Manufacturing method of fiber reinforced plastic molded product

The mold system with a U-shaped groove and elastic sealing members addresses cutting and vacuum maintenance issues in fiber-reinforced resin molding, ensuring precise cutting and efficient resin impregnation without tool wear or air leakage.

JP7552425B2Active Publication Date: 2024-09-18TOYOTA BOSHOKU KK
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2021026147
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-22
Publication Date
2024-09-18
Estimated Expiration
2041-02-22

AI Technical Summary

Technical Problem

The existing methods for manufacturing fiber-reinforced resin molded products face challenges such as difficulty in cutting the reinforcing fiber body after impregnation, high wear on cutting tools, and maintaining a reduced pressure state during resin injection due to air leakage at the shear edge part.

Method used

A mold system with a U-shaped groove and through-hole design allows cutting the reinforcing fiber body while the mold is closed, using a pressing member with a cutting blade and elastic sealing members to maintain a vacuum state, enabling resin injection without air leakage.

Benefits of technology

The method enables precise cutting of the fiber body without tool wear and maintains a consistent vacuum for efficient resin impregnation, eliminating post-molding trimming and reducing tool wear.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007552425000005
    Figure 0007552425000005
  • Figure 0007552425000004
    Figure 0007552425000004
  • Figure 0007552425000009
    Figure 0007552425000009
Patent Text Reader

Abstract

To provide a manufacturing method of a fiber-reinforced resin molded product using the RTM method, capable of cutting a reinforcing fiber body into a predetermined shape while clamping a mold and of injecting resin into a cavity in a decompressed state.SOLUTION: There is provided a method for manufacturing a fiber-reinforced resin molded product, which comprises: a first step of placing a reinforcing fiber body 2 between a lower mold 20 and an upper mold 30 and clamping the molds; a second step of inserting a wall portion 42 of a pressing member 40 into a through hole 31 of the upper mold 30 and a groove portion 21 of the lower mold 20 to cut an end portion of the reinforcing fiber body 2 by a cutting edge 43, and sealing a space between a cavity C and an outside of the mold by a lower sealing member 23 and an upper sealing member 33; a third step of sucking air in the cavity C to reduce the pressure; a fourth step of injecting resin 3 in a liquid state into the cavity C to impregnate and solidify the reinforcing fiber body 2; and a fifth step of opening the lower mold 20 and the upper mold 30 to take out a cushion pan 1.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a fiber-reinforced plastic molded product. [Background technology]

[0002] Conventionally, when a fiber-reinforced plastic molded product is molded using the RTM (Resin Transfer Molding) method, a molded product in which a reinforcing fiber body is impregnated with resin and solidified is molded larger than the product shape, and the end portion is cut off to obtain the product shape after molding. Patent Document 1 discloses a technique for manufacturing a fiber-reinforced plastic molded product using such a method. Patent Document 2 discloses a technique for obtaining a molded product in which a planar skin material is integrally molded on the surface of a resin using an injection molding method. According to this technique, a shear edge portion is provided on the outer periphery of a cavity formed by a pair of molding dies, and the end portion of the skin material arranged between the pair of molding dies is thinned or cut by the shear edge portion, and then molten resin material is injected to mold it integrally with the skin material. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-84788 A [Patent Document 2] JP 2006-334808 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the manufacturing method of fiber-reinforced resin molded products described in Patent Document 1, there are problems in that the reinforcing fiber body impregnated and solidified with resin is difficult to cut, takes time, and wears a lot on the blade of the cutting tool. Also, as in the injection molding method described in Patent Document 2, a method is conceivable in which a planar reinforcing fiber body arranged between a pair of molds is cut by a shear edge portion when the molds are closed, and then resin is injected. However, according to this method, the RTM method requires that the air in the cavity be sucked out after the molds are closed to create a reduced pressure state in the cavity, but when the air is sucked out, air leaks from the gap in the shear edge portion, making it difficult to create a reduced pressure state in the cavity.

