Manufacturing method for semiconductor devices

The method forms a modified layer within the substrate to control gas expansion, addressing deformation and crack issues, enabling precise semiconductor substrate division.

JP2026181758APending Publication Date: 2026-11-19DENSO CORP +3
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2025077392
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-07
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing methods for dividing semiconductor substrates using laser irradiation can result in gas accumulation, leading to substrate deformation and shape accuracy issues, as well as unintended cracks due to excessive gas generation.

Method used

A method involving the formation of a modified layer within the substrate with a laser focal point, followed by pressing and heating to expand gas within voids, allowing controlled division along a specific plane with an unmodified outer periphery, suppressing deformation and crack formation.

Benefits of technology

Enables precise and efficient division of semiconductor substrates by expanding gas within controlled voids, reducing deformation and crack risks, and allowing for easier substrate separation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026181758000001_ABST
    Figure 2026181758000001_ABST
Patent Text Reader

Abstract

This invention provides a technology that can appropriately divide a semiconductor substrate using laser irradiation when dividing a semiconductor substrate. [Solution] A semiconductor device manufacturing method comprises the steps of forming a modified layer inside a semiconductor substrate by irradiating the semiconductor substrate with a laser so as to form a focal point inside the semiconductor substrate, wherein the modified layer is formed along a specific surface that extends laterally within the semiconductor substrate by moving the focal point along that specific surface, and the modified layer is formed such that, when the semiconductor substrate is viewed from above, an unmodified region where no modified layer has been formed remains on the outer periphery of the semiconductor substrate; pressing and heating the irradiated area where the laser has been irradiated in the thickness direction of the semiconductor substrate; and dividing the semiconductor substrate along the specific surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The technology disclosed in the present specification relates to a method for manufacturing a semiconductor device.

[0002] Patent Document 1 discloses a technology for obtaining a thin semiconductor substrate by dividing a semiconductor substrate along its surface. In Patent Document 1, a modified layer is formed inside the semiconductor substrate by irradiating a laser focused inside the semiconductor substrate. The modified layer is formed to extend along the surface of the semiconductor substrate. Then, a force is applied to the upper surface of the semiconductor substrate in a direction away from the lower surface, so that the semiconductor substrate is divided along the modified layer. Thereby, a thinner semiconductor substrate can be obtained.

[0003] When forming the modified layer inside the semiconductor substrate, the crystal structure is disrupted by laser irradiation, and the atoms constituting the semiconductor are vaporized. The pressure of the generated gas may cause cracks in unintended directions inside the semiconductor substrate. In Patent Document 1, by heating the semiconductor substrate after forming the modified layer, the modified layer is melted, and the gas generated inside the semiconductor substrate is discharged from the end face of the semiconductor substrate to the outside together with the molten modified layer under the pressure of the gas.

Prior Art Documents

Patent Documents

[0004]

Patent Document 1

Summary of the Invention

Problems to be Solved by the Invention

[0005] In the technology described in Patent Document 1, the generated gas is discharged using its pressure. Depending on the size of the semiconductor substrate and the shape of the edge of the semiconductor substrate, the gas may not move sufficiently laterally, and some gas may remain inside the semiconductor substrate. As a result, the semiconductor substrate may deform, and the shape accuracy of the thin semiconductor substrate may decrease. In addition, depending on the laser irradiation conditions, excessive gas may be generated, causing unintended cracks in the semiconductor substrate. This specification provides a technology that can appropriately divide a semiconductor substrate using laser irradiation when dividing a semiconductor substrate. [Means for solving the problem]

[0006] A method for manufacturing a semiconductor device disclosed herein comprises the steps of forming a modified layer inside a semiconductor substrate by irradiating the semiconductor substrate with a laser such that a focal point is formed inside the semiconductor substrate, wherein the modified layer is formed along a specific surface extending laterally within the semiconductor substrate by moving the focal point along the specific surface, and the modified layer is formed such that, when the semiconductor substrate is viewed from above, an unmodified region where the modified layer is not formed remains on the outer periphery of the semiconductor substrate; pressing and heating the irradiated area where the laser has been irradiated in the thickness direction of the semiconductor substrate; and dividing the semiconductor substrate along the specific surface.

