Cu-Co-containing electrode and method for fabrication

Cu-Co-containing electrodes in an electrochemical pathway address the inefficiencies of conventional methods by enabling direct hydrocarbon utilization, producing H2 and CO efficiently and cost-effectively without separate purification, suitable for on-site production and greenhouse gas conversion.

JP2026538949APending Publication Date: 2026-11-19UTILITY GLOBAL INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2026518565
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-11-02
Filing Date
2024-10-09
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Conventional methods for producing hydrogen (H2) and carbon monoxide (CO) require extensive and expensive separation and purification processes, making them inefficient and costly.

Method used

The use of Cu-Co-containing electrodes in an electrochemical pathway that allows direct utilization of hydrocarbons without reforming, utilizing a mixed conductive film and membrane to produce H2 and CO efficiently, eliminating the need for separate purification steps.

Benefits of technology

This approach enables cost-effective and efficient production of H2 and CO with minimal coke formation, facilitating on-site production and reducing greenhouse gas emissions by converting CO2 into CO, while avoiding the need for electricity and separate purification processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026538949000001_ABST
    Figure 2026538949000001_ABST
Patent Text Reader

Abstract

This specification describes a method for producing a Cu-Co-containing electrode precursor, comprising: (a) preparing a mixed conductive film; (b) depositing a dispersion containing CuO particles and CoCGO particles on the film; and (c) sintering the CuO and CoCGO particles at a temperature of 800°C to 1350°C to form a Cu-Co-containing electrode precursor. In one embodiment, the molar ratio of Cu to Co is 3:1 to 70:1. In another embodiment, the molar ratio of Cu to Co is 10:1 to 50:1. In another embodiment, sintering is performed at a temperature of 1100°C to 1250°C.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention generally relates to Cu-Co-containing electrodes and methods of making the same. More specifically, the present invention relates to the use of Cu-Co-containing electrodes to produce hydrogen (H2), carbon monoxide (CO), or both.

Background Art

[0002] Carbon monoxide (CO) is a colorless, odorless, tasteless, and flammable gas that is slightly less dense than air. CO readily combines with hemoglobin to form carboxyhemoglobin, which is well known for its toxic effects as it becomes extremely poisonous when its concentration exceeds a certain level. However, CO is an important component in many chemical and industrial processes. CO has a wide range of functions across all fields of chemistry, for example, in metal-carbonyl catalysts, radical chemistry, cation, and anion chemistry. Carbon monoxide is a strong reducing agent and has been used in pyrometallurgy for centuries to reduce metals from ores. As an example for producing special compounds, CO is used in the production of vitamin A.

[0003] Large amounts of hydrogen (H2) are required in the petroleum industry and the chemical industry. For example, large amounts of hydrogen are used for upgrading fossil fuels and producing methanol or hydrochloric acid. In petrochemical plants, hydrogen is required for hydrocracking, hydrodesulfurization, and hydrodealkylation. Hydrogen is also required in hydrogenation processes to increase the saturation level of unsaturated fats and oils. Hydrogen is also a reducing agent for metal ores. Hydrogen can be produced by water electrolysis, steam reforming, laboratory-scale metal-acid processes, thermochemical methods, or anaerobic corrosion. Many countries are aiming for a hydrogen society.

[0004] In the Fischer-Tropsch process, both CO and H2 are essential building blocks and are often produced by converting carbon-rich raw materials (e.g., coal). A mixture of CO and H2 (singus) can be combined, for example, via the Fischer-Tropsch process to produce various liquid fuels. Synus can also be converted into lighter hydrocarbons, methanol, ethanol, or plastic monomers (e.g., ethylene). The CO / H2 ratio is crucial in all such processes for producing the desired compounds. Conventional techniques require extensive and expensive separation and purification processes to obtain CO and H2 as building blocks.

[0005] Clearly, there is a growing need for and interest in developing new technological platforms for producing these building blocks and beneficial products. This disclosure considers the production of CO and / or H2 via an efficient electrochemical pathway using Cu-Co-containing electrodes. Furthermore, the methods and systems disclosed herein do not require the extensive and expensive separation and purification processes required in the prior art. [Overview of the project]

[0006] This specification describes a method for producing a Cu-Co-containing electrode precursor, comprising: (a) preparing a mixed conductive film; (b) depositing a dispersion containing CuO particles and CoCGO particles on the film; and (c) sintering the CuO and CoCGO particles at a temperature of 800°C to 1350°C to form a Cu-Co-containing electrode precursor. In one embodiment, the molar ratio of Cu to Co is 3:1 to 70:1. In another embodiment, the molar ratio of Cu to Co is 10:1 to 50:1. In another embodiment, sintering is performed at a temperature of 1100°C to 1250°C.

