Mechanochemical activation of mineral materials

Large-scale grinding mills with specific energy and residence time parameters optimize mechanochemical activation of clay, addressing inefficiencies and environmental issues in existing methods, producing effective cement additives.

JP2026539311APending Publication Date: 2026-11-24THYSSENKRUPP POLYSIUS GMBH +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2026525612
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-11-29
Filing Date
2024-10-02
Publication Date
2026-11-24

AI Technical Summary

Technical Problem

Existing mechanochemical activation methods for clay in the cement industry are inefficient and energy-intensive, leading to undesirable material changes and environmental emissions, and there is a lack of optimization in energy conversion during grinding.

Method used

The use of a large-scale grinding mill with a minimum internal volume of 1 m³, an energy density of at least 200 kW/m³, and a residence time of at least 5 minutes for mechanochemical activation, optimizing energy input to enhance activation efficiency.

Benefits of technology

Achieves efficient mechanochemical activation with reduced energy consumption and minimized environmental impact, producing activated clay suitable for cement additives.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026539311000001_ABST
    Figure 2026539311000001_ABST
Patent Text Reader

Abstract

The present invention relates, for example, to the selection of grinding mill sizes for economically reasonable mechanochemical activation of clay in the cement industry.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates, for example, to the selection of grinding mill sizes for economically reasonable mechanochemical activation of clay in the cement industry.

[0002] Activated clay is established as an additive, particularly in the cement industry. The current method involves drying and calcining the clay, i.e., thermal activation. On the one hand, this requires energy for heating, and on the other hand, the high temperatures can potentially cause further undesirable material changes. Furthermore, the thermal process requires flue gas scrubbing to remove the resulting nitrogen oxide and sulfur oxide emissions. In addition, in the future, the thermal process will require the use of processes for capturing and, if necessary, purifying the generated or released carbon dioxide.

[0003] Therefore, mechanochemical activation through powerful grinding is increasingly being discussed.

[0004] The publicly released DE102023106210 discloses a method for grinding and pozzolane activation in a stirred ball mill.

[0005] The published DE102023106217 discloses a method for grinding and pozzolanic activation in two separate stages of a stirred ball mill.

[0006] The publicly released DE102023106221 discloses a combination of mechanochemical and thermal activation in at least one stirred ball mill.

[0007] The publicly released DE102023106222 discloses color optimization in the mechanochemical activation of clay.

[0008] The publicly released DE102023123525 discloses cement additives manufactured from recycled concrete.

[0009] Because clay is a complex system (especially compared to limestone firing), different activation methods result in different products (activated clays) with different properties. Similarly, the diversity of clays that can be used means that not all methods can be used for all clays.

[0010] Mechanochemical activation differs fundamentally from thermal activation in terms of understanding the processes involved. While thermal activation is primarily determined by temperature and time, mechanochemical activation in grinding mills is far more complex and has been found to depend on significantly more parameters. Furthermore, a large portion of the input grinding energy is converted into heat, which means there is a clear opportunity for optimization here.

[0011] CN106345576A discloses a wet mill for the industrial processing of concrete additives.

[0012] AU2019338944A1 discloses a vertical ball mill.

[0013] The objective of the present invention is to optimize the mechanochemical activation in a grinding mill so as to maximize the activation (reactivity of the product) per unit of energy expended in the grinding mill.

[0014] This objective is achieved by the use of an apparatus for mechanochemical activation having the features specified in claim 1, a grinding mill having the features specified in claim 7, and a method having the features specified in claim 10. Advantageous further developments arise from the dependent claims, the following description, and the drawings.

[0015] The apparatus according to the present invention is suitable for mechanochemical activation. For example, not only clay, but also recycled concrete or other materials can be activated not only thermally but also mechanochemically, and then exhibit suitable setting behavior and other properties for use, for example, as a clinker substitute or additive. Such apparatuses are known, for example, from DE102023106210, DE102023106217, DE102023106221, DE102023106222, or DE102023123525. This apparatus has a grinding mill. This grinding mill is operated for mechanochemical activation to which a grinding energy significantly greater than the energy required for grinding is introduced, and to a extent in which size growth can be observed again during grinding.

[0016] In material grinding, three stages are observed depending on the energy input. In the first stage, particle size decreases (almost linearly) with increasing energy input (Rittinger zone). Simply put, as grinding progresses, the product becomes finer. However, there is a limit to the particle size that is difficult to overcome. From this point, a second stage arises where further energy input cannot change the particle size further (aggregation zone). For economic reasons, the transition from the first to the second stage is avoided during grinding because there is no additional grinding effect for the additional effort. If the energy supply is further increased, a third stage can be reached, where an increase in particle size can be observed again (aggregation zone). Therefore, it is far more important to avoid this region during grinding because better results can be achieved with less effort in terms of particle size distribution.

[0017] However, at high energy inputs, i.e., in the third stage, a change occurs in the material itself, which has been found to result in activation, i.e., reactivity that enables its use as a binder (and therefore as a clinker substitute), similar to thermal activation in the case of clay, for example. Thus, this third stage is a mechanochemical activation and is different from the grinding that takes place in the first stage. Therefore, according to the prior art, grinding is not a mechanochemical activation.

