Mold manufacturing method and foamed resin material manufacturing method using the mold produced by the mold manufacturing method

By applying thermoplastic resist to core vents in molds, the method addresses the issue of visible core vent marks on foamed resin materials, improving design quality through integrated patterned cavity forming surfaces.

JP7555572B2Active Publication Date: 2024-09-25SANKO GIKEN
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020171011
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-09
Publication Date
2024-09-25
Estimated Expiration
2040-10-09

AI Technical Summary

Technical Problem

Conventional methods fail to process the cavity forming surface of core vents in molds, leading to visible core vent marks on foamed resin materials, which affect design quality.

Method used

A mold manufacturing method that includes applying thermoplastic resist, such as beeswax clay, to the core vents before intaglio processing to prevent corrosion and etching solution ingress, allowing for patterned cavity forming surfaces while suppressing vent hole expansion.

Benefits of technology

The method effectively reduces the visibility of core vent marks on foamed resin materials by integrating the cavity forming surface into the intaglio treatment, enhancing design quality without additional post-processing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555572000001
    Figure 0007555572000001
  • Figure 0007555572000002
    Figure 0007555572000002
  • Figure 0007555572000003
    Figure 0007555572000003
Patent Text Reader

Abstract

To provide a mold manufacturing method capable of suppressing an expansion of a ventilation hole of a core vent due to corrosion while including a cavity forming surface in the core vent as a target of corrosion intaglio treatment, and a foamed resin material manufacturing method that presents core vent marks into a low-profile manner to increase design characteristics.SOLUTION: There is provided a mold manufacturing method, in which after filling a ventilation hole 21 of a core vent 20 with, for example, a beeswax clay 50, a mold 11 is subjected to corrosion intaglio treatment (for example, wet etching). Since the beeswax clay 50 is a substance stable to an etching solution, only a cavity forming surface 22 is corroded, and a wall surface 24 of the ventilation hole 21 is not corroded. As a result, the mold 11 can be continuously patterned over the cavity forming surface 22, and the core vent marks on a surface of a foamed resin material molded using the mold 11 can be presented in a low-profile manner.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for manufacturing a mold for molding a foamed resin molding material, and a method for manufacturing a foamed resin material using a mold manufactured by the mold manufacturing method. [Background technology]

[0002] In foam resin molding, material such as foam beads is placed in a mold and high-temperature steam is pumped into the mold to heat the material. The heated material expands and fills the mold while fusing together, forming a foam resin material in a shape that matches the mold. The space inside the mold where the material is placed (or filled with the material) is called the cavity.

[0003] The mold has a passage (a through hole from the mold surface to the mold inner wall) for sending steam into the cavity, and a roughly cylindrical member called a core vent is embedded in the passage flush with the mold inner wall. Steam passes through this steam passage in the mold and finally passes through a vent hole in the core vent before being sent into the cavity.

[0004] Incidentally, it is known that in order to improve the design of the foamed resin material thus molded, the mold is subjected to an intaglio etching process. Specifically, a pattern is formed on the inner wall of the mold by a process such as wet etching, and then the foamed resin material is molded to obtain a foamed resin material surface corresponding to the pattern. For example, the design of the foamed resin material can be improved by applying a grained or geometric pattern.

[0005] However, in addition to the intended pattern, the surface of the foamed resin inevitably has "core vent marks" due to the molding process. Because these marks affect the design of the foamed resin material as a product, technologies have been devised to make them as inconspicuous as possible.

[0006] For example, in Patent Document 1, the vent holes of the core vent are lattice-shaped slits, thereby reducing the contact area between the cavity forming surface of the core vent (the surface of the core vent that comes into contact with the filled material) and the material. As a result, the softening speed of the material is suppressed and the amount of material that melts into the slits is reduced, making the core vent marks less noticeable. Note that Fig. 11 is a diagram showing a foamed resin material molded using a conventional mold. The core vent marks 100 can be seen in the grain pattern on the surface of the foamed resin material. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2016-112811 A Summary of the Invention [Problem to be solved by the invention]

[0008] However, in the conventional technology, although various processing can be applied to the shape of the vent hole of the core vent, it is not possible to apply any processing to the cavity forming surface of the core vent itself.

[0009] The present disclosure has been devised in consideration of these points, and has an objective of providing a mold manufacturing method that can suppress the expansion of the air holes in a core vent due to corrosion while including the cavity-forming surface of the core vent in the target of etching intaglio treatment, and a foamed resin material manufacturing method that can make the core vent marks less noticeable, thereby improving the design. [Means for solving the problem]

[0010] In order to achieve the above object, the mold manufacturing method disclosed herein is a mold manufacturing method that includes embedding a core vent in a steam passage of a mold body, applying a required resist, and then performing an etching intaglio process, and includes a filling step of filling the ventilation hole of the core vent with thermoplastic resist prior to the etching intaglio process.

