Quality control method for die castings
Patent Information
- Application Number
- JP2020203192
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-12-08
- Publication Date
- 2024-09-26
- Estimated Expiration
- 2040-12-08
AI Technical Summary
【0016】 本発明によれば、鋳造不良や機会損失が発生する段階よりも前の初期状態の微妙な変化を精度良く検知でき、検知結果に基づいて、鋳造品質の変化や機会損失の兆候を数値化して予測する品質管理方法により、鋳造品の品質安定化と鋳造運転の安定稼働の予防管理が確実にできる。
Smart Images

Figure 0007556278000005 
Figure 0007556278000004 
Figure 0007556278000006
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for quality control of cast products produced by a die casting machine or the like. [Background technology]
[0002] In casting using a die casting machine, molten metal supplied inside an injection sleeve is injected and filled into a die cavity by the forward movement of a plunger tip set at a predetermined injection speed and casting pressure.
[0003] However, the injection sleeve is heated and deformed by the high temperature molten metal, and the sliding resistance between the injection sleeve and the plunger tip increases, which can cause the movement of the plunger tip to become unstable. In addition, the sliding resistance can vary greatly due to the adhesion of molten metal residues caused by the solidification of the molten metal to the inside of the injection sleeve. Furthermore, wear of the plunger tip can increase the gap between the injection sleeve, increasing the penetration of the molten metal and promoting the accumulation of molten metal residues, which can result in even greater fluctuations in the sliding resistance.
[0004] These large fluctuations in sliding resistance cause fluctuations in the injection speed and casting pressure, which causes the molten metal to ripple and become unstable during injection filling, inducing casting defects such as air entrapment (voids), poor molten metal wrinkles, poor molten metal flow, etc. In addition, when molten metal residues accumulated inside the injection sleeve peel off and mix with the molten metal, they cause new casting defects such as blowholes and foreign matter contamination. Furthermore, due to frequent casting defects and excessive wear on the plunger tip and injection sleeve that interferes with the normal operation of the die casting machine, casting operations must be stopped for recovery work such as part replacement, resulting in a significant drop in productivity (opportunity loss).
[0005] Here, because the origin of casting defects and opportunity loss is the change in the sliding resistance between the injection sleeve and the plunger tip, it has been proposed to detect the change in this sliding resistance with high accuracy.Furthermore, it is desirable to combine the prediction of the change in casting quality with the prediction of the life until the opportunity loss occurs, leading to quality control (preventive control) that stabilizes the quality of cast products and ensures stable operation of casting operations. For example, Patent Document 1 and Patent Document 2 disclose that the change in sliding resistance is detected from the fluctuation of the operating oil pressure (casting pressure) of the hydraulic cylinder or the like that controls the plunger tip during the injection filling process. Also, Patent Document 3 discloses that the change in sliding resistance is detected from the fluctuation of the moving speed (injection speed) of the plunger tip during the injection filling process. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Special Publication No. 60-2952 [Patent Document 2] Japanese Patent Application Publication No. 3-32460 [Patent Document 3] Japanese Patent Application Publication No. 2-303667 Summary of the Invention [Problem to be solved by the invention]
[0007] In order to realize preventive management by predicting changes in casting quality and the lifespan until mechanical loss occurs, it is preferable to detect changes in sliding resistance at timing appropriate to the purpose. For example, in the preventive management of casting defects such as blowholes and foreign matter contamination, in order to accurately grasp the generation, accumulation and peeling of molten metal residue, the correct timing for detection is when there is no molten metal that causes direct contact between the plunger tip and the injection sleeve. In other words, it should be performed within the range of the plunger tip's retraction movement in preparation for the next shot after the injection filling process is completed. Furthermore, even when grasping the degree of wear of the plunger tip or injection sleeve, the detection can be performed with high accuracy by performing the detection within the range of the retraction movement of the plunger tip when there is no molten metal. In contrast, the detection timing shown in Patent Documents 1 to 3 is set to be within the range of forward movement of the plunger tip that injects and fills the mold cavity with molten metal. Because molten metal is present, disturbance factors such as thermal deformation of the injection sleeve due to high temperature molten metal, thermal softening of molten metal residue, and the weight of the molten metal are included, so the inspection accuracy of only molten metal residue is greatly reduced, and this is an unfavorable state for preventive management of casting defects such as blowholes and foreign matter contamination.
