Heating elements for residential use, heated tiles, and methods for manufacturing the same.

A laminated heating element with a conductive thin film and fibrous or mesh-like layer addresses the inefficiencies of existing heating elements by providing low power consumption, high energy efficiency, and improved safety, suitable for residential thermal tiles.

JP2026182246APending Publication Date: 2026-11-19RIKEN TECHNOS CORP +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2025078316
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-08
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing layered heating elements for residential use, such as underfloor heating sheets and sauna components, require high power consumption and have low energy efficiency, making them costly and inefficient for generating sufficient heat, while also posing safety risks due to scorching or combustion.

Method used

A novel heating element comprising a conductive thin film layer, such as a copper thin film or single-walled carbon nanotube-SiO2 thin film, combined with a fibrous or mesh-like layer, such as glass fibers or ceramic mesh, and optionally plastic sol or hot melt adhesive layers, is used to create a laminated structure that generates sufficient heat with low power consumption and high energy efficiency, allowing for easy manufacturing and excellent design.

Benefits of technology

The laminated structure provides sufficient heat with low power consumption, high energy efficiency, and improved safety, while being easily manufactured and suitable for applications like residential thermal tiles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026182246000001_ABST
    Figure 2026182246000001_ABST
Patent Text Reader

Abstract

This invention provides a novel heating element for residential use that can generate sufficient heat even with relatively low power consumption, is highly energy-efficient, and can form a laminate with excellent design aesthetics, as well as products containing this element. [Solution] One aspect of the present invention is a heating element for residential use in which a conductive thin film layer and a fiber layer or mesh-like layer are laminated, the conductive thin film layer being a layer of copper thin film or single-walled carbon nanotube-SiO2 thin film, and the fiber layer or mesh-like layer being formed from at least one selected from glass fiber and ceramic mesh. The heating element may be laminated in the order of conductive thin film layer, plastic sol layer or hot melt adhesive layer, fiber layer or mesh-like layer, and plastic sol layer or hot melt adhesive layer, and may also be a thin film layer having a thickness of 10 nm to 100 μm produced by a molecular precursor method.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a novel residential heating element having a specific laminated structure, articles such as novel residential thermal tiles containing the same, and a method for manufacturing the residential heating element and residential thermal tiles containing the same. [Background technology]

[0002] Conventionally, in fields such as underfloor heating sheets, floor panels, and sauna components, layered heating elements used at relatively low temperatures, such as 200°C or less, have been known, which have a structure in which various heat-generating and heat-dissipating material layers are covered with an electrically insulating layer. Examples of such layered heating elements include heating elements in which conductive resin is impregnated into a fibrous cloth, and those in which conductive resin is applied to or printed onto a substrate such as a polyester sheet, polyimide sheet, or mica. More specifically, a thermal tile has been developed that combines such a layered heating element with a backing material layer and a decorative sheet to provide aesthetic appeal.

[0003] However, many layered heating elements have the disadvantage of high operating costs due to the large amount of electricity required to generate sufficient heat and their low energy efficiency. Therefore, there is a need for the development of layered heating elements that can generate sufficient heat with relatively low power, have high energy efficiency, and can be easily manufactured, as well as products such as thermal tiles that utilize such heating elements. Furthermore, products containing heating elements are required to possess sufficient heating performance, high safety that can reliably prevent the danger of scorching or combustion during use, and (where desired) excellent design.

[0004] Metal films or metal oxide films, when thinned, possess light transmittance and good thermal conductivity, and are known to function as heat-generating materials (heat-dissipating components) when used in lighting equipment, for example. An example of such a metal film is a copper thin film with high electrical conductivity and antibacterial properties. Metal films or metal oxide films, especially metal thin films with thicknesses on the order of microns or nanometers, are generally formed by vapor phase methods. However, since vapor phase methods such as sputtering require large-scale equipment for film formation, various wet methods for manufacturing metal films are being investigated.

[0005] For example, electroless plating allows for the deposition of a metal film on an inorganic substrate. However, the type of catalyst and other components in the electroless plating solution can affect the physical properties of the formed metal film. In contrast, a method of forming a metal film by applying a metal film-forming composition to a substrate offers greater freedom in selecting the composition of the metal film and the substrate compared to wet methods such as plating. However, such metal film formation methods require heating or sintering at relatively high temperatures, such as 100°C or higher, making it difficult to form metal films for wiring on substrates with poor heat resistance, and also increasing the electricity costs associated with high-temperature processing.

[0006] As a technology that can overcome the disadvantages of such metal film formation methods, a metal film forming composition and a method for forming such a metal film have been reported that can easily form a dense metal film on a substrate without requiring heat treatment at 100°C or higher (see Patent Document 1). The so-called molecular precursor method, which is a metal film formation method disclosed in this document, is a method for forming a thin film of metal or the like without requiring heat treatment at high temperatures or irradiation with active energy rays. According to this method, a metal precursor solution (molecular precursor solution) having a specific composition is prepared with a coating solution, and a uniform thin film can be formed by coating the substrate with the coating solution. Patent Document 1 describes that the metal film produced by this method is suitably used, for example, in circuits of large integrated circuits (LSIs), solar cell wiring, trench embedded wiring, electromagnetic shielding, infrared shielding glass, heat reflective glass, etc. [Prior art documents] [Patent Documents]

[0007] [Patent Document 1] Patent No. 7506404 [Overview of the Initiative] [Problems that the invention aims to solve]

[0008] Taking into consideration the requirements of the prior art described above, the first objective of the present invention is to provide a novel heating element for residential use that generates sufficient heat even with relatively low power consumption and has high energy efficiency, and a novel article such as a residential thermal tile containing the same. A second objective of the present invention is to provide a novel heating element for residential use that can generate sufficient heat even with relatively low power consumption, has high energy efficiency, can form a laminated structure article with excellent design, and can be easily manufactured, as well as a novel article such as a thermal tile for residential use that includes the same. [Means for solving the problem]

[0009] The inventors of the present invention diligently conducted research to solve the above problems and found that by combining a conductive thin film layer with a fiber layer or a mesh-like layer, a residential heating element that provides sufficient heat even with relatively low power and has high energy efficiency can be successfully obtained. Furthermore, the inventors of the present invention found that in a preferred embodiment, a residential heating element that provides sufficient heat can be obtained by a simple method, and thus completed the present invention.

[0010] Accordingly, various aspects or embodiments of the present invention for solving the above problems are as follows. [1]. (a) conductive thin film layer, and (c) Fibrous layer or mesh-like layer A residential heating element in which the following are stacked: The conductive thin film layer (a) is a layer of copper thin film or single-walled carbon nanotube-SiO2 thin film, The (c) fibrous layer or mesh-like layer is a fibrous layer or mesh-like layer formed from at least one selected from glass fibers and ceramic mesh. Heating element for residential use. [2]. A heating element for residential use as described in item [1] above, wherein (a) a conductive thin film layer, (b) a plastic sol layer or hot melt adhesive layer, (c) a fiber layer or mesh-like layer, and (d) a plastic sol layer or hot melt adhesive layer are laminated in this order. [3]. The heating element for residential use according to item [2], wherein the (b) plastic sol layer or hot melt adhesive layer and / or the (d) plastic sol layer or hot melt adhesive layer are integrated with the (c) fiber layer or mesh layer, so that at least a portion of the surface of the fiber or mesh material constituting layer (c) is covered with the plastic sol or hot melt adhesive constituting layers (b) and / or (d). [4]. The residential heating element according to any one of the above items [1] to [3], wherein the (a) conductive thin film layer is a thin film layer formed by a molecular precursor method and having a thickness of 10 nm or more and 100 μm or less. [5]. An article comprising the residential heating element according to any one of the above items [1] to [4]. [6]. The article according to the above item [5], which has at least one use selected from the group consisting of heating, heat retention, snow melting, dew condensation prevention, and anti-fogging. [7]. (1) A decorative sheet, (2) A middle backer, (3) The residential heating element according to any one of the above items [1] to [4], (4) A middle backer, and (5) A bottom backer A residential thermal tile in which the above components are laminated in this order. [8]. A method for producing a residential heating element, comprising: (c) a step of forming the (a) conductive thin film layer on a base material including a fiber layer or a mesh-like layer by a molecular precursor method, to obtain the residential heating element which is a laminate including the (a) conductive thin film layer and the (c) fiber layer or mesh-like layer, wherein the (a) conductive thin film layer is a layer of a copper thin film or a single-walled carbon nanotube-SiO₂ thin film, and the (c) fiber layer or mesh-like layer is a fiber layer or mesh-like layer formed from at least one selected from glass fibers and ceramic meshes, The method for producing a residential heating element. [9]. The base material including the (c) fiber layer or mesh-like layer is a laminated base material comprising (b) a plastic sol layer or a hot-melt adhesive layer, the (c) fiber layer or mesh-like layer, and (d) a plastic sol layer or a hot-melt adhesive layer in this order, The method according to the above item [8].

[10] . The method for obtaining a thermal tile involves using the residential heating element manufactured by the method described in item [8] or [9] above, and stacking (1) a decorative sheet, (2) a middle backer, (3) the residential heating element, (4) a middle backer, and (5) a bottom backer in this order. A method for manufacturing thermal tiles for residential use. [Effects of the Invention]

[0011] According to the present invention, it is possible to provide a novel heating element for residential use that generates sufficient heat even with relatively low power consumption and has high energy efficiency, as well as novel articles such as residential thermal tiles containing the same. Furthermore, the fibrous layer or mesh-like layer has the advantage of contributing to dimensional stability. Furthermore, according to a preferred embodiment of the present invention, it is possible to provide a novel heating element for residential use that can generate sufficient heat even with relatively low power, has high energy efficiency, and can form a laminated structure article with excellent design, and can be easily manufactured, as well as a novel article such as a residential thermal tile containing the same. [Brief explanation of the drawing]

[0012] [Figure 1] Figure 1 is a schematic diagram of a residential heating element according to one embodiment of the present invention. [Figure 2] Figure 2 is a schematic diagram of a residential thermal tile according to one embodiment of the present invention. [Modes for carrying out the invention]

[0013] A heating element for residential use according to the first embodiment of the present invention comprises a structure in which (a) a conductive thin film layer and (c) a fiber layer or mesh-like layer are laminated. Here, (a) the conductive thin film layer is a layer of copper thin film or single-walled carbon nanotube-SiO2 thin film, and (c) the fiber layer or mesh-like layer is a fiber layer or mesh-like layer formed from at least one selected from glass fibers and ceramic mesh. A heating element for residential use according to a second embodiment of the present invention is a form of the heating element according to the first embodiment, and comprises a structure in which (a) a conductive thin film layer, (b) a plastic sol layer or hot melt adhesive layer, (c) a fiber layer or mesh-like layer, and (d) a plastic sol layer or hot melt adhesive layer are laminated in this order. In the heating elements for residential use according to the first and second embodiments, the layers may be directly joined together, or any other layer may be interposed between them. Furthermore, in the heating elements for residential use according to the first and second embodiments, any additional layer (for example, a further conductive thin film layer) may be provided on at least one of the end faces of the laminated structure of the layers. Furthermore, in the residential heating elements according to the first and second embodiments, (a) the conductive thin film layer is usually placed on one side of the heating element that is primarily expected to perform the heat transfer function to the heat-transferring material when the article containing the heating element is used on site. Hereafter, this one side of the residential heating element may be referred to as the "surface side".

