Test probe and method for manufacturing the same
By employing reusable glass or conductive substrates in the MEMS process, the method addresses high manufacturing costs and ensures stable contact with hemispherical bump terminals, enhancing the reliability and cost-effectiveness of inspection probes.
Patent Information
- Application Number
- JP2026523980
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-10-27
- Filing Date
- 2024-10-23
- Publication Date
- 2026-11-24
AI Technical Summary
Conventional MEMS manufacturing processes for inspection probes incur high costs due to the use of expensive sacrificial substrates, and there is a need for a more stable and cost-effective method to inspect electrical characteristics of semiconductor objects.
A method involving the use of reusable glass or conductive substrates, combined with a MEMS process, to manufacture inspection probes with multiple tip portions that ensure stable contact with hemispherical bump terminals, reducing the need for expensive sacrificial substrates and lowering manufacturing costs.
The method reduces manufacturing costs by utilizing glass or conductive substrates, enabling stable and reliable inspection of semiconductor objects through multiple tip portions that securely engage with hemispherical bump terminals.
Smart Images

Figure 2026539278000001_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an inspection probe for inspecting electrical characteristics of an object to be inspected such as a semiconductor, and a method for manufacturing the inspection probe using a MEMS (Micro Electro-Mechanical System) process.
Background Art
[0002] The inspection probe includes a cylindrical barrel, a terminal partially inserted into one end of the barrel, a plunger partially inserted into the other end of the barrel, and a spring interposed between the terminal and the plunger inside the barrel. At least one of the terminal and the plunger is partially inserted so as to be slidable within the barrel. The terminal contacts a hemispherical bump terminal of the object to be inspected, and the plunger contacts a pad terminal of an inspection circuit board. The terminal includes a contact portion having a sharp tip for contacting the hemispherical bump terminal, and a body portion partially inserted into one end of the barrel. Such a terminal may be manufactured by machining or may be manufactured by a MEMS process.
[0003] In the MEMS manufacturing process of the terminal, a groove corresponding to the shape of a sharp tip, for example, a V-shaped groove, is filled with a hard metal and planarized on a sacrificial substrate to form a contact portion. A body portion is formed by repeating lamination of a dry film, exposure and development of a pattern, and filling of a metal material on the sacrificial substrate. Finally, the dry film and the sacrificial substrate are removed to complete the terminal. At this time, the sacrificial substrate to be finally removed is used as a base substrate for the MEMS lamination process to form a conical tip that is not constant in the lamination direction. Such a conventional MEMS manufacturing process for a terminal has a problem in that the manufacturing cost increases because an expensive sacrificial substrate is finally removed.
Summary of the Invention
Problems to be Solved by the Invention
[0004] An object of the present invention is to provide an inspection probe capable of stably inspecting an object to be inspected.
[0005] Another object of the present invention is to provide a method for manufacturing an inspection probe that can reduce manufacturing costs. [Means for solving the problem]
[0006] A method for manufacturing an inspection probe is provided to achieve the above-mentioned objectives. The method for manufacturing an inspection probe includes the steps of: laminating a first dry film on a substrate and filling a predetermined material into the molding groove of the lower dry film to form a terminal body portion; laminating an upper dry film on the upper surface of the lower dry film and filling a predetermined material into the molding groove of the upper dry film above the terminal body portion to form a chip portion; processing the upper part of the chip portion to form at least one chip; and removing the upper dry film and the lower dry film from the chip portion and the terminal body portion on which the chip is formed.
[0007] The substrate may include an insulating substrate or a conductive substrate coated with a conductive film. This allows for the use of reusable glass substrates or conductive substrates in the MEMS process, thereby reducing manufacturing costs, without the need for expensive sacrificial substrates as consumables.
[0008] The step of forming the tip portion may include filling a predetermined material into a plurality of molding grooves in the upper dry film, which are provided spaced apart along the circumferential direction on the upper part of the terminal body portion, to form a plurality of tip portions. This allows the plurality of tip portions to make stable contact with the hemispherical type bump terminal (relative terminal) of the object under inspection, thereby improving the reliability of the inspection.
