Semiconductor laser element

The semiconductor laser device addresses the challenge of high threshold current by employing a layer structure with an intermediate layer to alleviate strain and enhance carrier recombination, resulting in reduced threshold current and improved efficiency.

JP2024159900AActive Publication Date: 2024-11-08NICHIA CORP
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024139990
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-08
Estimated Expiration
2038-08-31

AI Technical Summary

Technical Problem

Semiconductor laser devices face challenges in reducing the threshold current, which is the current required for laser oscillation.

Method used

The semiconductor laser device incorporates a specific layer structure with a first and second nitride semiconductor layer, a single or multiple quantum well structure, and an intermediate layer with a larger lattice constant than the barrier layers but smaller than the well layer, where the well and second barrier layers are in contact or have a reduced distance, alleviating strain and enhancing carrier recombination.

Benefits of technology

This configuration reduces the threshold current and improves luminous efficiency, leading to better temperature characteristics and reduced probability of carrier overflow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024159900000001_ABST
    Figure 2024159900000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor laser element having a low threshold current.SOLUTION: Provided is a semiconductor laser element that comprises: a first nitride semiconductor layer of a first conductivity type; a second nitride semiconductor layer of a second conductivity type; and an active region arranged between the first nitride semiconductor layer and the second nitride semiconductor layer and that has a single quantum well structure or a multiquantum well structure. The active region has a first barrier layer, an intermediate layer, a well layer, and a second barrier layer sequentially from the first nitride semiconductor layer side. A lattice constant of the intermediate layer is larger than those of the first and second barrier layers and smaller than that of the well layer. A film thickness of the intermediate layer is thicker than that of the well layer. The well layer and the second barrier layer are contacted with each other, or alternatively, a distance between the well layer and the second barrier layer is smaller than that between the first barrier layer and the well layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor laser device. [Background technology]

[0002] Patent Documents 1 and 2 each describe a nitride semiconductor light-emitting device including an active region formed of a well layer, a barrier layer, and an intermediate layer disposed therebetween. The nitride semiconductor light-emitting device is, for example, a semiconductor laser device. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2004-356256 A [Patent Document 2] JP 2011-151275 A Summary of the Invention [Problem to be solved by the invention]

[0004] In semiconductor laser devices, there is a demand for further reduction in the threshold current, which is the current at which laser oscillation occurs. [Means for solving the problem]

[0005] This application includes the following inventions. a first conductivity type first nitride semiconductor layer; a second nitride semiconductor layer of a second conductivity type; a single quantum well disposed between the first nitride semiconductor layer and the second nitride semiconductor layer; and an active region having a multi-quantum well structure or a multi-quantum well structure, The active region includes, in order from the first nitride semiconductor layer side, a first barrier layer, an intermediate layer, and a well layer. a first barrier layer and a second barrier layer, The lattice constant of the intermediate layer is larger than the lattice constants of the first barrier layer and the second barrier layer. and smaller than the lattice constant of the well layer; the intermediate layer has a thickness greater than that of the well layer; The well layer and the second barrier layer are in contact with each other, or the well layer and the second barrier layer are in contact with each other. the distance between the first barrier layer and the well layer is smaller than the distance between the first barrier layer and the well layer. Effect of the Invention

[0006] With such a configuration, the threshold current of the semiconductor laser element can be reduced. [Brief description of the drawings]

[0007] [Figure 1] 1 is a schematic cross-sectional view of a semiconductor laser device according to one embodiment of the present invention. [Diagram 2] FIG. 2 is a diagram illustrating the band gap energy of an active region of a semiconductor laser device according to one embodiment of the present invention. [Diagram 3] 1 is a schematic top view of a semiconductor laser device according to an embodiment of the present invention; [Figure 4] FIG. 1 is a diagram illustrating a first modified example of an active region. [Diagram 5] FIG. 13 is a diagram illustrating a second modified example of an active region. [Figure 6] FIG. 13 is a diagram illustrating a third modified example of an active region. [Figure 7] 1 is a graph showing threshold current densities of the semiconductor laser devices of Examples 1 to 4 and Comparative Examples 1 and 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. However, the embodiment shown below is merely an example of a method for realizing the technical idea of ​​the present invention, and the present invention is not limited to the following embodiment. Furthermore, in the following description, the same names and symbols indicate the same or similar components, and detailed description will be omitted as appropriate.

[0009] (Semiconductor laser element 100) FIG. 1 is a schematic cross-sectional view of a semiconductor laser device 100 according to an embodiment of the present invention, showing a cross section in a direction perpendicular to the resonator direction of the semiconductor laser device 100. The semiconductor laser device 100 has a first nitride semiconductor layer of a first conductivity type (third n-type semiconductor layer 23), a second nitride semiconductor layer of a second conductivity type (second p-type semiconductor layer 43), and an active region 3 disposed between the first nitride semiconductor layer and the second nitride semiconductor layer. More specifically, the semiconductor laser device 100 has an n-side region 2 having an n-type nitride semiconductor layer, an active region 3, and a p-side region 4 having a p-type nitride semiconductor layer provided in this order on a substrate 1. A ridge 4a is provided on the surface of the p-side region 4. The portion of the active region 3 directly below the ridge 4a and its vicinity is a waveguide region. An insulating film 5 is provided on the surface of the p-side region 4 that is continuous with the upper surface of the ridge 4a and the side surface of the ridge 4a. The substrate 1 is of n-type, and an n-electrode 8 is provided on its lower surface. Furthermore, a p-electrode 6 is provided in contact with the ridge 4a on the surface of the p-side region 4, and a p-side pad electrode 7 is further provided thereon.