[0014] 1. Heating element for residential use (a) Conductive thin film layer (a) The copper thin film layer as a conductive thin film layer can function as a heat-generating layer (core of a heat-generating element) with excellent thermal conductivity. The copper thin film layer is not particularly limited as long as it contains copper as the main component (usually about 50 atomic mol% or more), and may contain one or more other metals, such as lithium, nickel, manganese, zinc, and cobalt. The proportion of copper in the copper thin film layer is preferably 60 atomic mol% or more, 70 atomic mol% or more, 80 atomic mol% or more, 90 atomic mol% or more, or 95 atomic mol% or more, more preferably substantially 100 atomic mol% (the proportion of other elements is below the detection limit). The copper content in the copper thin film layer can be measured, for example, by X-ray diffraction (XRD). By containing copper in the above proportions in the copper thin film layer as a conductive thin film layer, the required high thermal conductivity can be obtained.

[0015] The thickness of the copper thin film layer is usually between 10 nm and 100 μm, preferably between 20 nm and 50 μm, between 50 nm and 30 μm, between 100 nm and 20 μm, or between 200 nm and 10 μm, from the viewpoint of balancing the imparting of heat generation, flexibility in laminate design, and manufacturing costs.

[0016] A layer of single-walled carbon nanotube-SiO2 thin film, as a conductive thin film layer, can function as a heat-generating layer (the core of a heat-generating element) with thermal conductivity comparable to that of a copper thin film layer. The layer of single-walled carbon nanotube-SiO2 thin film is not particularly limited as long as it contains a composite material of single-walled carbon nanotubes and SiO2 as its main component (usually about 50% by mass or more), and may contain any other material (e.g., two or more layers of multi-walled carbon nanotubes). The proportion of the single-walled carbon nanotube-SiO2 composite in the layer of single-walled carbon nanotube-SiO2 thin film is preferably 60% by mass or more, 70% by mass or more, 80% by mass or more, 90% by mass or more, or 95% by mass or more, more preferably substantially 100% by mass (the proportion of other elements is below the detection limit). The content of the single-walled carbon nanotube-SiO2 composite in the layer of single-walled carbon nanotube-SiO2 thin film can be measured, for example, by X-ray diffraction (XRD). (a) The required high thermal conductivity can be obtained by having a layer of single-walled carbon nanotube-SiO2 thin film as a conductive thin film layer, containing a composite of single-walled carbon nanotube and SiO2 in the above proportion.

[0017] Single-walled carbon nanotubes may have a diameter of, for example, 0.5 nm to 500 nm, preferably 3 nm to 100 nm or 5 nm to 50 nm. Single-walled carbon nanotubes may have a length of, for example, 500 μm or less, preferably 100 μm or less. Single-walled carbon nanotubes may be obtained by any conventional manufacturing method, such as catalyst-assisted vapor deposition, arc discharge, laser evaporation, or HiPco (High-pressure carbon monoxide process). Furthermore, the composite of single-walled carbon nanotubes and SiO2 may be any composite used in the industry that includes single-walled carbon nanotubes and SiO2, such as those reported in numerous publications including International Publication No. 2004 / 096725, Japanese Patent Publication No. 2007-254189, Japanese Patent Publication No. 2015-171965, and International Publication No. 2016 / 126969.

[0018] The mass ratio of single-walled carbon nanotubes to SiO2 in a single-walled carbon nanotube-SiO2 thin film layer is not particularly limited, but may be, for example, 5:95 to 95:5, or 10:90 to 90:10, 20:80 to 80:20, 30:70 to 70:30, or 40:60 to 60:40.

[0019] The thickness of the single-walled carbon nanotube-SiO2 thin film layer, similar to the copper thin film layer, is usually 10 nm to 100 μm, preferably 50 nm to 30 μm, 100 nm to 10 μm, 200 nm to 5 μm, or 300 nm to 3 μm, from the viewpoint of balancing the imparting of heat generation, flexibility in laminate design, and manufacturing costs.

[0020] (a) The conductive thin film layer may have one or more holes. The presence of holes in the conductive thin film layer allows the molten plastic sol or hot melt adhesive to penetrate the holes when the (b) plastic sol layer or hot melt adhesive layer, described later, provided on the heating element for housing according to the second embodiment, softens and melts due to heating, thereby facilitating joining and bonding between the heating element and the layered material (e.g., the middle backer described later) placed above it. When one or more holes are formed in the conductive thin film layer, the ratio of the area occupied by the holes on the surface of the conductive thin film layer (opening ratio due to holes) is not particularly limited, but from the viewpoint of balancing improved penetration efficiency of the molten material and maintenance of the strength of the conductive thin film layer, it may be, for example, 0.1% to 50%, or 1% to 30%, 2% to 20%, or 3% to 10%.

[0021] (c) Fibrous layer or mesh-like layer (c) In the first embodiment, the fibrous layer or mesh-like layer provides the function of supporting the conductive thin film layer (a) on its surface. Alternatively, in the second embodiment, the fibrous layer or mesh-like layer provides the function of supporting the plastic sol layer or hot melt adhesive layer (b) described below, and / or the plastic sol layer or hot melt adhesive layer (d) on the surface of the fibrous or mesh-like material. Furthermore, the fact that this layer is made of fibers or mesh can suppress unevenness in heat transfer, improve in-plane uniformity of heat transfer, and contribute to dimensional stability. (c) The fibrous layer or mesh-like layer is not particularly limited as long as it is formed by including at least one selected from glass fibers and ceramic mesh. (c) The fibrous layer or mesh-like layer may be only one of these layers, or a combination of these layers. (c) The fibrous layer or mesh-like layer may be a single layer or a laminate of multiple layers.

[0022] The glass fibers used in the fibrous layer or mesh-like layer are not particularly limited, but may be, for example, glass fibers formed from one or more types of glass, such as alkali-free glass (E glass) with high insulating properties, alkali-containing glass (C glass) with excellent acid resistance, glass with high strength and elastic modulus (S glass, T glass, etc.), glass with excellent alkali resistance (AR glass), and NE glass. Both woven and nonwoven fabrics can be used as glass fibers. The glass fibers are not particularly limited, but may, for example, have a fiber diameter of 5 μm to 150 μm, preferably 10 μm to 100 μm. The glass fibers may be woven or nonwoven fabrics using fiber bundles composed of multiple fibers. Furthermore, the glass fibers are not particularly limited, but may, for example, have a fiber length of 100 μm to 5 mm, preferably 200 μm to 2 mm. It is preferable that the surface of the glass fibers be surface-treated with a silane coupling agent such as an acrylic silane-based silane coupling agent, urethane resin, polyester resin, epoxy resin, polylactic acid-based resin, etc.

[0023] When glass fibers are used as a fibrous layer or mesh-like layer, the specific surface area is not particularly limited, but from the viewpoint of balancing thermal conductivity and shape retention, for example, it is usually 10 m². 2 / g or more, preferably 50m 2 / g or more, 100m 2 / g or more, 200m 2 / g or more, or 300m 2 It may be 1 / g or more. The upper limit of the specific surface area of ​​the glass fiber is not particularly limited, but for example, 2000m 2 It may be less than or equal to / g.

[0024] (c) The glass fibers used in the fiber layer or mesh layer may be a woven fabric in which multiple fiber bundles are woven warp and weft. In the glass fibers, the number of fibers constituting the warp fiber bundles and the weft fiber bundles may be the same or different. In a form in which the glass fiber woven fabric is integrated with (b) a plastic sol layer or hot melt adhesive layer and (d) a plastic sol layer or hot melt adhesive layer to form a coating in at least a part of it, as described below, the coated glass fiber woven fabric may have cavities in the areas where there is no coating.

[0025] The material of the mesh-like substance used in the fibrous layer or mesh-like layer is not particularly limited as long as it is formed from ceramics. The mesh-like layer is not particularly limited, but for example, it may be a mesh-like layer with an opening size of about 10 μm to 500 μm, and preferably a mesh-like layer with an opening size of about 20 μm to 200 μm. By having the mesh-like layer with an opening size within the above range, sufficient insulation and safety can be obtained, the in-plane uniformity of heat transfer is improved, and the applicability to the backer material is further enhanced.

[0026] The insulating ceramics used in the mesh layer are not particularly limited, but may be, for example, one of aluminum nitride, aluminum oxide, silicon nitride, silicon carbide, zirconium oxide, cordierite, and mullite, or a composite material of several of these.

[0027] The fibrous layer or mesh-like layer may be a single layer, but may also be formed from multiple layers. The thickness of the fibrous layer or mesh-like layer (total thickness if it is formed from multiple layers) is usually 10 μm to 3000 μm, preferably 10 μm to 1000 μm, 20 μm to 500 μm, or 30 μm to 200 μm, from the viewpoint of stably supporting the conductive thin film layer (a) or the plastic sol layer or hot melt adhesive layer described later, and from the viewpoint of balancing manufacturing costs, etc.

[0028] (b) or (d) the plastic sol layer or hot melt adhesive layer In the second embodiment, when (b) a plastic sol layer or hot melt adhesive layer and (d) a plastic sol layer or hot melt adhesive layer are provided, layer (b) has the function of promoting and facilitating bonding between (a) a conductive thin film layer and (c) a fiber layer or mesh-like layer via it. Alternatively, as described above, in an embodiment in which one or more holes are formed in (a) a conductive thin film layer, the molten plastic sol or hot melt adhesive penetrates the holes, thereby facilitating bonding and adhesion between other members constituting the article (e.g., the middle backer in a thermal tile as an article) and (a) a conductive thin film layer and (c) a fiber layer or mesh-like layer. Furthermore, in the second embodiment, if (b) a plastic sol layer or hot melt adhesive layer and (d) a plastic sol layer or hot melt adhesive layer are provided, layer (d) has the function of facilitating joining and bonding between (c) a fibrous layer or mesh-like layer and other members constituting the article (for example, the middle backer in a thermal tile as an article).

[0029] In this embodiment, when (b) a plastic sol layer or hot melt adhesive layer and (d) a plastic sol layer or hot melt adhesive layer are provided, layers (b) and (d) and the fiber layer or mesh-like layer (c) may form three layers that are in contact with and separated from each other, or at least in part, layers (b) and / or (d) may be integrated with the fiber layer or mesh-like layer (c), so that the multilayer material of (b) / (c) or (c) / (d) or (b) / (c) / (d) has the appearance of a single aggregate layer. In this integrated form, at least a portion of the surface of the fibrous or mesh-like material constituting layer (c) is coated with the plastic sol or hot-melt adhesive constituting layers (b) and / or (d). The thickness of such coating is not particularly limited, but may be, for example, 5 μm to 100 μm. It is preferable from the viewpoint of homogenizing the performance of the heating element that the majority or substantially the entire surface of at least one of the fibrous or mesh-like material constituting layer (c) is coated with the plastic sol or hot-melt adhesive constituting layers (b) and / or (d). Furthermore, it is even more preferable from the viewpoint of homogenizing the performance of the heating element that the majority or substantially the entire surface of each of the two sides of the fibrous or mesh-like material constituting layer (c) is coated with a thin layer of the plastic sol or hot-melt adhesive constituting both layers (b) and (d). For example, such coating can be formed by immersing the fibrous or mesh-like material constituting layer (c) in a liquid containing the plastic sol or hot-melt adhesive. Alternatively, for example, after forming a coating on the raw linear material of each fiber or mesh-like substance, a woven fabric or mesh may be formed using the coated fiber or linear material.

