Gas sensor element

The gas sensor element addresses the issue of pressure pulsations by using slits with controlled vertical opening widths to maintain accurate gas concentration measurements by enhancing diffusion resistance and pressure loss, thereby improving measurement accuracy and responsiveness.

JP2024136538AInactive Publication Date: 2024-10-04NGK INSULATORS LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023047683
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-04
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 2024136538000001_ABST
    Figure 2024136538000001_ABST
Patent Text Reader

Abstract

To enable more effective suppression of the influence of pulsation in a measurement space on pressure of a measurement target gas in an internal space.SOLUTION: In a gas sensor according to an aspect of the present invention, at least one slit of one or more slits provided on a gas inlet side of an internal space includes a narrow portion having an average opening width of 3 μm or less in a longitudinal direction.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a gas sensor element. [Background technology]

[0002] Conventionally, oxygen and NO in gases to be measured, such as automobile exhaust gas, x Regarding gas sensor elements for detecting the concentration of specific gases such as those described above, for example, those having the following configuration are known: That is, a gas sensor element is known that includes an element substrate into whose internal space a gas to be measured is introduced from a gas inlet opening on the surface, and a measurement electrode (detection electrode) disposed in the internal space, and in which one or more slits are provided on the side of the gas inlet in the internal space.

[0003] Here, if the pressure of the measured gas in the internal space of the element substrate also changes suddenly in accordance with the sudden change in the pressure of the measured gas in the measurement space (e.g., exhaust pipe) in which the gas sensor including the above-mentioned gas sensor element is disposed, the following problem occurs. That is, the sensor output (sensor signal) of the gas sensor element may change due to the influence of the pressure change of the measured gas in the internal space of the element substrate, and the gas sensor may not be able to precisely measure the concentration of the specific gas. The change in the pressure of the measured gas in the measurement space such as the exhaust pipe in which the gas sensor is disposed is also called "pulsation". As described above, if the pressure of the measured gas in the internal space of the element substrate changes due to the pulsation in the measurement space such as the exhaust pipe, it may become difficult to precisely measure the concentration of the specific gas, so various attempts have been made to suppress the influence of such pulsation. For example, Patent Document 1 listed below discloses a gas sensor (gas sensor element) that has the following configuration to avoid the influence of the pulsation of exhaust pressure generated in the measured gas and improve the measurement accuracy at the measurement electrode (detection electrode). That is, a gas sensor (gas sensor element) is disclosed in which a diffusion control means formed of a slit for introducing the measurement gas from the external space through a gas inlet at a predetermined diffusion resistance has a dimension of one factor forming the cross-sectional shape that is equal to or smaller than a predetermined size. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2000-028576 A Summary of the Invention [Problem to be solved by the invention]

[0005] The present inventors have investigated a method for more effectively suppressing the effect of pulsation in the measurement space on the pressure of the measured gas in the internal space of the element body for a conventional gas sensor element such as that disclosed in Patent Document 1, and have identified the following phenomenon.

[0006] FIG. 8 is a diagram for explaining the cross-sectional shape of a slit in a conventional gas sensor element. Specifically, FIG. 8 shows a schematic configuration of a cross section parallel to a gas inlet of an element substrate 99 of a conventional gas sensor element. The element substrate 99 is an elongated rectangular parallelepiped including layers 4-6, each of which is an oxygen ion conductive solid electrolyte layer, and a gas to be measured is introduced into the internal space from a gas inlet opening on the surface. In the internal space of the element substrate 99, one or more slits are provided on the gas inlet side, and in the example shown in FIG. 8, slits OSl(1) and OSl(2) are provided. Specifically, the slit OSl(1) is a horizontally elongated opening provided between the upper surface of the first bridging portion 53a bridging the hollowed-out space of the layer 5 and the lower surface of the layer 6. The slit OSl(2) is a horizontally elongated opening provided between the lower surface of the first bridging portion 53a and the upper surface of the layer 4. The opening width in the vertical direction (up and down on the paper) is constant for each of the slits OSl(1) and OSl(2), and the opening width in the vertical direction is constant along the horizontal direction (left and right on the paper). That is, the slits OSl(1) and OSl(2) are each formed as a horizontally elongated opening with a constant opening width in the vertical direction. In the following description, when there is no need to distinguish between the slits OSl(1) and OSl(2), they may simply be referred to as "slits OSl". In addition, when distinguishing between the multiple slits OSl, "(1)", "(2)", "(3)", ..., "(n)", "(n+1)" are added after "OSl" to distinguish between them. "n" is an integer equal to or greater than "1".

[0007] As explained with reference to FIG. 8, in the conventional gas sensor element, one or more slits OSl are formed on the gas inlet side of the internal space of the element body 99. The slits OSl are "openings that are oblong in a cross section parallel to the gas inlet and have a constant opening width in the vertical direction"

[0008] The present inventors have repeatedly studied the above-mentioned slit "which is a horizontally elongated opening in a cross section parallel to the gas inlet and has a constant opening width in the vertical direction" formed on the gas inlet side of the internal space of the element body in a conventional gas sensor element, and have obtained the following findings: That is, the present inventors have confirmed that by devising the shape (particularly the cross-sectional shape) of the slit formed on the gas inlet side of the internal space, the effect of pulsation in the measurement space on the pressure of the measured gas in the internal space can be more effectively suppressed.

[0009] In one aspect, the present invention has been made in consideration of the above circumstances, and its object is to provide a gas sensor element in which the effect of pulsation in the measurement space on the pressure of the measured gas in the internal space of the element body is more effectively suppressed. [Means for solving the problem]

[0010] In order to solve the above-mentioned problems, the present invention employs the following configuration.

[0011] A gas sensor element according to a first aspect comprises an element substrate into which a gas to be measured is introduced through a gas inlet opening on a surface thereof, and a measurement electrode disposed in the internal space, wherein one or more slits are provided on the side of the gas inlet in the internal space, and in a cross section parallel to the gas inlet, each of the one or more slits is formed in a horizontally elongated shape, the average vertical opening width of each of the one or more slits is 3 μm or more, and at least one of the one or more slits includes one or more narrow portions, and in the cross section, the average vertical opening width of each of the one or more narrow portions is 3 μm or less.

[0012] In this configuration, the one or more slits are provided on the gas inlet side in the internal space into which the measurement gas is introduced. In the cross section parallel to the gas inlet, each of the one or more slits is formed in a horizontally elongated shape, and the average vertical opening width of each of the one or more slits is 3 μm or more. In addition, at least one of the one or more slits includes the one or more narrow portions, and in the cross section, the average vertical opening width of each of the one or more narrow portions is 3 μm or less.

[0013] The present inventors have studied a method for improving the effect of suppressing the influence of pulsation in the measurement space on the pressure of the measurement gas in the internal space with respect to a slit "provided on the side of the gas inlet in the internal space and having a horizontally elongated shape in a cross section parallel to the gas inlet." The present inventors have found that the influence of the pulsation on the pressure of the measurement gas in the internal space can be suppressed by increasing the diffusion resistance or pressure loss of the measurement gas introduced from the gas inlet into the internal space by the above-mentioned slit. In particular, the present inventors have found that the influence of the above-mentioned pulsation can be suppressed extremely effectively by configuring at least a part of the above-mentioned slit so that the average vertical opening width is 3 μm or less. In addition, the present inventors have found that the following problems arise when the average vertical opening width of the entire slit is less than 3 μm. In other words, it was found that the gas flow rate of the measured gas introduced into the internal space becomes small, and that in a gas sensor element having a slit whose average vertical opening width is less than 3 μm, the responsiveness to the measured gas deteriorates and the measurement accuracy decreases.

[0014] Therefore, in the internal space of the gas sensor element according to the first aspect, "the one or more slits, each of which has a horizontally elongated shape in a cross section parallel to the gas inlet" are provided on the side of the gas inlet. At least one of the one or more slits includes "the one or more narrow portions, each of which has an average opening width in the vertical direction of 3 μm or less." For example, the narrow portions can increase the diffusion resistance of the measurement gas introduced into the internal space. In addition, the outer periphery of the slit including the narrow portions is longer than the outer periphery of a conventional slit having a horizontally elongated rectangular cross section, so that the pressure loss of the measurement gas introduced into the internal space is also increased. Therefore, the gas sensor element according to the first aspect has an effect that the one or more narrow portions can extremely effectively suppress the influence of the pulsation in the measurement space on the pressure of the measurement gas in the internal space.

[0015] In the gas sensor element according to the first aspect, the average opening width in the vertical direction of each of the one or more slits is 3 μm or more. Therefore, the gas sensor element according to the first aspect has an advantage that it is possible to avoid a situation in which "the flow rate of the measurement gas introduced into the internal space is reduced due to the opening width of the slit in the vertical direction being made too small, resulting in deterioration of response accuracy, measurement accuracy, and the like."

[0016] Therefore, the gas sensor element according to the first aspect has the advantage that the influence of pulsation in the measurement space on the pressure of the measured gas in the internal space can be more effectively suppressed while avoiding deterioration of measurement accuracy.

[0017] A gas sensor element according to a second aspect may be the gas sensor element according to the first aspect, wherein a total lateral length of the one or more narrow portions in the cross section is 25% or more and 50% or less of a lateral length of an entire slit including the one or more narrow portions in the cross section.

[0018] In this configuration, in the gas sensor element, the total length of the one or more narrow portions in the lateral direction is 25% or more and 50% or less of the total length of the slit including the one or more narrow portions in the lateral direction. The inventors of the present invention have confirmed that when the total length of the one or more narrow portions in the lateral direction is less than 25% of the total length of the slit including the one or more narrow portions in the lateral direction, the effect of suppressing the influence of the pulsation by the one or more narrow portions is not sufficiently exhibited. In addition, the inventors of the present invention have confirmed that when the total length of the one or more narrow portions in the lateral direction is made larger than 50% of the total length of the slit in the lateral direction, the following problem occurs. That is, when the total length of the one or more narrow portions in the lateral direction is made larger than 50% of the total length of the slit in the lateral direction, it becomes difficult to sufficiently secure the gas flow rate of the measurement gas introduced into the internal space, and deterioration of responsiveness occurs. Therefore, in the gas sensor element, the total length of the one or more narrow portions in the lateral direction is set to 25% or more and 50% or less of the length of the entire slit in the lateral direction including the one or more narrow portions. With this configuration, the gas sensor element has an advantage that the narrow portions can suppress the influence of the pulsation extremely effectively while preventing deterioration of responsiveness by sufficiently securing the gas flow rate of the measurement gas introduced into the internal space.

[0019] A gas sensor element according to a third aspect is the gas sensor element according to the first or second aspect, wherein an average opening width in the vertical direction of a wide portion, which is a portion other than the one or more narrow portions of the slit including the one or more narrow portions in the cross section, may be 10 μm or less.

[0020] In this configuration, in the gas sensor element, the average vertical opening width of the wide portion, which is a portion other than the one or more narrow portions of the slit including the one or more narrow portions, is 10 μm or less. If the average vertical opening width of the wide portion is made larger than 10 μm, the effect of suppressing the influence of the pulsation by the slit, particularly by the narrow portion, decreases. Therefore, in the gas sensor element, the average vertical opening width of the wide portion is set to 10 μm or less. With this configuration, the gas sensor element exhibits the effect of extremely effectively suppressing the influence of the pulsation by the slit, particularly by the narrow portion.

[0021] A gas sensor element according to a fourth aspect is the gas sensor element according to any one of the first to third aspects, wherein the one or more slits each include the one or more narrow portions. In this configuration, in the gas sensor element, the one or more slits each include the one or more narrow portions. Therefore, the gas sensor element exhibits an effect that the influence of the pulsation can be extremely effectively suppressed by the one or more narrow portions included in each of the one or more slits.

[0022] A gas sensor element according to a fifth aspect is the gas sensor element according to any one of the first to fourth aspects, wherein, in the cross section, each of the one or more narrow portions has a constant opening width in the vertical direction.

[0023] In this configuration, in the gas sensor element, the one or more narrow portions each have a constant opening width in the vertical direction in the cross section. When the opening width of the narrow portion is constant (for example, the slit is configured to have an opening edge that changes stepwise in the cross section), the following effect is achieved compared to when the opening width is continuously changed along the horizontal direction (for example, the slit is configured to have a curved opening edge in the cross section). That is, when the opening edge of the slit is stepped, the entire circumference (perimeter) of the opening edge of the slit can be made longer than when the opening edge of the slit is curved, and the pressure loss of the measurement gas introduced into the internal space can be increased. Therefore, the gas sensor element has an effect that the influence of the pulsation can be more effectively suppressed by the one or more narrow portions each having a constant opening width in the vertical direction in the cross section.

[0024] A gas sensor element according to a sixth aspect is the gas sensor element according to any one of the first to fifth aspects, wherein at least one of the one or more slits includes one narrow portion. In this configuration, in the gas sensor element, at least one of the one or more slits includes one narrow portion. Providing a single narrow portion in the slit is easier than providing a plurality of narrow portions in the slit. Therefore, the gas sensor element has an effect that the slit including the narrow portion that extremely effectively suppresses the influence of the pulsation can be easily prepared.

[0025] A gas sensor element according to a seventh aspect is the gas sensor element according to any one of the first to sixth aspects, wherein the narrow portion is disposed at the center in the horizontal direction of a slit including the narrow portion in the cross section. In this configuration, in the gas sensor element, the narrow portion is disposed at the center in the horizontal direction of a slit including the narrow portion. Since it is easy to dispose the narrow portion at the center in the horizontal direction of the slit, the gas sensor element has an effect that the slit including the narrow portion that extremely effectively suppresses the influence of the pulsation can be easily prepared. Effect of the Invention

[0026] According to the present invention, it is possible to provide a gas sensor in which the influence of pulsation in the measurement space on the pressure of the gas to be measured in the internal space of the element substrate is more effectively suppressed. [Brief description of the drawings]

[0027] [Figure 1] FIG. 1 is a schematic cross-sectional view illustrating an example of a main configuration of a gas sensor element according to an embodiment. [Diagram 2] FIG. 2 is a diagram illustrating the cross-sectional shape of a slit in the gas sensor element of FIG. [Diagram 3] FIG. 3 is a diagram illustrating the cross-sectional shape of a slit according to the first modification. [Figure 4] FIG. 4 is a diagram illustrating the cross-sectional shape of a slit according to the second modification. [Diagram 5] FIG. 5 is a diagram illustrating the cross-sectional shape of a slit according to the third modification. [Figure 6] FIG. 6 is a diagram illustrating the cross-sectional shape of a slit according to the fourth modification. [Figure 7] FIG. 7 is a diagram illustrating the cross-sectional shape of a slit according to the fifth modification. [Figure 8] FIG. 8 is a diagram illustrating the cross-sectional shape of a slit in a conventional gas sensor element. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0028] Hereinafter, an embodiment according to one aspect of the present invention (hereinafter, also referred to as "the present embodiment") will be described with reference to the drawings. However, the present embodiment described below is merely an example of the present invention in every respect. It goes without saying that various improvements and modifications can be made without departing from the scope of the present invention. In other words, in implementing the present invention, a specific configuration according to the embodiment may be appropriately adopted.

[0029] As shown in FIG. 8, in the conventional gas sensor element, one or more slits OSl are formed on the gas inlet side of the internal space of the element body 99. The slits OSl are "openings that are oblong in a cross section parallel to the gas inlet and have a constant opening width in the vertical direction"

[0030] The present inventors have repeatedly studied the above-mentioned slit "which is a horizontally elongated opening in a cross section parallel to the gas inlet and has a constant opening width in the vertical direction" formed on the gas inlet side of the internal space of the element body in a conventional gas sensor element, and have obtained the following findings: That is, the present inventors have confirmed that by devising the shape (particularly the cross-sectional shape) of the slit formed on the gas inlet side of the internal space, the effect of pulsation in the measurement space on the pressure of the measured gas in the internal space can be more effectively suppressed.

[0031] Specifically, the present inventors have found that the above-mentioned influence of pulsation can be suppressed extremely effectively by configuring at least a part of the slit "which is provided on the gas inlet side in the internal space and is an opening with a horizontally elongated shape in a cross section parallel to the gas inlet" so that the average vertical opening width in the cross section is 3 μm or less. In addition, the present inventors have found that the following problem occurs when the average vertical opening width of the entire slit is less than 3 μm. That is, the gas flow rate of the measurement gas introduced into the internal space is reduced, and a gas sensor element having a slit with an average vertical opening width of less than 3 μm is found to have a deteriorated responsiveness to the measurement gas and a reduced measurement accuracy.

[0032] Therefore, in the internal space of the gas sensor element according to one aspect of the present invention, "the one or more slits, each of which has a horizontally elongated shape in a cross section parallel to the gas inlet" are provided on the side of the gas inlet. At least one of the one or more slits includes "one or more narrow portions, each of which has an average opening width in the vertical direction of 3 μm or less." For example, the narrow portions can increase the diffusion resistance of the measurement gas introduced into the internal space. In addition, the outer periphery of the slit including the narrow portions is longer than the outer periphery of a conventional slit having a horizontally elongated rectangular cross section, so that the pressure loss of the measurement gas introduced into the internal space is also increased. Therefore, the gas sensor element according to one aspect of the present invention has an effect that the influence of the pulsation in the measurement space on the pressure of the measurement gas in the internal space can be extremely effectively suppressed by the one or more narrow portions.