[0007] In one embodiment, the dispersion contains a pore-forming agent. In one embodiment, the pore-forming agent includes polymethyl methacrylate (PMMA), carbon black, graphite, carbon, cellulose, walnut shell, or a combination thereof. In one embodiment, the dispersion contains 2 to 20% by weight of the pore-forming agent.

[0008] In one embodiment, the film is supported on another electrode precursor. In one embodiment, the other electrode precursor comprises NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof. In one embodiment, the other electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ.

[0009] In one embodiment, the film comprises an electronically conductive phase and an ionically conductive phase, wherein the electronically conductive phase comprises doped lanthanum chromite or LST, or an electronically conductive metal, or a combination thereof, and the ionically conductive phase comprises a material selected from the group consisting of gadolinium-doped ceria or samarium-doped ceria, yttria-stabilized zirconia (YSZ), lanthanum strontium gallate magnesite (LSGM), scandia-stabilized zirconia (SSZ), Sc and Ce-doped zirconia (SCZ), and combinations thereof.

[0010] In one embodiment, the membrane comprises CoCGO or LST-stabilized zirconia. In one embodiment, the stabilized zirconia comprises YSZ, SSZ, or SCZ (scandiacelia-stabilized zirconia), and LST comprises LaSrCaTiO3. In one embodiment, the membrane comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

[0011] Furthermore, this specification considers an electrochemical cell comprising a first electrode precursor having CuO and CoCGO, wherein the molar ratio of Cu to Co is 3:1 to 70:1, a second electrode precursor, and a mixed conductive film between the two electrode precursors. In one embodiment, the molar ratio of Cu to Co is 10:1 to 50:1.

[0012] In one embodiment, the second electrode precursor comprises NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof. In one embodiment, the second electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ.

[0013] In one embodiment, the membrane comprises CoCGO or LST-stabilized zirconia. In another embodiment, the membrane comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

[0014] Further aspects and embodiments are provided in the following drawings, detailed description, and claims. Unless otherwise specified, the features described herein can be combined, and all such combinations are within the scope of this disclosure.

[0015] The following drawings are provided to illustrate certain embodiments described herein. The drawings are illustrative only and are not intended to limit the scope of the claims or to show all possible features or embodiments of the claims. The drawings are not necessarily drawn to a fixed scale, and in some cases, certain elements of the drawings may be enlarged relative to other elements of the drawings for illustrative purposes. [Brief explanation of the drawing]

[0016] [Figure 1] An example of an electrochemical (EC) reactor or electrochemical gas generator according to one embodiment of the present disclosure is provided. [Figure 2A] An example of a tubular electrochemical reactor according to one embodiment of the present disclosure is provided. [Figure 2B] A cross-sectional view of a tubular electrochemical reactor according to one embodiment of the present disclosure is shown as an example. [Figure 3] An example of a CO and H2 simultaneous production system having an electrochemical reactor according to one embodiment of this disclosure is provided. [Modes for carrying out the invention]

[0017] overview The following terms and phrases have the meanings expressed below unless otherwise specified herein. This disclosure may adopt other terms and phrases not expressly defined herein. Such other terms and phrases shall have the meanings that a person skilled in the art would have in the context of this disclosure. In some cases, a term or phrase may be defined in the singular or plural form. In such cases, it should be understood that any singular term may also have a plural form, and vice versa, unless otherwise expressly stated.

[0018] Where used herein, the singular forms “a,” “an,” and “the” include plural referents unless the context clearly indicates otherwise. For example, a reference to “substituents” includes a single substituent and two or more substituents, etc. Where used herein, “for example,” “for instance,” “such as,” or “including” means to introduce examples that further clarify a more general subject. Unless expressly otherwise, such examples are provided solely to aid in understanding the embodiments illustrated in this disclosure and are not intended to limit them in any way. Furthermore, these phrases do not expressly imply any priority of any kind over the disclosed embodiments.

[0019] As used herein, unless otherwise specified, composition and material are used interchangeably. Each composition / material may have a plurality of elements, phases, and components. Heating as used herein refers to actively applying energy to a composition or material.