[0011] According to this, since the thermoplastic resist is filled in the vent hole, the inner wall of the mold and the cavity forming surface of the core vent are corroded, while the etching solution or etching gas used in the intaglio etching process does not enter the vent hole of the core vent, and corrosion is suppressed. Therefore, it is possible to obtain a mold manufacturing method that can suppress the expansion of the vent hole of the core vent due to corrosion while including the cavity forming surface of the core vent in the target of the intaglio etching process.

[0012] The above mold manufacturing method may further include a heating and removing step of removing, by heating, the thermoplastic resist filled in the vent hole in the filling step, after the etching intaglio process.

[0013] This method requires no post-treatment such as waste liquid disposal, and thus reduces costs, compared to a method in which the thermoplastic resist is dissolved and washed with a chemical solvent.

[0014] In the above mold manufacturing method, the thermoplastic resist may be beeswax clay.

[0015] According to this, it is easier to inject or press into the ventilation holes and is also easier to disappear from the ventilation holes than thermoplastic resists whose main components are not beeswax.

[0016] In the above mold manufacturing method, the filling step may include a dipping step of dipping the core vent into the molten beeswax clay, and a cooling step of cooling the beeswax clay coated on the core vent by the dipping step.

[0017] According to this method, since the immersion can be performed without considering the orientation of the core vent, the beeswax clay can be simultaneously and easily filled into each of the ventilation holes of many core vents, compared to the method of filling from the cavity forming surface side or its back side. Also, the beeswax clay remaining in the small gaps between the steam passage and the side surface of the core vent can prevent the intrusion of etching solution and etching gas.

[0018] In the above mold manufacturing method, in the filling step, the thermoplastic resist may be filled from a rear surface of a cavity forming surface in the core vent.

[0019] According to this method, compared to the method of filling from the cavity forming surface side, thermoplastic resist is less likely to remain on the cavity forming surface of the core vent, thereby reducing the work required for the process of removing excess thermoplastic resist remaining on the cavity forming surface.

[0020] In the above mold manufacturing method, the filling process may include a closing process of closing the air hole on the cavity forming surface side of the core vent, an injection process of injecting the thermoplastic resist into the air hole from the back side of the cavity forming surface, a cooling process of cooling the thermoplastic resist injected into the air hole, and an opening process of opening the air hole closed by the closing process.

[0021] According to this, the outlet for the injected thermoplastic resist is blocked, and then the thermoplastic resist is cooled from the outlet side, which makes it possible to prevent the thermoplastic resist from leaking out to the cavity forming surface side, and makes it even more difficult for the thermoplastic resist to remain on the cavity forming surface, thereby further reducing the work required for the step of removing the excess thermoplastic resist remaining on the cavity forming surface.

[0022] In the above mold manufacturing method, the filling process may include a closing process of closing the air hole on the cavity forming surface side of the core vent, a pressing process of pressing the thermoplastic resist into the air hole from the back side of the cavity forming surface, and an opening process of opening the air hole closed by the closing process.

[0023] According to this, instead of waiting for the molten thermoplastic resist to drip into the ventilation hole under its own weight, the thermoplastic resist is actively forced into the ventilation hole, thereby shortening the filling time of the thermoplastic resist.

[0024] In the above mold manufacturing method, in the filling step, the thermoplastic resist may be filled from a cavity forming surface of the core vent.

[0025] This allows the amount of thermoplastic resist to be filled to just the necessary amount, compared to a method of filling from the back side of the cavity forming surface (which requires filling all of the air holes with thermoplastic resist).

[0026] In the above mold manufacturing method, the filling process may include a pressing process of pressing the thermoplastic resist into the air hole from the cavity forming surface side, and a removal process of removing the thermoplastic resist remaining on the cavity forming surface of the core vent.

[0027] According to this, instead of waiting for the molten thermoplastic resist to drip into the ventilation hole under its own weight, the thermoplastic resist is actively forced into the ventilation hole, thereby shortening the filling time of the thermoplastic resist.

[0028] In addition, in order to achieve the above object, the method of manufacturing a foamed resin material according to the present disclosure involves molding a foamed resin material using a mold produced by the above-mentioned mold manufacturing method.

