. Some modern prosthetics require extensive training to use effectively, especially those that are myoelectric or bionic. High-tech prosthetics often require regular maintenance and updates, which can be burdensome for users. For electric prostheses, battery life can be a limiting factor, requiring users to plan their activities based on charging time. While progress has been made, some users still experience difficulties integrating the prosthesis into their body's movement patterns. Issues raised with current silicone gloves include loss of mechanical properties or premature rupture of prosthetic limbs, which, in addition to being heavy, also incurs high costs for the target population. Other issues and problems for some artificial prostheses include organ sweating at the connection point of existing prostheses, lack of attention to the propertiesAntibacterial and infection, skin damage, and the low lifespan of existing prostheses and their high replacement costs. The evolution of prosthetics has been accompanied by significant challenges, but ongoing research and technological advances continue to improve their performance, comfort, and accessibility. The goal of the latest developments is not only to restore lost functions, but also to improve the quality of life of users through more intuitive interfaces and personalized designs. In this patent document, nanocomposite materials are used to prepare prosthetics. The fabrication and synthesis of elastomeric nanocomposites is the main subject of the present patent document, which has optimized the properties by varying the weight percentage of matrix phase polymers, alloying and percentage of additives, as well as the method of particle fabrication and dispersion, and ultimately leads to the fabrication of prosthetic limbs. A polymer nanocomposite is a multiphase composite solid material that contains nanoscale fillers distributed within a polymer matrix phase. These fillers have dimensions less than nanometers in at least one dimension. In the present patent document, an advanced blend of elastomeric nanocomposites based on a two-component polyurethane matrix is presented, which is used for the design and production of biomechanical parts, especially extracorporeal prostheses (such as hands, feet, ears and noses). This novel blend uses four types of nano-additives including nanoclay nanoparticles, silica fume (Aerosil), talc powder and titanium dioxide (TiO₂) coating to simultaneously improve the physical, mechanical and biological properties of the material. The presented formulation has improved properties such as tensile strength, elongation, Young's modulus, tear resistance, thermal stability, density reduction, lightening, crack growth prevention and resistance to sunlight and UV radiation. The final material also has surface hydrophobicity, resistance to body perspiration, skin non-sensitivity, and antibacterial properties, making it suitable for direct skin contact and use in biomimetic equipment. A description of the state of the prior art and the history of developments related to the claimed invention. Losing a limb can be a painful process and can affect the physical and mental life of the injured person. Therefore, with mental and physical help, valuable help can be provided to the injured. An artificial prosthesis is a device designed to replace a part of the body, usually due to injury, disease or congenital conditions. Prostheses can be used for various parts of the body, including limbs (arms and legs), teeth, eyes and other organs. Their goal is to restore function and improve the quality of life of people who have lost a part of their body. The history of the use of prostheses goes back to the past, as follows: In ancient times, the use of artificial devices dates back thousands of years. The first known prosthesis is a wooden finger found on an ancient Egyptian mummy and dates back to around 1000 BC. The ancient Greeks and Romans also developed rudimentary artificial limbs. Then in the Middle Ages, during this period, prosthetics became more sophisticated but were still mainly functional rather than aesthetic.They were often made of wood and metal. During the Renaissance, there were significant advances in anatomy and surgery, which led to improved designs for prosthetics. In the 19th century, the Industrial Revolution brought new materials and manufacturing techniques that allowed for lighter and more durable prostheses. The introduction of rubber and later aluminum improved the comfort and usability of artificial limbs. In the 20th century, World Wars I and II accelerated advances in prosthetic technology due to the large number of amputees. Innovations include the development of myoelectric prostheses, which can be controlled by muscle signals. In the 21st century, modern prosthetics use advanced materials such as carbon fiber, robotics, and artificial intelligence. Bionic limbs, which can mimic natural movement and respond to neural signals, have become increasingly common.The manufacture and synthesis of elastomeric nanocomposites is the main subject of the present invention document, which has optimized the properties by changing the weight percentage of matrix phase polymers, alloying and percentage of additives, as well as the method of manufacturing and dispersing particles, and ultimately leads to the manufacture of artificial organ prostheses. Polymer nanocomposite is a multiphase composite solid material that contains nanoscale fillers distributed within a polymer matrix phase. These fillers have dimensions less than nanometers in at least one dimension. In the present invention document, an advanced combination of elastomeric nanocomposites based on a two-component polyurethane matrix is presented, which is used for the design and production of biomechanical parts, especially extracorporeal prostheses (such as hands, feet, ears and noses). This new composition utilizes four types of nano-additives, including nanoclay nanoparticles, silica fume (Aerosil), talc powder, and titanium dioxide (TiO₂) coating, to simultaneously enhance the physical, mechanical, and biological properties of the material.The proposed formulation has improved properties such as tensile strength, elongation, Young's modulus, tear resistance, thermal stability, density reduction, lightening, crack growth prevention, and resistance to sunlight and UV radiation. The final material also has surface hydrophobicity, resistance to body perspiration, skin non-sensitivity, and antibacterial properties, making it suitable for direct skin contact and use in biomimetic equipment. Among domestic inventions, the closest documents to the present invention document are: The invention entitled (Combination of polymer-based composites and metal reinforcements in the manufacture of hand prostheses) and with registration number (100933), is the design and manufacture of a hand prosthesis by implanting aluminum reinforcements among polymer-based composites, which is in the field of mechanics, biomechanics, and medical engineering. The body and parts of robotic hand prostheses (with a motor and controller) are typically made of metal and plastic (by injection molding or 3D printing), which have a low strength-to-weight ratio. On the other hand, having high strength and very low weight are two important factors in the manufacture of prostheses. To solve this problem, this invention uses carbon fiber composite fibers, which have very high strength and resistance and very low weight. In addition, to prevent damage caused by contact and crushing stresses on composite parts and subsequent looseness in the system, aluminum reinforcements have been used at the joints and pins, which are proportional to the shape and geometry of the composite parts and are placed in them.This combination can be used in the manufacture of various prostheses, especially hand prostheses that have size and weight limitations. The present invention is an innovation in the field of advanced formulation of soft polymer nanocomposites that are in direct contact with