[0033] In the gas sensor element according to one aspect of the present invention, the average opening width in the vertical direction of each of the one or more slits is 3 μm or more. Therefore, the gas sensor element according to one aspect of the present invention has an advantage that it is possible to avoid a situation in which "the flow rate of the measurement gas introduced into the internal space is reduced due to an excessively small opening width in the vertical direction of the slit, resulting in deterioration of response accuracy, measurement accuracy, and the like."

[0034] Therefore, the gas sensor element according to one embodiment of the present invention has an effect of more effectively suppressing the influence of the pulsation in the measurement space on the pressure of the gas to be measured in the internal space while avoiding deterioration of the measurement accuracy. First, an overall outline of a gas sensor element 101 according to one embodiment of the present invention will be described below with reference to FIG.

[0035] [Configuration example] <Overview of gas sensors> FIG. 1 is a schematic cross-sectional view showing an example of the configuration of a gas sensor element 101. The gas sensor element 101 has, for example, a long and narrow plate shape extending along the longitudinal direction (axial direction) and is formed into, for example, a rectangular parallelepiped shape. The gas sensor element 101 shown in FIG. 1 has a front end and a rear end as ends in the longitudinal direction, and in the following description, the front end is the end on the left side of FIG. 1 (i.e., the front end), and the rear end is the end on the right side of FIG. 1 (i.e., the rear end). However, the shape of the gas sensor element 101 is not limited to this example and may be appropriately selected depending on the embodiment. In the following description, the back side of the paper in FIG. 1 is the right side of the gas sensor element 101, and the front side of the paper is the left side of the gas sensor element 101.

[0036] 1, the gas sensor element 101 includes an element substrate 100 through which a measured gas is introduced into a measured gas flow section 7 from a gas inlet 10 opening on the surface, and a measurement electrode 44 disposed in the measured gas flow section 7. The element substrate 100 is an example of the "element substrate" of the present invention, the gas inlet 10 is an example of the "gas inlet" of the present invention, and the measured gas flow section 7 is an example of the "internal space" of the present invention. The measurement electrode 44 is an example of the "measurement electrode" of the present invention.

[0037] The element substrate 100 is a laminated body formed by laminating a first substrate layer 1, a second substrate layer 2, a third substrate layer 3, a first solid electrolyte layer 4, a spacer layer 5, and a second solid electrolyte layer 6 in this order from the bottom. Each of the layers 1-6 is formed of a solid electrolyte layer having oxygen ion conductivity such as zirconia (ZrO2). The solid electrolyte forming each of the layers 1-6 may be dense. Dense refers to a porosity of 5% or less.

[0038] The element substrate 100 is manufactured, for example, by performing predetermined processing, printing of wiring patterns, and other processes on ceramic green sheets corresponding to each layer, stacking them, and further firing them to integrate them. As an example, the element substrate 100 is a laminate of multiple ceramic layers. In this embodiment, the upper surface of the second solid electrolyte layer 6 constitutes the upper surface of the element substrate 100, the lower surface of the first substrate layer 1 constitutes the lower surface of the element substrate 100, and each side surface of the layers 1 to 6 constitutes each side surface of the element substrate 100.

[0039] In this embodiment, an internal space configured to receive the measurement gas from an external space is provided at one end of the element substrate 100 between the lower surface of the second solid electrolyte layer 6 and the upper surface of the first solid electrolyte layer 4. The internal space according to this embodiment is configured such that the gas inlet 10, the first diffusion rate-limiting section 11, the buffer space 12, the second diffusion rate-limiting section 13, the first internal cavity 15, the third diffusion rate-limiting section 16, the second internal cavity 17, the fourth diffusion rate-limiting section 18, and the third internal cavity 19 are adjacently formed in a manner communicating with each other in this order. That is, the internal space according to this embodiment has a three-chamber structure (the first internal cavity 15, the second internal cavity 17, and the third internal cavity 19).

[0040] In one example, this internal space is provided by hollowing out the spacer layer 5. An upper portion of the internal space is defined by the lower surface of the second solid electrolyte layer 6. A lower portion of the internal space is defined by the upper surface of the first solid electrolyte layer 4. A side portion of the internal space is defined by the side surface of the spacer layer 5.

[0041] The first diffusion rate-controlling portion 11 is provided as one or more horizontally elongated (openings with their long sides in the direction perpendicular to the drawing) slits Sl (details of the slits Sl will be described later with reference to FIG. 2). For example, the first diffusion rate-controlling portion 11 is provided as a slit (opening) between the first cross-linked portion 53a and the layer 6, and between the first cross-linked portion 53a and the layer 4. The second diffusion rate-controlling portion 13, the third diffusion rate-controlling portion 16, and the fourth diffusion rate-controlling portion 18 are each provided as a hole whose length extending in the direction perpendicular to the drawing is shorter than that of the first internal space 15, the second internal space 17, and the third internal space 19, respectively. The second diffusion rate-controlling portion 13 may be provided as a slit (opening) between the second cross-linked portion 53b and the layer 6, and between the second cross-linked portion 53b and the layer 4. The third diffusion rate-controlling portion 16 may be provided as a slit (opening) between the third crosslinked portion 53c and the layer 6, and between the third crosslinked portion 53c and the layer 4. The fourth diffusion rate-controlling portion 18 may be provided as a slit (opening) between the fourth crosslinked portion 53d and the layer 6.

[0042] As illustrated in FIG. 1, the second diffusion rate-controlling section 13 and the third diffusion rate-controlling section 16 may be provided as two horizontally elongated slits (the opening has a long side direction perpendicular to the drawing) similar to the first diffusion rate-controlling section 11. In contrast, the fourth diffusion rate-controlling section 18 is provided as a single horizontally elongated slit (the opening has a longitudinal direction perpendicular to the drawing) formed as a gap with the lower surface of the second solid electrolyte layer 6. However, the fourth diffusion rate-controlling section 18 may be provided as two horizontally elongated slits (the opening has a long side direction perpendicular to the drawing) similar to the first diffusion rate-controlling section 11. The second diffusion rate-controlling section 13, the third diffusion rate-controlling section 16, and the fourth diffusion rate-controlling section 18 will be described in detail later. The portion (internal space) from the gas inlet 10 to the third internal space 19 is referred to as the measurement gas flow section 7.

[0043] A reference gas introduction space 43 is provided between the upper surface of the third substrate layer 3 and the lower surface of the spacer layer 5 at a position farther from the tip side (the front side of the gas sensor element 101 (element body 100)) than the measurement gas flow section 7, and at a position defined by the side surface of the first solid electrolyte layer 4. A reference gas such as the atmosphere is introduced into the reference gas introduction space 43. However, the configuration of the element body 100 is not limited to this example. As another example, the first solid electrolyte layer 4 may be configured to extend to the rear end of the element body 100, and the reference gas introduction space 43 may be omitted. In this case, the atmosphere introduction layer 48 may be configured to extend to the rear end of the element body 100.

[0044] An air introduction layer 48 is provided on a portion of the upper surface of the third substrate layer 3 adjacent to the reference gas introduction space 43. The air introduction layer 48 is made of porous alumina, and is configured so that the reference gas is introduced through the reference gas introduction space 43. In addition, the air introduction layer 48 is formed so as to cover the reference electrode 42.

[0045] The reference electrode 42 is formed so as to be sandwiched between the upper surface of the third substrate layer 3 and the first solid electrolyte layer 4, and is surrounded by an air introduction layer 48 connected to the reference gas introduction space 43. The reference electrode 42 is used to measure the oxygen concentration (oxygen partial pressure) in the first internal space 15 and the second internal space 17. Details will be described later.

[0046] The gas inlet 10 is a portion of the measurement gas flow section 7 that opens to the external space. The element substrate 100 is configured to take in the measurement gas from the external space through the gas inlet 10. In this embodiment, as illustrated in FIG. 1, the gas inlet 10 is disposed on the tip surface (front surface) of the gas sensor element 101 (element substrate 100). That is, the measurement gas flow section 7 is configured to have an opening on the tip surface of the element substrate 100. However, it is not essential that the measurement gas flow section 7 has an opening on the tip surface of the element substrate 100, that is, that the gas inlet 10 is disposed on the tip surface of the element substrate 100. It is sufficient for the element substrate 100 to be able to take in the measurement gas from the external space into the measurement gas flow section 7, and the gas inlet 10 may be disposed on the right surface or the left surface of the element substrate 100, for example.

[0047] The first diffusion rate-controlling part 11 is a part that imparts a predetermined diffusion resistance to the measurement gas taken in through the gas inlet 10. The first diffusion rate-controlling part 11 is a slit Sl provided on the inlet side of the internal space (measurement gas flow part 7) of the gas sensor element 101 (element body 100), i.e., on the gas inlet 10 side.

[0048] The buffer space 12 is a space provided for guiding the measurement gas introduced from the first diffusion rate-controlling portion 11 to the second diffusion rate-controlling portion 13 .

[0049] The second diffusion rate-controlling portion 13 is a portion that imparts a predetermined diffusion resistance to the measurement gas introduced from the buffer space 12 into the first internal space 15 .

[0050] When the measurement gas is introduced from the external space (e.g., the measurement space) of the gas sensor element 101 (element substrate 100) into the first internal space 15, the measurement gas may be suddenly taken into the element substrate 100 from the gas inlet 10 due to pressure fluctuations of the measurement gas in the external space (exhaust pressure pulsations if the measurement gas is automobile exhaust gas). Even in this case, in this configuration, the measurement gas is not introduced directly into the first internal space 15, but is introduced into the first internal space 15 after the concentration fluctuations of the measurement gas are cancelled through the first diffusion rate-controlling section 11, the buffer space 12, and the second diffusion rate-controlling section 13. As a result, the concentration fluctuations of the measurement gas introduced into the first internal space 15 are almost negligible.

[0051] The first internal space 15 is provided as a space for adjusting the oxygen partial pressure in the measurement gas introduced through the second diffusion rate-controlling part 13. The oxygen partial pressure is adjusted by the operation of the main pump cell 21.

[0052] The main pump cell 21 is an electrochemical pump cell including an inner pump electrode 22, an outer pump electrode 23, and a second solid electrolyte layer 6 sandwiched between these electrodes. The inner pump electrode 22 has a ceiling electrode portion 22a provided on almost the entire lower surface of the second solid electrolyte layer 6 adjacent to (facing) the first internal space 15. The outer pump electrode 23 is provided in a region corresponding to the ceiling electrode portion 22a on the upper surface of the second solid electrolyte layer 6 in a manner adjacent to the external space.

[0053] The inner pump electrode 22 is formed across the upper and lower solid electrolyte layers (the second solid electrolyte layer 6 and the first solid electrolyte layer 4) that define the first internal space 15, and the spacer layer 5 that provides the side walls. Specifically, a ceiling electrode portion 22a is formed on the lower surface of the second solid electrolyte layer 6 that provides the ceiling surface of the first internal space 15, and a bottom electrode portion 22b is formed on the upper surface of the first solid electrolyte layer 4 that provides the bottom surface. Then, side electrode portions (not shown) are formed on the side wall surfaces (inner surfaces) of the spacer layer 5 that constitute both side wall portions of the first internal space 15 so as to connect to the ceiling electrode portion 22a and the bottom electrode portion 22b. That is, the inner pump electrode 22 is arranged in a tunnel-shaped structure at the arrangement portion of the side electrode portion.

[0054] The inner pump electrode 22 and the outer pump electrode 23 are formed as porous cermet electrodes (for example, cermet electrodes made of Pt and ZrO2 containing 1% Au). The inner pump electrode 22, which comes into contact with the measurement gas, is used to measure nitrogen oxides (NO x ) are formed using materials that have weakened reducing ability against the components.

[0055] The gas sensor element 101 (element base 100) is configured to be able to pump oxygen in the first internal space 15 out to the external space, or pump oxygen in the external space into the first internal space 15, by applying a desired pump voltage Vp0 between the inner pump electrode 22 and the outer pump electrode 23 in the main pump cell 21, and flowing a pump current Ip0 in a positive or negative direction between the inner pump electrode 22 and the outer pump electrode 23.

[0056] In addition, in order to detect the oxygen concentration (oxygen partial pressure) in the atmosphere in the first internal space 15, the inner pump electrode 22, the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, the third substrate layer 3, and the reference electrode 42 constitute an oxygen partial pressure detection sensor cell 80 for controlling the main pump (i.e., an electrochemical sensor cell).

[0057] The gas sensor element 101 (element substrate 100) is configured to be able to identify the oxygen concentration (oxygen partial pressure) in the first internal space 15 by measuring the electromotive force V0 in the main pump control oxygen partial pressure detection sensor cell 80. Furthermore, the pump current Ip0 is controlled by feedback controlling Vp0 so that the electromotive force V0 is constant. This makes it possible to maintain the oxygen concentration in the first internal space 15 at a predetermined constant value.

[0058] The third diffusion rate-controlling section 16 is a section that applies a predetermined diffusion resistance to the measurement gas whose oxygen concentration (oxygen partial pressure) has been controlled by the operation of the main pump cell 21 in the first internal space 15, and guides the measurement gas to the second internal space 17.

[0059] The second internal space 17 is provided as a space for further adjusting the oxygen partial pressure in the measurement gas introduced through the third diffusion-controlling part 16. The oxygen partial pressure is adjusted by the operation of the auxiliary pump cell 50.

[0060] The auxiliary pump cell 50 is an auxiliary electrochemical pump cell composed of an auxiliary pump electrode 51, an outer pump electrode 23 (not limited to the outer pump electrode 23, but any appropriate electrode on the outside of the element substrate 100 will suffice), and the second solid electrolyte layer 6. The auxiliary pump electrode 51 has a ceiling electrode portion 51a provided on almost the entire lower surface of the second solid electrolyte layer 6 facing the second internal space 17.

[0061] The auxiliary pump electrode 51 is disposed in the second internal space 17 in a tunnel-shaped structure similar to the inner pump electrode 22 provided in the first internal space 15. That is, a ceiling electrode portion 51a is formed on the lower surface of the second solid electrolyte layer 6 that provides the ceiling surface of the second internal space 17, and a bottom electrode portion 51b is formed on the upper surface of the first solid electrolyte layer 4 that provides the bottom surface of the second internal space 17. Side electrode portions (not shown) connecting the ceiling electrode portion 51a and the bottom electrode portion 51b are formed on both wall surfaces of the spacer layer 5 that provide the side walls of the second internal space 17. As a result, the auxiliary pump electrode 51 has a tunnel-shaped structure.

[0062] Like the inner pump electrode 22, the auxiliary pump electrode 51 is also made of a material with a weakened ability to reduce nitrogen oxide components in the measurement gas.

[0063] The gas sensor element 101 (element base 100) is configured so that, by applying a desired voltage Vp1 between the auxiliary pump electrode 51 and the outer pump electrode 23 in the auxiliary pump cell 50, oxygen in the atmosphere within the second internal space 17 can be pumped out to the external space or pumped in from the external space into the second internal space 17.

[0064] In addition, in order to control the oxygen partial pressure in the atmosphere within the second internal space 17, the auxiliary pump electrode 51, the reference electrode 42, the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, and the third substrate layer 3 constitute an oxygen partial pressure detection sensor cell 81 for controlling the auxiliary pump (i.e., an electrochemical sensor cell).

[0065] The auxiliary pump cell 50 pumps with the variable power supply 52, the voltage of which is controlled based on the electromotive force V1 detected by the auxiliary pump control oxygen partial pressure detection sensor cell 81. As a result, the oxygen partial pressure in the atmosphere in the second internal space 17 is adjusted to NO x The partial pressure is controlled to a low level that has virtually no effect on the measurement of

[0066] In addition, the pump current Ip1 is used to control the electromotive force of the main pump control oxygen partial pressure detection sensor cell 80. Specifically, the pump current Ip1 is input as a control signal to the main pump control oxygen partial pressure detection sensor cell 80, and the electromotive force V0 is controlled so that the gradient of the oxygen partial pressure in the measurement gas introduced from the third diffusion rate-controlling portion 16 into the second internal space 17 is always constant. x When used as a sensor, the oxygen concentration in the second internal space 17 is maintained at a constant value of about 0.001 ppm by the action of the main pump cell 21 and the auxiliary pump cell 50.

[0067] The fourth diffusion rate-controlling section 18 is a section that applies a predetermined diffusion resistance to the measurement gas whose oxygen concentration (oxygen partial pressure) has been controlled by the operation of the auxiliary pump cell 50 in the second internal space 17, and guides the measurement gas to the third internal space 19.

[0068] The third internal space 19 is a space for absorbing nitrogen oxides (NO x The space is provided for carrying out the process related to the measurement of NO concentration. x The concentration is measured by the operation of the measuring pump cell 41. In this embodiment, after the oxygen concentration (oxygen partial pressure) is adjusted in advance in the first internal space 15, the oxygen partial pressure of the measurement gas introduced into the second internal space 17 through the third diffusion rate-controlling section 16 is further adjusted by the auxiliary pump cell 50. This makes it possible to keep the oxygen concentration of the measurement gas introduced from the second internal space 17 to the third internal space 19 constant with high accuracy. Therefore, the gas sensor element 101 according to this embodiment can measure NO x It becomes possible to measure the concentration.