[0010] (Substrate 1) The substrate 1 may be a nitride semiconductor substrate made of, for example, GaN or AlN. Substrates other than nitride semiconductor substrates may also be used. Examples of such substrates include insulating substrates such as sapphire, semiconductor substrates such as SiC, Si, ZnO, Ga2O3, and GaAs, and template substrates in which a nitride semiconductor is grown on glass. The piezoelectric field described below is particularly likely to occur when the substrate 1 is used as a growth substrate and the growth direction of the semiconductor layer grown thereon is the +c axis. Therefore, when the substrate 1 is a growth substrate, it is preferable to use a GaN substrate having a +c plane as the main surface or a sapphire substrate having a c plane as the main surface for the substrate 1 so that the nitride semiconductor grows along the +c axis. Here, the +c plane or the c plane as the main surface may include those having an off angle of 1 degree or less in addition to those strictly speaking being these planes. Furthermore, it is preferable to use a GaN substrate rather than a sapphire substrate because it is possible to reduce the dislocation density of the nitride semiconductor layer grown thereon and it is considered easy to provide the intermediate layer 32 described below as a thick film.

[0011] (n side area 2) The n-side region 2 can be formed of a single layer or a multilayer structure made of a nitride semiconductor. An example of an n-type semiconductor layer included in the n-side region 2 is a layer made of a nitride semiconductor containing n-type impurities such as Si or Ge. The n-side region 2 has, for example, a first n-type semiconductor layer 21, a second n-type semiconductor layer 22, a third n-type semiconductor layer 23 (n-type nitride semiconductor layer), and a fourth n-type semiconductor layer 24, in that order from the substrate 1 side. Layers other than these may be arranged in the n-side region 2, and some layers may be omitted.

[0012] The first to fourth n-type semiconductor layers 21 to 24 contain n-type impurities. The first n-type semiconductor layer 21 is made of, for example, AlGaN. The second n-type semiconductor layer 22 is made of, for example, InGaN. The third n-type semiconductor layer (n-type nitride semiconductor layer) 23 is made of, for example, AlGaN having a larger band gap energy than the first n-type semiconductor layer 21. x Ga 1-xN (0≦x<1). The third n-type semiconductor layer 23 may have the maximum band gap energy in the n-side region 2. The third n-type semiconductor layer 23 can function as an n-side cladding layer (first cladding layer). The film thickness of the third n-type semiconductor layer 23 is, for example, about 0.7 to 1.2 μm. The fourth n-type semiconductor layer 24 is, for example, made of GaN. The film thickness of the fourth n-type semiconductor layer 24 is, for example, smaller than the film thickness of the third n-type semiconductor layer 23.

[0013] The n-side compositionally graded layer 25 is a layer whose composition gradually changes, for example, with GaN on the substrate 1 side and InGaN on the active region 3 side. The thickness of the n-side compositionally graded layer 25 can be 50 nm to 500 nm. The n-side compositionally graded layer 25 preferably contains an n-type impurity. Since the compositionally graded layer has a laminated structure of layers whose compositions change gradually, negative fixed charges are generated at the heterointerface in the laminated structure, and the band spike caused by this acts as a carrier injection barrier. By containing an n-type impurity in the n-side compositionally graded layer 25, the band spike can be alleviated.

[0014] The third n-type semiconductor layer 23, the fourth n-type semiconductor layer 24, and the n-side compositionally graded layer 25 preferably have a relationship in which the lattice constant gradually increases from the third n-type semiconductor layer 23 toward the well layer 33. This can alleviate the strain on the well layer 33 and reduce the influence of the piezoelectric field. Examples of layers that function as the n-side light guide layer (first light guide layer) include the fourth n-type semiconductor layer 24 and / or the n-side compositionally graded layer 25. The fourth n-type semiconductor layer 24 may be omitted. When the film thickness of a barrier layer in the active region 3 described later is thin, the n-side compositionally graded layer 25 may also function as a barrier layer.

[0015] (active area 3) The active region 3 has a single quantum well structure or a multiple quantum well structure. FIG. 2 is a diagram showing the band gap energy of the active region 3 of the semiconductor laser element 100. The active region 3 shown in FIG. 2 has a single quantum well structure. As shown in FIG. 2, the active region 3 can have, in order from the first nitride semiconductor layer side, a first barrier layer 31, an intermediate layer 32, a well layer 33, and a second barrier layer 34. Layers other than these may be disposed in the active region 3, and some layers may be omitted. The lattice constant of the intermediate layer 32 is larger than the lattice constants of the first barrier layer 31 and the second barrier layer 34, and smaller than the lattice constant of the well layer 33. The film thickness of the intermediate layer 32 is thicker than the film thickness of the well layer 33. In FIG. 2, the well layer 33 and the second barrier layer 34 are in contact with each other. Another layer may be disposed between the well layer 33 and the second barrier layer 34. In this case, the other layer is disposed so that the distance between the well layer 33 and the second barrier layer 34 is smaller than the distance between the first barrier layer 31 and the well layer 33.

