Arc welding control method and arc welding apparatus
The arc welding control method stabilizes welding current by limiting the ON period of the inverter circuit, addressing sudden arc length increases and ensuring consistent heat input for improved welding quality with high inert gas ratios.
Patent Information
- Application Number
- JP2025077697
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-08
- Publication Date
- 2026-11-19
AI Technical Summary
Conventional arc welding methods using high inert gas ratios result in sudden increases in arc length and decreases in welding current, leading to poor welding quality due to cathode spot formation away from the wire and fluctuations in heat input.
An arc welding control method that limits the ON period of the inverter circuit to maintain a lower limit ratio, preventing sharp decreases in welding current by setting a lower limit current value based on welding wire diameter and inert gas ratio, using a shielding gas with 90% or more inert gas.
The method effectively suppresses sudden decreases in welding current, maintaining consistent heat input and improving welding quality by stabilizing the arc length during spray transfer.
Smart Images

Figure 2026181895000001_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present invention relates to an arc welding control method and an arc welding apparatus capable of improving the welding state in a spray transfer mode. BACKGROUND ART
[0002] Arc welding methods and arc welding apparatuses for feeding a welding wire to weld carbon steel, stainless steel, aluminum and the like are in use. In the arc welding method, when the average value of the welding current is equal to or higher than a predetermined value, the droplet transfer state becomes a globular transfer mode or a spray transfer mode. In this state, short circuits between the welding wire and the base material hardly occur, and the arc period continues. During the arc period, the arc length may suddenly increase due to disturbances such as fluctuations in the feeding speed, irregular movement of the molten pool, and fluctuations in cathode spots formed on the oxide film. Since the arc welding apparatus is controlled at a constant voltage, when the arc length increases and the welding voltage rises, the welding current sharply decreases. After that, when the disturbance disappears and the arc length returns to its original state, the welding current gradually increases and returns to the original state. During the period when the welding current is decreasing, the heat input to the base material decreases, so the penetration depth, bead appearance and the like fluctuate, leading to degraded welding quality.
[0003] To address the above-mentioned problem, the invention disclosed in Patent Document 1 suppresses the decrease of the welding current by limiting the rate of change of the welding current when a variation that sharply increases the arc length occurs. PRIOR ART DOCUMENTS PATENT DOCUMENTS
[0004] PATENT DOCUMENT 1 Japanese Unexamined Patent Publication No. 2004-181526 SUMMARY OF THE INVENTION PROBLEMS TO BE SOLVED BY THE INVENTION
[0005] When arc welding is performed using a shielding gas with a ratio of 90% or more of inert gas such as argon or helium, and droplet transfer is performed in a spray transfer state, a cathode spot may form on the oxide film away from directly beneath the welding wire. In this state, the arc length increases instantaneously, causing a sharp increase in welding voltage, and consequently a sharp decrease in welding current. Because the position of the cathode spot moves at high speed and the arc length increases instantaneously, the conventional technology described in Patent Document 1 could not adequately suppress the sharp decrease in welding current. As a result, there was a problem of poor welding quality.
[0006] Therefore, the present invention aims to provide an arc welding control method and an arc welding apparatus that can obtain good welding quality by suppressing a sudden decrease in welding current caused by the formation of the cathode point at a position away from directly below the wire and the instantaneous increase in arc length when performing arc welding by droplet transfer in a spray transfer state using a shielding gas with an inert gas ratio of 90 volume% or more. [Means for solving the problem]
[0007] An arc welding control method provided by a first aspect of the present invention is an arc welding control method in which a welding wire is fed, a welding current is supplied by an inverter circuit to control the output, and welding is performed by transferring molten droplets in a spray transfer state, wherein when the ratio of inert gas to shielding gas is 90 volume% or more, the ratio of the ON period of the inverter circuit is limited so as not to fall below a lower limit ratio.
[0008] In a preferred embodiment of the present invention, the lower limit ratio is set so that the welding current value does not fall below the lower limit current value.
[0009] In a preferred embodiment of the present invention, the lower limit current value is set to a value obtained by subtracting a reduction value from the set value or average value of the welding current.
[0010] In a preferred embodiment of the present invention, the reduction value is set according to the diameter of the welding wire.
[0011] In a preferred embodiment of the present invention, the reduction value is set according to the ratio of the inert gas.
