Manufacturing method for foamed molded products
The innovative foaming mold design with a storage groove and intrusion feature addresses the challenge of insufficient material filling in conventional methods, enabling defect-free production of thin-walled foam molded articles using various materials.
Patent Information
- Application Number
- JP2025079075
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-09
- Publication Date
- 2026-11-19
AI Technical Summary
Conventional foam molding methods face limitations in manufacturing thin-walled foam molded articles due to insufficient filling of foam raw material, especially when using materials with lower expansion ratios or viscosities, leading to manufacturing defects and reduced freedom in product design.
A foaming mold design with an upper and lower mold featuring annular slopes and a storage groove in the lower mold, where the foam material is stored below the slope, and an intrusion portion from the upper mold directs the material into the wall-forming space, allowing for the formation of thin walls without defects.
This method enables the production of thin-walled foam molded products without defects, even with low-viscosity or low-expansion materials, thereby increasing the freedom in manufacturable designs.
Smart Images

Figure 2026182664000001_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method for manufacturing a foam molded article.
Background Art
[0002] As a foam molding die used for manufacturing foam molded articles, there is a die in which a cavity for molding the inclined wall of the foam molded article is formed on the inclined surface of the lower die (for example, refer to Patent Document 1). In the conventional manufacturing method, the foam raw material is pooled in the cavity of the lower die and then the mold is closed, or the viscosity of the foam raw material is increased and the mold is closed before the foam raw material flows out of the cavity, so as to mold the wall and produce the foam molded article.
Prior Art Documents
Patent Documents
[0003]
Patent Document 1
[0043] , Figure 4)
Summary of Invention
Problems to be Solved by the Invention
[0004] However, in the conventional manufacturing method described above, if the cavity is made shallow to reduce the wall thickness of the foam molded article, the amount of foam raw material pooled therein decreases, which may cause a problem that the manufacture of the foam molded article becomes impossible due to insufficient filling. The same problem may also occur when a foam raw material with a lower expansion ratio or lower viscosity than conventional ones is used. That is, the conventional manufacturing method described above has a low degree of freedom for manufacturable foam molded articles. Accordingly, the present application discloses a technique for increasing the degree of freedom of manufacturable foam molded articles compared with the prior art.
Means for Solving the Problems
[0005] One aspect of the invention is a method for manufacturing a foamed molded product having an annular thin wall using a foaming mold, wherein the upper and lower molds of the foaming mold are provided with an upper mold-side annular molding slope and a lower mold-side annular molding slope that face each other across a wall molding space for forming the thin wall, and the lower mold is provided with an annular storage groove for storing foaming material below the lower mold-side annular molding slope, while the upper mold is provided with an annular intrusion portion that protrudes into the storage groove, and the thin wall is formed by the foaming material that flows from the storage groove into the wall molding space due to the intrusion of the intrusion portion. [Brief explanation of the drawing]
[0006] [Figure 1] Figure 1A is a side cross-sectional view of the foamed molded product, and Figure 1B is a top view of the foamed molded product. [Figure 2] Figure 2 is a side cross-sectional view of a foamed molded product attached to the end plate of a pressure vessel. [Figure 3] Figure 3 is a side cross-sectional view of a mold used to mold foamed products. [Figure 4] Figure 4 is an enlarged cross-sectional view of the mold. [Figure 5] Figure 5 is a side cross-sectional view of the raw material injected into the storage groove of the lower mold. [Figure 6] Figure 6 is a side cross-sectional view of the raw material flowing from the storage groove to the wall forming space when the mold is closed. [Figure 7] Figure 7 is a side cross-sectional view of the thin-walled wall formed by foam molding in the mold and the removed film. [Figure 8] Figure 8 is a side cross-sectional view of the mold after it has been opened. [Figure 9] Figure 9A is a side cross-sectional view of the foamed molded product with the removed film attached, and Figure 9B is a side cross-sectional view of the removed film removed from the foamed molded product. [Figure 10] Figure 10A is a side cross-sectional view of the cavity of a conventional mold, and Figure 10B is a side cross-sectional view of a foamed molded product formed with a conventional mold. [Figure 11] Figure 11 is a side cross-sectional view of the raw material injected into the lower cavity of a conventional mold. [Figure 12] Figure 12 is a side cross-sectional view of the raw material injected into the cavity of the lower mold, which lacks a storage groove. [Figure 13] Figure 13 is a side cross-sectional view of a foamed molded product formed in a mold without a storage groove. [Modes for carrying out the invention]
[0007] [First Embodiment] Figures 1A and 1B show the foamed molded product 10 of this embodiment. The foamed molded product 10 has a thin wall 11. The thin wall 11 is annular and inclined with respect to its central axis J. In this embodiment, the foamed molded product 10 is bowl-shaped without a bottom (i.e., has an opening 12 that penetrates the bottom) and is entirely composed of the thin wall 11.