[0016] For example, InGaN is used as the well layer 33 in the active region 3. For example, AlGaN and GaN are used as the third n-type semiconductor layer 23 and the second p-type semiconductor layer 43 sandwiching the active region 3. As semiconductor layers with different lattice constants are stacked in this way, the active region 3, particularly the well layer 33, is subjected to, for example, compressive strain. The strain applied to the well layer 33 generates a piezoelectric field. The generation of the piezoelectric field spatially separates the wave function of holes and the wave function of electrons, decreasing the probability of carrier recombination. This reduces the light emission efficiency of the semiconductor laser element and increases the threshold current for the semiconductor laser element to oscillate.

[0017] Therefore, in this embodiment, the intermediate layer 32 is provided. By providing the intermediate layer 32 having a lattice constant between the first barrier layer 31 and the well layer 33, the strain applied to the well layer 33 can be alleviated. In addition, by providing the intermediate layer 32, the peak of the wave function of the second conductive type carriers (e.g., holes) can be brought closer to the first barrier layer 31. As a result, the recombination probability of the carriers can be increased. Therefore, the light emission efficiency of the semiconductor laser device 100 can be increased and the threshold current can be reduced. If the intermediate layer 32 is too thin, the effect of bringing the peak of the wave function closer to the first barrier layer 31 is weakened, so it is preferable that the film thickness of the intermediate layer 32 is thicker than the film thickness of the well layer 33. In addition, the threshold current increases as the threshold current density increases, and it is considered that the higher the threshold current density, the higher the probability that carriers will overflow from the active region 3. By reducing the threshold current, the probability of overflow can be reduced, and thus the temperature characteristic of the optical output can be improved. In this specification, the temperature characteristic of the optical output refers to the ratio of the optical output at a high temperature to the optical output at normal temperature.

[0018] The well layer 33 and the second barrier layer 34 are in contact with each other, or if not, the distance between the well layer 33 and the second barrier layer 34 is preferably smaller than the distance between the first barrier layer 31 and the well layer 33. If a layer such as the intermediate layer 32 is provided between the second barrier layer 34 and the well layer 33, the peak of the wave function of the first conductive type carrier (electrons) approaches the second barrier layer 34 side, and the peak of the wave function of the second conductive type carrier (holes) approaches the first barrier layer 31 side. This reduces the spatial overlap of the wave functions, resulting in a decrease in luminous efficiency. Therefore, the above-mentioned configuration is preferable. Furthermore, if another layer is provided between the well layer 33 and the second barrier layer 34, it is preferable that the film thickness of the other layer is thin enough that it does not function as the intermediate layer 32. Specifically, it is preferable that the distance between the well layer 33 and the second barrier layer 34 is smaller than the film thickness of the well layer 33. Furthermore, another layer provided between the well layer 33 and the second barrier layer 34 is a layer having a lattice constant and band gap energy between those of the well layer 33 and the second barrier layer 34 .

[0019] Each layer constituting the active region 3 is preferably made of a binary or ternary compound semiconductor such as GaN or InGaN. If a quaternary compound semiconductor such as AlInGaN is used, a laminate structure with a large band gap energy difference but a small lattice constant difference can be formed by adjusting the composition ratio. However, it is easier to manufacture a composition ratio closer to the design value with a binary or ternary compound semiconductor than with a quaternary compound semiconductor. For this reason, it is preferable that the active region 3 is made of a binary or ternary compound semiconductor. In this case, the lattice constant difference between the layers is likely to be large, so it is more preferable to provide an intermediate layer 32 capable of relaxing distortion.

[0020] When the active region 3 has a multiple quantum well structure, as shown in FIG. 4, a plurality of well layers 33 are arranged, and an intermediate barrier layer 37 is arranged between them. In this case, the active region 3 may have a relationship between all well layers 33 and the layers sandwiching them, such as the first barrier layer 31, intermediate layer 32, well layer 33, and second barrier layer 34 shown in FIG. 2. The intermediate layer 32 may or may not be a compositionally graded layer. The active region 3 shown in FIG. 2 has a single quantum well structure. With a single quantum well structure, the light emitted from the well layer 33 is not absorbed by another well layer, so that the light loss can be reduced, and the number of barrier layers 31 is small, so that the crystallinity of the layer (for example, the layer of the p-side region 4) grown next to the active region 3 can be improved. On the other hand, the single quantum well structure may have a lower optical confinement coefficient than the multiple quantum well structure, which increases the threshold current in this case, but the intermediate layer 32 can be provided to reduce the threshold current. Furthermore, in the case of a multiple quantum well structure, multiple intermediate layers 32 are provided, and increasing the thickness of each intermediate layer 32 may lead to a concern of deteriorating the crystallinity of the well layer 33. For this reason, a single quantum well structure may be more likely to achieve the effect of reducing the threshold current by increasing the thickness of the intermediate layer 32.

[0021] (First barrier layer 31) The first barrier layer 31 is made of a material having a larger band gap energy than the well layer 33, and may be, for example, InGaN, GaN, or AlGaN. When the In composition ratio of the well layer 33 is relatively large, such as when the oscillation wavelength is 430 nm or more, the In composition ratio is set to 0.1 to 0.25 μm so that the difference in lattice constant between the well layer 33 and the first barrier layer 31 is not too large. a Ga 1-a N (0≦a<1) is preferable. The first barrier layer 31 is preferably made of GaN to improve the crystallinity of the well layer 33. The thickness of the first barrier layer 31 may be one atomic layer or more and may be 20 nm or less.

