Parts having a color gradient, and methods for manufacturing the same
By laminating metal alloys and machining to form an inclined surface, the method achieves a visible color gradient at least 100 μm deep, addressing the limitations of existing methods with faster heat treatment and controlled depth.
Patent Information
- Application Number
- JP2026072422
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-09
- Filing Date
- 2026-04-24
- Publication Date
- 2026-11-19
AI Technical Summary
Existing methods struggle to produce a color gradient in metal components with gradual transitions between colors over a depth of at least 100 μm without using powder or PVD, and require excessively long heat treatment times or numerous alloy layers, complicating industrial implementation.
A method involving laminating metal alloys with different compositions, applying stress, and performing localized machining to form an inclined surface, allowing for a color gradient through controlled diffusion zones and machining to achieve a visible gradient at least 100 μm deep.
The method enables a gradual color transition visible over time, extending to a depth of at least 100 μm, with controlled depth and visibility maintained despite wear, and reduces heat treatment time significantly.
Smart Images

Figure 2026182786000001_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present invention relates to a component, in particular a solid metal component exhibiting a color gradient, and a method for producing the same. BACKGROUND ART
[0002] To obtain a color gradient on a metal material, there are various main approaches, such as using powder or depositing a thin layer by, for example, PVD (Physical Vapor Deposition). While methods using powder require mixing to obtain various desired colors, PVD methods are limited to depositing layers, and cannot produce products having a color gradient throughout the entire volume.
[0003] It is also possible to create a color gradient by using layers of alloys with similar colors, welding the layers together, and then cutting perpendicularly across these layers. However, it is difficult to have a gradual color transition between these layers. Diffusion by heat treatment smooths the transition between layers, but only over a small distance of about several tens of microns. In fact, the diffusion distance is a function of the square root of the heat treatment time. This diffusion distance, combined with the low diffusion rate, makes obtaining a transition zone of about 1 millimeter visible to the naked eye extremely slow. Therefore, unless an extremely long heat treatment is used, the transition between colors is not gradual, which is impractical from an industrial point of view. A remedy for this problem is to use a larger number of alloy layers with similar colors to reduce the contrast between the two layers. However, this method requires the production of a large number of alloys of various compositions, which significantly complicates implementation. SUMMARY OF THE INVENTION PROBLEMS TO BE SOLVED BY THE INVENTION
[0004] The present invention aims to propose a new method for producing a component that exhibits a color gradient with gradual transitions between colors on at least a portion of its outer surface and to a depth of at least 100 μm, without using powder, PVD methods, or excessively time-consuming processes. MEANS FOR SOLVING THE PROBLEMS
[0005] The method according to the present invention comprises obtaining a color gradient from a laminate of layers having restricted diffusion zones between the layers, and then geometrically expanding the diffusion zones on a finished product. More specifically, the laminate of layers is subjected to a heat treatment for a reasonable duration to obtain diffusion zones of tens or hundreds of microns between the layers. The laminate is then subjected to localized machining or machining across the entire base surface of the laminate to form an inclined surface that passes through the laminate of layers relative to the plane of the base surface, thereby revealing the color gradient.
[0006] More specifically, the present invention relates to a method for manufacturing a part, wherein the part exhibits a color gradient on at least a portion of the surface that is intended to be visible during use, and at a depth of at least 100 μm below the surface, and the method comprises the following sequential steps: - A step of preparing several semi-finished products, each composed of a metal alloy, with different chemical compositions and colors from one another, -A step of layering the aforementioned semi-finished products in order to form a laminate, wherein the laminate is defined by the outer surface, and The method includes, and the method is performed sequentially or in parallel, -In order to form an aggregated laminate having a thickness E of 100 μm or more, the steps include applying stress to the laminate at room temperature or high temperature, - The step of performing diffusion heat treatment between semi-finished aggregate laminates, and then, - A step of machining the outer surface of an aggregated laminate to form at least one inclined surface with respect to the outer surface plane, wherein the inclined surface extends to a depth greater than at least the thickness of the semi-finished product with respect to the outer surface in order to show a color gradient on the surface. The method further includes, and the method may optionally include, - A step to finish the surface of the part in order to obtain the part. It also includes.
[0007] The resulting parts have a color gradient that extends to a depth of at least 100 μm, ensuring visibility over time regardless of wear and impact. This differs from the color gradients obtained by PVD, where the color gradient is limited to thicknesses of less than 20 μm. The color gradient may also be present throughout the entire volume of the part. The depth is easily controlled by selecting the thickness of each layer of the laminate.