[0020] As used herein, YSZ refers to yttria-stabilized zirconia, SDC refers to samaria-doped ceria, SSZ refers to scandia-stabilized zirconia, and LSGM refers to lanthanum strontium gallate magnesite.

[0021] In the present disclosure, the absence of a substantial amount of H2 means that the volume content of hydrogen is 5% or less, or 3% or less, or 2% or less, or 1% or less, or 0.5% or less, or 0.1% or less, or 0.05% or less.

[0022] As used herein, CGO refers to gadolinium-doped ceria, also known as gadolinia-doped ceria, gadolinium-doped cerium oxide, cerium(IV) oxide, gadolinium-doped, GDC, or GCO (formula Gd:CeO₂). CGO and GDC are used interchangeably unless otherwise specified. Syngas (i.e., synthesis gas) in the present disclosure refers to a mixture mainly composed of hydrogen, carbon monoxide, and carbon dioxide.

[0023] Mixed ionic-electronic conducting membranes can transport both electrons and ions. Ionic conductivity includes ionic species such as oxygen ions (or oxide ions), protons, halide anions, and chalcogenide anions. In various embodiments, the mixed ionic-electronic conducting membrane of the present disclosure comprises an electronically conductive phase and an ionically conductive phase.

[0024] In the present disclosure, although the axial cross-section of the tubular body is shown as being circular, this is merely illustrative and not limiting. The axial cross-section of the tubular body may be any suitable shape known to those skilled in the art, such as a square, a rounded square, a rectangle, a rounded rectangle, a triangle, a hexagon, a pentagon, an ellipse, or an irregular shape.

[0025] As used herein, ceria refers to cerium oxide, also known as ceric oxide or cerium dioxide, which is an oxide of the rare earth metal cerium. Doped ceria refers to ceria doped with other elements, such as samaria-doped ceria (SDC) or gadolinium-doped ceria (GDC or CGO). As used herein, chromite refers to chromium oxide, which includes all oxidation states of chromium oxide.

[0026] As used herein, an impermeable layer or substance refers to being impermeable to fluid flow. For example, the impermeable layer or substance has a permeability of less than 1 microdarcy, or less than 1 nanodarcy.

[0027] In the present disclosure, sintering refers to the process of forming a solid mass of a material by heat or pressure, or a combination thereof, without melting the material to the point of liquefaction. For example, material particles are aggregated by heating to form a solid or porous mass, and atoms within the material particles diffuse across the boundaries of the particles, causing the particles to fuse and form a single solid piece.

[0028] The term "in situ" in the present disclosure refers to a treatment (e.g., heating or decomposition) process that is performed either in the same location or in the same device. For example, ammonia decomposition that occurs in an electrochemical reactor at the anode is considered in situ.

[0029] Electrochemistry is a branch of physical chemistry that deals with the relationship between electric potential as a measurable and quantitative phenomenon and electric potential as a result of a particular chemical change, or vice versa, of a identifiable chemical change. These reactions involve electrons moving between electrodes via an electron-conducting phase (typically, but not necessarily, an external electrical circuit) separated by an ionic-conducting and electronically insulating film (or ionic species in solution). When a chemical reaction is influenced by a potential difference, as in electrolysis, or when a potential is generated from a chemical reaction, as in a battery or fuel cell, it is called an electrochemical reaction. Unlike chemical reactions, in electrochemical reactions electrons (and the ions that inevitably result) move not directly between molecules, but via the aforementioned electron-conducting and ion-conducting circuits, respectively. This phenomenon distinguishes electrochemical reactions from chemical reactions.

[0030] In relation to electrochemical reactors and their use, various components of the reactor, such as electrodes and membranes, are described along with the materials used to construct them. The following description enumerates various aspects and embodiments of the invention disclosed herein. No particular embodiment is intended to define the scope of the invention. Rather, the embodiments provide non-limiting examples of various compositions and methods that fall within the scope of the claimed invention. This description should be read from the perspective of those skilled in the art. Therefore, it does not necessarily contain information that is well known to those skilled in the art.

[0031] Interconnections within electrochemical devices (e.g., fuel cells) are often either metal or ceramic, placed between individual cells or repeating units. Their purpose is to connect each cell or repeating unit so that electricity can be distributed or combined. Interconnections are also referred to as bipolar plates in electrochemical devices. As used herein, an impermeable layer of an interconnection refers to a layer that is impermeable to the flow of fluid.