[0009] The step of forming at least one chip may include forming a plurality of chips on the upper part of each chip portion, each chip being provided at the same distance from the center of the sphere, such that the plurality of chip portions contact a portion of the spherical surface of the relative terminal while accommodating it. This makes it possible to form a plurality of chips suitable for contacting a hemispherical type bump terminal of an object under test in a simple and low-cost manner during terminal manufacturing by MEMS process.
[0010] The plurality of chip portions are columnar in shape, extending in the stacking direction and each having opposing side edges. The step of forming the plurality of chips may include the step of forming a recess on the upper surface of each chip portion that extends toward the side edge with a predetermined width and depth. This makes it possible to form a plurality of chips suitable for contacting hemispherical type bump terminals of an object to be inspected using a simpler and lower-cost processing method. [Effects of the Invention]
[0011] The method for manufacturing an inspection probe according to an embodiment of the present invention can reduce manufacturing costs by using a glass substrate or a conductive substrate instead of a sacrificial substrate. [Brief explanation of the drawing]
[0012] [Figure 1] This is a perspective view showing an inspection probe according to the first embodiment of the present invention.
[0013] [Figure 2] Figure 1 is an exploded perspective view showing the inspection probe in disassembled form.
[0014] [Figure 3] This is a cross-sectional view taken along line AA in Figure 1.
[0015] [Figure 4] This diagram shows the contact state between the bump terminals of the object under inspection and the chip.
[0016] [Figure 5] It is a flowchart showing a method of manufacturing the terminal of FIG. 1.
[0017] [Figure 6] It is a figure which shows typically the method of manufacturing the terminal of FIG. 5.
[0018] [Figure 7] It is a figure which shows typically the method of manufacturing the terminal of FIG. 5.
[0019] [Figure 8] It is a flowchart which shows the method of manufacturing the terminal which concerns on 2nd Example of this invention.
[0020] [Figure 9] It is a figure which shows typically the method of manufacturing the terminal of FIG. 8.
[0021] [Figure 10] It is a figure which shows typically the method of manufacturing the terminal of FIG. 8. MODES FOR CARRYING OUT THE INVENTION
[0022] Hereinafter, the inspection probe 1 and its manufacturing method will be described in detail with reference to the accompanying drawings.
[0023] FIG. 1 is a perspective view showing the inspection probe 1, FIG. 2 is an exploded perspective view showing the inspection probe 1 of FIG. 1 in an exploded manner, and FIG. 3 is taken along line AA of FIG. 4 is a cross-sectional view, and FIG. 4 is a diagram showing a contact state between the bump terminal 110 of the device under test 100 and the chip 32c.
[0024] Referring to Figures 1 to 3, the inspection probe 1 includes a cylindrical barrel 2, a terminal 3 partially inserted into one end of the barrel 2, a plunger 4 partially inserted into the other end of the barrel 2, and a spring 5 provided between the terminal 3 and the plunger 4 within the barrel 2. The terminal 3 is fixed to one end of the barrel 2, and the plunger 4 can slide within the barrel 2 while compressing and releasing the spring 5.
[0025] Barrel 2 is tubular and may be made of a conductive metal, such as brass.
[0026] Terminal 3 includes a terminal body portion 31 that is partially inserted into one end of barrel 2, and three tip portions 32 that are stacked on the terminal body portion 31 and contact the relative terminal (hereinafter referred to as "bump terminal 110 of the object under inspection 100"). The number of tip portions 32 is not limited to three, but may be two or four or more.
[0027] The terminal body portion 31 includes a barrel insertion portion 31a having a diameter corresponding to the inner diameter of the barrel 2, a spring support portion 31b that is housed and supported on one side of a spring 5 provided at the inner end of the barrel 2 of the barrel insertion portion, a barrel support portion 31c for fixing the terminal body portion 31 to the barrel 2, and a tip support portion 31d that faces the end of the barrel 2 on the outside of the barrel 2 and supports three tip portions 32 on its back surface.