human skin and simultaneously target biological, surface and functional properties. While the above invention focuses solely on the hard and mechanical structure of a robotic hand prosthesis that uses traditional non-nano metals and fibers for strength. None of the biocompatible, antiperspirant, antibacterial or UV-resistant properties are mentioned in the above invention. Also, the type of polymer, nanoscale and multifunctionality of the formulation are considered very important innovations. In the present invention, the development of a multidimensional nanocomposite formulation for the manufacture of lightweight, biocompatible and UV-resistant shells is considered. The raw materials of the present invention include a combination of two-component polyurethane matrix materials, nanoclay nanoparticles, silica fume, talc powder, and TiO₂ coating, which are different from the raw materials of the above invention, including carbon fiber and metal reinforcement (aluminum). The invention is entitled (Passive Viscoelastic Ankle-Foot Prosthesis) and has the registration number (77726). This invention is a viscoelastic ankle-foot joint prosthesis in the field of rehabilitation engineering. Existing prostheses have fixed mechanical properties such that the behavior of these prostheses remains constant with changes in the speed or phase of walking. While one of the important characteristics of the leg muscles is adaptation to different conditions. Therefore, in order to design a prosthesis that is as similar as possible to the natural behavior of the ankle joint during walking, it seems logical to design the ankle-foot prosthesis based on the viscoelastic behavior of the anatomical ankle. Accordingly, in the above invention, the ankle-foot prosthesis for use by below-knee amputees has been designed and manufactured based on viscoelastic behavior. The innovative aspect of this invention is that the artificial ankle joint is provided by considering the elastic and elastic stiffness components, the objectives of which are to change the viscoelastic characteristics of the ankle based on the steps and speed of walking and also to adjust the position of the joint in the swing phase with the help of two actuators connected to it.The innovation of the above invention is mainly in the field of designing the mechanical and dynamic system of an artificial joint based on viscoelastic behavior and having moving components and actuators, but the present invention has innovation in the level of material design and nanocomposite formulation that can be used for the body of any type of prosthesis. The above invention is designed only for the ankle joint; but the present invention is a flexible base material that can be adapted to different molds that can be used in the nose, ear, finger and other artificial limbs. The present invention has properties such as biocompatibility, UV resistance, anti-allergy, anti-bacterial, and improved mechanical properties that the above invention lacks. No nanotechnology or engineered surface is seen in the above invention 77726; but the present invention uses silica fume, nanoclay and a plasma-modified surface that give very special properties to the material. The invention entitled (Flexible composite prosthesis for walking of the disabled with the ability to carry heavy loads (double-bladed)) and with registration number (82926) is a carbon artificial leg prosthesis that can be used for the disabled in the foot area. This prosthesis is made of carbon fibers in such a way that it has high flexibility and will provide smooth movement for the disabled person. The above invention is different from the raw materials used in the present patent document, namely carbon fibers, and the production method and process. The above invention is an engineering design for the motor and load-bearing structure of the foot at the macro level and mechanical engineering, which improves the motor efficiency of the disabled with the help of carbon fibers. In contrast, the present invention seeks to create an advanced nanoscale material with multipurpose properties for direct contact with the human skin, which, in addition to flexibility, has important properties such as high biocompatibility, resistance to UV radiation, resistance to perspiration and bacterial growth, lightness, and prevention of allergies. The invention, entitled (Acrocomposite Eye Prosthesis) and with registration number (101056), annually many people lose their eyes due to various causes, including trauma, cancer, infection, which cause serious physical, mental and psychological damage to the individual. Therefore, the construction of an artificial organ to compensate for some of the psychological damage caused to the individual is of great importance. Unfortunately, in most cases, patients who use conventional eye prostheses, the presence of the artificial eye as a foreign body causes severe sensitivity and discharge. This invention uses a 300-micron layer of composite on an acrylic artificial eye. Since composite is a very biocompatible material, it significantly reduces the rate of allergies and sensitivity of body tissues compared to acrylic. In addition, it should be noted that the composite material is more transparent than acrylic, which is why it makes the artificial eye look more beautiful and natural. Composite is also a very durable material, and its use increases the useful life of the artificial eye and prevents scratches and corrosion.The above invention differs from the raw materials used in the present invention, namely a 300 micron composite and acrylic layer with a classic composite coating, and the manufacturing method and process. Focusing on improving the appearance and reducing sensitivity in the artificial eye, the above invention uses only a composite layer to coat an acrylic structure to improve beauty, transparency and durability. While the present invention uses multiple and specialized nanoparticles not only in the surface layer, but also in the complete formulation of the matrix (polyurethane) for better mechanical performance (tensile, tear, durability), high biocompatibility, resistance to UV and body perspiration, lightness and prevention of adhesion and skin sensitivity, and has also clearly proven its difference from previous inventions by conducting a wide range of specialized tests. The invention entitled (Composite prosthetic leg for running for the disabled) and with registration number (80906), due to the inability of disabled people to run from the foot area, a composite prosthetic leg has been designed and manufactured. This leg is made of a composite composite of carbon and Kevlar fibers and, while being light in weight, is able to withstand impact loads while running. People with disabilities in the foot area can run like normal people using these prosthetic legs and even participate in running competitions. The above invention is different from the raw materials used, namely carbon and Kevlar fibers, and the production method and process. The above invention focuses on specialized sports applications (running), and the materials used are mainly carbon and Kevlar fibers, which are more related to physical properties and impact resistance during running. In contrast, the present invention takes a comprehensive look at the mechanical, surface, thermal, and biological properties of a nanocomposite formulation designed for more general application in a variety of extracorporeal prostheses.In the present invention, not only are smart and lightweight materials used, but the properties of the formulation have been proven through rigorous standard tests. The invention, titled (Construction of Artificial Muscle Based on Electrically Active Nanocomposite) and with registration number (84977), uses wheels, motors, gears, and multi-fabric joints to create structures that can move on land, in the air, or underwater. The construction of artificial muscles using IPMNCs is a major step forward in advancing the development of artificial limbs in the human body and robots with soft and