[0069] The measurement pump cell 41 measures the nitrogen oxide concentration in the measurement gas in the third internal space 19. The measurement pump cell 41 is an electrochemical pump cell including a measurement electrode 44, an outer pump electrode 23, a second solid electrolyte layer 6, a spacer layer 5, and a first solid electrolyte layer 4. In the example of FIG. 1, the measurement electrode 44 is provided on the upper surface of the first solid electrolyte layer 4 adjacent to (facing) the third internal space 19.

[0070] The measurement electrode 44 is a porous cermet electrode. The measurement electrode 44 detects NO 2 present in the atmosphere in the third internal space 19. x Reduce NO x 1, the measurement electrode 44 is exposed in the third internal space 19. In another example, the measurement electrode 44 may be covered with a diffusion-controlling portion. The diffusion-controlling portion may be made of a porous membrane mainly composed of alumina (Al2O3). The diffusion-controlling portion controls the NO 2 flowing into the measurement electrode 44. xIt also acts as a protective film for the measurement electrode 44.

[0071] The gas sensor element 101 is configured so as to pump out oxygen produced by decomposition of nitrogen oxides in the atmosphere surrounding the measurement electrode 44 in the measurement pump cell 41, and to be able to detect the amount of oxygen produced as a pump current Ip2.

[0072] In order to detect the oxygen partial pressure around the measurement electrode 44, the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, the third substrate layer 3, the measurement electrode 44, and the reference electrode 42 constitute a measurement pump control oxygen partial pressure detection sensor cell 82 (i.e., an electrochemical sensor cell). The variable power supply 46 is controlled based on the voltage (electromotive force) V2 detected by the measurement pump control oxygen partial pressure detection sensor cell 82.

[0073] The measurement gas introduced into the third internal space 19 reaches the measurement electrode 44 under conditions in which the oxygen partial pressure is controlled. Nitrogen oxides in the measurement gas around the measurement electrode 44 are reduced (2NO→N2+O2) to generate oxygen. The generated oxygen is then pumped by the measurement pump cell 41, and the voltage Vp2 of the variable power supply is controlled so that the control voltage V2 detected by the measurement pump control oxygen partial pressure detection sensor cell 82 is constant. The amount of oxygen generated around the measurement electrode 44 is proportional to the concentration of nitrogen oxides in the measurement gas, so the pump current Ip2 in the measurement pump cell 41 is used to calculate the nitrogen oxide concentration in the measurement gas.

[0074] In addition, the measurement electrode 44, the first solid electrolyte layer 4, the third substrate layer 3, and the reference electrode 42 are combined to form an electrochemical sensor cell that constitutes an oxygen partial pressure detection means, thereby detecting NO in the atmosphere around the measurement electrode 44. x It is possible to detect the electromotive force corresponding to the difference between the amount of oxygen generated by the reduction of the components and the amount of oxygen contained in the reference atmosphere, which makes it possible to determine the concentration of nitrogen oxide components in the measurement gas.

[0075] Additionally, an electrochemical sensor cell 83 is configured by the second solid electrolyte layer 6, the spacer layer 5, the first solid electrolyte layer 4, the third substrate layer 3, the outer pump electrode 23, and the reference electrode 42. The gas sensor element 101 is configured to be able to detect the oxygen partial pressure in the measurement gas outside the sensor by the electromotive force Vref obtained by the sensor cell 83.

[0076] In the gas sensor element 101 having the above-mentioned configuration, the main pump cell 21 and the auxiliary pump cell 50 are operated to maintain the oxygen partial pressure at a constant low value (NO x Therefore, the gas sensor element 101 can detect NO x The nitrogen oxide concentration in the measurement gas can be determined based on a pump current Ip2 that flows when oxygen generated by reduction of the nitrogen oxide is pumped out of the measurement pump cell 41.

[0077] Furthermore, the gas sensor element 101 includes a heater 70 that adjusts the temperature by heating and keeping the gas sensor element 101 warm in order to increase the oxygen ion conductivity of the solid electrolyte. The heater 70 mainly includes a heater electrode 71, a heater element 72, a heater lead (not shown), a through hole 73, a heater insulating layer 74, and a heater resistance detection lead (not shown). In the example of FIG. 1, the heater 70 further includes a pressure release hole 75.

[0078] The heater 70 is embedded in the base portion of the gas sensor element 101 (element base 100) except for the heater electrode 71. In this embodiment, the heater 70 is disposed at a position closer to the lower surface of the gas sensor element 101 than to the upper surface of the gas sensor element 101 in the thickness direction (vertical direction / stacking direction) of the gas sensor element 101 (element base 100). However, the position of the heater 70 is not limited to this example and may be appropriately selected depending on the embodiment.

[0079] The heater electrode 71 is an electrode formed in a manner to contact the lower surface (the lower surface of the element body 100) of the first substrate layer 1. By connecting the heater electrode 71 to an external power supply, it is possible to supply power to the heater 70 from the outside.

[0080] The heater element 72 is an electric resistor sandwiched between the second substrate layer 2 and the third substrate layer 3 from above and below, that is, a resistance heating element provided between the second substrate layer 2 and the third substrate layer 3. The heater element 72 generates heat when power is supplied from a heater power source (not shown) provided outside the gas sensor element 101 through the heater electrodes 71, the through holes 73, and the heater leads, which are current paths, and heats and keeps warm the solid electrolyte forming the gas sensor element 101 (element substrate 100). The heater element 72 is made of Pt or contains Pt as a main component. The heater element 72 is embedded in a predetermined range on the side of the gas sensor element 101 (element substrate 100) where the measured gas flow section 7 is provided, so as to face the measured gas flow section 7 in the element thickness direction. The heater element 72 is provided to have a thickness of, for example, about 10 μm to 20 μm.

[0081] A pair of heater leads connected to both ends of the heater element 72 are provided to have substantially the same shape, that is, to have the same resistance value. Each of the pair of heater leads is connected to a different heater electrode 71 via a corresponding through hole 73.

[0082] Furthermore, a heater resistance detection lead is provided so as to be drawn out from the connection between the heater element 72 and one of the heater leads. The resistance value of the heater resistance detection lead is assumed to be negligible. The heater resistance detection lead is connected to the heater electrode 71 via a corresponding through hole 73.

[0083] The heater element 72 can adjust the temperature of the entire gas sensor element 101 (element substrate 100) to a temperature at which the solid electrolyte is activated. That is, in the gas sensor element 101, a current is passed through the heater element 72 via the heater electrode 71 to cause the heater element 72 to generate heat, thereby heating and keeping each part of the gas sensor element 101 at a predetermined temperature. Specifically, the gas sensor element 101 is heated so that the temperature of the solid electrolyte and the electrodes in the vicinity of the measurement gas flow portion 7 becomes, for example, about 700°C to 900°C (or 750°C to 950°C). This heating enhances the oxygen ion conductivity of the solid electrolyte constituting the substrate part in the gas sensor element 101 (element substrate 100). The heating temperature by the heater element 72 when a gas sensor including the gas sensor element 101 is used (when the gas sensor element 101 is driven) is sometimes referred to as the sensor element driving temperature.

[0084] The degree of heat generation by the heater element 72 can be grasped by the magnitude of the resistance value (heater resistance) of the heater element 72. The heater resistance detection lead is provided for measuring the heater resistance.

[0085] The heater insulating layer 74 is an insulating layer formed in a manner to cover the heater element 72, and is, for example, an insulating layer formed of an insulator such as alumina on the upper and lower surfaces of the heater element 72. The heater insulating layer 74 is formed for the purpose of obtaining electrical insulation between the second substrate layer 2 and the heater element 72, and between the third substrate layer 3 and the heater element 72. The heater insulating layer 74 has a thickness of about 70 μm to 110 μm, and is provided at a position separated from the tip surface and side surface of the gas sensor element 101 (element base 100) by about 200 μm to 700 μm. However, the thickness of the heater insulating layer 74 does not need to be constant, and may be different between a portion where the heater element 72 is present and a portion where it is not present.

[0086] Pressure relief hole 75 is a portion that penetrates third substrate layer 3 and is provided so as to communicate with reference gas introduction space 43, and is formed for the purpose of mitigating an increase in internal pressure that accompanies an increase in temperature within heater insulation layer 74. However, providing pressure relief hole 75 is not essential, and pressure relief hole 75 does not necessarily have to be provided.

[0087] As described above, in the gas sensor element 101, the first diffusion rate-controlling portion 11 is formed on the gas inlet 10 side of the measurement gas flow section 7, and the first diffusion rate-controlling portion 11 is formed as one or more slits Sl. For example, the first diffusion rate-controlling portion 11 is formed as two slits Sl. Hereinafter, the first diffusion rate-controlling portion 11 (slits Sl) in the gas sensor element 101 will be described in detail with reference to FIG. 2. In the following description, the thickness direction (stacking direction of layers 1 to 6) of the gas sensor element 101 (element substrate 100) is also referred to as the vertical direction (up-down direction). In addition, in a cross section parallel to the gas inlet 10 of the measurement gas flow section 7, a direction perpendicular to the vertical direction (up-down direction) is also referred to as the horizontal direction (left-right direction).

[0088] <Details of slit configuration> Fig. 2 is a diagram illustrating the cross-sectional shape of the slit Sl (first diffusion rate-controlling portion 11) in the gas sensor element 101. In particular, Fig. 2 is a diagram illustrating the details of the slit Sl in a cross section parallel to the gas inlet 10 of the measurement gas flow portion 7. In Fig. 2, the up-down direction of the paper is the thickness direction (vertical direction) of the element body 100, and the left-right direction of the paper is the horizontal direction. For example, the back side of the paper in Fig. 2 is the rear end side of the gas sensor element 101 (element body 100), and the front side of the paper is the front end side of the gas sensor element 101 (element body 100).

[0089] In the element substrate 100, one or more slits Sl are formed on the side of the gas inlet 10 of the measurement gas flow section 7. In the example shown in FIG. 2, a slit Sl(1) and a slit Sl(2) are formed. The slit Sl(1) is provided between the upper surface of the first bridging section 53a bridging the hollowed-out space of the spacer layer 5 and the lower surface of the second solid electrolyte layer 6. The slit Sl(2) is provided between the lower surface of the first bridging section 53a and the upper surface of the first solid electrolyte layer 4. In the example shown in FIG. 2, the slit Sl(1) is formed as an opening between the upper surface of the first bridging section 53a and the lower surface of the opening width adjustment layer 54(1) provided on the lower surface of the second solid electrolyte layer 6. The slit Sl(2) is formed as an opening between the lower surface of the first bridging section 53a and the upper surface of the opening width adjustment layer 54(2) provided on the upper surface of the first solid electrolyte layer 4.

[0090] The opening width adjustment layer 54(1) may be formed integrally with the second solid electrolyte layer 6, and the lower surface of the opening width adjustment layer 54(1) may constitute the lower surface of the second solid electrolyte layer 6. FIG. 2 and other figures show an example in which the opening width adjustment layer 54(1) and the second solid electrolyte layer 6 are separate members. However, this is merely for the purpose of facilitating understanding of the slit Sl according to one embodiment of the present invention, and is merely an example for emphasizing the difference between the slit Sl and the conventional slit OSl, which is an opening having a horizontally elongated shape in a cross section parallel to the gas inlet and has a constant opening width in the vertical direction. The opening width adjustment layer 54(1) and the second solid electrolyte layer 6 may be integral. For example, the opening width adjustment layer 54(1) may be formed by bending the lower surface of the second solid electrolyte layer 6 so as to be convex downward, that is, the opening width adjustment layer 54(1) may be a portion of the second solid electrolyte layer 6 that is bent so as to be convex downward. For example, the opening width adjustment layer 54(1) may be formed by firing a ceramic green sheet corresponding to the second solid electrolyte layer 6 so that the lower surface of the ceramic green sheet is warped downward in a convex shape. However, the method for forming the opening width adjustment layer 54(1) is not limited to this, and the opening width adjustment layer 54(1) and the second solid electrolyte layer 6 do not have to be integral with each other.

[0091] Similarly, the opening width adjustment layer 54(2) may be formed integrally with the first solid electrolyte layer 4, and the upper surface of the opening width adjustment layer 54(2) may constitute the upper surface of the first solid electrolyte layer 4. The opening width adjustment layer 54(2) and the first solid electrolyte layer 4 may be integral. For example, the opening width adjustment layer 54(2) may be formed by bending the upper surface of the first solid electrolyte layer 4 so as to be convex upward, that is, the opening width adjustment layer 54(2) may be a portion of the first solid electrolyte layer 4 that is bent so as to be convex upward. For example, the opening width adjustment layer 54(2) may be formed by firing a ceramic green sheet corresponding to the first solid electrolyte layer 4 so that the upper surface of the ceramic green sheet is bent in an upward convex shape. However, the method of forming the opening width adjustment layer 54(2) is not limited to this, and the opening width adjustment layer 54(2) and the first solid electrolyte layer 4 may not be integral.

[0092] The slit Sl(1) is an opening formed on the upper side in the thickness direction (vertical direction) of the gas sensor element 101 (element base 100). The slit Sl(1) is a slit Sl on the side closer to the outer pump electrode 23 than the heater 70 in the thickness direction of the gas sensor element 101, and is also referred to as a P-plane slit (upper slit). The slit Sl(2) is a slit Sl (opening) formed on the lower side in the thickness direction (vertical direction) of the gas sensor element 101 (element base 100). The slit Sl(2) is a slit on the side closer to the heater 70 than the outer pump electrode 23 in the thickness direction of the gas sensor element 101, and is also referred to as an H-plane slit (lower slit).

[0093] In the following description, when there is no need to distinguish between slit Sl(1) and slit Sl(2), they may simply be referred to as "slit Sl." When distinguishing between multiple slits Sl, "(1)," "(2)," "(3)," ..., "(n)," "(n+1)" are added after "Sl" to distinguish between them. "n" is an integer equal to or greater than "1."

[0094] 2, the slit Sl is formed in a horizontally elongated shape in a cross section parallel to the gas inlet 10, that is, formed as a horizontally elongated opening. The slit Sl is formed as an opening whose horizontal opening width is larger than its vertical opening width in a cross section parallel to the gas inlet 10. The average vertical opening width of the slit Sl (the entire slit Sl) is 3 μm or more.

[0095] The present inventors have confirmed that if the vertical opening width of the slit Sl (the entire slit Sl) is made too small, the flow rate of the measurement gas introduced into the measurement gas flow section 7 becomes too small, and the response accuracy, measurement accuracy, etc. of the gas sensor element 101 deteriorate. Specifically, the present inventors have confirmed that if the average vertical opening width of the slit Sl is less than 3 μm, the response accuracy, measurement accuracy, etc. of the gas sensor element 101 deteriorate. Therefore, the gas sensor element 101 has the slit Sl with an average vertical opening width of 3 μm or more in a cross section parallel to the gas inlet 10. By making the average vertical opening width of the slit Sl 3 μm or more, the gas sensor element 101 can avoid a situation in which "the response accuracy, measurement accuracy, etc. deteriorate due to the vertical opening width of the slit being made too small."

[0096] In the element substrate 100, at least one of the one or more slits Sl formed on the side of the gas inlet 10 of the measurement gas flow section 7 includes one or more narrow portions Np. In the example shown in FIG. 2, the slit Sl(1) and the slit Sl(2) each include one narrow portion Np. Specifically, the slit Sl(1) includes a narrow portion Np(1). The slit Sl(2) includes a narrow portion Np(2). In the following description, when it is not necessary to distinguish between the narrow portion Np(1) and the narrow portion Np(2), they may simply be referred to as "narrow portion Np". In addition, when it is necessary to distinguish between the multiple narrow portions Np, "(1)", "(2)", "(3)", ..., "(n)", "(n+1)" are added after "Np" to distinguish between them.

[0097] In a cross section parallel to the gas inlet 10, the average vertical opening width of the narrow portion Np is 3 μm or less. The present inventors have studied a method for improving the effect of suppressing the influence of pulsation in the measurement space on the pressure of the measured gas in the measured gas flow section 7 with respect to the slit Sl. The present inventors have found that the influence of the pulsation on the pressure of the measured gas in the measured gas flow section 7 can be suppressed by increasing the diffusion resistance or pressure loss of the measured gas introduced from the gas inlet 10 to the measured gas flow section 7 by the slit Sl. In particular, the present inventors have found that the influence of the pulsation can be suppressed extremely effectively by configuring at least a part of the slit Sl so that the average vertical opening width is 3 μm or less.

[0098] Therefore, in the element substrate 100, at least one of the one or more slits Sl formed on the gas inlet 10 side of the measured gas flow section 7 includes one or more narrow portions Np. The one or more narrow portions Np are each a portion having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10. For example, in FIG. 2, the vertical opening width H1(1) of the narrow portion Np(1) in a cross section parallel to the gas inlet 10 is 3 μm or less. Similarly, the vertical opening width H1(2) of the narrow portion Np(2) in a cross section parallel to the gas inlet 10 is 3 μm or less. For example, the narrow portion Np can increase the diffusion resistance of the measured gas introduced into the measured gas flow section 7. In addition, the outer periphery of the slit Sl including the narrow portion Np is longer than the outer periphery of a conventional slit OSl having a horizontally elongated rectangular cross section, so that the pressure loss of the measured gas introduced into the measured gas flow section 7 is also increased. Therefore, the gas sensor element 101 exhibits the effect that the influence of pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow portion 7 can be extremely effectively suppressed by the one or more narrow portions Np.

