In-situ metal liner for improved high aspect ratio etching with warp control
The method of partial etching and sidewall passivation with metal deposition addresses the challenges of etching high aspect ratio features in semiconductor devices, improving selectivity, reducing twisting and bowing, and maintaining efficient etch rates.
Patent Information
- Application Number
- JP2026525672
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-10-31
- Filing Date
- 2024-10-15
- Publication Date
- 2026-11-24
AI Technical Summary
The etching of high aspect ratio features in semiconductor devices, such as those found in DRAM and NAND applications, faces challenges including insufficient mask selectivity, twisting of features, non-circularity, aspect ratio-dependent etching rate, bowing, and low etch rate, which are difficult to balance in conventional processes.
A method involving partial etching of a stack beneath a patterned mask, followed by metal passivation on sidewalls using atomic layer deposition and plasma-enhanced chemical vapor deposition, and further etching with controlled RF power and gas plasma to form concave features with reduced bowing and improved etch rate.
The method achieves high stack-to-mask selectivity, reduces feature twisting and bowing, maintains reasonable etch rates, and enhances etching uniformity, addressing the trade-offs of conventional etching processes.
Smart Images

Figure 2026539317000001_ABST
Abstract
Description
[Technical Field]
[0001] Cross-Reference to Related Applications This application claims the benefit of priority from U.S. Patent Application No. 63 / 594,757, filed October 31, 2023, which is incorporated herein by reference for all purposes. [Background Art]
[0002] One process that is frequently used during the fabrication of semiconductor devices is forming recessed features in a stack beneath a carbon-containing mask. The stack may be alternating / repeating layers of material in which the recessed features are formed, or a thick film of a single layer. One example of a circumstance where such processes may occur is for memory applications, such as dynamic random access memory (DRAM) and "not and" devices (NAND). In some semiconductor device fabrications, metal or other materials may be etched beneath the carbon-containing mask. As the semiconductor industry advances and device dimensions get smaller, such recessed features become increasingly difficult to uniformly etch, especially for high aspect ratio features with narrow widths and / or deep depths.
[0003] The background description provided herein is to generally present the context of the present disclosure. To the extent it is described in this background section, the work of the present inventors is not explicitly or implicitly admitted as prior art to the present disclosure, including aspects of the description that may not be otherwise admitted as prior art at the time of filing. [Summary of Invention]
[0004] To achieve the above, a method is provided for etching a concave feature in a stack beneath a patterned mask forming a mask feature, in accordance with the purposes of this disclosure. The stack is partially etched to form a concave feature having sidewalls. Metal passivation is deposited on the sidewalls of the concave feature by at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition, by supplying a passivation gas containing a metal halide gas and a hydrogen-containing gas and exposing the sidewalls of the concave feature to a plasma formed from the passivation gas or metal-containing passivation on the sidewalls of the concave feature. The stack is further etched.
[0005] Another embodiment provides a method for etching concave features in a stack beneath a patterned mask forming a mask feature. The stack is partially etched to form concave features with sidewalls. Metal passivation is deposited on the sidewalls through at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition by the steps of supplying a passivation gas containing a metal halide-containing gas and a hydrogen-containing gas, converting the passivation gas into a plasma by supplying multi-state pulsed RF power having two or three states, and exposing the sidewalls of the concave features to the plasma to form metal passivation on the sidewalls of the concave features. The stack is further etched.
[0006] In another embodiment, an apparatus is provided for etching concave features in a stack beneath a patterned mask forming mask features. A substrate support supports a substrate in a processing chamber. An RF power supply provides RF power to the processing chamber. A gas source includes an etching gas source and a passivation gas source supplying hydrogen-containing gas and metal halide-containing gas. A controller is controllably connected to the RF power supply and gas source and is configured to further etch the stack, including at least partially etching the stack, forming concave features with sidewalls by supplying etching gas from the etching gas source, depositing a metal passivation on the sidewalls through at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition, which includes supplying a passivation gas containing metal halide-containing gas and hydrogen-containing gas from the passivation gas source, exposing the sidewalls of the concave features to the passivation gas or plasma formed from the passivation gas, thereby forming the metal passivation on the sidewalls of the concave features.
[0007] These and other features of this disclosure will be described in more detail in the following detailed description, in conjunction with the following figures.
[0008] This disclosure is shown as an example, not as an limitation, in the figures of the attached drawings, where similar reference numbers refer to similar elements. [Brief explanation of the drawing]
[0009] [Figure 1] This flowchart illustrates methods for etching concave features within a stack beneath a carbon-containing mask, using various implementation configurations. [Figure 2A] This is a schematic cross-sectional view of the stack being processed, based on several implementation configurations. [Figure 2B] This is a schematic cross-sectional view of the stack being processed, based on several implementation configurations. [Figure 2C] This is a schematic cross-sectional view of the stack being processed, based on several implementation configurations. [Figure 2D]This is a schematic cross-sectional view of the stack being processed, based on several implementation configurations. [Figure 2E] This is a schematic cross-sectional view of the stack being processed, based on several implementation configurations. [Figure 3] This figure shows a semiconductor processing system that may be used in several implementation forms. [Figure 4] This figure shows a computer system for implementing a controller used in several different implementation configurations. [Modes for carrying out the invention]
[0010] In drawings, similar reference numbers may be used to indicate similar structural elements. Please understand that the depictions in the drawings are approximate and not to scale.
[0011] The disclosure is then described in detail with reference to several preferred implementations thereof, as shown in the accompanying drawings. The following description includes numerous specific details to provide a complete understanding of the disclosure. However, it will be apparent to those skilled in the art that the disclosure can be practiced without some or all of these specific details. In other examples, well-known process steps and / or structures are not described in detail to avoid unnecessarily obscuring the disclosure.
