Rechargeable battery and method for manufacturing a rechargeable battery
By incorporating protrusions on the electrode active material layers formed via a rolling process, the misalignment issue between separators and electrodes is resolved, improving the quality and performance of secondary batteries.
Patent Information
- Application Number
- JP2025077523
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-07
- Publication Date
- 2026-11-19
AI Technical Summary
Existing electrode assemblies and stacks experience misalignment between the separator and electrodes in directions intersecting the stacking direction, leading to potential issues with electrode integrity and performance.
The electrodes are designed with protrusions on their active material layers that protrude towards the separator, formed through a rolling process using a roller with recesses, ensuring precise alignment and minimizing misalignment during stacking.
This configuration effectively suppresses misalignment between the separator and electrodes, enhancing the quality and performance of the secondary battery by maintaining electrode integrity and ion flow efficiency.
Smart Images

Figure 2026181813000001_ABST
Abstract
Description
Technical Field
[0001] The technology disclosed in the present specification relates to a secondary battery and a method for manufacturing the secondary battery.
Background Art
[0002] Patent Document 1 discloses an electrode assembly for a secondary battery, which includes a plurality of positive electrode plates, a plurality of negative electrode plates, and a separator disposed between the plurality of positive electrode plates and the plurality of negative electrode plates. According to Patent Document 1, the separator is folded in a zigzag shape (folded in a serpentine manner), and the plurality of positive electrode plates and the plurality of negative electrode plates are alternately stacked in the folded sections of the separator.
[0003] Patent Document 2 discloses an electrode stack in which positive electrode plates each having a positive electrode current collector and negative electrode plates each having a negative electrode current collector are alternately stacked via a strip-shaped separator folded in a serpentine manner. According to Patent Document 2, in the process of obtaining each of the positive electrode plate and the negative electrode plate from a base material, burrs protruding to one side in the thickness direction are formed at each of the peripheral edge of the positive electrode current collector and the peripheral edge of the negative electrode current collector. In addition, the respective edges of the positive electrode active material coated on the positive electrode current collector and the negative electrode active material coated on the negative electrode current collector also protrude along with the formation of the burrs.
[0004] According to Patent Document 3, in the negative electrode plate, a coating start end raised portion is formed at the end of the negative electrode active material layer coated on the current collector.
Prior Art Documents
Patent Documents
[0005]
Patent Document 1
Patent Document 2
Patent Document 3
Summary of Invention
[0006] In electrode assemblies and electrode stacks as described above, a problem has been that relative misalignment occurs between the separator and the electrode in a direction intersecting the stacking direction of the electrode and separator. This specification provides a useful technique for suppressing such misalignment. [Means for solving the problem]
[0007] This specification discloses a secondary battery. The secondary battery comprises an electrode stack in which a plurality of electrodes, each having an electrode active material layer coated on at least one surface of a sheet-like current collector, are stacked in a first direction via a zigzag separator, wherein the electrode active material layer has a plurality of protrusions at positions away from the edge of the first surface, on a portion of the first surface facing the separator in the first direction, which protrude toward the separator.
[0008] According to the above configuration, each of the protrusions formed at multiple positions away from the edge on the first surface of the electrode active material layer bites into the separator. This makes it possible to suppress misalignment between the separator and the electrode.