[0008] In this embodiment, the thin wall 11 (i.e., the foamed molded product 10) is annular in plan view and is formed so that it approaches the central axis J (i.e., its diameter decreases) as it moves toward one side of the central axis J (the bottom side) (see Figure 1A).
[0009] Furthermore, in this embodiment, the thin wall 11 is curved so as to bulge outwards (the inner surface of the thin wall 11 is concave). The thin wall 11 is formed such that the slope increases as it moves away from the bottom (i.e., the angle it makes with the central axis J decreases).
[0010] The angles between the inner and outer surfaces of the thin wall 11 and the central axis J (for example, the angles at the end of the thin wall 11 on the opening 12 side) are, for example, 70° or less, for example, 60° or less, and for example, 45° or less. The height of the thin wall 11 (length in the direction of the central axis J) is, for example, 10 times or more the thickness of the thin wall 11 (thickness of the thickest part), and the radius of the opening 12 is, for example, 4 times or more.
[0011] Figure 2 shows an example of the use of the foamed molded product 10 of this embodiment. The foamed molded product 10 of this embodiment is used, for example, as a protective member attached to the outer surface of a pressure vessel 30 to protect the pressure vessel 30. The pressure vessel 30 comprises a cylindrical body portion 31 and a pair of dome-shaped end portions 32 that close both ends of the body. The foamed molded product 10 of this embodiment is fixed (for example, bonded) to the outer surface of the end portions 32. A valve 36 for allowing fluid to flow in and out of the pressure vessel 30 is attached to one of the pair of end portions 32. Examples of pressure vessels include, but are not limited to, the fuel tank of a fuel cell vehicle (for example, the hydrogen tank of a hydrogen fuel cell vehicle).
[0012] The pressure vessel 30 is, for example, a fiber-reinforced plastic container, and has a structure in which a container-shaped plastic liner filled with fluid is covered from the outside with a reinforcing layer. The reinforcing layer is, for example, made of carbon fiber reinforced plastic and formed by the filament winding method. In this case, an annular container thin-walled portion 33 is formed in each end plate portion 32, which is the thinnest (the reinforcing layer is also the thinnest). The foamed molded product 10 is fixed so as to cover the container thin-walled portion 33, protecting the container thin-walled portion 33 from external heat.
[0013] In this embodiment, the foamed molded product 10 is made of polyurethane resin, but is not limited to this. The foaming ratio of the foamed molded product 10 is, for example, 1.2 to 1.7 times. From the viewpoint of impact absorption performance, the foamed molded product 10 as a protective member of the pressure vessel 30 preferably has an Asker C hardness (according to JIS K7312) of 70% or more. The foamed molded product 10 as a protective member of the pressure vessel 30 may also contain, for example, a flame retardant (e.g., expanded graphite). The foamed molded product 10 containing expanded graphite can be attached to both the end plate portion 32 on the valve 36 side and the end plate portion 32 on the opposite side of the valve 36 of the pressure vessel 30. The foamed molded product 10 containing expanded graphite can efficiently block external heat, thereby enabling stable gas release from the valve 36.
[0014] The foam molded article 10 of the present embodiment is produced, for example, as follows. FIG. 3 shows a mold 40 for molding the foam molded article 10. The mold 40 includes an upper mold 50 and a lower mold 60, and is configurable between a mold-closed state in which they are mated (see FIG. 3) and a mold-open state in which they are separated (see FIG. 8).