[0099] The lateral length of the narrow portion Np in a cross section parallel to the gas inlet 10 is 25 to 50% of the lateral length of the entire slit Sl including the narrow portion Np. The present inventors have confirmed that when the total lateral length of one or more narrow portions Np is less than 25% of the lateral length of the entire slit Sl including the "one or more narrow portions Np", the effect of suppressing the influence of pulsation by the "one or more narrow portions Np" is not sufficiently exhibited. In addition, the present inventors have confirmed that when the total lateral length of one or more narrow portions Np is made larger than 50% of the lateral length of the entire slit Sl including the "one or more narrow portions Np", the following problem occurs. That is, when the total lateral length of one or more narrow portions Np is made larger than 50% of the lateral length of the entire slit Sl, it becomes difficult to sufficiently secure the gas flow rate of the measurement gas introduced into the measurement gas flow portion 7, and deterioration of responsiveness occurs. Therefore, in the gas sensor element 101, the total lateral length of the one or more narrow portions Np is set to 25% or more and 50% or less of the lateral length of the entire slit Sl including the "one or more narrow portions Np." With this configuration, the gas sensor element 101 can avoid deterioration of responsiveness by ensuring a sufficient gas flow rate of the measurement gas introduced into the measurement gas flow portion 7, and can extremely effectively suppress the influence of pulsation by the narrow portions Np.

[0100] The slit Sl including the narrow portion Np includes a wide portion Wp as a portion other than the narrow portion Np. In the example shown in FIG. 2, the slit Sl(1) and the slit Sl(2) each include one or more wide portions Wp as a portion other than the narrow portion Np. Specifically, the slit Sl(1) includes a wide portion Wp(1-1) and a wide portion Wp(1-2). The wide portion Wp(1-1) and the wide portion Wp(1-2) are the wide portion Wp (wide portion Wp(1)) of the slit Sl(1). The slit Sl(2) includes a wide portion Wp(2-1) and a wide portion Wp(2-2). The wide portion Wp(2-1) and the wide portion Wp(2-2) are the wide portion Wp (wide portion Wp(2)) of the slit Sl(2). In the following description, when there is no need to distinguish between the wide portions Wp(1-1), Wp(1-2), Wp(2-1), and Wp(2-2), they may simply be referred to as "wide portion Wp." When distinguishing between the multiple wide portions Wp, "(1)," "(2)," "(3)," ..., "(n)," and "(n+1)" are added after "Wp" to distinguish between them. The wide portions Wp can be considered as portions whose average vertical opening width is larger (longer) than the narrow portions Np in a cross section parallel to the gas inlet.

[0101] In the slit Sl including the narrow portion Np, the average vertical opening width of the wide portion Wp in a cross section parallel to the gas inlet is 10 μm or less. For example, in FIG. 2, the vertical opening width H2(1) of the wide portion Wp(1) in a cross section parallel to the gas inlet 10 is 10 μm or less. Similarly, the vertical opening width H2(2) of the wide portion Wp(2) in a cross section parallel to the gas inlet 10 is 10 μm or less. If the average vertical opening width of the wide portion Wp is made larger than 10 μm, the effect of suppressing the influence of pulsation by the slit Sl, especially by the narrow portion Np, decreases. For example, if the average vertical opening width of the entire slit Sl is made larger than 10 μm, the slit Sl cannot provide sufficient diffusion resistance to the measurement gas introduced into the measurement gas flow portion 7, and the effect of suppressing the influence of pulsation decreases. Therefore, in the gas sensor element 101, the average opening width in the vertical direction of the wide portion Wp is set to 10 μm or less, and for example, the average opening width in the vertical direction of the entire slit Sl is set to 3 μm or more and 10 μm or less. With this configuration, the gas sensor element 101 can extremely effectively suppress the influence of pulsation in the measurement space by the slit Sl, particularly by the narrow portion Np.

[0102] In the element substrate 100, one or more slits Sl formed on the side of the gas inlet 10 of the measurement gas flow section 7 may each include one or more narrow portions Np. In the example shown in FIG. 2, the slit Sl(1) and the slit Sl(2) each include one narrow portion Np. With this configuration, the gas sensor element 101 can extremely effectively suppress the influence of pulsation in the measurement space by the one or more narrow portions Np included in each of the one or more slits Sl. In the example shown in FIG. 2, the gas sensor element 101 can extremely effectively suppress the influence of pulsation in the measurement space by the narrow portion Np(1) included in the slit Sl(1) and the narrow portion Np(2) included in the slit Sl(2).

[0103] In the element substrate 100, at least one of the one or more slits Sl may include one narrow portion Np, that is, at least one of the slits Sl may include "one" narrow portion Np. In the example shown in FIG. 2, each of the slits Sl(1) and Sl(2) includes one narrow portion Np. It is easier to provide the slit Sl with one narrow portion Np than to provide the slit Sl with a plurality of narrow portions Np. Therefore, the gas sensor element 101 can easily prepare the slit Sl including the narrow portion Np that extremely effectively suppresses the influence of pulsation in the measurement space.

[0104] In a cross section parallel to the gas inlet 10, the narrow portion Np may be disposed at the center in the horizontal direction of the slit Sl including the narrow portion Np. In the example shown in FIG. 2, the slit Sl(1) and the slit Sl(2) each include a narrow portion Np at the center in the horizontal direction of each slit Sl. In a cross section parallel to the gas inlet 10, the narrow portion Np(1) is disposed at the center in the horizontal direction of the slit Sl(1). In a cross section parallel to the gas inlet 10, the narrow portion Np(2) is disposed at the center in the horizontal direction of the slit Sl(2). Since it is easy to dispose the narrow portion Np at the center in the horizontal direction of the slit Sl, the gas sensor element 101 can easily prepare a slit Sl including a narrow portion Np that very effectively suppresses the influence of pulsation in the measurement space.

[0105] In a cross section parallel to the gas inlet 10, the vertical opening width of the narrow portion Np may change continuously. The vertical opening width of the narrow portion Np in a cross section parallel to the gas inlet 10 may change continuously along the horizontal direction, and for example, the vertical opening edge of the narrow portion Np may be configured to have a sloped shape. The vertical opening width of each of one or more narrow portions Np may change continuously, or the vertical opening width of at least one of the one or more narrow portions Np may change continuously.

[0106] Similarly, the opening width in the vertical direction of the wide portion Wp may change continuously in a cross section parallel to the gas inlet 10. The opening width in the vertical direction of the wide portion Wp in a cross section parallel to the gas inlet 10 may change continuously along the horizontal direction, and for example, the opening edge in the vertical direction of the wide portion Wp may be configured to have a sloped shape. The opening width in the vertical direction of each of one or more wide portions Wp may change continuously, or the opening width in the vertical direction of at least one of the one or more wide portions Wp may change continuously.

[0107] In the element substrate 100, at least one of the one or more slits Sl formed on the side of the gas inlet 10 of the measurement gas flow section 7 may have a continuously changing vertical opening width in a cross section parallel to the gas inlet 10. The vertical opening width of the slit Sl in a cross section parallel to the gas inlet 10 may continuously change along the horizontal direction, and for example, the vertical opening edge of the slit Sl may be configured to have a sloped shape.

[0108] 2 shows an example in which the vertical opening width of each of the narrow portion Np and the wide portion Wp in the element substrate 100 changes continuously in a cross section parallel to the gas inlet 10, and the vertical opening width of the slit Sl changes continuously. In the slit Sl(1), the vertical opening width of each of the narrow portion Np(1) and the wide portion Wp(1) changes continuously, and the vertical opening edge of the slit Sl(1) is configured to have a slope. In the slit Sl(2), the vertical opening width of each of the narrow portion Np(2) and the wide portion Wp(2) changes continuously, and the vertical opening edge of the slit Sl(2) is configured to have a slope.

[0109] <Considerations regarding the shape of the narrow part> Up to now, an example of the narrow portion Np in which the vertical opening width in a cross section parallel to the gas inlet 10 changes continuously has been described with reference to FIG. 2. However, the vertical opening width of the narrow portion Np in a cross section parallel to the gas inlet 10 may change discontinuously, for example, stepwise. The vertical opening width of the narrow portion Np in a cross section parallel to the gas inlet 10 may change discontinuously along the horizontal direction, for example, the vertical opening edge of the narrow portion Np may be configured in a stepped shape. In addition, the vertical opening width of the narrow portion Np in a cross section parallel to the gas inlet 10 may be constant, that is, it may not change along the horizontal direction. Hereinafter, an example of the narrow portion NpA in which the vertical opening width is constant will be described with reference to FIG. 3.

[0110] FIG. 3 is a diagram for explaining the cross-sectional shape of the slit SlA (first diffusion rate-controlling portion 11) in the element substrate 100A according to the first modification. In particular, FIG. 3 is a diagram for explaining the details of the slit SlA in a cross section parallel to the gas inlet 10 of the measurement gas flow section 7. In FIG. 3, the up-down direction of the paper is the thickness direction (vertical direction) of the element substrate 100A, and the left-right direction of the paper is the horizontal direction. Also, for example, the back side of the paper in FIG. 3 is the rear end side of the element substrate 100A, and the front side of the paper is the tip side of the element substrate 100A. The element substrate 100A has the same configuration as the element substrate 100, except that it includes the slit SlA including the "narrow width portion NpA whose opening width in the vertical direction in a cross section parallel to the gas inlet 10 is constant". The gas sensor element 101 may include the element substrate 100A illustrated in FIG. 3 instead of the element substrate 100.

[0111] In the element substrate 100A, one or more slits SlA are formed (provided) on the side of the gas inlet 10 of the measurement gas flow section 7, and in the example shown in Fig. 3, a slit SlA(1) and a slit SlA(2) are formed. In the following description, when there is no need to distinguish between the slit SlA(1) and the slit SlA(2), they may be simply referred to as "slit SlA".

[0112] 3, the slit SlA is formed in a horizontally elongated shape in a cross section parallel to the gas inlet 10, that is, formed as a horizontally elongated opening. The slit SlA is formed as an opening whose horizontal opening width is larger than its vertical opening width in a cross section parallel to the gas inlet 10. The average vertical opening width of the slit SlA is 3 μm or more, similar to the average vertical opening width of the slit Sl.

[0113] In the element substrate 100A, at least one of the one or more slits SlA formed on the side of the gas inlet 10 of the measurement gas flow section 7 includes one or more narrow portions NpA. In the example shown in FIG. 3, the slit SlA(1) and the slit SlA(2) each include one narrow portion NpA. Specifically, the slit SlA(1) includes the narrow portion NpA(1). The slit SlA(2) includes the narrow portion NpA(2). In the following description, when it is not necessary to distinguish between the narrow portion NpA(1) and the narrow portion NpA(2), they may be simply referred to as "narrow portion NpA". In the example shown in FIG. 3, the narrow portion NpA(1) of the slit SlA(1) is formed as an opening between the upper surface of the first bridge portion 53a and the lower surface of the opening width adjustment layer 54A(1) provided on the lower surface of the second solid electrolyte layer 6. The narrow portion NpA(2) of the slit SlA(2) is formed as an opening between the lower surface of the first bridge portion 53a and the upper surface of the opening width adjustment layer 54A(2) provided on the upper surface of the first solid electrolyte layer 4.

[0114] The opening width adjustment layer 54A(1) may be integral with the second solid electrolyte layer 6, similar to the opening width adjustment layer 54(1), and the lower surface of the opening width adjustment layer 54A(1) may constitute the lower surface (part of the lower surface) of the second solid electrolyte layer 6. For example, the opening width adjustment layer 54A(1) may be a portion of the second solid electrolyte layer 6 that is bent so as to be convex downward, or may be a protrusion (protrusion portion) that is provided on the lower surface of the second solid electrolyte layer 6 and is convex downward. In addition, the opening width adjustment layer 54A(2) may be integral with the first solid electrolyte layer 4, similar to the opening width adjustment layer 54(2), and the upper surface of the opening width adjustment layer 54A(2) may constitute the upper surface (part of the upper surface) of the first solid electrolyte layer 4. For example, the opening width adjustment layer 54A(2) may be a portion of the first solid electrolyte layer 4 that is bent so as to be convex upward, or may be a protrusion that is provided on the upper surface of the first solid electrolyte layer 4 and is convex upward.

[0115] In a cross section parallel to the gas inlet 10, the average vertical opening width of the narrow portion NpA is 3 μm or less, similar to the average vertical opening width of the narrow portion Np. For example, in FIG. 3, the vertical opening width H1A(1) of the narrow portion NpA(1) in a cross section parallel to the gas inlet 10 is 3 μm or less. Similarly, the vertical opening width H1A(2) of the narrow portion NpA(2) in a cross section parallel to the gas inlet 10 is 3 μm or less. Therefore, the gas sensor element 101 exhibits the effect that the influence of the pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow portion 7 can be extremely effectively suppressed by the one or more narrow portions NpA.

[0116] The lateral length of the narrow portion NpA in a cross section parallel to the gas inlet 10 is 25 to 50% of the lateral length of the entire slit SlA including the narrow portion NpA. With this configuration, the gas sensor element 101 can avoid deterioration of responsiveness by sufficiently ensuring the flow rate of the measurement gas introduced into the measurement gas flow portion 7, and can extremely effectively suppress the influence of pulsation by the narrow portion NpA.

[0117] The slit SlA including the narrow portion NpA includes a wide portion WpA as a portion other than the narrow portion NpA. In the example shown in FIG. 3, the slit SlA(1) and the slit SlA(2) each include one or more wide portions WpA as a portion other than the narrow portion NpA. Specifically, the slit SlA(1) includes a wide portion WpA(1-1) and a wide portion WpA(1-2). The wide portion WpA(1-1) and the wide portion WpA(1-2) are the wide portion WpA (wide portion WpA(1)) of the slit SlA(1). The slit SlA(2) includes a wide portion WpA(2-1) and a wide portion WpA(2-2). The wide portion WpA(2-1) and the wide portion WpA(2-2) are the wide portion WpA (wide portion WpA(2)) of the slit SlA(2). In the following description, when there is no need to distinguish between the wide portions WpA(1-1), WpA(1-2), WpA(2-1), and WpA(2-2), they may simply be referred to as "wide portion WpA." The wide portion WpA can be considered as a portion whose average vertical opening width is larger (longer) than the narrow portion NpA in a cross section parallel to the gas inlet.

[0118] In the slit SlA including the narrow portion NpA, the average vertical opening width of the wide portion WpA in a cross section parallel to the gas inlet is 10 μm or less. For example, in FIG. 3, the vertical opening width H2A(1) of each of the wide portions WpA(1-1) and WpA(1-2) in a cross section parallel to the gas inlet 10 is 10 μm or less. Similarly, the vertical opening width H2A(2) of each of the wide portions WpA(2-1) and WpA(2-2) in a cross section parallel to the gas inlet 10 is 10 μm or less. Note that the vertical opening width of the wide portion WpA(1-1) in a cross section parallel to the gas inlet 10 and the vertical opening width of the wide portion WpA(1-2) in a cross section parallel to the gas inlet 10 do not have to be the same, and each may be 10 μm or less. Similarly, the vertical opening width of the wide portion WpA(2-1) in a cross section parallel to the gas inlet 10 and the vertical opening width of the wide portion WpA(2-2) in a cross section parallel to the gas inlet 10 do not have to be the same, and each may be 10 μm or less. In the gas sensor element 101, the average vertical opening width of the wide portion WpA is 10 μm or less, and, for example, the average vertical opening width of the entire slit SlA is 3 μm or more and 10 μm or less. With this configuration, the gas sensor element 101 can extremely effectively suppress the influence of pulsation in the measurement space by the slit SlA, and particularly by the narrow portion NpA.

[0119] In the element substrate 100A, one or more slits SlA formed on the side of the gas inlet 10 of the measurement gas flow section 7 may each include one or more narrow portions NpA. In the example shown in FIG. 3, the slit SlA(1) and the slit SlA(2) each include one narrow portion NpA. With this configuration, the gas sensor element 101 can extremely effectively suppress the influence of pulsation in the measurement space by the one or more narrow portions NpA included in each of the one or more slits SlA. In the example shown in FIG. 3, the gas sensor element 101 can extremely effectively suppress the influence of pulsation in the measurement space by the narrow portions NpA(1) included in the slit SlA(1) and the narrow portions NpA(2) included in the slit SlA(2).

[0120] 3, in a cross section parallel to the gas inlet 10, the one or more narrow portions NpA may each have a constant opening width in the vertical direction. In a cross section parallel to the gas inlet 10, the opening width in the vertical direction of each narrow portion NpA may be constant along the horizontal direction. The opening width in the vertical direction of each of the one or more narrow portions NpA may be constant, or the opening width in the vertical direction of at least one of the one or more narrow portions NpA may be constant.