flexible movements. With this invention, we will see smooth and uniform movements (which were previously uncoordinated and intermittent), much greater displacement and power (compared to other smart materials), as well as low energy consumption with remarkable efficiency in artificial muscles. There is no history in Iran of designing and manufacturing an artificial muscle solely based on polymers (IPMNCs) and also of enhancing its response by creating a uniform electrode with a nanoscale, integrated, and uniform structure.The above invention differs from the raw materials used in the present invention, namely the IPMNCs metal polymer nanocomposite, and the manufacturing method and process. The above invention seeks to create a smart muscle that responds to electrical stimulation, which is suitable for robots or active limbs. It is in the field of electronics, robotics and active biomechanics. In contrast, the present invention is designed for passive, functional and real human prostheses that are exposed to radiation, humidity, mechanical pressure, abrasion and skin contact, and must be biocompatible, durable, hypoallergenic and lightweight. The present invention does not require any electrical stimulation but uses nanotechnology to improve the properties of the base material and the contact surface of the prosthesis. Among foreign inventions, the closest documents to the present invention document are: The invention, entitled "Spherical particles comprising nanoclay-filled-polymer and methods of production and uses thereof", and registered number "US20230051250", describes methods for producing highly spherical particles by mixing a mixture comprising: (a) a filled polymer composite comprising a nanoclay dispersed in a thermoplastic polymer, (b) a carrier fluid combined with the filled thermoplastic polymer, and these two materials are not naturally miscible. Use of thermoplastic polymer: In this step, a thermoplastic polymer is used that does not itself contain nanoclay. An emulsion stabilizer may also be used. This stabilizer operates at temperatures equal to or above the melting point or softening temperature of the thermoplastic polymer. Nanoclay dispersion: The purpose of this step is to disperse the nanoclay in the composite fluid and the filled polymer. This helps to create a uniform mixture. Cooling: After preparing the mixture, it is cooled until the temperature drops below the melting point or softening temperature of the thermoplastic polymer. This step causes the formation of polymer particles filled with nanoclay.Particle Separation: Finally, the polymer particles filled with nanoclay are separated from the carrier fluid. The method of the above invention deals with the production of spherical particles using nanoclay and polymers, which is possible by controlling the temperature and various steps. The above invention is different from the present patent document. In the above invention, the thermoplastic polymer is used solely for particle formation, but the two-component polyurethane used in the present invention is of the thermosetting type and has a final non-remeltable structure that is suitable for biological applications. The focus of the above invention is on the production of small polymer particles, but the present invention is the design of a final material used directly in the manufacture of human prosthetic parts. In the present invention, an extensive set of physical, surface, chemical and biological tests have been carried out, which indicate the high performance of the product in real human body conditions. While the above invention focuses more on the particle production process and does not address the functional characteristics of the end use.The present invention has anti-UV, antibacterial, allergy-preventing, sweat-resistant, and human skin-compatible properties, such features are not mentioned in the above invention. The invention is entitled " SYSTEMS AND METHODS FOR PRODUCTION OF MATERIALS USEFUL IN ADDITIVE MANUFACTURING " and has the registration number " WO2022081913 ", in one aspect, the present disclosure refers to a method for making a material with improved tensile strength for additive manufacturing. The method can include providing a raw material with a first tensile strength. The raw material can include a polymer. The method can include providing a filler material. The filler material can include clay, single-walled carbon nanotubes, multi-walled carbon nanotubes, or boron nitride. The method can include cavitation in a hydrodynamic cavitation chamber, the raw material and the filler material to produce a material with a second tensile strength greater than the first tensile strength. The present invention differs from the above invention: the above invention focuses on producing an industrial material for 3D printing, but the present invention directly seeks to replace lost tissues of the human body with a simulated material.In the above invention, only the cavitation technique was used for dispersing nanoparticles, but in the present invention, nanoclay surface modification, fumed silica composition, and plasma method are used for surface and biological reinforcement, which is a step forward. Entitled "Fibrillated biodegradable prosthesis" and having the patent number "US20070207186", the present invention is a more durable expanded material that allows for thinner wall thicknesses and more flexible reinforcement suitable for stenting. The present invention is particularly useful in the manufacture of grafts, stents, and stent grafts that are used, for example, in repairing or replacing blood vessels that have become narrowed or blocked due to disease, aneurysmal blood vessels, or other medical treatments. The inventive materials and configurations allow for gradual expansion or contraction in size or size adjustment to achieve optimal size, shape, and fit with other objects. The present invention is also optionally capable of more precisely delivering one or more active ingredients, such as drugs, over a longer period of time. The present invention optionally includes surface modifications and additives that enhance the surface adhesion of active ingredients, coatings, or combinations thereof.Finally, the present invention optionally includes the growth of cells on the inventive material, such that the expanded, reinforced or a combination thereof is useful, for example, in the production of blood vessels or blood organs grown in the laboratory. The above invention differs from the present invention in terms of the starting materials used, since the above invention focuses on replacing internal body tissues such as vessels, whereas the present invention focuses on replacing external body structures such as nose, finger, ear, etc. The material introduced in the above invention does not make any reference to skin similarity, natural appearance, or optical properties, while the present invention is precisely designed to achieve an appearance similar to natural skin. The present invention uses advanced methods such as nanoparticle surface modification + plasma + biocompatibility and soft surface, which simultaneously optimize mechanical and appearance properties, while in the US only the adhesion of materials or drugs to the surface is important. The invention, entitled "ANIONIC LATEX AS A CARRIER FOR ACTIVE INGREDIENTS AND METHODS FOR MAKING AND USING THE SAME", and having the registration number "WO2010019180", relates to the field of polymeric materials that can be used in combination with a wide range of substrates such as personal care products, textiles, metal, cellulosic materials, plastics and the like and in the field of active agents including antimicrobial, antibacterial and antifungal agents. The invention relates more particularly to latex polymer coatings comprising at least one active ingredient, as well as methods for making and using such latex compositions. In one embodiment, the at least one additive after addition can be an inorganic component such as an inorganic pigment independently selected from pigments