[0032] Cu-Co containing electrode Hydrocarbons, when used directly, cause coke in electrodes; therefore, hydrocarbons as fuel can be used in conventional electrochemical reactors after they have been reformed. Contrary to practice, Cu-Co-containing electrodes have been found to allow direct utilization of hydrocarbons without reforming and with minimal coke. Minimal coke, as used in this disclosure, means that any coke present is not sufficient to cause any significant degradation of electrode performance.

[0033] In one embodiment, the electrochemical cell includes a first electrode precursor having CuO and CoCGO, wherein the molar ratio of Cu to Co is 3:1 to 70:1, a second electrode precursor, and a mixed conductive film between the two electrode precursors. In one embodiment, the molar ratio of Cu to Co is 10:1 to 50:1.

[0034] In one embodiment, the second electrode precursor comprises NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof. In one embodiment, the second electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped strontium titanate)-SCZ. In one embodiment, the film comprises CoCGO-stabilized zirconia or LST-stabilized zirconia. In one embodiment, the film comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

[0035] In one embodiment, a method for producing such a Cu-Co-containing electrode precursor includes (a) preparing a mixed conductive film, (b) depositing a dispersion containing CuO particles and CoCGO particles on the film, and (c) sintering the CuO and CoCGO particles at a temperature of 800°C to 1350°C to form a Cu-Co-containing electrode precursor. In one embodiment, the film is supported on another electrode precursor. In one embodiment, step (c) is the final sintering step in producing an electrochemical cell / reactor. In one embodiment, sintering is carried out at a temperature of 1100°C to 1250°C.

[0036] In one embodiment, the molar ratio of Cu to Co is 3:1 to 70:1. In another embodiment, the molar ratio of Cu to Co is 10:1 to 50:1. In one embodiment, the dispersion contains a pore-forming agent. In another embodiment, the pore-forming agent includes polymethyl methacrylate (PMMA), carbon black, graphite, carbon, cellulose, walnut shell, or a combination thereof. In another embodiment, the dispersion contains 2 to 20% by weight of the pore-forming agent.

[0037] In one embodiment, another electrode precursor comprises NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof. In one embodiment, another electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ.

[0038] In one embodiment, the film comprises an electronically conductive phase and an ionically conductive phase, the electronically conductive phase comprising doped lanthanum chromite, or LST, or an electronically conductive metal, or a combination thereof, and the ionically conductive phase comprising a material selected from the group consisting of gadolinium or samarium-doped ceria, yttria-stabilized zirconia (YSZ), lanthanum strontium gallate magnesite (LSGM), scandia-stabilized zirconia (SSZ), Sc and Ce-doped zirconia (SCZ), and combinations thereof.

[0039] In one embodiment, the membrane comprises CoCGO or LST-stabilized zirconia. In one embodiment, the stabilized zirconia comprises YSZ, SSZ, or SCZ (scandiacelia-stabilized zirconia). In one embodiment, LST comprises LaSrCaTiO3. In one embodiment, the membrane comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

[0040] electrochemical reactor Contrary to conventional practices, electrochemical reactors have been discovered that include the Cu-Co-containing electrodes discussed above, and, in some cases, an ion-conducting membrane that is also electronically conductive. The reactors of this disclosure can directly utilize hydrocarbons as fuel without reforming and with minimal coke.

[0041] Figure 1A illustrates an electrochemical reactor or electrochemical (EC) gas generator 100 according to one embodiment of the present disclosure. The electrochemical reactor (or EC gas generator) device 100 includes a first electrode 101, a membrane 103, and a second electrode 102. The first electrode 101 is configured to receive a fuel 104 containing hydrocarbons. In various embodiments, the hydrocarbons include species having 1 to 4 carbon atoms. The flow 104 does not contain oxygen. In one embodiment, the anode / first electrode 101 contains Cu and CoCGO, with a Cu to Co molar ratio of 3:1 to 70:1. In one embodiment, the Cu to Co molar ratio is 10:1 to 50:1.

[0042] The second electrode 102 is configured to receive a flow 105 containing carbon dioxide (CO2) and / or water (H2O). In one embodiment, the reactor / device 100 is configured to receive CO2 and / or H2O and produce CO and / or H2 contained in the flow 107 at the second electrode (102). In some cases, the second electrode also receives small amounts of CO or H2, or both. In this situation, CO2 and / or H2O are considered oxidizing agents because they provide the oxide ions (transported through the membrane) necessary to oxidize the fuel at the opposite electrode. Reduction of CO2 produces CO. Reduction of H2O produces H2. Thus, the first electrode 101 undergoes an oxidation reaction in a reducing environment, and the second electrode 102 undergoes a reduction reaction in a reducing environment. In some cases, such an environment is reducing for both electrodes. In various embodiments, both electrodes are exposed to a reducing environment for the entire operating time.