[0030] When layer (b) or (d) is a plastic sol layer, the plastic sol is not particularly limited as long as it is a sol containing a plastic that performs the above functions. For example, the plastic used in the plastic sol may be polyvinyl chloride resin (PVC resin), polyacrylic resin, polyurethane resin, etc. A polyvinyl chloride resin sol may be obtained by mixing and kneading polyvinyl chloride resin and any additives such as plasticizers, fillers, weather stabilizers and heat stabilizers, and resins other than polyvinyl chloride resin for sol blends, using methods known in the industry, to form a sol, and then drying it. Other additives include any lubricant, antioxidant, processing aid, reinforcing agent, nucleating agent, mold release agent, antistatic agent, urea-formaldehyde wax, surfactant, and other additives known in the industry. These additives may be used individually or in mixtures of multiple types. The method for forming a polyvinyl chloride resin sol is not particularly limited, but for example, a mixture of the polyvinyl chloride resin and an optional additive can be homogenized in an aqueous medium by adding an emulsifier, and optionally a dispersing aid such as a higher alcohol or higher fatty acid, and an oil-soluble polymerization initiator, and then by fine suspension polymerization, or by emulsion polymerization or seed emulsion polymerization by adding a water-soluble initiator.

[0031] (b) or (d) The polyvinyl chloride resin constituting the sol layer of the polyvinyl chloride resin is, for example, polyvinyl chloride (polyvinyl chloride homopolymer); vinyl chloride-vinyl acetate copolymer, vinyl chloride-(meth)acrylic acid copolymer, vinyl chloride-methyl (meth)acrylate copolymer, vinyl chloride-(meth)acrylate copolymer, vinyl chloride-ethyl (meth)acrylate copolymer, vinyl chloride-maleic acid copolymer, vinyl chloride-ethylene copolymer, vinyl chloride-propylene copolymer, vinyl chloride-styrene copolymer, vinyl chloride-isobutylene copolymer, vinyl chloride-vinylidene chloride copolymer, vinyl chloride Examples include vinyl chloride copolymers of vinyl chloride and other monomers copolymerizable with vinyl chloride, such as styrene-maleic anhydride terpolymer, vinyl chloride-styrene-acrylonitrile terpolymer, vinyl chloride-butadiene copolymer, vinyl chloride-isoprene copolymer, vinyl chloride-chlorinated propylene copolymer, vinyl chloride-vinylidene chloride-vinyl acetate terpolymer, vinyl chloride-acrylonitrile copolymer, and vinyl chloride-various vinyl ether copolymers; and modified (chlorinated, etc.) polyvinyl chloride and vinyl chloride copolymers, such as post-chlorinated vinyl copolymers. Furthermore, chlorinated polyolefins, such as chlorinated polyethylene, which have a chemical structure similar to polyvinyl chloride, may also be used. Such chlorinated polyolefins with a chemical structure similar to polyvinyl chloride are also included in the category of "polyvinyl chloride resins" as used herein. One or more of these can be used as polyvinyl chloride resins.

[0032] Examples of plasticizers used in polyvinyl chloride resin sols include polyester plasticizers, phthalate ester plasticizers, trimellitic acid ester plasticizers, pyromellitic acid ester plasticizers, adipic acid ester plasticizers, itaconic acid ester plasticizers, citrate ester plasticizers, cyclohexane dicarboxylate plasticizers, and epoxy plasticizers. One or more of these plasticizers or mixtures thereof can be used. The amount of plasticizer is not particularly limited, but is usually greater than 0 parts by mass and less than or equal to 80 parts by mass, preferably 5 parts by mass or more and less than or equal to 50 parts by mass, 10 parts by mass or more and less than or equal to 40 parts by mass, or 15 parts by mass or more and less than or equal to 30 parts by mass, relative to 100 parts by mass of polyvinyl chloride resin.

[0033] Examples of polyacrylic resins that constitute the sol layer of the polyacrylic resin in (b) or (d) include polymethyl methacrylate, polyethyl methacrylate, polybutyl methacrylate, polyacrylonitrile, and other polyacrylic resins, or copolymers having acrylate units and styrene units or urethane structures. One or more of these can be used as the polyacrylic resin.

[0034] The polyacrylic resin sol may be obtained by mixing and kneading the above-mentioned resin components with any additives such as plasticizers, fillers, weather stabilizers and heat stabilizers, and resins for sol blends other than polyacrylic resins, using methods known in the industry, to form a sol, and then drying it. Furthermore, silane coupling agents or the like may be used as tackifiers to improve adhesion between adjacent layers in the laminate. Other additives include any lubricants, antioxidants, processing aids, reinforcing agents, nucleating agents, mold release agents, antistatic agents, urea-formaldehyde wax, and surfactants known in the industry. These additives may be used individually or in mixtures of multiple types.

[0035] Examples of polyurethane resins that constitute the sol layer of the polyurethane resin in (b) or (d) include polyester polyurethane resins, polylactone polyurethane resins, polyether polyurethane resins, polyurethane resins crosslinked with epoxy resins, or ionomer-type polyurethane resins. One or more of these can be used as the polyurethane resin.

[0036] The polyurethane resin sol may be obtained by mixing and kneading the above-mentioned resin components with any additives such as plasticizers, fillers, weather stabilizers and heat stabilizers, and resins for sol blends other than polyurethane resins, using methods known in the industry, to form a sol, and then drying it. Furthermore, silane coupling agents or the like may be used as tackifiers to improve adhesion between adjacent layers in the laminate. Other additives include any lubricants, antioxidants, processing aids, reinforcing agents, nucleating agents, mold release agents, antistatic agents, urea-formaldehyde wax, and surfactants known in the industry. These additives may be used individually or in mixtures of multiple types.

[0037] The hot melt adhesive in the case where layer (b) or (d) is a hot melt adhesive layer is not particularly limited, as long as it contains a resin that performs the above functions and has hot melt adhesive properties. Examples of resins that make up hot melt adhesives include ethylene-α-olefin copolymers such as ABS, polyvinyl chloride, polyamide, polyester, polyurethane, polycarbonate, polystyrene, polyethylene, polypropylene, poly-1-butene, polyisobutylene, polymethylpentene, ethylene-α-olefin copolymers such as ethylene-propylene copolymer, ethylene-butene copolymer, ethylene-hexene copolymer, and ethylene-octene copolymer; ethylene-unsaturated ester copolymers such as ethylene-vinyl acetate copolymer (EVA) and ethylene-ethyl acrylate copolymer (EEA); cyclic olefin-containing copolymers such as copolymers of cyclopentadiene and ethylene and / or propylene; ethylene-glycidyl methacrylate copolymer, ethylene-propylene-diene copolymer, ethylene-vinyl acetate-maleic anhydride terpolymer, ethylene-ethyl acrylate-maleic anhydride terpolymer; and ethylene-unsaturated glycidyl compound copolymers such as ethylene-vinyl acetate-glycidyl methacrylate terpolymer and ethylene-ethyl acrylate-glycidyl methacrylate terpolymer.

[0038] The hot melt adhesive constituting the hot melt adhesive layer of (b) or (d) may optionally contain, in addition to the resin, additives such as tackifiers to improve adhesion. The tackifier is not particularly limited, but examples include one or a mixture of several types of silane coupling agents, phenol resins, modified phenol resins, terpene phenol resins, xylene phenol resins, cyclopentadiene-phenol resins, xylene resins, aliphatic, alicyclic or aromatic petroleum resins, hydrogenated aliphatic, alicyclic or aromatic petroleum resins, phenol-modified petroleum resins, rosin ester resins, hydrogenated rosin ester resins, low molecular weight polystyrene resins, terpene resins, and hydrogenated terpene resins.

[0039] Other additives that may be used in hot melt adhesives include, but are not limited to, waxes for reducing viscosity, such as carnauba wax, candelilla wax, montan wax, paraffin wax, microwax, Fischer-Tropsch wax, polyethylene wax, polypropylene wax, oxides of these waxes, ethylene-acrylic acid copolymers, ethylene-methacrylic acid copolymers, and mixtures of several such waxes. Other additives that may be used in hot melt adhesives include any antioxidant, filler, flame retardant, plasticizer, antistatic agent, light stabilizer, UV absorber, heavy metal deactivator, or other additives known in the industry. These additives may be used individually or in combination. The amount of these additives in the hot melt adhesive constituting the hot melt adhesive layer of (b) or (d) (if used) is not particularly limited, but may be, for example, more than 0 parts by mass per 100 parts by mass of the resin, and 20 parts by mass or less, 10 parts by mass or less, or 5 parts by mass or less.

[0040] The plastic sol layer or hot melt adhesive layer of (b) or (d) may be a single layer, but may also be formed from multiple layers. If the layer of (b) or (d) is a single layer, that layer, or if the layer of (b) or (d) is formed from multiple layers, one of those layers may be integrated with the (c) fiber layer or mesh-like layer as described above to form the appearance of a single aggregate layer. The thickness of the plastic sol layer or hot melt adhesive layer of (b) or (d) (total thickness if formed from multiple layers), or the thickness including the coating of the plastic sol or hot melt adhesive when integrated with the (c) fiber layer or mesh-like layer, may usually be 10 μm or more and 1000 μm or less after the formation of the laminated structure (after melting and curing), preferably 20 μm or more and 500 μm or less, 30 μm or more and 300 μm or less, or 40 μm or more and 100 μm or less, from the viewpoint of providing sufficient bonding and adhesion functions as described above and from the viewpoint of balancing manufacturing costs, etc. In the second embodiment, when (b) the plastic sol layer or hot melt adhesive layer and (d) the plastic sol layer or hot melt adhesive layer are formed, the composition and / or thickness of layer (b) and the composition and / or thickness of layer (d) may be the same or different.

[0041] Figure 1 shows a schematic diagram of an example of a residential heating element according to a second embodiment of the present invention. In the figure, reference numeral 1 represents (a) a conductive thin film layer, reference numeral 2 represents (b) a plastic sol layer or hot melt adhesive layer, reference numeral 3 represents (c) a fiber layer or mesh-like layer, reference numeral 4 represents (d) a plastic sol layer or hot melt adhesive layer, and reference numeral 100 represents the entire heating element for residential use. Furthermore, as described above, layer 2(b) and / or layer 4(d) may be integrated with layer 3(c) (fiber layer or mesh layer), so that the (b) / (c) or (c) / (d) or (b) / (c) / (d) multilayer material has the appearance of a single layer. In the figure, the conductive thin film layer labeled 1 is positioned on one side of the residential heating element 100, which is primarily expected to perform a heat transfer function to the heat-transferring material when the article containing the residential heating element 100 is used on site.

[0042] As an additional embodiment, from the viewpoint of increasing heat transfer, the heating element for residential use according to the first embodiment may be configured to include a further conductive thin film layer similar to the conductive thin film layer on the side of the (c) fiber layer or mesh-like layer opposite to the (a) conductive thin film layer. Alternatively, as another additional embodiment, from the viewpoint of increasing heat transfer, the heating element for residential use according to the second embodiment may be configured to include a further conductive thin film layer similar to the conductive thin film layer on the side of the (d) plastic sol layer or hot melt adhesive layer opposite to the (a) conductive thin film layer.

[0043] A residential heating element according to any embodiment of the present invention can provide sufficient heat even with relatively low power, has high energy efficiency, and can form a laminated structure article with excellent design, making it suitable for use in various articles such as thermal tiles. Furthermore, according to the preferred manufacturing method described later, (a) the conductive thin film layer can be easily manufactured without requiring heat treatment of 100°C or higher, so the entire residential heating element according to any embodiment of the present invention, including this layer, can also be easily manufactured.

[0044] 2. Articles containing heating elements for residential use A heating element for residential use according to any embodiment of the present invention can be used as an article for various applications including the same. The uses of articles containing heating elements for residential use are not particularly limited, as long as they are for applications in houses or structures related to houses where heat supply is desirable or required. Examples of such uses include heating mats such as tiles, carpets, and hot carpets in apartments and general houses, floor heating equipment, wall heating equipment, roof snow melting heaters, sheet heaters used inside houses, anti-fog heaters and anti-fog glass for removing water droplets or ice buildup from windows and mirrors in houses, and condensation prevention heaters.