[0008] In addition, in the preventive management of casting defects such as air entrapment, poor molten metal wrinkles, and poor molten metal flow caused by fluctuations in the injection speed and casting pressure during the injection filling process, the correct timing for detection is within the range of forward movement of the plunger tip where molten metal is present. Here, the detection means shown in Patent Documents 1 to 3 are said to detect the injection speed and casting pressure at the timing of the forward movement of the plunger tip where the molten metal is present, but a sensor is placed in the drive unit such as a hydraulic cylinder downstream of the control, and the fluctuations in the injection speed and casting pressure are measured based on the signal information from the sensor. Therefore, it is difficult to completely solve problems such as errors due to temperature changes of the hydraulic oil and false detection due to sensor failure. Furthermore, when the injection speed and casting pressure fluctuate, the quality of the casting product has already fluctuated, so this cannot be considered preventive management.
[0009] The present invention has been made in consideration of the above problems, and relates to a quality control method for castings in a die casting machine, which aims to perform preventive management by combining prediction of changes in casting quality and prediction of the life until mechanical loss occurs by detecting minute changes in sliding resistance, which is the initial state before casting defects or opportunity loss occur, by selecting the detection timing of the retraction and advancement movements of the plunger tip according to the purpose. [Means for solving the problem]
[0010] The present invention provides a first means for solving the above problems, A quality control method for a die-cast product, comprising the steps of: supplying molten metal into an inside of an injection sleeve at a standby position after a plunger tip disposed in an injection sleeve is moved backward; and completing injection and filling of the molten metal into a die cavity at an injection completion position after a plunger tip is moved forward; A detection section is set within the moving range of the plunger tip's retraction operation, and a sliding resistance discriminating device is provided which continuously samples the sliding resistance between the plunger tip and the injection sleeve within the detection section and discriminates the quality of the sliding resistance for each shot during actual casting by comparing it with the sliding resistance during casting of a good product previously sampled, and the quality of the actual casting for each shot is discriminated based on the evaluation results of the sliding resistance discriminating device. According to the first means, by directly detecting the sliding resistance in the absence of molten metal, it is possible to perform preventive management by accurately predicting signs of changes in casting quality and opportunity losses.
[0011] As a second means for solving the above problem, the present invention provides a method for manufacturing a semiconductor device comprising the steps of: The detection section is the range from the injection completion position to the standby position. According to the second means, by accurately detecting the state of the molten metal residue in the injection sleeve and the wear state of the plunger tip and the injection sleeve, it is possible to reliably perform preventive management of casting defects such as blowholes and foreign matter contamination, and preventive management to avoid machine losses due to sudden production stoppages.
[0012] As a third means for solving the above problems, the present invention provides a method for manufacturing a semiconductor device according to any one of the first and second means, The sliding resistance is used as a control command value for an electrically controlled hydraulic servo valve system that controls the forward and backward movements of the plunger tip. According to the third means, it is possible to improve the accuracy of preventive management by eliminating disturbance factors such as changes in oil temperature and failures of sensors, and by accurately detecting even small changes in the initial state before mechanical abnormalities such as casting defects and wear occur.
[0013] As a fourth means for solving the above problems, the present invention provides a method for manufacturing a semiconductor device according to any one of the first and third means, The present invention further includes the step of collecting the sliding resistance during the forward movement of the plunger tip, and arbitrarily setting the detection range within the range of the injection completion position starting from the standby position. According to the fourth means, by detecting the sliding resistance in the presence of molten metal, it is possible to prevent and control casting defects such as air entrapment, poor molten metal wrinkles, and poor molten metal running caused by the injection filling operation.