[0121] The narrow portion NpA (opening with a constant vertical opening width) illustrated in FIG. 3 can more effectively suppress the influence of pulsation in the measurement space than the narrow portion Np (opening with a variable vertical opening width) illustrated in FIG. 2. When the vertical opening width is constant (for example, the slit is configured to have an opening edge that changes stepwise in cross section), the following effect is achieved compared to when the opening width is continuously changed (for example, the slit is configured to have a curved opening edge in cross section). That is, when the opening edge of the slit is stepped, the entire circumference (perimeter) of the opening edge of the slit can be made longer than when the opening edge of the slit is curved, and the pressure loss of the measurement gas introduced into the measurement gas flow portion 7 can be increased. Therefore, the gas sensor element 101 can more effectively suppress the influence of pulsation in the measurement space by one or more narrow portions NpA each having a constant vertical opening width in cross section than the narrow portion Np.

[0122] The opening width in the vertical direction of the wide portion WpA may be constant in a cross section parallel to the gas inlet 10. The opening width in the vertical direction of the wide portion WpA in a cross section parallel to the gas inlet 10 may be constant along the horizontal direction. The opening width in the vertical direction of each of the one or more wide portions WpA may be constant, or the opening width in the vertical direction of at least one of the one or more wide portions WpA may be constant.

[0123] In the element substrate 100A, at least one of the one or more slits SlA formed on the side of the gas inlet 10 of the measurement gas flow section 7 may have a vertical opening width that varies discontinuously (e.g., stepwise) in a cross section parallel to the gas inlet 10. The vertical opening width of the slit SlA in a cross section parallel to the gas inlet 10 may vary discontinuously along the lateral direction, and for example, the vertical opening edge of the slit SlA may be configured in a stepped shape.

[0124] 3 shows an example in which the vertical opening width of each of the narrow portion NpA and the wide portion WpA in the element substrate 100A is constant in a cross section parallel to the gas inlet 10, and the vertical opening width of the slit SlA changes discontinuously. In the slit SlA(1), the vertical opening width of each of the narrow portion NpA(1) and the wide portion WpA(1) is constant, and the vertical opening edge of the slit SlA(1) is configured in a stepped shape. In the slit SlA(2), the vertical opening width of each of the narrow portion NpA(2) and the wide portion WpA(2) is constant, and the vertical opening edge of the slit SlA(2) is configured in a stepped shape.

[0125] In the element substrate 100A, at least one of the one or more slits SlA may include one narrow portion NpA, that is, at least one of the slits SlA may include "one" narrow portion NpA. In the example shown in FIG. 3, each of the slits SlA(1) and SlA(2) includes one narrow portion NpA. It is easier to provide the slit SlA with one narrow portion NpA than to provide the slit SlA with multiple narrow portions NpA. Therefore, the gas sensor element 101 can easily prepare the slit SlA including the narrow portion NpA that effectively suppresses the influence of pulsation in the measurement space.

[0126] In a cross section parallel to the gas inlet 10, the narrow portion NpA may be disposed at the center in the horizontal direction of the slit SlA including the narrow portion NpA. In the example shown in FIG. 3, the slit SlA(1) and the slit SlA(2) each include a narrow portion NpA at the center in the horizontal direction of each slit SlA. In a cross section parallel to the gas inlet 10, the narrow portion NpA(1) is disposed at the center in the horizontal direction of the slit SlA(1). In a cross section parallel to the gas inlet 10, the narrow portion NpA(2) is disposed at the center in the horizontal direction of the slit SlA(2). Since it is easy to dispose the narrow portion NpA at the center in the horizontal direction of the slit SlA, the gas sensor element 101 can easily prepare a slit SlA including a narrow portion NpA that very effectively suppresses the influence of pulsation in the measurement space.

[0127] <Considerations regarding the placement of narrow parts> So far, an example has been described in which the narrow portion (narrow portion Np, NpA) having an average vertical opening width of 3 μm or less is disposed at the center of the slit (slit Sl, SlA) in the horizontal direction in a cross section parallel to the gas inlet 10. However, for the gas sensor element 101, it is not essential that the narrow portion is disposed at the center of the slit in the horizontal direction. The narrow portion may be disposed on the right or left side of the slit in the horizontal direction. Hereinafter, an example of the narrow portion NpB disposed on the right or left side of the slit in the horizontal direction in a cross section parallel to the gas inlet 10 will be described with reference to FIG. 4.

[0128] FIG. 4 is a diagram for explaining the cross-sectional shape of the slit SlB (first diffusion rate-controlling portion 11) in the element substrate 100B according to the second modification. In particular, FIG. 4 is a diagram for explaining the details of the slit SlB in a cross section parallel to the gas inlet 10 of the measurement gas flow section 7. In FIG. 4, the up-down direction of the paper is the thickness direction (vertical direction) of the element substrate 100B, and the left-right direction of the paper is the horizontal direction. Also, for example, the back side of the paper in FIG. 4 is the rear end side of the element substrate 100B, and the front side of the paper is the tip side of the element substrate 100B. The element substrate 100B has a similar configuration to the element substrate 100A, except that it includes the slit SlB including the "narrow portion NpB disposed on the right or left side of the slit in a cross section parallel to the gas inlet 10". The gas sensor element 101 may include the element substrate 100B illustrated in FIG. 4 instead of the element substrate 100.

[0129] As described above, the element body 100B has the same configuration as the element body 100A, except for the arrangement position of the narrow portion (narrow portion NpB). Therefore, a detailed description of the element body 100B will not be given, except for the arrangement position of the narrow portion NpB.

[0130] In the element substrate 100B, one or more slits SlB are formed (provided) on the side of the gas inlet 10 of the measured gas flow section 7. In the example shown in FIG. 4, slits SlB(1) and SlB(2) are formed on the side of the gas inlet 10 of the measured gas flow section 7. In the following description, when there is no need to distinguish between the slits SlB(1) and SlB(2), they may be simply referred to as "slits SlB". Like the slits SlA, the slits SlB are formed in a horizontally elongated shape in a cross section parallel to the gas inlet 10, and the average opening width in the vertical direction is 3 μm or more.

[0131] In the element substrate 100B, at least one of the one or more slits SlB formed on the side of the gas inlet 10 of the measurement gas flow section 7 includes one or more narrow portions NpB. In the example shown in FIG. 4, the slit SlB(1) includes the narrow portion NpB(1), and the slit SlB(2) includes the narrow portion NpB(2). In the following description, when it is not necessary to distinguish between the narrow portion NpB(1) and the narrow portion NpB(2), they may be simply referred to as "narrow portion NpB". In the example shown in FIG. 4, the narrow portion NpB(1) of the slit SlB(1) is formed as an opening between the upper surface of the first bridge portion 53a and the lower surface of the opening width adjustment layer 54B(1) provided on the lower surface of the second solid electrolyte layer 6. The narrow portion NpB(2) of the slit SlB(2) is formed as an opening between the lower surface of the first bridge portion 53a and the upper surface of the opening width adjustment layer 54B(2) provided on the upper surface of the first solid electrolyte layer 4.

[0132] The opening width adjustment layer 54B(1) may be integral with the second solid electrolyte layer 6, similar to the opening width adjustment layers 54(1) and 54A(1), and the lower surface of the opening width adjustment layer 54B(1) may constitute the lower surface (part of the lower surface) of the second solid electrolyte layer 6. For example, the opening width adjustment layer 54B(1) may be a portion of the second solid electrolyte layer 6 that is bent so as to be convex downward, or may be a protrusion that is convex downward and provided on the lower surface of the second solid electrolyte layer 6. In addition, the opening width adjustment layer 54B(2) may be integral with the first solid electrolyte layer 4, similar to the opening width adjustment layers 54(2) and 54A(2), and the upper surface of the opening width adjustment layer 54B(2) may constitute the upper surface (part of the upper surface) of the first solid electrolyte layer 4. For example, the opening width adjustment layer 54B(2) may be a portion of the first solid electrolyte layer 4 that is bent so as to be convex upward, or may be a protrusion that is provided on the upper surface of the first solid electrolyte layer 4 and convex upward.

[0133] In a cross section parallel to the gas inlet 10, the average vertical opening width of the narrow portion NpB is 3 μm or less, similar to the average vertical opening width of the narrow portion NpA. For example, in FIG. 4, the vertical opening width H1B(1) of the narrow portion NpB(1) in a cross section parallel to the gas inlet 10 is 3 μm or less. Similarly, the vertical opening width H1B(2) of the narrow portion NpB(2) in a cross section parallel to the gas inlet 10 is 3 μm or less. Moreover, the horizontal length of the narrow portion NpB in a cross section parallel to the gas inlet 10 is 25 to 50% of the horizontal length of the entire slit SlB including the narrow portion NpB.

[0134] The slit SlB including the narrow portion NpB includes the wide portion WpB as a portion other than the narrow portion NpB. In the example shown in FIG. 4, the slit SlB(1) includes the wide portion WpB(1), and the slit SlB(2) includes the wide portion WpB(2). In the following description, when it is not necessary to distinguish between the wide portion WpB(1) and the wide portion WpB(2), they may be simply referred to as "wide portion WpB". The wide portion WpB can be considered as a portion having a larger (longer) average vertical opening width than the narrow portion NpB in a cross section parallel to the gas inlet. In the slit SlB including the narrow portion NpB, the average vertical opening width of the wide portion WpB in a cross section parallel to the gas inlet is 10 μm or less. 4, for example, the vertical opening width H2B(1) of the wide portion WpB(1) of the slit SlB(1) in a cross section parallel to the gas inlet 10 is 10 μm or less. Similarly, the vertical opening width H2B(2) of the wide portion WpB(2) of the slit SlB(2) in a cross section parallel to the gas inlet 10 is 10 μm or less.

[0135] Like the narrow portion NpA, the narrow portion NpB has a constant vertical opening width in a cross section parallel to the gas inlet 10, that is, the vertical opening width of the narrow portion NpB is constant along the horizontal direction. In a cross section parallel to the gas inlet 10, one or more narrow portions NpB may each have a constant vertical opening width, that is, in a cross section parallel to the gas inlet 10, the vertical opening width of each narrow portion NpB may be constant along the horizontal direction. The vertical opening width of each of the one or more narrow portions NpB may be constant, or the vertical opening width of at least one of the one or more narrow portions NpB may be constant.

[0136] 4 shows an example in which the vertical opening width of each of the narrow portion NpB and the wide portion WpB in the element substrate 100B is constant in a cross section parallel to the gas inlet 10, and the vertical opening width of the slit SlB changes discontinuously. In the slit SlB(1), the vertical opening width of each of the narrow portion NpB(1) and the wide portion WpB(1) is constant, and the vertical opening edge of the slit SlB(1) is configured in a stepped shape. In the slit SlB(2), the vertical opening width of each of the narrow portion NpB(2) and the wide portion WpB(2) is constant, and the vertical opening edge of the slit SlB(2) is configured in a stepped shape.

[0137] In the element base 100B, the narrow portion NpB is disposed on the right or left side of the slit SlB in the horizontal direction in a cross section parallel to the gas inlet 10. In the example shown in FIG. 4, the narrow portion NpB(1) is disposed on the left side of the slit SlB(1) in the horizontal direction in a cross section parallel to the gas inlet 10. Moreover, the narrow portion NpB(2) is disposed on the right side of the slit SlB(2) in the horizontal direction in a cross section parallel to the gas inlet 10. That is, in the element base 100B, the narrow portion NpB may be disposed on the right or left side of the slit SlB including the narrow portion NpB in a cross section parallel to the gas inlet 10. In a cross section parallel to the gas inlet 10, the narrow portions NpB included in each slit SlB are one opening extending continuously in the horizontal direction, and may be disposed so as not to be aligned vertically with each other. For example, when one narrow portion NpB is disposed on the right side of a certain slit SlB, the other narrow portion NpB may be disposed on the left side of another slit SlB. In the example shown in Fig. 4, the narrow portion NpB(1) is disposed on the left side of the slit SlB(1), and the narrow portion NpB(2) is disposed on the right side of the slit SlB(2).

[0138] <Considerations on slits with narrower widths> Up to now, an example has been described in which each of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes a "narrow portion having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10". However, it is not essential for the gas sensor element 101 that each of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes such a narrow portion. For the gas sensor element 101, it is sufficient that at least one of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes such a narrow portion. Hereinafter, an example will be described with reference to FIG. 5 in which only one of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes a "narrow portion having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10".

[0139] FIG. 5 is a diagram for explaining the cross-sectional shape of the slit SlC (first diffusion rate-controlling portion 11) in the element substrate 100C according to the third modification. In particular, FIG. 5 is a diagram for explaining the details of the slit SlC in a cross section parallel to the gas inlet 10 of the measurement gas flow section 7. In FIG. 5, the up-down direction of the paper is the thickness direction (vertical direction) of the element substrate 100C, and the left-right direction of the paper is the horizontal direction. Also, for example, the back side of the paper in FIG. 5 is the rear end side of the element substrate 100C, and the front side of the paper is the front end side of the element substrate 100C. The element substrate 100C has the same configuration as the element substrate 100, except that only one slit SlC includes a narrow portion NpC among one or more slits SlC formed on the gas inlet 10 side of the measurement gas flow section 7. The gas sensor element 101 may have the element substrate 100C illustrated in FIG. 5 instead of the element substrate 100.

[0140] As described above, the element body 100C has the same configuration as the element body 100, except that only one of the one or more slits SlC has a narrow portion (narrow portion NpC). Therefore, details of the configuration of the element body 100C that is the same as that of the element body 100 will be omitted.

[0141] In the element substrate 100C, one or more slits SlC are formed (provided) on the side of the gas inlet 10 of the measured gas flow section 7. In the example shown in Fig. 5, slits SlC(1) and SlC(2) are formed on the side of the gas inlet 10 of the measured gas flow section 7. In the following description, when there is no need to distinguish between the slits SlC(1) and SlC(2), they may be simply referred to as "slits SlC". Like the slits SlA, the slits SlC are formed in a horizontally elongated shape in a cross section parallel to the gas inlet 10, and the average opening width in the vertical direction is 3 µm or more.

[0142] In the element substrate 100C, at least one of the one or more slits SlC formed on the side of the gas inlet 10 of the measurement gas flow section 7 includes one or more narrow portions NpC. In the example shown in FIG. 5, the slit SlC(1) includes the narrow portion NpC(1), and in particular, includes "one" narrow portion NpC(1). In the example shown in FIG. 5, the slit SlC(1) is formed as an opening between the upper surface of the first bridge portion 53a and the lower surface of the opening width adjustment layer 54C(1) provided on the lower surface of the second solid electrolyte layer 6. In contrast, the slit SlC(2) does not include a narrow portion NpC.

[0143] Like the opening width adjustment layers 54(1), 54A(1), and 54B(1), the opening width adjustment layer 54C(1) may be integral with the second solid electrolyte layer 6, and the lower surface of the opening width adjustment layer 54C(1) may form the lower surface of the second solid electrolyte layer 6. For example, the opening width adjustment layer 54C(1) may be a portion of the second solid electrolyte layer 6 that is bent so as to be convex downward, or may be a protrusion provided on the lower surface of the second solid electrolyte layer 6 that is convex downward.

[0144] In a cross section parallel to the gas inlet 10, the average vertical opening width of the narrow portion NpC (narrow portion NpC(1)) is 3 μm or less, similar to the average vertical opening width of the narrow portion Np. For example, in FIG. 5, the vertical opening width H1C(1) of the narrow portion NpC(1) in a cross section parallel to the gas inlet 10 is 3 μm or less. In addition, the horizontal length of the narrow portion NpC in a cross section parallel to the gas inlet 10 is 25 to 50% of the horizontal length of the entire slit SlC including the narrow portion NpC. In other words, the horizontal length of the narrow portion NpC(1) in a cross section parallel to the gas inlet 10 is 25 to 50% of the horizontal length of the entire slit SlC(1) including the narrow portion NpC(1).

[0145] The slit SlC including the narrow portion NpC includes the wide portion WpC as a portion other than the narrow portion NpC. In the example shown in FIG. 5, the slit SlC(1) includes the wide portion WpC(1-1) and the wide portion WpC(1-2). In the following description, when it is not necessary to distinguish between the wide portion WpC(1-1) and the wide portion WpC(1-2), they may be simply referred to as the "wide portion WpC". The wide portion WpC can be considered as a portion having a larger (longer) average vertical opening width than the narrow portion NpC (narrow portion NpC(1)) in a cross section parallel to the gas inlet. In the slit SlC including the narrow portion NpC (i.e., the slit SlC(1)), the average vertical opening width of the wide portion WpC in a cross section parallel to the gas inlet is 10 μm or less. 5, for example, the vertical opening width H2C(1) of each of the wide portions WpC(1-1) and WpC(1-2) in a cross section parallel to the gas inlet 10 is 10 μm or less. The vertical opening width of the wide portion WpC(1-1) in a cross section parallel to the gas inlet 10 and the vertical opening width of the wide portion WpC(1-2) in a cross section parallel to the gas inlet 10 do not have to be the same, and each may be 10 μm or less. As described above, the slit SlC(2) does not include the narrow portion NpC, and the vertical opening width H2C(2) of the slit SlC(2) in a cross section parallel to the gas inlet 10 is 10 μm or less.

[0146] In a cross section parallel to the gas inlet 10, the narrow portion NpC may be disposed at the center in the lateral direction of the slit SlC including the narrow portion NpC. In the example shown in Fig. 5, in a cross section parallel to the gas inlet 10, the narrow portion NpC(1) is disposed at the center in the lateral direction of the slit SlC(1).

