Feed containing wood kraft pulp

Crushing wood kraft pulp to 15 mm and mixing with molasses addresses the low specific gravity and nutrient deficiencies, resulting in a palatable and easily handled feed that enhances livestock productivity.

JP2026181938APending Publication Date: 2026-11-19NIPPON PAPER IND CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2025077771
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-08
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Wood kraft pulp has low specific gravity, limiting its widespread use due to transportation costs and is difficult to handle and palatable for ruminants, lacking essential nutrients like protein, fat, and minerals, which hinders its effectiveness as animal feed.

Method used

Crushing wood kraft pulp sheets to a size that can pass through a 15 mm mesh and mixing with molasses to achieve a bulk density of 0.15-0.5 g/cm³, enhancing palatability and handling properties while supplementing nutrients.

Benefits of technology

The resulting feed has improved texture and palatability, easy handling, and increased nutritional value, promoting effective use in livestock farming by mixing with other feed ingredients and improving milk fat content in ruminants.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026181938000003
    Figure 2026181938000003
  • Figure 2026181938000004
    Figure 2026181938000004
  • Figure 2026181938000001
    Figure 2026181938000001
Patent Text Reader

Abstract

The object of this invention is to provide a technology for efficiently producing animal feed from wood kraft pulp sheets. [Solution] By crushing wood kraft pulp sheets to a specific size and then adding molasses, it is possible to produce an excellent feed containing wood kraft pulp.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] This invention relates to a technology for producing feed containing wood kraft pulp. [Background technology]

[0002] In ruminant feed, fibrous raw materials such as beet pulp, bamboo, and wood kraft pulp are used to properly maintain microbial fermentation in the rumen. For example, Patent Document 1 discloses a ruminant feed containing wood kraft pulp. [Prior art documents] [Patent Documents]

[0003] [Patent Document 1] Japanese Patent Publication No. 2015-198653 [Overview of the Initiative] [Problems that the invention aims to solve]

[0004] Generally, wood kraft pulp has a low specific gravity, which can hinder its widespread adoption due to transportation costs. As a result, its use as animal feed is sometimes limited to areas near pulp manufacturing plants. Furthermore, given the limited amount of feed livestock can consume at one time, feed efficiency requires increasing the nutrient and fiber concentration in the feed, i.e., reducing the volume of the mixed feed. To reduce the volume of feed, wood kraft pulp is manufactured in sheet form. However, in sheet form, it is difficult to handle when feeding to ruminants, and there is room for improvement in terms of palatability, such as taste, texture, and color, which may lead to selective eating. Furthermore, although wood kraft pulp is rich in fiber, it is poor in nutrients such as protein, fat, and minerals, making it difficult to increase livestock productivity with wood kraft pulp alone. For example, while the aforementioned reference 1 mentions wood craft pulp in sheet form, it does not examine detailed methods of utilization, including improvements to handling. In light of these circumstances, the present invention aims to establish a technology that achieves both high palatability and good handling properties for feed containing wood kraft pulp. Furthermore, the present invention aims to provide a technology for producing feed containing wood kraft pulp that has high affinity when mixed with other feed ingredients and that allows for the addition of nutrients that are lacking in wood kraft pulp alone. [Means for solving the problem]

[0005] As a result of diligent research to achieve the above objectives, we confirmed that by crushing wood kraft pulp sheets to a specific size and mixing them with molasses, it is possible to prepare a feed with high specific gravity, excellent handling properties, and high nutritional value and palatability, thus completing the present invention. In other words, the present invention includes the following embodiments. [1] A process of crushing a wood kraft pulp sheet to a size that can pass through a 15 mm mesh screen, and mixing the crushed wood kraft pulp with molasses to achieve a bulk density of 0.15-0.5 g / cm³. 3 A method for producing feed, which includes the following steps. [2] The method according to [1], wherein the wood kraft pulp and the molasses (in terms of undiluted liquid) are mixed in a weight ratio of 4:1 to 15:1. [3] The method according to [1] or [2], wherein the moisture content of the wood kraft pulp sheet is 5-30%. [4] The method according to [1] or [2], wherein the feed is for ruminants. [5] The method according to [4], wherein the ruminant is selected from the group consisting of cattle, goats, sheep, and camels. [6] The method according to [1] or [2], wherein in the crushing step, the wood kraft pulp sheet is crushed in multiple stages, first to a size that can pass through a screen with a mesh size of 50 mm, and then to a size that can pass through a screen with a mesh size of 15 mm. [7] The method according to [1] or [2], wherein the wood kraft pulp and molasses are mixed by spraying an aqueous molasses solution having a concentration of 10 to 90% by weight onto the wood kraft pulp. [8] The method according to [1] or [2], wherein the crushed wood kraft pulp does not pass through a screen with a mesh size of 4 mm. [9] The method according to [1] or [2], further comprising the step of mixing with other feed materials.

