Method for manufacturing double container, and double container
By covering the inner preform with the outer preform and using a reinforcing structure and support mold to suppress stretching, the method addresses the vulnerability of the pinch-off portion, ensuring robust manufacturing of double containers.
Patent Information
- Application Number
- JP2024161436
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-11-29
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-28
- Estimated Expiration
- 2040-10-15
AI Technical Summary
The pinch-off portion of a blow molded inner preform is prone to rupture due to low strength, especially when vigorously stretched during the manufacturing process.
A method involving blow molding with the inner preform covered by the outer preform, where stretching of the outer preform's bottom is suppressed by using a reinforcing structure such as an annular convex portion and supported by a bottom support mold, ensuring the pinch-off portion is protected.
This method effectively reduces the risk of rupture at the pinch-off portion, enhancing the structural integrity of the double container by preventing excessive stretching during the manufacturing process.
Smart Images

Figure 2024166376000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a double container and a double container. [Background technology]
[0002] Patent Document 1 discloses a method for producing a double container by blow molding an inner preform and an outer preform in a stacked state. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] WO2004 / 071887 Summary of the Invention [Problem to be solved by the invention]
[0004] When the inner preform is a blow molded article, a pinch-off portion is formed at the bottom of the inner preform where the parison is closed. Since the strength of the pinch-off portion is relatively weak, if the area near the pinch-off portion is stretched forcefully during blow molding, the pinch-off portion may rupture.
[0005] The present invention has been made in consideration of the above circumstances, and provides a method for manufacturing a double container and a double container that can reduce the possibility of the pinch-off portion tearing. [Means for solving the problem]
[0006] [1] A method for manufacturing a double-walled container, comprising a blow molding step, the blow molding step being carried out by heating and softening the inner preform and the outer preform while the inner preform is covered with an outer preform, and then blowing air into the inner preform in that state, the inner preform being a blow molded body, and the blow molding step being carried out while suppressing extension of the bottom of the outer preform. [2] The method according to [1], wherein the outer preform has a reinforcing structure that suppresses elongation of a bottom portion of the outer preform. [3] The method according to [2], wherein the reinforcing structure is an annular protrusion provided at the bottom of the outer preform. [4] The method according to any one of [1] to [3], wherein the blow molding step is carried out in a state in which the bottom of the outer preform is supported by a bottom support mold to suppress stretching of the bottom. [5] A method for manufacturing a double container having an inner bag and an outer shell, comprising a blow molding process, in which a preform having a portion that will become the inner bag and a portion that will become the outer shell is heated and softened, and air is blown into the preform in that state, and the blow molding process is performed while suppressing extension of the bottom of the portion that will become the outer shell. [6] The method according to [5], wherein the portion that becomes the outer shell has a reinforcing structure that suppresses extension of a bottom portion of the portion that becomes the outer shell. [7] The method according to [6], wherein the reinforcing structure is an annular protrusion provided at the bottom of the portion that becomes the outer shell. [8] The method according to [7], wherein an outside air introduction hole is arranged in the outer shell in the inner region of the annular protrusion. [9] The method according to any one of [5] to [8], wherein the blow molding step is carried out in a state in which the bottom of the part that will become the outer shell is supported by a bottom support mold, thereby suppressing the stretching of the bottom.
[10] A double container having an outer shell and an inner bag, the inner bag being a shrinkable container body, the container body being formed by blow molding a preform having a portion that will become the inner bag and a portion that will become the outer shell, the blow molding being performed in a state in which stretching of the bottom of the portion that will become the outer shell is suppressed.
[11] A double container as described in
[10] , wherein the portion that becomes the outer shell has a reinforcing structure that suppresses extension of the bottom portion of the portion that becomes the outer shell.
[12] A double container having an outer shell and an inner bag, the inner bag being capable of shrinking, the container body having a cylindrical body and a bottom provided at the lower end of the body, the outer shell having an annular protrusion at the bottom, and an outside air inlet hole arranged in the outer shell in the area inside the annular protrusion.
[0007] According to the present invention, there is provided a method for manufacturing a double container, which includes a blow molding step, in which the blow molding step is carried out by heating and softening the inner preform and the outer preform while the outer preform is placed over the inner preform, and then blowing air into the inner preform in that state, the inner preform being a blow molded body, and the blow molding step is carried out in a state in which extension of the bottom of the outer preform is suppressed, and a double container is provided.