[0012] An arc welding apparatus provided by a second aspect of the present invention is an arc welding apparatus that feeds a welding wire, controls the output of an inverter circuit to supply a welding current, and performs welding by transferring molten metal in a spray transfer state, wherein when the ratio of inert gas to shielding gas is 90 volume% or more, the ratio of the ON period of the inverter circuit is limited so as not to fall below a lower limit ratio. [Effects of the Invention]
[0013] In this invention, when using a shielding gas with an inert gas ratio of 90% by volume or more and performing arc welding by droplet transfer in a spray transfer state, it is possible to suppress the sharp decrease in welding current caused by the cathode point being formed at a position away from directly below the wire and the arc length instantaneously increasing, thereby obtaining good welding quality. [Brief explanation of the drawing]
[0014] [Figure 1] This is a block diagram of an arc welding apparatus according to an embodiment of the present invention. [Figure 2] Figure 1 shows a timing chart of each signal in an arc welding apparatus illustrating an arc welding control method according to an embodiment of the present invention. [Modes for carrying out the invention]
[0015] Embodiments of the present invention will be described below with reference to the drawings.
[0016] Figure 1 is a block diagram of an arc welding apparatus according to an embodiment of the present invention. Each block will be described below with reference to this figure.
[0017] The main power supply circuit MC takes a commercial power supply such as 3-phase 200V (not shown) as input and performs output control such as inverter control according to the on-period ratio limiting signal Oc, which will be described later, and outputs the welding voltage Vw and welding current Iw. This main power supply circuit MC, although not shown, includes a primary rectifier circuit that rectifies the commercial power supply, a capacitor that smooths the rectified DC, an inverter circuit driven by the on-period ratio limiting signal Oc that converts the smoothed DC to high-frequency AC, an inverter transformer that steps down the high-frequency AC, a secondary rectifier circuit that rectifies the stepped-down high-frequency AC, and a reactor that smooths the rectified DC.
[0018] A welding voltage Vw is applied between the welding wire 1 and the base material 2, a welding current Iw is passed through, and a shielding gas (not shown in the diagram) is ejected to generate an arc 3. As the shielding gas, a gas with an inert gas ratio of 90% or more by volume, such as argon or helium, is used. When the material of the base material 2 is carbon steel, a mixed gas with an inert gas ratio of 90-95% by volume and the remainder being carbon dioxide is used. When the material of the base material 2 is stainless steel, a mixed gas with an inert gas ratio of 95-98% by volume and the remainder being oxygen is used. When the material of the base material 2 is aluminum, a gas with an inert gas ratio of 100% by volume is used.
[0019] The voltage detection circuit VD detects the welding voltage Vw and outputs a voltage detection signal Vd. The current detection circuit ID detects the welding current Iw and outputs a current detection signal Id.
[0020] The voltage setting circuit VR outputs a predetermined voltage setting signal Vr. The voltage error amplification circuit EV takes the above voltage setting signal Vr and the above voltage detection signal Vd as input, amplifies the error between the two values, and outputs a voltage error amplification signal Ev.
[0021] The welding current setting circuit IAR outputs a predetermined welding current setting signal Iar for setting the average value of the welding current Iw that is equal to or greater than the critical current value at which droplet transfer enters a spray transfer state. The welding current average value detection circuit IAD receives the aforementioned current detection signal Id as input, calculates the average value of the current detection signal Id, and outputs a welding current average value detection signal Iad.
[0022] The reduction value setting circuit DR outputs a reduction value setting signal Dr set by the following 1) and 2). 1) The value of the reduction value setting signal Dr is set according to the diameter of the welding wire. For example, the reference reduction value (50A) is defined for a welding wire diameter of 1.2mm; when the diameter is 1.0mm, the value is obtained by subtracting 10A from the reference reduction value, and when the diameter is 1.6mm, the value is obtained by adding 10A to the reference reduction value. 2) The value of the reduction value setting signal Dr is set according to the ratio of the inert gas. For example, Dr = Dr set in the above 1) + (inert gas ratio - 90). When the welding wire diameter is 1.2mm, Dr = 50A, so when the inert gas ratio is 90% by volume, Dr = 50A, and when it is 100% by volume, Dr = 60A.
[0023] The lower limit current value setting circuit IR receives the aforementioned welding current setting signal Iar, the aforementioned welding current average value detection signal Iad, and the aforementioned reduction value setting signal Dr as inputs, performs an operation of either Ir = Iar - Dr or Ir = Iad - Dr, and outputs a lower limit current value setting signal Ir.
[0024] The lower limit ratio setting circuit BR receives the aforementioned lower limit current value setting signal Ir as input, and outputs a lower limit ratio setting signal Br that is set according to the value of the lower limit current value setting signal Ir. The value of the lower limit ratio setting signal Br is set to a larger value (approximately 25 to 35%) as the value of the lower limit current value setting signal Ir increases.
[0025] The pulse width modulation circuit PWM receives the aforementioned voltage error amplification signal Ev as input, performs pulse width modulation control, and outputs a pulse width modulation signal Pwm.