[0018] Surprisingly, it can provide a sufficiently high energy input, making it suitable for mechanochemical activation, and at least 1 m 3 It has been found that grinding mills with an internal volume of 1 m³ can be used for activation in a particularly efficient, and therefore particularly economical, manner. The difference in efficiency is that grinding mills with an internal volume of less than 100 liters are completely inefficient, but 1 m³ 3 Grinding mills with internal volumes exceeding a certain size exhibit economically reasonable efficiency. Surprisingly, trials on a pilot scale have shown that the ratio between activation achieved and energy input is highly dependent on the size of the machine, from which the minimum machine size for economically reasonable operation can be derived. This means that a relatively large grinding mill must be selected regardless of the required throughput. While large grinding mills are known to those skilled in the art, they are typically only suitable for simple grinding and therefore cannot be used for mechanochemical activation.

[0019] In a further embodiment of the present invention, the grinding mill is a stirring ball mill.

[0020] In a further embodiment of the present invention, the grinding mill has a minimum power output of 200 kW / m 3 It has an energy density of .

[0021] In a further embodiment of the present invention, the grinding mill has a length of at least 2 m, preferably at least 2.5 m.

[0022] In a further embodiment of the present invention, the grinding mill has a cross-sectional area perpendicular to the longitudinal axis of at least 0.71 m 2 , preferably at least 0.75 m 2 .

[0023] In a further embodiment of the present invention, the grinding mill has a length-to-diameter ratio of at least 3, preferably at least 3.5.

[0024] In a further aspect, the present invention relates to the use of a grinding mill having an internal volume of at least 1 m 3 for mechanochemical activation.

[0025] In a further embodiment of the present invention, the grinding mill used is an agitated ball mill.

[0026] In a further embodiment of the present invention, the grinding mill used has an energy density of at least 200 kW / m 3 .

[0027] In a further aspect, the present invention relates to a method for the mechanochemical activation of clay, for example for use in the cement industry. A grinding mill having an internal volume of at least 1 m 3 is selected for the mechanochemical activation.

[0028] In a further embodiment of the present invention, an agitated ball mill is selected as the grinding mill.

[0029] In a further embodiment of the present invention, the grinding mill is operated at an energy density of at least 200 kW / m 3 .

[0030] In a further embodiment of the present invention, the grinding mill is operated such that the residence time of the ground material in the grinding mill is at least 5 minutes, preferably at least 10 minutes, particularly preferably at least 20 minutes.

[0031] In further embodiments of the present invention, phyllosilicates are activated. Phylosilicates have been shown to be particularly suitable, and the beneficial effect of large grinding mills is even more pronounced with them. Clay minerals in a 1:1 ratio, especially kaolin, and clay minerals in a 2:1 ratio, especially muscovite and illite, have been shown to be particularly suitable.

[0032] The relationship between the size of the internal space and the activation efficiency is shown below. [Brief explanation of the drawing]

[0033] [Figure 1] These are measurement data from two exemplary mills. [Figure 2] This is the dependence of the specific energy input on the internal volume.

[0034] Figure 1 shows two exemplary grinding mills that differ only in the size of their internal spaces. The internal space of B is 10 times larger than that of A. The energy input in kWh / t is plotted on the x-axis, and the degree of activation achieved is plotted on the y-axis, where 100% represents the maximum achievable activation.

[0035] The curves for grinding mill A and grinding mill B run parallel, but it is clear that in larger grinding mills, significantly higher activation is achieved with the same energy input, or in other words, the same activation is achieved with significantly lower energy input per ton of product.

[0036] In Figure 2, the internal volume of the grinding mill in liters (l) is plotted against the introduced energy density in kW / l. It is clear that 1000l or 1m³ 3 The energy density below a certain mill volume is significantly dependent on volume, and the slope of the determined curve is strongly negative. Only for volumes of 1000 liters or more, the curve becomes significantly flatter. From this point, economic efficiency is achieved.

Claims

1. An apparatus for mechanochemical activation, comprising a grinding mill, wherein the grinding mill is at least 1 m 3 A device characterized by having an internal volume.

2. The apparatus according to claim 1, characterized in that the grinding mill is a stirring ball mill.

3. The aforementioned grinding mill has a power output of at least 200 kW / m². 3 The apparatus according to claim 1 or 2, characterized in having an energy density of the specified value.

4. The apparatus according to any one of claims 1 to 3, characterized in that the grinding mill has a length of at least 2 m, preferably at least 2.5 m.

5. The aforementioned grinding mill has a minimum of 0.71 m 2 Preferably at least 0.75 m 2 The apparatus according to any one of claims 1 to 4, characterized in that it has a cross-sectional area perpendicular to the longitudinal axis.

6. The apparatus according to any one of claims 1 to 5, characterized in that the grinding mill has a length-to-diameter ratio of at least 3, preferably at least 3.

5.

7. For mechanochemical activation, at least 1 m 3 Use of a grinding mill with an internal volume.

8. The use according to claim 7, characterized in that the grinding mill is a stirring ball mill.

9. The aforementioned grinding mill has a power output of at least 200 kW / m². 3 The use according to claim 7 or 8, characterized by having an energy density of the above.

10. A method for mechanochemical activation, wherein at least 1 m 3 A grinding mill having an internal volume is selected for mechanochemical activation.

11. The method according to claim 10, characterized in that a stirring ball mill is selected as the grinding mill.

12. The aforementioned grinding mill has a power output of at least 200 kW / m². 3 The method according to claim 10 or 11, characterized in that it is operated at an energy density of .

13. The method according to any one of claims 10 to 12, characterized in that the residence time of the pulverized material in the pulverizing mill is at least 5 minutes, preferably at least 10 minutes, and particularly preferably at least 20 minutes.

14. The method according to any one of claims 10 to 13, characterized in that a phyllosilicate is activated.