[0007] In this manufacturing method, first, a modified layer is formed inside the semiconductor substrate along a specific plane, such that an unmodified region remains on the outer periphery of the semiconductor substrate. At this time, gas is generated inside the modified layer, and voids are formed. Next, the irradiated area is pressed in the thickness direction of the semiconductor substrate and heated. This causes the generated gas to expand. The modified layer has lower mechanical strength than other semiconductor regions. Therefore, due to the expansion of the gas, the voids inside the modified layer connect with each other. Since an unmodified region remains on the outer periphery, the gas expands without being released from inside the semiconductor substrate. However, in this process, the semiconductor substrate is pressed in its thickness direction, so deformation of the semiconductor substrate due to gas expansion is suppressed. After that, the semiconductor substrate is divided. Since the voids inside the modified layer are connected, the semiconductor substrate can be easily divided along the specific plane. Therefore, this manufacturing method allows for more appropriate division of the semiconductor substrate than conventional methods. [Brief explanation of the drawing]

[0008] [Figure 1] Plan view of a semiconductor substrate. [Figure 2] Diagram illustrating the modified layer formation process. [Figure 3] Diagram illustrating the modified layer formation process. [Figure 4] Diagram illustrating the pressing and heating processes. [Figure 5] Diagram illustrating the process of forming the decomposition region. [Figure 6] Diagram illustrating the division process. [Figure 7] Diagram illustrating the polishing and pulverization process. [Figure 8] An explanatory diagram of a modified version of the modified layer formation process. [Figure 9] Diagram illustrating other variations of the modified layer formation process. [Figure 10] Diagram illustrating variations of the pressing and heating processes. [Figure 11] An explanatory diagram of a modified example of the decomposition region formation process. [Figure 12] An explanatory diagram of other variations of the decomposition region formation process. [Modes for carrying out the invention]

[0009] An example manufacturing method disclosed herein may further include, after the step of pressing and heating the semiconductor substrate in the thickness direction, and before the step of dividing the semiconductor substrate, a step of forming a decomposition region that extends from the top surface of the semiconductor substrate to the modified layer, along the boundary between the modified layer and the unmodified region, when the semiconductor substrate is viewed from above.

[0010] In this configuration, the semiconductor substrate can be more preferably divided along the decomposition region and the modified layer.

[0011] In one example of a manufacturing method disclosed herein, the step of forming the decomposition region may involve irradiating a laser along the boundary to form a modified region extending from the upper surface to the modified layer, and the modified region may be the decomposition region.

[0012] In this configuration, the formation of the modified layer and the formation of the modified region can be carried out by a single device.

[0013] In one example of a manufacturing method disclosed herein, the semiconductor substrate may be composed of a III-V semiconductor or gallium oxide.

[0014] (Examples) The manufacturing method of the embodiment will be described with reference to the drawings. Figure 1 is a plan view of a semiconductor substrate 2 on which a plurality of element structures 6 are arranged in a matrix. Each element structure 6 is formed on the first surface 2a side of the semiconductor substrate 2. Each element structure 6 includes, for example, structures for realizing the functions of a semiconductor device, such as trenches and gate electrodes. Inside the semiconductor substrate 2, structures having functions of transistors and diodes are respectively formed at positions corresponding to each element structure 6. The semiconductor substrate 2 is composed of a gallium nitride single crystal. Note that the semiconductor substrate 2 may be composed of other light-transmissive semiconductors (for example, III-V semiconductors such as aluminum nitride and gallium arsenide, gallium oxide, etc.). The semiconductor substrate 2 has a main portion 21 and an outer peripheral portion 22. The outer peripheral portion 22 is a region near the end face of the semiconductor substrate 2, and is a region where the element structure 6 is not formed. As shown in Figure 2 and the like, the semiconductor substrate 2 has a second surface 2b located on the back side of the first surface 2a.

[0015] The manufacturing method of the embodiment includes a modified layer forming step, a pressing and heating step, a decomposition region forming step, and a dividing step.