[0045] Preferred uses for the article include, for example, at least one use selected from heating, heat retention, snow melting, condensation prevention, and anti-fogging. A particularly preferred use for the product is residential thermal tiles, which can be used in the floors and walls of residential buildings for heating, heat retention, and condensation prevention.

[0046] 3. Thermal tiles for residential use In one embodiment, the thermal tile for residential use according to the present invention is: (1) Decorative sheet, (2) Middle backer, (3) A heating element for residential use according to any embodiment of the present invention (typically a heating element for residential use according to the second embodiment described above), (4) Middle backer, and (5) Bottom backer It has a structure in which these are stacked in this order. Here, (1) the decorative sheet and (2) the middle backer are typically placed on one side of (3) the residential heating element, which is primarily expected to perform a heat transfer function to the heat-transferring material when the residential thermal tile is used on site. Residential thermal tiles may further include any one or more layers other than those described in (1) to (5) above (for example, layers such as heat-resistant adhesive applied between each layer), as long as the desired thermal function is not hindered.

[0047] The decorative sheet (1) that constitutes the residential thermal tiles is not particularly limited, as long as it provides the desired design and aesthetic appeal. For example, any colored or uncolored resin sheet can be used as the decorative sheet.

[0048] Examples of resins used in colored or uncolored resin sheets that can be used as decorative sheets include, but are not limited to, polyester resins such as aromatic polyesters and aliphatic polyesters; acrylic resins; polycarbonate resins; poly(meth)acrylimide resins; polyolefin resins such as polyethylene, polypropylene, and polymethylpentene; cellulosic resins such as cellophane, triacetylcellulose, diacetylcellulose, and acetylcellulose butyrate; styrene resins such as polystyrene, acrylonitrile-butadiene-styrene copolymer (ABS resin), styrene-ethylene-propylene-styrene copolymer, styrene-ethylene-ethylene-propylene-styrene copolymer, styrene-ethylene-butadiene-styrene copolymer, and styrene-ethylene-butadiene-styrene copolymer; polyvinyl chloride resins; polyvinylidene chloride resins; fluorine-containing resins such as polyvinylidene fluoride; and others such as polyvinyl alcohol, ethylene vinyl alcohol, polyetheretherketone, nylon, polyamide, polyimide, polyurethane, polyetherimide, polysulfone, and polyethersulfone. These resin sheets include unoriented sheets, uniaxially oriented sheets, and biaxially oriented sheets. Laminated sheets, which consist of two or more layers of one or more of the above-mentioned resin sheets, may also be used.

[0049] The decorative sheet may optionally include a printed layer on its surface to enhance its aesthetic appeal. The printed layer is provided to give it a high level of design appeal and can be formed by printing any pattern using any ink and any printing press.

[0050] The printing layer can be applied directly or via an anchor coat to the entire resin sheet, or partially. Examples of patterns include metallic patterns such as hairline, wood grain patterns, stone patterns that mimic the surface of rocks such as marble, fabric patterns that mimic the texture of cloth or fabric, tile patterns, brick patterns, parquet patterns, and patchwork. As the printing ink, a binder can be used which is appropriately mixed with pigments, solvents, stabilizers, plasticizers, catalysts, and curing agents. Examples of binders that can be used include polyurethane resins, vinyl chloride / vinyl acetate copolymer resins, vinyl chloride / vinyl acetate / acrylic copolymer resins, chlorinated polypropylene resins, acrylic resins, polyester resins, polyamide resins, butyral resins, polystyrene resins, nitrocellulose resins, and cellulose acetate resins, as well as compositions of these resins. Furthermore, in order to create a metallic appearance, aluminum, tin, titanium, indium, and their oxides may be deposited onto the resin sheet, either directly or via an anchor coat, either entirely or partially, by known methods.

[0051] In one modified form, the decorative sheet is composed of a printed layer, and the printed layer may be formed on the surface of the middle backer of (2) as a resin substrate. In this modified form, the middle backer of (2) can function as a substitute for the above-mentioned colored or uncolored resin sheet.

[0052] The thickness of the decorative sheet (including the printed layer if one is formed) is not particularly limited, but is usually 50 μm or more, preferably 100 μm or more, and more preferably 200 μm or more. Also, from the viewpoint of meeting the demand for thinner articles, the thickness of the decorative sheet is usually 3000 μm or less, preferably 2000 μm or less, and more preferably 1000 μm or less.

[0053] The surface side of the decorative sheet may optionally be further provided with a transparent film layer and / or a transparent coating layer (hereinafter, these layers may be collectively referred to as the "clear layer") containing an acrylic resin, fluororesin, or vinyl chloride resin, which has the function of providing high weather resistance, scratch resistance, and impact resistance to the laminate of residential thermal tiles. The clear layer may form the outermost surface of the residential thermal tile. In this specification, "acrylic resin" refers to either acrylic resin or methacrylic resin. "Transparent" for the transparent film layer and transparent coating layer means a state in which light in substantially the entire wavelength range of visible light, or light in a part of the wavelength range of visible light, is transmitted through the clear layer, and the other side of the clear layer is visible from one side. "Transparent" for the transparent film layer and transparent coating layer includes not only colorless transparency, but also colored transparency and translucency. The clear layer containing an acrylic resin, fluororesin, or vinyl chloride resin may be a single layer, or it may be a laminate of multiple layers with the same or different compositions. Furthermore, the transparent film layer may be an unoriented film, a uniaxially oriented film, or a biaxially oriented film. If the transparent film layer is a laminate of multiple layers, it may be formed from a combination of two or more of the unoriented film, uniaxially oriented film, and biaxially oriented film. The transparent coating layer can be formed by methods such as spin coating, spray coating, bar coating, knife coating, roll coating, blade coating, die coating, or gravure coating. The transparent coating layer may also have a multilayer structure. In addition, the transparent coating layer may be laminated on top of the transparent film layer.

[0054] Examples of acrylic resins used as the main component of the clear coat include, but are not limited to, (meth)acrylic acid ester (co)polymers, copolymers mainly containing (usually 50 mol% or more) structural units derived from (meth)acrylic acid esters, and modified versions thereof. (Meth)acrylic means acrylic or methacrylic. (Co)polymer means polymer or copolymer. As the acrylic resin used as the main component of the clear coat, one of these resins can be used alone or in the form of any mixture of two or more. Examples of (meth)acrylic acid ester (co)polymers include poly(meth)acrylate methyl, poly(meth)acrylate ethyl, poly(meth)acrylate propyl, poly(meth)acrylate butyl, (meth)acrylate-(meth)acrylate butyl copolymer, and (meth)acrylate-(meth)acrylate butyl copolymer. These resins can be used alone or in the form of any mixture of two or more.

[0055] Examples of fluororesins used as the main component of the clear coat include, but are not limited to, polyvinyl fluoride (PVF), polyvinylidene fluoride (PVDF), polychlorotrifluoroethylene (PCTFE), polyethylene tetrafluoroethylene (ETFE), polytetrafluoroethylene (PTFE), tetrafluoroethylene perfluoroalkyl vinyl ether copolymer (PFA), tetrafluoroethylene-hexafluoropropylene copolymer (FEP), chlorotrifluoroethylene-ethylene copolymer (ECTFE), fluoroolefin-vinyl ether copolymer, or modified versions of these fluororesins. These resins can be used individually or in any mixture of two or more.

[0056] Examples of vinyl chloride resins used as the main component of the clear layer include, but are not limited to, homopolymers of vinyl chloride or copolymers of vinyl chloride with other monomers. Examples of these other monomers include, but are not limited to, olefins such as ethylene, propylene, and isobutene or their chlorinated derivatives; dienes such as isoprene and butadiene; vinyl compounds such as acrylonitrile, methacrylonitrile, and vinyl acetate; maleic acid or its esters or acid anhydrides; acrylic acid or its esters; methacrylic acid or its esters; and vinylidene chloride. Furthermore, the vinyl chloride resin may be a resin in which the homopolymer or copolymer is partially crosslinked. These resins can be used individually or in any mixture of two or more.

[0057] The clear layer may, to the extent that it does not contradict the objectives of the present invention, further contain optional components other than the resin constituting the main component, as desired. Examples of such optional components include resins such as core-shell rubber and ethylene-vinyl acetate copolymer, ultraviolet absorbers, light stabilizers, flame retardants, photopolymerization initiators, antistatic agents, surfactants, leveling agents, thixotropic agents, antifouling agents, printability improvers, antioxidants, weather-resistant stabilizers, heat stabilizers, pigments, and fillers. The amount of the above optional components (if used) is not particularly limited, but is usually about 0.01 parts by mass or more and 50 parts by mass or less, relative to 100 parts by mass of the main component resin forming the clear layer.

[0058] The thickness of the clear layer (or the total thickness if it consists of multiple layers) is not particularly limited, but from the viewpoint of balancing the provision of high weather resistance and impact resistance with manufacturing costs and ease of handling, it may be, for example, 1 μm or more and 1000 μm or less. This thickness may preferably be 80 μm or more, 100 μm or more, 150 μm or more, 200 μm or more, or 300 μm or more, and / or 800 μm or less, 700 μm or less, 600 μm or less, 500 μm or less, or 400 μm or less.

[0059] The middle backers (2) and (4) and the bottom backer (5) that constitute the residential thermal tile are layers of backup material formed from synthetic resin. The middle backers (2) and (4) and the bottom backer (5) are all provided to impart hardness and strength to the residential thermal tile, to mitigate surface irregularities of the adherend, and to provide impact resistance.

[0060] (2) and (4) as the middle backer and (5) as the bottom backer, a resin sheet made of thermoplastic resin can usually be used. Examples of such thermoplastic resins include polyolefins such as polypropylene and polyethylene, polyacrylics, polymethylenes, polymethylpentenes, polyethylene terephthalates, polybutylene terephthalates, polycarbonates, polyarylates, polyimides, polystyrenes, polyamides, polyvinyl chlorides, polyurethanes, ethylene-vinyl alcohol copolymers, polyethylene naphthalate-isophthalate copolymers, and ABS resins. These resins can be used individually or in combination of two or more.

[0061] The thickness of the middle backer in (2) and (4) and the bottom backer in (5) can be appropriately selected according to the requirements of each product, but from the viewpoint of balancing the provision of hardness, strength, impact resistance, etc., the specifications of the resulting product, aesthetics, and manufacturing costs, it is usually 0.5 mm to 20 mm, preferably 1 mm to 15 mm, 3 mm to 12 mm, or 5 mm to 10 mm.

[0062] Figure 2 shows a schematic diagram of an example of a residential thermal tile including a heating element according to one embodiment of the present invention. In the figure, reference numeral 10 denotes a decorative sheet, reference numeral 20 denotes a middle backer, reference numeral 100a denotes a residential heating element according to one embodiment of the present invention, reference numeral 30 denotes a middle backer, reference numeral 40 denotes a bottom backer, and reference numeral 200 denotes the entire residential thermal tile. In the figure, the decorative sheet 10 and the middle backer 20 are arranged on one side of the residential heating element 100a, which is primarily expected to perform a heat transfer function to the heat-transferring material when the residential thermal tile 200, including the residential heating element 100a, is used on site.