[0028] The barrel insertion portion 31a is cylindrical, contacts the inner surface of the barrel 2, and has a diameter corresponding to the inner diameter of the barrel 2.
[0029] The spring support portion 31b is cylindrical, has a diameter smaller than the inner diameter of the barrel 2, and contacts one side of the spring 5.
[0030] The barrel support portion 31c is recessed along the circumferential direction on the outer surface of the barrel insertion portion 31a so as to accommodate the projections created by pressurizing and deforming the barrel 2 inward through dimples.
[0031] The tip support portion 31d is cylindrical and has a diameter equal to or smaller than the outer diameter of the barrel 2 and larger than the inner diameter. For example, three tip portions 32 are stacked on the upper surface of the tip support portion 31d.
[0032] The three tip portions 32 are arranged at predetermined intervals in the circumferential direction with respect to the central axis O of the barrel 2. The three tip portions 32 have a fan-shaped cross-section along the axial direction. Each of the three tip portions 32 includes a tip step portion 32a provided at a predetermined depth on the side edge facing the central axis O at the top, and a recessed portion 32b extending radially toward the central axis O with a predetermined width. Each of the three tip portions 32 includes a lower tip portion 321 having a fan-shaped cross-section along the axial direction on the tip support portion 31d, and two upper tip portions 322 divided into two by the recessed portion 32b on the lower tip portion 321, each having a fan-shaped cross-section along the axial direction. One lower tip portion 321 may have one lower tip 32c formed on the side edge facing the central axis O, and the two upper tip portions 322 may have two upper tips 32c formed on the side edges facing the central axis O. As a result, the lower chip 32c and the upper chip portion 32c are separated in the stacking direction and can be positioned at different distances from the central axis O.
[0033] Referring to Figure 4, the hemispherical bump terminal 110 is essentially pressed against the inspection probe 1 while positioned between the three tip portions 32 during inspection. The three lower tips 32c located on the upper part of the lower tip portion 321 and the six upper tip portions 32c located on the upper part of the upper tip portion 322 each make contact with the hemispherical bump terminal 110 at the same distance from the central axis O, while accommodating a portion of its spherical surface. As a result, the nine tips 32c located on each of the three tip portions 32 bite into the bump terminal 110, ensuring stable contact.
[0034] Figure 5 is a flowchart showing the method for manufacturing terminal 3 in Figure 1, and Figures 6 and 7 are schematic diagrams showing the method for manufacturing terminal 3 in Figure 5. In Figures 6 and 7, multiple terminals 3 are manufactured simultaneously on a single glass substrate 61 by the MEMS process, but for the sake of explanation, only one terminal 3 is shown.
[0035] In step S1, a flat insulating substrate of a predetermined thickness, such as a glass substrate 61, is prepared. The insulating substrate may be replaced with a conductive substrate.
[0036] In step S2, a conductive film 62, such as a gold (Au) film, is formed on one surface of the glass substrate 61 by sputtering. If a conductive substrate is used, step S2 may be omitted.
[0037] In step S3, a first dry film 63 is laminated on the conductive film 62 of the glass substrate 61, and a plurality of first molded grooves 64 separated from each other are formed by exposure and development of the pattern, and a first metal, such as nickel (Ni), is filled into the plurality of first molded grooves 64 by electroplating or electroless plating, and the portion protruding from the upper surface of the first dry film 63 is polished to form the first layer 65 (corresponding to the spring support portion 31b in Figure 2). In the electroplating method, an electric current is passed between a positive electrode plate made of nickel (Ni) and the conductive film 62 (negative electrode) on the glass substrate 61 in an aqueous solution, so that the nickel (Ni) dissolves and is deposited on the plated film 62. In the electroless plating method, metal ions in the plating solution are deposited as metal on the conductive film 62 of the glass substrate 61 by a chemical reaction of a reducing agent.
