Window components for optical elements
By forming through holes and dividing transparent substrates along imaginary lines, the method enhances the yield of usable window components for optical elements, improving airtightness and reliability through chamfered edges and metallized films, addressing the low yield issue in existing manufacturing methods.
Patent Information
- Application Number
- JP2026196025
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-25
- Filing Date
- 2026-08-28
- Publication Date
- 2026-11-19
AI Technical Summary
Existing methods for manufacturing window components for optical elements, such as those described in Patent Document 1, result in a low yield of usable window glasses due to the inability to utilize portions of the glass substrate other than the hollowed-out window glass, limiting the number of obtainable pieces.
A method involving forming through holes in a transparent substrate and dividing it along imaginary lines connecting the centers of these holes, utilizing techniques like laser irradiation and etching to create a transparent member with chamfered corners and edges, which can be further enhanced with metallized films for improved airtightness and reliability.
This method increases the number of obtainable transparent members from a substrate by minimizing waste and enhancing the airtightness and reliability of the window components for optical elements, reducing the likelihood of damage and interference with surrounding structures.
Smart Images

Figure 2026182896000001_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for producing a transparent member, a transparent member, and a window component for an optical element using the transparent member.
Background Art
[0002] Optical elements such as optical semiconductors used in optical communications, optical system systems and the like are usually housed in an enclosure such as a package. A wall portion of the enclosure is provided with a light transmission hole for allowing the optical element to perform optical communication with the outside. For the purpose of ensuring airtightness in the enclosure and the like, the light transmission hole is covered with a window component for an optical element.
[0003] For example, the following Patent Document 1 discloses a window component for an optical element including a window glass whose outer contour is a regular octagon or a regular polygon with more sides than a regular octagon. In Patent Document 1, if the window glass of the window component for an optical element is a regular octagon, a plurality of positions of the glass substrate 14 shown in FIG. 5 of the document are only subjected to a total of four cutting processes in the directions of arrows a to d, and it is described that a large number of window components for optical elements can be manufactured.
Prior Art Documents
Patent Documents
[0004]
Patent Document 1
Summary of Invention
Problems to be Solved by the Invention
[0005] However, as shown in FIG. 5 of Patent Document 1, in the method of cutting a glass substrate so as to hollow it out into a window glass of a regular octagon or the like, portions of the glass substrate other than the hollowed-out window glass cannot be used, and there is a problem that it is difficult to increase the number of obtainable window glasses.
[0006] The object of the present invention is to provide a method for manufacturing a transparent member, a transparent member, and a window component for an optical element using the transparent member, which can increase the number of pieces that can be obtained from a transparent substrate that serves as the base material. [Means for solving the problem]
[0007] This paper describes a method for manufacturing a transparent member, a transparent member, and various embodiments of a window component for an optical element using the transparent member, all of which solve the above problems.
[0008] A method for manufacturing a transparent member according to Embodiment 1 of the present invention is characterized by comprising a first step of forming a plurality of through holes in a transparent substrate, and a second step of dividing the transparent substrate along a virtual line connecting the centers of the plurality of through holes to obtain a transparent member.
[0009] In the manufacturing method of the transparent member according to Embodiment 2, the planar shape of the through-hole may be polygonal in Embodiment 1. In this case, it is preferable to divide the transparent substrate along imaginary lines connecting the vertices of the polygons in the plurality of through-holes.
[0010] In the manufacturing method of the transparent member according to Embodiment 3, it is preferable that in Embodiment 1 or 2, the first step includes the steps of providing a modified portion by irradiating the transparent substrate with laser light at the location where the through-hole is to be formed, and forming a through-hole by etching the location where the through-hole is to be formed on the transparent substrate with the modified portion.
[0011] In the method for manufacturing a transparent member according to Embodiment 4, it is preferable that the division of the transparent substrate in the second step is performed by dicing in any one embodiment from Embodiment 1 to Embodiment 3.
[0012] In the method for manufacturing a transparent member according to Embodiment 5, it is preferable that, in any one embodiment from Embodiments 1 to 4, a film is formed on at least one of the two main surfaces of the transparent substrate after the first step and before the second step.
[0013] In the method for manufacturing a transparent member according to embodiment 6, in embodiment 5, the film is a metallized film provided in a frame shape corresponding to the transparent member after the second step, and it is preferable to form the metallized film such that the width γ of the corner portion is equal to or greater than the width α of the side portion.
[0014] In the method for manufacturing a transparent member according to Embodiment 7, it is preferable that, in any one embodiment from Embodiments 1 to 6, grooves are formed by etching the transparent substrate along a virtual line connecting the centers of the through holes after the first step and before the second step.
[0015] A transparent member according to aspect 8 of the present invention is a transparent member having a first main surface and a second main surface facing each other, a side surface connecting the first main surface and the second main surface, and having a plurality of corners and a plurality of edges in a plan view, characterized in that at least one of the plurality of corners the side surface is an etching surface, and at least one of the plurality of edges the side surface is a dicing surface.
