Packaging laminate and package

JP2024152144AInactive Publication Date: 2024-10-25TOPPAN HOLDINGS INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023066164
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-14
Publication Date
2024-10-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The polyethylene laminate for packaging materials described in Patent Document 1 has a high monomaterial ratio, resulting in poor bag-making suitability and insufficient sealing strength, making it difficult to obtain high-quality recycled products.

Method used

A packaging laminate comprising a base layer made of a single resin film and a sealant layer made of a heat-sensitive adhesive composition that can be peeled off with a water-containing liquid, allowing for efficient recycling and sufficient sealing strength by thermal bonding at a temperature below the resin's melting point.

Benefits of technology

The laminate enables high-quality recycling with a high monomaterial ratio and provides excellent bag-making suitability and sufficient sealing strength, preventing gas penetration and reducing thermal adhesion defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024152144000001_ABST
    Figure 2024152144000001_ABST
Patent Text Reader

Abstract

To provide a packaging laminate which enables acquisition of a high-quality recycled product of a high mono-material ratio, has excellent bag-making suitability, and can apply a sufficient sealing strength to a package, and the package.SOLUTION: This packaging laminate comprises: a base material layer containing a resin film mainly made of a single resin; and a sealant layer. The sealant layer is a layer including a heat-sensitive adhesive composition and peelable from the base material layer by a water-containing solution.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to packaging laminates and packages. [Background technology]

[0002] In recent years, there has been an increasing demand for the creation of a recycling-oriented society with less environmental impact, and in response to this, attempts have been made to recycle and reuse packaging materials. For example, the following Patent Document 1 proposes a polyethylene laminate for packaging material that includes, in this order, a stretched polyethylene film, a polyethylene layer including a vapor deposition film, and a heat-sealable polyethylene layer. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-166810 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, the polyethylene laminate for packaging material described in the above-mentioned Patent Document 1 has the following problems. In other words, the polyethylene laminate for packaging materials described in Patent Document 1 has a high monomaterial ratio, and therefore although it is possible to obtain a high-quality recycled product (regenerated material) with a high monomaterial ratio, there is room for improvement in terms of suitability for bag making and the seal strength imparted to the package.

[0005] Therefore, an object of the present disclosure is to provide a packaging laminate and a packaging body that can produce high-quality recycled products with a high mono-material ratio, while having excellent bag-making suitability and being able to impart sufficient sealing strength to the packaging body. [Means for solving the problem]

[0006] One aspect of the present disclosure provides a packaging laminate comprising a base layer including a resin film mainly made of a single resin, and a sealant layer, the sealant layer being made of a heat-sensitive adhesive composition and being a layer that can be peeled off from the base layer by a water-containing liquid.

[0007] According to the packaging laminate of the present disclosure, since the sealant layer is a layer that can be peeled off from the base layer by a water-containing liquid, when the packaging laminate is brought into contact with a water-containing liquid, the sealant layer can be easily peeled off from the base layer, and it becomes possible to leave the base layer including the resin film mainly made of a single resin. Therefore, according to the packaging laminate of the present disclosure, it is possible to obtain a high-quality recycled product with a high mono-material ratio. In addition, according to the packaging laminate of the present disclosure, the sealant layer is a layer made of a heat-sensitive adhesive composition, and the heat-sensitive adhesive composition generally exhibits adhesion at a lower temperature than the resin film contained in the base layer. Therefore, when manufacturing a packaging bag using the packaging laminate, if the heat-bonding portion at the periphery of the packaging laminate is heated and heat-bonded at a temperature lower than the melting point of the resin film, the sealant layers of the packaging laminate can be firmly heat-bonded to each other at the heat-bonding portion while preventing the resin film from melting. Therefore, the following advantages are obtained. (1) The shrinkage of the portion to be thermally sealed can be suppressed, and the shortening of the passage path of gas from the outside to the inside of the packaging bag can be suppressed in the obtained thermally sealed portion, thereby suppressing the intrusion of gas into the packaging bag. (2) When the portion to be thermally sealed is heated using a sealing bar to produce a packaging bag, the resin film can be prevented from sticking to the sealing bar, thereby preventing partial damage to the resin film that occurs when the sealing bar is separated from the resin film. (3) Unintentional thermal bonding between sealant layers in non-thermal-bonded areas and thermal bonding between resin films when a folded portion of the packaging laminate is positioned between areas to be thermally bonded are suppressed, thereby preventing the space for accommodating the packaged items within the packaging bag from becoming narrower. (4) When the peripheral portions of the packaging laminate to be heat-sealed are heated at a temperature lower than the melting point of the resin film to effect heat sealing, sufficient sealing strength is imparted between the sealant layers of the packaging laminate. Thus, the packaging laminate of the present disclosure has excellent suitability for bag formation and can impart sufficient seal strength to the package.