[0009] This specification discloses a method for manufacturing a secondary battery. The method comprises a rolling step of rolling an electrode active material layer coated on an electrode current collector by pressing a cylindrical roller having at least one recess formed on its surface against the electrode active material layer, and a lamination step of stacking a plurality of electrodes, each having a plurality of protrusions formed on the electrode active material layer as a result of the at least one recess being pressed against it in the rolling step, via a zigzag-folded separator, thereby forming an electrode stack in which the plurality of electrodes are sandwiched between the separators with the protrusions protruding toward the separators. According to this method, a secondary battery in which misalignment between the separator and the electrodes is suppressed can be easily manufactured. [Brief explanation of the drawing]
[0010] [Figure 1] A simplified diagram showing an electrode sheet being roll-pressed, viewed from a perspective opposite one side of the electrode sheet. [Figure 2] Cross-sectional view of a secondary battery. [Figure 3] Decomposed perspective view of the electrode stack. [Figure 4] A diagram showing a magnified cross-section of a portion of a secondary battery. [Figure 5] A diagram showing the negative electrode from a viewpoint opposite the first surface of the negative electrode active material layer. [Figure 6] A diagram showing the negative and positive electrodes from the same viewpoint as in Figure 5. [Figure 7] This diagram shows an enlarged view of a cross-section of a secondary battery, illustrating an example where a protrusion is formed on the second surface. [Modes for carrying out the invention]
[0011] The main features of the embodiments described below are listed. These features can be combined in any way.
[0012] According to the secondary battery disclosed herein, the height of the protrusion from the first surface may be 10% or less of the thickness of the electrode active material layer excluding the protrusion. According to the above configuration, by setting the height of the protrusion to 10% or less of the thickness of the electrode active material layer excluding the protrusion, it is possible to suppress variations in the density of the active material in the electrode active material layer including the protrusion.
[0013] According to the secondary battery disclosed herein, the height of the protrusion from the first surface may be 20% or more of the thickness of the separator. According to the above configuration, by setting the height of the protrusion to 20% or more of the thickness of the separator, it is possible to appropriately ensure the amount of penetration of the protrusion into the separator.
[0014] According to the secondary battery disclosed herein, the protrusion may have a shape that tapers towards its tip. According to the above configuration, the protruding portions easily bite into the separator, so that misalignment between the separator and the electrode can be further suppressed.
[0015] According to the secondary battery disclosed in the present specification, the electrode laminate may be formed by alternately laminating the positive electrode as the electrode and the negative electrode as the electrode in the first direction with the separator interposed therebetween, wherein the size of the negative electrode in the plane orthogonal to the first direction is larger than that of the positive electrode, and the electrode active material layer applied to the current collector of the negative electrode is provided with the protruding portion in a range not overlapping with the positive electrode. According to the above configuration, since the protruding portion is formed in the range not overlapping with the positive electrode in the electrode active material layer of the negative electrode, the influence of the protruding portion on the ion flow between the electrodes is avoided.
[0016] According to the secondary battery disclosed in the present specification, the electrode active material layer may include the two protruding portions that are in a diagonal positional relationship within the first plane. According to the above configuration, the misalignment can be accurately suppressed with the minimum number of protruding portions.
[0017] According to the secondary battery disclosed in the present specification, the electrode active material layer may further include a protruding portion in which a part of a second surface facing the separator in a second direction intersecting the first direction protrudes toward the separator. According to the above configuration, the electrode active material layer includes, in addition to the protruding portion protruding from the first surface toward the separator, the protruding portion protruding from the second surface toward the separator. As a result, the misalignment between the separator and the electrode can be suppressed even more strongly.
[0018] Embodiments will be described with reference to the drawings. Each drawing is merely an example, and the present embodiment is not limited to the illustrated content. In addition, since each drawing is an example, a part thereof may be omitted.
[0019] Figure 1 shows a simplified view of an electrode sheet 2 being roll-pressed, from a viewpoint facing one side of the electrode sheet 2. The electrode sheet 2 comprises a long, sheet-like current collector 4 and an electrode active material layer 6 coated on at least one side of the current collector 4. The current collector 4 is a metal foil. The area of the current collector 4 coated with the electrode active material layer 6 is called the coated area 40. The area of the current collector 4 not coated with the electrode active material layer 6 is called the uncoated area 42. In Figure 1, the symbol D1 indicates the longitudinal direction D1 of the electrode sheet 2, and the symbol D2 indicates the width direction D2 of the electrode sheet 2, which is perpendicular to the longitudinal direction D1. According to Figure 1, the electrode sheet 2 has uncoated areas 42 at one end and the other end in the width direction D2.