[0012] The fabrication of certain semiconductor devices involves etching features into a stack of materials. In various packaging configurations described herein, the stack of materials comprises one or more layers of one or more materials beneath a carbon-containing mask. In some packaging configurations, at least one layer of the stack comprises at least one of silicon, germanium, and metal. The silicon-containing layer may include silicon nitride, silicon oxide, silicon carbide, silicon oxynitride, silicon oxycarbide, polysilicon, or silicon germanium. In one example, the stack comprises alternating layers of silicon oxide and polysilicon (OPOP). In some packaging configurations, the stack comprises alternating silicon oxide and silicon nitride (ONON) films, or a single silicon oxide layer, or a single silicon layer. In some packaging configurations, the stack may be a conductive layer or dielectric layer that is a metal or silicon-containing layer beneath a carbon-containing mask. In some packaging configurations, the carbon-containing mask is carbon containing at least one of photoresist, doped carbon, and amorphous carbon mask.
[0013] Features etched within a stack may be cylinders, trenches, or other concave features. The aspect ratio of such features is defined as the ratio of the depth to the lateral limiting dimension. As the aspect ratio of such features continues to increase, several problems arise, including (1) insufficient mask selectivity, (2) etching resolution, (3) twisting of features, (4) non-circularity of features, (5) aspect ratio-dependent etching rate, (6) bowing of the etching profile, and (7) slow etching rate.
[0014] When the etching process removes an excess amount of carbon-containing mask, insufficient mask selectivity is a problem, resulting in either no mask remaining at the end of the process, or insufficient mask residue to properly transfer the pattern from the mask to the stack. One common consequence of insufficient mask selectivity is degradation of the feature profile near the tops of concave features. To compensate for insufficient mask selectivity, a thicker mask may be formed. However, a thicker mask results in lower mask resolution and a higher overall aspect ratio, causing more problems during etching of both the mask material and the underlying material.
[0015] Twist refers to a random deviation between the intended bottom position of a feature and the actual final bottom position of the feature (for example, the final position of the feature corresponding to the bottom position of the feature after etching). For example, in some cases, cylindrical features are intended to be etched in a regular pattern. If some or all of the features deviate randomly at the bottom from this pattern, they are understood to be twisted.
[0016] The non-circularity of a feature refers to a deviation of the bottom hole shape from a circular hole shape. This issue is relevant when etching circular features, such as cylinders, where a circular bottom is desirable for concave features. When the bottom hole shape deviates from circularity, it often forms an ellipse, triangle, or a shape close to an irregular polygon. In many cases, these non-circular shapes are undesirable.
[0017] Aspect ratio-dependent etching rate refers to the problem where the etching rate slows down as the aspect ratio of a feature increases. In other words, the etching process slows down as more features are etched into the stack. This is a problem because it can result in low throughput and associated high processing costs.
[0018] Etching profile bowing refers to the tendency of a feature to etch laterally within a stack such that the final profile bulges excessively outward somewhere along the depth of the feature. In other words, the actual maximum critical dimension of the feature exceeds the desired maximum critical dimension of the feature, potentially compromising the integrity of the formed structure or limiting the electrical performance of the final device.
[0019] Low etch rate refers to an etch rate that is slower than desired for a particular application. Low etch rates are problematic because they lead to longer etch times, lower throughput, and higher processing costs.
[0020] Unfortunately, techniques that improve some of these problems, such as poor mask selectivity, often exacerbate other problems. These problems are therefore balanced against each other when designing an etch operation. For example, conventional commercially implemented dielectric etch processes often result in substantial bowing. Previously, it has been difficult to avoid such tradeoffs.
[0021] The techniques described herein may be used to etch recessed features into an underlying stack without some or all of the problems identified above. In other words, the disclosed techniques may be used to etch recessed features into a stack underlying a mask with high stack-to-mask selectivity, reduced mask twisting, reasonably circular features, an acceptable degree of aspect ratio dependent etch rate, acceptable bowing, reduced nonuniformity, reduced asymmetric mask shadowing, and sufficient etch rate.
[0022] Current high aspect ratio contact (HARC) etching processes in both DRAM and NAND applications require more sidewall protection as the aspect ratio increases. Conventional carbon polymer protection is not self-limiting and has aspect ratio dependence due to neutral shadowing. Therefore, more protection is provided on top of the mask than on the sidewalls of HARC features. The resulting HARC bowing CD can be large due to ion scattering in deep features.
[0023] Some implementations provide methods and apparatuses for providing metal-containing sidewall passivation. Such sidewall passivation reduces the bowing phenomenon.
[0024] partial etching For ease of understanding, Figure 1 is a high-level flowchart of a method that may be used in some implementations. A stack having a mask is provided in a process chamber (step 104). Figure 2A is a schematic cross-sectional view of a stack 204 that may be processed according to some implementations, where the stack is under a patterned mask 216, such as an organic mask, an example of which is an amorphous carbon mask. The amorphous carbon mask may also contain some amount of hydrogen and / or oxygen. The mask 216 has mask features. In some implementations, the stack 204 may be formed over a substrate 208. In some implementations, the stack 204 may include silicon-containing layers such as silicon oxide, silicon nitride, or silicon. In some implementations, the stack 204 may be a conductive metal layer of pure metal or alloy, or a metal-containing layer such as metal nitride or metal oxide. In some implementations, the stack 204 may include a germanium-containing layer. In some implementations, the stack is a single bulk layer. In some implementations, the stack is multiple layers. In some implementations, the stack is multiple bilayers, trilayers, or more multilayers. In some implementations, the stack 204 includes multiple bilayers 212, where each bilayer 212 includes a silicon oxide layer 224 and a silicon nitride layer 228.