[0016] (Modified layer forming step) As shown in Figure 2, first, a mask 20 is formed on the second surface 2b of the semiconductor substrate 2. The mask 20 is formed to have an opening at the top of the main part 21 and to cover the outer peripheral part 22. Then, a modified layer formation process is carried out to form a modified layer 14 inside the semiconductor substrate 2. In the modified layer formation process, as shown in Figure 2, a laser 110 is irradiated onto the semiconductor substrate 2 from the second surface 2b side through the mask 20. The laser 110 is irradiated to form a focal point S1 in a predetermined depth range inside the semiconductor substrate 2. At the location of the focal point S1, gallium nitride is heated and decomposed, and nitrogen gas is generated. As a result, a void 15 filled with nitrogen gas is formed at the location of the focal point S1, and a modified layer 14 composed of a gallium precipitate layer, etc., is formed around the focal point S1. The strength of the modified layer 14 is lower than the strength of the original gallium nitride single crystal. Therefore, the strength of the modified layer 14 is lower than the strength of the surrounding gallium nitride single crystal. Here, as shown by arrow 120, the laser 110 is irradiated intermittently while moving the irradiation position of the laser 110 in a direction parallel to the first surface 2a and the second surface 2b of the semiconductor substrate 2. As a result, a modified layer 14 is formed along a specific surface (a surface parallel to the first surface 2a) that extends laterally within a predetermined depth range inside the semiconductor substrate 2, and discrete voids 15 are formed inside the modified layer 14. In addition, in this process, by moving the focal point S1 to scan the entire semiconductor substrate 2 as shown by the dashed arrow in Figure 3, the modified layer 14 is formed along the specific surface in almost the entire area not covered by the mask 20. That is, as shown in Figure 2, in the outer peripheral part 22 of the semiconductor substrate 2 covered by the mask 20, an unmodified region 24 remains where the modified layer 14 has not been formed. As described above, when gallium nitride is decomposed by irradiation of the semiconductor substrate 2 with the laser 110 (i.e., when the modified layer 14 is formed), nitrogen gas is generated and voids 15 are formed. Within the semiconductor substrate 2, voids 15 are formed so as to be distributed at intervals. The semiconductor region around the focal point of the laser 110 is modified by the heat of the laser 110. As a result, in the cross-section shown in Figure 2, the voids 15 are distributed discretely, while the semiconductor region located between adjacent voids 15 becomes a modified layer 14.In other words, in this process, a modified layer 14 is formed along a specific surface, and voids 15 are formed inside the modified layer 14. During the modified layer formation process, the laser irradiation conditions (e.g., energy density, pulse width, number of irradiations, pitch, etc.) are appropriately adjusted so as not to generate excessive nitrogen gas that could cause deformation of the semiconductor substrate 2.

[0017] (Pressing and heating process) Next, a pressing and heating step is performed. In the pressing and heating step, as shown in Figure 4, the entire semiconductor substrate 2 is pressed in the thickness direction by a pair of hot plates 34 so as to sandwich the semiconductor substrate 2 from the first surface 2a side and the second surface 2b side thereof. The pressure applied to the semiconductor substrate 2 is not particularly limited, and can be, for example, approximately 0.1 MPa to 0.5 MPa. Thereafter, the temperature of the hot plates 34 is raised to heat the semiconductor substrate 2. The heating temperature of the semiconductor substrate 2 is not particularly limited, and can be, for example, approximately 100°C to 300°C. In this step, the state where the semiconductor substrate 2 is pressed and heated is maintained for a predetermined time. The holding time is not particularly limited, and can be, for example, approximately 10 minutes to 30 minutes. By heating the semiconductor substrate 2, the nitrogen gas in the voids 15 expands. Since the unmodified region 24 remains in the outer peripheral portion 22, the nitrogen gas is not discharged from the semiconductor substrate 2 to the outside, and expands inside the semiconductor substrate 2. As described above, the mechanical strength of the modified layer 14 is lower than the mechanical strength of the surrounding semiconductor region. Therefore, when the nitrogen gas in the voids 15 expands, the partition walls between the plurality of voids 15 (that is, the partition walls constituted by the modified layer 14) are broken, and the plurality of voids 15 are connected to each other. As a result, as shown in Figure 4, the adjacent voids 15 are connected to each other in the lateral direction. In this step, the semiconductor substrate 2 is pressed in the thickness direction by the pair of hot plates 34. This suppresses deformation of the semiconductor substrate 2 due to the expansion of the nitrogen gas. In addition, since the semiconductor substrate 2 is pressed in the thickness direction, expansion of the voids 15 in the thickness direction is suppressed, and unintended cracks in the semiconductor substrate 2 are suppressed. When the pressing and heating step is completed, the semiconductor substrate 2 is cooled to room temperature. As a result, the expanded nitrogen gas contracts. Thereafter, the pressure applied to the semiconductor substrate 2 is released. This further suppresses deformation of the semiconductor substrate 2. In this step, it is sufficient to press and heat at least the irradiation range of the semiconductor substrate 2 irradiated with the laser 110. That is, the outer peripheral portion 22 does not need to be pressed and heated.