[0016] In the transparent member according to embodiment 9, it is preferable that the maximum valley depth Rv measured in accordance with JIS B 0601:2013 on the etching surface is smaller than the maximum valley depth Rv measured in accordance with JIS B 0601:2013 on the dicing surface.
[0017] In the transparent member according to embodiment 10, in embodiment 8 or 9, it is preferable that the maximum valley depth Rv measured in accordance with JIS B 0601:2013 on the etching surface is 0.100 μm or more and 1.100 μm or less.
[0018] In the transparent member according to embodiment 11, it is preferable that at least one of the plurality of corners has a chamfered shape in any one embodiment from embodiment 8 to embodiment 10.
[0019] The transparent member according to Aspect 12 is, in any one of Aspects 8 to 11, preferably configured such that at least one side portion among the plurality of side portions has a fine chamfered shape.
[0020] The transparent member according to Aspect 13 is, in any one of Aspects 8 to 12, preferably provided with a metallized film on at least one of the first main surface and the second main surface, wherein in the metallized film, a width γ at a corner portion is equal to or greater than a width α at a side portion.
[0021] The transparent member according to Aspect 14 is, in any one of Aspects 8 to 13, preferably provided with an antireflection film on at least one of the first main surface and the second main surface.
[0022] A window component for an optical element according to Aspect 15 is characterized by comprising the transparent member configured according to any one of Aspects 8 to 14. Effects of the Invention
[0023] According to the present invention, it is possible to provide a method for manufacturing a transparent member, a transparent member, and a window component for an optical element using the transparent member, which can increase the number of obtainable pieces from a transparent substrate serving as a base material. Brief Description of the Drawings
[0024] [Figure 1] Figure 1 is a schematic plan view showing a transparent substrate used in the method for manufacturing a transparent member according to one embodiment of the present invention. [Figure 2] Figure 2 is a schematic plan view showing the transparent substrate of Figure 1 in an enlarged manner. [Figure 3] Figure 3 is a schematic plan view showing a transparent substrate of a modified example. [Figure 4] Figures 4(a) to (c) are schematic views showing shapes of through-holes of modified examples. [Figure 5] Figure 5 is a schematic plan view showing a transparent member according to one embodiment of the present invention. [Figure 6] Figure 6 is a schematic cross-sectional view of the portion along line AA in Figure 5. [Figure 7] Figure 7 is a schematic cross-sectional view showing an example in which a transparent member according to one embodiment of the present invention is used as a window component for an optical element. [Figure 8] Figure 8 shows a laser microscope image of the transparent material obtained in the experimental example. [Figure 9] Figure 9 is a laser microscope image of the side surface (dicing surface) at the edge of the transparent material obtained in the experimental example. [Figure 10] Figure 10 is a laser microscope image of the side surface (etched surface) at the corner of the transparent material obtained in the experimental example. [Figure 11] Figure 11(a) shows the roughness curve in the edge direction (X direction) of the side surface (dicing surface) at the edge of the transparent material obtained in the experimental example, and Figure 11(b) shows the roughness curve in the thickness direction (Z direction). [Figure 12] Figure 12(a) shows the roughness curve in the edge direction (X direction) of the side surface (etched surface) at the corner of the transparent material obtained in the experimental example, and Figure 12(b) shows the roughness curve in the thickness direction (Z direction). [Figure 13] Figure 13 is a schematic plan view of a comparative example transparent substrate. [Modes for carrying out the invention]
[0025] Preferred embodiments are described below. However, the following embodiments are merely illustrative, and the present invention is not limited to these embodiments. In addition, in each drawing, components having substantially the same function may be referred to by the same reference numerals.
[0026] [Manufacturing method for transparent components] In the method for manufacturing the transparent member of the present invention, first, multiple through holes are formed in a transparent substrate (first step). Next, the transparent substrate is divided along imaginary lines connecting the centers of the multiple through holes. This allows the transparent member of the present invention to be obtained (second step).
[0027] (First step) Figure 1 is a schematic plan view showing a transparent substrate used in a method for manufacturing a transparent member according to one embodiment of the present invention. Figure 2 is a schematic plan view showing an enlarged view of the transparent substrate in Figure 1. As shown in Figures 1 and 2, in the first step, a plurality of through holes 3 are formed in the transparent substrate 2.
[0028] The transparent substrate 2 transmits at least some light in the wavelength range of 450 nm to 700 nm. In this specification, "transparent" means that the light transmittance in the visible wavelength range of 450 nm to 700 nm is 70% or more.
