Technical Problem

Existing methods for producing carbonates, such as evaporating seawater to concentrate carbon dioxide and alkaline earth metal ions, require significant energy and result in alkaline earth metal carbonates adhering as scale to membrane surfaces, deteriorating treatment performance.

Method used

A carbonate fixation device and method using semipermeable membranes with specific rejection rates for calcium and magnesium chloride, allowing some carbonates to pass through, reducing energy consumption and preventing scale buildup.

Benefits of technology

Efficient fixation of carbon dioxide into carbonates with reduced energy use and minimized membrane deterioration, maintaining treatment performance by allowing some carbonates to be discharged, thus preventing scale formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024137635000001_ABST
    Figure 2024137635000001_ABST
Patent Text Reader

Abstract

To provide a carbonate immobilization device and a carbonate immobilization method for immobilizing carbon dioxide using membrane filtration, which are a device and a method for suppressing adhesion of alkaline earth metal carbonate as scale to the membrane surface, and suppressing a decrease in the treatment performance of water to be treated.SOLUTION: A carbonate immobilization device of the present invention is characterized in that it uses a membrane with a calcium chloride rejection rate of 1.0% or more and 99.0% or less to concentrate water to be treated containing alkaline earth metal ions to produce alkaline earth metal carbonates. By using the membrane with a calcium chloride rejection rate of 1.0% or more and 99.0% or less, some of the alkaline earth metal carbonates produced during the concentration of the water to be treated pass through the membrane. This can prevent deterioration in the treatment performance of the water to be treated caused by deposition of carbonates, known as scale, on the surface of the membrane, and can efficiently fix carbon dioxide.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Method for completely dissolving all minerals of evaporated seawater

    JP2006070011A

Cited By

  • Carbon dioxide fixation method and carbon dioxide fixation device, and method for evaluating amount of carbon dioxide fixed and system for evaluating amount of carbon dioxide fixed

    WO2026004762A1