[0025] The stack is partially etched (step 106). In some implementations, an etching gas is supplied and converted into a plasma. In some implementations, radio frequency (RF) power is used to convert the etching gas into a plasma. The RF power may be supplied in a sinusoidal or other tuned waveform. In some implementations, the plasma is formed within the process chamber. In some implementations, the plasma is formed separately outside the process chamber and then supplied into the process chamber. In some implementations, the etching gas includes OF2 and phosphorus-containing components. In some implementations, the etching gas includes phosphorus-containing components, at least one of phosphorus trifluoride (PF3) and phosphorus pentafluoride (PF5).
[0026] In some implementations, the plasma may be generated with radio frequency (RF) power between approximately 5 and 200 kilowatts (kW), for example between approximately 10 and 100 kW, or in some implementations between approximately 10 and 65 kW. In some cases, two-frequency RF may be used to generate the plasma. Thus, the RF power may be supplied with two or more frequency components, for example, a first frequency component at approximately 400 kilohertz (kHz) and a second frequency component at approximately 60 megahertz (MHz). Different power may be supplied to each frequency component. For example, the first frequency component (e.g., approximately 400 kHz) may be supplied with power between approximately 10 and 65 kW, and the second frequency component (e.g., approximately 60 MHz) may be supplied with a different power, for example between approximately 0.5 and 8 kW. In some implementations, the first frequency component (e.g., approximately 400 kHz) may be supplied with power exceeding 65 kW. These power levels assume that the RF power is supplied to a single 300 mm wafer. The power level can be linearly scaled based on the substrate area of additional substrates and / or other sizes of substrates (therefore, a uniform power density supplied to the substrate is maintained). In other cases, three-frequency RF power may be used to generate the plasma.
[0027] In some implementations, the applied RF power is continuous RF power. In some implementations, the applied RF power may be pulsed. In some implementations, the pulsed RF may have two or three states, providing multi-state pulsed RF power. In three-state pulsing, pulsing occurs between three different (high, medium, low) power levels. In some implementations, the high power level has a duty cycle of 1% to 20%, the medium power level has a duty cycle of 10% to 90%, and the low power level has a duty cycle of 20% to 90%. In some implementations, the low power level is 0 watts. In some implementations, the high power level is 2 to 20 times the low power level, and the medium power level is between the high and low power levels. In some implementations, the RF power is pulsed at a repetition rate of 1 to 50,000 Hz. The RF power may be pulsed between two non-zero values (e.g., between a higher power state and a lower power state) or between zero and a non-zero value (e.g., between an off state and an on state). When the RF power is pulsed between two non-zero values, the power may be in a higher power state and a lower power state. The lower power state may correspond to RF power of approximately 4 kW or less. The duty cycle of the pulse may be in the range of 1 to 50%. The pulsing may have a repetition rate in the range of 100 Hz to 20 kHz. The maximum ion energy on the substrate may be relatively high, for example, about 1 to 10 kilovolts (kV). The maximum ion energy is determined by the applied RF power in combination with the RF excitation frequency, electrode size, electrode arrangement, chamber shape, and plasma interaction details. In some implementations, pulsing can promote the deposition of neutral species.
[0028] In some implementations, a bias ranging from 0 watts (W) to 100 kilowatts (kW) is supplied to accelerate ions toward the top surface of stack 204. In other implementations, a bias ranging from 100 W to 1 kW is supplied.
[0029] Stack 204 is exposed to plasma, and the concave features are partially etched within the stack 204. Figure 2B is a schematic cross-sectional view of stack 204 after the concave features 240 have been partially etched.
[0030] Activation (optional) An optional activation step activates the sidewalls of the concave feature 240 (step 108). In some implementations, an activating gas is provided. In some implementations, the activating gas contains an oxygen-containing component. In some implementations, the oxygen-containing component includes at least one of the following: oxygen gas (O2), ozone (O3), hydrogen peroxide such as hydrogen peroxide (H2O2), carbon monoxide (CO), carbon dioxide (CO2), sulfur dioxide (SO2), carbonyl sulfide (COS), oxygen difluoride (OF2), nitrous oxide (N2O), and nitric oxide (NO). In some implementations, the activating gas may further include the inert gases nitrogen gas (N2), helium (He), xenon (Xe), neon (Ne), and argon (Ar). In some implementations, the activating gas does not contain an inert gas. In some implementations, the activating gas contains a hydrogen-containing component. In some implementations, the hydrogen-containing component includes at least one of hydrogen gas (H2), ammonia (NH3), acetylene (C2H2), ethylene (C2H4), methane (CH4), propyne (C3H4), and silane (SiH4). In some implementations, the hydrogen-containing component is a hydrocarbon. In some implementations, the activating gas may further include the inert gas nitrogen gas (N2), helium (He), xenon (Xe), neon (Ne), and argon (Ar).
[0031] In some implementations, the activating gas is converted into plasma. In some implementations, radio frequency (RF) power is used to convert the activating gas into plasma. In some implementations, the plasma is formed within the process chamber. In some implementations, the plasma is formed separately outside the process chamber and then supplied into the process chamber. In some implementations, the activating gas is supplied at a pressure of 1 milliliter to 10 tors.
[0032] In some implementations, the plasma may be generated with radio frequency (RF) power of approximately 10 watts (W) to 1 kilowatt (kW). In some cases, two-frequency RF may be used to generate the plasma. Thus, the RF power may be supplied with two or more frequency components, for example, a first frequency component of approximately 400 kilohertz (kHz) and a second frequency component of approximately 60 megahertz (MHz). Different power may be supplied to each frequency component. For example, the first frequency component (e.g., approximately 400 kHz) may be supplied with power of approximately 0 to 500 W, and the second frequency component (e.g., approximately 60 MHz) may be supplied with a different power, for example, approximately 10 W to 1 kW. These power levels assume that the RF power is supplied to a single 300 mm wafer. The power levels can be linearly scaled based on the substrate area of additional substrates and / or other sized substrates (thereby maintaining a uniform power density supplied to the substrate). In other cases, three-frequency RF power may be used to generate the plasma.