[0005] In view of these problems, an object of the present invention is to provide a manufacturing method for producing fiber-reinforced plastic molded products by the RTM method, which enables cutting of a reinforcing fiber body into a predetermined shape in a clamped mold state and injection of resin into a cavity in a reduced pressure state. [Means for solving the problem]

[0006] The first invention of the present invention is a method for producing a fiber-reinforced resin molded product in which a planar reinforced fiber body is impregnated and solidified with a resin, using a molding device having a first mold and a second mold which form a cavity having a shape of a product when the molds are clamped, and a pressing member which moves in a mold clamping direction relative to the clamped first mold and the clamped second mold, wherein the first mold is formed with a groove portion having a substantially U-shaped cross section which extends along the outer periphery of the face of the cavity and is recessed toward the opposite side to the second mold, and the second mold is formed with a through hole which extends corresponding to the groove portion when the molds are clamped and penetrates in the mold clamping direction, and the pressing member is formed with a wall portion which has a shape corresponding to the through hole and the groove portion when the first mold and the second mold are clamped and which is inserted from the outside into the through hole and the groove portion and loosely fits therein, and the wall portion is formed with a blade which extends along a wall surface on the cavity side of the groove portion and has a blade on the side of the groove portion. a cutting blade having a tip, and a sealing member for preventing air from flowing from the cavity to the outside of the mold is interposed between the pressing member and the second mold and between the pressing member and the first mold when the wall-shaped portion is inserted into the through hole and the groove, and the molding machine is characterized in having a first step of arranging the reinforced fiber body between the first mold and the second mold and clamping the mold, a second step of inserting the wall-shaped portion into the through hole and the groove and cutting an end of the reinforced fiber body with the cutting blade and sealing between the cavity and the outside of the mold with the sealing member, a third step of sucking air from within the cavity to create a reduced pressure state, a fourth step of injecting liquid resin into the cavity to impregnate and solidify the reinforced fiber body, and a fifth step of opening the first mold and the second mold to remove a fiber-reinforced resin molded product.

[0007] According to the first invention, the reinforcing fiber body can be cut along the outer peripheral edge shape of the cavity surface while the first and second dies are clamped, so there is no need to trim after the molded product is demolded, and there is no problem of large wear on the blade of the cutting tool. In addition, with the wall-like portion inserted from the outside into the through-hole and groove portion, the cavity and the outside of the mold are sealed by the sealing members interposed between the pressing member and the second die and between the pressing member and the first die to prevent air from passing from the cavity to the outside of the mold, so that the reduced pressure inside the cavity can be maintained well while the resin is injected.

[0008] A second invention of the present invention is characterized in that, in the above-mentioned first invention, the pressing member is formed so that the wall-shaped portion extends vertically from the plate-shaped portion, the sealing member is composed of a first sealing member disposed between the wall-shaped portion and a wall surface of the groove portion and extending therefrom, and a second sealing member disposed between the plate-shaped portion and the second mold and extending therefrom, the second sealing member being formed of a compressible elastic body, and in the second step, the second sealing member is pressed by the pressing member and compressively deformed to perform sealing.

[0009] According to the second aspect of the present invention, since the second seal member is made of an elastic body that is compressible and deformable, it is conveniently not necessary to replace the second seal member every time molding is performed.

[0010] The third invention of the present invention is characterized in that, in the second invention, the first sealing member is formed of a compressible elastic body, and in the second step, the first sealing member and the second sealing member are pressed by the pressing member and compressively deformed to perform sealing.

[0011] According to the third invention, the first seal member as well as the second seal member are formed from a compressible elastic body, so there is no need to replace the first seal member and the second seal member every time molding is performed, which is even more convenient.

[0012] The fourth invention of the present invention is characterized in that, in the above-mentioned third invention, the first sealing member is a hollow tubular body, and in the second step, the first sealing member is compressed and deformed in a state in which air is injected into the tubular body.

[0013] According to the fourth aspect of the present invention, the first seal member is more easily compressively deformed, improving the sealing performance between the cavity and the outside of the mold, and enabling the resin to be injected while maintaining a reduced pressure state within the cavity more satisfactorily.

[0014] The 5th invention of the present invention is characterized in that, in the above-mentioned 2nd invention, the first sealing member is a prepreg in which the reinforcing fiber body is impregnated with uncured resin in advance, is placed in the groove portion in the first step, and is solidified in a compressed state in the second step.