[0029] The transparent substrate 2 can be made of, for example, glass such as quartz glass or sapphire. In this embodiment, the shape of the transparent substrate 2 is approximately rectangular, but its shape is not particularly limited. The area of the transparent substrate 2 can be, for example, 100 mm². 2 Above, 90,000 mm 2 The following is possible. Furthermore, the thickness of the transparent substrate 2 can be, for example, 0.05 mm or more and 2.00 mm or less.
[0030] In this embodiment, multiple through holes 3 are formed so as to be arranged at equal intervals along the X direction (length direction). Furthermore, multiple through holes 3 are formed so as to be arranged at equal intervals along the Y direction (width direction), which is perpendicular to the X direction. The distance between the centers of adjacent through holes 3 in the X and Y directions can be, for example, 0.50 mm or more and 300 mm or less.
[0031] In this embodiment, multiple through holes 3 are formed such that the planar shape is approximately rhombic. The area of each through hole 3 in plan view is not particularly limited, but for example, 0.01 mm 2 Above, 100mm 2 The following is possible. The number of through holes 3 provided in the transparent substrate 2 is not particularly limited, but for example, it can be 6 or more and 3,000 or less.
[0032] In this invention, the position and shape of the through-holes 3 are not particularly limited and can be appropriately determined according to the shape of the transparent member after individual piece formation. Also, the through-holes 3 do not have to be arranged at equal intervals as in this embodiment.
[0033] The method for forming the through-hole 3 is not particularly limited, but for example, it can be formed by etching the planned location for the through-hole 3 (the planned through-hole formation location) in the transparent substrate 2. In this embodiment, a modified portion is created inside the transparent substrate 2 by irradiating the planned through-hole formation location with laser light, and then the through-hole 3 is formed by etching the planned through-hole formation location of the transparent substrate 2 with the modified portion.
[0034] Laser irradiation can be performed by conventionally known methods, while appropriately adjusting the laser output. As the laser light, for example, a pulsed laser can be used. The wavelength of the pulsed laser is preferably 400 nm or more, more preferably 500 nm or more, particularly preferably 700 nm or more, preferably 1500 nm or less, and more preferably 1000 nm or less. The upper limit of the pulsed laser wavelength is not particularly limited, but for example, it can be 2000 nm.
[0035] Furthermore, the etching process can be carried out by conventionally known methods. The etching process can be performed, for example, by bringing the etching solution into contact with the position where the through-hole 3 is to be formed. Examples of etching solutions include aqueous hydrofluoric acid solution, aqueous nitric acid solution, aqueous hydrochloric acid solution, aqueous ferric chloride solution, aqueous oxalic acid solution, or a mixed solution containing aqueous solutions of at least two of these. Alternatively, the etching solution may be an alkaline detergent.
[0036] As shown in Figure 2, in the manufacturing method of this embodiment, an anti-reflective film 4 and a metallized film 5 are formed on the main surface of a transparent substrate 2. More specifically, a frame-shaped metallized film 5 is formed on the anti-reflective film 4. The anti-reflective film 4 and the metallized film 5 can be formed, for example, by applying a metal mask or the like to areas other than the intended film formation location and depositing them by sputtering or vacuum deposition. Furthermore, as shown in Figure 1, through holes 6 for positioning the metal mask may be provided in advance during film formation.
[0037] In the manufacturing method of this embodiment, the width γ of the metallized film 5 at the corner shown in Figure 2 is preferably greater than or equal to the width α along the Y direction of the metallized film 5 at the edge, more preferably greater than the width α along the Y direction of the metallized film 5 at the edge, even more preferably 1.001 to 5.0 times the width α along the Y direction of the metallized film 5 at the edge, particularly preferably 1.01 to 3.0 times, and most preferably 1.2 to 2.7 times. Furthermore, the width γ of the metallized film 5 at the corner shown in Figure 2 is preferably greater than or equal to the width β along the X direction of the metallized film 5 at the edge, more preferably greater than the width β along the X direction of the metallized film 5 at the edge, even more preferably 1.001 to 5.0 times the width β along the X direction of the metallized film 5 at the edge, particularly preferably 1.01 to 3.0 times, and most preferably 1.2 to 2.7 times.
[0038] This makes it easier to improve airtightness when the transparent member 1 is used as a window component for an optical element. As a result, the reliability of the window component for the optical element can be further improved.
[0039] The width γ of the metallized film 5 at the corners may be, for example, 0.1 mm to 5.0 mm, or 0.2 mm to 3.0 mm. By doing so, when the transparent member 1 is used as a window component for an optical element, it becomes easier to more reliably improve airtightness. As a result, the reliability of the window component for the optical element can be more reliably improved.