[0063] A residential thermal tile containing a residential heating element according to any embodiment of the present invention can be designed to provide sufficient heat even with relatively low power consumption, to be highly energy-efficient, and to offer excellent aesthetic appeal. Furthermore, as described later, (3) the conductive thin film layer included in the heating element for residential use can be easily manufactured without requiring heat treatment of 100°C or higher, so the entire residential thermal tile including the heating element according to any embodiment of the present invention can also be easily manufactured.

[0064] 4. Manufacturing method of heating elements for residential use The method for manufacturing a residential heating element according to any embodiment of the present invention described above is not particularly limited, as long as it has the above configuration. The heating element for residential use according to the first embodiment described above can be manufactured, for example, by individually creating (a) a conductive thin film layer and (c) a fibrous layer or mesh-like layer (and a laminate of any other layer) and laminating them by known means, or by applying the raw material or precursor of the conductive thin film layer (a) onto the fibrous layer or mesh-like layer (and a laminate of any other layer) and subjecting it to a treatment such as drying under predetermined conditions as necessary. The heating element for residential use according to the second embodiment described above can be manufactured, for example, by individually creating (a) a conductive thin film layer, (b) a plastic sol layer or hot melt adhesive layer, (c) a fiber layer or mesh-like layer, and (d) a plastic sol layer or hot melt adhesive layer (and a laminate of any other layer) and laminating them by known means, or by applying the raw material or precursor of the conductive thin film layer (a) onto a laminate of (b) a plastic sol layer or hot melt adhesive layer, (c) a fiber layer or mesh-like layer, and (d) a plastic sol layer or hot melt adhesive layer (and any other layer), and subjecting it to treatment such as drying under predetermined conditions as necessary. Here, the laminate of layer (b), layer (c), and layer (d) (and any other layer) may be in a form in which layer (b) and / or (d) are integrated with layer (c), thereby the surface of at least a portion of the fibrous or mesh-like material constituting layer (c) is covered with the plastic sol or hot melt adhesive constituting layer (b) and / or (d).

[0065] (c) A fibrous layer or mesh-like layer or (d) a plastic sol layer or hot melt adhesive layer onto which the raw material or precursor of (a) a conductive thin film layer can be applied, and if necessary, subjected to treatment such as drying under predetermined conditions. This method can be described below.

[0066] (a) Formation of conductive thin film layer by molecular precursor method (a) The copper thin film or single-walled carbon nanotube-SiO2 thin film layer as the conductive thin film layer of the heating element according to any embodiment of the present invention can be manufactured by any method known in the art, but preferably by the so-called molecular precursor method. The molecular precursor method does not require heating at high temperatures or irradiation with active energy rays, so a conductive thin film layer can be easily formed on substrates with poor heat resistance. Furthermore, the molecular precursor method can provide sufficient heat even with relatively low power (for example, by dry cell batteries alone), and a conductive thin film layer with high energy efficiency can be obtained. The copper thin film or single-walled carbon nanotube-SiO2 thin film layer obtained by the molecular precursor method has a dense structure and high purity, and therefore has excellent electrical and thermal conductivity. Hereafter, a method for manufacturing copper thin films or single-walled carbon nanotube-SiO2 thin films using the molecular precursor method will be described. The methods for manufacturing these layers using the molecular precursor method described below can also be applied to embodiments in which a portion of the copper constituting the copper thin film is replaced with one or more other metals, such as lithium, nickel, manganese, zinc, and cobalt, and to embodiments in which a portion of the single-walled carbon nanotube-SiO2 composite constituting the single-walled carbon nanotube-SiO2 thin film is replaced with other substances (for example, two or more multi-walled carbon nanotubes).

[0067] The method for manufacturing copper thin films using molecular precursors is typically: (Step I) A step to obtain a copper precursor solution by reacting at least one copper complex and / or copper salt with at least one selected from ammonia and amine in a mixed solution containing at least one copper complex and / or copper salt, at least one selected from ammonia and amine, and a solvent. (Step II) A step of preparing a copper thin film forming composition containing the obtained copper precursor liquid and an organic reducing agent, and (Step III) Step of applying the obtained copper thin film forming composition to a substrate. Includes.

[0068] (Process I) The copper salt used in step I is preferably a copper salt soluble in water at 25°C. Soluble in water at 25°C means that the solubility in water at 25°C is 0.1% by mass or more, and preferably 1% by mass or more. Because the copper salt is soluble in water, it dissociates in a water-containing solvent to form copper ions, and these copper ions react with amines contained in the solvent to obtain a copper complex. The copper salt is not particularly limited, but examples include copper formate, copper acetate, and copper chloride. Furthermore, if the solvent optionally contains a compound for complex formation described later, the copper ions may react with the compound for complex formation to form a copper complex.

[0069] The copper complex that may be contained in the mixture is preferably a reaction product of copper ions with one or more compounds for copper complex formation selected from compounds having diamine-derived ligands such as NH3 ligands, RNH2 ligands (where R represents an alkylene group), OH2 ligands, ethylenediamine, and hexamethylenediamine as partial structures. As the copper complex, a copper complex previously formed by the above reaction can be used. Examples of copper complexes are not particularly limited, but ethylenediaminetetraacetate copper and tetraamminecopper are preferred.

[0070] More specifically, compounds for copper complex formation include at least one selected from ammonia, ammonium formate, and ethylenediaminetetraacetic acid. These compounds are preferably included in the mixture as aqueous solutions. In particular, the mixture is more preferably an aqueous solution of H4EDTA as the copper complex formation compound.

[0071] The amines used in the mixture include primary amines, secondary amines, and tertiary amines. Examples of amines include alkylamines. The mixture may contain ammonia in place of or in addition to amines. Hereafter, at least one selected from ammonia and amines will be referred to as amines. Amines may be included in the mixture as salt compounds. The mixture may contain only one type of amine, or two or more types. Amines are basic and react with copper complexes and / or copper salts in the mixture to obtain a copper precursor solution.

[0072] The solvent used in the mixture may be water, or a mixture of one or more aqueous solvents such as a mixture of water and an alcohol. The water may be purified water, deionized water, or pure water. Examples of alcohols include monohydric alcohols having 1 to 10 carbon atoms such as methanol, ethanol, isopropanol, n-propanol, isobutanol, and n-butanol, and polyhydric alcohols such as ethylene glycol, propylene glycol, diethylene glycol, polyethylene glycol, and glycerin. As the aqueous solvent, water or a mixture of water and a monohydric alcohol having 1 to 5 carbon atoms is preferred, water or a mixture of water and an alcohol selected from methanol, ethanol, and propanol is more preferred, and water is even more preferred. When a mixture of water and an alcohol is used as the solvent, for example, the alcohol content relative to the total amount of the water-alcohol mixture is preferably 1% by mass or more and 60% by mass or less. According to this manufacturing method, even when water is used as the solvent, a uniform copper precursor solution can be obtained, and by using the obtained copper precursor solution, a dense copper thin film can be formed through the process described later.

[0073] A copper precursor solution can be prepared by thoroughly stirring and mixing a copper complex and / or copper salt with amines in a solvent. Mixing may be carried out at room temperature, or the solvent may be heated to 40°C to 60°C to promote dissolution. Known stirring methods can be applied. Stirring methods include placing the solution containing the copper complex and / or copper salt with amines in a container and stirring with a rotor such as a magnetic stirrer, stirring with a stirring device equipped with a rotating stirring blade such as a paddle, placing the solution in a sealable container and stirring by shaking the container, and irradiating with ultrasonic waves. A simple method is to use a stirring device equipped with a stirring blade. The rotation speed of the rotor can be 300 rpm (revolutions / minute: the same applies below) to 800 rpm, with 400 rpm to 600 rpm being preferred. Stirring is preferably continued until the reaction between the copper complex and / or copper salt and the amines proceeds sufficiently. When stirring with a stirring device equipped with a rotor at room temperature as described above, stirring is preferably done for about 30 to 90 minutes, and more preferably for about 50 to 80 minutes. For example, when preparing a copper precursor solution containing a copper complex, a well-stirred copper precursor solution will exhibit a blue color due to copper ions.

[0074] From the viewpoint of obtaining a copper precursor of higher purity, step I preferably includes the following step I-2. Step I-2 is a reaction apparatus comprising a pair of electrolyte tanks connected via a channel equipped with a filter that does not allow copper ions to pass through but allows hydrogen ions to pass through, wherein an electrolyte containing an amine is stored in each of the pair of electrolyte tanks, and copper electrodes are placed in a position where at least a portion of them are in contact with the electrolyte, and the pair of electrodes are connected via a DC power supply, and a voltage is applied between the pair of electrodes by the DC power supply to react copper ions derived from the copper electrodes with the electrolyte in the electrolyte tank in which the electrode that will become the anode is immersed, in order to obtain a copper precursor solution.

[0075] A filter that does not allow copper ions to pass through but allows hydrogen ions to pass through is a filter that has the function of controlling permeability or non-permeability depending on the size of the ions, and is not particularly limited as long as it functions as a semipermeable membrane that does not allow copper ions to pass through but allows hydrogen ions to pass through. Examples of such filters include cellulose-based filters such as regenerated cellulose membranes (cellophane), acetylcellulose membranes, and collodion membranes; ceramic filters such as unglazed plates and porous ceramics; porous membranes such as polyacrylonitrile, polysulfone, and polyester polymer alloys; and semipermeable membranes selected from fluororesins, cellulose acetate, etc. Among these, cellulose filters selected from ceramic filters and cellulose tubing for dialysis are preferred from the viewpoint of having good durability even when in constant contact with the electrolyte. Examples of commercially available products include Visking tubing from Nippon Medical Science Co., Ltd., which is commercially available as a cellulose filter used in hemodialysis.

[0076] As the electrolyte, an electrolyte capable of reacting with the generated copper ions to form a copper complex is used. The electrolyte contains amines capable of forming a copper complex. The amines are the same as those described in the precursor method described in step I, and are preferably one or more compounds for copper complex formation selected from compounds having diamine-derived ligands such as NH3 ligands, RNH2 ligands (where R represents an alkylene group), ethylenediamine, and hexamethylenediamine as partial structures. It is preferable that the amines are included in the electrolyte as an aqueous solution. In addition to amines, the compounds for copper complex formation may also include compounds having an OH2 ligand as a partial structure. More specifically, the compounds for copper complex formation are preferably aqueous solutions containing at least one amine selected from ammonia, ammonium formate, and ethylenediaminetetraacetic acid (H4EDTA), which are included in the amines, and it is more preferable that they contain an aqueous solution of H4EDTA. The amines may also be included in the electrolyte as salt compounds.

[0077] The electrolyte may contain only one copper complex-forming compound, such as amines, or two or more. In particular, the electrolyte preferably contains at least one ammonia having an NH3 ligand, or an ammonium derivative such as ammonium formate having an RNH2 ligand, and at least one H4EDTA having a diamine-derived ligand. The content of copper complex-forming amines in the electrolyte is preferably in the range of 0.1% to 20% by mass, more preferably 0.5% to 10% by mass, and even more preferably 1.0% to 8% by mass.

[0078] The solvent for the electrolyte may be the same as that used in the mixture in step I as described above. The electrolyte can be prepared by mixing water, which is the solvent, with a compound containing amines for copper complex formation and stirring. The electrolyte may be prepared at room temperature (25°C), or the solvent may be heated to 30°C to 60°C to promote dissolution. It is preferable to continue stirring until the compound for copper complex formation is dissolved and the electrolyte is a visually uniform solution. When preparing the electrolyte at room temperature, it is preferable to stir for about 30 to 90 minutes, and more preferably for about 50 to 80 minutes. Stirring can be carried out using known stirring devices. Known stirring devices include stirrers, paddle mixers, impeller mixers, etc., but the stirring device is not limited to the above devices.