[0029] According to this, by using, for example, a mold in which a continuous pattern is applied across the cavity forming surface of the core vent to mold the foamed resin material, it is possible to prevent core vent marks from remaining in spots on the surface of the foamed resin material, thereby providing a method for manufacturing foamed resin material that makes the core vent marks less noticeable and enhances the design. Effect of the Invention

[0030] According to the present disclosure, it is possible to provide a mold manufacturing method that can suppress the expansion of the air holes in a core vent due to corrosion while including the cavity-forming surface of the core vent in the target of etching intaglio processing, and a foamed resin material manufacturing method that can improve design by making the core vent marks less noticeable. [Brief description of the drawings]

[0031] [Figure 1] FIG. 2 is a schematic diagram showing a method for molding a foamed resin material. [Diagram 2] FIG. 2 is an enlarged view of a portion of the core mold. [Diagram 3] This is an enlarged view of a mold in which corrosion has spread to the cavity forming surface of the core vent. [Figure 4] 2A to 2C are diagrams illustrating a mold manufacturing method according to the first embodiment. [Diagram 5] FIG. 2 is a diagram showing a mold manufactured by the mold manufacturing method of the present disclosure. [Figure 6] 1 is a diagram showing a foamed resin material molded using a mold manufactured by the mold manufacturing method of the present disclosure. [Figure 7] 11A to 11C are diagrams illustrating a mold manufacturing method according to a second embodiment. [Figure 8] 13A to 13C are diagrams illustrating a mold manufacturing method according to a third embodiment. [Figure 9] 13A to 13C are diagrams illustrating a mold manufacturing method according to a fourth embodiment. [Figure 10] 13A to 13C are diagrams illustrating a mold manufacturing method according to a fifth embodiment. [Figure 11] FIG. 1 is a diagram showing a foamed resin material molded by a conventional mold. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0032] First embodiment of die manufacturing method Hereinafter, a mold manufacturing method according to an embodiment of the present disclosure will be described.

[0033] Before describing the mold manufacturing method according to this embodiment, first, one embodiment of how a foamed resin material is molded using the mold will be briefly described with reference to Figs.

[0034] As shown in Fig. 1, a foam resin molding device 10 is a device that heats and expands a foam resin molding material 30 (made of foam beads fed by a raw material feeding gun 17) in a cavity 12 of a mold 11 using high-temperature steam introduced through a plurality of core vents 20 embedded in the mold 11 to mold a foam resin material. The mold 11 is made up of a core mold 11a and a cavity mold 11b, and the space surrounded by the inner walls 14 of these is called a cavity 12, which is formed in a shape corresponding to the outer shape of the foam resin material, for example, a resin part for an automobile.

[0035] 2 is an enlarged view of a portion of the core mold 11a, and as shown in Fig. 2, the mold 11 is provided with steam passages 13 at various locations, and the core vents 20 are embedded one by one into each of the steam passages 13. Specifically, each core vent 20 is embedded until its surface is flush with the inner wall 14 of the mold 11, and forms a cavity 12 together with the inner wall 14.

[0036] In such a foam resin molding apparatus 10, steam is sent from the steam passage 13 to the foam resin molding material 30 charged into the cavity 12. Specifically, steam is sent from the core-side steam-in 15a with the core-side steam-out 15b closed, and passes through the vent hole 21 of the core vent 20 in the core mold 11a and enters the cavity 12, as shown by the arrow in Fig. 2. Then, the steam sent into the cavity 12 passes through the vent hole 21 of the core vent 20 in the cavity mold 11b and is discharged from the cavity-side steam-out 16b.

[0037] Next, steam is sent in from the cabinet-side steam-in 16a with the core-side steam-out 15b closed to melt the surfaces of the foam beads with heat and promote fusion bonding. The steam passes through the vent hole 21 of the core vent 20 in the cabinet mold 11b and enters the cavity 12, passes through the vent hole 21 of the core vent 20 in the core mold 11a, and is discharged from the core-side steam-out 15b. This flow of steam from the cabinet to the core and back to the cabinet is repeated several times to mold the foamed resin material.

[0038] Here, according to the mold manufacturing method of this embodiment, it is possible to manufacture a mold 11 in which various patterns such as unevenness, texture, and geometric patterns are applied by etching intaglio processing not only to the inner wall 14 of the mold 11 that forms the cavity 12, but also to the cavity forming surface in the core vent 20.

