Injection molded body for mobile vehicle and method for manufacturing an injection molded body for mobile vehicle

A five-layered injection-molded article with controlled fiber orientation in odd and even layers, manufactured via a two-step process, addresses mechanical strength issues by ensuring uniform fiber alignment and structural integrity without adhesive layers.

JP2026182442APending Publication Date: 2026-11-19TOYODA GOSEI CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2025078686
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-09
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Conventional injection-molded articles for mobile bodies require further improvements in mechanical strength, particularly due to the orientation of reinforcing fibers being influenced by the molding process, leading to uneven fiber alignment and reduced structural integrity.

Method used

The injection-molded articles are designed with a five-layer structure where the primary orientation direction of reinforcing fibers in odd-numbered layers is perpendicular to that in even-numbered layers, with continuous changes in orientation tensors between adjacent layers, and are manufactured using a two-step process involving gates oriented in different directions to control fiber alignment.

Benefits of technology

This configuration enhances mechanical strength by ensuring uniform fiber orientation throughout the thickness of the molded body, improving structural integrity without the need for adhesive layers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026182442000001_ABST
    Figure 2026182442000001_ABST
Patent Text Reader

Abstract

This allows for an improvement in mechanical strength. [Solution] The injection-molded body for the mobile body is made of thermoplastic resin containing reinforcing fibers. When the direction perpendicular to the thickness direction of the injection-molded body is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, the injection-molded body consists of five overlapping layers 11, 12, 13, 12, 11 in the thickness direction. The primary orientation direction of the reinforcing fibers in the odd-numbered layers 11 and 13 from one side of the thickness direction is the first direction, and the primary orientation direction of the reinforcing fibers in the even-numbered layer 12 from one side of the thickness direction is the second direction. The orientation tensor Ax in the first direction and the orientation tensor Ay in the second direction of the reinforcing fibers change continuously between adjacent layers.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an injection-molded article for mobile bodies and a method for producing the injection-molded article for mobile bodies.

Background Art

[0002] Conventionally, there are automobile parts that are injection-molded articles (see, for example, Patent Document 1). As shown in Figure 5, a conventional injection-molded article 110 including the one disclosed in Patent Document 1 is formed by injection molding a molten thermoplastic resin (hereinafter referred to as resin 20) containing reinforcing fibers 21.

[0003] As shown in Figure 5 and Figure 6, the injection-molded article 110 is composed of three layers 132, 131, 132 in which the main orientation directions of the reinforcing fibers 21 in adjacent layers differ by 90 degrees. As shown in Figure 7 and Figure 8, when a molten thermoplastic resin containing reinforcing fibers 21 (hereinafter referred to as molten resin) is supplied into the cavity 153 of the mold 150 through the gate 151 oriented in the first direction X, a core layer 131 and skin layers 132 located between the core layer 131 and the molding surfaces of the cavity 153 are formed.

[0004] Here, in the skin layer 132, the reinforcing fibers 21 are likely to be oriented in the first direction X, which is the flow direction of the molten resin, because the skin layer 132 is easily affected by the molding surfaces of the cavity 153 whose temperature is lower than that of the molten resin. As a result, the main orientation direction of the reinforcing fibers 21 in the skin layer 132 is the first direction X. In addition, in the core layer 131, the reinforcing fibers 21 are likely to be oriented in a direction orthogonal to both the flow direction of the molten resin and the thickness direction Z, so the main orientation direction of the reinforcing fibers 21 in the core layer 131 is the second direction Y.

Prior Art Documents

Patent Documents

[0005]

Patent Document 1

Summary of Invention

[0006] Further improvements in mechanical strength are required for injection-molded products. [Means for solving the problem]

[0007] This paper describes various embodiments of injection-molded articles for mobile bodies and methods for manufacturing injection-molded articles for mobile bodies that address the above-mentioned problems. [Aspect 1] An injection-molded mobile body made of thermoplastic resin containing reinforcing fibers, When the direction perpendicular to the thickness direction is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, It consists of five layers that overlap in the thickness direction, Of the five layers, the primary orientation direction of the reinforcing fibers in the odd-numbered layers from one side in the thickness direction is the first direction, and the primary orientation direction of the reinforcing fibers in the even-numbered layers from one side in the thickness direction is the second direction. The orientation tensor in the first direction and the orientation tensor in the second direction of the reinforcing fiber change continuously between adjacent layers. Injection molded body for moving objects.