[0015] Between the upper mold 50 and the lower mold 60 of the mold 40 in the mold-closed state, a wall molding space 21 for molding the thin-walled wall 11 is provided (see FIG. 4). In the example of the present embodiment, the thin-walled wall 11 is molded such that the direction of the central axis J is the vertical direction, and the wall molding space 21 is inclined so as to approach the central axis J as it goes downward relative to the vertical direction. The upper mold 50 and the lower mold 60 are respectively formed with an upper mold-side molding inclined surface 51 and a lower mold-side molding inclined surface 61 that face each other across the wall molding space 21. The upper mold-side molding inclined surface 51 and the lower mold-side molding inclined surface 61 are annular (in the example of the present embodiment, they are in the form of a circular ring).
[0016] An annular storage groove portion 62 is formed in the lower mold 60 below the lower mold-side molding inclined surface 61. In the lower mold 60, the storage groove portion 62 is disposed inside the lower mold-side molding inclined surface 61. Further, the upper mold 50 is provided with an annular protruding portion 52 that protrudes into the storage groove portion 62 when the mold 40 is in the mold-closed state. In the upper mold 50, the protruding portion 52 is disposed inside the upper mold-side molding inclined surface. Between the inner surface of the storage groove portion 62 and the outer surface of the protruding portion 52, a removal film molding space 22 in which a removal film 15 described later is molded is formed. In the removal film molding space 22, the thickness of the end portion on the wall molding space 21 side is reduced to provide a thin film molding portion 23. In the example of the present embodiment, the thickness of the removal film molding space 22 is smaller than that of the wall molding space 21.
[0017] The lower mold 60 is provided with a raised portion 63 that is surrounded by a storage groove 62 and rises upward. On the upper part of the inner groove surface 64 (outer circumferential surface of the raised portion 63) of the raised portion 63 on the storage groove 62 side, there is a lower mold side seal portion 65 that comes into contact with the upper mold side seal portion 55, which is part of the intrusion portion 52, when the mold is closed. The upper mold side seal portion 55 and the lower mold side seal portion 65 are provided at a position higher than, for example, the thin film molding portion 23.
[0018] The inner surface of the storage groove 62 has an inclined surface 66 that extends from the lower end of the lower mold side molding slope 61 to the lower end of the storage groove 62, and an upright surface 67 which is the portion of the groove inner surface 64 that is continuous with the lower end of the storage groove 62. For example, the gradient (angle of inclination with respect to the horizontal plane) of the inclined surface 66 is smaller than the gradient of the upright surface 67.
[0019] As shown in Figure 5, when the mold 40 is in the open state, the raw material G for the foamed molded product 10 (for example, the raw material for polyurethane foam) is injected into the lower mold 60.
[0020] Here, when the raw material G is injected with the mold open, in order to form the foamed molded product 10, the necessary raw material G must be stored in a cavity formed in a concave shape on the slope of the lower mold 60. In conventional foamed molded products with a thick, inclined wall 11V (see Figure 10B), the cavity 68 is either deep or wide (see Figures 10A and 11), so the cavity 68 has sufficient capacity to store the necessary raw material G. As a result, it was possible to form a wall 11V that fills the wall molding space 21 (see Figure 10B). For example, in the examples shown in Figures 10 and 11, the horizontal width W of the cavity 68 is wide and the wall 11V is thicker than the maximum diameter D of the raw material inlet 46 of the injection device 45 for injecting the raw material G (or the distance between the two furthest points in the raw material inlet 46 if it is not circular).
[0021] On the other hand, as shown in Figure 12, when the wall of a foamed molded product is thinned (when a thin wall 11 is foam-molded), the cavity 68 on the slope of the lower mold 60 becomes shallow or narrow, for example, the horizontal width W of the cavity 68 becomes narrower than the maximum diameter D of the raw material injection port 46. In this case, for example, the thin wall 11 becomes thinner than the raw material injection port 46. In this way, when the cavity 68 is shallow or narrow, the necessary raw material G cannot be stored in the cavity 68, and a defect V may occur in the molded thin wall 11 (see Figure 13). A defect V may also occur when a raw material G with a low foaming ratio or low viscosity is used. In other words, the conventional manufacturing method described above had a low degree of freedom in the foamed molded products that could be manufactured.