[0008] This method allows for easy acquisition of gradual color changes between layers with a reasonable diffusion heat treatment time. Typically, the heat treatment time for gold alloys is between 1 and 6 hours, resulting in a diffusion region of 100–150 μm, which extends across the visible surface over distances 2 to 50 times greater by machining at a given angle to the base surface.
[0009] The present invention also relates to a component having a color gradient visible on at least a portion of the surface of the component and extending to a depth of at least 100 μm below the surface, wherein the color gradient is formed by a set of layers, each composed of a metal alloy, with different chemical compositions and colors from one another, and all layers have diffusion zones between them, measurable by, for example, EDX, such that a gradual color change is obtained across all layers. [Brief explanation of the drawing]
[0010] [Figure 1] This is a schematic diagram of the sequential steps a) to e) of the manufacturing method according to the present invention. [Figure 2] Figure 1 shows a modified form of any further step d) of the method. [Figure 3] This is a graph of EDX measurements showing the progression of Cu and Ag aggregation between the two layers of 2N and 5N gold at the end of step c). [Figure 4] This shows a schematic diagram of the diffusion zone between layers after step c), and a magnified view of the shape of the diffusion zone after step d). [Figure 5]This is a schematic diagram of the diffusion zone distance D2 between two layers at the depth of the finished part, and the diffusion zone distance D1 between these same two layers on the visible surface of the finished part, where the upper configuration has a recess on the visible surface, and the lower configuration has an inclined plane on the visible surface. [Figure 6] This is a schematic diagram of the ratio difference between D1 and D2, based on the angle α of the inclined surface relative to the base surface and the diffusion heat treatment time for a given alloy system. [Figure 7] This is a schematic diagram of the ratio difference between D1 and D2, based on the angle α of the inclined surface relative to the base surface and the diffusion heat treatment time for a given alloy system. [Modes for carrying out the invention]
[0011] The present invention relates to a method for manufacturing a component exhibiting a color gradient, wherein the color gradient is intended to be visible during use. The method is particularly suited to manufacturing components having flat surfaces that are primarily visible during use. Therefore, the method is particularly suited to manufacturing timekeeping components such as dials, case backs, oscillators, bridges, or bezels.
[0012] The present invention also relates to a part 1 exhibiting this color gradient 1a, 1b, 1c, 1d, visible in a recess 9 on the visible surface 7 of the part in Figure 1d)e), or in the plane of the visible surface 7 in Figure 2. According to the present invention, this color gradient visible on the surface exists to a depth of at least 100 μm, and this depth can extend beyond the entire thickness of the part.
[0013] The components are made of metal alloys. More specifically, the components may be solid components of gold alloys and optionally pure gold, including at least two different color grades. For example, the components can be made in at least two shades classified between 2N and 6N according to the classification established by the Swiss Watch Industry Standards (NIHS). These shades between 2N and 6N have increasing copper content and gradually become redder. These shades may also contain other elements such as Ag. For example, the components may have at least two shades selected from the following shades, whether gradually colored or not: 24K gold (pure gold), 18K 2N gold, 18K 3N gold, 18K 4N gold, 18K 5N gold, and 18K 6N gold. Advantageously, the components can be made in four gradually colored shades, such as: 24K gold (pure gold), 18K 2N gold, 18K 4N gold, and 18K 6N gold. Laminates with alternative gold colorations, such as 2N-6N-2N-6N, can also be realized.
[0014] Generally, a color gradient can be fabricated from any metal alloy, provided that it allows for gradual, rather than discontinuous, adjustment of the color due to changes in the surrounding composition of the substrate composition. Harmony with alloys having various substrate compositions cannot be ruled out, provided that this gradual color change can be observed between the various compositions after the manufacture of the parts. The color gradient has at least two hues, with 2, 3, 4, 5, 6, 7, 8, etc.