[0008] In this configuration, the primary orientation direction of the reinforcing fibers in the odd-numbered layers of the five layers constituting the injection-molded body is the first direction, while the primary orientation direction of the reinforcing fibers in the even-numbered layers is the second direction. In other words, the primary orientation directions of adjacent layers differ by 90 degrees from each other. Furthermore, the injection-molded body does not have an adhesive layer that bonds the layers together but does not contain reinforcing fibers. That is, reinforcing fibers are present throughout the entire thickness direction of the injection-molded body.

[0009] Therefore, it is possible to improve mechanical strength. [Aspect 2] A method for manufacturing an injection-molded body for a mobile device, comprising supplying a molten thermoplastic resin containing reinforcing fibers into the cavity of a mold, When the direction perpendicular to the thickness direction of the cavity is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, A first step of forming a first core layer and a first skin layer located between the first core layer and the molded surface of the cavity, wherein the main orientation direction of the reinforcing fibers is the first direction, by supplying the molten thermoplastic resin containing the reinforcing fibers to the cavity through a first gate oriented in the first direction, The method comprises a second step of supplying the molten thermoplastic resin containing the reinforcing fibers to the cavity through a second gate oriented in the second direction, thereby creating a molten first core layer, a molten portion of the first skin layer adjacent to the first core layer flowing in the second direction, resulting in a second core layer in which the main orientation direction of the reinforcing fibers is the first direction, and a second skin layer located between the second core layer and the first skin layer, in which the main orientation direction of the reinforcing fibers is the second direction. A method for manufacturing injection-molded articles for mobile devices.

[0010] According to this method, in the first step, a molten thermoplastic resin containing reinforcing fibers (hereinafter referred to as molten resin) is supplied to the cavity through a first gate oriented in a first direction. This forms a first core layer and a first skin layer located between the first core layer and the molded surface of the cavity. In the first skin layer, the reinforcing fibers tend to orient in the first direction, which is the flow direction of the molten resin, because they are more susceptible to the influence of the molded surface of the cavity, which is at a lower temperature than the molten resin. As a result, the primary orientation direction of the reinforcing fibers in the first skin layer is the first direction. In the first core layer, the reinforcing fibers tend to orient in a direction perpendicular to both the flow direction and the thickness direction of the molten resin, so the primary orientation direction of the reinforcing fibers in the first core layer is the second direction.

[0011] Next, in the second step, molten resin is supplied to the cavity through a second gate oriented in the thickness direction and in a second direction perpendicular to the first direction. As a result, the molten first core layer and the molten portion of the first skin layer adjacent to the first core layer flow in the second direction, forming a second core layer and a second skin layer located between the second core layer and the first skin layer. In the second skin layer, the reinforcing fibers tend to orient in the second direction, which is the flow direction of the molten resin, because they are more susceptible to the influence of the relatively lower temperature of the first skin layer. Consequently, the main orientation direction of the reinforcing fibers in the second skin layer is the second direction. In the second core layer, the reinforcing fibers tend to orient in a direction perpendicular to both the flow direction and the thickness direction of the molten resin, so the main orientation direction of the reinforcing fibers in the second core layer is the first direction.

[0012] Therefore, the aforementioned injection-molded articles can be manufactured. [Effects of the Invention]

[0013] According to the present invention, it is possible to improve mechanical strength. [Brief explanation of the drawing]

[0014] [Figure 1] Figure 1 is a cross-sectional view showing the layer structure of an injection-molded body for a mobile device according to one embodiment. [Figure 2] Figure 2 is a graph showing the relationship between the position in the thickness direction of an injection-molded body in one embodiment and each orientation tensor. [Figure 3] Figure 3 is a cross-sectional view of a mold according to one embodiment. [Figure 4] Figure 4(a) is a cross-sectional view showing the state of the molten resin inside the mold during the first step of one embodiment, and Figure 4(b) is a cross-sectional view showing the state of the molten resin inside the mold during the second step of one embodiment. [Figure 5] Figure 5 is a cross-sectional view showing the layer structure of a conventional injection-molded body. [Figure 6] Figure 6 is a graph showing the relationship between the position in the thickness direction of a conventional injection-molded body and each orientation tensor. [Figure 7]Figure 7 is a cross-sectional view of a conventional mold. [Figure 8] Figure 8 is a cross-sectional view showing the interior state of a conventional mold. [Mode for Carrying Out the Invention]

[0015] Hereinafter, one embodiment will be described with reference to Figures 1 to 4. <Configuration of Injection Molded Article> As shown in Figure 1, an injection molded article for a moving body (hereinafter referred to as injection molded article 10) is made of a thermoplastic resin containing reinforcing fibers 21 (hereinafter referred to as resin 20).