[0008] In the above-mentioned packaging laminate, the water-containing liquid may contain hot water having a temperature of 60° C. or higher, or may contain an alkaline component. In this case, when the water-containing liquid is hot water or contains an alkaline component, the sealant layer can be effectively peeled off from the base layer when the packaging laminate is brought into contact with the water-containing liquid, and therefore the packaging laminate of the present disclosure makes it possible to more efficiently obtain a high-quality recycled product with a high mono-material ratio.

[0009] The packaging laminate may further include a printed layer between the base layer and the sealant layer, the printed layer being peelable from the base layer by a water-containing liquid. In this case, since the printed layer can be peeled off from the base layer by the water-containing liquid, when the packaging laminate is brought into contact with the water-containing liquid, not only the sealant layer but also the printed layer can be peeled off from the base layer. Therefore, according to the packaging laminate of the present disclosure, it is possible to obtain a high-quality recycled product with a high mono-material ratio.

[0010] In the packaging laminate, the base layer may further include a gas barrier layer. Because the base layer of this packaging laminate includes a gas barrier layer, even if an item to be packaged is placed in a packaging bag obtained using the packaging laminate, the intrusion of gas into the packaging bag is inhibited, thereby inhibiting deterioration of the quality of the packaged item due to gas.

[0011] In the packaging laminate, the resin film may contain a polyolefin resin. In this case, the water vapor barrier property of the packaging laminate can be improved.

[0012] Another aspect of the present disclosure is a packaging bag comprising: a packaging bag; and an item to be packaged contained within the packaging bag; the packaging bag is obtained by using the above-described packaging laminate and heating and thermally bonding a portion to be heat-sealed at a peripheral portion of the packaging laminate at a temperature lower than the melting point of the resin film. According to the package of the present disclosure, for example, after the packaged items are discharged, the remaining package bag can be brought into contact with a water-containing liquid to peel off the sealant layer from the base layer. Therefore, the package of the present disclosure makes it possible to obtain a high-quality recycled product with a high mono-material ratio. The packaging body of the present disclosure is obtained by using the above-mentioned packaging laminate and by heating and heat-sealing the portions to be heat-sealed at the periphery of the packaging laminate at a temperature lower than the melting point of the resin film. The above-mentioned packaging laminate has excellent suitability for bag making and can impart sufficient seal strength to the packaging body. Therefore, the packaging body of the present disclosure can be in a state suitable for use as a packaging body and have sufficient seal strength. Effect of the Invention

[0013] According to the present disclosure, a packaging laminate and a packaging body are provided that enable the production of high-quality recycled products with a high mono-material ratio, while having excellent suitability for bag making and being able to impart sufficient sealing strength to the packaging body. [Brief description of the drawings]

[0014] [Figure 1] 1 is a cross-sectional view showing one embodiment of a packaging laminate of the present disclosure. [Diagram 2] FIG. 1 is a front view of one embodiment of a package of the present disclosure. [Diagram 3] FIG. 3 is a cross-sectional view taken along line III-III in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. In the following description, the same or equivalent components are designated by the same reference numerals, and overlapping descriptions will be omitted.

[0016] <Packaging laminate> Fig. 1 is a cross-sectional view showing one embodiment of a packaging laminate of the present disclosure. As shown in Fig. 1, the packaging laminate 100 includes a base layer 10 including a resin film 11 mainly made of a single resin, and a sealant layer 20. The sealant layer 20 is made of a heat-sensitive adhesive composition and is a layer that can be peeled off from the base layer 10 by a water-containing liquid.

[0017] The packaging laminate 100 may further include a printed layer 30 between the base layer 10 and the sealant layer 20 .

[0018] According to the packaging laminate 100, the sealant layer 20 is a layer that can be peeled off from the base layer 10 by a water-containing liquid, so that when the packaging laminate 100 is brought into contact with a water-containing liquid, the sealant layer 20 can be easily peeled off from the base layer 10, and it becomes possible to leave the base layer 10 including the resin film 11 mainly made of a single resin. Therefore, according to the packaging laminate 100, it is possible to obtain a high-quality recycled product with a high mono-material ratio.