[0014] As a fifth means for solving the above problems, the present invention provides a method for manufacturing a semiconductor device according to any one of the first to fourth means, The sliding resistance discrimination device displays the position of the plunger tip and the control command value in the detection section as waveforms, superimposes the conforming product waveform when a conforming product is cast and the casting waveform when an actual cast is performed, calculates the total area of the deviating waveforms, and compares it with a preset judgment standard area to judge the quality of the actual cast product for each shot. According to the fifth means, the prediction accuracy can be improved and highly accurate preventive management can be performed by quantifying the signs of changes in casting quality and opportunity losses. Furthermore, by identifying abnormal parts of the injection sleeve and predicting the replacement time, the machine loss due to sudden production stop can be minimized.
[0015] As a sixth means for solving the above problems, the present invention provides a method for manufacturing a semiconductor device according to any one of the first to fifth means, When the quality of the actual casting is judged to be poor, the sliding resistance discriminator issues a warning alarm and starts counting the number of warning alarms. When the count exceeds a preset number, the actual casting operation is stopped and a danger alarm is issued. According to the sixth means, by classifying the castings for each shot (good, inspection required, defective) and quantifying the signs of changes in casting quality and opportunity loss, it is possible to stabilize the quality of the castings and perform preventive management to ensure stable operation of the casting process. Effect of the Invention
[0016] According to the present invention, it is possible to accurately detect subtle changes in the initial state before casting defects or opportunity losses occur, and by using a quality control method that quantifies and predicts changes in casting quality and signs of opportunity losses based on the detection results, it is possible to reliably stabilize the quality of cast products and perform preventive management to ensure stable operation of casting operations. [Brief description of the drawings]
[0017] [Figure 1] FIG. 2 is a conceptual diagram of an injection device of the die casting machine of the present invention. [Diagram 2] FIG. 11 is a waveform diagram showing sliding resistance during a plunger tip retraction operation. [Diagram 3] FIG. 11 is a process flow diagram for the plunger tip retraction operation. [Figure 4] FIG. 11 is a waveform diagram showing sliding resistance during forward movement of the plunger tip. [Diagram 5] FIG. 11 is a flow diagram of a process for a plunger tip retraction operation. [Figure 6] FIG. 2 is a configuration diagram of a sliding resistance determining device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will be described in detail with reference to the drawings. (Outline of die casting machine configuration) The die casting machine 1 shown in FIG. 1 includes a fixed mold 2 supported by a fixed platen (not shown), a movable mold 3 supported by a movable platen (not shown) and movable toward and away from the fixed platen 2, an injection device 10 that injects molten metal, an injection control unit 20 that controls the operation of the injection device 10, and a sliding resistance determination device 30 that includes part of the processing module of the injection control unit 20. Molten metal such as aluminum or an aluminum alloy is injected by an injection device 10 into a mold cavity 4 between a fixed mold 2 and a movable mold 3 to fill the mold cavity 4, thereby producing a casting.
[0019] (injection device) The injection device 10 includes an injection sleeve 11 into which molten metal is supplied, a plunger tip 12 inside the injection sleeve 11 that can move forward and backward relative to the injection sleeve 11, a plunger rod 13 connected to the plunger tip 12, and a drive source such as a hydraulic cylinder 14 connected to the plunger rod 13 and driving the plunger tip 12. Regarding the movement of the plunger tip 12 of the injection device 10, the movement toward the side F closer to the mold cavity 4 is defined as the "forward movement", the movement toward the side B farther from the mold cavity 4 is defined as the "rearward movement", the completion position of the rearward movement of the plunger tip 12 is defined as the "standby position BE", and the completion position of the forward movement of the plunger tip 12 is defined as the "injection completion position FE". In other words, the plunger tip 12 advances and retreats in the front-rear direction D1 between the standby position BE and the injection completion position FE.
[0020] (Injection sleeve) The injection sleeve 11 is a cylindrical body supported horizontally in a state where it protrudes rearward from a fixed platen (not shown). The axial direction of the injection sleeve 11 coincides with the front-rear direction D1. The front side of the injection sleeve 11 penetrates the fixed platen so as to communicate with the mold cavity 4, and is fastened to a predetermined position of the fixed mold 2. A through-hole pouring port 15 is provided on the rear side of the injection sleeve 11. When the plunger tip 12 is waiting at the waiting position BE, molten metal is poured into the inside of the injection sleeve 11 through the pouring port 15 from a molten metal supply device or the like (not shown). If necessary, the injection sleeve 11 is provided with a cooling mechanism (not shown) including a flow path through which a cooling medium such as water flows. In addition, it is preferable to apply a lubricant to the sliding surfaces of the injection sleeve 11 and the plunger tip 12 in order to prevent wear damage to the plunger tip 12, stabilize the sliding state, and suppress adhesion of molten metal residue.