[10] The method according to [8], wherein the other feed material comprises at least one selected from the group consisting of cereals, plant oil cakes, cereal brans, and herbaceous plants.

[11] Feed containing at least wood kraft pulp and molasses that are small enough to pass through a 15 mm mesh screen.

[12] The feed according to claim 11, wherein the wood kraft pulp does not pass through a screen with a mesh size of 4 mm.

[13] A method of raising ruminants, comprising feeding them the feed described in

[11] or

[12] .

[14] The method according to

[13] for improving the milk fat content of milk obtained from ruminants.

[15] A method for producing ruminant milk, comprising feeding the ruminant with the feed described in

[11] or

[12] . [Effects of the Invention]

[0006] According to the present invention, by crushing wood kraft pulp sheets to a size of 15 mm or less and attaching molasses, it becomes possible to produce molasses-containing wood kraft pulp feed with improved palatability and texture. The feed of the present invention has a relatively high bulk density and suppressed fluffing, making it easy to handle and easily mix with grains and other feed ingredients. The molasses-containing wood pulp mixed feed composition prepared by mixing with other feed ingredients supplements nutrients such as protein that are lacking in wood kraft pulp, and by making it a highly palatable feed, it can promote the effective use of domestically produced materials and bring benefits to livestock farming. [Brief explanation of the drawing]

[0007] [Figure 1] Figure 1 is a photograph showing the external appearance of pulp crushed pieces and pulverized pieces obtained by crushing and pulverizing wood kraft pulp sheets (left: pulp crushed pieces crushed by a primary crusher, right: pulp crushed pieces pulverized by a secondary crusher). [Figure 2] Figure 2 is a photograph showing the external appearance of a mixed feed obtained by mixing pulp crushed pieces added with molasses with other feed raw materials.