[0019] Moreover, according to the packaging laminate 100, the sealant layer 20 is a layer made of a heat-sensitive adhesive composition, which generally exhibits adhesiveness at a lower temperature than the resin film 11 contained in the base layer 10. Therefore, when manufacturing a packaging bag using the packaging laminate 100, by heating and heat-bonding the portions to be heat-bonded in the packaging laminate 100 at a temperature lower than the melting point of the resin film 11, it is possible to firmly heat-bond the sealant layers 20 of the packaging laminate 100 to each other in the portions to be heat-bonded, while avoiding melting of the resin film 11. This provides the following advantages. (1) The shrinkage of the portion to be thermally sealed can be suppressed, and the shortening of the passage path of gas from the outside to the inside of the packaging bag can be suppressed in the obtained thermally sealed portion, thereby suppressing the intrusion of gas into the packaging bag. (2) When the portion to be thermally bonded is heated using a sealing bar to manufacture a packaging bag, the resin film 11 can be prevented from sticking to the sealing bar, thereby preventing partial damage to the resin film 11 that occurs when the sealing bar is separated from the resin film 11. (3) Unintentional thermal bonding between the sealant layers 20 in the non-thermal-bonded portions and between the resin films 11 when the folded portion of the packaging laminate 100 is positioned between the portions to be thermally bonded are suppressed, thereby preventing the space for accommodating the packaged items in the packaging bag from becoming narrower. (4) When the portions to be heat-sealed at the peripheral portions of the packaging laminate 100 are heated at a temperature lower than the melting point of the resin film 11 and heat-sealed, the sealant layer 20 becomes adhesive, thereby providing sufficient sealing strength between the sealant layers 20 of the packaging body. Thus, the packaging laminate 100 has excellent suitability for bag formation and can impart sufficient seal strength to the package.

[0020] The packaging laminate 100 will now be described in detail.

[0021] (A) Base material layer The base layer 10 includes a resin film 11. The base layer 10 may further include a gas barrier layer 12.

[0022] (Resin film) The resin film 11 is mainly made of a single resin. A "single resin" refers to one type of resin. Resins that have a specific structural unit in common are considered to be of the same type. Thus, for example, homopolymers, copolymers, or homopolymers and copolymers of a resin are all of the same type, since they are resins that have a specific structural unit in common. The phrase "mainly made of a single resin" means that the resin film 11 contains 50% by mass or more of a single resin. From the viewpoint of obtaining a recycled product with a high mono-material ratio, the content of the single resin in the resin film 11 is preferably 80% by mass or more, and more preferably 90% by mass or more. The content of the single resin in the resin film 11 may be 100% by mass. A recyclable film can be used as the resin film 11. Here, recycling refers to material recycling or chemical recycling. Examples of the resin used for the resin film 11 include thermoplastic resins such as polyolefin resins, polyester resins, and polyamide resins. Among them, polyolefin resins are preferred. In this case, the water vapor barrier properties of the packaging laminate 100 can be improved. In particular, from the viewpoint of packaging bag applications, polyethylene or polypropylene is preferred as the polyolefin resin. As the polyester resin used for the resin film 11, polyethylene terephthalate is preferable from the viewpoint of use in packaging bags. As the polyamide resin used for the resin film 11, nylon is preferable from the viewpoint of use as a packaging bag.

[0023] The resin may be a resin obtained using a raw material (monomer) derived from a fossil fuel or a resin obtained using a raw material (monomer) derived from biomass, but from the viewpoint of reducing the environmental load, it is preferable that the resin is a resin obtained using a raw material derived from biomass. Alternatively, the resin may be a recycled resin. The recycled resin may be a mechanically recycled resin or a chemically recycled resin.

[0024] The resin film 11 may contain at least one additive selected from a filler, an antistatic agent, a plasticizer, a lubricant, an antioxidant, and the like, as necessary.

[0025] The resin film 11 may be composed of a single layer or a laminate of multiple layers. The resin film 11 may be either a stretched film or an unstretched film.

[0026] The thickness of the resin film 11 is not particularly limited and can be adjusted appropriately depending on the application or desired characteristics. When the resin film 11 is a stretched film, the thickness of the resin film 11 is preferably 10 μm or more, more preferably 20 μm or more. The thickness of the resin film 11 is preferably 80 μm or less, more preferably 50 μm or less. When the resin film 11 is an unstretched film, the thickness of the resin film 11 is preferably 30 μm or more, more preferably 40 μm or more. The thickness of the resin film 11 is preferably 100 μm or less, more preferably 60 μm or less.

[0027] (Gas barrier layer) The gas barrier layer 12 is a layer having a barrier property against gases such as oxygen and water vapor. The gas barrier layer 12 is disposed on the sealant layer 20 side of the resin film 11, as shown in FIG. Examples of the gas barrier layer 12 include a deposition layer, a coating layer, and a hydroxyl group-containing resin layer. Each of these may be used alone or in a combination of two or more.

[0028] A vapor-deposited layer is a layer formed by vapor deposition. A vapor-deposited layer is composed of inorganic materials. Examples of inorganic materials include metals and metal oxides.

[0029] The metal constituting the metal or metal oxide includes at least one metal selected from the group consisting of Si, Al, Mg, Sn, Ti, and In. As the metal oxide, silicon oxide (SiOx), aluminum oxide (AlOx), or a mixture thereof is preferable. Both SiOx and AlOx have excellent water vapor barrier properties, and therefore can improve the water vapor barrier properties of the packaging laminate 100. Among them, SiOx is preferable as the metal oxide. In this case, it becomes possible for the packaging laminate 100 to have more excellent water vapor barrier properties. The vapor-deposited layer may consist of a single layer or multiple layers.