[0022] (Middle class 32) It is considered that the thicker the intermediate layer 32 is, the greater the effect of relaxing the distortion of the well layer 33. For this reason, it is more preferable that the thickness of the intermediate layer 32 is 1.5 times or more the thickness of the well layer 33. As shown in FIG. 7 described later, when the thickness of the intermediate layer 32 is in a range less than the thickness of the well layer 33, the degree of change in the threshold current density due to the increase in thickness is large, and when the thickness of the intermediate layer 32 is in a range greater than the thickness of the well layer 33, the degree of change in the threshold current density tends to be gentle. In order to stabilize the quality of the semiconductor laser device 100 obtained, it is considered preferable to adopt a thickness in a range in which the degree of change in the threshold current density is gentle. For this reason, it is preferable that the thickness of the intermediate layer 32 is 1.5 times or more the thickness of the well layer 33. Also, from FIG. 7, it can be said that the thickness of the intermediate layer 32 is preferably 3 nm or more. On the other hand, it is considered that the probability of overflow of carriers (e.g., holes) increases as the thickness increases. For this reason, it is preferable that the thickness of the intermediate layer 32 is less than 6 times the thickness of the well layer 33, and more preferably 3 times or less. Also, from FIG. 7, it can be seen that the thickness of the intermediate layer 32 is preferably less than 13 nm, and more preferably 6 nm or less.

[0023] The intermediate layer 32 may be made of a material having a lattice constant between that of the first barrier layer 31 and the well layer 33. Such a material may be an In-type material having a higher In composition ratio than the first barrier layer 31 and a lower In composition ratio than the well layer 33. b Ga 1-bN (a < b < 1) can be cited. When the first barrier layer 31 is GaN, its In composition ratio is 0%. When the intermediate layer 32 is In b Ga 1-b N, the closer the In composition ratio b of the intermediate layer 32 is to the well layer 33, the greater the effect of relaxing the strain on the well layer 33, but the probability of carrier overflow is considered to increase. Therefore, the In composition ratio b of the intermediate layer 32 is preferably set to be equal to or less than half of the sum of the In composition ratio c of the well layer 33 and the In composition ratio a of the first barrier layer 31. The In composition ratio b of the intermediate layer 32 may be set to be equal to or less than half of the In composition ratio c of the well layer 33. The In composition ratio b of the intermediate layer 32 can be, for example, 5 to 15%. In FIG. 2, the intermediate layer 32 is in contact with the first barrier layer 31.

[0024] The intermediate layer 32 is preferably disposed between the well layer 33 and the n-side region 2. This is because holes are more difficult to move than electrons in a nitride semiconductor. By disposing the intermediate layer 32 on the side of the n-side region 2 of the well layer 33, the strain applied to the well layer 33 can be efficiently relaxed, and the carrier recombination probability can be increased. Further, when a nitride semiconductor is used as each semiconductor layer, there is a tendency to grow in the order of the n-side region 2, the active region 3, and the p-side region 4, and growing the intermediate layer 32 before growing the well layer 33 is considered to be advantageous for relaxing the strain of the well layer 33.

[0025] The intermediate layer 32 may be undoped, but may contain an impurity of the first conductivity type (for example, an n-type impurity). By containing an impurity of the first conductivity type, the probability of carrier (for example, hole) overflow can be reduced. Further, when the intermediate layer 32 contains an impurity instead of being undoped, the crystallinity tends to deteriorate as the film thickness increases. Therefore, when the intermediate layer 32 contains an impurity, it is particularly preferable that the film thickness is less than 13 nm as described above. As the n-type impurity and the p-type impurity, the same materials as those cited in the n-side region 2 and the p-side region 4 can be used. For example, when an n-type impurity is contained, the electron carrier concentration is preferably 1×10 18 cm 3 or more, and more preferably 1×10 19 cm3 More than 1×10 20 cm 3 Less than or equal to 6×10 is preferable. 19 cm 3 By setting the range as described above, it is possible to more efficiently reduce the probability of hole overflow.

[0026] 5, the intermediate layer 32 may be a compositionally graded layer. The intermediate layer 32 has a lattice constant that increases from the first barrier layer 31 to the well layer 33 (In b Ga 1-b It is believed that forming a compositionally graded layer (in the case of N, the In composition ratio b increases) enhances the effect of relaxing strain in the well layer 33. In FIG. 4, the In composition ratio b of the portion of the intermediate layer 32 closest to the first barrier layer 31 is greater than the In composition ratio a (0%) of the first barrier layer 31, but it may be the same as that of the first barrier layer 31.

[0027] In this specification, the term "compositionally graded layer" refers to a multilayer structure in which a plurality of layers are stacked, and the layer as a whole has a compositional gradient. For example, In X Ga 1-X In the case of a composition gradient layer consisting of N (0≦X<1), each of the layers constituting the layer has a thickness of 25 nm or less and a difference in In composition ratio with adjacent layers of 0.5% or less. Furthermore, the thickness of each layer is preferably 20 nm or less. The lower limit of the thickness of each layer is, for example, one atomic layer. The difference in In composition ratio with adjacent layers is preferably 0.1% or less. The lower limit is, for example, about 0.007%. By setting the thickness in such a range, it is possible to reduce distortion occurring in the composition gradient layer. In addition, when comparing the In composition ratio or lattice constant of the composition gradient layer with those of other layers, the average value of the composition gradient layer is used. For example, in the case of a composition gradient layer in which the In composition ratio gradually changes from 7% to 10%, the average value of 8.5% is used as the In composition ratio of the composition gradient layer to compare the magnitude relationship with other layers.

