Porous and encapsulated aggregates for abradable sealant materials and methods for making same - Patents.com

Powder agglomerates with enhanced porosity and hollow structures address the limitations of conventional abradable sealants, improving fuel efficiency and wear resistance in turbomachinery by selecting suitable materials and encapsulating components for thermal spraying.

JP2024543523AInactive Publication Date: 2024-11-21OERLIKON METCO (US) INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024529332
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-18
Filing Date
2022-10-28
Publication Date
2024-11-21
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional abradable sealant materials for turbomachinery face limitations such as limited heating capacity, density mismatch, and high cost, which affect their application temperatures and deposition efficiency, particularly in automotive turbochargers and gas turbines.

Method used

The development of powder agglomerates that form coatings with enhanced porosity and hollow structures directly from primary powder particles, allowing for the selection of suitable materials based on properties and cost, and encapsulating components like graphite or YSZ powder to improve thermal spraying efficiency.

Benefits of technology

The new coating technology enhances fuel efficiency by minimizing wear on rotating parts, reducing debris formation, and maintaining clearance adjustment, while overcoming the drawbacks of traditional materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543523000001_ABST
    Figure 2024543523000001_ABST
Patent Text Reader

Abstract

A powder agglomerate for an abradable sealant coating is provided, comprising a first powder having a pure metal or metal alloy and a second powder comprising a mineral, the powder agglomerate having at least one morphology selected from a porous agglomerate, a hollow agglomerate, a composite agglomerate, and a hybrid agglomerate. A powder agglomeration method is also provided that does not use a fugitive phase such as a polymer and a porosity former.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application claims the benefit of and priority to U.S. Provisional Application No. 63 / 280,821, filed November 18, 2021, the disclosure of which is expressly incorporated herein by reference in its entirety.

[0002] FIELD OF THEINVENTION The present disclosure relates to powder agglomerates using metallic or non-metallic powders for abradable sealant coatings to increase engine efficiency in the high temperature areas of gas turbines, aircraft engines, or automotive turbochargers. [Background technology]

[0003] Background information Abradable seals are traditionally applied by the aviation and power generation industries to stationary components in turbomachinery to reduce the clearance between the rotating components (e.g., blades and labyrinth seal knife edges) and the stationary components (e.g., engine casing). Reducing the clearance between the rotating components and the engine casing improves turbine engine efficiency, reduces fuel consumption, and reduces the clearance safety margin by eliminating the possibility of catastrophic contact between the blades and the engine casing. Abradable seals are produced by applying an abradable coating to the stationary parts (e.g., engine casing) that is scraped off upon contact with the tips of the rotating components (e.g., blades or knife edges) during operation. This process provides substantially no clearance between the blade tips and the inner engine housing.

[0004] In turbomachinery, when a rotating component contacts a stationary component, which can lead to penetration and friction, the stationary component is ideally worn to preserve the integrity of the rotating component and provide in-situ clearance adjustment. To achieve this desired functionality, the surface layer of the stationary component is composed of an abradable material. There are two main mechanisms that contribute to abradability. The first mechanism is a sufficiently high porosity level. The second mechanism is the presence of spallation. Conventional abradable materials contain one of two non-metallic phases as secondary components to achieve the mechanisms that contribute to abradability: (1) a sacrificial phase, which is typically a polymer and is removed by post-processing to generate a high porosity level in the finished coating or bulk material, and (2) a fugitive phase, which is typically a solid lubricant such as graphite or hexagonal boron nitride (hBN). The fugitive phase allows for microscopic material destruction and subsequent macroscopic material removal in the finished coating or bulk material. Although effective, such single non-metallic phases have several drawbacks for certain applications. The first is the limited heating capacity of the polymers, which narrows their application temperature to a relatively low range up to a maximum temperature of 350°C. The second is the large density mismatch with the primary metal powder components, which results in undesirable material loss and low deposition efficiency during thermal spraying. This drawback is especially pronounced in simple powder blends. The third drawback is that certain polymers and boron nitride powders are expensive, which makes it difficult to produce a high quality powder product at a competitive price.