[0026] The ON-period ratio limiting circuit OC takes the lower limit ratio setting signal Br and the pulse width modulation signal Pwm as inputs and limits the ON-period ratio of the pulse width modulation signal Pwm so that it does not fall below the value of the lower limit ratio setting signal Br, and outputs an ON-period ratio limiting signal Oc. The ON-period ratio of the pulse width modulation signal Pwm has a maximum value of 95% considering the dead time, so if there is no limit, it will vary in the range of 0 to 95%. Therefore, if the value of the lower limit ratio setting signal Br is 25%, the value of the ON-period ratio limiting signal Oc will vary in the range of 25 to 95%.
[0027] The feed speed setting circuit FR takes the welding current setting signal Iar as input and outputs a feed speed setting signal Fr that corresponds to the value of the welding current setting signal Iar.
[0028] The feed control circuit FC takes the feed speed setting signal Fr as input and outputs a feed control signal Fc for feeding the welding wire 1 at the value of the feed speed setting signal Fr.
[0029] The feeder WF is equipped with a feed motor and, taking the above-mentioned feed control signal Fc as input, feeds the welding wire 1 through the welding torch 4 to the base material 2. The feeding speed of the welding wire 1 is the value of the above-mentioned feed speed setting signal Fr.
[0030] The welding torch 4 guides the welding wire 1 into the base material 2 and supplies power to the welding wire 1 via a power supply tip (not shown in the figure).
[0031] Figure 2 is a timing chart of each signal in the arc welding apparatus shown in Figure 1, illustrating an arc welding control method according to an embodiment of the present invention. Figure (A) shows the time variation of the welding current Iw, and Figure (B) shows the time variation of the welding voltage Vw. The operation of each signal will be explained below with reference to the same figure.
[0032] The welding current setting signal Iar in Figure 1 sets the average value of the welding current Iw that is greater than or equal to the critical current value at which droplet transfer becomes spray transfer. During the period before time t1, as shown in Figure (A), the welding current Iw has a waveform that is almost constant with slight fluctuations up and down, and as shown in Figure (B), the welding voltage Vw also has a waveform that is almost constant with slight fluctuations up and down.
[0033] At time t1, the arc length instantaneously increases because the cathode point is formed on the oxide film away from directly beneath the wire, and the welding voltage Vw increases as shown in Figure (B). Consequently, the welding current Iw decreases sharply as shown in Figure (A). At time t2, as shown in Figure (A), when the welding current Iw decreases to the value of the lower limit current value setting signal Ir in Figure 1, the ratio of the on period of the pulse width modulation signal Pwm in Figure 1 becomes less than the value of the lower limit ratio setting signal Br in Figure 1. Therefore, the ratio of the on period of the on period limiting signal Oc in Figure 1 is limited so as not to fall below the value of the lower limit ratio setting signal Br. This on period ratio limiting signal Oc drives the inverter circuit in the power supply main circuit MC in Figure 1 and controls the output, so as shown in Figure (A), the value of the welding current Iw is limited so as not to fall below the value of the lower limit current value setting signal Ir. As a result, in this embodiment, it is possible to suppress the welding current Iw from decreasing drastically and resulting in poor welding quality. The value of the lower limit current setting signal Ir is obtained by subtracting the value of the reduction value setting signal Dr in Figure 1 from the value of the welding current setting signal Iar or the welding current average value detection signal Iad in Figure 1. The value of the reduction value setting signal Dr is set to an appropriate value according to the diameter of the welding wire 1 and / or the inert gas ratio.
[0034] At time t3, the cathode point returns to the oxide film near the wire, shortening the arc length, and as shown in Figure (B), the welding voltage Vw returns to its value before time t1. Consequently, as shown in Figure (A), the welding current Iw gradually increases from time t3 back to its value before time t1.
[0035] The effects of this embodiment will now be explained. According to this embodiment, in an arc welding control method in which welding wire is fed, the output is controlled by an inverter circuit to supply welding current, and welding is performed by droplet transfer in a spray transfer state, when the ratio of inert gas in the shielding gas is 90 volume% or more, the ratio of the ON period of the inverter circuit is limited so as not to fall below a lower limit ratio. In the conventional technology, when arc welding is performed using a shielding gas with an inert gas ratio of 90 volume% or more and droplet transfer in a spray transfer state, a cathode point may be formed on the oxide film away from directly below the welding wire. When this occurs, the arc length increases instantaneously, causing a rapid increase in welding voltage, and consequently the welding current to drop sharply, resulting in poor welding quality. In this embodiment, the output is controlled so that the ratio of the ON period of the inverter circuit does not fall below a lower limit ratio, so the sharp decrease in welding current can be suppressed. As a result, the decrease in heat input to the base material can be suppressed, and poor welding quality can be prevented.