[0040] The width α of the metallized film 5 along the Y direction is not particularly limited, but for example, α may be 0.1 mm to 1.0 mm or 0.1 mm to 0.5 mm. Similarly, the width β of the metallized film 5 along the X direction may be β may be 0.1 mm to 1.0 mm or 0.1 mm to 0.5 mm. By doing so, when the transparent member 1 is used as a window component for an optical element, it becomes easier to more reliably improve airtightness. As a result, the reliability of the window component for the optical element can be more reliably improved. Also, when the width of the metallized film 5 is such that the width α along the Y direction equals the width β along the X direction, it becomes easier to distribute the stress when bonding the transparent member 1 to the window component for the optical element by soldering. Of course, depending on the design of the window component for the optical element, the width of the metallized film 5 may be α ≠ β.
[0041] In this invention, only one of the anti-reflective film 4 and the metallizing film 5 may be formed, or the other film may be formed. Furthermore, the metallizing film 5 may be formed directly on the transparent substrate 2. Alternatively, no film may be formed on the transparent substrate 2. The anti-reflective film 4 may be provided on the main surfaces on both sides of the transparent substrate 2.
[0042] (Second step) In the second step, the transparent substrate 2 is divided along the imaginary lines X1 and Y1 shown in Figures 1 and 2. This separates the transparent substrate 2 into individual pieces, thereby obtaining transparent components. Note that imaginary line X1 is a straight line connecting the centers of the through holes 3 in the X direction, and imaginary line Y1 is a straight line connecting the centers of the through holes 3 in the Y direction.
[0043] The method for dividing the transparent substrate 2 is not particularly limited, but for example, it can be done by dicing. For example, the transparent substrate 2 is divided by passing a dicing blade along the virtual line X1. Next, the transparent substrate 2 is divided by passing a dicing blade along the virtual line Y1 to obtain a transparent component.
[0044] In the manufacturing method of this embodiment, as shown in Figure 5, a transparent member 1 having a substantially rectangular shape with chamfered corners 11a to 11d can be obtained. According to the manufacturing method of this embodiment, even when manufacturing a transparent member having such a shape, the number of pieces that can be obtained from the transparent substrate 2, which is the base material, can be increased. This point can be explained as follows.
[0045] Conventionally, when forming a transparent member having a roughly rectangular shape with chamfered corners by dicing, it was necessary to divide the transparent substrate 100 along the dashed lines shown in Figure 13. However, in this case, it was not possible to use the parts of the transparent substrate 100 other than the transparent member cut out in the desired shape, which presented the problem of being difficult to obtain a large number of transparent members 1.
[0046] In contrast, the manufacturing method of this embodiment divides the transparent substrate 2 along the virtual lines X1 and Y1 shown in Figures 1 and 2, thereby minimizing the unusable portion of the transparent substrate 2 and increasing the number of transparent members obtained.
[0047] In the transparent member 1 obtained by the manufacturing method of this embodiment, the corners 11a to 11d have a chamfered shape. Therefore, for example, when the transparent member 1 is used as a window component for an optical element, as described later, and is joined to a surrounding body 22 such as the package shown in Figure 7, the corners 11a to 11d of the transparent member 1 are less likely to interfere with the frame of the surrounding body 22. In addition, conventionally, when cutting a substrate with a dicing blade, unnecessary protrusions (burrs) sometimes occur on the cut surface. In contrast, in the transparent member 1 of this embodiment, unlike the transparent member obtained by cutting with a dicing blade, no burrs like those described above are formed on the corners 11a to 11d, and as a result, the corners 11a to 11d of the transparent member 1 are less likely to interfere with the frame of the surrounding body 22. Therefore, the transparent member 1 obtained by the manufacturing method of this embodiment can be suitably used as a window component for an optical element.
[0048] Furthermore, in the manufacturing method of this embodiment, through-holes 3 are formed by etching the positions where through-holes are to be formed in the transparent substrate 2. Therefore, if the transparent member 1 is divided along virtual lines X1 and Y1 connecting the centers of the through-holes 3, the side surfaces 10c at the corners 11a to 11d become the etched surfaces.
[0049] Incidentally, as shown in Figures 5 and 7, when the transparent member 1 of this embodiment is used as a window component for an optical element, soldering is performed between the transparent member 1 and the surrounding body 22 in the metallized film 5. In this case, the amount of solder provided near the corners 11a to 11d tends to be large, so the stress of the solder joint tends to concentrate at the corners 11a to 11d. However, in the transparent member 1 of this embodiment, the side surfaces 10c of the corners 11a to 11d are etched surfaces, so chipping (breakage) like that that occurs in dicing is less likely to occur. Therefore, in the transparent member 1 of this embodiment, the strength of the corners 11a to 11d is high, and even when the stress of the solder joint concentrates, damage is less likely to occur. Thus, from this point of view as well, the transparent member 1 obtained by the manufacturing method of this embodiment can be suitably used as a window component for an optical element.