[0033] In some implementations, the applied RF power is continuous RF power. In some implementations, the applied RF power may be pulsed. In some implementations, the pulsed RF may have two or three states, providing multi-state pulsed RF power. In three-state pulsing, pulsing occurs between three different (high, medium, low) power levels. In some implementations, the high power level has a duty cycle of 1% to 20%, the medium power level has a duty cycle of 10% to 90%, and the low power level has a duty cycle of 20% to 90%. In some implementations, the low power level is 0 watts. In some implementations, the high power level is 2 to 20 times the low power level, and the medium power level is between the high and low power levels. In some implementations, the RF power is pulsed at a repetition rate of 1 to 50,000 Hz. The RF power may be pulsed between two non-zero values (e.g., between a higher power state and a lower power state) or between 0 and a non-zero value (e.g., between an off state and an on state). When the RF power is pulsed between two non-zero values, the power may be in a higher power state and a lower power state. The lower power state may correspond to RF power of approximately 4 kW or less. The duty cycle of the pulse may be in the range of 1 to 50%. The pulsed state may have a repetition rate in the range of 100 Hz to 20 kHz. The maximum ion energy in the substrate may be relatively low, for example, approximately 0 to 100 electron volts (eV). The maximum ion energy is determined by the applied RF power in combination with the RF excitation frequency, electrode size, electrode arrangement, chamber shape, and plasma interaction details.
[0034] In some implementations, a bias ranging from 0 watts (W) to 1 kilowatt (kW) is supplied to accelerate ions toward the top surface of the stack 204.
[0035] Stack 204 is exposed to a plasma formed from an activated gas, which generates dangling bonds along the sidewalls of the concave features 240. Figure 2C is a schematic cross-sectional view of stack 204 after the activation step (step 108). For ease of understanding, the dangling bonds 244 are schematically shown. In some implementations, optional activation (step 108) provides conformally dangling bonds along the entire exposed surface of stack 204, as shown.
[0036] Dangling bonds help facilitate the subsequent deposition of the metal passivation layer. In some implementations, partial etching (step 106) forms dangling bonds, so the activation step (step 108) is unnecessary.
[0037] In some implementations, the flow of an inert gas is maintained or started while the flow of the oxygen-containing or hydrogen-containing component of the activated gas is stopped. RF power is supplied to form a low-energy plasma from the inert gas. In some implementations, the low-energy plasma has an ionic energy in the range of 0 to 100 eV. In some implementations, a high-frequency power RF source, such as a 60 MHz RF source, supplies 10 W to 1 kW of power, and a low-frequency bias RF source, such as a 400 kHz RF source, supplies 0 to 500 W of power. In some implementations, the ionic energy from the inert gas during this step is higher than the ionic energy supplied when the oxygen-containing or hydrogen-containing component is supplied. In such implementations, the ionic energy supplied when the oxygen-containing or hydrogen-containing component is supplied is kept lower so that the plasma from the oxygen-containing or hydrogen-containing component does not mask the plasma. The plasma from the inert gas may have a higher ionic energy without masking. In some implementations, a cycle in which a plasma with lower ion energy is supplied from an oxygen-containing or hydrogen-containing component and a plasma with slightly higher ion energy is supplied from an inert gas may be repeated over one or more cycles.
[0038] sidewall passivation Next, a metal passivation is deposited on the sidewalls of the concave features using at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition (step 112). The deposition of the metal passivation includes supplying a metal halide gas and a hydrogen-containing gas. Although the metal halide gas and the hydrogen-containing gas are considered passivation gases, in some implementations the metal halide gas is supplied before the hydrogen-containing gas in the atomic layer deposition process. In some implementations the passivation gas is supplied in the atomic layer deposition process by periodically alternating between supplying the metal halide gas and then supplying the hydrogen-containing gas multiple times. In some implementations the passivation gas is supplied by simultaneously supplying the metal halide gas and the hydrogen-containing gas in the plasma-enhanced chemical vapor deposition process.
[0039] In some implementations, the metal halide includes at least one of titanium (Ti), tantalum (Ta), tungsten (W), hafnium (Hf), molybdenum (Mo), and cobalt (Co). In some implementations, the metal halide may further include at least one of fluorine (F), chlorine (Cl), bromine (Br), and iodine (I). In some implementations, the metal halide is at least one of molybdenum hexafluoride (MoF6), tungsten hexafluoride (WF6), tantalum pentafluoride (TaF5), tantalum tetrachloride (TaCl4), hafnium tetrachloride (HfCl4), titanium trichloride (TiCl3), titanium tetrachloride (TiCl4), cobalt dichloride (CoCl2), and titanium dichloride (TiCl2). In some implementations, the hydrogen-containing gas includes at least one of hydrogen gas (H2), ammonia (NH3), acetylene (C2H2), ethylene (C2H4), methane (CH4), propyne (C3H4), and silane (SiH4). In some implementations, the hydrogen-containing gas is a hydrocarbon.
[0040] In some implementations, the passivation gas is converted into a plasma. In some implementations, both a metal halide gas and a hydrogen-containing gas are formed in the plasma. In some implementations, only one of the metal halide gas and / or hydrogen-containing gas is formed in the plasma. In some implementations, radio frequency (RF) power is used to convert the passivation gas into a plasma. In some implementations, the plasma is formed within the process chamber. In some implementations, the plasma is formed outside the process chamber and then supplied into the process chamber. In some implementations, the passivation gas is supplied at a pressure of 1 milliliter to 10 tors. In some implementations, the pressure supplied by the passivation gas is less than 200 mtorr while depositing the metal passivation.