[0008] As a result of intensive research, the inventors have found that the above-mentioned problem can be solved by expanding the preform while suppressing the stretching of the bottom of the outer preform. Since the pinch-off portion is disposed at a position facing the bottom of the outer preform, when the stretching of the bottom is suppressed, the stretching of the portion near the pinch-off portion is also suppressed, and the above-mentioned problem is solved.
[0009] Various embodiments of the present invention will be described below. The embodiments described below can be combined with each other. Preferably, in the double container described above, the spacer is a protrusion provided on the outer shell or the inner bag. Preferably, in the dual container described above, the spacers are arranged radially. Preferably, in the double container described above, the spacer is arranged to form an intermittent circle. Preferably, in the double container described above, the container body is a double container formed by heating and blow molding an inner preform that becomes the inner bag and an outer preform that becomes the outer shell, with the inner preform that becomes the inner bag being covered with an outer preform that becomes the outer shell. Preferably, the double container described above is one in which the inner preform has a positioning pin at the bottom of the inner preform, the outer preform has a positioning hole at the bottom of the outer preform, and the blow molding is performed with the positioning pin inserted into the positioning hole. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1A shows a container body 2 of a double container 1 according to a first embodiment of the present invention, and FIG. 1B is a bottom view. [Diagram 2] 2A is a perspective view of the container body 2 in FIG. 1 as viewed from the bottom 7 side, and FIG. 2B is a cross-sectional perspective view of the vicinity of the bottom 7 of the outer shell 3 as viewed from the inside of the container. [Diagram 3] 3A is a cross-sectional view taken along line AA in FIG. 1B, and FIG. 3B is a cross-sectional view taken along line BB in FIG. 3A. [Figure 4] FIG. 2 is a perspective view showing a state in which the inner preform 14 and the outer preform 13 are separated. [Diagram 5] 5 is a cross-sectional perspective view of the vicinity of a bottom portion 13c of the outer preform 13 in FIG. 4, as viewed from the inside of the outer preform 13. FIG. [Figure 6] FIG. 6A is a perspective view of an assembly 15 formed by covering an outer preform 13 on an inner preform 14, and FIG. 6B is a perspective view of FIG. 6A seen from a different angle. [Figure 7] FIG. 2 is a cross-sectional view showing the biaxial stretch blow molding process, illustrating a state in which an assembly 15 is attached to a mouth support mold 21. [Figure 8] 8 is a cross-sectional view showing a state after the molding dies 23, 24 are closed and the bottom support die 22 supports the bottom 13c of the outer preform 13 from the state shown in FIG. 7. FIG. [Figure 9] 9 is a cross-sectional view showing the state after the assembly 15 has been longitudinally stretched by extending the support rod 25 and retracting the bottom support mold 22 from the state shown in FIG. 8. FIG. [Figure 10] 6 is a cross-sectional perspective view corresponding to FIG. 5, showing an outer preform 13 having intermittent circular projections 13c1. FIG. [Figure 11] 1 is a perspective view showing an inner preform 14 having radial projections 14c2 on a bottom portion 14c. FIG. [Figure 12] 1 is a perspective view showing an inner preform 14 having a bottom portion 14c on which intermittent circular projections 14c2 are provided. FIG. [Figure 13] 13 is an enlarged view of the vicinity of a bottom 14g of an inner preform 14 of a modified example. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, embodiments of the present invention will be described. Various features shown in the following embodiments can be combined with each other. Also, each feature can be an invention independently.
[0012] 1. First embodiment As shown in Fig. 1, the double container 1 of the first embodiment of the present invention includes a container body 2. As shown in Fig. 3A, the container body 2 has an outer shell 3 and an inner bag 4, and is configured so that the inner bag 4 shrinks as the contents decrease.
[0013] As shown in FIG. 1, the container body 2 has a mouth portion 5, a body portion 6, and a bottom portion 7. The mouth portion 5 has an engagement portion 5a to which a pump (not shown) can be attached. The engagement portion 5a is a male thread portion in the case of a screw-type pump, and is an annular projection protruding in the circumferential direction in the case of a tapping-type pump. The mouth portion 5 is provided so as to extend from an upper end 6a of the body portion 6. The mouth portion 5 is cylindrical. The body portion 6 has a larger outer diameter (in this specification, "outer diameter" means the circumscribed circle diameter when the cross section is not circular) than the mouth portion 5.