[0050] In particular, when the width γ of the metallized film 5 at the corners is set to be greater than or equal to the width α along the Y direction of the metallized film 5 at the edges, the amount of solder provided near the corners 11a to 11d tends to increase, and therefore the stress of the solder joint tends to concentrate, especially at the corners 11a to 11d. However, in the transparent member 1 of this embodiment, the side surface 10c of the corners 11a to 11d is an etched surface, so chipping (breakage) like that that occurs during dicing is less likely to occur. Therefore, in the transparent member 1 of this embodiment, the strength of the corners 11a to 11d is high, and even when the stress of the solder joint concentrates, damage is less likely to occur.
[0051] In this invention, after forming through holes 3 in the first step, etching may be performed along virtual lines X1 and Y1 connecting the through holes 3 to form grooves 7 as shown in Figure 3. It is desirable to apply a metal mask to areas other than the intended location for forming grooves 7 during the etching process. In the transparent member 1 obtained by dividing the transparent substrate 2 along these grooves 7, the side surfaces 10c of the edges 12a to 12d can also be chamfered. In this case, when the transparent member 1 is used as a window component for an optical element and soldered, it can be made even less prone to damage.
[0052] Furthermore, in the above embodiment, a through-hole 3 with a substantially rhombic planar shape was formed, but the shape of the through-hole 3 is not particularly limited. The planar shape of the through-hole 3 may be substantially square, as shown in Figure 4(a), or substantially circular, as shown in Figure 4(b). Alternatively, as shown in Figure 4(c), a substantially circular through-hole 3A for positioning may be provided between the substantially rhombic through-holes 3. When this positioning through-hole 3A is divided, it becomes crescent-shaped and can be used, for example, for positioning when using the transparent member 1 as a window component for an optical element and attaching it to the surrounding body 22. Note that the multiple through-holes 3 do not necessarily have the same shape, and a combination of through-holes 3 having different planar shapes is also possible.
[0053] [Transparent material] Figure 5 is a schematic plan view showing a transparent member according to one embodiment of the present invention. Figure 6 is a schematic cross-sectional view of the portion along line AA in Figure 5.
[0054] As shown in Figures 5 and 6, the substrate body 10 of the transparent member 1 has opposing first main surface 10a and second main surface 10b. The substrate body 10 of the transparent member 1 also has a side surface 10c connecting the first main surface 10a and the second main surface 10b.
[0055] The substrate body 10 of the transparent member 1 can be made of, for example, glass such as quartz glass or sapphire. In this embodiment, the shape of the transparent member 1 is approximately rectangular, but its shape is not particularly limited. The area of the transparent member 1 is, for example, 1 mm². 2 Above, 400mm 2 The following is possible. The thickness of the substrate body 10 of the transparent member 1 can be, for example, 0.05 mm or more and 2.00 mm or less.
[0056] As shown in Figure 5, the transparent member 1 has four corners 11a to 11d and four edges 12a to 12d. In the transparent member 1, the four corners 11a to 11d have a chamfered shape. For example, c (dimension of the cut-off edge) can be set to 0.05 mm to 0.20 mm in the four corners 11a to 11d.
[0057] Furthermore, the transparent member 1 may have chamfered edges on its four sides 12a to 12d. In this case, as described above, when the transparent member 1 is used as a window component for an optical element and soldered to the surrounding body 22, damage can be made even less likely. The chamfered edge shape can be, for example, c (dimension of the cut-off edge) = 0.01 mm or more and 0.20 mm or less, and c (dimension of the cut-off edge) = 0.03 mm or more and 0.06 mm or less is more preferable.
[0058] In the transparent member 1, the side surfaces 10c at the four corners 11a to 11d are the etching surfaces. Also, the side surfaces 10c at the four edges 12a to 12d are the dicing surfaces. Such a transparent member 1 can be manufactured, for example, by the method for manufacturing a transparent member of the present invention described above.
[0059] In this invention, it is sufficient that an etched surface is provided on the side surface 10c at at least one of the four corners 11a to 11d. Also, it is sufficient that a diced surface is provided on the side surface 10c at at least one of the four edges 12a to 12d.
[0060] As in the transparent member 1 of this embodiment, when the side surface 10c at the corners 11a to 11d is an etched surface, chipping (breakage) that occurs during dicing is less likely to occur. Therefore, in the transparent member 1, the strength of the corners 11a to 11d is high, and even when stress from solder joints is concentrated at the corners 11a to 11d, damage is less likely to occur. Accordingly, the transparent member 1 of this embodiment can be suitably used as a window component for optical elements.