[0022] In contrast, in this embodiment, as described above, a storage groove 62 is provided below the wall molding space 21 in the mold 40 (see Figure 5). This allows the injected raw material G to be stored in the storage groove 62 in the amount necessary for molding the foamed molded product 10 when the mold is closed. The raw material G may be stored not only in the storage groove 62 but also in part of the wall molding space 21. For example, it is preferable that the horizontal width W of the portion of the cavity 68 formed in a concave shape in the lower mold 60 that can store the raw material G is wider than the maximum diameter D of the raw material inlet 46 in the injection device 45.
[0023] It is preferable that the raw material G is injected so that its liquid level is lower than the upper surface of the raised portion 63. In this embodiment, the raw material G is injected so that its liquid level is lower than the lower mold side seal portion 65 of the raised portion 63.
[0024] Next, the mold 40 is closed (see Figure 6), and the intrusion portion 52 of the upper mold 50 enters the storage groove portion 62. As a result of this entry, the raw material G flows from the storage groove portion 62 into the wall forming space 21, and as this raw material G foams, the thin wall 11 is foam-molded in the wall forming space 21 (see Figure 7). In this embodiment, the thickness of the thin wall 11 is thinner than the maximum diameter D of the raw material injection port 46 of the injection device 45. Also, as the raw material G remaining in the removal film forming space 22 between the storage groove portion 62 and the intrusion portion 52 foams, the removal film 15 connected to the lower end of the thin wall 11 is foam-molded in the removal film forming space 22. In this embodiment, the removal film 15 has a shape that is sharply bent in a side cross-sectional view. A thin film portion 16 is formed at the end of the removal film 15 on the thin wall 11 side by the thin film forming portion 23. In this embodiment, the removal film 15 is thinner than the thin-walled wall 11. When the mold 40 is closed, the intrusion portion 52 enters the storage groove 62, and the lower mold-side seal portion 65 of the storage groove 62 and the upper mold-side seal portion 55 of the intrusion portion 52 come into contact, preventing the raw material G from leaking to the outside (for example, the upper part of the raised portion 63).
[0025] Once the thin wall 11 and the removal film 15 are integrally foam-molded, the mold 40 is opened (see Figure 8), and the thin wall 11 and the removal film 15 are removed from the mold 40 (see Figure 9A).
[0026] Next, the removal film 15 is removed from the thin wall 11, forming an opening 12 and yielding a foamed molded product 10 with the thin wall 11 (see Figure 9B). The removal film 15 has a thin film portion 16, which allows it to be easily cut (for example, it can be torn by hand). Preferably, the removal film 15 is thinner than the thin wall 11 and has a small weight. This reduces the amount of waste that is not included in the foamed molded product 10.
[0027] As described above, in this embodiment, a storage groove 62 is provided in the lower mold 60 of the mold 40 below the wall molding space 21, and the raw material G necessary for foam molding the foamed molded product 10 can be stored in the storage groove 62. Therefore, compared to the case where the storage groove 62 is not provided, it is possible to suppress the occurrence of material defects in the thin-walled wall 11 foamed in the wall molding space 21 of the mold 40. In addition, by providing the storage groove 62, it becomes possible to mold a foamed molded product 10 without material defects using a raw material G with a low foaming ratio. As a result, it is possible to increase the degree of freedom in the foamed molded products that can be manufactured compared to the conventional method.
[0028] [Other embodiments] The foamed molded product 10 may be a protective member that covers and protects articles other than the pressure vessel 30. Furthermore, the foamed molded product 10 may be used for purposes other than protective membership.
[0029] In the above embodiment, the direction in which the thin-walled wall 11 bulges was outward (radially outward), but it may also be radially inward. The thin-walled wall 11 may not have a bulging shape, but rather a tapered shape with a straight cross-section.