[0043] In this disclosure, "absence of oxygen" means that oxygen is not present at the first electrode 101, or at least not enough oxygen to prevent the reaction. Furthermore, in this disclosure, "water" means only that the raw material in question is water, and does not exclude trace elements or intrinsic components in the water. For example, water containing salts or ions is considered to be within the range of water only. Even if it is water only, 100% pure water is not required, but this includes the embodiments described here.

[0044] In one embodiment, the cathode / second electrode 102 comprises Ni or NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof. In one embodiment, the cathode / second electrode 102 comprises Ni-YSZ or Ni-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ. In some embodiments, the anode and cathode of the reactor (i.e., the first and second electrodes 101 and 102) are activated before receiving flows 104 and 105. In some cases, during activation, CuO is reduced to Cu in the anode and NiO is reduced to Ni in the cathode.

[0045] In various embodiments, 103 represents an oxide ion conductive film. In various embodiments, 103 represents a mixed conductive film, i.e., oxide ion conductive and electronically conductive. In various embodiments, the film comprises an electronically conductive phase and an ionic conductive phase. In one embodiment, the electronically conductive phase comprises a doped lanthanum chromite or an electronically conductive metal, or a combination thereof, and the ionic conductive phase comprises a material selected from the group consisting of gadolinium-doped ceria or samarium-doped ceria, yttria-stabilized zirconia (YSZ), lanthanum-strontium gallate-magnesite (LSGM), scandia-stabilized zirconia (SSZ), Sc and Ce-doped zirconia (SCZ), and combinations thereof.

[0046] In one embodiment, the membrane comprises CoCGO or LST (lanthanum-doped strontium titanate) stabilized zirconia. In one embodiment, the stabilized zirconia comprises YSZ, SSZ, or SCZ (scandiaceria-stabilized zirconia). In one embodiment, LST comprises LaSrCaTiO3. In one embodiment, the membrane comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, or niobium-doped zirconia.

[0047] In one embodiment, the membrane contains cobalt-CGO (CoCGO), i.e., cobalt-doped CGO. In one embodiment, the membrane consists essentially of CoCGO. In one embodiment, the membrane consists of CoCGO. In one embodiment, the membrane contains LST (lanthanum-doped trontium titanate)-YSZ, LST-SSZ, or LST-SCZ (scandiaceria-stabilized zirconia). In one embodiment, the membrane consists essentially of LST-YSZ, LST-SSZ, or LST-SCZ. In one embodiment, the membrane consists of LST-YSZ, LST-SSZ, or LST-SCZ. In this disclosure, LST-YSZ refers to a composite of LST and YSZ. In various embodiments, the LST phase and YSZ phase are interpenetrated with each other. In this disclosure, LST-SSZ refers to a composite of LST and SSZ. In various embodiments, the LST phase and SSZ phase are interpenetrated with each other. In this disclosure, LST-SCZ refers to a composite of LST and SCZ. In various embodiments, the LST phase and the SCZ phase are permeated with each other. YSZ, SSZ, and SCZ are types of stabilized zirconia.

[0048] In various embodiments, the reactor neither produces nor receives electricity. In one embodiment, the reactor does not include interconnects and does not include current collectors. No electricity is required, and such a device is not an electrolytic device. This is a major advantage of the EC reactor of this disclosure. The membrane 103 is configured to conduct electrons and is itself mixed conductive, i.e., both electronic and ionic conductive. In one embodiment, the membrane 103 conducts oxide ions and electrons. In one embodiment, electrodes 101, 102 and membrane 103 are tubular (see Figures 2A and 2B). In one embodiment, electrodes 101, 102 and membrane 103 are planar. In these embodiments, the electrochemical reaction at the electrodes occurs spontaneously without the need to apply potential / electricity to the reactor.

[0049] In one embodiment, the anode / first electrode 101 has a minimum amount of coke. In one embodiment, the flow 105 also contains hydrogen or carbon monoxide, or both. In one embodiment, the produced CO and / or H2 are separated from the cathode exhaust. In various embodiments, the separated CO and / or H2 are used to produce methanol, ethanol, hydrocarbons, plastic monomers, polyethylene, or a combination thereof.