[0028] Since the intermediate layer 32 is adjacent to the well layer 33, it can also be considered to serve as the core layer of the core-clad structure. Therefore, it can be expected that the optical confinement factor will be improved by providing the intermediate layer 32. If the optical confinement factor is improved, the luminous efficiency will be improved and the threshold current can be reduced.

[0029] (Well layer 33) The well layer 33 can be In c Ga 1-c N (b < c < 1). The In composition ratio c of the well layer 33 can be, for example, 17% or more. As the oscillation wavelength of the semiconductor laser element 100 becomes longer, the In composition ratio c of the well layer 33 becomes larger, and the lattice constant difference from the layer outside the active region 3 becomes larger. For this reason, it becomes more likely to be significantly affected by the piezoelectric field. Therefore, it is particularly preferable to provide the intermediate layer 32 when the oscillation wavelength of the semiconductor laser element 100 is 430 nm or more. When the semiconductor laser element has an oscillation wavelength of 430 nm or more, the In composition ratio c of the well layer 33 increases or decreases somewhat depending on the overall layer structure, but is, for example, 10% or more. The In composition ratio c of the well layer 33 can be, for example, 50% or less. At this time, the oscillation wavelength of the semiconductor laser element is considered to be about 600 nm or less. The film thickness of the well layer 33 can be, for example, 2 to 4 nm. The well layer 33 is preferably undoped from the viewpoints of improving crystallinity and reducing light absorption.

[0030] (Second barrier layer 34) The second barrier layer 34 has a larger bandgap energy than the well layer 33. The second barrier layer 34 is, for example, In d Ga 1-d N (0 ≦ d < b). The composition and film thickness range of the second barrier layer 34 can be the same as those of the first barrier layer 31 described above. If the second barrier layer 34 contains an n-type impurity, there is a risk of light absorption and hole trapping. Also, since Mg, which is a p-type impurity, causes light absorption, the second barrier layer 34 is preferably undoped. For example, the second barrier layer 34 is made of undoped GaN.

[0031] (Other layers) In FIG. 2, the first barrier layer 31 is disposed at the outermost position of the active region 3, i.e., the position closest to the n-side region 2, but another layer may be disposed on the n-side region 2 side of the first barrier layer 31. For example, as shown in FIG. 6, the thickness of the first barrier layer 31 may be set to 5 nm or less, and an InGaN layer 35 having a larger lattice constant and a larger thickness than the first barrier layer 31 may be disposed on the n-side region 2 side of the first barrier layer 31. By providing such an InGaN layer 35, it is possible to relax the strain in the well layer 33. The thickness of this InGaN layer 35 may be set to 30 nm or less. When the InGaN layer 35 is provided, a GaN layer 36 may be further provided on the substrate 1 side. The thickness of the GaN layer 36 may be set to 5 nm or less. As will be described later, it is preferable to dispose the intermediate layer 32 between the well layer 33 and the n-side region 2, and therefore it is preferable to dispose the first barrier layer 31 between the well layer 33 and the n-side region 2. In order for the first barrier layer 31 to function as a barrier layer in the quantum well structure, it is preferable that the first barrier layer 31 be located in the vicinity of the well layer 33. For example, the first barrier layer 31 is preferably located at a position that is 20 nm or less away from the well layer 33.

[0032] In FIG. 2, the well layer 33 and the intermediate layer 32 are in contact with each other, but a thin film layer (first thin film layer) may be provided between the well layer 33 and the intermediate layer 32. In order to obtain the effect of the intermediate layer 32, it is preferable to place the intermediate layer 32 close to the well layer 33, so the first thin film layer is provided with a thickness that does not inhibit the effect of the intermediate layer 32. For example, the thickness of the first thin film layer can be equal to or less than the thickness of the well layer 33, and can be 2 nm or less. In other words, the distance between the well layer 33 and the intermediate layer 32 can be equal to or less than the thickness of the well layer 33, and can be 2 nm or less. The first thin film layer may be a compositionally graded layer having a composition in which the lattice constant increases from the intermediate layer 32 toward the well layer 33. This can relieve the strain applied to the well layer 33. The first thin film layer does not have to be a compositionally graded layer. In this case, it can be provided as a layer having a lattice constant and band gap energy between the intermediate layer 32 and the well layer 33.

[0033] 2, the second barrier layer 34 is in contact with the well layer 33, but a thin film layer (second thin film layer) may be provided between the second barrier layer 34 and the well layer 33. The second thin film layer may be a layer having a lattice constant and band gap energy between the second barrier layer 34 and the well layer 33. The second thin film layer is preferably thick enough not to have a function like the intermediate layer 32. The thickness of the second thin film layer may be less than the thickness of the well layer 33. The thickness of the second thin film layer may be, for example, 2 nm or less.

[0034] (p side region 4) The p-side region 4 can be formed in a single layer or multilayer structure made of a nitride semiconductor layer. An example of the p-type nitride semiconductor layer included in the p-side region 4 is a layer made of a nitride semiconductor containing p-type impurities such as Mg. The p-side region 4 has, for example, a p-side compositionally graded layer 41, a first p-type semiconductor layer 42, a second p-type semiconductor layer 43 (p-type nitride semiconductor layer), and a third p-type semiconductor layer 44, in this order from the active region 3 side. Layers other than these may be disposed in the p-side region 4, and some layers may be omitted. The semiconductor laser element 100 is provided with a ridge 4a, and the portion of the active region 3 directly below the ridge 4a and its vicinity is a waveguide region. The ridge 4a may not be formed.