[0079] A voltage is applied between a pair of electrodes by a DC power supply, and in an electrolytic solution tank in which the electrode serving as the anode is immersed, a copper precursor liquid containing a reaction product obtained by reacting the electrolytic solution with copper ions derived from the anode electrode can be obtained. The previously prepared electrolytic solution is stored in each of a pair of electrolytic solution tanks, electrodes (copper plates) are placed at positions immersed in the electrolytic solution stored in the electrolytic solution tanks, and a voltage is applied between the electrode (anode) and the electrode (cathode) by a DC power supply. The voltage can be applied in a range exceeding 0V and not more than 100V, preferably in a range of 1V to 80V, and more preferably in a range of 10V to 60V. As the power supply, a known DC power supply can be appropriately selected and used. Examples of usable known DC power supplies include a stabilized DC power supply (PMC18-2, trade name, Kikusui Electronics Corporation).

[0080] The general reaction when a direct current is applied to the electrodes is, for example, the same as the reaction in copper electrolytic refining and the like. As shown in the following reaction formula, copper at the anode is oxidized and dissolved as copper ions, and a reduction reaction occurs at the cathode. Anode: Cu→Cu 2+ +2e - Cathode: H + +2e - →H2

[0081] Note that the above reaction similarly occurs when the same set of electrodes is arranged in one electrolytic solution tank and a voltage is applied. After that, when the reaction proceeds and the copper ion concentration in the electrolytic solution increases, over time, at the cathode, compared with the above hydrogen (H2) generation reaction, the reaction of Cu 2+ +2e - →Cu occurs preferentially. This is a phenomenon that occurs because the generated copper ions (Cu 2+ ) have a lower ionization tendency than hydrogen ions (H + ) generated on the cathode side. Therefore, as shown below, when the copper ion concentration in the electrolytic solution exceeds a predetermined amount, copper precipitates on the cathode side, the concentration of copper ions contained in the electrolytic solution does not increase beyond the predetermined amount, and when voltage application is continued, the generation efficiency of the metal complex tends to decrease over time. Anode: Cu→Cu2+ +2e - Cathode:Cu 2+ +2e - →Cu

[0082] In step I-2, a preferred embodiment of step I, a filter is provided in the flow path connecting the pair of electrolyte tanks. As a result, copper ions generated in the electrolyte tank where the anode is located do not move to the electrolyte tank where the cathode is located, but remain in the electrolyte in the electrolyte tank on the anode side, and react with compounds for copper complex formation in the electrolyte to form a copper complex. For example, when H4EDTA is used as a compound for copper complex formation, the following reaction occurs. Cu 2+ +H4EDTA→[Cu(H2EDTA)] 2- +2H + On the other hand, the hydrogen ions produced in this reaction can pass through the filter and move to the electrolyte tank on the cathode side, where the above-mentioned "H + +2e - The reaction "→H2" proceeds, and hydrogen is produced. The copper ions on the anode side are used to form copper complexes, so on the anode side, "Cu → Cu 2+ +2e - The reaction proceeds, and it is thought that a copper complex as a copper precursor is efficiently produced. Therefore, in the manufacturing method of this disclosure, by including step I-2, a copper precursor solution containing a high concentration of copper precursor stably can be efficiently produced without going through intermediates such as copper salt compounds.

[0083] (Process II) Step II is a step of preparing a copper thin film forming composition comprising the copper precursor solution obtained in Step I (preferably including Step I-2) and an organic reducing agent. In Step II, it is preferable to prepare the copper thin film forming composition by mixing the copper precursor solution obtained in Step I with an aqueous solution containing the organic reducing agent. The copper precursor solution used in Step II is a solution obtained in Step I that contains at least a copper complex and / or copper salt and amines. The copper complex contained in the copper precursor solution may be a reaction product of a copper salt, amines, and optionally further contained compounds for copper complex formation as described above, or it may be a pre-prepared copper complex. The copper precursor solution may contain only one type of copper complex and / or copper salt, or it may contain two or more types.

[0084] The organic reducing agent used in the preparation of the copper thin film forming composition preferably contains at least one compound selected from compounds having a carboxyl group. It is preferable to appropriately select and use an organic carboxylic acid compound that has a carboxyl group in its molecule and functions as an organic reducing agent. Examples of such organic reducing agents include at least one selected from ascorbic acid, citric acid, oxalic acid, formic acid, and 3,4,5-trihydroxybenzoic acid. From the viewpoint of better copper thin film formation, the organic reducing agent is preferably at least one selected from ascorbic acid, citric acid, and 3,4,5-trihydroxybenzoic acid, and more preferably at least one selected from ascorbic acid and citric acid. Including ascorbic acid as the organic reducing agent is one preferred embodiment of the copper thin film forming composition.

[0085] The organic reducing agent is preferably used as an aqueous solution. The water used to prepare the aqueous solution should not contain metal ions, or should have the lowest possible metal ion concentration, from the viewpoint of uniformity of the resulting copper thin film. Therefore, it is preferable to use purified water, deionized water, or pure water for preparing the aqueous solution. When dissolving the organic reducing agent in water, the water solvent may be heated to 30°C to 60°C, and preferably to 35°C to 45°C, to improve solubility. Dissolution may be carried out with stirring, and the stirring method can be the same as that described in the section on the preparation of the copper complex solution. The content of the organic reducing agent in the aqueous solution is preferably in the range of 10% to 40% by mass, and more preferably in the range of 10% to 30% by mass. A content of 10% by mass or more of the organic reducing agent relative to the total volume of the aqueous solution ensures that the aqueous solution contains sufficient organic reducing agent for the reaction, while a content of 40% by mass or less results in better stability of the aqueous solution.

[0086] In step II, there are no particular restrictions on the content of the copper precursor solution and the organic reducing agent in the copper thin film forming composition obtained by mixing the copper precursor solution and the organic reducing agent solution, and these can be appropriately selected according to the target copper thin film. The copper ions contained in the copper precursor solution can be 50 to 400 parts by mass per 100 parts by mass of the organic reducing agent contained in the copper thin film forming composition, and in particular, from the viewpoint of obtaining better copper thin film forming properties of the resulting copper thin film forming composition, it is preferable that the copper ions contained in the copper precursor solution are 100 to 350 parts by mass per 100 parts by mass of the organic reducing agent, and more preferably that the copper ions contained in the copper precursor solution are 150 to 350 parts by mass per 100 parts by mass of the organic reducing agent.

[0087] By setting the copper ion content in the organic reducing agent to the above-mentioned preferred range, a more efficient and denser copper thin film can be formed on the substrate. According to the inventors' theory, when the copper ion content is 50 parts by mass or more per 100 parts by mass of the organic reducing agent, the reducing power of the copper ions in the copper complex is further improved, leading to faster copper deposition through the reduction of copper ions attached to the substrate, and thus the formation of a dense copper thin film. Furthermore, when the copper ion content is 400 parts by mass or less per 100 parts by mass of the organic reducing agent, the copper deposition rate due to the reduction of copper ions is maintained within a favorable range, suppressing copper deposition by ammonia or amines in the copper precursor compound, and preventing the deposition of copper particles that do not adhere to the substrate due to the redissolution of the deposited copper thin film.

[0088] The resulting copper thin film forming composition is useful for forming copper thin films. The content of the metal precursor solution in the preparation of the copper thin film forming composition can be controlled by adjusting the type and content of the metal complex when preparing the metal precursor solution in step I, or by adjusting the type of electrolyte, the concentration of the electrolyte, the applied energy of the DC current, and the application time in step I-2. In general, it is difficult to measure the content of the copper complex and / or copper salt relative to the total amount of the copper thin film forming composition. However, the physical properties of the copper thin film formed by the copper thin film forming composition depend on the copper content in the copper thin film forming composition. From the viewpoint of being able to form a dense and uniform copper thin film, the copper content relative to the total amount of the copper thin film forming composition is preferably in the range of 0.5% to 10% by mass, and more preferably in the range of 1% to 8% by mass. When the copper content is within the above range, the structure of the copper thin film formed by the copper thin film forming composition becomes more uniform, and the electrical conductivity and thermal conductivity can be improved.

[0089] The copper content in a copper thin film forming composition can be measured, for example, by the method described in "Fundamentals of Coordination Chemistry: Werner Complexes and Organometallic Complexes" (KS Chemistry Textbook: Kodansha, 1989). On the other hand, the content of organic reducing agents in a copper thin film forming composition can be measured, for example, by the following method. First, the copper thin film forming composition is dried to produce a powder. The content of organic reducing agents can be measured by analyzing the obtained powder using a thermogravimeter-differential thermal analyzer (TG-DTA). As a specific example, the content of organic reducing agents in a copper thin film forming composition can be measured using a TG-DTA2000S (product name) manufactured by MacScience, Inc., while passing 100 ml (milliliters) / min of air through it, at a heating rate of 10°C / min.

[0090] The pH of the copper thin film forming composition at room temperature (25°C) is preferably 6 to 8, and more preferably in the neutral range around pH 7.5. The pH of the copper thin film forming composition can be measured using a known pH meter.

[0091] The copper thin film forming composition used in this manufacturing method contains an organic reducing agent as an organic component, and as a metallic component, it contains only copper ions that contribute to the formation of the desired copper thin film. It does not need to contain other metallic components, such as reducing metals used in displacement plating or catalysts used in electroless plating. Therefore, copper thin films formed with such a copper thin film forming composition do not contain catalysts, are highly pure, and can become dense copper thin films.

[0092] (Process III) Step III is the process of applying the copper thin film forming composition obtained in Step II to a substrate. The copper thin film forming composition obtained through Step II described above has copper complexes uniformly present at high concentrations in an aqueous solvent, and the stability of the copper complexes is good due to the function of the coexisting organic reducing agent. Since the copper complexes contained in the composition have good adsorption properties to the surface of hard substrates, a copper thin film with a dense structure can be formed on the substrate surface. In other words, in Step III, by applying the copper thin film forming composition to a substrate, the copper complexes are adsorbed onto the substrate surface, and a dense copper thin film is formed. Copper nanoparticles derived from the copper complexes adhere to the substrate to form a copper thin film, and the formed copper thin film can have excellent electrical and thermal conductivity. When the copper complexes contained in the copper thin film forming composition have ligands derived from ammonium groups, ethylenediamine, etc., the copper complexes can have particularly good adhesion to glass fiber substrates. Therefore, copper thin films formed using such copper complexes can be expected to have excellent adhesion to inorganic substrates.

[0093] In the manufacture of the heating element according to the first embodiment of the present invention described above, the substrate to which the copper thin film forming composition is applied is usually (c) a fibrous layer or a mesh-like layer. In this case, the copper thin film forming composition can be applied to the surface of the fibrous layer or mesh-like layer. Furthermore, in the manufacture of the heating element according to the second embodiment of the present invention described above, the substrate to which the copper thin film forming composition is applied may be a laminate in which (b) a polyvinyl chloride sol layer or a hot melt adhesive layer, (c) a fiber layer or a mesh-like layer, and (d) a polyvinyl chloride sol layer or a hot melt adhesive layer are laminated in this order. In this case, the copper thin film forming composition may be applied to the surface of the polyvinyl chloride sol layer or the hot melt adhesive layer.

[0094] In step III, the obtained copper thin film forming composition is applied to a substrate to form a layer of the copper thin film forming composition. Since the copper complex contained in the copper thin film forming composition has good adsorption properties to the substrate, a dense copper thin film is formed on the substrate by removing the solvent from the copper thin film forming composition layer. There are no particular restrictions on the method of applying the copper thin film forming composition to the substrate in step III, and known coating methods can be appropriately selected.