[0014] The body 6 is cylindrical, and the bottom 7 is provided at the lower end of the body 6 and closes the lower end of the body 6. The bottom 7 has a central recess 7a provided in the center of the bottom 7, and a peripheral portion 7b surrounding the central recess 7a.
[0015] As shown in FIG. 2A, the central recess 7a is provided with a locking portion 7a1, an outside air introduction hole 7a2, an annular protrusion 7a3, and a positioning recess 7a4. As shown in FIG. 3A, the locking portion 7a1 is formed by inserting a locking protrusion 4a provided on the inner bag 4 into an insertion hole 3a provided on the outer shell 3. The locking portion 7a1 prevents the inner bag 4 from coming off the outer shell 3. The outside air introduction hole 7a2 is a through hole that penetrates the outer shell 3, and as the inner bag 4 contracts, outside air is introduced into the intermediate space between the outer shell 3 and the inner bag 4 through the outside air introduction hole 7a2. The locking portion 7a1 and the outside air introduction hole 7a2 are arranged in the annular protrusion 7a3. The positioning recess 7a4 is used to position the container body 2 in the circumferential direction when printing or the like is performed on the container body 2.
[0016] The peripheral portion 7b is provided with a grounding portion 7b1 and a peripheral recess 7b2. The grounding portion 7b1 is a portion that comes into contact with the placement surface on which the container body 2 is placed when the container body 2 is erected. If the entire peripheral portion 7b were to be the grounding portion 7b1, the central recess 7a would become an airtight space between the container body 2 and the placement surface when the container body 2 is erected, and there is a risk that the introduction of outside air through the outside air introduction hole 7a2 would be hindered. Therefore, the peripheral recess 7b2 is provided as an air passage so that the inside of the central recess 7a does not become an airtight space.
[0017] When the contents in the inner bag 4 are discharged by the pump attached to the mouth portion 5, the inner bag 4 shrinks and tries to move away from the outer shell 3. At this time, outside air is introduced into the space between the inner bag 4 and the outer shell 3 through the outside air introduction hole 7a2. On the other hand, as shown in FIG. 3A, the peripheral portion 7b has a small radius of curvature, so that the inner bag 4 does not easily separate from the outer shell 3 at the peripheral portion 7b, and it is difficult to form an air passage through which the outside air introduced from the outside air introduction hole 7a2 passes. Therefore, it is difficult for the outside air to be introduced into the body portion 6. In this case, there is a problem that the outer shell 3 shrinks together with the inner bag 4 as the contents decrease. Therefore, in this embodiment, a spacer 9 is disposed between the outer shell 3 and the inner bag 4. In this embodiment, a protrusion 3b protruding from the outer shell 3 toward the inner bag 4 is provided as the spacer 9. When the spacer 9 is provided, a gap 8 is formed between the outer shell 3 and the inner bag 4 at a position adjacent to the spacer 9, and the gap 8 forms an air passage connecting the body 6 and the bottom 7, making it easier for outside air introduced from the outside air introduction hole 7a2 to be introduced into the body 6 through the peripheral edge 7b. The spacers 9 are provided radially so as to straddle the bottom 7 and the body 6, making it easier to form an air passage spanning the bottom 7 and the body 6.
[0018] As shown in Figures 4 to 6, the container body 2 can be formed by heating and biaxially stretching blow molding an inner preform 14, which will become the inner bag 4, and an outer preform 13, which will become the outer shell 3, while covering the inner preform 14, which will become the inner bag 4, with the outer preform 13.
[0019] 4, the inner preform 14 is a cylindrical member with a bottom, and includes a mouth portion 14a, a body portion 14b, and a bottom portion 14c. A flange 14a1 is provided at the open end of the mouth portion 14a. A positioning pin 14c1 is provided at the bottom portion 14c.