[0020] As shown in Figure 1, a long roller 8 in the width direction D2 contacts the electrode sheet 2 being transported along the longitudinal direction D1. The roller 8 is a cylindrical component. To increase the density and uniformity of the electrode active material layer 6, the electrode sheet 2 is subjected to roll pressing with a predetermined pressing pressure using the roller 8. In roll pressing, the electrode active material layer 6 is rolled as the roller 8 rotates while being pressed against it. Roll pressing corresponds to the rolling process.
[0021] At least one recess 8a is formed on the surface of the roller 8. Therefore, a protrusion 18 corresponding to the shape of the recess 8a is formed on the electrode active material layer 6 against which the roller 8 is pressed. The recess 8a may be referred to as a depression, and the protrusion 18 may be referred to as a projection. As the roller 8 with the recess 8a rotates while pressed against the electrode active material layer 6, the protrusions 18 are repeatedly formed on the electrode active material layer 6 of the electrode sheet 2 as it is conveyed along the longitudinal direction D1. Figure 1 shows only some of the multiple protrusions 18 formed on the electrode active material layer 6.
[0022] In Figure 1, the size of one electrode 12 is illustrated by a dashed line. After roll pressing, the electrode sheet 2 is cut and separated into multiple electrodes 12 of the sizes shown in Figure 1, for example. Therefore, it can be understood that the electrode sheet 2 contains multiple electrodes 12, and each electrode 12 undergoes roll pressing (rolling process). In this embodiment, the size of each electrode 12 is not particularly limited, but it is assumed that as a result of roll pressing using the roller 8, multiple protrusions 18 are formed within the plane of the electrode active material layer 6 for each electrode 12.
[0023] The electrodes 12 are used as part of the configuration of the secondary battery 10, as shown in Figures 2 and 3. Figure 2 shows a simplified cross-section of the secondary battery 10. The secondary battery 10 is, for example, a rechargeable lithium-ion battery. The secondary battery 10 includes an electrode stack 16 formed by stacking multiple electrodes 12 in a first direction with a separator 14 in between them. Figure 3 shows a simplified exploded perspective view of the electrode stack 16. The electrodes 12 are a positive electrode 20 and a negative electrode 30.
[0024] The secondary battery 10 has a flexible outer casing (not shown), and an electrode stack 16 is sealed inside the casing. An electrolyte (not shown) is sealed inside the casing. The casing is, for example, a laminate sheet. In Figures 2 to 7, mutually orthogonal X, Y, and Z axes are shown for convenience of explanation. The Z-axis direction (Z-axis+ direction and Z-axis- direction) corresponds to the first direction. The first direction may also be called the stacking direction. Figure 2 is a cross-sectional view taken with a cross-section perpendicular to the Y-axis.
[0025] As shown in Figures 2 and 3, the electrode stack 16 is formed by alternately stacking substantially rectangular positive electrodes 20 and substantially rectangular negative electrodes 30 in a first direction via a strip-shaped separator 14 that is folded in a zigzag pattern, alternating between mountain and valley folds. In this case, each of the multiple positive electrodes 20 is sandwiched between one of the two surfaces of the separator 14, and each of the multiple negative electrodes 30 is sandwiched between the two surfaces of the separator 14. The positive electrodes 20 and negative electrodes 30 extend in the X-axis and Y-axis directions, respectively. With respect to the electrode 12, the Y-axis direction can be understood to correspond to the width direction D2 in Figure 1. The separator 14 is made of a material that has both permeability to allow the movement of charge carriers (in this case, lithium ions) during charging and discharging, and insulating properties to prevent short circuits caused by contact between the positive electrode 20 and the negative electrode 30. Examples of materials for the separator 14 include polypropylene and polyethylene.