such as titanium oxide or zinc oxide. Black pigments such as black iron oxide; fancy or multi-colored pigments such as ultramarine or iron oxide red. Glossy pigments, metallic effect pigments, pearlescent pigments as well as fluorescent or phosphorescent pigments.The present invention differs from the above invention: the above invention is mainly designed for general coating applications such as textiles and personal care products. The present invention is specifically developed for medical aesthetic prostheses with a surface similar to human skin. The above invention seeks an active carrier for coating, but the present invention creates a bulky, three-dimensional, skin-like material that can replace visible body organs. In the present invention, a special combination of polymer + nanoclay + fumed silica + surface modification and biocompatibility is designed, which creates a natural prosthesis by controlling the surface properties, softness, appearance and mechanical performance. However, in the above invention, the goal is only to make a coating latex with various additives. The most important innovative step of the present invention is that it simultaneously combines biological (antibacterial, non-allergenic), mechanical (softness, flexibility, strength) and optical (transparency, skin-like texture) properties in a nanocomposite material. Such an advanced combination for the purpose of medical aesthetics has not been seen in previous inventions. Among foreign articles, the closest documents to the present invention document are: The article entitled "RTV silicone elastomers in hand prosthetics: Properties, applications and techniques" presents an overview of RTV (room temperature-vulcanization) silicone elastomers. The properties and applications of 3 different types of RTV silicones in the production of hand prosthetics are discussed. Vinyl polysiloxanes are excellent silicone molding materials that offer the advantages of rapid cure, fine detail, and ease of removal of the dried mold without permanent deformation. RTV-2 dimethyl polysiloxanes are ideal for mold making and prosthetic fabrication due to their desirable qualities ranging from ease of pigmenting, adjustable consistency, controllable cure speed, and accuracy in recording fine details in the liquid state to excellent stain resistance, elasticity, and biodurable properties in the vulcanized state. RTV-1 dimethyl polysiloxanes are ready-to-use, self-curing silicones that adhere well to most substrates and are useful for exterior color changes and waterproofing of the prosthesis.The treatment of the inhibition of RTV silicones by addition curing by contaminants containing sulfur, tin and nitrogen and their detrimental consequences are highlighted. A set of known contaminants is presented so that prior contact with these objects can be avoided when working with addition curing silicones. The above article differs from the present invention: in the article only commercial silicones and ready for molding and prosthetic fabrication are discussed, whereas in the present invention a novel nanocomposite with tuned properties is built on the basis of a novel nanocomposite with tuned properties. The article only examined the mechanical and process properties of silicones, whereas the present invention simultaneously provides several important properties for human bioapplication (antibacterial, natural adhesion, rheology, softness and skin-like appearance) in one material. The article is mainly about hand prostheses (functional or internal). The present invention focuses on superficial body prostheses for medical aesthetic purposes. Unlike RTV silicones that require precise molding, your material is moldable and directly usable with high flexibility and natural appearance. The article entitled "Fabrication of a glove type finger prosthesis using silicone elastomers" Maxillofacial prosthetics is an art and science that gives a realistic appearance to the patient's missing structures. Prosthetic restoration is usually considered difficult for the whole or part of the finger and is made worse when multiple fingers are involved. Conventional semi-custom finger prostheses made of polyvinyl chloride are often rejected due to poor aesthetics and tendency to stain. Rejection is frustrating for the patient as well as the prosthetist. A case report is presented in which a custom, comfortable to use and aesthetically acceptable glove prosthesis for the patient was fabricated using silicone elastomers. The above article differs from the present invention: the article is merely a case report of the fabrication of a specific finger prosthesis using silicone. However, the present invention provides a general solution that can be extended to all superficial areas of the body (face, neck, arm, ...) with a need for a natural look and feel. In the article, the fabrication method has changed but the material remains the same common elastomer.The present invention introduces a new material that, even when using conventional methods, will have a different and improved final output. The article only refers to aesthetics but does not go into details of the optical properties, texture or natural adhesion of the skin. While your material, by utilizing nanoparticles and fine-tuning the formulation, aims for transparency, colorability, softness, elasticity and adhesion similar to real skin. The present invention considers dynamic properties such as adhesion or softness to be adjustable depending on the conditions, while the article prosthesis is made with fixed properties. Providing a solution to an existing technical problem along with an accurate, sufficient, and integrated description of the invention The invention is entitled Polyurethane Elastomer for Biomechanical Structures. The main components of the product introduced in the present invention document include polyurethane elastomer grade A80 as the main material and matrix of the presented composite, modified nanoclay Cloisite 15A as a strengthening agent for mechanical and thermal properties, titanium dioxide grade Anatase as an agent for antibacterial properties, photocatalytic properties and self-cleaning, silica fume powder Aerosil grade 200 as a bulking agent, density reducer and lightening agent and talc powder as a reinforcing and strengthening agent for mechanical and thermal properties. The matrix polymer, polyurethane grade Shore 80, is a two-component material consisting of two components polyol and isocyanate in the ratio of 30 to 100, and the matrix polymer produces the target polyurethane. The main subject of the present invention is the provision of elastomeric nanocomposite prostheses that have features such as improved mechanical properties, including tear strength, reduced density and final weight of the product due to the creation of interparticle space between polymer chains in the matrix phase, the use of nanotechnology and nanostructures in the compositions of prosthetic materials, antibacterial and hydrophilic properties, elastomeric / thermoplastic-based prostheses with a new formulation reinforced with mineral and organic micro / nanomaterials with high elasticity, dimensions appropriate to the defective limb and dependent on individuals, the ability to design for individual skin color, better processability and molding with fewer defects. The manufacture and synthesis of elastomeric nanocomposites is the main subject of the present invention, which has optimized properties by changing the weight percentage of matrix phase polymers, alloying and percentage of additives, as well as the method of manufacturing and dispersion of particles, and ultimately leading to the manufacture of artificial limb prostheses. A polymer nanocomposite is a multiphase composite solid material that contains nanoscale fillers distributed within a polymer matrix phase.These fillers have dimensions less than nanometers in at least one dimension. Among the objectives of this patent document are to introduce this artificial nanocomposite prosthesis product, to obtain technical knowledge