[0020] As shown in FIG. 4, the outer preform 13 is a bottomed tubular shape, and includes a mouth portion 13a, a body portion 13b, and a bottom portion 13c. As shown in FIG. 5, the inner surface of the bottom portion 13c of the outer preform 13 is provided with radially arranged protrusions 13c1. The bottom portion 13c is provided with a positioning hole 13c2 and an outside air introduction hole 13c3. As shown in FIG. 6B, the outer surface of the bottom portion 13c is provided with an annular protrusion 13c4. The positioning hole 13c2 and the outside air introduction hole 13c3 are arranged in the inner region of the annular protrusion 13c4. The outer preform 13 has a size that allows the inner preform 14 to be inserted therein.
[0021] The inner preform 14 and the outer preform 13 can be formed by blow molding, injection molding, or the like, of thermoplastic resin such as polyester (e.g., PET) or polyolefin (e.g., polypropylene, polyethylene). In one example, the inner preform 14 is formed by blow molding of polypropylene, and the outer preform 13 is formed by injection molding of PET. By making the inner preform 14 and the outer preform 13 from different materials, welding to each other during blow molding is suppressed. Furthermore, when the outer preform 13 is formed by injection molding, the outside air introduction hole 13c3 can be formed during injection molding, so that the effort of post-processing can be saved.
[0022] 2. Biaxially stretched blow molding The biaxial stretch blow molding can be carried out by the following method.
[0023] First, as shown in Fig. 6, the outer preform 13 is placed over the inner preform 14 (in other words, the inner preform 14 is inserted into the outer preform 13) to form an assembly 15. At this time, the flange 14a1 is abutted against the open end of the mouth portion 13a, and the positioning pin 14c1 is inserted into the positioning hole 13c2. This positions the inner preform 14 and the outer preform 13 relative to each other. In this state, the mouth portion 14a faces the mouth portion 13a, and the body portion 14b faces the body portion 13b.
[0024] The assembly 15 is then heated to soften it.
[0025] Next, the assembly 15 is placed in a mold for blow molding, and while the mouth portion 13a and the annular protrusion 13c4 are supported by a jig, air is blown into the inner preform 14 to expand the assembly 15 and make it adhere to the inner surface of the cavity of the mold. At this time, a support rod (not shown) may be pressed against the inner bottom surface of the inner preform 14 to prevent the assembly 15 from shaking within the mold. Also, a recess into which the support rod fits may be provided on the inner bottom surface of the inner preform 14 to make it easier to fix the support rod to the inner preform 14.
[0026] The assembly 15 expands by blow molding to obtain the container body 2 shown in Figs. 1 to 3. The mouth parts 13a and 14a become the mouth part 5, the body parts 13b and 14b become the body part 6, and the bottom parts 13c and 14c become the bottom part 7. The projection 13c1, the annular projection 13c4, and the outside air introduction hole 13c3 become the projection 3b, the annular projection 7a3, and the outside air introduction hole 7a2, respectively. During blow molding, the mouth parts 13a and 14a, the annular projection 13c4, and the area inside thereof are hardly deformed, and other parts are mainly deformed. The outside air introduction hole 13c3 is disposed in the area inside the annular projection 13c4, so that it is prevented from being deformed and blocked during blow molding. The flange 14a1 becomes the flange 4b that covers the open end of the mouth part 5 of the container body 2, as shown in Fig. 1A.
[0027] After blow molding, the positioning hole 13c2 becomes the insertion hole 3a shown in Fig. 3A, and the positioning pin 14c1 is inserted into the insertion hole 3a. Then, the positioning pin 14c1 is deformed (i.e., crushed or bent) to become the locking protrusion 4a shown in Fig. 3A. This forms the locking portion 7a1 of the container body 2.
[0028] 3. Details of biaxial stretch blow molding The biaxial stretch blow molding described above can be performed, in one example, by using a mold unit 20 shown in Figures 7 to 9. The mold unit 20 includes a mouth support mold 21, a bottom support mold 22, and molding molds 23 and 24.
[0029] The mouth support mold 21 is configured to be able to support the mouth 13a of the outer preform 13. An insertion hole 21a is provided in the mouth support mold 21, and a support rod 25 is inserted into the insertion hole 21a. The support rod 25 can be extended and retracted by a driving mechanism (not shown). The bottom support mold 22 is configured to be driven by a driving mechanism 22c and can move in the vertical extension direction (up and down direction in FIG. 7). The forming molds 23 and 24 can be opened and closed, and each have a cavity surface 23a and 24a. The cavity surfaces 23a and 24a come together to form a cavity having a shape corresponding to the outer shape of the container body 2.