[0041] In some implementations, the plasma may be generated with radio frequency (RF) power of approximately 10 watts (W) to 1 kilowatt (kW). In some cases, two-frequency RF may be used to generate the plasma. Thus, the RF power may be supplied with two or more frequency components, for example, a first frequency component of approximately 400 kilohertz (kHz) and a second frequency component of approximately 60 megahertz (MHz). Different power may be supplied to each frequency component. For example, the first frequency component (e.g., approximately 400 kHz) may be supplied with power of approximately 0 to 500 W, and the second frequency component (e.g., approximately 60 MHz) may be supplied with a different power, for example, approximately 10 W to 1 kW. These power levels assume that the RF power is supplied to a single 300 mm wafer. The power levels can be linearly scaled based on the substrate area of additional substrates and / or other sized substrates (thereby maintaining a uniform power density supplied to the substrate). In other cases, three-frequency RF power may be used to generate the plasma.
[0042] In some implementations, the applied RF power is continuous RF power. In some implementations, the applied RF power may be pulsed. In some implementations, the pulsed RF may have two or three states, providing multi-state pulsed RF power. In three-state pulsing, pulsing occurs between three different (high, medium, low) power levels. In some implementations, the high power level has a duty cycle of 1% to 20%, the medium power level has a duty cycle of 10% to 90%, and the low power level has a duty cycle of 20% to 90%. In some implementations, the low power level is 0 watts. In some implementations, the high power level is 2 to 20 times the low power level, and the medium power level is between the high and low power levels. In some implementations, the RF power is pulsed at a repetition rate of 1 to 50,000 Hz. The RF power may be pulsed between two non-zero values (e.g., between a higher power state and a lower power state) or between 0 and a non-zero value (e.g., between an off state and an on state). When the RF power is pulsed between two non-zero values, the power may be in a higher power state and a lower power state. The lower power state may correspond to RF power of approximately 4 kW or less. The duty cycle of the pulse may be in the range of 1 to 50%. The pulsing may have a repetition rate in the range of 100 Hz to 20 kHz. The maximum ion energy on the substrate may be relatively low, for example, about 0 to 100 electron volts (eV). The maximum ion energy is determined by the applied RF power in combination with the RF excitation frequency, electrode size, electrode arrangement, chamber shape, and details of plasma interaction. In some implementations, pulsing may promote the deposition of neutral species.
[0043] In some implementations, a bias ranging from 0 watts (W) to 1 kilowatt (kW) is supplied to accelerate ions toward the top surface of the stack 204.
[0044] Stack 204 is exposed to a plasma formed from a passivation gas, which generates a metal passivation layer along the sidewalls of the concave features 240. Figure 2D is a schematic cross-sectional view of stack 204 after metal sidewall deposition (step 112). The metal passivation layer 248 is shown schematicly for ease of understanding. In some implementations, the metal passivation layer 248 is deposited conformally along the entire exposed surface of stack 204, as shown. In some implementations, the metal passivation layer has a thickness ranging from 1 nm to 20 nm. In some implementations, metal halide ions are bonded to dangling bonds. In some implementations, hydrogen from a halogen-containing gas is used to remove halogens from the metal halide bonded to the dangling bonds to form the metal passivation layer, by removing halides and forming elemental metals bonded to the dangling bonds. In some implementations, the metal may be bonded to other elements. For example, titanium may be bonded to nitrogen to form a titanium nitride layer. In some implementations, the metal passivation layer includes at least one of titanium nitride (TiN), titanium (Ti), titanium oxide (TiO), tantalum (Ta), tantalum nitride (TaN), tantalum oxide (TaO), molybdenum (Mo), molybdenum nitride (MoN), molybdenum oxide (MoO), cobalt (Co), cobalt oxide (CoO), cobalt nitride (CoN), hafnium (Hf), hafnium oxide (HfO), hafnium nitride (HfN), tungsten (W), tungsten oxide (WO), and tungsten nitride (WN). In some implementations, atomic layer deposition provides a more conformable layer than plasma-enhanced vapor deposition and improves the uniformity of the passivation layer on the sidewalls near the top and bottom of the feature.
[0045] In some implementations, no plasma is formed, providing a plasma-less process. Instead, the stack is exposed to a passivation gas at a pressure ranging from 100 mTor to 1 Tor. The substrate support is kept at a temperature below 70°C during the plasma-less metal passivation deposition process. In some implementations, if no plasma is formed, no RF power and bias power are provided. Instead, the passivation gas provides a reaction that deposits metal passivation without requiring ions, energy neutrals, or radicals.
[0046] Further etching The stack is further etched (step 116). In some implementations, an etching gas is supplied and converted into plasma. In some implementations, radio frequency (RF) power is used to convert the etching gas into plasma. In some implementations, the plasma is formed within the process chamber. In some implementations, the plasma is formed separately outside the process chamber and then supplied into the process chamber. In some implementations, further etching of the stack (step 116) uses the same recipe as the partial etching of the stack (step 106). In some implementations, further etching of the stack (step 116) uses a different recipe than the partial etching of the stack (step 106) because it etches to a different depth than the partial etching of the stack (step 106) and / or further etching of the stack (step 116) may etch different materials than the partial etching of the stack (step 106).
[0047] The metal passivation layer 248 prevents or reduces further etching of the stack (step 116) by etching the sidewalls of the concave features 240 to prevent or reduce bowing. Figure 2E is a schematic cross-sectional view of the stack 204 after further etching (step 116). The metal passivation layer 248 (shown in Figure 2D) has been etched away. In some configurations, the metal passivation layer 248 may be removed before etching is complete. In such cases, it is decided that the process will return to an optional activation step (step 108) or metal sidewall deposition (step 112) to etch more (step 120). Once etching of the stack 204 is complete (step 120), the stack 204 may then be removed from the substrate support in the process chamber (step 124). In some configurations, additional steps may be performed, such as removing the metal passivation layer 248, before the stack 204 is removed from the process chamber (step 124).