[0018] (Decomposition region forming step) Next, a decomposition region formation process is performed to form a decomposition region 26 inside the semiconductor substrate 2. In the decomposition region formation process, as shown in Figure 5, a laser 130 is irradiated onto the semiconductor substrate 2 from the first surface 2a side. The laser 130 is irradiated along the boundary 23 between the modified layer 14 and the unmodified region 24 (i.e., the boundary between the main part 21 and the outer peripheral part 22). In this process, the position of the focal point S2 of the laser 130 is moved to a depth that reaches the modified layer 14 from the first surface 2a, while moving around the boundary 23. As a result, a modified region 27 in which gallium nitride is decomposed is formed along the boundary 23 between the modified layer 14 and the unmodified region 24, in the range from the first surface 2a to the modified layer 14 of the semiconductor substrate 2. That is, a modified region 27 connecting the first surface 2a and the modified layer 14 is formed over the entire circumferential area of ​​the semiconductor substrate 2. In this embodiment, the formed modified region 27 is the decomposition region 26. In addition, the laser 130 irradiated onto the semiconductor substrate 2 in the decomposition region formation process may be a laser irradiated from the same apparatus as the laser 110 irradiated onto the semiconductor substrate 2 in the modification layer formation process.Hereinafter, of the two parts of the semiconductor substrate 2 that are demarcated by the modification layer 14 and the decomposition region 26, the part that does not include the second surface 2b will be referred to as the first part 8a, and the part that includes the second surface 2b will be referred to as the second part 8b.

[0019] (splitting process) Next, as shown in Figure 6, the semiconductor substrate 2 is divided along the modified layer 14 and the decomposition region 26. Here, the semiconductor substrate 2 is divided along the modified layer 14 and the decomposition region 26 by applying an external impact to the semiconductor substrate 2 while applying a force to the first portion 8a in a direction away from the second portion 8b. That is, the first portion 8a is separated from the second portion 8b. As described above, the modified layer 14 is not formed on the outer periphery 22 of the semiconductor substrate 2. However, a decomposition region 26 is formed between the first portion 8a and the second portion 8b, extending from the first surface 2a to the modified layer 14. The strength of the decomposition region 26 is lower than the strength of the gallium nitride single crystal, similar to the strength of the modified layer 14. Therefore, when a force is applied in a direction that pulls the first portion 8a away from the second portion 8b, the first portion 8a is easily peeled off from the second portion 8b in the modified layer 14 and the decomposition region 26. In particular, in the modified layer 14, the voids 15 are connected laterally by the pressing and heating processes, so the first portion 8a can be peeled off more easily from the second portion 8b.

[0020] (Polishing and fragmentation process) As described above, by dividing the semiconductor substrate into a first portion 8a and a second portion 8b, a thin first portion 8a can be obtained. Then, if necessary, the lower surface (i.e., the dividing surface) of the first portion 8a is polished and cleaned. Then, the first portion 8a is divided into individual pieces using known methods such as dicing with a laser or blade, so that each piece contains an element structure 6. This makes it possible to manufacture multiple semiconductor devices 10.

[0021] Furthermore, the second part 8b may be reused in the manufacture of semiconductor devices. For example, the thickness of the second part 8b can be increased back to its original thickness by polishing, etching, etc., the dividing surface of the second part 8b, and then epitaxially growing a gallium nitride layer on the dividing surface. The second part 8b with increased thickness can then be reused to manufacture semiconductor devices.