[0015] According to the fifth invention, the first sealing member needs to be replaced every time molding is performed, but since the first sealing member can always be a prepreg that has been impregnated with new uncured resin, the sealing performance between the cavity and the outside of the mold is improved and the reduced pressure state inside the cavity can be maintained better when injecting resin.

[0016] The 6th invention of the present invention is characterized in that, in the above-mentioned 2nd invention, the first sealing member is a wax body that is softened by heating and solidified by cooling, and is placed in the groove portion in a heated and softened state in the first step, and is solidified in a compressed state in the second step.

[0017] According to the sixth invention, the first sealing member needs to be replaced every time molding is performed, but a new wax body that is softened by heating and solidified by cooling can always be used as the first sealing member, improving the sealing performance between the cavity and the outside of the mold and allowing the resin to be injected while maintaining a better reduced pressure state within the cavity. [Brief description of the drawings]

[0018] [Figure 1]1 is a plan view seen from above of a molding apparatus used in a manufacturing method of a fiber-reinforced plastic molded product according to a first embodiment of the present invention, in which only the shape of a wall portion is indicated by a dashed line. [Diagram 2] 2 is a cross-sectional view taken along line II-II in FIG. [Diagram 3] 3 is a cross-sectional view of the lower die, upper die, and pressing member of FIG. 2 in an open state. [Figure 4] FIG. 3 is an enlarged view of a portion IV in FIG. 2. [Diagram 5] 5 is a diagram illustrating a manufacturing process of the fiber-reinforced plastic molded product in FIG. 4. [Figure 6] 5 is a diagram illustrating a manufacturing process of the fiber-reinforced plastic molded product in FIG. 4. [Figure 7] 5A and 5B are diagrams illustrating a manufacturing process of a fiber-reinforced plastic molded product according to a second embodiment of the present invention. [Figure 8] 4A to 4C are views for explaining a manufacturing process of a fiber-reinforced plastic molded product according to a second embodiment of the present invention. [Figure 9] 5A to 5C are diagrams illustrating a manufacturing process of a fiber-reinforced plastic molded product according to a third embodiment of the present invention. [Figure 10] 4A to 4C are views for explaining a manufacturing process of a fiber-reinforced plastic molded product according to a third embodiment of the present invention. [Figure 11] 5A to 5C are diagrams illustrating a manufacturing process of a fiber-reinforced plastic molded product according to a fourth embodiment of the present invention. [Figure 12] 10A to 10C are views for explaining a manufacturing process of a fiber-reinforced plastic molded product according to a fourth embodiment of the present invention, and correspond to FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] 1 to 6 show a first embodiment of the present invention. This embodiment is an example in which the present invention is applied to the manufacture of a cushion pan 1, which is the frame of an automobile seat. In each figure, arrows indicate each direction when a lower mold 20 and an upper mold 30 for forming the cushion pan 1 are closed. In the following explanation, descriptions of directions will be made based on these directions. Here, the cushion pan 1 corresponds to the "fiber-reinforced resin molded product" in the claims.

[0020] As shown in Figs. 1 to 3, the cushion pan 1 is a plate-shaped molded product obtained by impregnating a planar reinforced fiber body 2 with a resin 3 and solidifying it. The cushion pan 1 has a substantially rectangular shape with two rear corners chamfered when viewed from above, and includes a main part 1A that is substantially flat in the center in the left-right direction and a pair of left and right side parts 1B that protrude downward on both the left and right sides of the main part 1A. When the cushion pan 1 is mounted on an automobile upside down after molding, the main part 1A supports the lower surface parts of the buttocks and thighs of a seated occupant via a cushion material (not shown), and both side parts 1B support the sides of the buttocks and thighs of the seated occupant via a cushion material (not shown). A seat back (not shown) that supports the back of the seated occupant is attached to the rear side of the cushion pan 1. The reinforced fiber body 2 is a laminate of multiple carbon fiber woven fabrics, but may be a glass fiber woven fabric or an aramid fiber woven fabric. Furthermore, the resin 3 is an epoxy resin, which is a thermosetting resin, but it may also be an unsaturated polyester resin.