[0048] In some configurations, the substrate is placed on a substrate support within a process chamber. In some configurations, the substrate support is cooled to a temperature below 0°C. In some configurations, partial etching (step 106), an optional activation step (step 108), metal sidewall deposition (step 112), and further etching of the stack (step 116) are performed in situ within the same chamber and mounted on the same substrate support. The ability to perform the process in situ enables faster throughput, less contamination, and a wider process window.
[0049] Some implementations significantly extend the current process window without causing other trade-offs by providing more robust sidewall protection. Some implementations provide the activation step (step 108) before depositing the metal sidewall (step 112) so that there is no overlap between the timing of the activation step (step 108) and the deposition of the metal sidewall (step 112). In some implementations, supplying the metal halide and the hydrogen-containing gas to supply the passivation gas does not overlap in time in the atomic layer deposition process. In some implementations, a periodic process of supplying the metal halide and the hydrogen-containing gas separately in time is repeated for one, two, three or more cycles. In some implementations, the purge gas is supplied between supplying the metal halide and supplying the hydrogen-containing gas. In some implementations, supplying the metal halide and the hydrogen-containing gas overlaps or is simultaneous in at least a partial plasma-enhanced chemical vapor deposition process. In some implementations, supplying the metal halide and the hydrogen-containing gas completely overlaps in the plasma-enhanced chemical vapor deposition process. In some implementations, the metal halide and hydrogen-containing gas are formed in the plasma simultaneously. In some implementations, the metal halide and hydrogen-containing gas are formed sequentially in the plasma.
[0050] In some implementations, the metal halide comprises a metal from at least one of titanium, tungsten, tantalum, molybdenum, hafnium, and cobalt, and a halide from at least one of chlorine, fluorine, and bromine. In some implementations, the metal halide is a gas containing at least one of molybdenum hexafluoride (MoF6), tungsten hexafluoride (WF6), tantalum pentafluoride (TaF5), tantalum tetrachloride (TaCl4), hafnium tetrachloride (HfCl4), titanium trichloride (TiCl3), titanium tetrachloride (TiCl4), cobalt dichloride (CoCl2), and titanium dichloride (TiCl2).
[0051] One application of the disclosed method relates to forming vertical NAND. In this case, the material on which the features are etched may have a repeating layered structure. For example, the material may include alternating layers of silicon oxide and silicon nitride. In other configurations, the stack may include alternating layers of silicon oxide and polysilicon. The alternating layers form pairs or repeating groups of material. In various cases, the number of pairs or repeating groups can be about 10 to 500 (e.g., about 20 to 1000 individual layers). Features etched into the stack of layers may have a depth of about 2 to 15 μm, for example, about 5 to 9 μm. Features may have a CD width between about 3 to 500 nm, for example, between about 50 to 100 nm or between about 40 to 85 nm. In some configurations, features have a width of less than 100 nm. In some configurations, features have a width of less than 85 nm. In some configurations, the stack includes at least one of layers of SiO, SiN, and SiON.
[0052] As used herein, “high aspect ratio” applied to features within a substrate refers to a depth-to-width aspect ratio of approximately 60:1 or greater. More preferably, this range may include ratios exceeding 100:1, 120:1, 140:1, etc., or even higher. However, the processes described herein may be beneficial for lower aspect ratios such as 30:1 or 10:1. In some mounting configurations, features may have depths ranging from 3 nm to 10 μm.
[0053] The dimensional / parametric details provided herein, such as aspect ratio, thickness, width, and depth, are for illustrative purposes only. It should be understood that various other dimensions / parameters may also be applicable or usable based on the disclosures herein.
[0054] Device The various hardware and method implementations described above may be used in conjunction with lithography patterning tools or processes for the fabrication or manufacture of semiconductor devices, displays, LEDs, photovoltaic panels, and the like. Typically, but not always, such tools / processes are used or performed together in a common manufacturing facility.
[0055] Film lithography patterning typically involves some or all of the following steps, each of which can be performed using several possible tools: (1) coating a workpiece, e.g., a substrate on which a silicon-containing film has been formed, using a spin-on or spray-on tool; (2) curing the photoresist using a hot plate or furnace or other suitable curing tool; (3) exposing the photoresist to visible light, ultraviolet (UV) light, or X-ray light using a tool such as a wafer stepper; (4) selectively removing the resist and thereby developing the resist for patterning using a tool such as a wet bench or spray developer; (5) transferring the resist pattern to the underlying film or workpiece by using a dry or plasma-assisted etching tool; and (6) removing the resist using a tool such as an RF or microwave plasma resist stripper. In some configurations, an ashingable hard mask layer (e.g., an amorphous carbon layer) and other suitable hard masks (e.g., an anti-reflective layer) may be deposited before coating the photoresist.
[0056] In this application, the terms “semiconductor wafer,” “wafer,” “substrate,” “wafer substrate,” and “partially manufactured integrated circuit” are used interchangeably. Those skilled in the art will understand that the term “partially manufactured integrated circuit” can refer to a silicon wafer in any of the many stages of integrated circuit manufacturing on which it is manufactured. Wafers or substrates used in the semiconductor device industry typically have a diameter of 200 mm, 300 mm, or 450 mm. The above detailed description assumes that the mounting configuration is carried out on a wafer. However, the mounting configuration is not limited in this way. Workpieces may vary in shape, size, and material. In addition to semiconductor wafers, other workpieces that may utilize the disclosed mounting configuration include a variety of articles such as printed circuit boards, magnetic recording media, magnetic recording sensors, mirrors, optical elements, and micromechanical devices.
[0057] Unless otherwise specifically defined for a particular parameter, the terms “about” and “approximately” as used herein are intended to mean ±10% of the relevant value.