[0039] For example, Fig. 3 is an enlarged view of a mold in which corrosion has spread to the cavity forming surface of the core vent. As shown in Fig. 3, the mold 11 has an inner wall 14 with a continuous uneven pattern extending over the cavity forming surface 22 of the core vent 20, so that there is no boundary between the inner wall 14, which is the target of the intaglio etching treatment, and the core vent 20, which is not the target. In addition, since corrosion does not spread to the wall surface 24 of the vent hole 21, the strength of the core vent 20 itself can be maintained even after the intaglio etching treatment. In this disclosure, the intaglio etching treatment will be described as being performed by wet etching (hereinafter, simply referred to as etching).

[0040] Hereinafter, the mold manufacturing method according to the first embodiment will be described with reference to Fig. 4. First, as shown in Fig. 4(A), the core vent 20 is placed in a container 80 containing molten beeswax clay 50. As a result, both the cavity forming surface 22 of the core vent 20 and the back surface 23 of the cavity forming surface 22 come into contact with the molten beeswax clay 50, and the beeswax clay enters and fills the vent hole 21. This is the same technique as so-called dipping or dipping, and the entire core vent 20 is covered with the beeswax clay.

[0041] Here, the beeswax clay 50 in this disclosure is a clay made by mixing beeswax and wax, and although the hardness varies depending on the season, it is hard at room temperature and softens at body temperature. The melting point is about 60 degrees, and once it cools and solidifies, it can be used repeatedly.

[0042] Although only one core vent 20 is shown in FIG. 4, multiple core vents 20 may be inserted, and in that case, the core vents 20 can be immersed without considering the orientation thereof. Therefore, compared to embodiments 2 to 5 described below, the beeswax clay 50 can be simultaneously and easily filled into each of the ventilation holes 21 of multiple core vents 20.

[0043] 4, the beeswax clay 50 in the container 80 is large enough to immerse the entire core vent 20, but it is sufficient that the beeswax clay 50 fills at least the vent hole 21, and may be large enough to immerse the core vent 20 halfway. In that case, the core vent 20 may be placed directly on the bottom of the container 80 with the cavity forming surface 22 as the bottom surface, or the core vent 20 may be used as a cup to scoop up the beeswax clay and then similarly placed on the bottom of the container 80. In this embodiment, placing the core vent 20 in the container 80 containing molten beeswax clay corresponds to the immersion step of the present disclosure.

[0044] Next, as shown in Fig. 4(B), the core vent 20 is removed from the container 80. Specifically, the core vent 20 is placed on the metal plate 40 that has been cooled in advance, with the cavity forming surface 22 facing downward. This allows the beeswax clay 50 to harden more quickly than if it were to drip out of the vent hole 21. For the metal plate 40, it is preferable to use a tray or the like made of a material with good thermal conductivity, such as aluminum, in order to effectively cool it with the cooling agent 41.

[0045] Next, as shown in FIG. 4(C), the beeswax clay 50 is cooled and hardened. As described above, the metal plate 40 has already been cooled by the cooling agent 41, and the core vent 20 placed on the metal plate 40 and the beeswax clay 50 covering the core vent 20 are cooled. In other words, the beeswax clay 50 covers the entire surface of the core vent 20 and is solidified while being filled inside the vent hole 21. The beeswax clay 50 is a stable substance against the etching solution, so it functions as a thermoplastic resist during the etching process of the mold 11 and suppresses corrosion of the wall surface 24 of the vent hole 21. In this embodiment, placing the core vent 20 on the cooled metal plate 40 corresponds to the cooling process of the present disclosure.

[0046] Next, as shown in FIG. 4(D), the core vent 20 is transferred from the metal plate 40 to the steam passage 13 of the mold 11, and the core vent 20 is embedded in the steam passage 13. The specific embedding method may be the same as the conventional method, and in this way, the mold 11 in which the vent hole 21 of the core vent 20 is filled with the beeswax clay 50 can be obtained. Here, in the above-mentioned immersion process, the entire surface of the core vent 20 is covered with the beeswax clay 50. Among them, the beeswax clay 50 that is covered on the side surface 26 of the core vent is peeled off because the side surface 26 of the core vent and the wall surface 13a of the steam passage 13 are rubbed against each other during the embedding process. On the other hand, the beeswax clay 50 that remains in the minute gap 27 between the side surface 26 of the core vent and the wall surface 13a of the steam passage 13 without peeling off also plays a role in preventing the etching solution from entering the minute gap 27 in the etching process described later.

[0047] The mold 11 obtained by the above steps is subjected to an etching process. Before the etching process, in order to remove oil and foreign matter from the surface of the mold 11, for example, sandblasting is performed by a conventional method. Here, the entire surface of the core vent 20 is covered with beeswax clay 50. Among them, the coating on the cavity forming surface 22 of the core vent 20 can be easily removed by this sandblasting (the ventilation hole 21 can remain filled with beeswax clay 50 even after sandblasting). The process up to this point corresponds to the filling process of the present disclosure.