Mode for Carrying Out the Invention

[0008] The feed according to the present invention contains pulp pulverized pieces obtained by pulverizing wood kraft pulp sheets and molasses. The feed according to the present invention contains pulverized pieces of wood kraft pulp sheets pulverized to a size that passes through a screen with an opening of 15 mm, and by further adding molasses, fuzzing of the pulp is suppressed, and the bulk specific gravity is 0.15 to 0.5 g / cm 3 is adjusted. In addition, the feed according to the present invention is excellent in nutritional value by containing molasses, has good palatability including texture, and further has improved handleability due to suppressed fuzzing. In a preferred embodiment, the bulk specific gravity of the feed according to the present invention is 0.2 to 0.45 g / cm 3 and may be 0.25 to 0.40 g / cm 3 . In a preferred embodiment, the feed according to the present invention has an L value after mixing molasses and wood kraft pulp * of 50 or more and 75 or less. In general, ruminant livestock such as cattle have a habit of avoiding feeds with unfamiliar color tones such as white, and by adding brown molasses to the white feed raw material derived from wood kraft pulp, the color tone of the feed can be adjusted to a favorable one. In addition, L * a * b * The L value in the color system * is obtained by calculating the result obtained by measurement according to the method described in JIS Z8722 in accordance with JIS Z8781-4, and the L value of white wood kraft pulp * is 85 or more and 100 or less, and the L value of brown molasses * is 5 or more and 40 or less. The animals to which the feed of the present invention is fed are not particularly limited, and examples thereof include livestock such as dairy cows (particularly Holstein, Jersey, etc.), beef cattle (Wagyu, etc.), pigs, horses, sheep, goats, buffaloes, camels, yaks, and pet animals such as dogs, cats, rabbits, ferrets, hamsters, etc., and the feed can be suitably applied particularly to ruminants such as cows, goats, sheep and camels. The feed according to the present invention is particularly suitable as a feed for ruminants, and by feeding the present invention to ruminants, an effect of improving colostrum quality, particularly increasing milk fat content, is observed. molasses The feed according to the present invention is produced by adding molasses to wood kraft pulp pulverized to a specific size. Molasses is a sugar production by-product produced when manufacturing sugar from beets, sugarcane and the like. Molasses contains 50 to 60% of total sugars including sucrose, and also contains polymerized brown substances generated by the reaction of glucose or fructose with nitrogen-containing components such as amino acids, peptides and proteins. Therefore, by adding molasses to wood kraft pulp, the palatability of the feed can be improved, and the feed intake can be increased. Since the molasses added to wood kraft pulp is viscous in its undiluted form, it is preferably diluted to 10 to 90% by weight before addition in order to make it adhere uniformly to the wood kraft pulp, and more preferably diluted to 40 to 60% by weight. The method for attaching molasses to wood kraft pulp is not particularly limited, but in order to attach molasses uniformly without unevenness, it is preferable to perform impregnation by adding molasses through spraying treatment or impregnation treatment. In the present invention, impregnation means attaching molasses to the pulverized pieces to make the molasses soak into the surface and interior of the pulverized pieces. In the present invention, the weight ratio of the pulverized pulp pieces to molasses (as undiluted solution) is, for example, in the range of 4:1 to 15:1, preferably 6:1 to 12:1, and more preferably 7:1 to 10:1. If there is too much pulp relative to molasses, the bulk specific gravity of the feed will be 0.15 to 0.5 g / cm 3It may become difficult to adjust the size. Furthermore, while the size of the crushed wood kraft pulp sheets may shrink when molasses is added through spraying or impregnation, the upper and lower limits of the size can be considered to be roughly the same. Wood craft pulp crushed to a size of 15 mm or less The feed according to the present invention contains wood kraft pulp sheets crushed to a size of 15 mm or less (wood kraft pulp sheet crushed pieces). If the size of the crushed pieces exceeds 15 mm, uneven adhesion of molasses is likely to occur, resulting in insufficient improvement of texture and palatability, and unevenness may occur when mixing with other feed ingredients. From the viewpoint of uniformly adhering to molasses, suppressing pulp fluffing, and improving texture and palatability, the size of the crushed pieces is preferably 12 mm or less or 10 mm or less. The size of the crushed pieces can be evaluated using a screen, for example, a size of 15 mm or less means that the crushed pieces are small enough to pass through a screen with a mesh size of 15 mm. If the size of the crushed pieces is 4 mm or less, they are likely to be scattered when molasses is sprayed, and may also hinder uniform adhesion of molasses, so the size of the crushed pieces is preferably 4 mm or larger, and may be 6 mm or larger. Here, a size of 4 mm or larger means that the pieces are too large to pass through a screen with a mesh size of 4 mm. Furthermore, due to the nature of the crushing process, it is expected that fragments smaller than 4 mm may be included, and this does not exclude the possibility that the pulp fragments according to the present invention may contain fragments smaller than 4 mm. The pulp fragments according to the present invention are obtained by crushing a wood kraft pulp sheet to the above size. Since the fibers of the wood kraft pulp sheet are intricately and densely intertwined, it is necessary to crush the wood kraft pulp sheet with sufficient strength to obtain fragments. To suppress variations in the size of the fragments, it is preferable to use equipment such as a crusher or pulverizer for the crushing process. The crushing of the wood kraft pulp sheet may be carried out in a single process, or the fragments may be obtained by a multi-stage process. In a preferred embodiment, by going through at least two steps, it is possible to easily obtain fragments to which molasses can be uniformly attached. The apparatus used to obtain the pulp fragments according