[0147] As described above, the slit SlC(1) is similar to the slit Sl(1) described with reference to FIG. 2. The narrow portion NpC(1) is similar to the narrow portion Np(1) of the slit Sl(1). The wide portion WpC is similar to the wide portion Wp of the slit Sl(1). However, while the slit Sl(1) which is an H-plane slit in the element substrate 100 includes the narrow portion Np(1), the slit SlC(2) which is an H-plane slit in the element substrate 100C does not include the narrow portion NpC. That is, in the element substrate 100C, the slit SlC(2) does not include a "narrow portion having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10." However, the gas sensor element 101 having the element substrate 100C instead of the element substrate 100 can suppress the influence of the pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow portion 7 extremely effectively by the narrow portion NpC. That is, the gas sensor element 101 includes the narrow portion NpC only in one slit SlC among one or more slits SlC formed on the gas inlet 10 side of the measurement gas flow portion 7. Specifically, the gas sensor element 101 includes the narrow portion NpC (narrow portion NpC(1)) only in the slit SlC(1) among the slits SlC(1) and SlC(2). The gas sensor element 101 can suppress the influence of the pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow portion 7 extremely effectively by the narrow portion NpC.

[0148] In the gas sensor element according to one embodiment of the present invention, at least one of the one or more slits formed on the gas inlet 10 side of the measurement gas flow section 7 may include one or more narrow portions. The gas sensor element according to one embodiment of the present invention may include a slit that does not include a "narrow portion having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10". For example, of two slits formed on the gas inlet 10 side of the measurement gas flow section 7, only one slit may include one or more narrow portions, and the other slit may not include a narrow portion.

[0149] <Considerations regarding the number of narrow parts> Up to now, an example has been described in which at least one of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes "one narrow portion having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10". However, for the gas sensor element 101, it is not essential that at least one of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes "one" such narrow portion. For the gas sensor element 101, it is sufficient that at least one of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes one or more such narrow portions. Hereinafter, an example will be described with reference to FIG. 6 and FIG. 7 in which at least one of the one or more slits formed on the gas inlet 10 side of the measured gas flow section 7 includes a plurality of "narrow portions having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10".

[0150] FIG. 6 is a diagram for explaining the cross-sectional shape of the slit SlD (first diffusion rate-controlling portion 11) in the element substrate 100D according to the fourth modification. In particular, FIG. 6 is a diagram for explaining the details of the slit SlD in a cross section parallel to the gas inlet 10 of the measurement gas flow section 7. In FIG. 6, the up-down direction of the paper is the thickness direction (vertical direction) of the element substrate 100D, and the left-right direction of the paper is the horizontal direction. Also, for example, the back side of the paper in FIG. 6 is the rear end side of the element substrate 100D, and the front side of the paper is the tip side of the element substrate 100D. The element substrate 100D has a similar configuration to the element substrates 100A and 100B, except that the element substrate 100D includes a plurality of "narrow portions having an average opening width of 3 μm or less in the vertical direction in a cross section parallel to the gas inlet 10" (narrow portions NpD). The gas sensor element 101 may include an element substrate 100D, as shown in FIG.

[0151] As described above, the element base 100D has the same configuration as the element base 100A and 100B, except that "at least one of the one or more slits includes a plurality of narrow portions (narrow portions NpD)." Therefore, details of the configuration of the element base 100D that is the same as that of the element bases 100A and 100B will be omitted.

[0152] In the element substrate 100D, one or more slits SlD are formed (provided) on the side of the gas inlet 10 of the measurement gas flow section 7. In the example shown in Fig. 6, a slit SlD(1) and a slit SlD(2) are formed on the side of the gas inlet 10 of the measurement gas flow section 7. In the following description, when there is no need to distinguish between the slits SlD(1) and SlD(2), they may be simply referred to as "slits SlD". Like the slits SlA, the slits SlD are formed in a horizontally elongated shape in a cross section parallel to the gas inlet 10, and the average opening width in the vertical direction is 3 µm or more.

[0153] In the element substrate 100D, at least one of the one or more slits SlD formed on the side of the gas inlet 10 of the measurement gas flow section 7 includes one or more narrow portions NpD. In the example shown in FIG. 6, the slit SlD(1) includes a narrow portion NpD(1-1) and a narrow portion NpD(1-2). In the example shown in FIG. 6, the narrow portion NpD(1-1) is formed as an opening between the upper surface of the first bridging portion 53a and the lower surface of the opening width adjustment layer 54D(1-1) provided on the lower surface of the second solid electrolyte layer 6. The narrow portion NpD(1-2) is formed as an opening between the upper surface of the first bridging portion 53a and the lower surface of the opening width adjustment layer 54D(1-2) provided on the lower surface of the second solid electrolyte layer 6. The narrow portion NpD(1-1) and the narrow portion NpD(1-2) are each the narrow portion NpD (narrow portion NpD(1)) of the slit SlD(1).

[0154] In the example shown in FIG. 6, the slit SlD(2) includes a narrow portion NpD(2-1) and a narrow portion NpD(2-2). In the example shown in FIG. 6, the narrow portion NpD(2-1) is formed as an opening between the upper surface of the first bridging portion 53a and the lower surface of the opening width adjustment layer 54D(2-1) provided on the lower surface of the second solid electrolyte layer 6. The narrow portion NpD(2-2) is formed as an opening between the upper surface of the first bridging portion 53a and the lower surface of the opening width adjustment layer 54D(2-2) provided on the lower surface of the second solid electrolyte layer 6. The narrow portion NpD(2-1) and the narrow portion NpD(2-2) are the narrow portions NpD (narrow portion NpD(2)) of the slit SlD(2), respectively.

[0155] The opening width adjustment layer 54D(1-1) and the opening width adjustment layer 54D(1-2) may be integral with the second solid electrolyte layer 6, similar to the opening width adjustment layers 54(1) and 54A(1) to 54C(1). The lower surfaces of the opening width adjustment layer 54D(1-1) and the opening width adjustment layer 54D(1-2) may form the lower surface (part of the lower surface) of the second solid electrolyte layer 6. For example, the opening width adjustment layer 54D(1-1) and the opening width adjustment layer 54D(1-2) may be a portion of the second solid electrolyte layer 6 that is bent so as to be convex downward, or may be a protrusion that is provided on the lower surface of the second solid electrolyte layer 6 and is convex downward. The opening width adjustment layer 54D(2-1) and the opening width adjustment layer 54D(2-2) may be integral with the first solid electrolyte layer 4, similar to the opening width adjustment layers 54(2) and 54A(2) to 54C(2). The upper surfaces of the opening width adjustment layer 54D(2-1) and the opening width adjustment layer 54D(2-2) may form the upper surface (a part of the upper surface) of the first solid electrolyte layer 4. For example, the opening width adjustment layer 54D(2-1) and the opening width adjustment layer 54D(2-2) may be a curved portion of the first solid electrolyte layer 4 that is convex upward, or may be a protrusion that is convex upward and is provided on the upper surface of the first solid electrolyte layer 4.

[0156] In the following description, when there is no need to distinguish between the narrow portions NpD(1-1), NpD(1-2), NpD(2-1), and NpD(2-2), they may simply be referred to as "narrow portions NpD."

[0157] In a cross section parallel to the gas inlet 10, the average vertical opening width of the narrow portion NpD is 3 μm or less, similar to the average vertical opening width of the narrow portion NpA. For example, in FIG. 6, the vertical opening width H1D(1) of each of the narrow portions NpD(1-1) and NpD(1-2) in a cross section parallel to the gas inlet 10 is 3 μm or less. Similarly, the vertical opening width H1D(2) of each of the narrow portions NpD(2-1) and NpD(2-2) in a cross section parallel to the gas inlet 10 is 3 μm or less. Note that the vertical opening width of the narrow portion NpD(1-1) in a cross section parallel to the gas inlet 10 and the vertical opening width of the narrow portion NpD(1-2) in a cross section parallel to the gas inlet 10 do not have to be the same, and each may be 3 μm or less. Similarly, the vertical opening width of the narrow portion NpD(2-1) in a cross section parallel to the gas inlet 10 and the vertical opening width of the narrow portion NpD(2-2) in a cross section parallel to the gas inlet 10 do not have to be the same, and each may be 3 μm or less.

[0158] The horizontal length of the narrow portion NpD in a cross section parallel to the gas inlet 10 is 25 to 50% of the horizontal length of the entire slit SlD including the narrow portion NpD. In the element substrate 100D, the total horizontal length of the narrow portions NpD in each slit SlD in a cross section parallel to the gas inlet 10 is 25 to 50% of the horizontal length of the entire slit SlD including the narrow portions NpD. Specifically, the total horizontal length of the narrow portions NpD(1-1) and NpD(1-2) in a cross section parallel to the gas inlet 10 is 25 to 50% of the horizontal length of the entire slit SlD(1). Similarly, the total horizontal length of the narrow portions NpD(2-1) and NpD(2-2) is 25 to 50% of the horizontal length of the entire slit SlD(2).

[0159] The slit SlD including the narrow portion NpD includes a wide portion WpD as a portion other than the narrow portion NpD. In the example shown in FIG. 6, the slit SlD(1) includes wide portions WpD(1-1), WpD(1-2), and WpD(1-3). The wide portions WpD(1-1), WpD(1-2), and WpD(1-3) are the wide portions WpD (wide portion WpD(1)) of the slit SlD(1). Similarly, the slit SlD(2) includes wide portions WpD(2-1), WpD(2-2), and WpD(2-3). The wide portions WpD(2-1), WpD(2-2), and WpD(2-3) are the wide portions WpD (wide portion WpD(2)) of the slit SlD(2). In the following description, when there is no need to distinguish between the wide portions WpD(1-1), WpD(1-2), WpD(1-3), WpD(2-1), WpD(2-2), and WpD(2-3), they may simply be referred to as "wide portions WpD". The wide portions WpD can be considered as portions having a larger (longer) average vertical opening width than the narrow portions NpD in a cross section parallel to the gas inlet. In the slit SlD including the narrow portions NpD, the average vertical opening width of the wide portions WpD in a cross section parallel to the gas inlet is 10 μm or less. For example, in FIG. 6, the vertical opening width H2D(1) of each of the wide portions WpD(1-1) to WpD(1-3) in a cross section parallel to the gas inlet 10 is 10 μm or less. Similarly, the vertical opening width H2A(2) of each of the wide portions WpD(2-1) to WpD(2-3) in a cross section parallel to the gas inlet 10 is 10 μm or less. The vertical opening widths of each of the wide portions WpD(1-1) to WpD(1-3) in a cross section parallel to the gas inlet 10 do not have to be the same, as long as they are each 10 μm or less. Similarly, the vertical opening widths of each of the wide portions WpD(2-1) to WpD(2-3) in a cross section parallel to the gas inlet 10 do not have to be the same, as long as they are each 3 μm or less.

[0160] Like the narrow portion NpA, the narrow portion NpD has a constant vertical opening width in a cross section parallel to the gas inlet 10, that is, the vertical opening width of the narrow portion NpD is constant along the horizontal direction. In a cross section parallel to the gas inlet 10, one or more narrow portions NpD may each have a constant vertical opening width, that is, in a cross section parallel to the gas inlet 10, the vertical opening width of each narrow portion NpD may be constant along the horizontal direction. The vertical opening width of each of the one or more narrow portions NpD may be constant, or the vertical opening width of at least one of the one or more narrow portions NpD may be constant.

[0161] 6 shows an example in which the vertical opening width of each of the narrow portion NpD and the wide portion WpD in the element substrate 100D in a cross section parallel to the gas inlet 10 is constant, and the vertical opening width of the slit SlD changes discontinuously. In the slit SlD(1), the vertical opening width of each of the narrow portion NpD(1) and the wide portion WpD(1) is constant, and the vertical opening edge of the slit SlD(1) is configured in a stepped shape. In the slit SlD(2), the vertical opening width of each of the narrow portion NpD(2) and the wide portion WpD(2) is constant, and the vertical opening edge of the slit SlD(2) is configured in a stepped shape.

[0162] In the gas sensor element according to one aspect of the present invention, at least one of the one or more slits formed on the gas inlet 10 side of the measurement gas flow section 7 may include a plurality of "narrow portions having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10." The gas sensor element according to one aspect of the present invention can extremely effectively suppress the influence of pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow section 7 by the plurality of narrow portions.

[0163] 6 shows an example in which at least one of one or more slits formed on the gas inlet 10 side of the measurement gas flow section 7 includes "two" narrow portions having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10. However, for the gas sensor element 101, it is sufficient that at least one of one or more slits formed on the gas inlet 10 side of the measurement gas flow section 7 includes one or more such narrow portions. Hereinafter, an example in which at least one of one or more slits formed on the gas inlet 10 side of the measurement gas flow section 7 includes "three" or more narrow portions having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10 will be described with reference to FIG. 7.

[0164] FIG. 7 is a diagram for explaining the cross-sectional shape of the slit SlE (first diffusion rate-controlling portion 11) in the element substrate 100E according to the fifth modification. In particular, FIG. 7 is a diagram for explaining the details of the slit SlE in a cross section parallel to the gas inlet 10 of the measurement gas flow portion 7. In FIG. 7, the up-down direction of the paper is the thickness direction (vertical direction) of the element substrate 100E, and the left-right direction of the paper is the horizontal direction. Also, for example, the back side of the paper in FIG. 7 is the rear end side of the element substrate 100E, and the front side of the paper is the tip side of the element substrate 100E. The element substrate 100E has a similar configuration to the element substrate 100D, except that the element substrate 100E includes "three" or more "narrow portions having an average vertical opening width of 3 μm or less in a cross section parallel to the gas inlet 10" (narrow portions NpE). The gas sensor element 101 may include an element substrate 100E as shown in FIG.

[0165] As described above, the element base 100E has the same configuration as the element base 100D, except that "at least one of the one or more slits includes three or more narrow portions (narrow portions NpE)." Therefore, details of the configuration of the element base 100E that is the same as that of the element base 100D will be omitted.

[0166] In the element substrate 100E, one or more slits SlE are formed (provided) on the side of the gas inlet 10 of the measurement gas flow section 7. In the example shown in Fig. 7, slits SlE(1) and SlE(2) are formed on the side of the gas inlet 10 of the measurement gas flow section 7. In the following description, when there is no need to distinguish between the slits SlE(1) and SlE(2), they may be simply referred to as "slits SlE". Like the slits SlA, the slits SlE are formed in a horizontally elongated shape in a cross section parallel to the gas inlet 10, and the average opening width in the vertical direction is 3 µm or more.

[0167] In the element substrate 100E, at least one of the one or more slits SlE formed on the side of the gas inlet 10 of the measurement gas flow section 7 includes three or more narrow portions NpE. In the example shown in FIG. 7, the slit SlE(1) includes narrow portions NpE(1-1) to NpE(1-6). In the example shown in FIG. 7, the narrow portions NpE(1-1) to NpE(1-6) are each formed as an opening between the upper surface of the first bridging portion 53a and the lower surface of the opening width adjustment layer 54E(1) provided on the lower surface of the second solid electrolyte layer 6. The narrow portions NpE(1-1) to NpE(1-6) are each the narrow portions NpE (narrow portion NpE(1)) of the slit SlE(1).

[0168] In the example shown in FIG. 7, the slit SlE(2) includes narrow portions NpE(2-1) to NpE(2-6). In the example shown in FIG. 7, the narrow portions NpE(2-1) to NpE(2-6) are each formed as an opening between the upper surface of the first bridge portion 53a and the lower surface of the opening width adjustment layer 54E(2) provided on the lower surface of the second solid electrolyte layer 6. The narrow portions NpE(2-1) to NpE(2-6) are each the narrow portion NpE (narrow portion NpE(2)) of the slit SlE(2). In the following description, when it is not necessary to distinguish between the narrow portions NpE(1-1) to NpE(1-6) and the narrow portions NpE(2-1) to NpE(2-6), they may be simply referred to as "narrow portions NpE".

[0169] Each of the multiple aperture width adjustment layers 54E(1) illustrated in FIG. 7 may be integral with the second solid electrolyte layer 6, similar to the aperture width adjustment layers 54(1), 54A(1) to 54C(1), 54D(1-1), and 54D(1-2). The lower surface of each of the multiple aperture width adjustment layers 54E(1) may constitute the lower surface (part of the lower surface) of the second solid electrolyte layer 6. For example, each of the multiple aperture width adjustment layers 54E(1) may be a portion of the second solid electrolyte layer 6 that is bent so as to be convex downward, or may be a protrusion that is convex downward and provided on the lower surface of the second solid electrolyte layer 6. Also, each of the multiple aperture width adjustment layers 54E(2) may be integral with the first solid electrolyte layer 4, similar to the aperture width adjustment layers 54(2), 54A(2) to 54C(2), 54D(2-1), and 54D(2-2). The upper surface of each of the plurality of opening width adjustment layers 54E(2) may constitute (a part of) the upper surface of the first solid electrolyte layer 4. For example, each of the plurality of opening width adjustment layers 54E(2) may be a curved portion of the first solid electrolyte layer 4 that is convex upward, or may be a protrusion provided on the upper surface of the first solid electrolyte layer 4 that is convex upward.