[0061] As described above, the transparent member 1 of this embodiment may have a metallized film 5 provided on the substrate body 10. The width γ of the metallized film 5 at the corner is preferably greater than or equal to the width α along the Y direction of the metallized film 5 at the edge, more preferably greater than the width α along the Y direction of the metallized film 5 at the edge, even more preferably 1.001 to 5.0 times the width α along the Y direction of the metallized film 5 at the edge, particularly preferably 1.01 to 3.0 times, and most preferably 1.2 to 2.7 times. Also, the width γ of the metallized film 5 at the corner shown in Figure 5 is preferably greater than or equal to the width β along the X direction of the metallized film 5 at the edge, more preferably greater than the width β along the X direction of the metallized film 5 at the edge, even more preferably 1.001 to 5.0 times the width β along the X direction of the metallized film 5 at the edge, particularly preferably 1.01 to 3.0 times, and most preferably 1.2 to 2.7 times.
[0062] This makes it easier to improve airtightness when the transparent material 1 is used as a window component for an optical element. As a result, the reliability of the window component for the optical element can be further improved.
[0063] Furthermore, in the case of the metallized film 5 having the above-mentioned width characteristics, the amount of solder provided near the corners 11a to 11d tends to be large, and therefore, stress from solder joints tends to concentrate particularly at the corners 11a to 11d. However, in the transparent member 1 of this embodiment, the side surfaces 10c of the corners 11a to 11d are etched surfaces, so chipping (breakage) like that that occurs during dicing is less likely to occur. Therefore, in the transparent member 1 of this embodiment, the strength of the corners 11a to 11d is high, and even when stress from solder joints is concentrated, damage is less likely to occur.
[0064] The width γ of the metallized film 5 at the corners may be, for example, 0.1 mm to 5.0 mm, or 0.2 mm to 3.0 mm. This makes it easier to more reliably improve airtightness when the transparent member 1 is used as a window component for an optical element. As a result, the reliability of the window component for the optical element can be more reliably improved.
[0065] The width α of the metallized film 5 along the Y direction at the edge is not particularly limited, but for example, α may be 0.1 mm to 1.0 mm or 0.1 mm to 0.5 mm. Similarly, the width β of the metallized film 5 along the X direction at the edge may be β may be 0.1 mm to 1.0 mm or 0.1 mm to 0.5 mm. By doing so, when the transparent member 1 is used as a window component for an optical element, it becomes easier to more reliably improve airtightness. As a result, the reliability of the window component for the optical element can be more reliably improved. Also, when the width of the metallized film 5 is α along the Y direction = β along the X direction, it becomes easier to distribute the stress when bonding the transparent member 1 to the window component for the optical element by soldering. Of course, depending on the design of the window component for the optical element, the width of the metallized film 5 may be α ≠ β.
[0066] In this embodiment, it is preferable that the maximum valley depth Rv of the side surface 10c (etched surface) at the corners 11a to 11d is smaller than the maximum valley depth Rv of the side surface 10c (dicing surface) at the edges 12a to 12d. In this case, the strength of the corners 11a to 11d can be further increased, and even when solder joint stress is concentrated at the corners 11a to 11d, damage can be made even less likely to occur.
[0067] The maximum valley depth Rv of the side surface 10c (etched surface) at the corners 11a to 11d is preferably 0.100 μm or more, more preferably 0.300 μm or more, preferably 1.100 μm or less, more preferably 1.000 μm or less, and even more preferably 0.800 μm or less. When the maximum valley depth Rv of the side surface 10c (etched surface) at the corners 11a to 11d is within the above range, the strength of the corners 11a to 11d can be further increased, and even when stress from solder joints is concentrated at the corners 11a to 11d, damage can be made even less likely to occur. The maximum valley depth Rv can be measured in accordance with JIS B 0601:2013.
[0068] Furthermore, it is preferable that the maximum cross-sectional height Rt, load length ratio Rmr, and crustosis Rku of the side surface 10c (etched surface) at the corners 11a to 11d are smaller than those of the maximum cross-sectional height Rt, load length ratio Rmr, and crustosis Rku of the side surface 10c (dicing surface) at the edges 12a to 12d.
[0069] On the other hand, the maximum peak height Rp, average height Rc, skewness Rsk, and average length RSm of the roughness curve elements of the side surface 10c (etched surface) at the corners 11a to 11d are preferably larger than those of the maximum peak height Rp, average height Rc, skewness Rsk, and average length RSm of the roughness curve elements of the side surface 10c (dicing surface) at the edges 12a to 12d.
[0070] The maximum peak height Rp of the side surface 10c (etched surface) at corners 11a to 11d can be, for example, 0.500 μm or more and 3.000 μm or less. The maximum cross-sectional height Rt of the side surface 10c (etched surface) at corners 11a to 11d can be, for example, 0.500 μm or more and 2.500 μm or less. The load length ratio Rmr of the side surface 10c (etched surface) at corners 11a to 11d can be, for example, 10% or more and 50% or less. The average height Rc of the side surface 10c (etched surface) at corners 11a to 11d can be, for example, 0.500 μm or more and 3.000 μm or less. The average length RSm of the elements of the roughness curve of the side surface 10c (etched surface) at corners 11a to 11d can be, for example, 8 μm or more and 30 μm or less. The kurtosis Rku of the side surface 10c (etched surface) at corners 11a to 11d can be, for example, 1 μm or more and 10 μm or less. All parameters can be measured in accordance with JIS B 0601:2013.