[0030] In the above embodiment, the foamed molded product 10 was entirely composed of a thin wall 11, but the foamed molded product 10 may also be composed of a thin wall 11 and other parts.
[0031] In the above embodiment, the upper mold side sealing portion 55 and the lower mold side sealing portion 65 may be provided at the lower end of the protrusion portion 52 and the lower end of the raised portion 63, respectively.
[0032] In the above embodiment, the foamed molded product 10 was configured to have an annular wall (thin-walled wall 11), but the foamed molded product 10 can also be configured to have a non-annular wall (a wall that is foamed and molded in an inclined state with respect to the horizontal plane). This wall may be, for example, an arc shape in plan view, or a flat plate shape.
[0033] <Note> The following describes the features extracted from the above embodiment, showing their effects and other details as needed. For ease of understanding, the corresponding components in the above embodiment will be indicated in parentheses as examples; however, these features are not limited to the specific components shown in parentheses.
[0034] For example, the following set of features relates to a method for manufacturing foamed molded products, and the background technology is as follows: "As a foaming mold used for manufacturing foamed molded products, there are molds in which a cavity for forming the inclined wall of the foamed molded product is formed on the inclined surface of the lower mold (see, for example, Patent Document 1). In conventional manufacturing methods, the wall is formed by either accumulating the foaming material in the cavity of the lower mold and closing the mold, or by increasing the viscosity of the foaming material and closing the mold before the foaming material flows out of the cavity, thereby manufacturing a foamed molded product (see, for example, Japanese Patent Application Publication No. 2018-91442 (paragraph
[0043] , Figure 5))." It can be considered that this invention was conceived with the following problem in mind: "However, in the conventional manufacturing method described above, if the cavity is made shallow in order to thin the wall of the foamed molded product, the amount of foaming material that can accumulate there decreases, which can lead to a problem where it becomes impossible to manufacture the foamed molded product due to material deficiency. The same problem can also occur when using foaming materials with a lower foaming ratio or lower viscosity than conventional methods. In other words, the conventional manufacturing method described above had a low degree of freedom in the types of foamed molded products that could be manufactured. Therefore, this invention discloses a technology to increase the degree of freedom in the types of foamed molded products that can be manufactured compared to conventional methods." Furthermore, there has been a long-standing demand for novel technologies related to foamed molded products, their manufacturing methods, molds for foaming foamed molded products, etc.
[0035] [Feature 1] A manufacturing method for producing a foamed molded product (10) having an annular thin-walled wall (11) using a foaming mold (40), The upper mold (50) and lower mold (60) of the foam molding die are provided with an upper mold side annular molding slope (51) and a lower mold side annular molding slope (61) facing each other with a wall forming space (21) for forming the thin wall in between, The lower mold is provided with an annular storage groove (62) for storing foaming material (G) below the annular molding slope on the lower mold side, while the upper mold is provided with an annular intrusion (52) that protrudes into the storage groove. A method for manufacturing a foamed molded product, wherein the thin wall is formed by the foaming material that flows from the storage groove into the wall-forming space due to the intrusion of the intrusion portion.
[0036] [Feature 2] Between the intrusion portion and the storage groove portion, there is a removal film forming space (22) in which a removal film (15) is formed, which is connected to the lower end of the thin wall and removed after forming. The method for manufacturing a foamed molded product according to feature 1, wherein the thickness of the end portion (16) on the wall molding space side is reduced in the removal film molding space.
[0037] [Feature 3] The lower mold is provided with a raised portion (63) that is surrounded by the storage groove and rises upward, A method for manufacturing a foamed molded product according to feature 1 or 2, wherein the inner groove surface (64) of the raised portion on the storage groove side is provided with a lower mold side seal portion (65) at a position above the liquid level of the foaming material before the intrusion portion enters, which contacts the upper mold side seal portion (55), which is part of the intrusion portion, to restrict leakage of the foaming material to the outside.