[0026] According to Figure 3, the positive electrode 20 comprises a positive electrode current collector 22 and a positive electrode active material layer 24 coated on the positive electrode current collector 22. The positive electrode current collector 22 corresponds to an example of a current collector 4, and the positive electrode active material layer 24 corresponds to an example of an electrode active material layer 6. The positive electrode active material layer 24 is coated on both sides of the positive electrode current collector 22, for example. The positive electrode current collector 22 is, for example, aluminum foil. The positive electrode active material layer 24 contains a positive electrode active material. Examples of positive electrode active materials include lithium nickel-based composite oxide, lithium cobalt-based composite oxide, lithium manganese-based composite oxide, and the like.
[0027] The negative electrode 30 comprises a negative electrode current collector 32 and a negative electrode active material layer 34 coated on the negative electrode current collector 32. The negative electrode current collector 32 is an example of a current collector 4, and the negative electrode active material layer 34 is an example of an electrode active material layer 6. The negative electrode active material layer 34 is coated on both sides of the negative electrode current collector 32, for example. The negative electrode current collector 32 is, for example, copper foil. The negative electrode active material layer 34 contains a negative electrode active material. Examples of negative electrode active materials include carbon materials such as graphite, hard carbon, and soft carbon, materials that form alloys with lithium such as silicon (Si), and lithium alloys. The electrode active material may be composed of a single type of material or multiple types of materials. The electrode active material layer may contain conductive additives, binders, etc.
[0028] Each electrode 12 (positive electrode 20, negative electrode 30) has an unpainted portion 42 that protrudes in a direction intersecting the first direction. For example, the Y-axis direction (Y-axis+ direction and Y-axis- direction) corresponds to the direction intersecting the first direction. According to Figure 3, the unpainted portion 42 of the positive electrode 20 protrudes in the Y-axis+ direction, and the unpainted portion 42 of the negative electrode 30 protrudes in the Y-axis- direction. Although not shown in the figure, the unpainted portions 42 of each of the multiple positive electrodes 20 are electrically connected to the positive electrode terminals outside the range enclosed by the separator 14, for example, via current collection tabs. Similarly, although not shown in the figure, the unpainted portions 42 of each of the multiple negative electrodes 30 are electrically connected to the negative electrode terminals outside the range enclosed by the separator 14, for example, via current collection tabs.
[0029] Figure 4 shows a cross-section of a portion of the secondary battery 10, from the same viewpoint as Figure 2, but with greater magnification. In Figure 4, the negative electrode 30 is shown as the electrode 12. According to Figure 4, a negative electrode active material layer 34 is coated on both sides of the negative electrode current collector 32. As shown in Figure 4, the negative electrode active material layer 34 has a protrusion 34b on a portion of the first surface 34a facing the separator 14 in the first direction, which protrudes toward the separator 14. The protrusion 34b is an example of a protrusion 18. Hereinafter, the protrusion 34b will be referred to as the negative electrode protrusion 34b.
[0030] Figure 5 shows a single negative electrode 30 from a viewpoint facing the first surface 34a of the negative electrode active material layer 34. In Figure 5, the uncoated portion 42 of the negative electrode 30 is omitted, and only the coated portion 40 is shown. According to Figure 5, negative electrode protrusions 34b are formed on the first surface 34a at multiple positions away from the edge of the first surface 34a. In Figure 5, the edge of the first surface 34a refers to the two sides parallel to the X-axis direction and the two sides parallel to the Y-axis direction of the first surface 34a. According to Figure 5, there are two negative electrode protrusions 34b on the first surface 34a, and these two negative electrode protrusions 34b are, for example, diagonally opposite each other within the first surface 34a, which is roughly rectangular in shape and extends in the X-axis and Y-axis directions. The number of negative electrode protrusions 34b on the first surface 34a may be more than two.