[0016] The resin 20 is, for example, polypropylene. The reinforcing fibers 21 are, for example, glass fibers. In the following description, the thickness direction of the injection molded article 10 (the vertical direction in Figure 1) is defined as thickness direction Z, the direction orthogonal to thickness direction Z (the horizontal direction in Figure 1) is defined as first direction X, and the direction orthogonal to both thickness direction Z and first direction X (the direction perpendicular to the plane of the drawing in Figure 1) is defined as second direction Y.

[0017] The injection molded article 10 is composed of five layers 11, 12, 13, 12, 11 that overlap in the thickness direction Z. Specifically, the injection molded article 10 has first skin layers 11 located at both ends in the thickness direction Z, second skin layers 12 adjacent to the inner side of the first skin layers 11 in the thickness direction Z, and a second core layer 13 located between the second skin layers 12.

[0018] The main orientation direction of the reinforcing fibers 21 in the first skin layers 11 and the second core layer 13 is the first direction X. That is, among the five layers 11, 12, 13, 12, 11, the main orientation direction of the reinforcing fibers 21 in the odd-numbered layers 11, 13 counted from one side in the thickness direction Z is the first direction X.

[0019] The primary orientation direction of the reinforcing fibers 21 in the second skin layer 12 is the second direction Y. That is, among the five layers 11, 12, 13, 12, 11, the primary orientation direction of the reinforcing fibers 21 in the even-numbered layer 12 from one side of the thickness direction Z is the second direction Y.

[0020] Figure 2 shows the relationship between the thickness direction position (mm) of the injection-molded body 10, which is the position in the thickness direction Z, and the orientation tensor Ax in the first direction X, the orientation tensor Ay in the second direction Y, and the orientation tensor Az in the thickness direction Z. At any thickness direction position, the sum of the orientation tensors Ax, Ay, and Az is 1.

[0021] As shown in Figure 2, in the first skin layer 11 on the far left of Figure 2, the orientation tensor Ax in the first direction X is larger than the orientation tensor Ay in the second direction Y and the orientation tensor Az in the thickness direction Z. Furthermore, as we approach the second skin layer 12 in the thickness direction Z, the orientation tensor Ax in the first direction X decreases sharply, while the orientation tensor Ay in the second direction Y increases sharply.

[0022] In the second skin layer 12, the second from the left in Figure 2, the orientation tensor Ay in the second direction Y is greater than the orientation tensor Ax in the first direction X and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ay in the second direction Y increases sharply with increasing position in the thickness direction, and then gradually decreases as it approaches the second core layer 13 in the thickness direction. On the other hand, the orientation tensor Ax in the first direction X decreases sharply with increasing position in the thickness direction, and then gradually increases as it approaches the second core layer 13 in the thickness direction.

[0023] In the second core layer 13, the orientation tensor Ax in the first direction X is greater than the orientation tensor Ay in the second direction Y and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ax in the first direction X gradually increases with increasing position in the thickness direction, and then gradually decreases as the position in the thickness direction approaches the second core layer 13. On the other hand, the orientation tensor Ay in the second direction Y gradually decreases with increasing position in the thickness direction, and then gradually increases as the position in the thickness direction approaches the second skin layer 12, which is the second from the right in Figure 2.

[0024] In the second skin layer 12, the second from the right in Figure 2, the orientation tensor Ay in the second direction Y is greater than the orientation tensor Ax in the first direction X and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ay in the second direction Y gradually increases with increasing position in the thickness direction, and then decreases sharply as the position in the thickness direction approaches the rightmost first skin layer 11. On the other hand, the orientation tensor Ax in the first direction X gradually decreases with increasing position in the thickness direction, and then increases sharply as the position in the thickness direction approaches the rightmost first skin layer 11.

[0025] In the first skin layer 11 on the far right of Figure 2, the orientation tensor Ax in the first direction X is greater than the orientation tensor Ay in the second direction Y and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ax in the first direction X gradually increases with increasing position in the thickness direction, while the orientation tensor Ay in the second direction Y gradually decreases with increasing position in the thickness direction.