[0035] The p-side compositionally graded layer 41 is a layer in which the composition gradually changes, for example, with the active region 3 side being InGaN and the first p-type semiconductor layer 42 side being GaN. For the same reason as the second barrier layer 34, the p-side compositionally graded layer 41 is preferably undoped. The thickness of the p-side compositionally graded layer 41 can be 50 nm to 500 nm. The p-side compositionally graded layer 41 preferably does not have a band offset of approximately 0.004 eV / nm or more over the entire region except for the interface on the active region 3 side of the p-side compositionally graded layer 41 and the interface on the first p-type semiconductor layer 42 side. If a steep band offset exists, holes may be trapped, but if it is within such a range, the probability of holes being trapped can be reduced. When the p-side compositionally graded layer 41 is (In)GaN, it is preferable that there is no steep composition ratio change of 0.1% / nm or more when converted to the In composition ratio of InGaN. When the thickness of the barrier layer in the active region 3 is thin, the p-side compositionally graded layer 41 may also function as a barrier layer.

[0036] The first to third p-type semiconductor layers 42 to 44 contain p-type impurities. The first p-type semiconductor layer 42 is made of, for example, AlGaN. The first p-type semiconductor layer 42 functions as, for example, an electron block layer. The first p-type semiconductor layer 42 may be provided as a layer having the highest band gap energy in the p-side region 4 and having a smaller film thickness than the p-side compositionally graded layer 41. The second p-type semiconductor layer 43 (this layer is a p-type nitride semiconductor layer in this embodiment) is made of, for example, AlGaN. The second p-type semiconductor layer 43 may have the second highest band gap energy in the p-side region 4 after the electron block layer. An undoped or second p-type semiconductor layer 43 may be disposed between the first p-type semiconductor layer 42 and the second p-type semiconductor layer 43. The undoped layer and the second p-type semiconductor layer 43 may have a larger thickness than each other, but the undoped layer and the second p-type semiconductor layer 43 may have the same thickness in order to reduce light absorption in the p-side region 4. The undoped layer and the second p-type semiconductor layer 43 are layers of the same composition, for example. The third p-type semiconductor layer 44 is made of, for example, GaN and functions as a p-type contact layer. Examples of layers that function as a p-side light guide layer (second light guide layer) include the p-side composition gradient layer 41 and / or the p-type semiconductor layer 43. The second p-type semiconductor layer 43 may be a layer that functions as a p-side cladding layer (second cladding layer), but when a material having the function of a cladding layer, such as ITO, is used as the p-electrode 6 described later, the p-electrode 6 may be a cladding layer, and a cladding layer may not be provided in the p-side region 4.

[0037] (Other materials) The semiconductor laser element 100 may have an insulating film 5 provided on a part of the surface of the p-side region 4. The insulating film 5 may be formed of a single layer film or a multilayer film of an oxide or nitride of, for example, Si, Al, Zr, Ti, Nb, Ta, or the like. The insulating film 5 may have a thickness of about 10 to 500 nm. The p-electrode 6 is provided on, for example, the upper surface of the ridge 4a. The p-side pad electrode 7 is provided in contact with the p-electrode 6. The p-side pad electrode 7 has a larger area than the p-electrode 6, and a wire or the like is connected to the p-side pad electrode 7. The n-electrode 8 is provided on, for example, almost the entire lower surface of the n-type substrate 1. Examples of materials for each electrode include a single layer film or a multilayer film of a conductive oxide containing at least one selected from metals or alloys such as Ni, Rh, Cr, Au, W, Pt, Ti, and Al, Zn, In, and Sn. Examples of conductive oxides include ITO (indium tin oxide), IZO (indium zinc oxide), and GZO (gallium-doped zinc oxide). The thickness of each electrode is, for example, about 0.1 to 2 μm. In this specification, the side where the p-side region 4 is located from the active region 3 is defined as the upper side, and the side where the n-side region 2 is located is defined as the lower side. The upper surface and the lower surface refer to the surfaces in this vertical direction.

[0038] FIG. 3 shows a schematic top view of the semiconductor laser element 100. As shown in FIG. 3, it is preferable to provide the p-electrode 6 at a position separated from the light-emitting end face and the light-reflecting end face. This can reduce current concentration at and near each end face. In addition, it is preferable to provide each electrode such that the distance from the light-emitting end face and the light-reflecting end face is smaller than that of the p-electrode 6 when viewed from above. This allows the p-side pad electrode 7 to dissipate heat generated at and near the light-emitting end face and the light-reflecting end face. These configurations can reduce the probability of the semiconductor laser element 100 suddenly dying. Since the light-emitting end face is more likely to generate heat than the light-reflecting end face, it is preferable to provide the p-electrode 6 at a greater distance from the light-emitting end face than from the light-reflecting end face.