[0050] Figure 2A illustrates a tubular electrochemical (EC) reactor or EC gas generator 200 according to one embodiment of the present disclosure (not to scale). The tubular generator 200 includes an inner tubular structure 202, an outer tubular structure 204, and membranes 206 positioned between the inner tubular structure 202 and the outer tubular structure 204, respectively. The tubular generator 200 further includes a void space 208 for fluid passage. Figure 2B illustrates a cross-sectional view of the tubular generator 200 according to one embodiment of the present disclosure (not to scale). The tubular generator 200 includes a first inner tubular structure 202, a second outer tubular structure 204, and membranes 206 between the inner tubular structure 202 and the outer tubular structure 204. The tubular generator 200 further includes a void space 208 for fluid passage.

[0051] In one embodiment, the electrodes and membrane are tubular, with the first electrode on the outermost side and the second electrode on the innermost side, and the second electrode is configured to receive H2O and / or CO2. In another embodiment, the electrodes and membrane are planar.

[0052] Electrochemical reactions occurring within a reactor include electrochemical half-cell reactions. In various embodiments, half-cell reactions occur at a three-phase boundary, which is the intersection of a pore and an electronically conductive phase and an ionically conductive phase. In various embodiments, the ionically conductive membrane conducts protons or oxide ions. In various embodiments, the membrane contains a solid oxide. In various embodiments, the membrane is impermeable to fluid flow.

[0053] Electrochemical production of H2 and / or CO The EC reactor discussed above is suitable for electrochemically producing CO from CO2 and H2 from H2O, either individually or simultaneously, on the cathode side. In one embodiment, the reactor comprises porous electrodes including a metallic phase and a ceramic phase, where the metallic phase is electronically conductive and the ceramic phase is ionically conductive. In various embodiments, no current collectors are attached to the electrodes. In various embodiments, the reactor does not contain current collectors or interconnects. Clearly, such a reactor is fundamentally different from an electrolytic device or any fuel cell.

[0054] As illustrated in Figure 3, a simultaneous production system (300) for CO and H2 is shown as an example. This system can also be used to produce CO and H2 separately. System 300 comprises an EC reactor 331, a fuel source 311, carbon dioxide and water sources 321, and a separator 341. 301 represents the anode in the reactor, 302 represents the cathode in the reactor, and 303 represents the membrane between the electrodes in the reactor. A first flow 392 containing fuel passes through the anode 301, is oxidized, and exits the anode as flow 393. A second flow 394 from the feed source 321 passes through the cathode 302, where CO2 is reduced to CO and H2O is reduced to H2. The exhaust flow 395 from the cathode passes through the separator 341, where CO is separated from CO2 and H2 is separated from H2O. The product flow 396 exits the separator 341 and consists essentially of CO and H2. A portion of flow 395 or flow 396 may be recirculated to the cathode 302 (not shown in Figure 3). In various embodiments, the cathode receives hydrogen or carbon monoxide in addition to vapor and carbon dioxide to ensure a true reducing environment throughout the reactor operation. In various embodiments, both electrodes are exposed to a reducing environment for the entire operating time.

[0055] The process and system for the simultaneous production of CO and H2 as disclosed herein offers several advantages. The production of CO from CO2 is desirable for reducing greenhouse gas emissions. Local (on-site) production of CO and H2 is inherently safer than transporting CO and H2 in pressurized vessels or vessels. The process of this disclosure utilizes an efficient electrochemical pathway but still requires no electricity. Separation of CO / CO2 and H2 / H2O from the cathode exhaust is easy and inexpensive. Thus, the method and system of this disclosure are cost-competitive in terms of both capital investment and operating costs.

[0056] In various embodiments, the H2 / CO co-production ratio is controlled by changing the H2O / CO2 input ratio, by changing the operating temperature, by changing the fuel composition, or by a combination thereof. Thus, the products from the separator are suitable for various downstream chemical productions without requiring further purification or modification. This is another major advantage of the processes and systems of this disclosure.

[0057] Production of beneficial products The production system 300 may further include chemical producers (not shown in Figure 3) selected from the group consisting of a Fischer-Tropsch reactor, a methanol producer, an ethanol producer, a hydrocarbon producer, a plastic monomer producer, and combinations thereof. The Fischer-Tropsch reactor can produce beneficial products such as naphtha, gasoline, diesel, and wax. The produced methanol can further be converted to gasoline, ethylene, acetic acid, formaldehyde, methyl acetate, polyolefins, dimethyl ether (DME), or combinations thereof. In various embodiments, the chemical producers are configured to receive carbon monoxide and hydrogen from a separator. Furthermore, the system may include polymerization units for converting plastic monomers into various types of plastics. Configurations and arrangements for utilizing the produced CO and H2 are known to those skilled in the art, and all such configurations and arrangements are within the scope of this disclosure.