of new prosthetic materials in order to manufacture artificial limbs for patients or persons with amputations due to diseases such as tumors and occupational accidents or accidents, to improve the mechanical properties of current prostheses by replacing matrix phase polymer materials and reinforcing materials by providing better elastic, hydrophobic / friendly and antibacterial properties using the properties of photocatalytic materials, and to manufacture prototypes of prostheses based on new generation nanocomposite materials for in vitro use. Table 1 shows the composition and percentages of the ingredients of the final product. Among the raw materials used to make this prosthesis is polyurethane elastomer. Grade A80 polyurethane elastomer is a type of thermoplastic elastomer (TPE). The name "A80" usually indicates a specific hardness level that measures the hardness of rubber-like materials. In this case, A80 suggests a medium hardness that balances flexibility and durability. The higher branch of polyurethane elastomers can be classified into two main types based on their structure: thermoplastic polyurethanes and thermoset polyurethanes. Alternatives to polyurethane elastomers for the production of prosthesis include silicone elastomers, thermoplastic elastomers, ethylene vinyl acetate (EVA), natural rubber, nitrile rubber, polyethylene foam, 3D printing materials. Other raw materials used to make this prosthesis are clay nanoparticles. Modified nanoclay, specifically Cloisite 15A, is a type of organic clay that has been introduced to increase its compatibility with organic polymers.Cloisite 15A is derived from montmorillonite clay and modified with quaternary ammonium compounds to improve its dispersion in polymer matrices. This modification allows the clay to exfoliate within the polymer, resulting in enhanced properties. The higher branch of modified nanoclays usually refers to nanoclays or layered silicates, which are a class of nanomaterials that include various types of natural clays that have been modified to be more compatible with polymers. Alternatives to modified nanoclays for prosthetics include graphene, graphene oxide, carbon nanotubes, metal matrix composites (MMCs), and ceramic composites. By laminating clay nanoparticles in the polyurethane matrix phase, the properties of the polymer are improved, including reduced gas permeability, improved tensile strength, thermal stability, and flame retardancy, increased strength and modulus, better oxidative stability, resistance to solvents, and reduced biodegradation.The factor that improves the properties of nanocomposites is attributed to the very large surface area between the polymer matrix phase and the clay nanoparticles, which increases the interactions between the polymer matrix phase and the clay nanoparticles. As the clay nanoparticles are laminated, the amount of these interactions increases. Another raw material used to prepare this artificial prosthesis is titanium dioxide. Titanium dioxide is found in nature in three different states: rutile, anatase, and brookite. Anatase is a semiconductor material that is mainly used in optical coatings, photosensitive dyes, and photocatalysis due to its low cost, strong oxidation power against UV radiation, and hydrophilic nature. Anatase is characterized by its tetragonal crystal structure and is known for its unique properties, including high refractive index, UV light absorption, and photocatalytic activity. The higher branch of titanium dioxide (TiO2) primarily refers to the rutile form of titanium dioxide. Rutile is one of the three main crystalline forms of TiO2, the other two being anatase and brookite.Another raw material used to prepare this artificial prosthesis is silica foam Aerosil. Aerosil is the scientific name for silica foam, which is a lightweight and bulking agent used to increase material density and enhance adhesion properties. Aerosil powder is a type of silica or silica foam that can replace carbon black as a rubber filler. The functional benefits of Aerosil powder include scratch and abrasion resistance, lubricant and anti-caking, anti-sedimentation, thickening and shedding resistance, advanced absorption ability, and corrosion resistance. Aerosil silica is often used as a filler in polymer composites to improve mechanical properties and reduce weight. This is particularly useful in creating lightweight yet strong artificial limbs and joints, and it can be used in coatings for prosthetics and devices to enhance surface properties such as scratch resistance and durability. Alternatives to silica aerosil foam powder for the production of artificial prostheses include ethylene vinyl acetate, polylactic acid, polyhydroxyalkanoates, carbon fiber composites, and glass fiber composites.Another raw material used to prepare this artificial prosthesis is talc powder. Talc powder with the chemical formula 𝑀𝑔3[𝑆𝑖4𝑂10](𝑂𝐻)2 is a hydrous silicate material that consists of two major parts, silicon and magnesium oxides. Talc powder serves as a versatile base material in the preparation of artificial prostheses due to its beneficial properties such as moisture absorption, friction reduction, and compatibility with various materials. Its applications range from increasing comfort in artificial liners to improving the mechanical properties of composite materials, making it a valuable component in the field of prosthetics. The higher branch of talc powder falls into the category of mineral fillers, which are materials used to improve the properties of polymers and other materials. Talc, in particular, is a hydrous magnesium silicate mineral. Alternatives to talc powder for the production of artificial prostheses include calcium carbonate, silica, wood flour, and glass fibers. Artificial prosthesis product manufacturing process: Preparing the templates: Initially, Plexiglas molds were prepared for tensile strength and tear strength tests according to ASTM D882 and ASTM D624 Die C standards, respectively, and an MDF mold was also made for salt hardness testing according to ASTM D2240. After that, prototyping was carried out, which is described below in the mold and prototyping process. Figure 1 shows the steps for making a tensile test plexiglass mold and a tear test plexiglass mold. Steps for making a tensile test plexiglass mold and a tear test plexiglass mold: Plexiglass sheets and glass substrates were used to make tensile and tear test specimens. A- First, plexiglass sheets with the thickness defined in the standard (ASTM D882) were selected and then, using a laser cutting machine and according to the dimensions defined in the standard, the plexiglass sheets were cut (10), B- In the next step, the Plexiglas sheets were glued onto a glass substrate of appropriate dimensions using aquarium glue (11), C- Then it was placed at ambient temperature until the chamber was dry and ready to use (12). Figure 2 shows the steps for making a hardness test plexiglass mold. Steps for making a hardness test plexiglass mold: To make Shore hardness grade A test specimens, 10 sheets of 3 mm MDF were used and the molds were cut by laser. A- First, MDF sheets with the thickness defined in the standard (ASTM D2240) were selected and then the MDF sheets were cut using a laser cutting machine according to the dimensions defined in the standard (20), B- In the next step, the MDF sheets were glued together and all on a thicker MDF substrate of appropriate dimensions using wood glue (21), C- Then it was placed at ambient temperature until the chamber was dry and ready to use (22). Figure 3 shows the steps for making tensile specimens. Steps for making tensile specimens: (General process of making the product) A- First, two-component polyurethane resin Shor 80 was prepared as the reference matrix polymer (92-95% by weight of the total mixture) by combining two materials, polyol and isocyanate, in a ratio of 30 to 100. Foil sheets and disposable non-stick plastic containers were used for mixing, and manual and ultrasonic mixing methods were used for mixing (30). B- To make