[0015] More specifically, the components can also be made from non-precious metal alloys such as Cu / Cu-Sn, Cu / Cu-Ni, Cu / Cu-As, Cu / Cu-Sb, and Cu / Cu-Zn, and variations in composition result in gradual color changes. For example, in the case of Cu / Cu-Sn, these can be variations in composition between pure Cu and Cu containing 11% by weight of Sn. For example, in the case of Cu / Cu-Ni, these can be variations in composition between pure Cu and Cu containing 7.9% by weight of Ni. For example, in the case of Cu / Cu-As, these can be variations in composition between pure Cu and Cu containing 15% by weight of As. For example, in the case of Cu / Cu-Sb, these can be variations in composition between pure Cu and Cu containing 7.3% by weight of Sb. In the case of Cu / Cu-Zn alloys, the gradient was observed at the intermediate Zn level, with the weight percentage of Zn ranging from approximately 45% to 48% as the color changed from pale yellow to a darker yellow. Overall, it is simply important that the composition exhibits a continuous color change to achieve the gradient, rather than discontinuously abrupt.
[0016] A manufacturing method comprising manufacturing steps a) to e) is schematically shown in Figure 1. In the first step a), semi-finished products 2a, 2b, 2c, 2d composed of variations with different metal alloy compositions are provided and layered so as to form a laminate 2, which is defined by an outer surface 10, also known as the base surface of the laminate. In this example, four semi-finished products 2a, 2b, 2c, 2d, also referred to as layers hereinafter, are layered to form the laminate 2. The color may be gradually varied along the thickness of the layer, and the color becomes darker along the thickness of the layer, or vice versa. It is also possible to layer a first set of layers with gradually changing color over a second set of layers with gradually changing color, wherein the gradual color change becomes darker or lighter for the respective set for each set, or becomes darker for one set and reversed for the other set. In the case of gold and gold alloys, it is also possible to alternate layers with varying fineness, such as 4N-3N-5N-2N or 2N-3N-2N-5N. It is also possible to place two layers of the same composition in a laminate having at least three layers, and place one or more layers of other compositions therebetween.
[0017] The number of layers, the respective thickness of each layer, the alloy in question, and the shape of the layers are selected based on the result and the intended use. For example, the semi-finished product may be in the form of a disk to form a circular part. It will be appreciated that any shape (square, rectangular, annular, etc.) can be contemplated. For example, the semi-finished product may be in the form of a strip. The semi-finished products may be polished in advance or subjected to other surface treatments such as chemical etching so as to improve the interface between the semi-finished products.
[0018] According to this method, the thickness of each layer is not a limiting factor. As long as the total thickness of the layers is 100 μm or more, it can vary from one layer to the other. Each layer can have a thickness of several microns, tens of microns, or several millimeters or more. For example, in the case of a dial or case back, the total thickness of the laminate is between 0.2 mm and 4 mm, and each layer is between 0.05 mm and 2 mm thick. It is possible to have considerably thicker layers; for example, layer 2d defines the surface opposite the visible surface. For example, the last layer 2d may have a thickness of 10-15 mm, and the upper layer may have a thickness of several tens of microns. One application is for a dial, where the lower half of the dial's thickness is formed from one layer, and the upper half is formed from several layers, thereby creating a color gradient in only one half of the dial's thickness.
[0019] In the second step b), all layers are subjected to stress, preferably at a high temperature, to join layers 2a, 2b, 2c, and 2d together, thereby forming an aggregated laminate 3. Various consolidation techniques are possible. Some examples include flash sintering (SPS, representing Spark Plasma Sintering), co-thinning, co-extrusion, ultrasonic welding with stress applied by press, Joule welding with stress applied by press, etc. For example, the strip-shaped semi-finished product in step a) can be co-thinned. After this co-thinning, the dimensions of the consolidated laminate can be adjusted, for example by stamping, to obtain a desired shape, such as a circle.
[0020] The pressure and temperature depend on the metal alloy and the shape of the semi-finished product. Typically, for a set of layers based on gold alloy and optionally pure gold, the temperature is between ambient temperature and 890°C, preferably between 350°C and 870°C, more preferably between 400°C and 650°C, and the pressure is between 1 MPa and 1000 MPa, preferably between 5 MPa and 350 MPa, more preferably between 50 MPa and 250 MPa. The stress application time may be between 10 seconds and 48 hours, preferably between 5 minutes and 2 hours, more preferably between 10 minutes and 1 hour. This step can be carried out under an inert atmosphere or a controlled atmosphere to improve the results according to the alloy.