[0021] (plunger tip) The plunger tip 12 has a cylindrical shape that pushes the molten metal in the injection sleeve 11 forward to inject and fill the mold cavity 4, and has an appropriate gap with the injection sleeve 11. In other words, the gap is precisely adjusted so that the molten metal does not leak, the injection sleeve 11 and the plunger tip 12 do not stick to each other, and the plunger tip 12 can move forward and backward smoothly. The plunger rod 13 is an intermediate body that connects the plunger tip 12 and the hydraulic cylinder 14, and transmits the drive of the hydraulic cylinder 14 to the plunger tip 12. In addition, the plunger tip 12 is provided with a water cooling mechanism including a flow path through which a cooling medium such as water flows.
[0022] (Injection control device) The injection control device 20 is connected to the hydraulic cylinder 14, and controls the drive of the hydraulic cylinder 14 to control the forward or backward movement of the plunger tip 12 via the plunger rod 13. In particular, the forward movement of the plunger tip 12 is an important operation that directly affects the quality of the casting, since it is an operation for injecting and filling the molten metal in the injection sleeve 11 into the mold cavity 4. The injection filling operation is composed of a multi-stage forward speed (injection speed) of the plunger tip 12 to accurately fill the molten metal in the injection sleeve 11 into the mold cavity 4, and a multi-stage casting pressure to accurately cool and solidify the molten metal in the filled mold cavity 4. Therefore, it is preferable to use a control device equipped with an electrically controlled hydraulic servo valve system that is optimal for highly accurate control of the multi-stage injection speed and casting pressure as the injection control device 20.
[0023] (Sliding resistance determination device) The sliding resistance determination device 30 calculates the sliding resistance between the plunger tip 12 and the injection sleeve 11 and determines whether it is good or bad based on information on the control command value of the injection control device 20 that controls the drive of the hydraulic cylinder 14. The sliding resistance determination device 30 is composed of a signal input unit 31, a waveform display unit 32, a detection range setting unit 33, a calculation unit 34, a determination unit 35, and an alarm transmission unit 36, as shown in Figure 2.
[0024] Here, with the conventional method (galling detection) of detecting changes in sliding resistance by measuring the fluctuations in injection speed and casting pressure based on the signal information from a sensor placed in the driving part of a hydraulic cylinder or the like downstream of the control, it is difficult to completely solve the problems of errors due to temperature changes of the hydraulic oil and false detection due to sensor failure. Furthermore, when the injection speed or casting pressure changes, the quality of the casting has already changed, so this cannot be considered preventive management.
[0025] In contrast, the present invention uses the control command value of the injection control device 20, which is the most upstream control, to realize highly accurate detection of changes in sliding resistance without problems such as errors and false detections. Also, by being able to accurately detect even extremely minute changes in sliding resistance before abnormal phenomena occur in fluctuations in injection speed and casting pressure, preventive management can be performed at an early stage before mechanical abnormalities such as casting defects and wear occur.
[0026] Furthermore, the timing for detecting the sliding resistance during a series of operations in the casting operation is preset in the sliding resistance determining device 30. For example, in the preventive management of casting defects such as blowholes and foreign matter contamination, in order to accurately grasp the generation, accumulation, and peeling of molten metal residue, detection is performed in a state where there is a high probability of direct contact between the plunger tip 12 and the injection sleeve 11. Also, in order to grasp the degree of wear of the plunger tip 12 and the injection sleeve 11, a state where there is no molten metal is preferable. In other words, it is correct to set the range of the retraction movement of the plunger tip 12 in preparation for the next shot after the injection filling process is completed. In addition, in the preventive management of casting defects such as air entrapment, poor molten metal wrinkles, and poor molten metal flow caused by fluctuations in the injection speed and casting pressure during the injection filling process, the range is set within the range of injection filling of the molten metal into the mold cavity 4 by the forward movement of the plunger tip 12 when molten metal is present. In this way, by detecting changes in sliding resistance at timing appropriate to the purpose, it is possible to ensure preventive management by predicting changes in casting quality and the lifespan until mechanical damage occurs.