[0030] In addition, when the base layer 10 is a laminate of OPP (oriented polypropylene) as the resin film 11 and a VM layer (AL vapor deposition layer) as a gas barrier layer, for example, VM-OPP can be used as the base layer 10.

[0031] The coating layer includes, for example, a resin composition. The resin composition includes, for example, a copolymer of an olefin and an unsaturated fatty acid or an anhydride thereof (hereinafter, also referred to as a "polyolefin copolymer resin").

[0032] The polyolefin copolymer resin is a copolymer of an olefin such as ethylene and an unsaturated fatty acid or an anhydride thereof.

[0033] Examples of the unsaturated fatty acid include acrylic acid, methacrylic acid, maleic acid, itaconic acid, fumaric acid, and crotonic acid.

[0034] Examples of the anhydrides of unsaturated fatty acids include maleic anhydride and itaconic anhydride.

[0035] The hydroxyl-containing resin layer is a layer containing a hydroxyl-containing resin, and examples of the hydroxyl-containing resin include ethylene-vinyl alcohol copolymer (EVOH) and polyvinyl alcohol (PVA), etc. Among them, EVOH is preferred from the viewpoint of improving the oxygen barrier property. In addition, when the base layer 10 is a laminate of a resin film 11 and a hydroxyl-containing resin layer as a gas barrier layer, the base layer 10 can be obtained by co-extruding the resin film 11 and the hydroxyl-containing resin layer.

[0036] (B) Sealant layer The sealant layer 20 is made of a heat-sensitive adhesive composition that exhibits adhesion at a temperature lower than the melting point of the resin film 11, and is a layer that can be peeled off from the base layer 10 by a water-containing liquid.

[0037] A heat-sensitive adhesive composition is a composition that does not exhibit adhesiveness at room temperature (35° C. or lower) but develops adhesiveness when heated. The melting point Tm of the resin film 11 means the "peak melting temperature" determined in accordance with the method described in JIS K7121-1987, and when two or more melting peaks appear, it means the lowest peak melting temperature. The temperature T1 at which the heat-sensitive adhesive composition exhibits adhesiveness (adhesiveness exhibiting temperature) may be any temperature lower than the melting point Tm of the resin film 11, and Tm-T1 (hereinafter also referred to as "ΔT") is not particularly limited as long as it is greater than 0° C., but ΔT is preferably 20° C. or more, and more preferably 30° C. or more. In this case, by having ΔT of 20° C. or more, the packaging laminate 100 has better bag-making suitability and can impart more sufficient seal strength to the package.

[0038] The water-containing liquid may be any liquid containing water. The water-containing liquid may be water or an aqueous solution. The water may be at room temperature (35° C. or less), but warm water of 60° C. or more is preferable. Since the water-containing liquid contains warm water, when the packaging laminate 100 is brought into contact with the water-containing liquid, the sealant layer 20 can be effectively peeled off from the base material layer 10. Therefore, the packaging laminate 100 makes it possible to more efficiently obtain a high-quality recycled product with a high mono-material ratio. More preferably, the temperature of the hot water is 75° C. or higher. However, from the viewpoint of suppressing evaporation, the temperature of the hot water is preferably 100° C. or lower, and more preferably 90° C. or lower. The water-containing liquid may further contain an alkaline component. In this case, as in the case where the water is warm water, when the packaging laminate 100 is brought into contact with the water-containing liquid, the sealant layer 20 can be effectively peeled off from the base material layer 10. Therefore, the packaging laminate 100 makes it possible to more efficiently obtain a high-quality recycled product with a high mono-material ratio. An example of the alkaline component is sodium hydroxide.

[0039] Examples of heat-sensitive adhesive compositions include water-soluble hot melt adhesives that are solid at room temperature, or compositions obtained by drying a water-soluble delayed tack adhesive (heat-sensitive varnish) that is liquid at room temperature to remove the solvent.

[0040] The water-soluble hot melt adhesive contains, for example, a thermoplastic resin and a tackifier.

[0041] The thermoplastic resin improves the flexibility of the hot melt adhesive and imparts cohesive strength. The acid value of the thermoplastic resin is preferably 90 mgKOH / g or more, more preferably 95 mgKOH / g or more, and particularly preferably 98 mgKOH / g or more. Examples of thermoplastic resins having an acid value of 90 mgKOH / g or more include ethylene-(meth)acrylic acid copolymers, (meth)acrylic acid-(meth)acrylic acid ester copolymers, α-olefin-maleic anhydride copolymers, and styrene-(meth)acrylic acid copolymers. When the acid value is 90 mgKOH / g or more, the sealant layer 20 is easily peeled off by a water-containing liquid containing an alkaline component.