[0022] As described above, in the manufacturing method of this embodiment, first, a modified layer 14 is formed inside the semiconductor substrate 2 along a specific surface so that an unmodified region 24 remains on the outer periphery 22 of the semiconductor substrate 2. That is, in this step, the modified layer 14 is formed in the region of the semiconductor substrate 2 excluding the vicinity of the edge face. At this time, nitrogen gas is generated inside the modified layer 14, and voids 15 are formed. Next, the semiconductor substrate 2 is pressed in its thickness direction and heated. This causes the generated nitrogen gas to expand. The modified layer 14 has lower mechanical strength than other semiconductor regions. Therefore, due to the expansion of the nitrogen gas, the voids 15 inside the modified layer 14 connect with each other. Since an unmodified region 24 remains on the outer periphery 22, the nitrogen gas expands without being discharged from inside the semiconductor substrate 2. However, in this step, since the semiconductor substrate 2 is pressed in its thickness direction, deformation of the semiconductor substrate 2 due to the expansion of nitrogen gas is suppressed. After that, the semiconductor substrate 2 is divided. Since the voids 15 are connected within the modified layer 14, the semiconductor substrate 2 can be easily divided along a specific plane. Therefore, this manufacturing method allows for more appropriate division of the semiconductor substrate 2 than conventional methods.

[0023] Furthermore, in this manufacturing method, the nitrogen gas generated is expanded by heating the semiconductor substrate 2 after the modified layer 14 is formed. In other words, in this manufacturing method, the nitrogen gas generated in the modified layer 14 can be appropriately expanded by adjusting the heating temperature and heating time of the semiconductor substrate 2. Therefore, in the modified layer formation process, it is not necessary to irradiate with a laser under the harsh conditions of the conventional method, and the laser irradiation conditions can be relaxed compared to the conventional method. As a result, it is possible to suppress the generation of excessive nitrogen gas in the modified layer formation process, which could cause unintended cracks in the semiconductor substrate 2.

[0024] Furthermore, in the above-described embodiment, a decomposition region 26 is formed along the boundary 23 between the modified layer 14 and the unmodified region 24. Therefore, the semiconductor substrate 2 can be more preferably divided along the decomposition region 26 and the modified layer 14.

[0025] Furthermore, in the above-described embodiment, in the decomposition region formation step, the decomposition region 26 is formed by irradiating the area from the first surface 2a to the modified layer 14 with the laser 130 along the boundary 23. Therefore, the formation of the modified layer 14 and the formation of the decomposition region 26 can be carried out with a single device.

[0026] In the above-described embodiment, the decomposition region formation step does not need to be performed. Since the width of the outer peripheral portion 22 is very narrow relative to the size of the semiconductor substrate 2, the semiconductor substrate 2 can be suitably divided along the modified layer 14 even without forming the decomposition region 26.

[0027] Furthermore, in the above-described embodiment, the laser 110 was irradiated onto the semiconductor substrate 2 from the second surface 2b side during the modified layer formation process. However, a mask 20 may be formed on the first surface 2a, and the laser 110 may be irradiated onto the semiconductor substrate 2 from the first surface 2a side.

[0028] Furthermore, in the above-described embodiment, it is not necessary to form a mask 20 on the second surface 2b of the semiconductor substrate 2 during the modified layer formation process. In this case, for example, the focal point S1 can be moved to scan an area excluding the outer periphery 22, as shown by the dashed arrow in Figure 8. Also, the scanning direction of the laser 110 is not limited to the direction shown by the dashed arrow in Figure 3. For example, as shown by the dashed arrow in Figure 9, the focal point S1 may be moved along the circumferential direction of the semiconductor substrate 2 with respect to an area excluding the outer periphery 22 (an area closer to the center than the boundary 23).

[0029] Furthermore, in the above-described embodiment, in the pressing and heating process, only one of the first surface 2a and the second surface 2b of the semiconductor substrate 2 may be heated.

