Filler having blast furnace slag fine particles as main material

JP2025150469APending Publication Date: 2025-10-09TODA CORP
-1 Cites -1 Cited by

Patent Information

Application Number
JP2024051350
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-03-27
Publication Date
2025-10-09

Smart Images

  • Figure 2025150469000001_ABST
    Figure 2025150469000001_ABST
Patent Text Reader

Abstract

To provide a filler that can contribute to realization of a decarbonized society, and has blast furnace slag fine particles with excellent filling performance as a main material.SOLUTION: This filler is formed by using blast furnace slag fine particles and gypsum as a binder, and mixing bentonite as an admixture into the binder, where the concentration of bentonite to water is 5 to 8 mass%, and the addition rate of gypsum to the binder is 2 to 6 mass%. The content rate of sulfur trioxide contained in the binder is 1.4 to 2.4 mass%. The water-binder ratio is 100 to 150 mass%. Hemihydrate gypsum is used as the gypsum.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art