[0005] In recent years, there has been considerable interest from the automotive industry in applying abradable coatings to automotive turbochargers, particularly compressors, to further increase engine efficiency and reduce greenhouse gas emissions. Unlike turbomachinery used in aircraft engines and gas turbines, where thermal and inertial expansion or shock load events occur periodically, abradable coatings in automotive turbochargers are generally only required in the event of unexpected intrusion of the rotor blades into the stationary part. Conventional automotive turbochargers have a permanent gap between the rotor blades and the stationary part. Nevertheless, the rotating part on the compressor side of the turbocharger, which is primarily composed of lightweight aluminum alloys, is particularly sensitive to unbalance effects caused by blade tip damage or debris originating from the stationary part or other contamination sources. Thus, there is a need to produce an abradable coating to minimize the clearance safety margin, reduce wear on the rotating parts, and improve overall fuel efficiency. Summary of the Invention

[0006] The present disclosure provides powder agglomerates that form coatings that improve fuel efficiency in turbomachinery from the aviation, power generation, and automotive industries. In embodiments of the present disclosure, alternative powder morphologies and material microstructures achieve desired abradability and avoid the shortcomings of traditional abradable materials.

[0007]

[0010] Embodiments of the present disclosure allow for the direct formation of porous or hollow agglomerates made from primary powder particles formed during the powder agglomeration manufacturing process. In embodiments, the porous microstructure remains in the finished product, such as a coating.

[0008] Due to the direct formation of porous and hollow aggregates, the choice of secondary components for the abradable material is broadened and is no longer limited to a single non-metallic phase such as a polymer or solid lubricant. Depending on the application, the most suitable material can be selected based on properties, coating economics, or cost savings to create the desired microstructure.

[0009] The present disclosure also provides an agglomeration process for producing powder agglomerates. The agglomeration process and the powder agglomerates obtained by the disclosed process provide several advantageous functionalities. First, the porous (400) or hollow (300) agglomerates, encapsulated particles, or encapsulated agglomerates (500) are formed directly from the primary powder particles without any post-treatment. Second, the enhanced porosity and particle / agglomerate encapsulation remain in the finished coating without any post-treatment. The enhanced porosity is achieved based on the novel powder particle morphology. That is, the hollow or porous particle morphology gives rise to pores and voids in the coating that are not only created by the thermal spray process, but also directly from the powder particles or agglomerates. Third, in the event of unexpected intrusion of a rotating part into a stationary part during operation, the abradable material obtained by the powder agglomerates of the present disclosure achieves the following: (1) clean stationary parts (e.g., blades, stators, liners, and casings) as well as removal of surface material from the stationary parts with particle size <1 mm; (2) prevents significant wear to rotating parts (e.g., blades, knives, seal strips, and impellers) that are typically composed of aluminum alloys, iron alloys, nickel alloys, and titanium alloys; (3) prevents significant accumulation of surface material from the stationary parts; and (4) prevents the formation of debris or pieces with particle size >1 mm that are detrimental to the design functionality or hydrodynamic performance of the turbomachinery parts.

[0010] In an embodiment of the present disclosure, the agglomeration process provides encapsulation of one powder component with another powder component to form a hybrid agglomerate. In an embodiment, the "one powder component" is graphite powder that is encapsulated by the "other powder component" such as YSZ powder. This is particularly beneficial for light materials that can be encapsulated by another material with higher density and remain longer as an agglomerate in the powder jet and plasma plume during thermal spraying. Thus, coating repeatability and economics are improved. [Brief description of the drawings]