to the present invention may be a single type of apparatus or a combination of two or more types of apparatus. The type of apparatus is not particularly limited, but examples include crushers, hammer mills, and roller mills. Wood kraft pulp sheets are aggregates of fine fibers and have a tendency to produce fluff when crushed and pulverized. Therefore, in order to efficiently suppress fluffing by uniformly adhering molasses, it is preferable to use an apparatus that has the ability to cut fibers. For example, a pusher-type single-shaft shredder that crushes the material to be crushed by pressing it is suitably used. Furthermore, using an apparatus equipped with a screen is preferable because it allows the wood kraft pulp sheet to be crushed and pulverized to a specific size. For example, a pusher-type cutting single-shaft shredder equipped with a perforated screen can be used. When processing using multiple crushers and pulverizers, for example, the material can be processed with a pusher-type cutting shredder equipped with a perforated screen with a hole diameter of 30 mm, and then crushed and pulverized using a cutting shredder equipped with a perforated screen with a hole diameter of 15 mm. Attempting to obtain fragments smaller than 15 mm in size in a single crushing process places a heavy load on the equipment, significantly reduces the processing volume, and tends to result in uneven fragment size. Therefore, considering industrial production, it is preferable to crush the wood kraft pulp sheets in multiple stages. In the first crushing stage, a pusher-type cutting-type single-shaft crusher capable of processing 10 or more stacked wood kraft pulp sheets is preferably used, taking into consideration the efficiency of the crushing process and the reduction of the workload. Furthermore, for example, it is preferable to use a crusher equipped with a perforated screen with a hole diameter of 25 to 50 mm for the first stage, and more preferably a perforated screen with a hole diameter of 30 to 45 mm. In the second stage of crushing, a cutting-type single-shaft shredder is preferably used to crush the fragments obtained in the first stage while suppressing fluffing as much as possible. To obtain pulp fragments in which the sprayed molasses is uniformly impregnated, it is preferable to use a pusher-type cutting-type single-shaft shredder equipped with a perforated screen with a hole diameter of 15 mm or less. The hole diameter (mesh opening) of the screen is more preferably 8 to 15 mm. (Woodcraft pulp sheet) In this invention, the crushed pieces, which are pulverized to a size of 15 mm or less, are manufactured from a wood kraft pulp sheet. The moisture content of the wood kraft pulp sheet used as raw material is not particularly limited, but it is preferably in the range of 5 to 30% as it affects the shape of the crushed pieces and the pulverization accuracy. From the viewpoint of reducing unevenness in the crushed size, facilitating molasses impregnation, and increasing the specific gravity for better handling, the moisture content of the wood kraft pulp sheet is preferably 7 to 25%, and more preferably 10 to 20%. If the moisture content is less than 5%, the pulverization accuracy will decrease, and the crushed pieces may harden, hindering molasses impregnation. Also, if the moisture content is too high, the pulverization efficiency and pulverization accuracy may decrease. The basis weight of the wood kraft pulp sheet is not particularly limited, but for example, 45 to 2000 g / m². 2 It is 150-1600 g / m² 2 300-1200g / m 2 Preferably, 500-1000 g / m 2 This is more preferable. The wood kraft pulp sheet can be in the form of a roll and / or a flat sheet, and a manufacturing apparatus that can be finished into any shape can be appropriately selected and used. The thickness of the wood kraft pulp sheet is preferably between 1 mm and 15 mm, and more preferably between 1 mm and 10 mm, considering the grinding efficiency and precision. The bulk density of the wood kraft pulp sheet is, for example, 0.4 to 1.0 g / cm³. 3 Therefore, 0.5~0.9 g / cm³ 3 or 0.6~0.8 g / cm³ 3 That is also acceptable. The wood kraft pulp sheet according to the present invention is obtained by producing kraft pulp (KP) from wood and forming the wood kraft pulp into a sheet. In the present invention, either bleached pulp or unbleached pulp can be used as the wood kraft pulp. Among these, unbleached chemical pulp treated with oxygen delignin and bleached chemical pulp are preferred. In the case of unbleached pulp, the kappa number of the pulp is, for example, about 1 to 30, and the kappa number can be measured according to JIS P 8212. In the present invention, in addition to wood kraft pulp, pulp produced by other known pulping methods can be used in combination, for example, either mechanical pulp or chemical pulp can be applied. Examples of mechanical pulps include groundwood pulp (GP), refined groundwood pulp (RGP), thermomechanical pulp (TMP), and chemothermetic pulp (CTMP), while examples of chemical pulps include sulfite pulp (SP) and dissolved sulfite pulp (DSP). Examples of wood that can be used as raw materials include hardwoods, conifers, deciduous trees, bamboo, kenaf, bagasse, and empty cellars after palm oil extraction. Specifically, examples of hardwoods include beech, linden, birch, poplar, eucalyptus, acacia, oak, Japanese maple, Japanese ash, elm, paulownia, magnolia, willow, Japanese ash, evergreen oak, sawtooth oak, horse chestnut, zelkova, Japanese bush beetle, dogwood, and Japanese ash. Examples of coniferous trees include Japanese cedar, Yezo spruce, Japanese larch, Japanese black pine, Sakhalin fir, Japanese white pine, Japanese yew, Japanese cedar, Japanese fir, Japanese spindle tree, Japanese yew, Japanese fir, Japanese cypress, Japanese cypress, Japanese cedar, Japanese thorn, Japanese cypress, Japanese cedar, Japanese spruce, yellow cedar (Western cedar), Lowson cypress (Western cedar), Douglas fir (Western pine), Sitka spruce (Western spruce), Radiata pine, Eastern spruce, Eastern white pine, Western larch, Western fir, Western hemlock, and tamalac. Preferably, broad-leaved trees or coniferous trees are preferred. When broad-leaved trees are used, they are preferred because their fiber length is shorter compared to coniferous trees, resulting in higher digestibility for cattle. When coniferous trees are used, they are preferred because their fiber length is