[0042] The tackifier can improve the adhesive strength of the sealant layer 20 and improve the wettability and workability of the hot melt adhesive. Specific examples of the tackifier include rosin, rosin derivatives (hydrogenated rosin, disproportionated rosin, polymerized rosin, acrylic acid modified rosin, fumaric acid modified rosin, maleic acid modified rosin, and their rosin esters (rosins esterified with alcohol, glycerin, pentaerythritol, etc.)), terpene resins (α-pinene, β-pinene), terpene phenol resins, aromatic modified terpene resins, hydrogenated terpene resins, aliphatic petroleum resins, aromatic petroleum resins, copolymerized petroleum resins, alicyclic petroleum resins, coumarone-indene resins, styrene resins, and phenol resins. Considering alkali dispersibility, the acid value of the tackifier is preferably 150 mgKOH / g or more. Examples of such tackifiers include rosin and rosin derivatives. Examples of rosin or rosin derivatives include raw rosin, (meth)acrylic acid modified rosin, (anhydrous) maleic acid modified rosin, fumaric acid modified rosin, hydrogenated rosin, and polymerized rosin. Considering the blocking property of the packaging laminate 100, the softening point of the tackifier is 75° C. or higher, preferably 85° C. or higher, and more preferably 100° C. or higher.

[0043] The water-soluble hot melt adhesive may further contain a wax. Wax can reduce the melt viscosity of the hot melt adhesive to improve workability, prevent blocking, adjust the open time, and improve heat resistance. When wax is used in the hot melt adhesive, the viscosity is low, workability is improved, and stringiness during application is less likely to occur. Examples of wax include carnauba wax, candelilla wax, montan wax, fatty acid, fatty acid glyceride, polyethylene wax, paraffin wax, microcrystalline wax, Fischer-Tropsch wax, polypropylene wax, waxes obtained by oxidizing these, ethylene-acrylic acid copolymer wax, and ethylene-methacrylic acid copolymer wax. Considering the peelability due to the alkaline component, montan wax and ethylene-acrylic acid copolymer wax are preferred as the wax.

[0044] The viscosity of the hot melt adhesive is preferably 10 to 1,000,000 cps, and more preferably 50 to 500,000 cps at 140° C. When the viscosity of the hot melt adhesive is 10 to 1,000,000 cps or 10 cps at 140° C., coating is facilitated.

[0045] In order to prevent thermal degradation and decomposition, hot melt adhesives are often used with high molecular weight hindered polyhydric phenols, triazine derivatives, high molecular weight hindered phenols, dialkyl phenol sulfides, 2,2'-methylene-bis-(4-methyl-6-tert-butylphenol), 4,4'-methylene-bis-(2,6-di-tert-butylphenol), 2,6-di-tert-butyl-p-cresol, 2,2'-methylene-bis-(4-methyl-6-tert-butylphenol), 2,5- It may contain antioxidants such as di-tert-butylhydroquinone, 2,2,4-trimethyl-1,2-dihydroquinoline, 2,2,4-trimethyl-1,2-dihydroquinoline polymers, 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline, dibutyl dithiocarbamate nickel, 1-oxy-3-methyl-4-isopropylbenzene, 4,4'-butylidenebis-(3-methyl-6-tert-butylphenol), and 2-mercaptobenzimidazole.

[0046] The acid value of the hot melt adhesive is preferably 100 mgKOH / g or more, more preferably 150 mgKOH / g or more. When the acid value is 100 mgKOH / g or more, the sealant layer 20 is provided with water resistance and is easily dispersed or dissolved in a water-containing liquid containing an alkaline component. The softening point of the hot melt adhesive is preferably 50° C. or higher. When the softening point of the hot melt adhesive is 50° C. or higher, the blocking resistance is improved, and blocking is less likely to occur when the adhesive is stored in a rolled form. The softening point of the hot melt adhesive is preferably 120° C. or lower.

[0047] The water-soluble hot melt adhesive may contain, in addition to the thermoplastic resin, tackifier, and wax, silicone to prevent blocking.

[0048] In the hot melt adhesive, for example, 10 to 70 parts by mass of thermoplastic resin, 10 to 70 parts by mass of tackifier, and 1 to 70 parts by mass of wax are mixed.

[0049] Methods for applying the hot melt adhesive to the base layer 10 or the printing layer 30 include a roll coater method using a direct roll, a gravure roll, etc., an extrusion coater method, a slit orifice coater method, etc., but any coating method may be used. The coating method may involve dissolving the hot melt adhesive in a solvent, coating it, and then heating and drying to remove the solvent.