micro / nano composite and hybrid samples, first a higher density additive, namely nanoclay powder (2-3% by weight of the total composition) is added to the isocyanate (31), P- Then, silica fume aerosil powder (2-3% by weight of the total mixture) and talc powder (0.5-1% by weight of the total mixture) were added to the isocyanate and mixed and homogenized using manual mixing, mechanical mixer, and ultrasonic homogenizer at 2500 rpm, which causes high particle separation and dispersion (32). D- After that, polyol is added to the resulting mixture and mixed (33), (an important point in this section is that polyol, isocyanate, and additives should not be poured simultaneously because it leads to faster hardening and, consequently, the particles becoming lumpy, which causes uneven mixing and the composite will not have the desired quality. For this reason, additives and nanoparticles are first poured and mixed with isocyanate, and then polyol is added and mixed) E- The materials prepared from the laboratory beaker were poured into Plexiglas molds (34), C- To eliminate the bubbles created, the molds filled with the samples were placed in a vacuum oven (35), (the time range varies depending on the applied pressure). G- The molds filled with the sample materials were placed in a place with a constant level at ambient temperature until the samples were completely cured and the composite was created (36). H- After complete curing, the samples are cut according to standard dimensions and prepared for testing (37), X- In the final sample, after 3 days of initial baking, a layer of titanium dioxide (0.1–0.5% by weight of the total composition) was deposited on the sample using the solid coating method and the baking process continued at ambient temperature for another 4 days (38). The steps for making tear samples are completely similar to tensile samples, and only the tear test mold is used. The steps for making salt hardness samples are also completely similar to tensile and tear samples, and only the hardness test mold is used. The method of using the product is to take a plaster and arginal mold of the desired limb of the patient, disabled person, or veteran, and the Melt Mixing method and initial preparation of the base material. During the desired period, the mold is taken and the final product, which is the required prosthesis, is prepared. Tensile test: In order to evaluate the mechanical properties of the samples, tensile testing was performed on a universal machine according to ASTM D882 standard. Samples with approximate dimensions of 70×11×1 mm3 were cut from the original composite plates. The tensile speed was selected to be 20 mm / min and the test was performed under ambient conditions at ambient temperature. The tensile test was performed to determine the tensile properties, Young's modulus and percentage of plastic strain in film form. Steps for performing tensile tests: A- The two ends of the cut samples are completely covered with double-sided adhesive tape to prevent damage by the jaws of the tensioning device, and paper adhesive tape is used on top of it to prevent adhesion to the jaws. B- The tensile machine conducted the test at the speed specified in the standard for elastomers, and the results were reviewed and scored based on three parameters: tensile strength, elongation (maximum possible elongation), and Young's modulus, and the best results became the basis for prototyping in the next stages. Figure 4 shows the results of the tensile test, which indicates a desirable tensile strength in the final prosthesis polymer nanocomposite using nanoclay particles and silica aerosil of about 2.5%. The steps for performing tear tests are similar to tensile tests. The tear test was performed for the purpose of tear strength. Figure 5 shows the results of the tear test, which indicates a desirable tear strength in the polymer nanocomposite of the final prosthesis using nanoclay particles and silica aerosil of about 2.5%. In general, other additional tests that were performed on this introduced product include scanning calorimeter analysis tests for thermal and transfer properties, hardness tests for surface hardness properties, densitometry tests for density properties, water contact angle tests for hydrophilic and hydrophobic properties, UV radiation degradation tests for degradation under UV radiation, perspiration degradation tests for degradation due to body perspiration, skin sensitivity tests for measuring acid and alkali changes, antibacterial toxicity tests for antibacterial properties and biocompatibility, X-ray diffraction analysis tests for identifying material compounds and phases, and scanning electron microscopy tests for imaging and determining the surface morphology structure. Figure 6 shows the results of the salt hardness test, which indicates a desirable hardness strength in the final prosthesis polymer nanocomposite using nanoclay and silica aerosil particles of about 2.5%. This indicates an increase in hardness due to the composite of the polyurethane matrix phase using nano and micro additives. Figure 7 shows the results of the hardness test, which indicates an increase in the hardness of the final sample compared to the reference samples (marketed silicone and pure polyurethane). Figure 8 shows the results of the antibacterial test. Figure 9 shows the results of the density test, which indicates a low and light density of about 2.5% in the final prosthetic polymer nanocomposite using nanoclay and silica aerosil particles. In accordance with the objectives of this invention of lightening prosthetic limbs for ease of use by patients, the density property of the elastomer samples being tested is one of the important properties. Figure 10 shows the results of the field emission scanning electron microscope analysis of the final sample. The field emission scanning electron microscope analysis was performed to analyze and investigate the distribution of reinforcing particles in the base polymer matrix phase, observe and investigate the pores and internal defects of the sample under test, and investigate the adhesion of the matrix phase and additives. Figure 11 shows the results of thermal analysis (DSC) which examines the thermal properties. In this test, it was observed that the glass transition temperature of the final sample increased, indicating an increase in the thermal properties and strength of the final sample, as well as confirming proper dispersion and distribution and confirming the manufacturing process. - Polyurethane elastomer grade A80: A80 Grade Polyurethane Elastomer is a type of thermoplastic elastomer (TPE). The name "A80" usually indicates a specific hardness level that measures the hardness of the rubber-like material. In this case, A80 suggests a medium hardness that balances flexibility and durability. A80 polyurethane elastomer is often used to create socket liners for prosthetic limbs. These liners provide cushioning and comfort against the residual limb and help reduce friction and pressure. In prosthetic legs, polyurethane elastomers can be used to create flexible and durable components that mimic the natural movement of the leg. A80 polyurethane can also be used for cosmetic overlays for prosthetic limbs, providing a realistic appearance while maintaining durability and flexibility. Advantages of A80 grade polyurethane elastomer in the preparation of artificial prostheses: - Flexibility and elasticity: A80 grade elastomeric polyurethane offers high flexibility and elasticity, allowing it to withstand repeated bending and stretching without losing its shape or function. - Durability: This material is known for its high wear resistance, making it suitable for applications that require long-term performance under mechanical stress. - Chemical resistance: Elastomer polyurethanes exhibit good resistance to various chemicals, oils, and solvents, which is essential for maintaining integrity in diverse environments. - Lightweight: Compared to other materials such as metals or some rigid plastics, elastomeric polyurethanes are