[0021] In the third step c), the heat treatment is performed to achieve chemical diffusion between the layers, so as to make it possible to achieve a color gradient between the layers 2a, 2b, 2c, 2d, rather than a discontinuous separation line. Again, the temperature of the heat treatment depends on the material. For example, for a set of layers based on gold alloy and optionally pure gold, the temperature is between 700°C and 890°C. The treatment time can be between 1 minute and several tens of hours, and the maximum time is limited exclusively by economic efficiency. Therefore, preferably, the treatment time is optimally between 1 hour and 8 hours, more preferably between 1 hour and 6 hours. In general, regardless of the type of alloy, the temperature and treatment time are adapted so that a diffusion distance of between 10 μm and 400 μm, preferably between 100 μm and 250 μm, is obtained between the two layers. It is specified that this heat treatment may be used depending on the alloy to obtain specific properties, for example hardening. This heat treatment can also be accompanied by quenching, or can be carried out under a specific atmosphere as required. It should be noted that according to a variant of the method, steps b) and c) can be carried out in a single step. In this case, this single step is referred to as a simultaneous step.
[0022] In the fourth step d), the outer surface 10 of the laminate 3 is machined, for example by grinding, laser ablation, or milling, in local areas or over the entire outer surface, to form an inclined surface with respect to the plane of the top surface 10. Preferably, the inclined surface is flat and inclined at an angle α with respect to the plane of the top surface 10, where the angle α is between 0.1° and 40°, preferably between 0.5° and 20°, and more preferably between 1° and 10°. The inclined surface can also be curved, for example, to produce a domed dial. The inclined surface extends from the top surface 10 to a depth exceeding the thickness of at least one layer of the laminate so as to show at least a portion of the color gradient. Preferably, the inclined surface extends through the entire thickness P of the laminate. Thus, in the example of Figure 2, the inclined surface forms an inclined plane that passes through all layers 1a, 1b, 1c, and 1d of the laminate. In the example of Figures 1d)e), the inclined surface forms a recess 9, which extends partially or completely through the thickness of the laminate. On the left of Figure 1d)e), the recess 9 extends to a depth P corresponding to the thickness of two layers 1a and 1b. On the right of Figure 1d)e), the recess 9 extends to a depth P corresponding to the thickness of four layers 1a, 1b, 1c, and 1d. The final surface 7 of the part is no longer perfectly flat. The final surface 7 is formed from a flat portion 7a having a color corresponding to the color of the layer at the level of the outer surface of the laminate, and another portion having one or more recesses 9 from which a color gradient appears. These recesses have, for example, a V-shaped inclined surface. According to another variant not shown, the surface 7 may form an inclined plane that shows a color gradient by having at least one further recess fabricated on the surface 7 to show the color gradient at a different angle.
[0023] Next, there is an optional fifth step e) finishing the surface by polishing, shot blasting, microblasting, sandblasting, satin finish and / or sunray finish, etc., which are performed, for example, mechanically or by laser. Chemical and / or electrochemical erosion may also be used to produce a specific effect.
[0024] The resulting part 1 exhibits a color gradient on its surface 7 that is visible within the inclined plane and / or recess.
[0025] It should be noted that further heat treatment steps may be performed at various points in the process to optimize the mechanical or cosmetic properties of the resulting part.
[0026] According to the present invention, the diffusion region is obtained in step c), is typically several tens of microns in size, and extends across the visible surface 7 or within a recess 9 created on the visible surface 7. An example of the principle of the present invention is as follows: Two layers of 2N and 5N gold alloys were hot-pressed together. Next, a diffusion heat treatment was performed at 870°C for 3 hours. In Figure 3, for example, by EDX (energy-dispersive X-ray spectroscopy), the diffusion regions of Cu and Ag measured in a straight line perpendicular to the layers are found to be approximately 150 μm, or more precisely, 170 μm. Next, the outer surface was machined according to an inclined plane with an α angle of 4°. As shown in Figure 4, the diffusion region at a distance D2 of approximately 150 μm between the two layers thus extends over a distance D1 of approximately 2150 μm. For comparison, obtaining the same migration distance using diffusion alone would require a heat treatment at 870°C for more than 600 hours.