[0170] In a cross section parallel to the gas inlet 10, the average vertical opening width of the narrow portions NpE is 3 μm or less, similar to the average vertical opening width of the narrow portions NpD. For example, in FIG. 7, the vertical opening width H1E(1) of each of the narrow portions NpE(1-1) to NpE(1-6) in a cross section parallel to the gas inlet 10 is 3 μm or less. Similarly, the vertical opening width H1E(2) of each of the narrow portions NpE(2-1) to NpE(2-6) in a cross section parallel to the gas inlet 10 is 3 μm or less. Note that the vertical opening widths of each of the narrow portions NpE(1-1) to NpE(1-6) in a cross section parallel to the gas inlet 10 do not have to be the same, and may be 3 μm or less. Similarly, the vertical opening widths of the narrow portions NpE(2-1) to NpE(2-6) in a cross section parallel to the gas inlet 10 do not have to be the same, and each may be 3 μm or less.

[0171] The lateral length of the narrow portion NpE in a cross section parallel to the gas inlet 10 is 25 to 50% of the lateral length of the entire slit SlE including the narrow portion NpE. In the element substrate 100E, the sum of the lateral lengths of the narrow portions NpE in each slit SlE in a cross section parallel to the gas inlet 10 is 25 to 50% of the lateral length of the entire slit SlE including the narrow portions NpE. Specifically, the sum of the lateral lengths of the narrow portions NpE(1-1) to NpE(1-6) in a cross section parallel to the gas inlet 10 is 25 to 50% of the lateral length of the entire slit SlE(1). Similarly, the sum of the lateral lengths of the narrow portions NpE(2-1) to NpE(2-6) in a cross section parallel to the gas inlet 10 is 25 to 50% of the lateral length of the entire slit SlE(2).

[0172] The slit SlE including the narrow portion NpE includes a wide portion WpE as a portion other than the narrow portion NpE. In the example shown in FIG. 7, the slit SlE(1) includes wide portions WpE(1-1) to WpE(1-7). The wide portions WpE(1-1) to WpE(1-7) are respectively the wide portion WpE (wide portion WpE(1)) of the slit SlE(1). Similarly, the slit SlE(2) includes wide portions WpE(2-1) to WpE(2-7). The wide portions WpE(2-1) to WpE(2-7) are respectively the wide portion WpE (wide portion WpE(2)) of the slit SlE(2). In the following description, when there is no need to distinguish between the wide portions WpE(1-1) to WpE(1-7) and WpE(2-1) to WpE(2-7), they may simply be referred to as "wide portions WpE". The wide portions WpE can be considered as portions having a larger (longer) average vertical opening width than the narrow portions NpE in a cross section parallel to the gas inlet. In the slit SlE including the narrow portions NpE, the average vertical opening width of the wide portions WpE in a cross section parallel to the gas inlet is 10 μm or less. For example, in FIG. 7, the vertical opening width H2E(1) of each of the wide portions WpE(1-1) to WpE(1-7) in a cross section parallel to the gas inlet 10 is 10 μm or less. Similarly, the vertical opening width H2A(2) of each of the wide portions WpE(2-1) to WpE(2-7) in a cross section parallel to gas inlet 10 is 10 μm or less. The vertical opening widths of each of the wide portions WpE(1-1) to WpE(1-7) in a cross section parallel to gas inlet 10 do not have to be the same, as long as they are each 10 μm or less. Similarly, the vertical opening widths of each of the wide portions WpE(2-1) to WpE(2-7) in a cross section parallel to gas inlet 10 do not have to be the same, as long as they are each 3 μm or less.

[0173] Like the narrow portion NpA, the narrow portion NpE has a constant vertical opening width in a cross section parallel to the gas inlet 10, that is, the vertical opening width of the narrow portion NpE is constant along the horizontal direction. In a cross section parallel to the gas inlet 10, one or more narrow portions NpE may each have a constant vertical opening width, that is, in a cross section parallel to the gas inlet 10, the vertical opening width of each narrow portion NpE may be constant along the horizontal direction. The vertical opening width of each of the one or more narrow portions NpE may be constant, or the vertical opening width of at least one of the one or more narrow portions NpE may be constant.

[0174] 7 shows an example in which the vertical opening width of each of the narrow portion NpE and the wide portion WpE in the element substrate 100E is constant in a cross section parallel to the gas inlet 10, and the vertical opening width of the slit SlE changes discontinuously. In the slit SlE(1), the vertical opening width of each of the narrow portion NpE(1) and the wide portion WpE(1) is constant, and the vertical opening edge of the slit SlE(1) is configured in a stepped shape. In the slit SlE(2), the vertical opening width of each of the narrow portion NpE(2) and the wide portion WpE(2) is constant, and the vertical opening edge of the slit SlE(2) is configured in a stepped shape.

[0175] [Features] As described above, the gas sensor element 101 according to this embodiment is a gas sensor capable of detecting a specific gas concentration in a measurement gas. The gas sensor element 101 includes an element substrate (element substrates 100, 100A to 100E) through which a measurement gas is introduced into a measurement gas flow section 7 (internal space) from a gas inlet 10 opening on a surface thereof, and a measurement electrode 44 disposed in the measurement gas flow section 7. A first diffusion rate-controlling section 11 is provided on the gas inlet 10 side of the measurement gas flow section 7. The first diffusion rate-controlling section 11 is provided as one or more slits (slits Sl, SlA to SlE). That is, one or more slits are provided on the gas inlet 10 side of the measurement gas flow section 7. For example, two slits may be provided vertically side by side, that is, side by side in the thickness direction of the element substrate 100, or one slit may be provided.

[0176] In a cross section parallel to the gas inlet 10, each of the one or more slits is formed in a horizontally elongated shape, that is, formed as an opening whose width in the horizontal direction is longer than its width in the vertical direction (thickness direction of the element substrate 100). The average width of each of the one or more slits in the vertical direction is 3 μm or more.

[0177] At least one of the one or more slits described above includes one or more narrow portions (narrow portions Np, NpA to NpE). As long as at least one of the one or more slits described above includes one or more narrow portions, the other slits may not include narrow portions. At least one of the one or more slits may include one, two, or three or more narrow portions.

[0178] In a cross section parallel to the gas inlet 10, the average vertical opening width of each of the one or more narrow portions is 3 μm or less. In each narrow portion, the vertical opening width may vary or may be constant. In each narrow portion, the vertical opening width may vary continuously or discontinuously (e.g., stepwise) along the horizontal direction. In each narrow portion, the vertical opening width may be constant along the horizontal direction. For example, the vertical opening width of each slit in a cross section parallel to the gas inlet 10 may be sloped, that is, may vary continuously along the horizontal direction. The vertical opening width of each slit in a cross section parallel to the gas inlet 10 may be stepped, that is, may vary discontinuously (e.g., stepwise) along the horizontal direction.

[0179] The present inventors have studied a method for improving the effect of suppressing the influence of pulsation in the measurement space on the pressure of the measured gas in the measured gas flow section 7, for a slit "provided on the gas inlet 10 side in the measured gas flow section 7 and having a horizontally elongated opening in a cross section parallel to the gas inlet 10." The present inventors have found that the influence of pulsation on the pressure of the measured gas in the measured gas flow section 7 can be suppressed by increasing the diffusion resistance or pressure loss of the measured gas introduced from the gas inlet 10 to the measured gas flow section 7 by the above-mentioned slit. In particular, the present inventors have found that the influence of the above-mentioned pulsation can be suppressed extremely effectively by configuring at least a part of the above-mentioned slit so that the average vertical opening width is 3 μm or less. In addition, the present inventors have found that the following problems arise when the average vertical opening width of the entire slit is less than 3 μm. In other words, the gas flow rate of the measurement gas introduced into the measurement gas flow section 7 becomes small, and it has been found that in a gas sensor element having a slit with an average vertical opening width of less than 3 μm, the responsiveness to the measurement gas deteriorates and the measurement accuracy decreases.

[0180] Therefore, in the measurement gas flow section 7 of the gas sensor element 101, "one or more slits each having a horizontally elongated shape in a cross section parallel to the gas inlet 10" are provided on the gas inlet 10 side. At least one of the one or more slits includes "one or more narrow portions (narrow portions Np, NpA to NpE) each having an average opening width in the vertical direction of 3 μm or less". For example, the narrow portions enable the gas sensor element 101 to increase the diffusion resistance of the measurement gas introduced into the measurement gas flow section 7. In addition, the outer periphery of the slit including the narrow portions is longer than the outer periphery of a conventional slit having a horizontally elongated rectangular cross section, so that the pressure loss of the measurement gas introduced into the measurement gas flow section 7 is also increased. Therefore, the gas sensor element 101 has an effect that the influence of the pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow section 7 can be extremely effectively suppressed by the one or more narrow portions.

[0181] In the gas sensor element 101, the average opening width in the vertical direction of each of the one or more slits is 3 μm or more. Therefore, the gas sensor element 101 has an advantage that it is possible to avoid a situation in which "the flow rate of the measurement gas introduced into the measurement gas flow portion 7 becomes small due to the vertical opening width of the slit being too small, resulting in deterioration of response accuracy, measurement accuracy, and the like."

[0182] Therefore, the gas sensor element 101 exhibits the effect of more effectively suppressing the influence of pulsation in the measurement space on the pressure of the measurement gas in the measurement gas flow portion 7 while avoiding deterioration of the measurement accuracy.

[0183] [Variations] Although the embodiments of the present invention have been described above, the above description of the embodiments is merely an example of the present invention in every respect. Various improvements and modifications may be made to the above embodiments. Regarding each component of the above embodiments, components may be omitted, replaced, or added as appropriate. In addition, the shape and dimensions of each component of the above embodiments may be changed as appropriate depending on the embodiment. For example, the following modifications are possible. In the following, the same reference numerals are used for components similar to those of the above embodiments, and the description of the same points as those of the above embodiments is omitted as appropriate. The following modifications can be combined as appropriate.

[0184] (Number of slits) So far, an example of a gas sensor element has been described in which the measurement gas flow section 7 has two slits on the gas inlet 10 side. However, it is not essential that the measurement gas flow section 7 has two slits on the gas inlet 10 side. The measurement gas flow section 7 may have one slit on the gas inlet 10 side, or three or more slits. In the gas sensor according to the present invention, one or more slits are provided on the gas inlet 10 side of the measurement gas flow section 7, and at least one of the slits may include a narrow portion having an average vertical opening width of 3 μm or less.

[0185] (Method of forming narrow part) So far, an example has been described in which a narrow portion (e.g., narrow portion Np(1)) is formed in a P-surface slit (e.g., slit Sl(1)) by forming a part of the lower surface of the second solid electrolyte layer 6 in a downwardly convex shape, for example, by providing an aperture width adjustment layer (e.g., aperture width adjustment layer 54(1)) on the lower surface of the second solid electrolyte layer 6. As described above, the aperture width adjustment layer provided on the lower surface of the second solid electrolyte layer 6 may be integral with the second solid electrolyte layer 6, and may be, for example, a part of the second solid electrolyte layer 6 that is bent so as to be convex downward, or may be a protrusion provided on the lower surface of the second solid electrolyte layer 6 that is convex downward. However, the gas sensor element 101 may form a narrow portion in the P-surface slit by forming a part of the upper surface of the first bridge portion 53a in an upwardly convex shape. The gas sensor element 101 may have a narrow portion in the P-surface slit by at least one of forming a portion of the lower surface of the second solid electrolyte layer 6 in a downwardly convex shape and forming a portion of the upper surface of the first bridging portion 53a in an upwardly convex shape.

[0186] Further, so far, an example has been described in which a narrow portion (e.g., narrow portion Np(2)) is formed in an H-plane slit (e.g., slit Sl(2)) by forming a part of the upper surface side of the first solid electrolyte layer 4 in an upwardly convex shape, for example, by providing an aperture width adjustment layer (e.g., aperture width adjustment layer 54(2)) on the upper surface of the first solid electrolyte layer 4. As described above, the aperture width adjustment layer provided on the upper surface of the first solid electrolyte layer 4 may be integral with the first solid electrolyte layer 4, and may be, for example, a part of the first solid electrolyte layer 4 that is bent so as to be convex upward, or may be a protrusion provided on the upper surface of the first solid electrolyte layer 4 that is convex upward. However, in the gas sensor element 101, a narrow portion may be formed in the H-plane slit by forming a part of the lower surface of the first bridge portion 53a in a downwardly convex shape. The gas sensor element 101 may have a narrow portion in the H-plane slit by at least one of forming a part of the upper surface of the first solid electrolyte layer 4 in an upwardly convex shape and forming a part of the lower surface of the first bridging portion 53 a in a downwardly convex shape.

[0187] [Example] In order to verify the effects of the present invention, the following reference element 1, reference element 2, and gas sensor elements according to Examples 1 to 17 were produced. However, the present invention is not limited to the following Examples.

[0188] [Table 1]

[0189] [Table 2]

[0190] Tables 1 and 2 show the results of tests (dynamic pressure measurement tests) on gas sensors including the gas sensor elements according to each of Reference Elements 1 and 2, and Examples 1 to 17. Specifically, Table 1 shows the response evaluation and dynamic pressure dependency of the gas sensors including Reference Elements 1 and the gas sensor elements according to Examples 1 to 12 (each of which is a gas sensor element having two slits). Table 2 shows the response evaluation and dynamic pressure dependency of the gas sensors including Reference Elements 2 and the gas sensor elements according to Examples 13 to 17 (each of which is a gas sensor element having one slit).

[0191] The reference element 1 and the reference element 2 are gas sensor elements in which the slit "is provided on the gas inlet side in the internal space and is a horizontally elongated opening in a cross section parallel to the gas inlet" does not include the range A. The range A is a range in which the vertical opening width is continuously 3 μm or less, and can also be regarded as a continuous (horizontal) range in which the vertical opening width is 3 μm or less. The range A can be regarded as another way of saying the narrow portion (narrow portions Np, NpA to NpE) described with reference to FIGS. 2 to 7, in which "the average vertical opening width is 3 μm or less in a cross section parallel to the gas inlet 10". For example, the reference element 1 and the reference element 2 are conventional gas sensor elements that include a slit "is provided on the gas inlet side in the internal space and is a horizontally elongated rectangular opening in a cross section parallel to the gas inlet".

[0192] The reference element 1 in Table 1 has two of the above-mentioned slits, specifically, a P-surface slit and an H-surface slit. The P-surface slit is a slit closer to the external pump electrode than the heater in the thickness direction of the gas sensor element, and is also called "a slit provided on the upper side (upper slit)". The H-surface slit is a slit closer to the heater than the external pump electrode in the thickness direction of the gas sensor element, and is also called "a slit provided on the lower side (lower slit)". In the reference element 1, neither the P-surface slit nor the H-surface slit includes the range A. In addition, the reference element 2 in Table 2 does not include the H-surface slit, and only the P-surface slit is included, and the P-surface slit does not include the range A.

[0193] Each of Examples 1 to 17 is a gas sensor element having one or more slits that are "provided on the gas inlet side in the internal space and are horizontally elongated openings in a cross section parallel to the gas inlet," and at least one of the slits includes range A.

[0194] Examples 1 to 12 in Table 1 each include a P-plane slit and an H-plane slit, and at least one of the P-plane slit and the H-plane slit includes range A. However, Examples 1 to 12 differ from each other in at least one of the following conditions. That is, they differ from each other in at least one of "the number of ranges A," "the total horizontal length of ranges A / horizontal length of all slits," "the average vertical height [μm] of range A," "the average vertical height [μm] of ranges other than range A," and "slits including range A." "Slits including range A" refers to whether the slits including range A are only P-plane slits, only H-plane slits, or both P-plane slits and H-plane slits.

[0195] Note that "total horizontal length of range A / horizontal length of entire slit" is the ratio of "total horizontal length of range A" to "horizontal length of entire slit". In the following explanation, the unit "μm" for "average vertical height of range A" and "average vertical height of ranges other than range A" will be omitted. Similarly, in the following explanation, the unit "%" for "total horizontal length of range A / horizontal length of entire slit" will be omitted.

[0196] Example 1 is a gas sensor element in which, for each of the P-surface slit and the H-surface slit, the "total horizontal length of the range A / horizontal length of the entire slit" is "100." That is, in Example 1, the P-surface slit and the H-surface slit each have a vertical opening width of 3 μm or less over the entire slit.

[0197] In Example 2, the P-surface slit includes one range A, and the H-surface slit does not include range A. In Example 2, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-surface slit" is "25", the "average vertical height of range A" in the P-surface slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0198] In Example 3, the P-plane slit and the H-plane slit each include one range A. In Example 3, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "100", and the "average vertical height of range A" in the P-plane slit is "3". In Example 3, the P-plane slit has a vertical opening width of 3 μm or less throughout the entire slit, so the "average vertical height of ranges other than range A" in the P-plane slit is "-". In Example 3, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "25", and the "average vertical height of range A" in the H-plane slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0199] In Example 4, the P-plane slit and the H-plane slit each include one range A. In Example 4, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "25", the "average vertical height of range A" in the P-plane slit is "3", and the "average vertical height of ranges other than range A" is "10". Also, in Example 4, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "25", the "average vertical height of range A" in the H-plane slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0200] In Example 5, the P-plane slit and the H-plane slit each include one range A. In Example 5, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "25", the "average vertical height of range A" in the P-plane slit is "1", and the "average vertical height of ranges other than range A" is "7". Also, in Example 5, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "25", the "average vertical height of range A" in the H-plane slit is "1", and the "average vertical height of ranges other than range A" is "7".