[0058] Figure 3 is a schematic diagram of an etching reactor system 300, which may be used in several implementation configurations. In some implementation configurations, the etching reactor system 300 comprises a gas distribution plate 306 providing a gas inlet and an electrostatic chuck (ESC) 308 within an etching (or process) chamber 309 enclosed by chamber walls 352. Within the etching chamber 309, a stack 204 is positioned on the ESC 308, which is used as a substrate support. A bias may be supplied to the ESC 308 from an ESC source 348. A gas source 310 is connected to the etching chamber 309 via the gas distribution plate 306. In some implementation configurations, the gas source 310 comprises an etching gas source 312, an activation gas source 316, and a passivation gas source 318. An ESC temperature controller 350 is connected to the ESC 308. A radio frequency (RF) source 330 supplies RF power to the lower electrode and / or upper electrode, which in this embodiment are the ESC 308 and the gas distribution plate 306, respectively. In some implementations, 400 kHz, 60 MHz, and optionally 2 MHz, and 27 MHz power supplies constitute the RF source 330 and ESC source 348. In some implementations, the upper electrode is grounded. In some implementations, one generator is provided for each frequency. In some implementations, the generators may be on separate RF sources, or separate RF generators may be connected to different electrodes. For example, the upper electrode may have an inner electrode and an outer electrode connected to different RF sources. Other implementations may use other arrangements of RF sources and electrodes. The controller 335 is controllably connected to the RF source 330, ESC source 348, exhaust pump 320, and gas source 310. An example of such an etching chamber is the Vantex® etching system manufactured by Lam Research Corporation in Fremont, California. The process chamber can be a CCP (capacitance-coupled plasma) reactor or an ICP (inductively coupled plasma) reactor.
[0059] Figure 4 is a high-level block diagram showing a computer system 400 suitable for implementing a controller 335 used in an implementation configuration. The computer system 400 may have many physical forms, ranging from integrated circuits, printed circuit boards and small handheld devices to massive supercomputers. The computer system 400 may include one or more processors 402 and further include an electronic display device 404 (for displaying graphics, text, and other data), main memory 406 (e.g., random access memory (RAM)), storage device 408 (e.g., hard disk drive), removable storage device 410 (e.g., optical disc drive), user interface device 412 (e.g., keyboard, touchscreen, keypad, mouse or other pointing device, etc.), and a communication interface 414 (e.g., wireless network interface). The communication interface 414 allows software and data to be transferred between the computer system 400 and external devices via links. The system may also include a communication infrastructure 416 (e.g., communication bus, crossover bar, or network) to which the aforementioned devices / modules are connected.
[0060] The information transmitted via the communication interface 414 may be in the form of electronic, electromagnetic, or optical signals, or other signals that can be received by the communication interface 414, via a communication link that carries signals, and may be implemented using wired or cable, optical fiber, telephone line, mobile phone link, radio frequency link, and / or other communication channels. Using such a communication interface 414, in the process of performing the method steps described above, one or more processors 402 may receive information from or output information to the network. Furthermore, the implementation of the method may be performed by a single processor or by a network such as the Internet with a remote processor that shares part of the processing.
[0061] The term “non-temporary computer-readable medium” is generally used to refer to media such as main memory, secondary memory, removable storage devices, and storage devices such as hard disks, flash memory, disk drive memory, CD-ROMs, and other forms of persistent memory, and should not be interpreted as covering temporary subjects such as carrier waves or signals. Examples of computer code include machine code, such as that generated by a compiler, and files containing higher-level code executed by a computer using an interpreter. Computer-readable medium may also be computer code transmitted by computer data signals, which are embodied in carrier waves and represent sequences of instructions executable by a processor.
[0062] In some implementations, the controller 335 is configured to a) at least partially etch the concave features into the stack, b) activate the surface of the stack, c) deposit a metallic passivation on the sidewalls of the concave features by at least one of atomic layer deposition and chemical vapor deposition, and then e) further etch the stack. The controller 335 may be further configured to repeat steps b to e multiple times. The controller 335 is further configured to provide a passivation gas containing a metal halide gas and a hydrogen-containing gas, convert the passivation gas into a plasma, and deposit a metallic passivation by exposing the sidewalls of the concave features to the plasma.
[0063] The configurations and / or techniques described herein are essentially illustrative, and numerous variations are possible; therefore, it should be understood that these particular implementations or examples should not be considered in an exclusive sense. The specific routines or methods described herein may represent one or more of any number of processing strategies. Accordingly, the various operations illustrated may be performed in the illustrated order, in other orders, in parallel, or, in some cases, omitted. Similarly, the order of the processes described above may be changed. Certain references are incorporated herein by reference. Any waiver or denial made in such references should be understood not necessarily apply to the implementations described herein. Similarly, any features described as necessary in such references may be omitted in the implementations herein. The subject matter of this disclosure includes all novel and non-trivial combinations and partial combinations of the various processes, systems and configurations disclosed herein, as well as other features, functions, operations and / or characteristics, and all their equivalents.
[0064] conclusion While this disclosure describes several preferred implementations, there are many variations, modifications, substitutions, and various equivalents that fall within the scope of this disclosure. It should also be noted that there are many alternative ways of implementing the methods and apparatus of this disclosure. Accordingly, the following appended claims are intended to be interpreted as including all such variations, modifications, substitutions, and various equivalents that fall within the true intent and scope of this disclosure. Where used in this disclosure, the phrase "A, B, or C" should be interpreted as meaning a logic ("A OR B OR C") using the non-exclusive logic "OR", and not as meaning "only one of A, B, or C". Each step in the process may be an optional step, not mandatory. Different implementations may have one or more steps removed, and may provide the steps in a different order. Furthermore, different implementations may provide different steps simultaneously rather than sequentially. [Explanation of Symbols]
[0065] 204 stacks 208 circuit boards 212 double layer 216 Patterned Masks 224 Silicon oxide layer 228 Silicon Nitride Layer 240 concave features 244 Dangling Bond 248 Metal passivation layer 300 Etching Reactor System 306 Gas Distribution Plate 308 Electrostatic Chuck (ESC) 309 Etching (or process) chamber 310 Gas sources 312 Etching gas source 316 Activated gas source 318 Passivation gas source 320 Exhaust Pump 330 RF source 335 Controller 348 ESC source 350 ESC Temperature Controller 352 Chamber Wall 400 Computer Systems 402 Processors 404 Electronic Display Devices 406 Main Memory 408 Storage Devices 410 Removable Storage Devices 412 User Interface Devices 414 Communication Interface 416 Communication Infrastructure
Claims
1. A method for etching concave features in a stack beneath a patterned mask that forms a mask feature, a. The step of etching the stack at least partially to form a concave feature having a side wall, b. A step of depositing a metal passivation on the sidewall through at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition, i. A step of supplying a passivation gas containing a metal halide gas and a hydrogen gas, ii. A step of exposing the side wall of the concave feature to the passivation gas or a plasma formed from the passivation gas, thereby forming a metal-containing passivation on the side wall of the concave feature. Steps including, c. The step of further etching the stack A method that includes this.