[0026] As explained above, the orientation tensor Ax in the first direction X and the orientation tensor Ay in the second direction Y of the reinforcing fiber 21 change continuously between adjacent layers 11, 12, 13, 12, 11.

[0027] <Method for manufacturing injection-molded articles> Next, the method for manufacturing the injection-molded article 10 will be described with reference to Figures 3 and 4. The method for manufacturing the injection-molded article 10 involves supplying a molten thermoplastic resin containing reinforcing fibers 21 (hereinafter referred to as molten resin) to the cavity 53 of the mold 50.

[0028] As shown in Figure 3, the mold 50 for molding the injection-molded body 10 has a cavity 53. In the following explanation, the thickness direction of the cavity 53 (the direction perpendicular to the plane of the paper in Figure 3) will be referred to as the thickness direction Z, the direction perpendicular to the thickness direction Z (the left-right direction in Figure 3) will be referred to as the first direction X, and the direction perpendicular to both the thickness direction Z and the first direction X (the up-down direction in Figure 3) will be referred to as the second direction Y.

[0029] The mold 50 has a first gate 51 that points in a first direction X and a second gate 52 that points in a second direction Y. The first gate 51 is, for example, one end of the cavity 53 in the first direction X (the left end in Figure 3), and multiple gates are provided spaced apart from each other in the second direction Y. In this embodiment, three first gates 51 are provided.

[0030] The second gate 52 opens, for example, in the center of the cavity 53 in the first direction X and the center in the second direction Y. The method for manufacturing the injection-molded body 10 comprises a first step and a second step.

[0031] <1st process> As shown by the white arrows in Figure 3, in the first step, molten resin is supplied to the cavity 53 through the first gate 51. This forms a first core layer 31 and a first skin layer 32 located between the first core layer 31 and the molding surface of the cavity 53, with the main orientation direction of the reinforcing fibers 21 being the first direction X, as shown in Figure 4(a).

[0032] Once the first process is complete, the supply of molten resin is stopped by closing the first gate 51. <Second process> The second step is performed after the first step.

[0033] As shown by the black arrow in Figure 3, in the second step, molten resin is supplied to the cavity 53 through the second gate 52. As a result, as shown in Figure 4(b), the molten first core layer 31 and the molten portion of the first skin layer 32 adjacent to the first core layer 31 are flowed in the second direction Y, resulting in a second core layer 13 where the main orientation direction of the reinforcing fibers 21 is the first direction X, and a second skin layer 12 located between the second core layer 13 and the first skin layer 32(11), where the main orientation direction of the reinforcing fibers 21 is the second direction Y.

[0034] <Operation of this embodiment> In the injection-molded body 10, the primary orientation direction of the reinforcing fibers 21 in the odd-numbered layers 11 and 13 is the first direction X, while the primary orientation direction of the reinforcing fibers 21 in the even-numbered layer 12 is the second direction Y. That is, the primary orientation directions of adjacent layers 11, 12, 13, 12, 11 are 90 degrees apart from each other. Furthermore, the injection-molded body 10 does not have an adhesive layer that bonds the layers 11, 12, 13, 12, 11 together but does not contain the reinforcing fibers 21. In other words, the reinforcing fibers 21 are present throughout the entire thickness direction Z of the injection-molded body 10.

[0035] <Effects of this embodiment> (1) The injection-molded body 10 consists of five layers 11, 12, 13, 12, 11 that overlap in the thickness direction Z. Of the five layers 11, 12, 13, 12, 11, the main orientation direction of the reinforcing fibers 21 in the odd-numbered layers 11 and 13 from one side of the thickness direction Z is the first direction X, and the main orientation direction of the reinforcing fibers 21 in the even-numbered layer 12 from one side of the thickness direction Z is the second direction Y. The orientation tensor Ax for the first direction X and the orientation tensor Ay for the second direction Y of the reinforcing fibers 21 change continuously between adjacent layers.

[0036] With this configuration, the above-mentioned effects are achieved, making it possible to improve the mechanical strength of the injection-molded body 10. (2) The method for manufacturing the injection-molded body 10 comprises a first step and a second step.