[0048] According to the mold manufacturing method of this embodiment, the cavity forming surface 22 of the core vent 20 can also be the target. The ventilation holes 21 of the core vent 20 are filled with beeswax clay 50, and while the inner wall 14 of the mold 11 and the cavity forming surface 22 of the core vent 20 are each corroded, the etching solution does not enter the ventilation holes 21, and there is no risk of the ventilation holes 21 being corroded.

[0049] For example, the entire inner wall 14 of the mold 11, including the cavity forming surface 22 of the core vent 20, can be embossed, or a cutting sheet with an arbitrary geometric pattern can be attached to form a resist, and then the resist can be contacted with an etching solution for processing.

[0050] After the etching process, the beeswax clay 50 in the vent hole 21 of the core vent 20 is made to disappear by heating. For example, the beeswax clay 50 can be dissolved in hot water by passing the mold 11 through a water tank filled with hot water. The beeswax clay 50 can also be dissolved and washed away by steam cleaning the mold 11. Steam cleaning is also performed after the etching process in the conventional mold manufacturing process, and since the beeswax clay 50 can be dissolved and washed together with the steam cleaning process, it is more preferable without the need to add a new process. In this embodiment, these actions correspond to the heating disappearance process of the present disclosure. This method can reduce costs by not requiring post-processing such as waste liquid treatment compared to the method of dissolving and cleaning with a chemical solvent.

[0051] For example, FIG. 5 is a diagram showing a mold manufactured by the mold manufacturing method of the present disclosure. As shown in FIG. 5(A), the texture processing can be continuously performed not only on the inner wall 14 of the mold 11 but also on the cavity forming surface 22 of the core vent 20. When focusing on the vent hole 21 of the core vent 20, it can be seen that corrosion is suppressed. Also, as shown in FIG. 5(B), a continuous geometric pattern can be applied from the inner wall 14 of the mold to the cavity forming surface 22 of the core vent 20. In this case, the vent hole 21 of the core vent 20 will blend well into the geometric pattern. Of course, it can be seen that corrosion is suppressed for the vent hole 21 of the core vent 20.

[0052] In this way, the inner wall 14 of the mold 11 and the cavity forming surface 22 of the core vent 20 have a continuous pattern, so that by molding a foamed resin material using the mold 11, a foamed resin material surface corresponding to that pattern can be obtained. Since the core vent marks are prevented from remaining dotted on the foamed resin material surface, the core vent marks are made less noticeable in the foamed resin material, and a foamed resin material with high designability can be produced. The use of the mold 11 to mold a foamed resin material corresponds to the foamed resin material manufacturing method of the present disclosure.

[0053] For example, Fig. 6 is a diagram showing a foamed resin material molded using a mold manufactured by the mold manufacturing method of the present disclosure. A geometric pattern corresponding to the mold of Fig. 5(B) is applied to the surface of the foamed resin material, and this geometric pattern extends over all areas except the convexity formed by the vent hole 21 of the core vent 20. In fact, even the convexity blends in well with the geometric pattern, to the extent that it cannot be distinguished from other patterns unless one looks carefully. It is possible to apply such a pattern because the cavity forming surface 22 of the core vent 20 is included in the target of the intaglio etching treatment, and a foamed resin material with a high design quality can be obtained.

[0054] Second embodiment of die manufacturing method Hereinafter, the mold manufacturing method according to the second embodiment will be described with reference to Fig. 7. The mold manufacturing method according to this embodiment is characterized in that the beeswax clay is filled only from the cavity forming surface side of the core vent, unlike the first embodiment. Note that the description of the matters already described in the second embodiment will be omitted as appropriate.

[0055] First, as shown in FIG. 7(A), the core vent 20 is placed on the metal plate 40 in a cup shape, that is, with the cavity forming surface 22 at the bottom. This closes the cavity forming surface 22 side of the vent hole 21. For the metal plate 40, it is preferable to use a tray or the like made of a material with good thermal conductivity such as aluminum, in anticipation of the cooling process described below. Also, although only one core vent 20 is shown in FIG. 7, multiple core vents 20 may be placed side by side, which improves workability since the process described below can be performed on many core vents 20 at once. Note that in this embodiment, placing the core vent 20 on the metal plate 40 with the cavity forming surface 22 at the bottom corresponds to the closing process of the present disclosure.