[0030] The method includes the steps of preform heating, bottom supporting, stretching, and blow molding.
[0031] <Preform heating process> In the preform heating step, the assembly 15 formed by covering the inner preform 14 with the outer preform 13 is attached to the mouth support mold 21 as shown in Fig. 7, and in this state, the assembly 15 is heated and softened. The assembly 15 may be heated while it is disposed between the molding dies 23 and 24, or may be heated outside the space between the molding dies 23 and 24. Furthermore, before the preform heating step, the tip of the support rod 25 may be abutted against the inner bottom surface of the inner preform 14. This prevents the softened assembly 15 from shaking.
[0032] <Bottom support process> In the bottom support step, as shown in FIG. 8, the bottom support mold 22 moves toward the bottom 13c of the outer preform 13, and supports the bottom 13c of the outer preform 13 with the bottom support mold 22. The bottom support mold 22 is provided with a recess 22a capable of accommodating the annular convex portion 13c4, and the bottom support mold 22 preferably supports the bottom 13c so that the annular convex portion 13c4 is accommodated in the recess 22a. This prevents the annular convex portion 13c4 and its inner region from being stretched during the blow molding step. The recess 22a is preferably annular. In addition, the bottom support mold 22 preferably includes a recess 22b capable of accommodating the positioning pin 14c1, and supports the bottom 13c so that the positioning pin 14c1 is accommodated in the recess 22b. This prevents the positioning pin 14c1 from interfering with the bottom support mold 22. FIG. 8 shows a state in which the molding dies 23, 24 are closed, but the molding dies 23, 24 may be closed at any time before the blow molding step, and may be closed after the longitudinal stretching step.
[0033] <Longitudinal stretching process> In the longitudinal stretching step, as shown in Figs. 8 to 9, the support rod 25 is pressed against the inner bottom surface of the inner preform 14 and stretched, thereby stretching the assembly 15 in the longitudinal direction (the vertical direction in Fig. 9). At this time, it is preferable to move the bottom support mold 22 backward in synchronization with the extension of the support rod 25. This allows the assembly 15 to be stably stretched. Note that the longitudinal stretching step can also be performed in a state where the bottom 13c is not supported by the bottom support mold 22, so the bottom support step may be performed after the longitudinal stretching step.
[0034] <Blow molding process> In the blow molding process, air is blown into the inner preform 14 from the state shown in Fig. 9 to stretch (i.e. expand) the assembly 15 laterally and shape it into the shape of the cavity surfaces 23a, 24a. The air can be blown in through the air passage 26 between the mouth support mold 21 and the support rod 25, but for example, an air passage may be provided in the support rod 25 so that the air can be blown out from the side of the support rod 25.
[0035] In this embodiment, air is blown into the outer preform 13 while the bottom portion 13c is supported by the bottom support mold 22, so that the extension of the bottom portion 13c of the outer preform 13 is suppressed.
[0036] The blow molding step can be performed simultaneously with the longitudinal stretching step. That is, air can be blown into the inner preform 14 while stretching the assembly 15 in the longitudinal direction. Also, the longitudinal stretching step can be omitted, and air can be blown in after the bottom supporting step without stretching the assembly 15 in the longitudinal direction.
[0037] 4. Other embodiments In the above embodiment, the spacers 9 are provided radially, but the spacers 9 may have another shape. For example, the spacers 9 may be arranged to form an intermittent circle. In this case, an air passage is formed in the missing portion of the circle. It is preferable that a plurality of intermittent circles are arranged concentrically. For example, such a spacer 9 can be formed by using an outer preform 13 having intermittent circular projections 13c1 as shown in FIG. 10. In the above embodiment, the protrusion 3b protruding from the outer shell 3 towards the inner bag 4 is formed by providing the protrusion 13c1 on the outer preform 13. However, as shown in Figures 11 and 12, a protrusion (spacer) protruding from the inner bag 4 towards the outer shell 3 may be formed by providing a protrusion 14c2 (e.g., a radial protrusion as shown in Figure 11 or an intermittent circular protrusion as shown in Figure 12) on the bottom 14c of the inner preform 14. The spacer 9 may be formed of a separate member. The spacer 9 can be disposed between the outer shell 3 and the inner bag 4 by performing blow molding with a member serving as a spacer disposed between the inner preform 14 and the outer preform 13.