[0021] As shown in Figs. 1 to 6, a molding device 10 for molding a cushion pan 1 by the RTM method includes a lower mold 20, an upper mold 30 for forming a cavity C when closed against the lower mold 20, and a pressing member 40 for maintaining a reduced pressure state of the cavity C. A cavity lower surface C1 for forming the surface shape of the cushion pan 1, which is a product, is formed on the upper surface of the lower mold 20. A groove 21 having a substantially U-shaped cross section that is recessed downward is formed on the outer periphery of the cavity lower surface C1. As shown in Figs. 1 and 2, the groove 21 is formed in a substantially rectangular frame shape with two rear corners chamfered when viewed from above. As shown in Fig. 5, the groove 21 has an opening 21a on the upper side. An inner side surface portion 21b is formed extending downward from an edge portion of the opening 21a of the groove portion 21 on the side of the cavity bottom surface portion C1, and an outer side surface portion 21c is formed extending downward from an edge portion of the opening 21a opposite to the cavity bottom surface portion C1. The inner side surface portion 21b is set to extend downward longer than the outer side surface portion 21c. The lower end portion of the inner side surface portion 21b and the lower end portion of the outer side surface portion 21c are connected by a bottom surface portion 21d that is bent and extends in the left-right direction. The bottom surface portion 21d has an upper bottom surface portion 21d1 on the side of the outer side surface portion 21c and a lower bottom surface portion 21d2 on the side of the inner side surface portion 21b. The upper bottom surface portion 21d1 and the lower bottom surface portion 21d2 extend in the horizontal direction. The lower seal member 23, which is a rubber-like member capable of elastic deformation and has a rectangular cross section, is attached to the upper bottom surface portion 21d1 in a manner that a part of the cross section is embedded. A lower parting surface 22 is formed extending horizontally toward the outside of the mold from the edge of the opening 21a of the groove portion 21 opposite the cavity lower surface portion C1. The lower parting surface 22 has a lower outer parting surface 22a formed on the outside of the mold and directly abutting against the upper mold 30, and a lower inner parting surface 22b formed on the opening 21a side of the groove portion 21 and positioned slightly below the lower outer parting surface 22a. The lower inner parting surface 22b abuts against the upper mold 30 with the outer peripheral edge of the reinforcing fiber body 2 interposed therebetween. Here, the lower mold 20 and the upper mold 30 correspond to the "first mold" and "second mold" in the claims, respectively. The lower seal member 23 corresponds to the "first seal member, seal member" in the claims.

[0022] As shown in Figs. 1 to 6, the upper mold 30 includes a main body 30a and a frame-shaped portion 30b attached to the upper portion of the main body 30a. A cavity upper surface C2 for forming the back surface shape of the cushion pan 1, which is a product, is formed on the lower surface of the main body 30a. In addition, an outer peripheral surface 34a and a central surface 34b that is slightly recessed downward from the outer peripheral surface 34a are formed on the upper surface of the main body 30a. The frame-shaped portion 30b includes a thick plate-shaped base portion 30b1 extending horizontally and an extension portion 30b2 extending downward from the outer peripheral edge of the base portion 30b1. A cylinder attachment hole 30b3 that is recessed upward and for attaching a cylinder 40a described later is provided in the central portion of the base portion 30b1. The lower surface of the substrate portion 30b1 and the upper surface of the main body portion 30a are connected by a plurality of cylindrical column members 30c, and the main body portion 30a and the frame portion 30b are integrated. An inner side surface portion 31c is formed on the outer periphery of the cavity upper surface portion C2 of the main body portion 30a, connecting the outer peripheral edge of the cavity upper surface portion C2 and the outer peripheral edge of the outer peripheral surface portion 34a and extending up and down. An upper seal member 33, which is an elastically deformable rubber-like member and has a rectangular cross section, is attached to the outer peripheral surface portion 34a adjacent to the inner side surface portion 31c in a manner that a part of the cross section is embedded. The lower surface of the extension portion 30b2 of the frame portion 30b is formed as an upper parting surface 30b4 extending in the horizontal direction. The upper parting surface 30b4 is made to be the same plane as the outer peripheral edge of the cavity upper surface portion C2. In addition, the surface portion of the extension portion 30b2 of the frame-shaped portion 30b facing the inner surface portion 31c is formed as an outer surface portion 31d. Between the inner surface portion 31c and the outer surface portion 31d, a through hole 31 is formed penetrating in the vertical direction. As shown in Figs. 1, 2 and 4, when the upper mold 30 is closed on the lower mold 20, the through hole 31 matches the shape of the groove portion 21 when viewed from above. As shown in Fig. 5, the through hole 31 has a lower opening 31a on the lower side. When the upper mold 30 is closed on the lower mold 20, the inner surface portion 31c of the through hole 31 is flush with the inner surface portion 21b of the groove portion 21, and the outer surface portion 31d is flush with the outer surface portion 21c of the groove portion 21. The upper parting surface 32 has its mold outer portion directly abutting against the lower outer parting surface 22a, and its portion on the lower opening 31a side of the through hole 31 abutting against the lower inner parting surface 22b with the outer peripheral edge of the reinforcing fiber body 2 interposed therebetween.Here, the upper seal member 33 corresponds to the "second seal member, seal member" in the claims.