[0056] Next, as shown in Fig. 7(B), the back surface 23 of the cavity forming surface 22 of the core vent 20 placed in a cup shape is filled with beeswax clay 50. For example, it is desirable to take an appropriate amount of beeswax clay 50 with a finger or tweezers, place it on the back surface 23 of the cavity forming surface 22 of the core vent 20, and spread it over the entire surface. Note that beeswax clay 50 may be poured in so that it overflows from the upper opening of the core vent 20. In that case, in the injection process described later, the molten beeswax clay 50 will cover the side surface of the core vent, and the same effect as in the first embodiment can be obtained.

[0057] 7B shows only one core vent 20, but if there are multiple core vents 20, the multiple core vents 20 are arranged in an orderly fashion in, for example, N rows and M columns. Then, using an injection tool capable of simultaneously pouring beeswax clay 50 into the N rows (or M columns) of core vents 20, the injection process may be repeated for M columns (or N rows).

[0058] Next, as shown in FIG. 7(C), the beeswax clay 50 is heated and melted, and then injected into the vent hole 21. For example, by continuously applying hot air from a hot gun to the beeswax clay 50, the melted beeswax clay 50 drips into the vent hole 21 under its own weight, and thus injection is possible. In addition, as long as the beeswax clay 50 melts, for example, the metal plate 40 on which the core vent 20 is placed may be placed in a high-temperature room and left until it melts and drips. In this embodiment, the process of heating the beeswax clay 50 to drip into the vent hole 21 under its own weight corresponds to the injection process of the present disclosure.

[0059] Next, as shown in FIG. 7(D), the beeswax clay 50 is cooled and hardened. For example, if the metal plate 40 is cooled with a cooling agent 41 or the like, the heat of the core vent 20 placed on the plate is removed, and as a result, the beeswax clay 50 in the core vent 20 is also cooled. It may be left at room temperature and waited until it hardens. In this embodiment, cooling the metal plate 40 with the cooling agent 41 corresponds to the cooling step of the present disclosure. The steps up to this point correspond to the filling step of the present disclosure.

[0060] 7(E), the core vent 20 is transferred from the metal plate 40 to the steam passage 13 of the mold 11 and embedded therein. A conventional method may be used to obtain the mold 11 in which the ventilation holes 21 of the core vent 20 are filled with the beeswax clay 50. In this embodiment, removing the core vent 20 placed on the metal plate 40 corresponds to the opening step of the present disclosure.

[0061] As explained above, the beeswax clay 50 may drip into the vent hole 21 under its own weight. For example, the beeswax clay 50 that has been preheated and melted may be poured into the core vent 20 placed in a cup shape (only the amount necessary to fill the vent hole may be poured, or the amount may be poured until it overflows and protrudes from the upper opening of the core vent 20). At this time, the metal plate 40 is also cooled in advance, and the beeswax clay that drips into the vent hole 21 and reaches the surface of the metal plate 40 is immediately cooled and hardened by the cooled metal plate 40. In other words, the injection process and the cooling process can be performed simultaneously, which is expected to improve workability.

[0062] Third embodiment of die manufacturing method Next, a mold manufacturing method according to a third embodiment of the present disclosure will be described. The mold manufacturing method according to this embodiment is characterized in that, unlike the second embodiment, a core vent is embedded in the mold body and then filled with beeswax clay. Note that the description of the matters already described in the first embodiment will be omitted as appropriate.

[0063] First, as shown in Fig. 8(A), the core vent 20 is embedded in the steam passage 13 of the mold 11. As in the first embodiment, a conventional method may be used.

[0064] Next, as shown in Fig. 8(B), the cavity forming surface 22 side of the vent hole 21 of the core vent 20 is closed. Specifically, a sealant 42 is applied so as to cover the entire cavity forming surface 22 of the core vent 20. Any means may be used as long as the beeswax clay 50, which will be pressed in in a later step, does not come out. For example, the die 11 may be placed on a flat metal plate to close the cavity forming surface 22 without bothering to apply the sealant 42. In this embodiment, applying the sealant 42 to the cavity forming surface 22 corresponds to the closing step of the present disclosure.

[0065] 8(C), beeswax clay 50 is poured and filled onto the back surface 23 of the cavity forming surface 22 of the core vent 20. For example, it is desirable to take an appropriate amount of beeswax clay 50 with fingers or tweezers, place it on the bottom of the core vent 20, and spread it over the entire bottom surface.