relatively lightweight, which is important for prosthetic applications where weight can affect the user's comfort and mobility. - Comfort: The softness and flexibility of A80 polyurethane helps provide a more comfortable fit for prosthesis users, minimizing irritation and pressure points on the skin. - Customization: This material can be easily processed and molded into various shapes, allowing for designs tailored to the user's specific needs. - Shock absorption: The elastic properties of polyurethane help absorb shock, providing greater comfort and protection for the user. -Modified nanoclay: Modified nanoclay, specifically Cloisite 15A, is a type of organic clay that has been introduced to increase its compatibility with organic polymers. Cloisite 15A is derived from montmorillonite clay and modified with quaternary ammonium compounds to improve its dispersion in polymer matrices. This modification allows the clay to exfoliate within the polymer, resulting in enhanced properties. Modified nanoclay can be used in the fabrication of prosthetic limbs to enhance mechanical properties while keeping weight low, improving comfort and mobility for the user. Some common types of modified nanoclays include: Cloisite (including Cloisite 15A, Cloisite 30B), montmorillonite, bentonite, saponite, and kaolinite. Benefits of Cloisite 15A Modified Nano Clay: - Mechanical strength: Cloisite 15A compound can significantly improve the mechanical properties of polymers, such as tensile strength and toughness, making them more durable. - Thermal stability: The presence of Cloisite 15A can improve the thermal stability of polymer composites, allowing them to withstand higher temperatures without degradation. - Lightweight: As a filler, Cloisite 15A can provide increased strength without significantly increasing weight, which is important in prosthetic applications where weight can affect comfort and usability. - Enhanced surface properties: The addition of nanoclay can improve surface properties such as hydrophobicity or hydrophilicity depending on the intended application. - Flexibility: For prostheses that require flexibility and durability (such as those used in sports), nano-clay composites can provide the necessary mechanical properties while maintaining flexibility. - Titanium dioxide grade anatase: Anatase grade titanium dioxide is one of the two primary crystalline forms of titanium dioxide (TiO2), the other being rutile. Anatase is characterized by its tetragonal crystal structure and is known for its unique properties including high refractive index, UV light absorption, and photocatalytic activity. Advantages of anatase grade titanium dioxide: - Biocompatibility: Titanium dioxide is generally considered biocompatible, making it suitable for medical applications including prosthetics, and does not cause harmful reactions in the body. - Corrosion resistance: TiO2 exhibits excellent chemical stability and corrosion resistance, which is important for prosthetic devices that may be exposed to body fluids. - Mechanical strength: When TiO2 is used in composites or as a coating, it can enhance the mechanical properties of the base materials. - Antimicrobial properties: Anatase has antimicrobial properties that can help reduce the risk of infection in prosthetic applications. - Protection against ultraviolet rays: TiO2's ability to absorb UV light can protect underlying materials from degradation caused by UV exposure, which is beneficial for prostheses used in outdoor environments. - Photocatalytic activity: Anatase grade titanium dioxide can degrade organic contaminants when exposed to UV radiation, which can be useful in self-cleaning applications or reducing biofilm formation on synthetic surfaces. - Aesthetic features: Its white color and ability to be used as a pigment can improve the aesthetic appearance of artificial dentures. Alternatives to titanium dioxide for the production of artificial prostheses include: zirconium dioxide (ZrO2), hydroxyapatite (HA), calcium phosphate ceramics, titanium alloys (e.g. Ti-6Al-4V), alumina (Al2O3). Aerosil silica foam powder: Aerosil silica fume powder is a type of fumed silica, a fine, amorphous form of silicon dioxide (SiO2) produced by the hydrolysis of silicon tetrachloride in an oxygen-rich flame. This process results in a highly porous, low-density powder with a large surface area and unique properties. Aerosil silica is often used as a filler in polymer composites to improve mechanical properties and reduce weight. This is particularly useful in creating lightweight yet strong artificial limbs and joints, and it can be used in coatings for prosthetics and devices to enhance surface properties such as scratch resistance and durability. Advantages of Aerosil silica foam powder: - Lightweight: Aerosil silica's low density makes it an ideal choice for applications where weight reduction is critical, such as prosthetics. -High surface area: With a high surface-to-volume ratio, it offers excellent bonding properties when used as a filler or composite material. Biocompatibility: Silica aerosil is considered biocompatible, making it suitable for medical applications including prosthetics. -Mechanical strength: When used as a filler in polymers or composites, it can increase the mechanical strength and durability of the final product. -Resistance to moisture: Silica aerosil is hydrophobic, which can help protect synthetic materials from moisture degradation. Talcum powder: Talc powder is a finely ground powder of talc, a natural mineral composed primarily of magnesium, silicon, and oxygen. Talc powder serves as a versatile base material in the preparation of prosthetics due to its beneficial properties such as moisture absorption, friction reduction, and compatibility with various materials. Its applications range from increasing comfort in prosthetic liners to improving the mechanical properties of composite materials, making it a valuable component in the prosthetic field. Benefits of talc powder in preparing artificial dentures: - Moisture absorption: Talcum powder can absorb moisture, which helps keep the skin dry and comfortable when used in prosthetic liners or connectors. This is especially helpful for people who may sweat under their prosthetics and devices. -Friction reduction: Powder can reduce friction between the prosthesis and the skin, minimizing irritation and discomfort. This feature is very important to ensure the user's comfort during movement. Lightweight: Talc powder is lightweight, making it an ideal additive for creating lighter synthetic components without compromising structural integrity. - Compatibility with polymers: Talc can be easily mixed with various polymers used in the manufacture of dentures and improves their physical properties such as stiffness and dimensional stability. - Affordability: Talc powder is relatively inexpensive compared to other fillers and additives, making it a cost-effective option for manufacturers. Explanation of shapes, maps and diagrams Table 1 shows the percentage composition of the ingredients of the final product. Figure 1 shows the steps for making a plexiglass tensile test mold and plexiglass mold. Figure number two shows the steps for making a Plexiglas hardness test mold. Figure 3 shows the steps for making tensile specimens. Figure 4 shows the results of the tensile test. Figure 5 shows the results of the tear test. Figure 6 shows the results of the salt hardness test. Figure 7 shows the results of the hardness test comparison. Figure 8 shows the results of the antibacterial test. Figure 9 shows the results of the density test. Figure 10 shows the results of field emission scanning electron microscopy analysis of the final sample. Figure 11 shows the results of thermal analysis (DSC). A clear and precise statement of the advantages of the claimed invention over prior inventions. Main advantage of the product: -Increasing mechanical properties using elastomer nanocomposites reinforced with nanomaterials - Reducing the density and final weight of the product due to the creation of