longer and they tend to intertwine and form clumps, making it easier to stimulate rumination in the rumen. When producing kraft pulp from wood chips, the wood chips are generally fed into a digester along with the digestate and subjected to kraft digestion. Alternatively, they may be subjected to digestion using modified kraft methods such as MCC, EMCC, ITC, or Lo-solid. Furthermore, there are no particular limitations on the digestion type, such as single-vessel liquid-phase, single-vessel gas-phase / liquid-phase, double-vessel liquid-phase / gas-phase, or double-vessel liquid-phase. For example, the step of impregnating with an alkaline aqueous solution and retaining it may be installed separately from the conventional equipment or parts intended for the penetration treatment of the digestate. Preferably, after digestion, the unbleached pulp is washed with a washing device such as a diffusion washer after the digestate has been extracted. The liquid ratio of wood chips to chemical solution can be, for example, 1.0 to 5.0 L / kg, preferably 1.5 to 4.5 L / kg, and more preferably 2.0 to 4.0 L / kg. Furthermore, in this invention, an alkaline digestate containing a quinone compound may be added to the digester. When adding an alkaline digestate containing a quinone compound, 0.01 to 1.5% by mass per oven-dried chips is preferred. If the amount of quinone compound added is less than 0.01% by mass, the amount is too small, and the kappa number of the pulp after digestion is not reduced, and the relationship between the kappa number and pulp yield is not improved. Moreover, the reduction of residue and the suppression of viscosity decrease are also insufficient. Furthermore, even if the amount of quinone compound added exceeds 1.5% by mass, no further reduction in the kappa number of the pulp after digestion, nor improvement in the relationship between the kappa number and pulp yield, is observed. The quinone compounds used are quinone compounds, hydroquinone compounds, or precursors thereof, which are known pulping aids, and at least one compound selected from these can be used. Examples of these compounds include anthraquinone, dihydroanthraquinone (e.g., 1,4-dihydroanthraquinone), tetrahydroanthraquinone (e.g., 1,4,4a,9a-tetrahydroanthraquinone, 1,2,3,4-tetrahydroanthraquinone), methylanthraquinone (e.g., 1-methylanthraquinone, 2-methylanthraquinone), methyldihydroanthraquinone (e.g., 2-methyl-1,4-dihydroanthraquinone), and methyltetrahydroanthraquinone (e.g., 1-methyl-1,4,4a,9a-tetrahydroanthraquinone, 2-methyl-1,4,4a,9a-tetrahydroanthraquinone). These are quinone compounds such as trahydroanthraquinone, and hydroquinone compounds such as anthrahydroquinone (generally 9,10-dihydroxyanthracene), methylanthrahydroquinone (e.g., 2-methylanthrahydroquinone), dihydroanthrahydroanthraquinone (e.g., 1,4-dihydro-9,10-dihydroxyanthracene) or their alkali metal salts (e.g., disodium salt of anthrahydroquinone, disodium salt of 1,4-dihydro-9,10-dihydroxyanthracene), and precursors such as anthrone, anthranol, methylanthrone, and methylanthranol. These precursors have the potential to be converted into quinone compounds or hydroquinone compounds under pulverization conditions. The pulp quenching solution preferably has an active alkali addition rate (AA) of 10 to 35% by mass per unit weight of oven-dry wood chips. If the active alkali addition rate is less than 10% by mass, the removal of lignin and hemilose will be insufficient, and if it exceeds 35% by mass, a decrease in yield and quality will occur. Here, the active alkali addition rate is calculated by converting the total addition rate of NaOH and Na2S to the addition rate of Na2O. This can be converted by multiplying NaOH by 0.775 and Na2S by 0.795. Furthermore, the degree of sulfidation is preferably in the range of 20 to 35%. In the range of a degree of sulfidation less than 20%, it leads to a decrease in deligninization, a decrease in pulp viscosity, and an increase in the amount of residue. Kraft pulping is preferably carried out in a temperature range of 120 to 180°C, and more preferably 140 to 160°C. If the temperature is too low, deligninization (decrease in kappa number) is insufficient, while if the temperature is too high, the degree of polymerization (viscosity) of cellulose decreases. Furthermore, the pulping time in this invention is the time from when the pulping temperature reaches the maximum temperature until the temperature begins to decrease, and the pulping time is preferably 60 minutes or more and 600 minutes or less, and more preferably 120 minutes or more and 360 minutes or less. If the pulping time is less than 60 minutes, pulping will not proceed, and if it exceeds 600 minutes, the pulp production efficiency will deteriorate, which is undesirable. Furthermore, in the Kraft pulping process of this invention, the processing temperature and processing time can be set using the H-factor (Hf) as an indicator. The H-factor is an indicator of the total amount of heat supplied to the reaction system during the pulping process and is expressed by the following formula. The H-factor is calculated by integrating the time from the time when the chips and water are mixed until the end of pulping. A H-factor of 300 to 2000 is preferred. Hf = ∫exp(43.20 - 16113 / T)dt [In the formula, T represents the absolute temperature at a given point in time.] In this invention, the unbleached pulp obtained after pulping can be subjected to various treatments as needed. For example, the unbleached pulp obtained after kraft pulping can be bleached. The pulp obtained by kraft pulping can be subjected to oxygen delignin treatment. The oxygen delignin used in this invention can be the same as the known medium-concentration method or high-concentration method. In the case of the medium-concentration method, it is preferable to use a pulp concentration of 8 to 15% by mass, and in the case of the high-concentration method, it is preferable to use 20 to 35% by mass. As the alkali in oxygen delignin, sodium hydroxide or potassium hydroxide can be used, and as the oxygen gas, oxygen from cryogenic separation, oxygen from PSA (Pressure Swing Adsorption), oxygen from VSA (Vacuum Swing Adsorption), etc., can be used. There are no particular limitations on the reaction conditions for oxygen delignin treatment, but the oxygen pressure should be 3-9 kg / cm². 2 , more preferably 4-7 kg / cm³ 2The alkali addition rate is 0.5 