[0058] A. A method for producing a Cu-Co-containing electrode precursor, comprising: a) preparing a mixed conductive film; b) depositing a dispersion containing CuO particles and CoCGO particles on the film; and c) sintering the CuO and CoCGO particles at a temperature of 800°C to 1350°C to form a Cu-Co-containing electrode precursor.

[0059] The method described in paragraph A, wherein the molar ratio of Cu to Co is 3:1 to 70:1.

[0060] The method according to paragraph A or B, wherein the molar ratio of C.Cu to Co is 10:1 to 50:1.

[0061] D. The method according to any one of paragraphs A to C, wherein the dispersion contains a pore-forming agent.

[0062] E. The method according to paragraph D, wherein the pore-forming agent comprises polymethyl methacrylate (PMMA), carbon black, graphite, carbon, cellulose, walnut shell, or a combination thereof.

[0063] F. The method according to any one of paragraphs A to E, wherein the dispersion comprises 2 to 20% by weight of a pore-forming agent.

[0064] G. The method according to any one of paragraphs A to F, wherein the film is supported on another electrode precursor.

[0065] H. The method according to any one of paragraphs A to G, wherein the other electrode precursor comprises NiO and a material selected from the group consisting of YSZ (yttria-stabilized zirconia), CGO (gadolinium-doped ceria), SDC (samaria-doped ceria), SSZ (scandia-stabilized zirconia), SCZ (scandia ceria-stabilized zirconia), LSGM (lanthanum strontium gallate magnesite), CoCGO, LST (lanthanum-doped strontium titanate), and combinations thereof.

[0066] I. The method according to any one of paragraphs A to G, wherein another electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ.

[0067] J. The method according to any one of paragraphs A to I, wherein the film comprises an electronically conductive phase and an ionically conductive phase, the electronically conductive phase comprising doped lanthanum chromite or LST, or an electronically conductive metal, or a combination thereof, and the ionically conductive phase comprising a material selected from the group consisting of gadolinium-doped ceria or samarium-doped ceria, yttria-stabilized zirconia (YSZ), lanthanum strontium gallate magnesite (LSGM), scandia-stabilized zirconia (SSZ), Sc and Ce-doped zirconia (SCZ), and combinations thereof.

[0068] K. The method according to any one of paragraphs A to J, wherein the membrane comprises CoCGO-stabilized zirconia or LST-stabilized zirconia.

[0069] The method according to any one of paragraphs A to K, wherein L. stabilized zirconia comprises YSZ, SSZ, or SCZ (scandiaceria stabilized zirconia), and LST comprises LaSrCaTiO3.

[0070] M. The method according to any one of paragraphs A to L, wherein the film comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

[0071] N. The method according to any one of paragraphs A to M, wherein sintering is performed at a temperature of 1100°C to 1250°C.

[0072] An electrochemical cell comprising a first electrode precursor having O.CuO and CoCGO, wherein the molar ratio of Cu to Co is 3:1 to 70:1, a second electrode precursor, and a mixed conductive film between the two electrode precursors.

[0073] P. The cell according to paragraph O, wherein the second electrode precursor comprises NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof.

[0074] Q. The cell described in paragraph O or P, wherein the second electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ.

[0075] A cell described in any one of paragraphs O to Q, where the molar ratio of R.Cu to Co is 10:1 to 50:1.

[0076] S. A cell according to any one of paragraphs O to R, wherein the membrane contains CoCGO-stabilized zirconia or LST-stabilized zirconia.

[0077] T. A cell according to any one of paragraphs O to S, wherein the membrane contains nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

[0078] It should be understood that this disclosure describes exemplary embodiments for implementing different features, structures, or functions of the present invention. For the sake of brevity of this disclosure, exemplary embodiments of components, arrangements, and configurations are described; however, these exemplary embodiments are provided merely as examples and are not intended to limit the scope of the present invention. Unless otherwise specified, the embodiments presented herein may be combined. Such combinations do not deviate from the scope of the disclosure.