[0031] In the configuration in which a negative electrode active material layer 34 is coated on both sides of the negative electrode current collector 32, each of the negative electrode active material layers 34 coated on both sides of the negative electrode current collector 32 has a first surface 34a that faces (contacts) the separator 14. Furthermore, the roll press described with reference to Figure 1 may be performed using a pair of rollers 8 that contact both sides of the electrode sheet 2 so as to sandwich the electrode sheet 2. The two rollers 8 constituting the pair may each have a recess 8a formed on their respective surfaces, or a recess 8a may be formed on only one of their surfaces. Therefore, for example, a plurality of negative electrode protrusions 34b that project toward the separator 14 are formed on each of the first surfaces 34a of the negative electrode active material layers 34 coated on both sides of the negative electrode current collector 32. Alternatively, a plurality of negative electrode protrusions 34b that project toward the separator 14 may be formed on only one of the first surfaces 34a of the negative electrode active material layer 34 coated on both sides of the negative electrode current collector 32.
[0032] The first surface of the positive electrode active material layer 24 of the positive electrode 20 that faces the separator 14 in a first direction may have a portion of the first surface that protrudes toward the separator 14, with a convex portion 18 (positive electrode convex portion) at multiple positions away from the edge of the first surface. In this embodiment, the description of the negative electrode convex portion 34b of the negative electrode active material layer 34 of the negative electrode 30 can be similarly applied to the positive electrode convex portion of the positive electrode active material layer 24 of the positive electrode 20.
[0033] As shown in Figures 2 and 3, the step of forming an electrode stack 16 by stacking multiple electrodes 12 via a zigzag-folded separator 14 corresponds to the stacking step. In the stacking step, multiple electrodes 12, each having multiple protrusions 18 formed on the electrode active material layer 6 by being pressed against by the recesses 8a of the roller 8 in the rolling step, are stacked via the separator 14. According to the stacking step, an electrode stack 16 is formed in which multiple electrodes 12 are each sandwiched between the separators 14 with the protrusions 18 protruding toward the separator 14. Thus, this embodiment discloses a method for manufacturing a secondary battery 10, which includes a rolling step and a stacking step.
[0034] In this embodiment, when the electrode 12 and the separator 14 are stacked in a first direction to form an electrode stack 16, the protrusions 18 formed at multiple positions away from the edge on the first surface of the electrode active material layer 6 bite into the separator 14. This prevents the electrode 12 from rotating relative to the separator 14 and suppresses misalignment between the separator 14 and the electrode 12. Therefore, the quality of the secondary battery 10 is improved. In this embodiment, the electrode 12 does not have protrusions (burrs) that project from the edge of the current collector toward the separator, as disclosed in Patent Document 2. Furthermore, the electrode 12 does not have protrusions that project from the edge of the electrode active material layer toward the separator, as disclosed in Patent Documents 2 and 3.
[0035] As shown in Figure 4, the negative electrode protrusion 34b has a shape that tapers towards its tip. As a result, the negative electrode protrusion 34b can easily bite into the separator 14, and the misalignment between the separator 14 and the electrode 12 is further suppressed.
[0036] Figure 4 shows the thickness T1 of the negative electrode active material layer 34, the height T2 of the negative electrode protrusion 34b from the first surface 34a, and the thickness T3 of the separator 14. Thickness T1 corresponds to the thickness of the electrode active material layer 6 excluding the protrusion 18. For example, thickness T1 is approximately 60 μm, and thickness T3 is approximately 12 μm. For example, height T2 is 10% or less of thickness T1. Also, for example, height T2 is 20% or more of thickness T3. By setting height T2 to 10% or less of thickness T1, variations in the density of the active material in the electrode active material layer 6 including the protrusion 18 can be suppressed. Furthermore, by setting height T2 to 20% or more of thickness T3, the amount of penetration of the protrusion 18 into the separator 14 can be appropriately ensured. Furthermore, assuming a configuration in which the positive electrode active material layer 24 and the negative electrode active material layer 34 are in contact with both sides of the separator 14, and protrusions 18 project toward the separator 14 from the positive electrode active material layer 24 and the negative electrode active material layer 34 respectively, it is preferable that the height T2 is less than 50% of the thickness T3.