[0066] Next, as shown in FIG. 8(D), the beeswax clay 50 is pressed into the vent hole 21 of the core vent 20. Specifically, the beeswax clay 50 is crushed from above with a cylinder 60 that corresponds to the inner diameter of the core vent 20 (the core vents 20 embedded in the steam passage 13 of the mold 11 do not all face the same direction, so the crushing direction is not necessarily from above). As a result, the beeswax clay 50 is pressed into the vent hole 21, but the sealing material 42 prevents the beeswax clay 50 from popping out from the surface of the core vent 20. In this embodiment, crushing the beeswax clay 50 with the cylinder 60 corresponds to the pressing step of the present disclosure. The steps up to this point correspond to the filling step of the present disclosure.

[0067] 8(E), the sealing material 42 is peeled off to open the closed vent hole 21 on the cavity forming surface side. In this manner, the mold 11 can be obtained in a state in which the vent hole 21 of the core vent 20 is filled with beeswax clay 50. In this embodiment, peeling off the sealing material 42 corresponds to the opening step of the present disclosure.

[0068] As explained above, the core vents 20 may be embedded one by one, the beeswax clay 50 may be placed on the back surface 23, and instead of applying the sealing material 42, the cavity forming surface 22 may be pressed in by pressing it with the cylinder 60 while pressing it with a finger. Since the degree of filling (whether the beeswax clay 50 has properly reached the cavity forming surface 22) can be visually checked every time the work is completed, the beeswax clay 50 can be filled without any omissions.

[0069] <Fourth embodiment of die manufacturing method> Next, a mold manufacturing method according to a fourth embodiment of the present disclosure will be described. The mold manufacturing method according to this embodiment is characterized in that the direction in which the beeswax clay is pressed into the vent hole of the core vent 20 is opposite to that in the second and third embodiments.

[0070] As shown in Fig. 9(A), first, the core vent 20 is placed so that the cavity forming surface 22 faces upward. That is, while in the first embodiment, it is placed like a cup, in this embodiment, it is placed in the opposite direction. Also, although only one core vent 20 is shown in Fig. 9, multiple core vents may be placed side by side, which improves workability since the process described below can be performed on many core vents at once.

[0071] Next, as shown in Fig. 9(B), beeswax clay 50 is placed and spread on the cavity forming surface 22 of the core vent 20. For example, in the case of one core vent 20, it is desirable to take an appropriate amount of beeswax clay 50 with fingers or tweezers, place it on the surface of the core vent 20, and spread it so that it spreads over the entire surface. If there are multiple core vents 20, for example, the multiple core vents 20 may be arranged in an orderly manner in N rows and M columns, and the beeswax clay 50 may be placed on the cavity forming surface 22 of the core vents 20 in N rows (or M columns) at the same time using a tool that can place the beeswax clay 50 on the cavity forming surface 22 of the core vents 20 in the N rows (or M columns), and the operation may be repeated for M rows (or N rows).

[0072] Next, as shown in FIG. 9(C), the beeswax clay 50 is pressed into the vent hole 21 of the core vent 20. Specifically, the beeswax clay 50 is pressed down with a finger from above. As a result, the beeswax clay 50 is pressed into the vent hole 21, but as long as it is possible to prevent the intrusion of the etching solution, it may be pressed in until the entire vent hole 21 is filled, or, for example, until half of the vent hole is filled. In this embodiment, pressing the beeswax clay 50 with a finger from above corresponds to the pressing step of the present disclosure. Note that, of the beeswax clay 50 placed on the surface of the core vent 20, the portion that is not pressed in remains on the surface of the core vent 20 as a residual portion 51.

[0073] Next, as shown in Fig. 9(D), the residual portion 51 on the surface of the core vent 20 is removed. Specifically, the surface of the core vent 20 is scraped with a spatula 70 to scrape off the residual portion 51. The residual portion 51 may be used to fill the next core vent 20. In this embodiment, scraping off the residual portion 51 corresponds to the removing step of the present disclosure. The steps up to this point correspond to the filling step of the present disclosure.

[0074] 9(E), the core vent 20 filled with beeswax clay is embedded in the steam passage 13 of the mold 11. As in the first embodiment, a conventional method may be used. In this manner, the mold 11 can be obtained in which the ventilation holes 21 of the core vent 20 are filled with beeswax clay 50.

[0075] Fifth embodiment of die manufacturing method Next, a mold manufacturing method according to a fifth embodiment of the present disclosure will be described. The mold manufacturing method according to this embodiment is characterized in that, unlike the fourth embodiment, a core vent is embedded in the mold body and then filled with beeswax clay.

[0076] First, as shown in Fig. 10(A), the core vent 20 is embedded in the steam passage 13 of the mold 11. As in the first embodiment, a conventional method may be used.