[0027] (Sliding resistance waveform: during backward movement) The procedure for detecting the sliding resistance at the timing of the retraction movement of the plunger tip 12 and performing preventive management will be described with reference to FIGS. 3 shows the waveform of the retraction movement of the plunger tip 12 in preparation for the next casting shot after injection filling is completed. When the signal input unit 31 of the sliding resistance discriminator 30 receives the control command value of the injection control unit 20, the control command value waveform is displayed on the waveform display unit 32. The horizontal axis of the waveform can be selected to represent either the position of the plunger tip 12 or the time elapsed since the start of retraction. For example, if you want to identify an abnormal part of the injection sleeve 11, it is preferable to select the position of the plunger tip 12. The range from the injection completion position FE of the plunger tip 12 to the standby position BE is displayed.
[0028] The vertical axis of the waveform is the control command value of the injection control device 20, and represents the sliding resistance between the plunger tip 12 and the injection sleeve 11 during the retraction movement. Here, by using the injection control device 20 as a control device equipped with an electrically controlled hydraulic servo system, the resolution of the control command value from the injection control device 20 is increased, and even small changes in sliding resistance can be detected with high accuracy. This makes it possible to accurately detect even small changes in the initial state before abnormal phenomena such as casting defects and wear occur, thereby enabling accurate prediction of changes in casting quality and prediction of the life until mechanical loss occurs. An electrically controlled hydraulic servo system is a control device that can precisely control the flow rate of hydraulic oil in hydraulic devices such as hydraulic cylinders. The flow rate of hydraulic oil is controlled by the position of an adjustment rod called a spool, and the position of the spool is driven by a connected servo motor. Therefore, the control command value 20 uses the "spool position control current value" for the servo motor that drives the spool position. Alternatively, if the control device has a function for monitoring the spool position, it is preferable to select the "spool monitor display value" as the control command value 20.
[0029] The dashed line in the waveform in Fig. 3 is a waveform of sliding resistance (reference value waveform 301) obtained in advance when a good product is cast. In Fig. 3, it is shown by a single dashed line for ease of understanding, but it is also possible to accumulate waveform data from multiple good product castings and show a range of good product castings including upper and lower limits. Alternatively, the waveform data when a casting defect occurs may be set as a limit value, and this limit value or the limit value may be multiplied by a safety factor to show a safety range in which a good product is reliably cast. Alternatively, data obtained during no-load operation after maintenance such as disassembly and cleaning may be used.
[0030] Next, a range in which the sliding resistance is to be evaluated based on the waveform displayed on the waveform display unit 32 is set as a detection range 302 by the detection range setting unit 33 according to the purpose. For example, when performing preventive management of casting defects such as blowholes and foreign matter contamination, a range is set in which the generation, accumulation, and peeling of molten metal residue that causes casting defects may occur. In other words, since the entire range in the injection sleeve 11 that comes into contact with the molten metal is a possibility, it is preferable to set the entire range from the injection completion position FE to the standby position BE. It is also preferable to set the entire range from the injection completion position FE to the standby position BE when performing preventive management by detecting damage such as localized wear in the injection sleeve 11, or looseness of mechanical parts of the injection device 10 including the hydraulic cylinder 14 and the plunger rod 13. If the location of the abnormality is known in advance, it is also possible to set the range only to a localized range including the abnormality.
[0031] The solid line in the waveform shown in Fig. 3 is the waveform of the sliding resistance of the backward movement in one shot of actual casting during continuous operation (actual casting waveform 303). By overlaying the waveform with the reference value waveform 301, it becomes clear whether there is a deviation between the reference value waveform 301 and the actual casting waveform 303 and the degree of the deviation. The calculation unit 34 uses a technique such as binarization processing to digitize the sum of the areas of the deviation parts of the overwritten waveforms within the range of the detection section 302 set by the detection section setting unit 33 (the area surrounded by the shaded area in Figure 3) as deviation area 303a, and transmits the data to the discrimination unit 35. The discrimination unit 35 receives the data sent from the calculation unit 34, and compares it with a preset judgment reference area to discriminate the quality of the cast product of one actual casting shot and predict the quality of the cast product of the next shot. By continuously performing this flow of information processing during continuous operation, the quality discrimination and quality prediction of the cast product for each actual casting shot during continuous operation are continuously performed. This makes it possible to convert changes in the casting quality into data, and to predict changes in the casting quality from the next shot onwards and to predict the life until mechanical loss occurs.