[0030] Furthermore, in the above-described embodiment, the semiconductor substrate 2 was heated by increasing the temperature of the heating plate 34 in contact with the semiconductor substrate 2 during the pressing and heating process. However, for example, as shown in Figure 10, the semiconductor substrate 2 may be pressed with a light-transmitting pressing member 36 and the nitrogen gas may be heated and expanded by irradiating it with ultraviolet or infrared light from a light source 38. Alternatively, for example, the nitrogen gas may be heated and expanded by flash lamp annealing. The gallium precipitated from the decomposition of gallium nitride has high light absorption properties, and the nitrogen gas can be heated efficiently by raising the temperature of this gallium.

[0031] Furthermore, in the above-described embodiment, the decomposition region 26 was formed by irradiation with a laser 130. However, for example, as shown in Figure 11, a groove 28 may be formed by dicing, extending from the first surface 2a to the modified layer 14 so as to encircle the boundary 23 between the modified layer 14 and the unmodified region 24. Alternatively, for example, as shown in Figure 12, a notch 30 may be formed by grinding, removing the outer peripheral portion 22 to the extent that the modified layer 14 is exposed. In these examples, the groove 28 and the notch 30 are examples of "decomposition regions."

[0032] Furthermore, in the embodiment described above, the element structure 6 was formed on the semiconductor substrate 2, but the element structure 6 does not necessarily have to be formed on the semiconductor substrate 2.

[0033] In addition, a beveled portion with an inclined surface may be provided near the edge of the semiconductor substrate 2. In the beveled portion, the laser's optical path is obstructed by reflection or refraction of the laser on the surface of the beveled portion, and the modified layer is not formed. For this reason, if the semiconductor substrate has a beveled portion, the laser 110 may be irradiated to scan the entire semiconductor substrate without forming a mask 20 during the modified layer formation process. In this case, the beveled portion becomes an unmodified region.

[0034] Although specific examples of the present invention have been described in detail above, these are merely illustrative and do not limit the scope of the claims. The technologies described in the claims include various modifications and changes to the specific examples illustrated above. The technical elements described in this specification or drawings exhibit technical usefulness individually or in various combinations, and are not limited to the combinations described in the claims at the time of filing. Furthermore, the technologies illustrated in this specification or drawings achieve multiple objectives simultaneously, and achieving even one of these objectives constitutes technical usefulness. [Explanation of Symbols]

[0035] 2: Semiconductor substrate, 2a: First surface, 2b: Second surface, 6: Device structure, 10: Semiconductor device, 14: Modified layer, 15: Void, 20: Mask, 21: Main part, 22: Peripheral part, 23: Boundary, 24: Unmodified region, 26: Decomposed region, 27: Modified region, 34: Heating plate, 110, 130: Laser

Claims

1. A method for manufacturing a semiconductor device (10), A step of forming a modified layer (14) inside a semiconductor substrate by irradiating the semiconductor substrate with a laser (110) such that a focal point (S1) is formed inside the semiconductor substrate, wherein the modified layer is formed along a specific surface by moving the focal point along a specific surface that extends laterally within the semiconductor substrate, and the modified layer is formed such that, when the semiconductor substrate is viewed from above, an unmodified region (24) where the modified layer is not formed remains on the outer periphery (22) of the semiconductor substrate. The process involves pressing and heating the irradiation area irradiated by the laser in the thickness direction of the semiconductor substrate, A step of dividing the semiconductor substrate along the specified surface, A manufacturing method that includes the following features.

2. The manufacturing method according to claim 1, further comprising the step of pressing and heating the semiconductor substrate in the thickness direction, and before the step of dividing the semiconductor substrate, forming a decomposition region (26) that extends from the upper surface (2a) of the semiconductor substrate to the modified layer, along the boundary (23) between the modified layer and the unmodified region, when the semiconductor substrate is viewed from above.

3. In the step of forming the decomposition region, a modified region (27) extending from the upper surface to the modified layer is formed by irradiating the boundary with a laser (130). The manufacturing method according to claim 2, wherein the modified region is the decomposition region.

4. The manufacturing method according to any one of claims 1 to 3, wherein the semiconductor substrate is composed of a group III-V semiconductor or gallium oxide.