[0201] In Example 6, the P-plane slit and the H-plane slit each include one range A. In Example 6, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "25", the "average vertical height of range A" in the P-plane slit is "3", and the "average vertical height of ranges other than range A" is "10". In Example 6, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "100", and the "average vertical height of range A" in the H-plane slit is "3". In Example 6, the H-plane slit has a vertical opening width of 3 μm or less throughout the entire slit, so the "average vertical height of ranges other than range A" in the H-plane slit is "-".

[0202] In Example 7, the P-plane slit and the H-plane slit each include one range A. In Example 7, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "70", the "average vertical height of range A" in the P-plane slit is "1", and the "average vertical height of ranges other than range A" is "7". Also, in Example 7, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "70", the "average vertical height of range A" in the H-plane slit is "1", and the "average vertical height of ranges other than range A" is "7".

[0203] In Example 8, the P-plane slit and the H-plane slit each include one range A. In Example 8, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "50", the "average vertical height of range A" in the P-plane slit is "3", and the "average vertical height of ranges other than range A" is "10". Also, in Example 8, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "50", the "average vertical height of range A" in the H-plane slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0204] In Example 9, the P-surface slit includes one range A, and the H-surface slit does not include range A. In Example 9, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-surface slit" is "20", the "average vertical height of range A" in the P-surface slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0205] In Example 10, the P-plane slit and the H-plane slit each include one range A. In Example 10, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-plane slit" is "20", the "average vertical height of range A" in the P-plane slit is "3", and the "average vertical height of ranges other than range A" is "10". Also, in Example 10, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "20", the "average vertical height of range A" in the H-plane slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0206] In each of Examples 11 and 12, the P-plane slits and the H-plane slits each include multiple ranges A, and for each of the P-plane slits and the H-plane slits, the "total horizontal length of ranges A / horizontal length of the entire slit" is "25."

[0207] Specifically, in Example 11, the P-plane slit and the H-plane slit each include two ranges A. In Example 11, the ratio of the "total horizontal length of the two ranges A" to the "total horizontal length of the P-plane slit" is "25", the "average vertical height of each of the two ranges A" in the P-plane slit is "3", and the "average vertical height of the ranges other than range A" is "10". Also, in Example 11, the ratio of the "total horizontal length of the two ranges A" to the "total horizontal length of the H-plane slit" is "25", the "average vertical height of each of the two ranges A" in the H-plane slit is "3", and the "average vertical height of the ranges other than range A" is "10".

[0208] In Example 12, the P-plane slit and the H-plane slit each include four ranges A. In Example 12, the ratio of the "total horizontal length of the four ranges A" to the "total horizontal length of the P-plane slit" is "25", the "average vertical height of each of the four ranges A" in the P-plane slit is "3", and the "average vertical height of the ranges other than range A" is "10". In Example 12, the ratio of the "total horizontal length of the four ranges A" to the "total horizontal length of the H-plane slit" is "25", the "average vertical height of each of the four ranges A" in the H-plane slit is "3", and the "average vertical height of the ranges other than range A" is "10".

[0209] Examples 13 to 17 in Table 2 are gas sensor elements each having either a P-plane slit or an H-plane slit, and the slit includes range A.

[0210] Specifically, Example 13 does not include an H-plane slit, and only includes a P-plane slit. In particular, Example 13 is a gas sensor element in which the "total horizontal length of range A / horizontal length of entire slit" for the P-plane slit is "100." That is, the P-plane slit in Example 13 has a vertical opening width of 3 μm or less over the entire slit.

[0211] Example 14 does not include an H-surface slit, but only a P-surface slit, and the P-surface slit includes one range A. In particular, in Example 14, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-surface slit" is "25", the "average vertical height of range A" in the P-surface slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0212] Example 15 does not include a P-plane slit, but only an H-plane slit, and the H-plane slit includes one range A. In particular, in Example 15, the ratio of the "horizontal length of range A" to the "horizontal length of the entire H-plane slit" is "25", the "average vertical height of range A" in the H-plane slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0213] Example 16 does not include an H-surface slit, but only a P-surface slit, and the P-surface slit includes one range A. In particular, in Example 16, the ratio of the "horizontal length of range A" to the "horizontal length of the entire P-surface slit" is "20", the "average vertical height of range A" in the P-surface slit is "3", and the "average vertical height of ranges other than range A" is "10".

[0214] Example 17 does not include an H-surface slit, but only a P-surface slit, and the P-surface slit includes multiple ranges A, specifically, two ranges A. In Example 17, the ratio of the "total horizontal length of the two ranges A" to the "horizontal length of the entire P-surface slit" is "25", the "average vertical height of each of the two ranges A" in the P-surface slit is "3", and the "average vertical height of the ranges other than range A" is "10".

[0215] The present inventors conducted the following test to compare the influence (dynamic pressure dependency) of the pulsation in the measurement space on the pressure of the measured gas in the internal space for the gas sensor elements according to each of the above-mentioned reference elements 1 and 2 and Examples 1 to 17. That is, a dynamic pressure measurement test was conducted for the gas sensors including the reference elements 1 and 2 and the gas sensor elements according to each of the Examples 1 to 17 to evaluate the dynamic pressure dependency (the effect of suppressing the influence of the pulsation). In the dynamic pressure measurement test, a pressure gauge and each gas sensor were attached to the exhaust pipe of an automobile engine, and dynamic pressure measurement was performed. A V-type 4.6L gasoline engine was used as the engine, and four of the eight cylinders were operated in the dynamic pressure measurement test. Dynamic pressure (pulsation) was generated by operating the engine, and in the dynamic pressure measurement, the rate of change (%) of the pump current (hereinafter referred to as "Ip0") of each gas sensor (each gas sensor element) was measured. Ip0 changes according to the pressure of the measured gas in the internal space of the gas sensor element (change in the pressure involved). In the dynamic pressure measurement test, ΔIp0 / (average Ip0) was taken as the rate of change (%) of Ip0. The peak-to-peak value of Ip0 was taken as ΔIp0. The acquisition interval of the signal indicating Ip0 was 1 msec. By adjusting the engine conditions (rpm, throttle opening, λ), multiple types of dynamic pressure were generated and the rate of change of Ip0 at each dynamic pressure was measured. The smaller the rate of change of Ip0, the more the dynamic pressure dependency is suppressed, that is, the more the effect of pulsation in the measurement space (inside the exhaust pipe) on the pressure of the measured gas in the internal space of the gas sensor element can be suppressed. In addition, the responsiveness of each gas sensor (each gas sensor element) was evaluated.

[0216] In Tables 1 and 2, a "response evaluation" of "good" indicates that the gas sensor elements (gas sensors) according to Examples 1 to 17 were confirmed to have a responsiveness equal to or greater than that of reference element 1 or reference element 2. In other words, the "response evaluation" was marked as "good" when the responsiveness of the gas sensor elements according to Examples 1 to 17 was not worse than that of reference element 1 or reference element 2 or was improved. A "response evaluation" of "poor" indicates that the responsiveness of the gas sensor elements according to Examples 1 to 17 was worse than that of reference element 1 or reference element 2.

[0217] In Tables 1 and 2, "Dynamic pressure dependency" of "◎ (very good)" indicates that the dynamic pressure dependency of the gas sensor element (gas sensor) according to each of Examples 1 to 17 is improved by 50% or more compared to the dynamic pressure dependency of the reference element 1 or the reference element 2. The dynamic pressure dependency can be understood as "the effect of suppressing the influence of the pulsation in the measurement space on the pressure of the measured gas in the internal space." "Dynamic pressure dependency" of "◯ (good)" indicates that the dynamic pressure dependency of the gas sensor element according to each of Examples 1 to 17 is improved by 25% or more and less than 50% compared to the dynamic pressure dependency of the reference element 1 or the reference element 2. "Dynamic pressure dependency" of "△ (slightly improved)" indicates that the dynamic pressure dependency of the gas sensor element according to each of Examples 1 to 17 is improved by 10% or more and less than 25% compared to the dynamic pressure dependency of the reference element 1 or the reference element 2. The "Dynamic pressure dependency" being "× (poor)" indicates that the dynamic pressure dependency of the gas sensor element according to each of Examples 1 to 17 is improved, is the same, or is worsened by less than 10% compared to the dynamic pressure dependency of reference element 1 or reference element 2.

[0218] (Verification of the effect of suppressing the influence of pulsation by narrow parts) The reference element 1 and Examples 1 to 12 are common in that they are provided with a P-plane slit and an H-plane slit. In addition, compared to the reference element 1 in which neither the P-plane slit nor the H-plane slit includes the range A, Examples 1 to 12 in which at least one of the P-plane slit and the H-plane slit includes the range A all have improved "dynamic pressure dependency". In particular, Example 1 in which "the total horizontal length of the range A / the horizontal length of the entire slit" is "100%" and Example 7 in which "the horizontal length of the range A / the horizontal length of the entire slit" is "70%" have significantly improved "dynamic pressure dependency" compared to the reference element 1. Therefore, it was confirmed that the dynamic pressure dependency (the effect of suppressing the influence of pulsation) is improved by configuring the slit "which is provided on the gas inlet side in the internal space and is an opening with a horizontally elongated shape in a cross section parallel to the gas inlet" to include the range A.

[0219] The effect was also observed in the gas sensor element having one slit, instead of two, which is "provided on the gas inlet side in the internal space and is an opening with a horizontally elongated shape in a cross section parallel to the gas inlet". That is, the reference element 2 and Examples 13 to 17 are common in that they have only one of the P-plane slit and the H-plane slit. In addition, compared with the reference element 2 in which the slit does not include the range A, Examples 13 to 17 in which the slit includes the range A all have improved "dynamic pressure dependency". Therefore, it was confirmed that the dynamic pressure dependency was also improved in the gas sensor element having one slit "provided on the gas inlet side in the internal space and is an opening with a horizontally elongated shape in a cross section parallel to the gas inlet" by configuring the slit to include the range A.

[0220] As confirmed above, by configuring at least one of the one or more slits to include one or more narrow portions Np "whose average opening width in the vertical direction in a cross section parallel to the gas inlet is 3 μm or less," the gas sensor element achieves the following effects: That is, by configuring at least one slit to include one or more narrow portions Np, the gas sensor element can extremely effectively suppress the influence of pulsation in the measurement space on the pressure of the measured gas in the internal space.

[0221] (Verification of the relationship between the length of the narrow portion of the slit and response) In Table 1, in Example 1, for all of the one or more slits (i.e., both the P-plane slits and the H-plane slits), the "sum of the horizontal length of range A / the horizontal length of all the slits" is greater than "50", specifically, "100". In addition, in Example 7, for all of the one or more slits, the "sum of the horizontal length of range A / the horizontal length of all the slits" is greater than "50", specifically, "70". And the "response evaluation" of Example 1 and Example 7 was both "X".

[0222] In contrast, in each of Examples 2 to 6 and 8 to 12, for at least one of the one or more slits, the "total horizontal length of range A / horizontal length of all slits" is "50" or less. For example, in Examples 3 and 6, for one of the P-plane slit and the H-plane slit, the "total horizontal length of range A / horizontal length of all slits" is "100", but for the other, the "total horizontal length of range A / horizontal length of all slits" is "25". In addition, in each of Examples 2, 4, 5, and 8 to 12, for all of the one or more slits, the "total horizontal length of range A / horizontal length of all slits" is "50" or less. And, the "response evaluation" of Examples 2 to 6, 8 to 12, and 14 to 17 was all "good".

[0223] A similar tendency was observed for a gas sensor element having one slit, instead of two, which is "provided on the gas inlet side in the internal space and is a horizontally elongated opening in a cross section parallel to the gas inlet." That is, in Example 13, for the only slit (P-surface slit), the "total horizontal length of range A / horizontal length of entire slit" is greater than "50," specifically, "100." The "response evaluation" of Example 13 was then "x."

[0224] In contrast, in each of Examples 14 to 17, for the only slit provided, the "total horizontal length of area A / horizontal length of entire slit" was less than or equal to 50. And the "response evaluation" of Examples 14 to 17 was all "good".

[0225] Therefore, from the viewpoint of "responsiveness", it was confirmed that it is desirable to set the ratio of the "total horizontal length of range A" to the "horizontal length of the entire slit" for at least one of the one or more slits to "50%" or less. By setting the ratio of the "total horizontal length of range A" to the "horizontal length of the entire slit" for at least one of the one or more slits to "50%" or less, the gas sensor element can achieve the following effects. That is, the gas sensor element can avoid a situation in which "the flow rate of the measurement gas introduced into the internal space is reduced due to the vertical opening width of the slit being made too small, resulting in deterioration of response accuracy, measurement accuracy, etc."

[0226] (Verification of the relationship between the length of the narrow portion of the entire slit and the dynamic pressure dependency) In Table 1, in Examples 9 and 10, for all of the one or more slits (i.e., both the P-plane slits and the H-plane slits), the "total lateral length of range A / lateral length of all slits" is smaller than "25." And, the "dynamic pressure dependency" of Examples 9 and 10 was both "△."

[0227] In contrast, in each of Examples 2 to 6, 8, 11, and 12, for at least one of the one or more slits, the "total horizontal length of range A / horizontal length of all slits" is "25" or more. For example, in Example 2, for the H-plane slit, the "total horizontal length of range A / horizontal length of all slits" is "0", but for the P-plane slit, the "total horizontal length of range A / horizontal length of all slits" is "25". In addition, in each of Examples 3 to 6, 8, 11, and 12, for all of the one or more slits, the "total horizontal length of range A / horizontal length of all slits" is "25" or more. And, the "dynamic pressure dependency" of Examples 2 to 6, 8, 11, and 12 was all "good".

[0228] A similar tendency was observed for a gas sensor element having one slit, instead of two, which is "a horizontally elongated opening provided on the gas inlet side in the internal space in a cross section parallel to the gas inlet." That is, in Example 16, for the only slit (P-surface slit), the "total horizontal length of area A / horizontal length of entire slit" is smaller than "25," specifically, "20." And the "dynamic pressure dependency" of Example 16 was rated "△."

[0229] In contrast, in each of Examples 14, 15, and 17, for the only slit provided, the "total horizontal length of area A / horizontal length of entire slit" was equal to or greater than 25. And, the "dynamic pressure dependency" of Examples 14, 15, and 17 was all rated "good."

[0230] Therefore, from the viewpoint of "dynamic pressure dependency (effect of suppressing the influence of pulsation in the measurement space on the pressure of the gas to be measured in the internal space)", it was confirmed that the ratio of "the total horizontal length of the range A" to "the horizontal length of the entire slit" for at least one of the one or more slits is preferably "25" or more. By setting the ratio of "the total horizontal length of the range A" to "the horizontal length of the entire slit" for at least one of the one or more slits to "25" or more, the gas sensor element can achieve the following effect. That is, the gas sensor element can suppress the influence of the above-mentioned pulsation extremely effectively by the range A, that is, by the narrow portion (narrow portions Np, NpA to NpE) "wherein the average vertical opening width is 3 μm or less in the cross section parallel to the gas inlet 10". [Explanation of symbols]

[0231] 101...sensor element (gas sensor element), 100, 100A to 100E...element base, 10: gas inlet; 7: measurement gas flow section (internal space); 44: measurement electrode; 11...first diffusion rate limiting section (slit), SlA to SlE, ...slit, Np, NpA~NpE...Narrow part, Wp, WpA~WpE...Wide part

Claims

1. an element substrate into whose internal space a gas to be measured is introduced through a gas inlet opening on the surface; A measurement electrode disposed in the internal space; Equipped with One or more slits are provided on the gas inlet side in the internal space, In a cross section parallel to the gas inlet, Each of the one or more slits is formed in a horizontally elongated shape, The average vertical opening width of each of the one or more slits is 3 μm or more; At least one slit of the one or more slits includes one or more narrow portions; In the cross section, the average opening width in the vertical direction of each of the one or more narrow portions is 3 μm or less. Gas sensor element.

2. The sum of the lateral lengths of the one or more narrow portions in the cross section is 25% or more and 50% or less of the lateral length of the entire slit including the one or more narrow portions in the cross section. The gas sensor element according to claim 1 .

3. In the cross section, the average opening width in the vertical direction of the wide portion other than the one or more narrow portions of the slit including the one or more narrow portions is 10 μm or less.

3. The gas sensor element according to claim 1.

4. Each of the one or more slits includes the one or more narrow portions.

3. The gas sensor element according to claim 1.

5. In the cross section, each of the one or more narrow portions has a constant opening width in the vertical direction.

3. The gas sensor element according to claim 1.

6. At least one slit of the one or more slits includes one of the narrow portions.

3. The gas sensor element according to claim 1.

7. In the cross section, the narrow portion is disposed at the center in the lateral direction of the slit that includes the narrow portion. The gas sensor element according to claim 6.

Citation Information

Patent Citations

  • Gas sensor and nitrogen oxide sensor

    JP2000028576A