[0050] The coating amount of the hot melt adhesive is preferably 7 to 15 g / m 2 The coating amount on the base layer 10 or the printing layer 30 is 7 g / m 2 If the adhesive is more than 15g / m, it will be more resistant to water and condensation after adhesion. 2 If the viscosity is less than 100 ppm, hot melt adhesives become economical.

[0051] Such water-soluble hot melt adhesives may be commercially available products. Examples of hot melt adhesives include KIC KRONES' "Colfix HM4433 / 1" and Toyo Petrolite Co., Ltd.'s product name "Label Melt".

[0052] The water soluble delayed tack adhesive comprises a thermoplastic resin, a tackifier, a plasticizer, and a solvent.

[0053] As the thermoplastic resin, for example, a water-soluble resin is preferably used. Examples of such water-soluble resin include ethylene-vinyl acetate copolymer resin, acrylic acid ester copolymer obtained by copolymerizing (meth)acrylic acid ester with unsaturated carboxylic acid such as acrylic acid or maleic acid, styrene-acrylic acid ester copolymer, styrene-butadiene copolymer, etc. Examples of the (meth)acrylic acid ester include methyl (meth)acrylate, ethyl (meth)acrylate, isopropylene (meth)acrylate, isobutyl (meth)acrylate, n-butyl (meth)acrylate, amyl (meth)acrylate, hexyl (meth)acrylate, and 2-ethylhexyl (meth)acrylate. Among these, ethylene-vinyl acetate copolymer resin is preferable, since in this case, it is possible to make it difficult for the sealant layers 20 to peel off from each other in the package.

[0054] Examples of the tackifier include terpene resins, aliphatic petroleum resins, aromatic petroleum resins, coumarone-indene resins, styrene resins, phenol resins, terpene-phenol resins, and rosin derivatives.

[0055] A plasticizer is in a crystalline state below its melting point and does not impart plasticity to the resin, but melts and dissolves in the resin when heated to or above its melting point, swelling or softening the resin. That is, a plasticizer imparts non-adhesive properties to the sealant layer 20 below its melting point, but causes the sealant layer 20 to exhibit adhesiveness when heated to or above its melting point. In other words, the melting point of the plasticizer is the temperature at which the sealant layer 20 exhibits adhesiveness. The melting point of the plasticizer is preferably 50 to 100° C. If the melting point of the plasticizer is 50° C. or higher, the sealant layer 20 is less likely to exhibit adhesion during storage of the packaging laminate 100, making it possible to eliminate the need for temperature control during storage or transportation before use. If the melting point of the plasticizer is 100° C. or lower, it becomes easier to increase the difference between the melting point of the resin film 11 and the melting point of the plasticizer, making it possible to impart sufficient seal strength to the package. Examples of plasticizers include sucrose benzoate, ethylene glycol dibenzoate, trimethylolethane tribenzoate, glyceride tribenzoate, pentaerythritol tetrabenzoate, diphenyl phthalate, dihexyl phthalate, dicyclohexyl phthalate, dihydroabietyl phthalate, dimethyl isophthalate, sucrose octaacetate, tricyclohexyl citrate, and N-cyclohexyl-p-toluenesulfonamide.

[0056] The sealant layer 20 is obtained by applying a water-soluble delayed tack adhesive in an emulsion state onto the base layer 10 or the printing layer 30 using a coating method such as gravure coating, roll coating, reverse roll coating, lip coating, knife coating, etc., and drying at a temperature of, for example, 40 to 60°C.

[0057] The amount of the water-soluble delayed tack adhesive applied is preferably 1.5 to 15 g / m 2 and more preferably 3 to 8 g / m 2 The coating amount is 1.5g / m 2 If the coating amount is more than 15g / m, sufficient adhesive strength can be obtained. 2 When the drying time is less than 10 minutes, the drying speed is increased, and therefore the productivity is improved.

[0058] Specific examples of the water-soluble delayed tack adhesive include a delayed tack agent (manufactured by Daicel Chemical Industries, Ltd., product name "KP011") and an acrylic pressure sensitive adhesive (manufactured by Toa Gosei Co., Ltd., product name "Arontack RP-275").

[0059] The thickness of the sealant layer 20 is not particularly limited and may be, for example, 1 μm or more, or 2 μm or more. However, from the viewpoint of ensuring sufficient seal strength of the packaging bag obtained by using the packaging laminate 100, the thickness of the sealant layer 20 is preferably 3 μm or more, and more preferably 5 μm or more. The thickness of the sealant layer 20 is not particularly limited, and may be 10 μm or less. However, the thickness of the sealant layer 20 is preferably 5 μm or less, and more preferably 3 μm or less. In this case, the sealant layer 20 becomes sufficiently thin, so that the sealant layer 20 can be easily peeled off in a short time when contacting with a water-containing liquid. In addition, the sealant layer 20 becomes sufficiently thin, so that flexibility can be imparted to the package.