[0011] The present disclosure is further described in the following detailed description with reference to a number of drawings which illustrate, by way of non-limiting examples, preferred embodiments of the present disclosure. [Figure 1A] 1 is a 2000x scanning electron microscope (SEM) image showing a phyllosilicate as a primary feedstock for a powder agglomeration process according to one embodiment of the present disclosure. [Figure 1B] 1 is a 500x SEM image showing a metal alloy powder as a primary feedstock for a powder agglomeration process according to one embodiment of the present disclosure; [Figure 2A] FIG. 1 illustrates a hybrid agglomerate having an encapsulated primary powder particle powder morphology according to one embodiment of the present disclosure. [Figure 2B] FIG. 1 illustrates a hybrid agglomerate having encapsulated primary particles and a partially hollow powder morphology according to another embodiment of the present disclosure. [Figure 2C] FIG. 1 illustrates a porous aggregate powder morphology according to one embodiment of the present disclosure. [Figure 2D] FIG. 1 illustrates hollow aggregate powder morphology according to one embodiment of the present disclosure. [Figure 3A] 1A-1D are SEM images showing the achieved powder morphology of hollow phyllosilicate aggregates, phyllosilicates, and metal alloys according to embodiments of the present disclosure. [Figure 3B] 1 is a SEM image showing the achieved powder morphology of porous phyllosilicate aggregates, phyllosilicate, and aluminum silicon alloy according to another embodiment of the present disclosure; [Figure 4A] 1 is a SEM image showing the hollow phyllosilicate aggregate microstructure of an abradable coating thermally sprayed using powder produced by an agglomeration process according to one embodiment of the present disclosure. [Figure 4B] 1 is a SEM image showing hollow phyllosilicate agglomerates and agglomerates with encapsulated metallic phase microstructures in an abradable coating thermally sprayed using powder produced by an agglomeration process according to one embodiment of the present disclosure; [Figure 4C]1 is a 3000x SEM image showing the hollow phyllosilicate aggregate microstructure of an abradable coating thermally sprayed using powder produced by an agglomeration process according to one embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] In an embodiment of the present disclosure, the powder agglomeration process is carried out by the following steps (1) to (3): In one embodiment, steps (1) to (3) are all carried out in a spray dryer. (1) Using liquid chemicals to mix and blend primary raw materials into a slurry mixture. In an embodiment, the primary raw materials are metal, non-metal, or a mixture of metal and non-metal powder materials. In an embodiment, the primary raw materials are alloys (e.g., aluminum silicon alloys), solid lubricants (e.g., graphite), minerals (e.g., clay or phyllosilicates). In an embodiment, the particle morphology is not limited to spheres, and thus may be irregular, angular, or plate-like. Examples of liquid chemicals include combinations of solvents, dispersants, and binders. Examples of solvents include water, ethanol, and acetone. Examples of dispersants include sodium polyacrylate. Examples of binders include polyvinyl alcohol (PVA) and carboxymethyl cellulose (CMC). (2) Feeding and dispersing the prepared slurry mixture through a hot gas stream into a drying chamber by an atomizer or spray nozzle. In an embodiment of the present disclosure, the slurry is converted into droplets by an atomization process. In an embodiment using an aqueous slurry, the hot gas is air. (3) Obtaining a powder agglomerate by separating the particles from the hot gas stream. In an embodiment, the droplets from step (2) are converted to solvent-free particles by the hot gas stream in the main chamber. In an embodiment, the particles are then separated from the hot gas by a separator, such as a cyclone, connected to the main chamber. In an embodiment, the desired powder fraction is collected in the main chamber. In another embodiment, the desired powder fraction is collected in the cyclone.

[0013] In one embodiment of the present disclosure, the powder agglomerates are produced by the process described above. In an embodiment, the powder agglomerates produced by the process described above are used in further material formation and processing methods, including powder blending, powder metallurgy, or thermal spraying (e.g., air plasma spraying), to form abradable materials that remain porous or hollow morphology and have enhanced performance.

[0014] In one embodiment of the present disclosure, the powder agglomerate is a composite agglomerate comprising two materials, a first powder component and a second powder component, in other embodiments, the powder agglomerate comprises one or more of the following forms: hollow agglomerates of the second component, porous agglomerates, composite agglomerates of both materials where the first component is partially or fully encapsulated by the second component, and hybrid agglomerates where the particles comprise both hollow pores in the second component and the first component is partially or fully encapsulated by the second component.

[0015] In one embodiment of the present disclosure, the raw material is comprised of 10-90% by weight of composite aggregates. In another embodiment, the raw material is comprised of 10-50% by weight of composite aggregates. In yet another embodiment, the raw material is comprised of 10-40% by weight of composite aggregates. In another embodiment, the raw material is comprised of 50-90% by weight of composite aggregates. In yet another embodiment, the raw material is comprised of 60-90% by weight of composite aggregates.

[0016] In one embodiment of the present disclosure, the composite aggregate is blended with one or more separate powder components to form a final product. In one embodiment, the raw material is a component of the final product, which may optionally be a blend of multiple materials. In another embodiment, the raw material includes both a composite aggregate of the first and second components and a hollow / porous aggregate of the second component.

[0017] In an embodiment, the first component is a pure metal (e.g., aluminum) or a metal alloy. In a preferred embodiment, the first component is an aluminum alloy. In another preferred embodiment, the first component is an aluminum silicon alloy. In yet another preferred embodiment, the first component is an aluminum alloy having 6-20 wt. % Si. In another preferred embodiment, the first component is an aluminum alloy having 8-14 wt. % Si.

[0018] In an embodiment, the second component is a mineral. In a preferred embodiment, the second component is a silicate mineral. In another preferred embodiment, the second component is a phyllosilicate. In yet another preferred embodiment, the second component is a mineral having the formula Mg 3 S 4 O 10 (OH) 2 It is a talc having the above structure.