[0038] In step S4, a second dry film 66 is laminated on the first dry film 63, and multiple second molding grooves 67 wider than the first molding groove 64 are formed by exposure and development of the pattern, a first metal, such as nickel (Ni), is filled into the multiple second molding grooves 67 by electroplating, and the portion protruding from the upper surface of the second dry film 66 is polished to form a second layer 68 (corresponding to a part of the barrel insertion portion 31a in Figure 2).
[0039] In step S5, a third dry film 69 is laminated on the second dry film 66, and multiple third molding grooves 70 with a width narrower than the second molding groove 67 are formed by exposure and development of the pattern, a first metal, such as nickel (Ni), is filled into the multiple third molding grooves 70 by electroplating, and the portion protruding from the upper surface of the third dry film 69 is polished to form a third layer 71 (corresponding to the barrel support portion 31c in Figure 2).
[0040] In step S6, a fourth dry film 72 is laminated on the third dry film 69, and multiple fourth molding grooves 73 wider than the third molding groove 70 are formed by exposure and development of the pattern, a first metal, such as nickel (Ni), is filled into the multiple fourth molding grooves 73 by electroplating, and the portion protruding from the upper surface of the fourth dry film 72 is polished to form a fourth layer 74 (corresponding to a part of the barrel insertion portion 31a in Figure 2).
[0041] In step S7, a fifth dry film 75 is laminated on the fourth dry film 72, and multiple fifth molding grooves 76 wider than the fourth molding groove 73 are formed by exposure and development of the pattern, a first metal, such as nickel (Ni), is filled into the multiple fifth molding grooves 76 by electroplating, and the portion protruding from the upper surface of the fifth dry film 75 is polished to form the fifth layer 77 (corresponding to the chip support portion 31d in Figure 2).
[0042] The first to fifth layers 65, 68, 71, 74, and 77, which are stacked by the process described above, form the terminal body portion 31.
[0043] In step S8, a sixth dry film 78 is laminated on a fifth dry film 75, and a plurality of sixth molding grooves 79 are formed on the upper part of the fifth layer 77 by exposure and development of the pattern, spaced apart along the circumferential direction with respect to the central axis of the lamination direction. A second metal with a higher hardness than the first metal, such as nickel boron (NiB), is filled into the plurality of sixth molding grooves 79 by electroplating, and the portion protruding from the upper surface of the sixth dry film 78 is polished to form the sixth layer 80 (corresponding to the tip portion 32 in Figure 2). The sixth molding grooves 79 and the sixth layer 80 each have a fan-shaped cross-section in the lateral direction of the lamination direction.
[0044] In step S9, a recessed portion 12b of a predetermined width and depth is formed on the upper surface of the sixth layer 80 (corresponding to the chip portion 32 in Figure 2) exposed on the upper surface of the sixth dry film 78, extending laterally in the lamination direction toward the center of the circumference O, for example, using a drill. As a result, two smaller, fan-shaped upper chip portions 322 are formed on the upper part of the sixth layer 80 (chip portion 32 in Figure 1), divided into two by the recessed portion 12b. At this time, the one chip 32c provided on the lower chip portion 321 and the two chips 32c provided on the two upper chip portions 322 are separated in the lamination direction and located at different distances from the central axis O. On the other hand, the three lower chips 32c provided on the upper part of the lower chip portion 321 and the six upper chip portions 32c provided on the upper part of the upper chip portion 322 are each located at the same distance from the central axis O.
[0045] In stage S10, remove the first to sixth dry films 63, 66, 69, 72, 75, and 78 to complete terminal 3.
[0046] Figure 8 is a flowchart showing a method for manufacturing terminal 3 according to a second embodiment of the present invention, and Figures 9 and 10 are schematic diagrams showing the method for manufacturing terminal 3 in Figure 8. In Figure 8, steps S11 to S17 are the same as steps S1 to S7 in Figure 5, and their explanation is omitted.