[0038] [Feature 4] The inner surface of the storage groove includes an inclined surface (66) extending from the lower end of the annular molding slope on the lower mold side to the lower end of the storage groove, and an upright surface (67) which is a portion of the inner surface of the groove that is continuous with the lower end of the storage groove. The method for manufacturing a foamed molded product according to feature 3, wherein the gradient of the inclined surface is smaller than the gradient of the upright surface.
[0039] [Feature 5] The method for manufacturing a foamed molded product according to feature 3 or 4, wherein the upper surface of the raised portion surrounded by the storage groove portion of the lower mold is located at a height that the foaming material does not reach when the intrusion portion intrudes.
[0040] [Feature 6] A method for manufacturing a foamed molded product according to any one of the features 1 to 5, wherein the thickness of the thin wall is thinner than the maximum diameter (D) of the injection port (46) of the injection device (45) for injecting the foaming material into the storage groove.
[0041] [Feature 7] A method for manufacturing a foamed molded product according to any one of features 1 to 6, wherein the foamed molded product is a protective member attached to the end plate portion (32) of a pressure vessel (30).
[0042] Based on the above characteristics, it becomes possible to increase the degree of freedom in manufacturing foamed molded products compared to conventional methods.
[0043] While this specification and drawings disclose specific examples of the technology included in the claims, the technology described in the claims is not limited to these specific examples, but also includes various modifications and changes to these examples, as well as parts of the examples taken individually. [Explanation of symbols]
[0044] 10 Foamed molded products 11 Thin wall 12 aperture 15 Removal membrane 16 Thin film section 21 Wall molding space 22 Removal film forming space 23 Thin film molding section 30 Pressure vessel 31 Torso 32 Each end plate section 32 End plate section 33 Thin-walled part of the container 36 valves 40 molds 45 Injection device 46 Inlet 50 upper mold 51 Upper mold side forming slope 52 Assault Section 55 Upper mold side seal section 60 Lower mold 61 Lower mold side forming slope 62 Storage channel 63 Ridge 64 Groove inner surface 65 Lower mold side sealing section 66 Slope 67 Erection surface 68 Cavity G raw material J center axis V lack of flesh
Claims
1. A manufacturing method for producing a foamed molded product having an annular thin-walled structure using a foaming mold, The upper and lower molds of the foam molding die are provided with an annular molding slope on the upper mold side and an annular molding slope on the lower mold side, facing each other with a wall forming space for forming the thin wall in between, The lower mold is provided with an annular storage groove for storing foaming material below the annular molding slope on the lower mold side, while the upper mold is provided with an annular intrusion portion that protrudes into the storage groove. A method for manufacturing a foamed molded product, wherein the thin wall is formed by the foaming material that flows from the storage groove into the wall-forming space due to the intrusion of the intrusion portion.
2. Between the intrusion portion and the storage groove portion, there is a removal film forming space in which a removal film is formed that is connected to the lower end of the thin wall and removed after forming, The method for manufacturing a foamed molded product according to claim 1, wherein the thickness of the end on the wall molding space side of the removal film molding space is reduced.
3. The lower mold is provided with a raised portion that is surrounded by the storage groove and rises upward, The method for manufacturing a foamed molded product according to claim 1, wherein the inner surface of the groove on the storage groove side of the raised portion is provided with a lower mold side seal portion at a position above the liquid level of the foaming material before the intrusion portion enters, which contacts the upper mold side seal portion, which is part of the intrusion portion, to restrict leakage of the foaming material to the outside.
4. The inner surface of the storage groove includes an inclined surface extending from the lower end of the annular molding slope on the lower mold side to the lower end of the storage groove, and an upright surface which is a portion of the inner surface of the groove that is continuous with the lower end of the storage groove. The method for manufacturing a foamed molded product according to claim 3, wherein the gradient of the inclined surface is smaller than the gradient of the upright surface.
5. The method for manufacturing a foamed molded product according to claim 1, wherein the thickness of the thin wall is thinner than the maximum diameter of the injection port of the injection device for injecting the foaming material into the storage groove.
Citation Information
Patent Citations
Pressure vessel and manufacturing method of pressure vessel
JP2018091442A