[0077] 10(B)-(D) of the subsequent process are the same as those of FIG. 9(B)-(D) of the fourth embodiment, and therefore the explanation will be omitted. It is also possible to press in the beeswax clay 50 and scrape it off with the spatula 70 each time a core vent 20 is embedded. This allows visual confirmation of the state of filling (whether the beeswax clay 50 is properly packed in the vent hole 21) each time the work is completed, so that the beeswax clay 50 can be filled without any omissions. In this way, the mold 11 can be obtained in a state in which the vent hole 21 of the core vent 20 is filled with the beeswax clay 50.

[0078] The above-mentioned embodiments have been described as the modes for carrying out the present disclosure. However, it is clear to those skilled in the art that various substitutions, modifications, or changes are possible without departing from the purpose of the present disclosure. In other words, the modes for carrying out the present disclosure may include all substitutions, modifications, or changes that do not depart from the spirit and purpose of the claims attached to this specification. For example, the following various modes can be adopted as modes for carrying out the present invention.

[0079] (1) In each of the above-described embodiments, wet etching is used as the intaglio etching process. However, in the intaglio etching process, it is sufficient that the beeswax clay filled in the vent holes of the core vent functions as a thermoplastic resist, and therefore dry etching, for example, may also be used.

[0080] (2) Although beeswax clay is used as the thermoplastic resist, other thermoplastic resists may be used as long as they are stable against the etching solution and etching gas.

[0081] (3) Although the core vent has been described with a drilled hole as an example of its vent shape, the same effect can be obtained with a vent hole having a slit shape. [Explanation of symbols]

[0082] 10. Foam resin molding equipment 11 Mold 11a Core type 11b Cavity type 12 Cavity 13 Steam passage 14 Inner wall 15a Core side steam in 15b Core side steam out 16a Steam in on cabinet side 16b Steam out from cabinet side 17 Raw material injection gun 20 Core Vent 21 Ventilation hole 22 Cavity forming surface 23 Back side 24 Wall 26 Core vent side 27 Gap 30 Foam resin molding materials 40 metal plate 41 Ice pack 42 Sealing material 50 Beeswax Clay 51 Residual 60 Cylinder 70 Spatula

Claims

1. A mold manufacturing method in which a core vent is embedded in a steam passage of a mold body, a necessary resist is applied, and then an etching intaglio process is performed, a step of filling the vent holes of the core vent with a thermoplastic resist before the intaglio etching process; a heating and removing step of removing the thermoplastic resist filled in the vent hole by the filling step after the etching intaglio processing, by heating; A mold manufacturing method comprising:

2. 2. The method of claim 1, wherein the thermoplastic resist is beeswax clay.

3. The filling step includes: a dipping step of dipping the core vent into the molten beeswax clay; a cooling step of cooling the beeswax clay coated on the core vent by the immersion step; The mold manufacturing method according to claim 2 , further comprising:

4. 3. The mold manufacturing method according to claim 1, wherein in the filling step, the thermoplastic resist is filled from a back side of the cavity forming surface in the core vent.

5. The filling step includes: a closing step of closing the vent hole on the cavity forming surface side of the core vent; an injection step of injecting the thermoplastic resist into the vent hole from a rear side of the cavity forming surface; a cooling step of cooling the thermoplastic resist injected into the vent hole; an opening step of opening the vent hole closed by the closing step; The mold manufacturing method according to claim 4, further comprising:

6. The filling step includes: a closing step of closing the vent hole on the cavity forming surface side of the core vent; a pressurizing step of pressurizing the thermoplastic resist into the vent hole from a side opposite to the cavity forming surface; an opening step of opening the vent hole closed by the closing step; The mold manufacturing method according to claim 4, further comprising:

7. 3. The mold manufacturing method according to claim 1, wherein in the filling step, the thermoplastic resist is filled from a cavity forming surface of the core vent.

8. The filling step includes: a pressurizing step of pressurizing the thermoplastic resist into the vent hole from the cavity forming surface side; a removing step of removing the thermoplastic resist remaining on the cavity forming surface of the core vent; The mold manufacturing method according to claim 7, further comprising:

9. A method for manufacturing a foamed resin material, comprising molding a foamed resin material using a mold produced by the mold manufacturing method described in any one of claims 1 to 8.

Citation Information

Patent Citations

  • Mold for in-mold foam-molding and manufacture thereof

    JP1990283428A

  • Mold for polyolefinic resin foam-molding

    JP1990283429A

  • METHOD FOR REPAIRING HOLE THROUGH METAL OBJECT

    JP1993239681A

  • Mold surfacing material and mold used for manufacturing in-mold foam molding

    JP1999058533A

  • Clay composition, manufacturing method therefor and molding kit

    JP2006064982A