[0037] Figure 6 shows the negative electrode 30 with a solid line from the same viewpoint as in Figure 5. In Figure 6, the positive electrode 20, which is stacked with the negative electrode 30 via the separator 14, is shown with a dashed line. Similar to Figure 5, only the coated portion 40 of the negative electrode 30 is shown in Figure 6. Also in Figure 6, the uncoated portion 42 of the positive electrode 20 is omitted, and only the coated portion 40 is shown. The size of the negative electrode 30 in the plane perpendicular to the first direction (Z axis direction) (X-Y plane) is larger than that of the positive electrode 20. In other words, when viewed from the viewpoint in Figure 6, the range of the coated portion 40 of the positive electrode 20 is contained within the range of the coated portion 40 of the negative electrode 30. In such a configuration, as shown in Figure 6, the negative electrode active material layer 34 of the negative electrode 30 may have a negative electrode protrusion 34b in a range that does not overlap with the positive electrode 20. This prevents the negative electrode protrusion 34b from influencing the ion flow between the positive electrode 20 and the negative electrode 30.
[0038] As described above, a protrusion 18 (positive electrode protrusion) may be formed on the positive electrode active material layer 24 of the positive electrode 20. Figure 6 shows a plurality of positive electrode protrusions 24b formed on the first surface 24a of the positive electrode active material layer 24 facing the separator 14. The position of the positive electrode protrusions 24b is preferably close to the edge of the positive electrode active material layer 24 (but not at the edge) so as to have as little influence as possible on the ion flow between the positive electrode 20 and the negative electrode 30.
[0039] Furthermore, as seen from the viewpoint in Figure 6, the negative electrode protrusion 34b and the positive electrode protrusion 24b are formed at offset positions from each other. Each of the negative electrode protrusion 34b and the positive electrode protrusion 24b bites into the separator 14. Therefore, because the negative electrode protrusion 34b and the positive electrode protrusion 24b are formed at offset positions from each other, it is possible to reduce poor biting of each of the negative electrode protrusion 34b and the positive electrode protrusion 24b into the separator 14.
[0040] The electrode active material layer 6 may further include a convex portion on a second surface facing the separator 14 in a second direction intersecting the first direction, which protrudes toward the separator 14. The X and Y axis directions, which are perpendicular to the first direction, the Z axis direction, are each one of the directions that intersect the first direction. Here, the X axis direction (X-axis + direction and X-axis - direction) is considered the second direction intersecting the first direction, and the Y axis direction (Y-axis + direction and Y-axis - direction) is considered the third direction intersecting the first and second directions.
[0041] According to Figures 2 and 3, the positive electrode 20 and the negative electrode 30 are sandwiched between the separator 14 in the Z-axis direction, but not sandwiched between the separator 14 in the Y-axis direction. The positive electrode 20 does not face the separator 14 in the X-axis+ direction, but faces the bent portion of the separator 14 in the X-axis- direction. On the other hand, the negative electrode 30 faces the bent portion of the separator 14 in the X-axis+ direction, but does not face the separator 14 in the X-axis- direction. Therefore, for the positive electrode 20, the side facing the X-axis- direction corresponds to the second surface. On the other hand, for the negative electrode 30, the side facing the X-axis+ direction corresponds to the second surface.