interparticle space between the polymer chains in the matrix phase. - Paying attention to hydrophobicity issues and related characterization - Use of photocatalytic nanoparticles, including titanium dioxide, to enhance antibacterial properties - Increased lifespan due to increased desired mechanical properties -Higher tear strength than current models (silicone base) - Moisture-proof and UV-proof - Antibacterial properties -Lower density than current models (silicon-based) -Better processability and molding with fewer defects - Ability to design people's skin color - Cost-effective Description of at least one implementation method for implementing the invention Product manufacturing process: Preparing the templates: Initially, Plexiglas molds were prepared for tensile strength and tear strength tests according to ASTM D882 and ASTM D624 Die C standards, respectively, and an MDF mold was also made for salt hardness testing. After that, prototyping was carried out, which is described below in the mold making and prototyping process. Figure 1 shows the steps for making a tensile test plexiglass mold and a tear test plexiglass mold. Steps for making a tensile test plexiglass mold and a tear test plexiglass mold: Plexiglass sheets and glass substrates were used to make tensile and tear test specimens. A- First, plexiglass sheets with the thickness defined in the standard (ASTM D882) were selected and then, using a laser cutting machine and according to the dimensions defined in the standard, the plexiglass sheets were cut (10), B- In the next step, the Plexiglas sheets were glued onto a glass substrate of appropriate dimensions using aquarium glue (11), C- Then it was placed at ambient temperature until the chamber was dry and ready to use (12). Figure 2 shows the steps for making a hardness test plexiglass mold. Steps for making a hardness test plexiglass mold: To make Shore hardness grade A test specimens, 10 sheets of 3 mm MDF were used and the molds were cut by laser. A- First, MDF sheets with the thickness defined in the standard (ASTM D2240) were selected and then the MDF sheets were cut using a laser cutting machine according to the dimensions defined in the standard (20), B- In the next step, the MDF sheets were glued together and all on a thicker MDF substrate of appropriate dimensions using wood glue (21), C- Then it was placed at ambient temperature until the chamber was dry and ready to use (22). Figure 3 shows the steps for making tensile specimens. Steps for making tensile specimens: (General process of making the product) A- First, two-component polyurethane resin Shor 80 was prepared as the reference matrix polymer (92-95% by weight of the total mixture) by combining two materials, polyol and isocyanate, in a ratio of 30 to 100. Foil sheets and disposable non-stick plastic containers were used for mixing, and manual and ultrasonic mixing methods were used for mixing (30). B- To make micro / nano composite and hybrid samples, first a higher density additive, namely nanoclay powder (2-3% by weight of the total composition) is added to the isocyanate (31), P- Then, silica fume aerosil powder (2-3% by weight of the total mixture) and talc powder (0.5-1% by weight of the total mixture) were added to the isocyanate and mixed and homogenized using manual mixing methods, mechanical mixers, and ultrasonic homogenizers at 2500 rpm, which results in high particle separation and dispersion (32). T- After that, polyol was added to the resulting mixture and mixed (33). (An important point in this section is that polyol, isocyanate, and additives should not be poured simultaneously because it will lead to faster hardening and, consequently, particle clumping, which will cause uneven mixing and the composite will not have the desired quality. For this reason, additives and nanoparticles are first poured and mixed with isocyanate, and then polyol is added and mixed.) E- The materials prepared from the laboratory beaker were poured into Plexiglas molds (34), C- To eliminate the bubbles created, the molds filled with the samples were placed in a vacuum oven (35), (the time range varies depending on the applied pressure). G- The molds filled with the sample materials were placed in a place with a constant level at ambient temperature until the samples were completely cured and the composite was created (36). H- After complete curing, the samples are cut according to standard dimensions and prepared for testing (37), X- In the final sample, after 3 days of initial baking, a layer of titanium dioxide (0.1–0.5% by weight of the total composition) was deposited on the sample using the solid coating method and the baking process continued at ambient temperature for another 4 days (38). Explicit mention of the industrial application of the invention The invention is entitled Polyurethane Elastomer for Biomechanical Structures. Artificial prostheses are devices used to replace missing or defective body parts. These prostheses are used in various fields, including limb prostheses to replace hands, feet or fingers, breast prostheses, ear and nose prostheses, and eye prostheses. This product is a nanocomposite artificial prosthesis, in order to manufacture artificial limbs for patients or persons with amputations due to diseases such as tumors and occupational accidents or accidents, to improve the mechanical properties of current prostheses by replacing matrix phase polymer materials and reinforcing materials by providing better elastic, hydrophobic / friendly and antibacterial properties using the properties of photocatalytic materials, and to manufacture prototypes of prostheses based on new generation nanocomposite materials for in vitro use.
Claims
Claims What is claimed: Claim 1) Flexible nanocomposite materials for use in in vitro biomechanical structures that include the following components: a) A80 grade elastomeric polyurethane at 92 to 95 percent by weight of the total composition as a polymer matrix, b) Cloisite 15A modified nanoclay at 2 to 3 percent by weight of the total composition as a reinforcing agent, c) Anatase grade titanium dioxide at 0.1 to 0.5 percent by weight of the total composition as an antibacterial agent, d) Aerosil grade 200 silica fume powder at 2 to 3 percent by weight of the total composition as a lightening agent, e) Talc powder at 0.5 to 1 percent by weight of the total composition as a mechanical and thermal strengthening agent, such that the fillers of this polymer nanocomposite have dimensions in the nanoscale in at least one dimension. Claim 2) According to claim 1, the modified nanoclay is distributed in the polyurethane matrix in an interlayered or laminated form. Claim 3) According to claim number 1, the nanoclay used is an organically modified nanoclay and its surface is modified with quaternary ammonium compounds.Claim 4) The process for preparing flexible nanocomposite materials for making tensile specimens and artificial prostheses includes the following steps: a) Preparing two-component polyurethane elastomeric grade 80 resin from a combination of polyol and isocyanate with a weight ratio of 30 to 100 using foil sheets and disposable non-stick plastic containers and using manual and ultrasonic mixing methods, b) Adding nanoclay powder with a higher density to the isocyanate, c) Adding silica fume aerosil powder and talc powder to the isocyanate mixture and performing a homogenization process using manual mixing methods, mechanical mixer and ultrasonic homogenizer at 2500 rpm, d) Adding polyol to the resulting mixture and continuing mixing, e) Pouring the prepared materials into plexiglass molds through a laboratory beaker, c) Placing the filled molds in a vacuum oven to remove the bubbles created, g) Curing The molds were placed at ambient temperature and on a level surface to fully cure and form the composite, h) cutting the samples after fully curing, h) depositing a layer of titanium dioxide on the surface of the samples using the solid coating method after 3 days of initial curing and continuingCook for another 4 days at room temperature.