[0039] 1 and 3, the insulating film 5 may cover a part of the p-electrode 6. The insulating film 5 has an opening 5a, and the p-electrode 6 is connected to the p-side pad electrode 7 through the opening 5a. With this configuration, the current injected from the p-side pad electrode 7 is blocked by the insulating film 5. Therefore, the current injection region can be adjusted by adjusting the coverage region of the insulating film 5. As shown in FIG. 3, by making the coverage region on the light-emitting end face side larger than the coverage region on the light-reflecting end face side, the amount of current injection on the light-emitting end face side can be reduced, and heat generation on the light-reflecting end face side can be reduced. In addition, since the end of the p-electrode 6 is located closer to the light-reflecting end face than the end of the light injection region, heat dissipation by the p-electrode 6 can be expected. A reflective film such as a dielectric multilayer film may be formed on the light-emitting end face and the light-reflecting end face. The width of the p-electrode 6 may be the same as the width of the upper surface of the ridge 4a.

[0040] [Example 1] As Example 1, the following semiconductor laser device was fabricated.

[0041] An n-side region 2 was grown on a GaN substrate (substrate 1) having a +c-plane as a principal surface. The n-side region 2 has the following layers, in this order from the GaN substrate side. 1.5μm thick Si-doped Al 0.02 Ga 0.98 N layer (first n-type semiconductor layer 21), 150 nm thick Si-doped In 0.05 Ga 0.95 N layer (second n-type semiconductor layer 22), 1μm thick Si-doped Al 0.07 Ga 0.93 N layer (third n-type semiconductor layer 23), a 300 nm-thick Si-doped GaN layer (fourth n-type semiconductor layer 24); A Si-doped compositionally graded layer (n-side compositionally graded layer 25) having a thickness of 250 nm. The n-side compositionally graded layer 25 has a growth starting point of GaN and a growth ending point of In. 0.05 Ga 0.95 N was grown by increasing the In composition substantially monotonically so that the composition gradient was nearly linear. Next, the active region 3 was grown. The active region 3 had the following layers, in this order from the n-side region 2 side. A 1 nm thick Si-doped GaN layer, An 8-nm-thick Si-doped InGaN layer, a 1 nm thick Si-doped GaN layer (first barrier layer 31); An undoped InGaN compositionally graded layer (intermediate layer 32) having a thickness of 3 nm; Undoped In with a thickness of 2.25 nm 0.2 Ga 0.8 N layer (well layer 33), An undoped GaN layer (second barrier layer 34) having a thickness of 1 nm. The intermediate layer 32 begins its growth at In 0.07 Ga 0.93 N, and the end of growth is In 0.1 Ga 0.9 N was grown by increasing the In composition substantially monotonically so that the composition gradient was nearly linear. Next, the p-side region 4 was grown. The p-side region 4 had the following layers, in this order from the active region 3 side. An undoped compositionally graded layer (p-side compositionally graded layer 41) having a thickness of 250 nm, a 10-nm-thick Mg-doped AlGaN layer having a high Al composition ratio (first p-type semiconductor layer 42); a 300-nm-thick AlGaN layer (second p-type semiconductor layer 43) partially doped with Mg and having a low Al composition ratio; Finally, a 15 nm thick Mg-doped GaN layer (third p-type semiconductor layer 44). The p-side compositionally graded layer 41 begins its growth at In. 0.05 Ga 0.95 The growth was performed with the In composition substantially monotonically decreasing so that the composition gradient was nearly linear, with the growth terminal being GaN and the growth terminus being GaN.

[0042] The epitaxial wafer on which the above layers were formed was then removed from the MOCVD furnace, and a ridge, an n-electrode, a p-electrode, etc. were formed, followed by singulation to obtain semiconductor laser elements. The semiconductor laser elements had a ridge width of 45 μm and a cavity length of 1200 μm.

[0043] [Examples 2 to 4] In Examples 2 to 4, semiconductor laser devices were fabricated in the same manner as in Example 1, except that the thickness of the intermediate layer 32 was different. In Example 2, the thickness of the intermediate layer 32 was 4 nm, in Example 3, the thickness of the intermediate layer 32 was 6.5 nm, and in Example 4, the thickness of the intermediate layer 32 was 13 nm. The intermediate layer 32 in Examples 2 to 4 was a compositionally graded layer like the intermediate layer 32 in Example 1, and the composition at the growth start point and the composition at the growth end point were the same as in Example 1.

[0044] [Comparative Example 1] As Comparative Example 1, a semiconductor laser device was fabricated in the same manner as in Example 1, except that the intermediate layer 32 was not provided.

[0045] [Comparative Example 2] As Comparative Example 2, a semiconductor laser device was fabricated in the same manner as in Example 1, except for the difference in the thickness of the intermediate layer 32. In Comparative Example 2, the thickness of the intermediate layer 32 was set to 1 nm.

[0046] (threshold current density, relative light output) A plurality of semiconductor laser elements of Examples 1 to 4 and Comparative Examples 1 and 2 were produced under the same conditions. Then, the threshold current density and the relative optical output were measured, and the median values ​​in each Example and Comparative Example were taken as the threshold current density and the relative optical output of each Example and Comparative Example. In each Example and Comparative Example, the median oscillation wavelength of the semiconductor laser element was about 455 nm. The relative optical output here refers to the value obtained by dividing the optical output measured at an environmental temperature of 80°C by the optical output measured at an environmental temperature of 25°C. It can be said that the larger the value of the relative optical output, the better the optical output temperature characteristic.