[0079] Additionally, specific terminology is used throughout the description and claims to refer to certain components or steps. As those skilled in the art will understand, various entities may refer to the same components or process steps by different names, and therefore the naming conventions of the elements described herein are not intended to limit the scope of the invention. Furthermore, the terminology and naming conventions used herein are not intended to distinguish components, functions, and / or steps that have different names but do not function differently.

[0080] While this disclosure can be modified and replaced in various ways, specific embodiments are shown as examples in the drawings and description. However, it should be understood that the drawings and detailed description are not intended to limit this disclosure to any particular form disclosed, but rather to cover all modifications, equivalents, and replacements that fall within the spirit and scope of this disclosure.

Claims

1. A method for producing a Cu-Co-containing electrode precursor, a) Prepare a mixed conductive film, b) Depositing a dispersion containing CuO particles and CoCGO particles on the film, c) Sintering the CuO and CoCGO particles at a temperature of 800°C to 1350°C to form the Cu-Co-containing electrode precursor, Methods that include...

2. The method according to claim 1, wherein the molar ratio of Cu to Co is 3:1 to 70:

1.

3. The method according to claim 1, wherein the molar ratio of Cu to Co is 10:1 to 50:

1.

4. The method according to claim 1, wherein the dispersion contains a pore-forming agent.

5. The method according to claim 4, wherein the pore-forming agent comprises polymethyl methacrylate (PMMA), carbon black, graphite, carbon, cellulose, walnut shell, or a combination thereof.

6. The method according to claim 1, wherein the dispersion comprises 2 to 20% by weight of a pore-forming agent.

7. The method according to claim 1, wherein the film is supported on another electrode precursor.

8. The method according to claim 7, wherein the other electrode precursor comprises NiO and a material selected from the group consisting of YSZ (yttria-stabilized zirconia), CGO (gadolinium-doped ceria), SDC (samaria-doped ceria), SSZ (scandia-stabilized zirconia), SCZ (scandia ceria-stabilized zirconia), LSGM (lanthanum strontium gallate magnesite), CoCGO, LST (lanthanum-doped strontium titanate), and combinations thereof.

9. The method according to claim 7, wherein the other electrode precursor comprises NiO-YSZ or NiO-CGO or LaSrFeCr-SSZ or LaSrFeCr-SCZ or LST (lanthanum-doped trontium titanate)-SCZ.

10. The method according to claim 1, wherein the film comprises an electronically conductive phase and an ionically conductive phase, the electronically conductive phase comprises doped lanthanum chromite, or LST, or an electronically conductive metal, or a combination thereof, and the ionically conductive phase comprises a material selected from the group consisting of gadolinium or samarium-doped ceria, yttria-stabilized zirconia (YSZ), lanthanum strontium gallate magnesite (LSGM), scandia-stabilized zirconia (SSZ), Sc and Ce-doped zirconia (SCZ), and combinations thereof.

11. The method according to claim 1, wherein the film comprises CoCGO-stabilized zirconia or LST-stabilized zirconia.

12. The method according to claim 11, wherein the stabilized zirconia comprises YSZ, SSZ, or SCZ (scandiacelia-stabilized zirconia), and the LST comprises LaSrCaTiO3.

13. The method according to claim 1, wherein the film comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.

14. The method according to claim 1, wherein sintering is carried out at a temperature of 1100°C to 1250°C.

15. An electrochemical cell comprising a first electrode precursor having CuO and CoCGO, wherein the molar ratio of Cu to Co is 3:1 to 70:1, a second electrode precursor, and a mixed conductive film between the two electrode precursors.

16. The cell according to claim 15, wherein the second electrode precursor comprises NiO and a material selected from the group consisting of YSZ, CGO, SDC, SSZ, SCZ, LSGM, CoCGO, LST, and combinations thereof.

17. The cell according to claim 15, wherein the second electrode precursor comprises NiO-YSZ, NiO-CGO, LaSrFeCr-SSZ, LaSrFeCr-SCZ, or LST (lanthanum-doped trontium titanate)-SCZ.

18. The cell according to claim 15, wherein the molar ratio of Cu to Co is 10:1 to 50:

1.

19. The cell according to claim 15, wherein the membrane comprises CoCGO-stabilized zirconia or LST-stabilized zirconia.

20. The cell according to claim 15, wherein the film comprises nickel-doped zirconia, copper-doped zirconia, cobalt-doped zirconia, lanthanum-doped zirconia, strontium-doped zirconia, titanium-doped zirconia, or niobium-doped zirconia.