[0019] In an embodiment of the present disclosure, the composite aggregate is produced by a spray drying process. In one embodiment, the composite aggregate is produced by a spray drying process without additional processing steps. In another embodiment, the composite aggregate is produced without the use of a polymer. In an embodiment, the composite aggregate is produced without the use of a fugitive phase.

[0020] Figure 1A is a 2000x magnification SEM image showing a phyllosilicate powder and Figure 1B is a higher magnification SEM image showing a metal alloy powder. The phyllosilicate powder and the metal alloy powder are used as primary feedstocks for the powder agglomeration process according to an embodiment of the present disclosure.

[0021] Figure 2 shows possible powder morphologies of the powder agglomerates of the present disclosure. Figure 2A shows a hybrid agglomerate powder morphology with encapsulated primary particles. In Figure 2A, the hybrid agglomerate includes larger primary powder particles encapsulated by smaller primary powder particles. Figure 2B shows a hybrid agglomerate with a blend of morphologies including larger primary powder particles encapsulated by smaller primary powder particles and partially hollow microstructures. In Figure 2C, a porous agglomerate powder morphology is shown. In Figure 2D, a hollow agglomerate powder morphology is shown.

[0022] Figure 3 provides SEM images of powder forms achieved in embodiments of the present disclosure. In Figure 3A, the SEM images show a hollow agglomerate of non-metallic particles 300, a dense agglomerate of non-metallic particles 100, and a metal alloy particle 200 in accordance with embodiments of the present disclosure. In one embodiment, the hollow agglomerate of non-metallic particles 300 is a hollow phyllosilicate agglomerate. In one embodiment, the dense agglomerate of non-metallic particles 100 is a phyllosilicate particle. In one embodiment, the metal alloy particle 200 is an aluminum silicon alloy particle.

[0023] In FIG. 3B, an SEM image shows a porous aggregate 400 of non-metallic particles (e.g., a porous phyllosilicate aggregate), a porous hybrid aggregate 500 in which metal particles are encapsulated by non-metallic particles (e.g., aluminum silicon alloy particles encapsulated by phyllosilicate particles), and metal alloy particles 200 (e.g., aluminum silicon alloy particles) according to other embodiments of the present disclosure. In one embodiment, the porous aggregate 400 of non-metallic particles is a porous phyllosilicate aggregate. In one embodiment, the porous hybrid aggregate 500 in which metal particles are encapsulated by non-metallic particles is an aluminum silicon alloy particle encapsulated by a phyllosilicate particle. In one embodiment, the metal alloy particle 200 is an aluminum silicon alloy particle.

[0024] Figure 4 provides an example of the microstructure of an abradable coating that was thermally sprayed using a powder produced by the agglomeration process of the present disclosure. In Figure 4A, an SEM image shows hollow agglomerates 300 of non-metallic particles of an abradable coating that was thermally sprayed using a powder produced by the agglomeration process according to an embodiment of the present disclosure. In one embodiment, the hollow agglomerates 300 of non-metallic particles are hollow phyllosilicate agglomerates.

[0025] In FIG. 4B, a higher magnification SEM image shows hollow agglomerates 300 of non-metallic particles and porous hybrid agglomerates 500 in which metallic particles are encapsulated by non-metallic particles of an abradable coating thermally sprayed using powder produced by the agglomeration process according to an embodiment of the present disclosure.

[0026] In FIG. 4C, a high magnification SEM image shows hollow agglomerates 300 of non-metallic particles of an abradable coating that was thermally sprayed using powder produced by the agglomeration process, according to one embodiment of the present disclosure.

[0027] The powder agglomerates produced by the agglomeration process are demonstrated in the examples below. EXAMPLES

[0028] Example 1 A powder agglomerate according to a preferred embodiment of the present disclosure was produced using an aluminum silicon alloy powder as a first component and a phyllosilicate powder as a second component. The first and second components were spray dried together to form the final powder product using the powder agglomeration process of steps (1)-(3) described above.

[0029] In the final powders, the content of the metal fraction (i.e., aluminum silicon alloy) was between 10% and 90% by weight. The following morphologies were observed: hollow / porous phyllosilicate agglomerates, aluminum silicon alloy particles encapsulated by phyllosilicate particles or by porous phyllosilicate agglomerates.

[0030] Example 2 The same first and second components were used to produce a powder agglomerate as described in Example 1. The first and second components were spray dried together to form an intermediate powder product using the powder agglomeration process of steps (1)-(3) described above. The intermediate powder component was then blended with the second powder component to form the final powder product. The second powder component can be another metal alloy (e.g., another multi-element aluminum silicon alloy) produced by another method (e.g., attrition milling).