[0071] In this embodiment, as shown in Figure 6, the anti-reflective film 4 and the metallized film 5 are provided on the substrate body 10 in this order. The anti-reflective film 4 may also be provided on both sides of the first main surface 10a and the second main surface 10b.
[0072] As the anti-reflective coating 4, for example, a laminated film can be used in which a low refractive index film, a medium refractive index film, and a high refractive index film are alternately laminated.
[0073] For low refractive index films, materials such as SiO, SiO2, and MgF2 can be used.
[0074] For example, Al2O3 can be used as the material for the medium refractive index film.
[0075] Examples of materials that can be used for high refractive index films include Ta2O5, TiO, TiO2, Nb2O5, HfO2, ZrO2, and Si.
[0076] The thickness of the low refractive index film can be, for example, 10 nm or more and 5000 nm or less. The thickness of the medium refractive index film can be, for example, 10 nm or more and 5000 nm or less. The thickness of the high refractive index film can be, for example, 10 nm or more and 5000 nm or less.
[0077] The anti-reflective coating 4 may consist of alternating layers of low-refractive-index and high-refractive-index coatings, alternating layers of low-refractive-index and medium-refractive-index coatings, or alternating layers of medium-refractive-index and high-refractive-index coatings. Furthermore, the anti-reflective coating 4 may consist solely of low-refractive-index coatings. The overall thickness of the anti-reflective coating 4 can be, for example, between 20 nm and 10,000 nm.
[0078] The metallized film 5 is not particularly limited, but a laminated film can be used in which a first layer, a second layer, and a third layer are stacked in that order.
[0079] The first layer may consist of Cr, Ti, Ta, or TiW. Among these, the first layer is preferably made of Cr. The second layer may consist of Ni, Pt, Pd, TiW, or an alloy containing Ni such as Ni-Cr. Among these, the second layer is preferably made of Ni. The third layer may consist of Au.
[0080] The thickness of the first layer can be, for example, 0.01 μm or more and 0.50 μm or less. The thickness of the second layer can be, for example, 0.10 μm or more and 8.00 μm or less. The thickness of the third layer can be, for example, 0.01 μm or more and 3.00 μm or less.
[0081] The metallized film 5 only needs to include at least one of the first layer, the second layer, and the third layer described above. The total thickness of the metallized film 5 can be, for example, 0.12 μm or more and 11.5 μm or less.
[0082] Furthermore, when joining using gold-tin solder or tin-silver-copper solder, it is desirable to provide both the anti-reflective coating 4 and the metallizing coating 5. On the other hand, when sealing with low-melting-point glass or when sealing with adhesive when hermetic sealing is not required, only the anti-reflective coating 4 may be provided without the metallizing coating 5.
[0083] [Window component for optical element] Figure 7 is a schematic cross-sectional view showing an example in which a transparent member according to one embodiment of the present invention is used as a window component for an optical element. In Figure 7, the optical element is shown as a schematic diagram of a rectangle with two diagonals added.
[0084] Figure 7 shows an example of an optical module 20 in which an optical element 21 is housed in a surrounding body 22. The surrounding body 22 has light-transmitting holes 23 that transmit light for optical communication, etc. The transparent member 1 in this embodiment is a window component for the optical element that covers the light-transmitting holes 23. The transparent member 1 transmits light for optical communication, etc. The transparent member 1 is soldered to the surrounding body 22 in a metallized film 5.
[0085] The window component (transparent member 1) for the optical element in this embodiment has a shape in which the corners 11a to 11d are chamfered. Therefore, when joining the transparent member 1 to a surrounding body 22 such as a package, the corners 11a to 11d of the transparent member 1 are less likely to interfere with the frame of the surrounding body 22.
[0086] Furthermore, the window component for the optical element (transparent member 1) of this embodiment has high strength at the corners 11a to 11d, making it less likely to break even when stress from solder joints is concentrated at the corners 11a to 11d.
[0087] The following describes experimental examples. However, the present invention is not limited in any way to the following experimental examples.
[0088] (Example of experiment) In the experimental example, through-holes 3 shown in Figures 1 and 2 were fabricated. Specifically, a modified area was created inside the transparent substrate 2 by irradiating the area where the through-hole was to be formed with laser light. Subsequently, the area where the through-hole was to be formed, containing the modified area, was etched to form a roughly diamond-shaped through-hole 3. The etching process was performed by bringing an etching solution into contact with the area where the through-hole was to be formed.
[0089] Next, the transparent substrate 2 was divided along the virtual lines X1 and Y1 shown in Figures 1 and 2 to obtain the transparent member 1 shown in Figures 5 and 6. As shown in Figure 5, the obtained transparent member 1 had a shape in which the corners 11a to 11d were chamfered.