[0060] The sealant layer 20 can be obtained by applying a heat-sensitive varnish to the surface of the base layer 10 and drying it (ie, removing the solvent from the heat-sensitive varnish) to form a heat-sensitive adhesive composition. The drying temperature is preferably lower than the adhesiveness developing temperature, for example, 40 to 60°C. Examples of methods for applying the heat-sensitive varnish include gravure coating, roll coating, reverse roll coating, lip coating, and knife coating.

[0061] (C) Printing layer The printed layer 30 is a layer formed using ink made of, for example, a urethane-based, acrylic-based, nitrocellulose-based, or rubber-based binder resin to which various pigments, plasticizers, drying agents, stabilizers, etc. are added. This printed layer 30 can display characters, pictures, etc.

[0062] 1, the printed layer 30 is provided between the base material layer 10 and the sealant layer 20, but the printed layer 30 may be provided not only between the base material layer 10 and the sealant layer 20, but also on the side of the base material layer 10 opposite the sealant layer 20 with respect to the resin film 11. Moreover, instead of being provided between the base material layer 10 and the sealant layer 20, the printed layer 30 may be provided on the side of the base material layer 10 opposite the sealant layer 20 with respect to the resin film 11.

[0063] The printing layer 30 may be a layer that can be peeled off from the base layer 10 with a water-containing liquid, but it is preferable that the printing layer 30 is a layer that can be peeled off from the base layer 10 with a water-containing liquid. In this case, when the packaging laminate 100 is brought into contact with a water-containing liquid, not only the sealant layer 20 but also the printing layer 30 can be peeled off from the base layer 10, making it possible to obtain a high-quality recycled product with a high mono-material ratio. Examples of inks that can form a printing layer that can be peeled off from the base layer 10 with a water-containing liquid include organic solvent-based printing inks containing polyurethane resin as a binder resin described in JP 2022-182777 A.

[0064] The ink for forming the printed layer 30 may be either water-based ink or oil-based ink, but is preferably water-based ink. Water-based ink uses water or alcohol as a solvent, and therefore can further reduce the environmental load.

[0065] The ink may or may not be a biomass ink, but from the viewpoint of reducing the environmental impact, it is preferable that the ink is a biomass ink. Here, biomass ink refers to ink that contains ingredients obtained from biological resources (biomass) such as cotton, pulp, rice bran, vegetable oil, and angiosperm seeds.

[0066] As the printing method, for example, a known printing method such as offset printing, gravure printing, flexographic printing, silk screen printing, inkjet printing, etc. Also, by subjecting the surface of the base material layer 10 or the sealant layer 20 to a corona treatment or ozone treatment as a pretreatment in advance, the adhesion of the printing layer 30 to the base material layer 10 or the sealant layer 20 can be improved.

[0067] <Package> Next, an embodiment of the package of the present disclosure will be described with reference to Fig. 2 and Fig. 3. Fig. 2 is a front view showing one embodiment of the package of the present disclosure, and Fig. 3 is a cross-sectional view taken along line III-III in Fig. 2.

[0068] As shown in Figs. 2 and 3, the packaging body 300 includes a packaging bag 200 and an item C to be packaged that is accommodated in the packaging bag 200. The packaging bag 200 is formed using a pair of packaging laminates 100. Here, the sealant layer 20 of the packaging laminate 100 faces inward, and the base layer 10 faces outward. The packaging bag 200 is composed of a storage section 302 that stores the item C to be packaged, and a heat-sealed section 301 provided around the storage section 302. The heat-sealed section 301 is a section formed by bonding the sealant layers 20 of opposing packaging laminates 100 together, and the storage section 302 is a section in which the sealant layers 20 of opposing packaging laminates 100 are not bonded together.

[0069] According to the packaging body 300, when the remaining packaging bag 200 is brought into contact with a water-containing liquid after the packaged item C is discharged, the sealant layer 20 can be easily peeled off from the base material layer 10 by the water-containing liquid. Therefore, according to the packaging body 300, it is possible to obtain a high-quality recycled product with a high mono-material ratio. The packaging body 300 is obtained by using the packaging laminate 100 and heat-bonding the portions to be heat-bonded at the periphery of the packaging laminate 100 at a temperature lower than the melting point of the resin film 11. The packaging laminate 100 has excellent bag-making suitability and can impart sufficient seal strength to the packaging body 300. This allows the packaging body 300 to be in a state suitable for use as a packaging body and to have sufficient seal strength.

[0070] (Packaged item) The packaged item C is not particularly limited and may be appropriately selected depending on the application. A package (primary package) made by packaging a solid with a low moisture content (for example, a solid with a moisture content of 20% by mass or less), a solid with a high moisture content (for example, a solid with a moisture content of more than 70% by mass), or a liquid in a packaging bag can be used as the packaged item C. When the packaged item C is a primary package, the package 300 is a secondary package. Examples of solids with low moisture content include dried foods, rice crackers, cookies, chocolates, and other confectioneries. Examples of solids with a high water content include fruits and vegetables. An example of the liquid is jelly.