[0047] FIG. 7 shows the threshold current density of the semiconductor laser elements of Examples 1 to 4 and Comparative Examples 1 and 2. It can be said that the threshold current is lower as the threshold current density is smaller. From the results shown in FIG. 7, it was found that the threshold current density is reduced by providing an intermediate layer. As shown in FIG. 7, the threshold current density decreases rapidly until the thickness of the intermediate layer becomes approximately the same as the thickness of the well layer, and decreases gradually at thicknesses greater than that. From these results, it can be said that a semiconductor laser element with a low threshold current can be stably obtained by making the thickness of the intermediate layer thicker than the thickness of the well layer. On the other hand, when the thickness of the intermediate layer was increased to 13 nm, the threshold current density became a slightly higher value. This is considered to be because the probability of holes overflowing increased as the intermediate layer became thicker.

[0048] In addition, the relative light output was 70% for Comparative Example 1 (0 nm), 72% for Comparative Example 2 (1 nm), 74% for Example 1 (3 nm), 74% for Example 2 (4 nm), 72% for Example 3 (6.5 nm), and 69% for Example 4 (13 nm). These values ​​are rounded off to the nearest whole number. Thus, the relative light output generally increased by providing the intermediate layer, but when the film thickness was 13 nm, the value was lower than when the intermediate layer was not provided. This is because the lower the threshold current density, the less holes are fixed by laser oscillation, which works in the direction of increasing the relative light output, but the thicker the intermediate layer, the more easily holes seep out to the n-side region, which works in the direction of decreasing the relative light output. From these results, it can be said that it is preferable that the film thickness of the intermediate layer is not too thick. [Industrial Applicability]

[0049] The semiconductor laser device according to the present invention can be used as a light source for optical disks, as well as a light source for displays such as projectors and televisions, as a light source for medical use, as a light source for illumination, and the like. [Explanation of symbols]

[0050] 100 Semiconductor laser element 1 Board 2 n-side area 21 First n-type semiconductor layer 22 Second n-type semiconductor layer 23 Third n-type semiconductor layer (n-type nitride semiconductor layer) 24 Fourth n-type semiconductor layer 25 N-side composition gradient layer 3 Active area 31 First barrier layer 32 Middle Class 33 Well Layer 34 Second Barrier Layer 35 InGaN layer 36 GaN layers 37 Intermediate barrier layer 4 p side region 41 P-side compositionally graded layer 42 First p-type semiconductor layer 43 Second p-type semiconductor layer (p-type nitride semiconductor layer) 44 Third p-type semiconductor layer 4a Ridge 5. Insulating film 5a aperture 6p electrode 7 P-side pad electrode 8n electrode

Claims

1. a first nitride semiconductor layer of a first conductivity type; a second nitride semiconductor layer of a second conductivity type; an active region having a single quantum well structure or a multiple quantum well structure, disposed between the first nitride semiconductor layer and the second nitride semiconductor layer; the active region has, in order from the first nitride semiconductor layer side, a first barrier layer, an intermediate layer, a well layer, and a second barrier layer, the lattice constant of the intermediate layer is larger than the lattice constants of the first barrier layer and the second barrier layer and is smaller than the lattice constant of the well layer; the intermediate layer has a thickness greater than that of the well layer; the well layer and the second barrier layer are in contact with each other, or the distance between the well layer and the second barrier layer is smaller than the distance between the first barrier layer and the well layer.

2. 2. The semiconductor laser device according to claim 1, wherein the intermediate layer has a thickness of less than 13 nm.

3. 3. The semiconductor laser device according to claim 1, wherein the intermediate layer has a thickness of 3 nm or more.

4. The first barrier layer is In a G 1-a N (0≦a<1), The intermediate layer is In b G 1-b N (a<b<1), The well layer is In c G 1-c N (b<c<1), The second barrier layer is In d G 1-d 4. The semiconductor laser device according to claim 1, wherein N (0≦d<b).

5. 5. The semiconductor laser device according to claim 1, wherein the intermediate layer is a compositionally graded layer having a lattice constant that increases from the first barrier layer toward the well layer.

6. the semiconductor laser element comprises a first cladding layer, a second cladding layer, a first optical guide layer, and a second optical guide layer; the active region is disposed between the first cladding layer and the second cladding layer; the first optical guiding layer is disposed between the first cladding layer and the active region; 6. The semiconductor laser device according to claim 1, wherein the second optical guiding layer is disposed between the second cladding layer and the active region.

7. the first nitride semiconductor layer is the first cladding layer or the first optical guiding layer, The semiconductor laser device according to claim 6 , wherein the second nitride semiconductor layer is the second cladding layer or the second optical guiding layer.

8. the first nitride semiconductor layer is an n-type nitride semiconductor layer, 8. The semiconductor laser device according to claim 1, wherein the second nitride semiconductor layer is a p-type nitride semiconductor layer.

9. The semiconductor laser element includes a substrate, 9. The semiconductor laser element according to claim 1, wherein the first nitride semiconductor layer, the active region, and the second nitride semiconductor layer are arranged in this order from the substrate side.

Citation Information

Patent Citations

  • Nitride semiconductor laser and manufacturing method thereof

    JP2004022989A

  • Nitride semiconductor light emitting device

    JP2004031770A

  • Nitride semiconductor light-emitting element, method for manufacturing the same, and optical device mounting the same

    JP2004087908A

  • Optoelectronic semiconductor chips

    JP2012522390A

  • Semiconductor laser element and method for manufacturing the same

    JP2018050021A