[0036] More preferably, according to this embodiment, the lower limit ratio is set so that the welding current value does not fall below the lower limit current value. In this way, even if the arc length increases and the welding current decreases sharply, the ratio of the ON period of the inverter circuit is limited so that the value does not fall below the predetermined lower limit current value, thereby preventing deterioration of welding quality.
[0037] More preferably, according to this embodiment, the lower limit current value is set to a value obtained by subtracting a reduction value from the set value or average value of the welding current. If the lower limit current value is greater than the appropriate value, the fluctuation of the welding current will be excessively restricted, resulting in an unstable welding state. If the lower limit current value is less than the appropriate value, the sudden decrease in the welding current cannot be sufficiently suppressed, resulting in poor welding quality. In this embodiment, the lower limit current value is set to a value obtained by subtracting a reduction value from the set value of the welding current for which the average value is set, or from the detected average value of the welding current. In this way, since the lower limit current value is set based on the average value of the welding current, the lower limit current value can be set to an appropriate value.
[0038] More preferably, according to this embodiment, the reduction value is set according to the diameter of the welding wire. If the diameter of the welding wire is different, the appropriate reduction value will be different. In this embodiment, since the reduction value is optimized according to the diameter of the welding wire, the lower limit current value becomes appropriate, and the welding quality can be improved.
[0039] More preferably, according to this embodiment, the reduction value is set according to the ratio of inert gas. If the ratio of inert gas is different, the appropriate value of the reduction value will be different. In this embodiment, since the reduction value is optimized according to the ratio of inert gas, the lower limit current value becomes appropriate, and the welding quality can be improved.
[0040] Furthermore, according to this embodiment, in an arc welding apparatus that feeds a welding wire, controls the output of an inverter circuit to supply a welding current, and performs welding by transferring molten metal in a spray transfer state, when the ratio of inert gas to shielding gas is 90 volume percent or more, the ratio of the ON period of the inverter circuit is limited so as not to fall below the lower limit ratio. The arc welding apparatus according to this embodiment provides the above-mentioned effects. [Explanation of symbols]
[0041] 1: Welding wire, 2: Base metal, 3: Arc, 4: Welding torch, BR: Lower limit ratio setting circuit, Br: Lower limit ratio setting signal, DR: Decrease value setting circuit, Dr: Decrease value setting signal, EV: Voltage error amplification circuit, Ev: Voltage error amplification signal, FC: Feeding control circuit, Fc: Feeding control signal, FR: Feeding speed setting circuit, Fr: Feeding speed setting signal, IAD: Welding current average value detection circuit, Iad: Welding current average value detection signal, IAR: Welding current setting circuit Iar: Welding current setting signal, ID: Current detection circuit, Id: Current detection signal, IR: Lower limit current value setting circuit, Ir: Lower limit current value setting signal, Iw: Welding current, MC: Power supply main circuit, OC: On-period ratio limiting circuit, Oc: On-period ratio limiting signal, PWM: Pulse width modulation circuit, Pwm: Pulse width modulation signal, VD: Voltage detection circuit, Vd: Voltage detection signal, VR: Voltage setting circuit, Vr: Voltage setting signal, Vw: Welding voltage, WF: Feeder
Claims
1. In an arc welding control method in which welding wire is fed, the output is controlled by an inverter circuit to supply welding current, and welding is performed by transferring molten droplets in a spray transfer state, When the ratio of inert gas to shielding gas is 90% by volume or more, the ratio of the ON period of the inverter circuit is limited so as not to fall below the lower limit ratio. An arc welding control method characterized by the following:
2. The lower limit ratio is set so that the welding current value does not fall below the lower limit current value. The arc welding control method according to feature 1.
3. The lower limit current value is set to a value obtained by subtracting a reduction value from the set value or average value of the welding current. The arc welding control method according to feature 2.
4. The aforementioned reduction value is set according to the diameter of the welding wire. The arc welding control method according to feature 3.
5. The aforementioned reduction value is set according to the ratio of the inert gas. The arc welding control method according to feature 3.
6. In an arc welding apparatus that feeds welding wire, controls the output of an inverter circuit to supply welding current, and performs welding by transferring molten droplets in a spray transfer state, When the ratio of inert gas to shielding gas is 90% by volume or more, the ratio of the ON period of the inverter circuit is limited so as not to fall below the lower limit ratio. An arc welding apparatus characterized by the following features.
Citation Information
Patent Citations
Method for controlling output of welding power source device
JP2004181526A