[0027] According to the present invention, the ratio between the distance D1 of the diffusion area visible on surface 7 after step d) and the distance D2 of the diffusion area after step c) is between 2 and 50, preferably between 5 and 20 (Figure 8). On the final part, the distance D2 can be measured, for example, based on EDX measurement in the sample, i.e., based on destructive testing. The testing does not have to be destructive if the final part includes a portion where the layer is exposed (e.g., on a machined periphery). This distance D2 is always measured along a line perpendicular to the layer. If the various layers are no longer easily separable, this distance D2 corresponds to the minimum distance of the diffusion area obtained on the various notches passing through the part. In other words, if the layers are no longer easily separable, the distance D2 corresponds to the distance between the location of composition c1 and the location of composition c2. Compositions c1 and c2 are the nominal compositions of the first layer. The same applies to distance D1. The distance D1 used to calculate the ratio corresponds to the diffusion distance between two corresponding layers within the inclined plane of surface 7 or within the recess 9, and this measurement is performed on a line and always along a line perpendicular to the layers (Figure 5).
[0028] Typically, D1 is between 20 μm and 20 mm, preferably between 0.5 mm and 5 mm, and D2 is between 10 μm and 400 μm, preferably between 100 μm and 250 μm.
[0029] The ratio between D1 and D2 is a function of the angle α of the inclined surface. The effects of angle α and diffusion heat treatment time are schematically shown in Figures 6 and 7 for a laminate of two layers of 2N and 5N gold alloys. In the example in Figure 7, the diffusion distance D2 is significant, and after a long heat treatment of several hours, the value is in the range of 400 μm. Next, the outer surface was machined at a large α angle, typically an angle greater than 20°. At a distance D1 of 800 μm on the visible side, a ratio of 2 is observed. Conversely, in the example in Figure 6, the treatment time was short, typically less than 2 hours, resulting in a low diffusion distance D2 of about 20 μm. The machining was performed at a small angle α of less than 1°. In this case, the same distance D1 of 800 μm is observed on the visible surface, or the ratio between D1 and D2 is 40. Each method has its advantages and disadvantages. The method in Figure 7 is not necessarily ideal because it requires a long diffusion heat treatment. On the one hand, a wide machining angle is more practical in manufacturing because it minimizes the visual differences resulting from variations in polishing depth. The advantage of the method shown in Figure 6 is that it requires less heat treatment time and is more economically appealing. On the other hand, a very close machining angle can be problematic in manufacturing because it increases the visual differences resulting from variations in polishing depth. There is a compromise that must be found on a case-by-case basis.
[0030] This method was performed for solid gold components and began with four layered gold discs having continuous shades of gold: 24K gold (pure gold), 18K 2N gold, 18K 4N gold, and 18K 6N gold. Each disc had a thickness of 0.3 mm and a diameter of 30 mm. The discs were pre-polished to improve the interfaces. Next, the discs were hot-pressed at 550°C under a pressure of 141 MPa for 90 minutes to obtain an aggregated laminate. The laminate was then heat-treated at 870°C for 5 hours under a protective atmosphere. The laminate was machined according to an inclined plane with an angle α of 2° extending through the four layers. A very good appearance was obtained, with a gradual color change from the bright yellow of pure gold to the rose color of 18K 6N gold. [Explanation of Symbols]
[0031] 1 part 2 Laminate 3. Aggregated laminate 7 sides 9 recesses 10 Exterior
Claims
1. A method for manufacturing a component (1), wherein the component (1) exhibits a color gradient (1a, 1b, 1c, 1d) on at least a portion of the surface (7) that is intended to be visible during use, and at a depth of at least 100 μm below the surface (7), and the method is carried out continuously. - A step of preparing several semi-finished products (2a, 2b, 2c, 2d), each composed of a metal alloy and having a different chemical composition and color from one another, - A step of layering the semi-finished products (2a, 2b, 2c, 2d) to form a laminate (2), wherein the laminate (2) is defined by the outer surface (10), and The method includes, and the method may be performed sequentially or simultaneously. - In order to form an aggregated laminate (3) having a thickness P of -100 μm or more, the step is to apply stress to the laminate (2) at room temperature or high temperature, - The step of performing diffusion heat treatment between the semi-processed products (2a, 2b, 2c, 2d) of the aggregated laminate (3), and then, - A step of machining the outer surface (10) of the aggregated laminate (3) in order to form at least one inclined surface with respect to the plane of the outer surface (10), wherein the inclined surface extends to a depth at least greater than the thickness of the semi-finished product (2a, 2b, 2c, 2d) with respect to the outer surface (10) in order to show the color gradient (1a, 1b, 1c, 1d) on the surface (7) and The method further includes, optionally, - A step of finishing the surface of the surface (7) in order to obtain the part (1) A manufacturing method that further includes the following.