[0023] As shown in Figs. 2 to 6, the pressing member 40 is formed with a plate-shaped portion 41 extending in the horizontal direction and a wall-shaped portion 42 extending downward from the lower surface side of the plate-shaped portion 41. The plate-shaped portion 41 is provided with a plurality of through holes 41a into which the respective column members 30c of the upper mold 30 are loosely fitted. The plate-shaped portion 41 is attached between the main body portion 30a and the frame-shaped portion 30b of the upper mold 30 so as to be movable up and down. A compression coil spring 44 with each column member 30c as an axis is disposed between the lower surface portion of the plate-shaped portion 41 and the central surface portion 34b of the main body portion 30a of the upper mold 30, and a hydraulic cylinder 40a is disposed between the upper surface portion of the plate-shaped portion 41 and the upper surface portion of the cylinder mounting hole 30b3 of the frame-shaped portion 30b of the upper mold 30. The pressing member 40 is configured to move up and down with respect to the upper mold 30 when the hydraulic cylinder 40a is operated. The wall-shaped portion 42 has a rectangular cross section with the long axis extending in the up-down direction, and a plate-shaped cutting blade 43 with a cutting edge 43a on the lower side is attached to the inner surface of the mold. The cutting edge 43a protrudes downward from the bottom surface 42a, which is the surface on the tip side of the wall-shaped portion 42. The thickness of the wall-shaped portion 42 with the cutting blade 43 attached is set to be slightly smaller than the width of the through hole 31 (the length in the left-right direction in FIG. 5). As described later, when the reinforced fiber body 2 is placed between the lower mold 20 and the upper mold 30 and the mold is closed, the pressing member 40 is lowered to insert the wall-shaped portion 42 with the cutting blade 43 attached into the through hole 31 and the groove portion 21. The surface of the cutting blade 43 opposite the wall-shaped portion 42 slides against the inner surface portion 31c of the upper mold 30 and the inner surface portion 21b of the lower mold 20 and lowers. Then, the end portion of the reinforced fiber body 2 is cut by the cutting blade 43. The bottom surface 42a of the wall-shaped portion 42 presses against the lower seal member 23 of the lower die 20, compressing and deforming it, and the lower surface of the plate-shaped portion 41 presses against the upper seal member 33 of the upper die 30, compressing and deforming it, thereby blocking the flow of air between the cavity C and the outside of the die. At this time, a part of the end portion of the cut reinforced fiber body 2 enters into the gap between the outer surface portion 21c of the lower die 20 and the surface of the wall-shaped portion 42 to which the cutting blade 43 is not attached. In this state, the cutting edge 43a of the cutting blade 43 is located above the lower bottom surface portion 21d2 of the lower die 20 at a distance.

