Propylene-Based Blend Compositions

JP2024544401AActive Publication Date: 2024-11-29EXXONMOBIL CHEMICAL PATENTS INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024536206
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-12-17
Filing Date
2022-12-14
Publication Date
2024-11-29
Estimated Expiration
2042-12-14

AI Technical Summary

Technical Problem

Conventional propylene-based elastomers fail to achieve a balanced combination of elasticity, stiffness, and flow properties, leading to issues such as pellet agglomeration and high handling costs in production facilities, and metallocene catalysts produce polymers with undesirable narrow molecular weight distributions and uniform comonomer distributions.

Method used

A propylene-based elastomer composition comprising a blend of a major polymer fraction with a molecular weight range of 100,000 to 300,000 and a minor fraction with 5,000 to 60,000, featuring a broad molecular weight distribution and comonomer distribution, achieved through a process involving two parallel reactors and a solvent-based polymerization method.

Benefits of technology

The blend exhibits improved properties like high modulus, stiffness, and flow, reduces pellet agglomeration, and allows for efficient production without the need for multiple polymers, enhancing the manufacturing process and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024544401000018
    Figure 2024544401000018
  • Figure 2024544401000019
    Figure 2024544401000019
  • Figure 2024544401000020
    Figure 2024544401000020
Patent Text Reader

Abstract

Higher M W The main polymer fraction has a lower M W A propylene-based elastomer composition comprising a major polymer fraction having a Mw of about 100,000 to about 300,000 and a melt flow rate according to ASTM D1238 of about 0.1 g / 10 min to about 70.0 g / 10 min, and a minor polymer fraction having a Mw of about 5,000 to about 60,000 and a Brookfield viscosity according to ASTM D-3236 (190°C) of about 500 cP to about 50,000 cP, wherein the amount of at least one other polyolefin comonomer in the minor polymer fraction is at least 7 wt% less than the amount of at least one other polyolefin comonomer in the major polymer fraction.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Polypropylenic resin composition

    JP2003073421A

  • Highly rigid polypropylene-based composition and production method

    JP2006045446A

  • Composition, laminated structure, and method for producing laminated structure

    JP2012188638A

  • Biaxially oriented polypropylene film

    JP2016030825A

  • Hot melt adhesive compositions based on propylene-based polymers and methods of using same

    JP2021502452A