[0042] Figure 7 shows a magnified view of a portion of the secondary battery 10, similar to Figure 4. In Figure 7, as in Figure 4, the negative electrode 30 is shown as the electrode 12. In Figure 7, the side surface of the negative electrode active material layer 34 that faces the separator 14 in the X-axis + direction is the second surface 34c. The second surface 34c can be said to be the surface corresponding to the thickness T1 of the negative electrode active material layer 34. According to Figure 7, a protrusion 34d is formed on the second surface 34c that projects toward the separator 14. There may be multiple protrusions 34d. By the protrusions 34d biting into the opposing separator 14 or interfering with the separator 14, the misalignment between the separator 14 and the electrode 12 can be suppressed even more strongly. Similarly, a protrusion projecting toward the separator 14 may be formed on the side surface (second surface) of the positive electrode active material layer 24 of the positive electrode 20 that faces the separator 14 in the X- direction.
[0043] The specific examples of the technologies disclosed herein have been described in detail above, but these are merely illustrative and do not limit the scope of the claims. The technologies described in the claims include various modifications and changes to the specific examples described above. Furthermore, the technical elements described herein or in the drawings exhibit technical usefulness individually or in various combinations, and are not limited to the combinations described in the claims at the time of filing. In addition, the technologies illustrated herein or in the drawings achieve multiple objectives simultaneously, and achieving even one of these objectives constitutes technical usefulness in itself. [Explanation of Symbols]
[0044] 2: Electrode sheet, 4: Current collector, 6: Electrode active material layer, 8: Roller, 8a: Recess, 10: Secondary battery, 12: Electrode, 14: Separator, 16: Electrode stack, 18: Protrusion, 20: Positive electrode, 22: Positive electrode current collector, 24: Positive electrode active material layer, 24a: First surface, 24b: Positive electrode protrusion, 30: Negative electrode, 32: Negative electrode current collector, 34: Negative electrode active material layer, 34a: First surface, 34b: Negative electrode protrusion, 34c: Second surface, 34d: Protrusion, 40: Coated part, 42: Uncoated part
Claims
1. It is a secondary battery, The electrode laminate comprises a plurality of electrodes, each having an electrode active material layer coated on at least one surface of a sheet-like current collector, stacked in a first direction via a zigzag-folded separator. A secondary battery wherein the electrode active material layer has a portion of the first surface facing the separator in the first direction, with a number of protrusions projecting toward the separator at positions away from the edge of the first surface.
2. The secondary battery according to claim 1, wherein the height of the protrusion from the first surface is 10% or less of the thickness of the electrode active material layer excluding the protrusion.
3. The secondary battery according to claim 1, wherein the height of the protrusion from the first surface is 20% or more of the thickness of the separator.
4. The secondary battery according to claim 1, wherein the convex portion has a shape that tapers towards its tip.
5. The electrode stack is formed by alternately stacking the positive electrode and the negative electrode in a first direction with the separator between them. In the plane perpendicular to the first direction, the size of the negative electrode is larger than that of the positive electrode. The secondary battery according to claim 1, wherein the electrode active material layer coated on the current collector of the negative electrode has the protrusions in a region that does not overlap with the positive electrode.
6. The secondary battery according to claim 1, wherein the electrode active material layer comprises two protrusions that are diagonally opposite each other in the first plane.
7. The secondary battery according to claim 1, wherein the electrode active material layer further comprises a convex portion on a second surface facing the separator in a second direction intersecting the first direction, the convex portion projecting toward the separator.
8. A method for manufacturing a secondary battery as described in claim 1, A rolling step in which a cylindrical roller having at least one recess formed on its surface is pressed against the electrode active material layer coated on the current collector of the electrode, thereby rolling the electrode active material layer, A method comprising a lamination step of stacking a plurality of electrodes, each having a plurality of protrusions formed on the electrode active material layer by pressing the at least one recess against it in the rolling step, via a zigzag-folded separator, thereby forming an electrode stack in which the plurality of electrodes are sandwiched between the separators with the protrusions protruding toward the separators.
Citation Information
Patent Citations
Negative electrode plate and nonaqueous electrolyte secondary battery using negative electrode plate
JP2001015103A
Secondary battery and manufacturing method of secondary battery
JP2021111538A
Electrode assembly for secondary battery, manufacturing method thereof, and lithium secondary battery comprising same