[0024] A method for manufacturing a cushion pan 1 using a molding device 10 will be described with reference to Figs. 2 to 6. In the first step, as shown in Figs. 3, 5, and 6, when the reinforcing fiber body 2 is placed on the lower surface C1 of the cavity of the lower mold 20 and the upper mold 30 is closed, the reinforcing fiber body 2 is disposed in the cavity C and the reinforcing fiber body 2 covers the opening 21a of the groove portion 21. At this time, the end portion of the reinforcing fiber body 2 is sandwiched between the lower inner parting surface 22b of the lower mold 20 and the upper parting surface 30b4 of the upper mold 30. In this state, in the second step, the hydraulic cylinder 40a is operated with respect to the closed lower mold 20 and upper mold 30 to lower the pressing member 40 from above, and the wall-like portion 42 is inserted into the through hole 31 of the upper mold 30 and the groove portion 21 of the lower mold 20 from the bottom surface portion 42a. At this time, the pressing member 40 descends with the surface of the attached cutting blade 43 opposite to the wall-shaped portion 42 in sliding contact with the inner surface portion 31c of the upper mold 30 and the inner surface portion 21b of the lower mold 20. Then, the end portion of the reinforced fiber body 2 is cut by the cutting blade 43. The bottom surface portion 42a of the wall-shaped portion 42 presses the lower seal member 23 of the lower mold 20 to compress and deform it, and the lower surface portion of the plate-shaped portion 41 presses the upper seal member 33 of the upper mold 30 to compress and deform it, thereby stopping the descent of the pressing member 40. In this state, the circulation of air between the cavity C and the outside of the mold is obstructed by the lower seal member 23 and the upper seal member 33. At this time, as shown in FIG. 4, the portion of the groove portion 21 side of the end portion of the cut reinforced fiber body 2 enters the gap between the outer surface portion 21c of the lower mold 20 and the surface of the wall-shaped portion 42 to which the cutting blade 43 is not attached. In this state, the cutting edge 43a of the cutting blade 43 is positioned above the lower bottom surface portion 21d2 of the lower mold 20 at a distance.

[0025] 2 and 4, an air suction device (not shown) connected to the cavity C is operated to suck air from the cavity C and reduce the pressure. At this time, the compressed lower seal member 23 and upper seal member 33 act to prevent air from entering the cavity C from outside the mold, so the cavity C is kept in a reduced pressure state. Next, in a fourth step, the operation of the air suction device is stopped, and liquid resin 3 is injected into the cavity C through an injection port (not shown) and solidified while impregnating the reinforced fiber body 2. Finally, in a fifth step, the pressing member 40 and upper die 30 are raised relative to the lower die 20, and the cushion pan 1, which is a molded product obtained by impregnating the reinforced fiber body 2 with the liquid resin 3 and solidifying it, is demolded.

[0026] The first embodiment configured as above has the following effects. The upper die 30 is lowered relative to the lower die 20 and clamped, and the pressing member 40 is lowered to cut the end portion of the reinforced fiber body 2 arranged in the cavity C along the outer peripheral edge shape of the cavity lower surface portion C1. This eliminates the need for trimming after demolding the molded product, and also eliminates the problem of large wear of the blade of the cutting tool. In addition, with the wall-shaped portion 42 of the pressing member 40 inserted from above into the through hole 31 of the upper die 30 and the groove portion 21 of the lower die 20, the lower seal member 23 and the upper seal member 33 are compressed and deformed, preventing air from circulating from inside the cavity C to the outside of the mold. This allows the injection of the liquid resin 3 while maintaining a good reduced pressure state in the cavity C in the third step, and promotes the impregnation of the liquid resin 3 into the reinforced fiber body 2. Furthermore, since the lower seal member 23 and the upper seal member 33 are made of an elastic body that can be compressed and deformed, there is no need to replace the lower seal member 23 and the upper seal member 33 every time molding is performed, which is convenient.