[0071] (packaging bag) It is not essential that the pair of packaging laminates 100 constituting the packaging bag 200 have the same layer structure, and they may have different layer structures.

[0072] The packaging bag 200 may have a half-cut line, and may further have an easy-open processed part at both ends or one end of the half-cut line. Examples of the easy-open processed part include a group of scars, and a V-shaped, U-shaped, or I-shaped notch.

[0073] In the heat-sealed portion 301 of the packaging bag 200, the sealant layers 20 of a pair of packaging laminates 100 may be directly bonded to each other by heat fusion (see FIG. 3), or may be bonded to each other by an adhesive.

[0074] (Manufacturing method of packaging body) Next, a method for producing a packaging body 300 using the packaging laminate 100 will be described.

[0075] First, a pair of packaging laminates 100 is prepared. Then, the sealant layers 20 of the pair of packaging laminates 100 are placed against each other and overlapped. Next, the portions to be heat-bonded on the periphery of the packaging laminate 100 are heated at a temperature lower than the melting point of the resin film 11 to heat-bond the sealant layers 20 together. Specifically, first, a part of the peripheral portion of the packaging laminate to be thermally bonded is bonded in a U-shape to form the thermally bonded portion 301, and the remaining portion of the thermally bonded portion is left as an unbonded portion. In this manner, the packaging bag 200 having an unbonded portion is obtained.

[0076] Next, the packaged item C is filled into the packaging bag 200 through the unbonded portion. Thereafter, the sealant layers 20 of the packaging laminate 100 are bonded together in the unbonded portion, so that the unbonded portion also becomes a thermally bonded portion 301. In this manner, a package 300 is obtained, which comprises the packaging bag 200 and the packaged item C contained therein.

[0077] Although the preferred embodiment of the present disclosure has been described above, the present disclosure is not limited to the above embodiment. For example, in the above embodiment, the packaging bag 200 is formed using a pair of packaging laminates 100, but the packaging bag may be manufactured by folding one packaging laminate 100 with the sealant layer 20 on the inside and bonding the overlapping peripheral portions together as a portion to be thermally bonded.

[0078] The outline of this disclosure is as follows. [1] A substrate layer including a resin film mainly made of a single resin, and a sealant layer; The packaging laminate, wherein the sealant layer is made of a heat-sensitive adhesive composition and is a layer that can be peeled off from the base layer by a water-containing liquid. [2] The packaging laminate according to [1], wherein the water-containing liquid contains hot water having a temperature of 60°C or higher or contains an alkaline component. [3] The packaging laminate described in [1] or [2], further comprising a printed layer between the base layer and the sealant layer, the printed layer being peelable from the base layer by a water-containing liquid. [4] The packaging laminate according to any one of [1] to [3], wherein the base material layer further comprises a gas barrier layer. [5] The packaging laminate according to any one of [1] to [4], wherein the resin film contains a polyolefin resin. [6] A packaging bag and an item to be packaged contained in the packaging bag; The packaging bag is obtained by using the packaging laminate according to any one of [1] to [5] and by heating and heat-bonding the portions to be heat-bonded in the peripheral portion of the packaging laminate at a temperature lower than the melting point of the resin film. [Explanation of symbols]

[0079] 100: packaging laminate, 10: base material layer, 20: sealant layer, 12: gas barrier layer, 200: packaging bag, 300: package, C: packaged item.

Claims

1. The adhesive tape includes a base layer including a resin film mainly made of a single resin, and a sealant layer, The packaging laminate, wherein the sealant layer is made of a heat-sensitive adhesive composition and is a layer that can be peeled off from the base layer by a water-containing liquid.

2. The packaging laminate according to claim 1 , wherein the water-containing liquid contains hot water having a temperature of 60° C. or higher, or contains an alkaline component.

3. The packaging laminate according to claim 1 , further comprising a printed layer between the base layer and the sealant layer, the printed layer being peelable from the base layer with a water-containing liquid.

4. The packaging laminate according to claim 1 , wherein the base layer further comprises a gas barrier layer.

5. The packaging laminate according to claim 1 , wherein the resin film comprises a polyolefin resin.

6. A packaging bag and an item to be packaged contained in the packaging bag, The packaging bag is obtained by using the packaging laminate according to any one of claims 1 to 5 and by heating and heat-bonding the portion to be heat-bonded in the peripheral portion of the packaging laminate at a temperature lower than the melting point of the resin film.

Citation Information

Patent Citations

  • Polyethylene laminate for packaging material and packaging material composed of laminate

    JP2019166810A