[0095] Methods for applying the copper thin film forming composition to a substrate include, for example, spray coating, spin coating, blade coating, bar coating, roll coating, die coating, and flow coating. Alternatively, the copper thin film forming composition may be applied to the substrate by casting. An appropriate coating method should be selected considering the physical properties of the copper thin film forming composition, such as viscosity, and the thickness of the copper thin film to be formed. As a method for locally applying the copper thin film forming composition to the substrate, printing methods such as screen printing and inkjet printing may be used. By using printing methods, a copper thin film can be formed locally only in a desired area of ​​the substrate. The amount of copper thin film forming composition applied is not particularly limited, but the wet film thickness is usually in the range of 10 nm to 200 μm, and preferably in the range of 20 nm to 100 μm.

[0096] After applying the copper thin film forming composition to the surface of the substrate to form a coating of the copper thin film forming composition (copper thin film forming composition layer), it is preferable to allow it to stand for a certain period of time, from the viewpoint of forming a denser film. The standing time is preferably 6 hours or more, and more preferably 12 hours or more, at room temperature (25°C). By allowing the copper thin film forming composition layer formed on the substrate to stand, the copper contained in the copper thin film forming composition is adsorbed onto the substrate to form a copper thin film. There is no particular upper limit to the standing time, but considering productivity, it can be 120 hours or less, and 90 hours or less is preferable.

[0097] Furthermore, when applying the copper thin film forming composition to the surface of a substrate to form a layer of the copper thin film forming composition and then allowing it to stand, the reaction rate increases by setting the ambient temperature of the standing area and the liquid temperature of the formed copper thin film forming composition layer to above room temperature, for example, 30°C or higher, preferably 40°C or higher. This allows for the formation of a dense copper thin film in a shorter standing time. From the viewpoint of minimizing the impact on the copper thin film forming composition, a temperature of 80°C or lower is preferred. For example, when the ambient temperature is 35°C, a standing time of 4 hours or more is preferred, and 8 hours or more is more preferred. The upper limit of the standing time is the same as in the case of room temperature. After the copper thin film is formed, any remaining copper thin film forming composition may be removed.

[0098] The thickness of the copper thin film layer formed on the substrate is not particularly limited and can be appropriately controlled by the amount of copper thin film forming composition applied to the substrate, the composition of the copper thin film forming composition, the contact time between the copper thin film forming composition and the substrate (standing time of the copper thin film forming composition layer), etc. From the viewpoint of balancing the imparting of heat generation in the heating element, the flexibility of the laminate design, and the manufacturing cost, the thickness of the copper thin film layer may usually be 10 nm to 100 μm, preferably 20 nm to 50 μm, 50 nm to 30 μm, 100 nm to 20 μm, or 200 nm to 10 μm.

[0099] (drying process) The present method for producing copper thin films may further include other steps in addition to steps I, II, and III. These other steps may include, for example, drying the copper thin film-forming composition applied in step III.

[0100] The solvent contained in the copper thin film forming composition can be removed by drying, allowing a copper thin film to be formed on the substrate. Drying includes natural drying at room temperature. Furthermore, by performing heat drying or other methods on the copper thin film forming composition as described later, a copper thin film that adheres more closely to the substrate can be formed more quickly than with natural drying. Here, drying refers to reducing the amount of solvent contained in the copper thin film forming composition, and does not necessarily mean completely removing the solvent.

[0101] Drying can be carried out by conventional methods. In addition to the aforementioned natural drying, drying methods include heat drying and drying by blowing air. When natural drying is performed, it is sufficient to leave it at room temperature for 60 minutes to 5 hours. When heat drying is performed, known heating methods can be appropriately selected and applied. Examples of heating methods include contacting the substrate with a heating means such as a plate heater or heat roll from the back surface, passing it through a heating zone such as an electric furnace, irradiating it with energy rays such as infrared rays or microwaves, and blowing hot air. There are no particular restrictions on the heating temperature when heat drying. Considering drying efficiency and minimizing the impact on the substrate, the heating temperature can be in the range of 30°C to less than 100°C, and is preferably in the range of 30°C to 60°C. When heat drying, the drying time is preferably in the range of 10 seconds to 20 minutes from the viewpoint of productivity.

[0102] The process of applying the copper thin film forming composition to a substrate and drying the copper thin film forming composition applied to the substrate may be repeated multiple times. By applying the copper thin film forming composition to the substrate and then drying the copper thin film forming composition, a copper thin film is formed on the substrate. Subsequently, when the copper thin film forming composition is applied again to the substrate on which the copper thin film has been formed, the metal complex contained in the copper thin film forming composition is adsorbed onto the surface of the copper thin film formed on the substrate. By drying it thereafter, a thicker copper thin film is formed.

[0103] When a copper thin film forming composition is applied to a substrate on which a copper thin film has already been formed, the copper thin film forming composition comes into contact with the already formed copper thin film. Copper precursors contained in the copper thin film forming composition adhere between the copper particles contained in the already formed copper thin film, causing copper nanoparticles to grow and accelerating copper deposition. As a result, the copper nanoparticles contained in the copper thin film become more densely packed, which is expected to improve not only the thickness of the copper thin film but also its physical properties, such as electrical conductivity.

[0104] According to this manufacturing method, small amounts of solvent-derived impurities may remain in the copper thin film, but these are mainly carbon atoms derived from the solvent used as a raw material, and there is no concern that they will impair the properties of the formed copper thin film. This is a significant advantage compared to electroless plating films that require catalysts, and copper thin films formed by precursor methods using anionic copper complexes.

[0105] According to this manufacturing method, a copper thin film can be uniformly formed over the entire surface of the substrate. Furthermore, a copper thin film can also be formed in a patterned manner. As described above, a patterned copper thin film can be formed by applying a copper thin film forming composition to the substrate in an arbitrary pattern using a printing method. As a method for forming a patterned copper thin film, another method is to form a uniform copper thin film on the substrate and then pattern it using a known method such as etching to form a patterned copper thin film.

[0106] In this manufacturing method, by using a solution containing the above-mentioned single-walled carbon nanotube and SiO2 composite instead of the copper thin-film forming composition, a layer of single-walled carbon nanotube-SiO2 thin film can be formed on the substrate as a conductive thin film layer. A non-limiting specific example of a method for forming a layer of single-walled carbon nanotube-SiO2 thin film as a conductive thin film layer on a substrate is to put 100 μL of a solution containing a composite of single-walled carbon nanotube and SiO2 into a quartz glass substrate (20 × 20 mm) using a micropipette. 2 A single-walled carbon nanotube-SiO2 thin film can be formed by dropping the material onto a surface, then forming a thin film using a two-stage spin-coating method (first stage: 500 rpm for 5 seconds, second stage: 2000 rpm for 30 seconds), and finally drying it at 70°C for 10 minutes. These manufacturing conditions can be adjusted according to the desired thin film thickness, etc.

[0107] 5. Manufacturing method of thermal tiles for residential use Using one of the above-mentioned residential heating elements, a residential thermal tile can be obtained by laminating (1) a decorative sheet, (2) a middle backer, (3) a residential heating element, (4) a middle backer, and (5) a bottom backer in this order. The (1) decorative sheet, (2) and (4) middle backer, and (5) bottom backer that make up the residential thermal tiles can also be any of the above-mentioned types.

[0108] The method for obtaining a residential thermal tile by laminating (1) a decorative sheet, (2) a middle backer, (3) a heating element for residential use, (4) a middle backer, and (5) a bottom backer in this order is not particularly limited, and any method known in the industry may be used. For example, a first partial laminate consisting of (1) a decorative sheet and (2) a middle backer (and optionally a clear layer provided on the surface side of (1) the decorative sheet) can be pre-formed using any lamination method known in the industry, and a second partial laminate consisting of (4) a middle backer and (5) a bottom backer can be pre-formed. Then, the (2) middle backer side of the first partial laminate faces one side of the (3) residential heating element, and the (4) middle backer side of the second partial laminate faces the other side of the (3) residential heating element, and the two laminates can be hot-laminated (hot-pressed). In this case, a heat-resistant adhesive may be optionally interposed between the layers during hot lamination (hot-pressing). The temperature, time, and other conditions for the hot lamination can be appropriately selected from suitable conditions known in the industry. The heat-resistant adhesive for hot lamination is not particularly limited, but for example, one or more types of epoxy resins, polyimide resins, silicone resins, etc., can be used.

[0109] In particular, as described above, in the (3) residential heating element according to the second embodiment, if one or more holes are formed in the (a) conductive thin film layer, the plastic sol or hot melt adhesive of the (b) layer, which is softened and melted by heating, can penetrate these holes, thereby joining and bonding the (3) residential heating element to the (2) middle backer positioned above it. In addition, the plastic sol or hot melt adhesive of the (d) layer, which is softened and melted by heating in the (3) residential heating element, can join and bond the (3) residential heating element to the (4) middle backer positioned below it.

[0110] Furthermore, residential thermal tiles can be formed to cover a predetermined area to be heated by joining together multiple thermal tile pieces, each having a roughly square or rectangular planar shape with a side length in the range of approximately 100 mm to approximately 1500 mm, typically in the range of approximately 150 mm to approximately 900 mm. The size of the planar shape of the thermal tile pieces may be, for example, roughly square or rectangular, such as approximately 300 mm × approximately 300 mm, approximately 450 mm × approximately 450 mm, approximately 900 mm × approximately 900 mm, or approximately 150 mm × approximately 900 mm. The installation of the residential thermal tiles according to the present invention is not particularly limited, but can be carried out by methods such as those described below. Furthermore, a combination of these methods can be used. (I) One or more electrode wires may be inserted from the bottom side (floor side) of each thermal tile piece toward the surface side opposite the bottom side, to the (5) bottom backer, (4) middle backer, and (3) conductive thin film layer of the residential heating element, and the lower ends of the electrode wires inserted into each thermal tile piece may be connected to each other. This makes it possible to spread electrode wires throughout the entire thermal tile consisting of multiple pieces. (II-a) A thin copper tape (e.g., approximately 0.2 mm to 0.3 mm thick) may be applied continuously to substantially the entire peripheral edge (e.g., approximately 5 mm to 10 mm wide) of the middle backer side surface of the (a) conductive thin film layer of the (3) residential heating element of each heating tile piece, and to substantially the entire side surface of the (a) conductive thin film layer. This allows the thin copper tape to function as an electrode on each heating tile piece, ensuring reliable electrical connection of the conductive thin film layers of each heating element throughout the entire heating tile consisting of multiple pieces. (II-b) A further conductive thin film layer may be provided on the side opposite to (the bottom side) of the (a) conductive thin film layer of the (3) residential heating element of each heating tile piece, in contact with the surface of the (c) fiber layer or mesh layer or the (d) plastic sol layer or hot melt adhesive layer. Then, a thin copper tape (e.g., about 0.2 mm to about 0.3 mm thick) may be applied continuously to substantially the entire periphery (e.g., about 5 mm to about 10 mm wide) of the (2) middle backer side surface of the former (a) conductive thin film layer, substantially the entire periphery (e.g., about 5 mm to about 10 mm wide) of the (4) middle backer side surface of the latter further conductive thin film layer, and substantially the entire side surface of the laminate including the former (a) conductive thin film layer and the latter further conductive thin film layer. This allows the thin copper tape to function as an electrode on each heating tile piece, making the electrical connection of the conductive thin film layers of each heating element more reliable throughout the entire heating tile consisting of multiple pieces. (III-a) Each thermal tile piece may be laminated such that two sides of the (a) conductive thin film layer (approximately square or rectangular planar shape) of the (3) residential heating element are exposed by a predetermined width (for example, about 5 mm to about 10 mm) to the corresponding two sides of the (2) middle backer and the (c) fibrous layer or mesh layer or (b) plastic sol layer or hot melt adhesive layer of the (3) residential heating element. By joining thermal tile pieces with partially exposed conductive thin film layers to each other to form a thermal tile, electrical connection of the conductive thin film layer of each heating element can be ensured. (III-b) A further conductive thin film layer may be provided on the side of each thermal tile piece opposite to the conductive thin film layer of the (a) residential heating element (bottom side), in contact with the surface of the (c) fiber layer or mesh layer or the (d) plastic sol layer or hot melt adhesive layer. The former (a) conductive thin film layer (approximately square or rectangular planar shape) may be laminated so that two sides are exposed to the corresponding two sides of the (2) middle backer and the corresponding two sides of the (c) fiber layer or mesh layer or the (b) plastic sol layer or hot melt adhesive layer of the (3) residential heating element by a predetermined width (for example, about 5 mm to about 10 mm), while the latter further conductive thin film layer (approximately square or rectangular planar shape) may be laminated so that two sides are exposed to the corresponding two sides of the (4) middle backer and the corresponding two sides of the (c) fiber layer or mesh layer or the (d) plastic sol layer or hot melt adhesive layer of the (3) residential heating element by a predetermined width (for example, about 5 mm to about 10 mm). In this case, the exposed edges of the former conductive thin film layer and the exposed edges of the latter further conductive thin film layer may be in corresponding directions, or they may be in partially different directions. By joining together these two partially exposed conductive thin film layers to form a thermal tile, the electrical connection of the conductive thin film layers of each heating element can be made even more reliable. [Examples]

[0111] The present invention will be described below with reference to examples, but the present invention is not limited to these examples.