[0027] 7 and 8 show a second embodiment of the present invention. The difference from the first embodiment is that a lower seal member 23A, which is a hollow tubular body capable of elastic deformation, is used instead of the lower seal member 23. The same reference numerals are used for structures common to the first embodiment, and the description thereof will be omitted. The lower seal member 23A is embedded and installed so that a part of it is exposed upward from the upper bottom surface portion 21d1 of the groove portion 21 in the lower mold 20 in a state in which air can be supplied from an air supply device (not shown) to the internal space 23A1. Then, in the second step, air is supplied to the internal space 23A1 before the bottom surface portion 42a of the wall-shaped portion 42 abuts, and the lower seal member 23A is pressed and deformed by the bottom surface portion 42a in an expanded state. As a result, the lower seal member 23A is more easily compressed and deformed than the lower seal member 23, improving the sealing performance between the cavity C and the outside of the mold, and the resin can be injected while maintaining a better reduced pressure state in the cavity C. Here, the lower seal member 23A corresponds to the "first seal member, seal member" in the claims.

[0028] 9 and 10 show a third embodiment of the present invention. The difference from the first embodiment is that a prepreg in which a strip of the reinforced fiber body 2 is impregnated with unhardened resin in advance is used as the lower seal member 23B instead of the lower seal member 23. The same reference numerals are used for structures common to the first embodiment, and the description is omitted. The lower seal member 23B is a prepreg in which a strip of the reinforced fiber body 2 is impregnated with unhardened resin in a liquid state in advance, and is arranged so that a part of it is exposed upward from the upper bottom surface portion 21d1 of the groove portion 21 in the lower mold 20 in the second step. Then, the bottom surface portion 42a of the wall-shaped portion 42 presses and deforms the lower seal member 23B to suppress the flow of air between the cavity C and the outside of the mold. The lower seal member 23B, which has been solidified after the cushion pan 1 is demolded in the fifth step, is discarded together with the cut end material of the reinforced fiber body 2. This allows the lower seal member 23B to always be a prepreg impregnated with new unsolidified resin in a liquid state, improving the seal between the cavity C and the outside of the mold and allowing the resin to be injected while maintaining a better reduced pressure state inside the cavity C. Here, the lower seal member 23B corresponds to the "first seal member, seal member" in the claims.

[0029] 11 and 12 show a fourth embodiment of the present invention. The difference from the first embodiment is that a wax body that is softened by heating and solidified by cooling is used as the lower seal member 23C instead of the lower seal member 23. The same reference numerals are used for the structures common to the first embodiment, and the description is omitted. The lower seal member 23C is a wax body that is softened by heating and solidified by cooling, and in the second step, in a heated and softened state, it is arranged so that a part of it is exposed upward from the upper bottom surface portion 21d1 of the groove portion 21 in the lower mold 20. Then, in a state in which the bottom surface portion 42a of the wall-shaped portion 42 presses and deforms the lower seal member 23C, the flow of air between the cavity C and the outside of the mold is suppressed. In the fifth step, the lower seal member 23C that has solidified after the cushion pan 1 is demolded is discarded together with the end material of the cut reinforced fiber body 2. This allows the lower seal member 23C to always be a new wax body, improving the seal between the cavity C and the outside of the mold, and allowing the resin to be injected while maintaining a better reduced pressure state inside the cavity C. Here, the lower seal member 23C corresponds to the "first seal member, seal member" in the claims.

[0030] Although specific embodiments have been described above, the present invention is not limited to those external appearances and configurations, and various modifications, additions, and deletions are possible without departing from the spirit of the present invention. For example, the following can be mentioned.

[0031] 1. In the above embodiment, the first mold is the lower mold 20 and the second mold is the upper mold 30, which open and close vertically. However, regardless of this, the first mold and the second mold may also be configured to open and close horizontally.

[0032] 2. In the above embodiment, the groove 21 is provided on the outer periphery of the cavity bottom surface C1. However, regardless of this, if there is a hole penetrating through the center of the molded product in the plate thickness direction, a groove can also be provided on the outer periphery of the hole. This eliminates the need to use a cutting tool to make holes after molding.