[0038] 5. Inventions from a different perspective When the inner preform 14 is a blow molded body (more specifically, a direct blow molded body), a pinch-off portion 14h is formed at the position where the parison is closed in the bottom portion 14g of the inner preform 14, as shown in Fig. 13. Since the strength of the pinch-off portion 14h is relatively weak, there is a risk that the pinch-off portion 14h will break if the area near the pinch-off portion 14h is stretched forcefully during biaxial stretch blow molding.
[0039] In one example, as shown in FIG. 13, the inner preform 14 has a multi-layer structure, and includes, from the inside, an innermost layer 14d, a gas barrier layer (e.g., an EVOH layer) 14e, and an outermost layer 14f. The innermost layer 14d and the outermost layer 14f are made of polyolefin (e.g., polyethylene, polypropylene), PET, or the like. In the pinch-off portion 14h, the opposing gas barrier layers 14e1 and 14e2 are connected to each other, or even if they are separated, the gap G between them is very small. If the area near the pinch-off portion 14h is stretched forcefully during biaxial stretch blow molding, the gas barrier layer 14e may tear or the gap G may become large, resulting in problems such as a decrease in gas barrier properties.
[0040] As explained in "2. Biaxial stretch blow molding" and "3. Details of biaxial stretch blow molding", the above problem can be solved by expanding the assembly 15 in a state where the stretching of the bottom part 13c of the outer preform 13 is suppressed. Since the pinch-off part 14h is disposed at a position facing the bottom part 13c of the outer preform 13, when the stretching of the bottom part 13c is suppressed, the stretching of the part near the pinch-off part 14h is also suppressed, and the above problem is solved.
[0041] In "2. Biaxial stretch blow molding", the rigidity of the bottom 13c is increased and the stretching of the bottom 13c is suppressed by providing an annular protrusion 13c4 on the bottom 13c of the outer preform 13. The structure provided to increase the rigidity of the bottom 13c may be a reinforcing structure other than the annular protrusion 13c4.
[0042] In "3. Details of biaxial stretch blow molding", stretching of the bottom 13c is suppressed by performing the blow molding process while the bottom 13c of the outer preform 13 is supported by the bottom support mold 22. In the above explanation, the annular convex portion 13c4 is accommodated in the concave portion 22a, but even if the bottom 13c does not have the annular convex portion 13c4, supporting the bottom 13c with the bottom support mold 22 suppresses stretching of the bottom 13c due to friction between the bottom 13c and the bottom support mold 22.
[0043] In consideration of the above, according to the present invention, A method for manufacturing a double container, comprising the steps of: A blow molding process is provided. The blow molding step is performed by heating and softening the inner preform and the outer preform in a state where the inner preform is covered with the outer preform, and then blowing air into the inner preform in that state. The inner preform is a blow molded body, A method is provided, wherein the blow molding step is performed with restrained stretching of a bottom portion of the outer preform.
[0044] Preferably, the outer preform comprises a reinforcing structure that inhibits elongation of a bottom portion of the outer preform. Preferably, the reinforcing structure is an annular protrusion provided on the bottom of the outer preform. Preferably, the blow molding step is performed in a state in which the bottom of the outer preform is supported by a bottom support mold to suppress stretching of the bottom.
[0045] Also, from another perspective, A method for manufacturing a double container, comprising the steps of: A blow molding process is provided. The blow molding step is performed by blowing air into the inner preform while the inner preform and the outer preform are covered with the inner preform and softened by heating, The inner preform is a blow molded body, A method is provided, wherein the outer preform has an annular protrusion at its bottom.