[0031] Furthermore, because at least the invention is disclosed herein in a manner that enables it to be made and used by disclosure of certain exemplary embodiments, for purposes of simplicity or efficiency, the invention can be practiced in the absence of any additional elements or additional structure not specifically disclosed herein.

[0032] It should be noted that the foregoing examples are provided for illustrative purposes only and are not to be construed as limiting the present invention in any way. Although the present invention has been described with reference to exemplary embodiments, it is understood that the terms used herein are terms of description and illustration, rather than terms of limitation. Changes may be made within the scope of the appended claims, as currently described and amended, without departing from the scope and spirit of the present invention in its aspects. Although the present invention has been described herein with reference to specific means, materials, and embodiments, the present invention is not intended to be limited to the details disclosed herein, but rather the present invention extends to all functionally equivalent structures, methods, and uses as are within the scope of the appended claims.

Claims

1. A powder agglomerate comprising: a first powder comprising 10-90 wt. % of a pure metal or metal alloy; a second powder comprising a mineral; 13. A powder agglomerate, wherein the powder agglomerate comprises at least one morphology selected from the group consisting of porous agglomerates, hollow agglomerates, composite agglomerates, and hybrid agglomerates.

2. 2. The powder agglomerate of claim 1, wherein the powder agglomerate is a composite agglomerate having the first powder partially or completely encapsulated by the second powder.

3. 2. The powder agglomerate of claim 1, wherein the powder agglomerate is a hybrid agglomerate having the first powder partially or completely encapsulated by the second powder, the second powder comprising hollow pores.

4. The powder agglomerate of claim 1 , wherein the first powder comprises the metal alloy, the metal alloy being an aluminum alloy.

5. 5. The powder agglomerate of claim 4, wherein the aluminum alloy is an aluminum silicon alloy containing 6-20 wt. % Si.

6. 5. The powder agglomerate of claim 4, wherein the aluminum alloy is an aluminum silicon alloy containing 8-14 wt.% Si.

7. 2. The powder aggregate of claim 1, wherein the mineral is a silicate.

8. 8. The powder agglomerate of claim 7, wherein the silicate is a phyllosilicate or a talc.

9. 10. The powder agglomerate of claim 1 further comprising a different metal alloy.

10. 2. The powder agglomerate of claim 1, wherein the first powder comprises 10-40% by weight of a pure metal or metal alloy.

11. 2. The powder agglomerate of claim 1, wherein the first powder comprises 50-90% by weight of a pure metal or metal alloy.

12. 2. The powder agglomerate of claim 1, wherein the first powder comprises 60-90% by weight of a pure metal or metal alloy.

13. 1. A method for producing a powder agglomerate comprising the steps of: (a) blending at least one primary material, the primary material comprising a metal powder material, a non-metallic material, or a mixture of said metal powder and said non-metallic material, with liquid chemicals into a slurry mixture; (b) dispersing the slurry mixture obtained in (a) into a drying chamber through a high temperature gas flow of more than 150°C by an atomizer or spray nozzle; (c) obtaining said powder agglomerates by separating particles from said hot gas stream.

14. 14. The method for producing a powder agglomerate according to claim 13, wherein the metallic feedstock is an alloy.

15. 15. The method for producing a powder agglomerate of claim 14, wherein the alloy is an aluminum silicon alloy.

16. 14. The method for producing powder agglomerates according to claim 13, wherein the non-metallic raw material is a solid lubricant or a mineral.

17. 14. The method for producing a powder agglomerate of claim 13, wherein the liquid chemical is at least one of a solvent, a dispersant, and a binder.

18. 14. The method for producing a powder agglomerate of claim 13, wherein the powder agglomerate is produced without the use of a polymer or a fugitive phase.

19. 1. A method for producing an abradable sealing coating comprising:

13. A method comprising plasma spraying the powder agglomerate of claim 1 onto a turbine blade, a portion of a jet engine, or a portion of an automotive turbocharger.

20. 10. An abradable sealant coating comprising the powder agglomerate of claim 1.

21. 21. The abradable sealant coating of claim 20, wherein the abradable sealant coating contains a higher level of porosity compared to coatings from powders produced by conventional methods.

22. 21. The abradable sealant coating of claim 20, wherein the coating is free of a fugitive phase.

23. A turbine blade comprising the abradable sealant coating of claim 20.

24. 21. A portion of a jet engine comprising the abradable sealant coating of claim 20.