[0112] Measurement of the surface temperature of a heating element The following thermometer was used to measure the surface temperature of the heating element (the conductive thin film layer that makes up the surface). Shinwa Measuring Instruments Co., Ltd. Infrared thermometer with laser pointing function • Measurement range: -60 to 500℃ • Distance coefficient D:S = 12:1 (D = distance, S = diameter of the measurement range) ·Material body ABS resin Dimensions: 185mm x 46mm x 143mm, Weight: 240g • Power supply: 2 AAA alkaline batteries; Accuracy: ±2% or ±2 (the higher value applies) • Battery life: 14 hours continuous use, laser wavelength: 635-660nm

[0113] Example 1: Example of manufacturing a heating element by forming a copper thin film on glass fiber. 67.4 g of copper sulfate pentahydrate was added to 1161 ml of pure water and stirred at room temperature for 5 minutes. Then 109.3 ml of aqueous ammonia was added and stirred at room temperature for 1 hour to obtain an aqueous copper complex solution (copper precursor solution). Furthermore, 161.7 g of L-ascorbic acid was added to this aqueous copper complex solution as an organic reducing agent and stirred at room temperature for 20 minutes to obtain a copper thin film forming composition (Cu 2+ A concentration of 0.18 mmol / g was obtained. 100 x 100 mm 2 A 100 μm thick coupling agent-treated urethane sol coated glass fiber film (raw fabric cloth M95F107 obtained from Unitika Ltd.) was immersed in IPA (isopropyl alcohol), washed by ultrasonic irradiation for 15 minutes twice, and dried in a 70°C dryer for 10 minutes. The washed glass fiber film was immersed in a container (24 mm deep) containing the above-mentioned copper thin film forming composition and left to stand in a 24°C incubator for 24 hours. Next, this coated glass fiber film was immersed in 1 L of pure water and shaken for 1 minute, and this operation was repeated three times. Then, it was dried in a 70°C dryer for 1 hour to obtain a heating element in which a copper thin film layer was formed on the glass fiber film layer.

[0114] When a predetermined voltage was applied to this copper thin film layer and the surface temperature was measured after 10 minutes, the following results were obtained: For voltages of 1.5V, 2.5V, and 3.0V, the temperature reached a substantially constant level after 5 minutes. Furthermore, for a voltage of 3.5V, the temperature exceeded approximately 45°C after 5 minutes, and for a voltage of 4.0V, the temperature exceeded approximately 50°C after 5 minutes. Voltage 1.5V - Surface temperature after 10 minutes: 28℃ Voltage 2.5V - Surface temperature after 10 minutes: 37℃ Voltage 3.0V - Surface temperature after 10 minutes: 42℃ Voltage 3.5V - Surface temperature after 10 minutes: 50℃ Voltage 4.0V - Surface temperature after 10 minutes: 60℃

[0115] Example 2: Single-walled carbon nanotubes-SiO2 onto glass fiber 2 Examples of manufacturing heating elements by thin-film formation A single-walled carbon nanotube-SiO2 composite was obtained by the following procedure, including spin coating. 10 g of ethanol was mixed with 5.2 g of oxalic acid (anhydrous) and stirred at room temperature for 30 minutes. Then 4.0 g of tetraethoxysilane was added and refluxed for 1 hour to form a SiO2 thin film composition (Si 4+ A concentration of 1.0 mmol / g was obtained. To 3.0 g of a single-walled carbon nanotube ethanol dispersion solution (0.2 wt%), 0.5 g of the SiO2 thin film formation composition obtained above and 1.5 g of ethanol were added, and the mixture was stirred at room temperature for 1 hour to obtain a single-walled carbon nanotube-SiO2 thin film formation composition. 100 x 100 mm 2 A 100 μm thick coupling agent-treated urethane sol coated glass fiber film (raw fabric cloth M95F107 obtained from Unitika Ltd.) was immersed in IPA (isopropyl alcohol), washed with two 15-minute ultrasonic irradiations, and dried in a 70°C oven for 10 minutes. 2 ml of ethanol was applied to the surface of the washed glass fiber film using a two-stage spin coating method: 500 rpm for 5 seconds, followed by 2000 rpm for 30 seconds. Then, 2 ml of the single-walled carbon nanotube-SiO2 thin film formation composition obtained above was applied using a spin coating method at 500 rpm for 10 seconds, and dried in a 70°C oven for 10 minutes to obtain a heating element with a single-walled carbon nanotube-SiO2 thin film layer formed on the glass fiber film layer. When a predetermined voltage was applied to this single-walled carbon nanotube-SiO2 thin film layer and the surface temperature was measured after 10 minutes, the following results were obtained: For voltages of 10V, 20V, and 30V, the temperature reached a substantially constant level after 5 minutes. Voltage 10V - Surface temperature after 10 minutes: 24℃ Voltage 20V - Surface temperature after 10 minutes: 28℃ Voltage 30V - Surface temperature after 10 minutes: 37℃

[0116] Comparative Example 1 In Example 1, instead of glass fiber, a stainless steel mesh plate (10 mesh, 0.4 mm thick) purchased from Monotaro was cut to 100 mm x 100 mm and used to obtain a heating element. This heating element could be thermally laminated and had good adhesion to the backing material, but it had a low resistance and did not generate heat.

[0117] Comparative Example 2 In Example 1, instead of glass fiber, a copper mesh (200 mesh, 0.077 mm opening) purchased from Monotaro was used to obtain a heating element. This heating element could be thermally laminated and had good adhesion to the backing material, but it had a low resistance and did not generate heat.

[0118] Comparative Example 3 In Example 1, instead of glass fiber, a transparent film heater without adhesive (double-sided PET) measuring 100mm x 100mm (terminal treatment: lug terminals attached to two electrode locations, thickness: 0.14~0.2mm) purchased from Monotaro was used to obtain a heating element. In this heating element, the transparent film heater deformed during the thermal lamination process, and the adhesion to the backing material was also insufficient.

[0119] Comparative Example 4 In Example 1, instead of glass fiber, an aluminum foil heater (15W capacity, 100 x 100 mm) purchased from Monotaro was used to obtain a heating element. The heating element had insufficient adhesion to the backing material, resulting in unevenness on the surface that detracted from the aesthetic appeal of the tile.

[0120] According to the embodiments of the present invention described above, it is understood that a residential heating element that provides sufficient heat with low power and has high energy efficiency can be obtained by a simple method. Such residential heating elements can be suitably used to construct articles such as residential thermal tiles with excellent design qualities by laminating decorative sheets via a middle backer. [Explanation of Symbols]

[0121] 1: Conductive thin film layer 2: Polyvinyl chloride sol layer or hot melt adhesive layer 3: Fibrous layer or mesh-like layer 4: Polyvinyl chloride sol layer or hot melt adhesive layer 100: Heating element for residential use 10: Decorative sheet 20: Middle Backer 100a: Heating element for residential use 30: Middle Backer 40: Bottombacker 200: Thermal tiles for residential use

Claims

1. (a) conductive thin film layer, and (c) Fibrous layer or mesh-like layer A residential heating element in which the following are stacked: The conductive thin film layer is a copper thin film or a single-walled carbon nanotube-SiO 2 It is a thin layer, The (c) fibrous layer or mesh-like layer is a fibrous layer or mesh-like layer formed from at least one selected from glass fibers and ceramic mesh. Heating element for residential use.

2. A heating element for residential use according to claim 1, wherein (a) a conductive thin film layer, (b) a plastic sol layer or a hot melt adhesive layer, (c) a fiber layer or a mesh-like layer, and (d) a plastic sol layer or a hot melt adhesive layer are laminated in this order.

3. The heating element for residential use according to claim 2, wherein the (b) plastic sol layer or hot melt adhesive layer and / or the (d) plastic sol layer or hot melt adhesive layer are integrated with the (c) fiber layer or mesh-like layer, so that at least a portion of the surface of the fiber or mesh-like material constituting layer (c) is covered with the plastic sol or hot melt adhesive constituting layers (b) and / or (d).

4. The heating element for residential use according to claim 1, wherein the conductive thin film layer (a) is a thin film layer having a thickness of 10 nm to 100 μm, which is produced by a molecular precursor method.

5. An article comprising a heating element for residential use as described in any one of claims 1 to 4.

6. The article according to claim 5, having at least one use selected from heating, heat retention, snow melting, condensation prevention, and anti-fogging.

7. (1) Decorative sheet, (2) Middle backer, (3) A heating element for residential use according to any one of claims 2 to 4, (4) Middle backer, and (5) Bottom backer These are residential thermal tiles stacked in this order.

8. A method for manufacturing a heating element for residential use, (c) A step of forming a conductive thin film layer (a) on a substrate containing a fibrous layer or a mesh-like layer by a molecular precursor method to obtain a residential heating element which is a laminate containing the conductive thin film layer (a) and the fibrous layer or mesh-like layer, The conductive thin film layer is a copper thin film or a single-walled carbon nanotube-SiO 2 It is a thin layer, The (c) fibrous layer or mesh-like layer is a fibrous layer or mesh-like layer formed from at least one selected from glass fibers and ceramic mesh. A method for manufacturing heating elements for residential use.

9. The method according to claim 8, wherein the substrate containing the (c) fibrous layer or mesh-like layer is a laminated substrate containing, in this order, (b) a plastic sol layer or hot melt adhesive layer, the (c) fibrous layer or mesh-like layer, and (d) a plastic sol layer or hot melt adhesive layer.

10. The present invention relates to obtaining a residential thermal tile by using the residential heating element manufactured by the method of claim 8 or claim 9, and laminating (1) a decorative sheet, (2) a middle backer, (3) the residential heating element, (4) a middle backer, and (5) a bottom backer in this order. A method for manufacturing thermal tiles for residential use.

Citation Information

Patent Citations

  • METAL FILM PRODUCTION METHOD, METAL FILM FORMING COMPOSITION, AND METAL FILM LAMINATE

    JP7506404B2