to 4% by mass per oven-dry weight of the pulp, the processing temperature is 80 to 140°C, and the processing time is 20 to 180 minutes. Other known conditions can be applied. In this invention, the oxygen delignin treatment may be performed multiple times. Furthermore, the copper number of the oxygen delignin kraft pulp after the oxygen delignin treatment is preferably 5 to 20. To further reduce the copper number, the pulp treated with oxygen delignin can be sent, for example, to a washing process, and after washing, to a multi-stage bleaching process for multi-stage bleaching. The multi-stage bleaching process of the present invention is not particularly limited, but it is preferable to combine known bleaching agents and bleaching aids such as acid (A), chlorine dioxide (D), alkali (E), oxygen (O), hydrogen peroxide (P), ozone (Z), and peracid. For example, the first stage of the multi-stage bleaching process uses a chlorine dioxide bleaching stage (D) or an ozone bleaching stage (Z), the second stage uses an alkali extraction stage (E) or a hydrogen peroxide stage (P), and from the third stage onward, a bleaching sequence using chlorine dioxide or hydrogen peroxide is preferably used. The number of stages from the third stage onward is not particularly limited, but considering energy efficiency, productivity, etc., it is preferable to end the process in a total of three or four stages. Furthermore, a chelating agent treatment stage using ethylenediaminetetraacetic acid (EDTA), diethylenetriaminepentaacetic acid (DTPA), etc., may be inserted during the multi-stage bleaching process. The wood kraft pulp sheet according to the present invention contains bleached or unbleached wood kraft pulp, more preferably containing 50% by mass or more of wood kraft pulp, even more preferably 80% by mass or more, and may consist solely of wood kraft pulp. The wood kraft pulp is preferably deligninized by oxygenation, and preferably has a copper number of 30 or less. A copper number of 30 or less results in good palatability for ruminants. There is no particular lower limit to the copper number. The wood kraft pulp sheet according to the present invention can be obtained, for example, by passing a slurry containing wood kraft pulp (moisture content: 90% or more) through a wire section, a press section, and a dryer section in sequence. The type of wire section of the pulp machine or paper machine used is not particularly limited, but examples include long wire type, cylindrical wire type, short wire type, twin wire type, etc. The type of press section is also not particularly limited, and one or more types such as twin bar press, tri-nip press, tri-vent press, extended nip press, shoe press, tandem shoe press, baby press, twin wire press, heavy-duty press, etc. can be used. Furthermore, the press rolls are also not particularly limited, and one or more types such as grooved rolls, suction rolls, plain rolls, etc., with rubber covers, resin covers, etc., can be appropriately selected and combined. Generally, in the production of wood kraft pulp sheets, the moisture content of the kraft pulp after pressing is between 35% and 70% by mass. If the pulp moisture content is below 35% by mass, it is difficult to manufacture with current paper machines due to equipment limitations. Conversely, if the pulp moisture content is above 70% by mass, it is undesirable because it increases the drying load in the subsequent drying process. The thickness of the pulp sheet after pressing can be between 1 mm and 30 mm. Pulp sheets thinner than 1 mm lack strength and are more likely to tear when passing through the wire section, press section, and dryer section in sequence. On the other hand, if the pulp sheet thickness exceeds 30 mm, moisture is difficult to remove, resulting in a high drying load. The type of dryer part is not particularly limited, and IR dryers, hot air dryers, cylinder dryers, etc., can be used, and one or more of these can be used in combination. The moisture content of the pulp sheet that has passed through the dryer part can be 5% by mass or more and 30% by mass or less, and more preferably 25% by mass or less. There is no particular lower limit to the moisture content, but it is preferably 6% by mass or more. If the moisture content is less than 5% by mass, it is necessary to increase the dryer drying, which is undesirable from the standpoint of energy saving. Preparation of mixed feed The feed according to the present invention has good palatability and can be given alone, but can also be used in combination with other feed ingredients. The feed according to the present invention has a high specific gravity due to the addition of molasses and suppresses fluffing, so it has excellent affinity when mixed with other ingredients. The feed according to the present invention is easy to handle when preparing mixed feed and can be mixed with other feed ingredients to make mixed feed. Examples of feed ingredients to be mixed include grains (corn, barley, rye, millet, cottonseed, soybeans, rice, etc.), plant essential oils (soybean meal, flaxseed meal, coconut meal, sesame meal, rapeseed meal, cottonseed meal, etc.), brans (soybean hulls, rice bran, millet bran, beet meal, barley shochu lees, soy sauce lees, corn gluten feed, brans (rice bran, wheat bran, etc.)), and herbaceous processed products (silage, alfalfa meal, hay cubes, etc.). As for the mixing ratio, for example, molasses-containing wood kraft pulp feed can be applied in a range of 20 to 60% by weight of the total weight of the mixed feed composition, and it is more preferable to use it in a range of 25 to 55% or 30 to 50% by weight. As an example of a feed ingredient to be mixed with molasses-containing wood kraft pulp feed, one method is to mix it with rice bran and processed herbaceous plants. The ratio of rice bran to processed herbaceous plants can be applied in a range of 5:1 to 1:5 by weight, and other ratios such as 3:1 to 1:3 and 1.5:1 to 1:1.5 can also be applied. Feeding of ruminants In one embodiment, the present invention is a method for raising ruminants, comprising feeding the ruminants the above-mentioned feed. According to the present invention, the milk fat content of the milk obtained from ruminants can be improved. In another embodiment, the present invention can also be understood as a method for producing ruminant milk, comprising feeding the ruminants the above-mentioned feed. [Examples]