[0037] In this method, in the first step, molten resin is supplied to the cavity 53 through a first gate 51 oriented in a first direction X. This forms a first core layer 31 and a first skin layer 32 located between the first core layer 31 and the molded surface of the cavity 53. In the first skin layer 32, the reinforcing fibers 21 tend to orient in the first direction X, which is the flow direction of the molten resin, because they are easily influenced by the molded surface of the cavity 53, which is at a lower temperature than the molten resin. As a result, the main orientation direction of the reinforcing fibers 21 in the first skin layer 32 is the first direction X. In the first core layer 31, the reinforcing fibers tend to orient in a direction perpendicular to both the flow direction and the thickness direction Z of the molten resin, so the main orientation direction of the reinforcing fibers 21 in the first core layer 31 is the second direction Y.

[0038] Next, in the second step, molten resin is supplied to the cavity 53 through a second gate 52 that is oriented in the second direction Y, which is perpendicular to the thickness direction Z and the first direction X. As a result, the molten first core layer 31 and the molten portion of the first skin layer 32 adjacent to the first core layer 31 flow in the second direction Y, forming a second core layer 13 and a second skin layer 12 located between the second core layer 13 and the first skin layer 11. In the second skin layer 12, the reinforcing fibers 21 tend to orient in the second direction Y, which is the flow direction of the molten resin, because they are easily influenced by the relatively lower temperature of the first skin layer 32(11). Consequently, the main orientation direction of the reinforcing fibers 21 in the second skin layer 12 is the second direction Y. In the second core layer 13, the reinforcing fibers tend to orient in a direction perpendicular to both the flow direction of the molten resin and the thickness direction Z, so the main orientation direction of the reinforcing fibers 21 in the second core layer 13 is the first direction X.

[0039] Therefore, the injection-molded body 10 described in (1) above can be manufactured. <Variation> This embodiment can be implemented with the following modifications. This embodiment and the following modifications can be combined with each other to the extent that they do not contradict each other technically.

[0040] The number of first gates 51 in the mold 50 is not limited to three; it may be two or fewer, or four or more. Furthermore, if three or more first gates 51 are provided, the multiple first gates 51 do not necessarily need to be arranged at equal intervals.

[0041] The second gate 52 is not limited to the one opening in the center of the cavity 53 in the first direction X and the center of the second direction Y. In addition to, or instead of, the second gate 52 in the above embodiment may be provided at least one of the two ends of the second direction Y, as shown by the dashed line in Figure 3.

[0042] The reinforcing fiber 21 is not limited to glass fiber. The reinforcing fiber 21 may be carbon fiber or aramid resin. • Resin 20 is not limited to polypropylene; any thermoplastic resin may be used, such as polyethylene terephthalate. [Explanation of symbols]

[0043] 10,110…Injection molded product 11…First Skin Layer 12…Second Skin Layer 13…Second Core Layer 20… Resin 21…Reinforced fiber 31…First Core Layer 32...First Skin Layer 50,150… molds 51…Gate 1 52,252…Gate 2 53,153... Cavity 131…Core layer 132...Skin layer 151...Gate

Claims

1. An injection-molded mobile body made of thermoplastic resin containing reinforcing fibers, When the direction perpendicular to the thickness direction is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, It consists of five layers that overlap in the thickness direction, Of the five layers, the primary orientation direction of the reinforcing fibers in the odd-numbered layers from one side in the thickness direction is the first direction, and the primary orientation direction of the reinforcing fibers in the even-numbered layers from one side in the thickness direction is the second direction. The orientation tensor in the first direction and the orientation tensor in the second direction of the reinforcing fiber change continuously between adjacent layers. Injection molded body for moving objects.

2. A method for manufacturing an injection-molded body for a mobile device, comprising supplying a molten thermoplastic resin containing reinforcing fibers into the cavity of a mold, When the direction perpendicular to the thickness direction of the cavity is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, A first step of supplying the molten thermoplastic resin containing the reinforcing fibers to the cavity through a first gate oriented in the first direction, thereby forming a first core layer and a first skin layer located between the first core layer and the molding surface of the cavity, wherein the main orientation direction of the reinforcing fibers is the first direction. The invention comprises a second step of supplying the molten thermoplastic resin containing the reinforcing fibers to the cavity through a second gate oriented in the second direction, thereby creating a first core layer in a molten state, a second core layer in which the main orientation direction of the reinforcing fibers is the first direction, and a second skin layer located between the second core layer and the first skin layer, in which the main orientation direction of the reinforcing fibers is the second direction. A method for manufacturing injection-molded articles for mobile devices.

Citation Information

Patent Citations

  • Car body structure

    WO2020148563A1