[0033] 3. In the above embodiment, the present invention is applied to an automobile seat, but it may also be applied to seats installed in airplanes, ships, trains, etc., and may also be applied to interior parts of automobiles. [Explanation of symbols]

[0034] 1 Cushion pan (fiber reinforced plastic molded product) 2 Reinforced fiber body 3. Resin 10 Molding equipment 20 Lower type (first type) 21 Groove 23 Lower seal member (first seal member, seal member) 23A Lower seal member (first seal member, seal member) 23B lower seal member (first seal member, seal member) 23C Lower seal member (first seal member, seal member) 30 Upper mold (2nd mold) 31 Through hole 33 Upper seal member (second seal member, seal member) 40 Pressing member 42 Wall-like part 43 Cutting blade 43a Cutting edge C Cavity C1 Cavity bottom C2 Cavity top

Claims

1. A method for producing a fiber-reinforced plastic molded product in which a planar reinforcing fiber body is impregnated and solidified with a resin using a molding device having a first mold and a second mold that form a cavity of a product shape when the molds are closed, and a pressing member that moves in a mold closing direction relative to the first mold and the second mold that are closed, The first die has a groove portion having a generally U-shaped cross section extending along an outer periphery of a surface of the cavity and recessed toward an opposite side to the second die, a through hole is formed in the second die, the through hole extending in a direction of clamping the die and corresponding to the groove when the die is clamped; the pressing member is formed with a wall-like portion having a shape corresponding to the through hole and the groove portion in a state in which the first die and the second die are clamped, the wall-like portion being inserted from the outside into the through hole and the groove portion and loosely fitted therein; The wall portion is provided with a cutting blade that extends along a wall surface of the groove portion on the side of the cavity and has a cutting edge on the side of the groove portion, a seal member that blocks air from passing through the cavity to the outside of the mold is interposed between the pressing member and the second mold and between the pressing member and the first mold in a state in which the wall-like portion is inserted into the through hole and the groove portion, A first step of placing the reinforcing fiber body between the first mold and the second mold and clamping the mold; a second step of inserting the wall-shaped portion into the through hole and the groove portion, cutting the end of the reinforcing fiber body with the cutting blade, and sealing the cavity and the outside of the mold with the sealing member; a third step of sucking air from the cavity to create a reduced pressure state; A fourth step of injecting a liquid resin into the cavity to impregnate and solidify the reinforcing fiber body; A fifth step of opening the first mold and the second mold to remove a fiber reinforced resin molded product, The pressing member is formed such that the wall portion extends vertically from a plate portion, the sealing member is composed of a first sealing member disposed between the wall portion and a wall surface of the groove portion and extending therefrom, and a second sealing member disposed between the plate portion and the second die and extending therefrom, the second sealing member being formed of a compressible elastic body; In the second step, the second seal member is pressed by the pressing member to perform compressive deformation, thereby achieving sealing.

2. In claim 1, A method for manufacturing a fiber-reinforced resin molded product, in which the first sealing member is formed of a compressible elastic body, and in the second step, the first sealing member and the second sealing member are pressed by the pressing member to perform sealing by compressive deformation.

3. 3. The method for manufacturing a fiber-reinforced plastic molded product according to claim 2, wherein the first seal member is a hollow tubular body, and in the second step, the tubular body is compressed and deformed while air is injected into the tubular body.

4. 2. The method for manufacturing a fiber-reinforced resin molded product according to claim 1, wherein the first sealing member is a prepreg in which the reinforced fiber body is impregnated with uncured resin in advance, the prepreg being placed in the groove portion in the first step, and being solidified in a compressed state in the second step.

5. 2. The method for manufacturing a fiber-reinforced plastic molded product according to claim 1, wherein the first sealing member is a wax body that is softened by heating and solidified by cooling, and is placed in the groove portion in the heated and softened state in the first step, and is solidified in a compressed state in the second step.

Citation Information

Patent Citations

  • Reaction injection molding device for molding fiber-resin reinforced molded article

    JP1992112015A

  • Monolithic molding method

    JP2006334808A

  • Apparatus and method for press molding of molded article containing reinforced fibers and thermoplastic resin

    JP2017222142A

  • Molding apparatus, and method for manufacturing fiber reinforced resin molded product

    JP2019084788A

  • Method for producing structural injection molded parts using lost motion movement between a mold and surrounding cutting blade

    US5182065A