[0046] In the invention from another viewpoint, the position of the outside air introduction hole is not limited, and it may be provided in any of the mouth portion 5, the body portion 6, or the bottom portion 7 of the container body 2. Moreover, the spacer 9 for forming a gap between the outer shell 3 and the inner bag 4 is not essential. [Explanation of symbols]
[0047] 1:Double container 2: Container body 3: Outer shell 3a: Insertion hole 3b: Protrusion 4: Inner bag 4a: Locking protrusion 4b: Flange 5: Mouth 5a: Engagement part 6: Torso 6a: Upper end 7: Bottom 7a: Central recess 7a1: Locking part 7a2: Outside air intake 7a3: Annular protrusion 7a4: Positioning recess 7b: Periphery 7b1: Grounding part 7b2: Peripheral recess 8: Gap 9: Spacer 13: Outer preform 13a: Mouth 13b: Torso 13c: Bottom 13c1 :Protrusion 13c2: Positioning hole 13c3: Outside air intake 13c4: Annular protrusion 14: Inner preform 14a: Mouth 14a1: Flange 14b: Torso 14c: Bottom 14c1: Positioning pin 14c2 :Protrusion 14d: Innermost layer 14e: Gas barrier layer 14e1: Gas barrier layer 14e2: Gas barrier layer 14f: Outermost layer 14g: Bottom 14h: Pinch-off section 15: Assembly 20: Mold unit 21: Mouth support type 21a: Insertion hole 22: Bottom support type 22a: Recess 22b: Recess 22c: Drive mechanism 23: Molding mold 23a: Cavity surface 24: Molding mold 24a: Cavity surface 25: Support rod 26: Air passage G: Gap
Claims
1. A method for manufacturing a double container, comprising the steps of: A blow molding process is provided. The blow molding step is performed by heating and softening the inner preform and the outer preform in a state where the inner preform is covered with the outer preform, and then blowing air into the inner preform in that state. The inner preform is a blow molded body, The method of claim 1, wherein the blow molding step is performed under conditions where stretching of a bottom portion of the outer preform is restrained.
2. 2. The method of claim 1 , The method of claim 1, wherein the outer preform comprises a reinforcing structure that inhibits stretching of a bottom portion of the outer preform.
3. 3. The method of claim 2, The method, wherein the reinforcing structure is an annular protrusion provided on a bottom of the outer preform.
4. The method according to any one of claims 1 to 3, The blow molding step is performed in a state in which the bottom of the outer preform is supported by a bottom support mold to suppress stretching of the bottom.
5. A method for manufacturing a double container having an inner bag and an outer shell, comprising the steps of: A blow molding process is provided. The blow molding step is performed by heating and softening a preform including a portion that becomes the inner bag and a portion that becomes the outer shell, and then blowing air into the preform in that state. The blow molding step is carried out in a state where stretching of a bottom portion of the portion that becomes the outer shell is suppressed.
6. 6. The method of claim 5, The method of claim 1, wherein the portion that will become the outer shell has a reinforcing structure that inhibits extension of a bottom portion of the portion that will become the outer shell.
7. 7. The method of claim 6, The method, wherein the reinforcing structure is an annular protrusion provided at the bottom of the portion that will become the outer shell.
8. 8. The method of claim 7, The method of claim 1, wherein an outside air introduction hole is disposed in the outer shell in an area inside the annular protrusion.
9. The method according to any one of claims 5 to 8, The blow molding step is performed in a state in which a bottom of the portion to become the outer shell is supported by a bottom support mold to suppress stretching of the bottom.
10. A double container having an outer shell and an inner bag, the inner bag comprising a contractible container body, the container body is formed by blow molding a preform having a portion that becomes the inner bag and a portion that becomes the outer shell, The blow molding is performed in a state where the stretching of the bottom part of the part that becomes the outer shell is suppressed.
11. The double container according to claim 10, The portion that becomes the outer shell has a reinforcing structure that suppresses extension of the bottom portion of the portion that becomes the outer shell.
12. A double container having an outer shell and an inner bag, the inner bag comprising a contractible container body, The container body includes a cylindrical body and a bottom provided at a lower end of the body, The outer shell is provided with an annular protrusion at the bottom, A double container, wherein an outside air introduction hole is arranged in the outer shell in the inner region of the annular convex portion.
Citation Information
Patent Citations
Stretching blow molding method of hollow vessel having raised bottom
JP1990078520A
Manufacture of biaxially oriented plastic bottle
JP1992131222A
Biaxially stretched polypropylene blow molded bottle with transparent bottom
JP1997048061A
Blow molding method
JP2017094677A
Laminated releasable bottle and method of producing the same
WO2004071887A1