[0047] In step S18, a sixth dry film 78 is laminated on a fifth dry film 75, and a plurality of sixth molding grooves 79 are formed on the upper part of the fifth layer 77, spaced apart along the circumferential direction with respect to the central axis of the lamination direction by exposure and development of the pattern, and a second metal having a higher hardness than the first metal, such as nickel boron (NiB), is filled into the plurality of sixth molding grooves 79 by electroplating, and the portion protruding from the upper surface of the sixth dry film 78 is polished to form the sixth layer 80 (corresponding to the lower tip portion 321 in Figure 2). The sixth molding grooves 79 and the sixth layer 80 each have a fan-shaped cross section in the lateral direction of the lamination direction.
[0048] In step S19, the seventh dry film 81 is laminated on the sixth dry film 78, and a plurality of seventh molding grooves 82 are formed on the upper part of the sixth layer 80 by exposure and development of the pattern, spaced apart along the circumferential direction with respect to the central axis of the lamination direction, and the plurality of seventh molding grooves 82 are filled with a second metal, such as nickel boron (NiB), by electroplating, and the portion protruding from the upper surface of the seventh dry film 81 is polished to form the seventh layer 83 (corresponding to the upper tip portion 322 in Figure 2). The seventh molding grooves 82 and the seventh layer 83 each have a fan-shaped cross section that is divided into two in the circumferential direction on the sixth molding groove 79 and the sixth layer 80. Thus, a lower chip 32c may be formed on the upper end of the side edge of the sixth layer 80 (321) facing the central axis O in the stacking direction, with contact for the bump terminal 110 of the object under inspection 100, and an upper chip 32c may be formed on the upper end of the side edge of the seventh layer 83 (322) facing the central axis O in the stacking direction, with contact for the bump terminal 110 of the object under inspection 100.
[0049] In stage S20, remove the first to seventh dry films 63, 66, 69, 72, 75, 78, and 81 to complete terminal 3.
[0050] Although preferred embodiments of the present invention have been illustrated and described above, the present invention is not limited to the specific embodiments described above, and it goes without saying that various modifications can be made by a person with ordinary skill in the art to which the invention belongs, without departing from the gist of the invention as claimed in the claims, and such modified embodiments should not be understood separately from the technical idea and prospects of the present invention.
Claims
1. A method for manufacturing a test probe, The steps include: laminating a lower dry film onto a substrate and filling a predetermined material into the molding groove of the lower dry film to form a terminal body; The steps include: laminating an upper dry film onto the upper surface of the lower dry film, and filling a predetermined material above the terminal body portion in the molding groove of the upper dry film to form a chip portion; The steps include: processing the upper part of the aforementioned chip portion to form at least one chip; A method comprising the step of removing the upper dry film and the lower dry film from the chip portion and the terminal body portion on which the chip is formed.
2. The method according to claim 1, wherein the substrate includes an insulating substrate or a conductive substrate coated with a conductive film.
3. The method according to claim 1, wherein the step of forming the chip portion includes filling a predetermined material into a plurality of molding grooves of the upper dry film provided on the upper part of the terminal body portion at intervals along the circumferential direction to form a plurality of chip portions.
4. The step of forming the aforementioned at least one chip is: The method according to claim 3, further comprising the step of forming a plurality of chips on the upper part of each chip portion, each chip being at the same distance from the center of the spherical surface, such that the plurality of chip portions contact each other while accommodating a portion of the spherical surface of the relative terminal.
5. The aforementioned multiple chip portions are columnar in shape, extending in the stacking direction and each having opposing side edges. The step of forming the aforementioned plurality of chips is, The method according to claim 4, further comprising the step of forming a recessed portion on the upper surface of each of the tip portions, having a predetermined width and depth and extending toward the side edge.