2. The method according to claim 1, wherein the semi-finished products (2a, 2b, 2c, 2d) are produced in large quantities from different gold alloys, and optionally, one of the semi-finished products (2a, 2b, 2c, 2d) is produced in large quantities from pure gold.
3. The method according to claim 2, wherein, in relation to the step of applying the stress, the temperature is between the ambient temperature and 890°C, preferably between 350°C and 870°C, more preferably between 400°C and 650°C, and the pressure is between 1 MPa and 1000 MPa, preferably between 5 MPa and 350 MPa, more preferably between 50 MPa and 250 MPa.
4. The method according to claim 2, wherein, in relation to the step of performing the diffusion heat treatment, the temperature is between 700°C and 890°C, and the treatment time is between 1 minute and several tens of hours, preferably between 1 hour and 8 hours, more preferably between 1 hour and 6 hours.
5. The method according to claim 1, wherein the machining step is a step of machining along the entire outer surface (10) to obtain an inclined plane that forms the surface (7).
6. The method according to claim 1, wherein the machining step is a machining step of a local area of the outer surface (10) to form at least one recess (9) within the surface (7).
7. The method according to claim 1, wherein in the machining step, the inclined surface extends to a depth corresponding to the thickness P of the aggregated laminate (3).
8. The method according to claim 1, wherein the inclined surface is flat and inclined at an angle α with respect to the plane of the outer surface (10), and the angle α is between 0.1° and 40°, preferably between 0.5° and 20°, and more preferably between 1° and 10°.
9. The method according to claim 1, wherein the laminate (2) comprises at least three, preferably at least four, semi-finished products (2a, 2b, 2c, 2d).
10. The method according to claim 1, wherein, in the laminate of the semi-finished products (2a, 2b, 2c, 2d), the semi-finished product (2d) located at the bottom with respect to the outer surface (10) has a thickness greater than that of the other semi-finished products (2a, 2b, 2c).
11. A component (1), wherein the component (1) has a color gradient visible on at least a portion of a surface (7) of the component (1) and extending to a depth of at least 100 μm below the surface (7), the color gradient (1a, 1b, 1c, 1d) is formed by a set of layers, each composed of a metal alloy, the chemical composition and color of each layer being different from one another, and the layers as a whole have diffusion zones between each layer, particularly measurable by energy-dispersive X-ray spectroscopy, such that a gradual color change is obtained throughout the layers.
12. The component (1) according to claim 11, wherein the color gradients (1a, 1b, 1c, 1d) are located within the plane of the surface (7) and / or within at least one recess (9) within the surface (7).
13. The diffusion area between two layers within the surface (7) and / or within the recess (9) of the surface (7) extends over a first distance D1, and the diffusion area between the same two layers extends over a second distance D2 to a depth of at least 100 μm below the surface (7), the ratio of D1 to D2 being between 2 and 50, and the first distance D1 and the second distance D2 being measured in particular along a line perpendicular to the two layers by energy-dispersive X-ray spectroscopy, part (1) according to claim 12.
14. The component (1) according to claim 13, wherein D1 is between 20 μm and 20 mm, preferably between 0.5 mm and 5 mm, and D2 is between 10 μm and 400 μm, preferably between 100 μm and 250 μm.
15. The part (1) according to claim 11, wherein the part (1) exhibits the color gradient (1a, 1b, 1c, 1d) over its entire depth.
16. The component (1) according to claim 11, wherein the entire layer is composed of multiple variations of one alloy selected from the list of gold / gold-copper, copper / copper-tin, copper / copper-nickel, copper / copper-arsenic, copper / copper-antimony, and copper / copper-zinc alloys.
17. The component (1) according to claim 16, wherein the entire layer is composed of multiple variations of a gold / gold-copper alloy, and the entire layer comprises at least two layers composed of two shades of gold selected from 24K gold, 18K 2N gold, 18K 3N gold, 18K 4N gold, 18K 5N gold and 18K 6N gold.
18. The component (1) according to claim 17, wherein the entire layer comprises four layers composed of four gold shades, which are 24K gold, 18K 2N gold, 18K 4N gold, and 18K 6N gold, in a continuous sequence.
19. The part (1) is a dial, a case back, a vibrator, a receiver, or a watch bezel, according to claim 11.
20. The component (1) according to claim 19, wherein the layer furthest opposite to the surface (7) has a thickness greater than that of the other layers.