[0009] The present invention will be described in more detail below with specific examples, but the present invention is not limited to these examples. Furthermore, unless otherwise specified in this specification, concentrations, parts, etc., are given on a weight basis, and numerical ranges are given including their endpoints. Experiment 1. Feed Production Wood kraft pulp sheet derived from hardwood (oak) (bleached kraft pulp, moisture content: 15%, basis weight: 750g / m²) 2 Thickness: 1mm, Bulk density: 0.70g / cm³ 3 The raw material used was wood kraft pulp. This wood kraft pulp sheet was crushed in a primary shredder (pusher-type single-shaft shredder, manufactured by Shoken: DS65220) fitted with a 40mm diameter circular hole screen, and then further crushed in a secondary shredder (high-speed single-shaft shredder, manufactured by Shoken: ES66160H) fitted with an 8mm diameter circular hole screen to obtain crushed wood kraft pulp (bulk density: 0.11 g / cm³). 3 Figure 1 shows the pulp fragments and crushed pieces obtained in each process (left: fragments after primary crushing, right: crushed pieces after secondary crushing). To the pulp fragments obtained as described above, add beet-derived molasses (concentration: 40%, L of the original solution) diluted twice with warm water. * The feed was prepared by spraying with a value of 10) and mixing it so that the weight ratio of pulp to molasses (converted to undiluted solution) was 7.5:1 (bulk density: 0.34 g / cm³). 3 Next, a mixed feed was prepared by adding 33% by weight of soybean hull pellets and 34% by weight of alfalfa cubes to 33% by weight of this feed material. As shown in Figure 2, the resulting mixed feed was homogeneously mixed with the other feed ingredients, demonstrating excellent handling properties and compatibility with other feed ingredients. The table below shows the results of the compositional analysis of the above-mentioned mixed feed and wood kraft pulp. The mixed feed prepared as described above was shown to have higher crude protein and crude fat content and higher nutritional value compared to wood kraft pulp alone. [Table 1] Experiment 2. Evaluation of feed (feeding to lactating cows) The mixed feed prepared in Experiment 1 was administered to four Holstein dairy cows in their second or third lactation, raised at the Kiyokawa Farm of Tokachi Railway Co., Ltd., for 30 days to investigate its effects on milk components. Specifically, the cows were fed 3 kg of the mixed feed of the present invention per cow per day, and were allowed to freely feed the mixed feed with the composition shown in the table below. A milking robot (Astronaut A5; manufactured by Relly) was used for milking. The amount of MR pellets and Super MR supplied by the milking robot as PMR (Partly Mixed Ration) varied according to the individual cow's milk yield. [Table 2] When the milk fat content of milk obtained from dairy cows was measured, it was found that the milk fat content was 4.4% before feeding with the feed of the present invention, while it increased to 5.0% after feeding with the mixed feed of the present invention. From the above, it was confirmed that the feed according to the present invention has an increased bulk density due to the impregnation of crushed wood kraft pulp with molasses. As a result, handling is improved and it has excellent affinity when mixed with other feed ingredients, making it easy to mix with other feed ingredients such as soybean hull pellets and other bran products, and herbaceous processed products such as alfalfa cubes. Furthermore, feeding this feed to lactating cows contributed to an improvement in milk fat content.