2. The method according to claim 1, further comprising the step of repeating steps b and c at least once.
3. The method according to claim 1, wherein the step of depositing the metal passivation further includes the step of activating the sidewall before supplying the passivation gas.
4. The step of activating the side wall is, The steps include supplying an activated gas and The steps include forming the aforementioned activated gas in the plasma, To generate a dangling bond, the steps include: exposing the sidewall to the plasma from the activating gas; The method according to claim 3, including the method described in claim 3.
5. The method according to claim 4, wherein the activated gas comprises at least one of an oxygen-containing component and a hydrogen-containing component.
6. The method according to claim 4, wherein the step of supplying the activating gas is performed before, but not simultaneously with, the step of supplying the passivating gas.
7. The step of depositing the metal passivation is carried out by atomic layer deposition, and the step of supplying the passivation gas is, The step of supplying the metal halide, The step of supplying the hydrogen-containing gas, wherein the step of supplying the metal halide precedes the step of supplying the hydrogen-containing gas. The method according to claim 1, including the method described in claim 1.
8. The method according to claim 7, wherein the step of supplying the metal halide and the step of supplying the hydrogen-containing gas are repeated periodically at least once.
9. The step of depositing the metal passivation is performed by plasma-enhanced chemical vapor deposition, and the step of supplying the passivation gas is performed by A step of simultaneously supplying the metal halide and the hydrogen-containing gas, wherein the metal halide and the hydrogen-containing gas are simultaneously converted into a plasma. The method according to claim 1, including the method described in claim 1.
10. The method according to claim 1, further comprising the step of converting the passivation gas into a plasma, which includes the step of supplying RF power, wherein the step of supplying RF power includes supplying at least one of the steps of supplying continuous RF power and supplying multi-state pulsed RF power.
11. The method according to claim 1, further comprising the step of converting the passivation gas into a plasma, which includes the step of supplying multi-state pulsed RF power having two or three states.
12. The method according to claim 1, further comprising the step of converting the passivation gas into a plasma, which includes the step of supplying pulsed RF power having a duty cycle in the range of 1% to 50%.
13. The method according to claim 1, wherein the stack comprises at least one of layers of SiO, SiN, and SiON.
14. The method according to claim 1, wherein the metal halide comprises a metal from at least one of titanium, tungsten, tantalum, molybdenum, hafnium, and cobalt, and a halide from at least one of chlorine, fluorine, and bromine.
15. The metal halide is molybdenum hexafluoride (MoF 6 ), tungsten hexafluoride (WF 6 ), tantalum pentafluoride (TaF 5 ), tantalum tetrachloride (TaCl 4 ), hafnium tetrachloride (HfCl 4 ), titanium trichloride (TiCl 3 ), titanium tetrachloride (TiCl 4 ), cobalt dichloride (CoCl 2 ), and titanium dichloride (TiCl 2 ), the method according to claim 1, wherein the gas contains at least one of the foregoing.
16. The method according to claim 1, wherein the step of depositing the metal passivation is a plasmaless process.
17. The steps include placing the aforementioned stack on a substrate support, The step of providing the substrate support to a temperature of less than 70°C during the step of depositing the metal passivation. The method according to claim 16, further comprising:
18. The method according to claim 17, further comprising the step of providing a pressure in the range of 100 mTor to 1 Tor during the step of depositing the metal passivation.
19. A method for etching concave features in a stack beneath a patterned mask that forms a mask feature, a. The step of etching the stack at least partially to form a concave feature having a side wall, b. A step of depositing a metal passivation on the sidewall through at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition, i. A step of supplying a passivation gas containing a metal halide gas and a hydrogen gas, ii. A step of converting the passivation gas into a plasma by supplying multi-state pulsed RF power having two or three states, iii. The step of exposing the side wall of the concave feature to the plasma in order to form a metal-containing passivation on the side wall of the concave feature. Steps including, c. The step of further etching the stack A method that includes this.
20. An apparatus for etching concave features in a stack beneath a patterned mask that forms a mask feature, process chamber and A substrate support for supporting the substrate within the processing chamber, An RF power supply for supplying RF power to the processing chamber, It is a gas source, Etching gas source and A passivation gas source that supplies hydrogen-containing gas and metal halide-containing gas, A gas source equipped with, A controller that is controllably connected to the RF power supply and the gas source, a. Etch the stack at least partially and supply etching gas from the etching gas source to form a concave feature having side walls. b. Depositing a metal passivation on the sidewall through at least one of atomic layer deposition and plasma-enhanced chemical vapor deposition, i. Passivation gas containing metal halide gas and hydrogen gas is supplied from the passivation gas source, ii. Exposing the side walls of the concave feature to the passivation gas or plasma formed from the passivation gas in order to form a metal-containing passivation on the side walls of the concave feature. Including, deposit, c. Further etching the stack. A controller and A device equipped with the following features.