[0090] Figure 8 shows a laser microscope image of the transparent material obtained in the experimental example. The laser microscope image was taken using a laser microscope (OLYMPUS, model number "OLS4000") at a magnification of 20x. As shown in Figure 8, chipping was observed on the side surface (dicing surface) at the edge of the obtained transparent material 1. On the other hand, no chipping was observed on the side surface (etching surface) at the corner of the obtained transparent material 1.
[0091] Figure 9 is a laser microscope image of the side surface (dicing surface) at the edge of the transparent material obtained in the experimental example. Figure 10 is a laser microscope image of the side surface (etching surface) at the corner of the transparent material obtained in the experimental example. The laser microscope images were measured at a magnification of 100x using a laser microscope (OLYMPUS, model number "OLS4000").
[0092] Furthermore, Figure 11(a) shows the roughness curve in the edge direction (X direction) of the side surface (dicing surface) at the edge of the transparent material obtained in the experimental example, and Figure 11(b) shows the roughness curve in the thickness direction (Z direction). Figure 12(a) shows the roughness curve in the edge direction (X direction) of the side surface (etching surface) at the corner of the transparent material obtained in the experimental example, and Figure 12(b) shows the roughness curve in the thickness direction (Z direction). The roughness curves were measured using a laser microscope (OLYMPUS, model number "OLS4000") in accordance with JIS B 0601:2013.
[0093] As shown in Figures 11(a) and (b), a linear waveform was observed as the roughness curve on the side surface (dicing surface) at the edge of the transparent member in both the edge direction (X direction) and the thickness direction (Z direction), but waveform disturbance (partial valley depth) due to chipping was also observed. On the other hand, as shown in Figures 12(a) and (b), no waveform disturbance due to chipping was observed on the side surface (etching surface) at the corner of the transparent member in either the edge direction (X direction) or the thickness direction (Z direction), but a convex waveform toward the center was observed as the roughness curve, especially in the thickness direction.
[0094] Next, the parameters of the roughness curve in the edge direction (X direction) and thickness direction (Z direction) were measured on the side surfaces (etched surfaces) at the corners of the obtained transparent material. Furthermore, the parameters of the roughness curve in the edge direction (X direction) and thickness direction (Z direction) were measured on the side surfaces (dicing surfaces) at the edges of the obtained transparent material. The parameters measured included maximum groove depth Rv, maximum cross-sectional height Rt, load length ratio Rmr, maximum peak height Rp, average height Rc, skewness Rsk, average length of roughness curve elements RSm, and crustosis Rku. The measurements were performed in accordance with JIS B 0601:2013 using a laser microscope (OLYMPUS, model number "OLS4000").
[0095] The results are shown in Table 1 below.
[0096] [Table 1]
[0097] As shown in Table 1, for example, it was confirmed that the maximum valley depth Rv was smaller on the side surface (etched surface) at the corner of the obtained transparent member than on the side surface (diced surface) at the edge. [Explanation of symbols]
[0098] 1…Transparent component 2…Transparent substrate 3,3A,6…Through hole 4…Anti-reflective film 5…Metallized film 7… Groove 10…Main board 10a, 10b… First and second main surfaces 10c...side 11a~11d…corner 12a~12d…Side part 20… Optical module 21… Optical element 22...Siege 23...Light transmission hole 100…Transparent substrate
Claims
1. A window component for an optical element, comprising a transparent member having a first main surface and a second main surface facing each other, a side surface connecting the first main surface and the second main surface, and having a plurality of corners and a plurality of edges in a plan view, In at least one of the aforementioned multiple corners, the side surface is an etched surface. A window component for an optical element, wherein at least one of the plurality of edges has a diced surface on its side.
2. The window component for an optical element according to claim 1, wherein the maximum valley depth Rv measured in accordance with JIS B 0601:2013 on the etching surface is smaller than the maximum valley depth Rv measured in accordance with JIS B 0601:2013 on the dicing surface.
3. The window component for an optical element according to claim 1 or 2, wherein the maximum valley depth Rv measured in accordance with JIS B 0601:2013 on the etched surface is 0.100 μm or more and 1.100 μm or less.
4. The optical element window component according to claim 1 or 2, wherein at least one of the plurality of corners has a chamfered shape.
5. The optical element window component according to claim 1 or 2, wherein at least one of the plurality of edges has a chamfered shape.
6. A frame-shaped metallized film is provided on at least one of the first main surface and the second main surface. The optical element window component according to claim 1 or 2, wherein the width γ of the corner portion of the metallized film is greater than or equal to the width α of the side portion.
7. The window component for an optical element according to claim 1 or 2, wherein an anti-reflective coating is provided on at least one of the first main surface and the second main surface.
Citation Information