Claims

1. The process involves crushing a wood craft pulp sheet to a size that can pass through a screen with a mesh opening of 15 mm, The crushed wood kraft pulp is mixed with molasses to achieve a bulk density of 0.15 to 0.5 g / cm³. 3 The process involves, A method for producing animal feed, including the following:

2. The method according to claim 1, wherein the wood kraft pulp and the molasses (in terms of undiluted liquid) are mixed in a weight ratio of 4:1 to 15:

1.

3. The method according to claim 1 or 2, wherein the thickness of the wood kraft pulp sheet is 1 to 15 mm and the moisture content is 5 to 30%.

4. The method according to claim 1 or 2, wherein the feed is for ruminants.

5. The method according to claim 4, wherein the ruminant is at least one selected from the group consisting of cattle, goats, sheep, and camels.

6. The method according to claim 1 or 2, wherein in the crushing step, the wood kraft pulp sheet is crushed in multiple stages, first to a size that can pass through a screen with a mesh opening of 50 mm, and then to a size that can pass through a screen with a mesh opening of 15 mm.

7. The method according to claim 1 or 2, wherein the wood kraft pulp and molasses are mixed by spraying an aqueous molasses solution having a concentration of 10 to 90% by weight onto the wood kraft pulp.

8. The method according to claim 1 or 2, wherein the crushed wood kraft pulp is of a size that does not pass through a screen with a mesh size of 4 mm.

9. The method according to claim 1 or 2, further comprising the step of mixing with other feed materials.

10. The method according to claim 8, wherein the other feed material comprises at least one selected from the group consisting of grains, plant essential oil residues, rice bran, and herbaceous plants.

11. A feed comprising at least wood kraft pulp of a size that can pass through a 15 mm mesh screen, and molasses.

12. The feed according to claim 11, wherein the wood kraft pulp is of a size that does not pass through a screen with a mesh opening of 4 mm.

13. A method for raising ruminants, comprising feeding the ruminants the feed described in claim 11 or 12.

14. The method according to claim 13 for improving the milk fat content of milk obtained from ruminant animals.

15. A method for producing milk from a ruminant, comprising feeding the ruminant with the feed described in claim 11 or 12.

Citation Information

Patent Citations

  • Feed for ruminants

    JP2015198653A