[0032] Here, the judgment reference area is an area obtained by multiplying the area of the width indicated by the upper and lower limits of a good casting obtained by accumulating waveform data of a plurality of good castings by a safety factor. Alternatively, the judgment reference area is an area indicating a safe range in which a good casting can be reliably obtained by multiplying the limit value or the limit value by a safety factor, with the waveform data when a casting defect due to peeling of the molten metal residue being set as a limit value. In other words, by making a judgment at the time of a minute change before a state in which a casting defect such as a blowhole or foreign matter contamination related to the molten metal residue has already occurred, or before a state in which a mechanical loss is suspected in the injection device such as the plunger tip 12 or the injection sleeve 11, it is possible to prevent abnormal situations such as defective products being mixed in with good products or production being stopped.
[0033] In addition, the discrimination unit 35 can predict the quality of the cast product of the next actual casting shot using the data of the maximum value 303b of the deviation between the reference value waveform 301 and the actual casting waveform 303. For example, the waveform when a clear casting defect or mechanical loss occurs is set as the reference value waveform 301, and when it is detected that the maximum value 303b exceeds the maximum value of the reference value waveform 301, the discrimination unit 35 can instantly determine that an abnormality has occurred as a sudden event, and prevent fatal mechanical loss such as production stoppage. Alternatively, the average value of the upper and lower limits of good casting obtained by accumulating data of multiple good castings is set as the reference average value 303c, and the number of times that the numerical value of the waveform of one actual casting shot exceeds the reference average value 303c can be counted, thereby making it possible to predict the tendency of change in the quality of the cast product and the life expectancy of mechanical loss.
[0034] (Process flow: During backward movement) 4 shows the processing flow of the sliding resistance determination device 30 during the retraction of the plunger tip 12. When the injection filling casting is completed, the hydraulic cylinder 14 is driven by the injection control unit 20, and the plunger tip 12 starts retracting at a set speed, and when the plunger tip 12 reaches the standby position BE, the retraction stops.
[0035] The control command value from the injection control unit 20 in the entire range from the start of retreat (injection completion position FE) to the end of retreat (standby position BE) is displayed as a waveform on the waveform display unit 32 via the signal input unit 31 (waveform measurement). The waveform of the detection section 302 set in the detection section setting unit 33 is extracted, and after a digitalization process is performed in the calculation unit 34, a discrimination process is performed in the discrimination unit 35 (waveform analysis).
[0036] The discrimination unit 35 performs a two-stage discrimination process. The first stage of discrimination process compares two waveforms, a reference value waveform 301 and an actual casting waveform 303, within the range of the detection section 302, and calculates, for example, a deviation area 303a (analysis result B1). The analysis result B1 is compared with a preset judgment reference area (reference value A1), and if A1≦B1, it is judged as "inspection required" and information on the discrimination result is sent to the alarm transmission unit 36. The alarm transmission unit 36 issues an alarm and at the same time starts counting the number of alarm signals from the discrimination unit 35. Note that inspection is required when the change in sliding resistance is so slight that it is difficult to clearly predict whether the quality of the casting for the next shot will be good or bad. The casting will be temporarily stored and will be re-evaluated for quality after the results of the next shot have been confirmed. If the judgment result of the judgment unit 35 is A1>B1, the casting is judged as a non-defective product C1 and stored as a non-defective product, and continuous casting is continued.
[0037] Furthermore, in the alarm issuing unit 36, the counted number of alarms E1 is compared with a preset reference number D1, and if D1≦E1, the alarm issuing unit 36 issues an abnormality judgment G1 and takes measures to stop the continuous casting operation (second stage judgment process). This abnormality judgment G1 indicates that the probability of obtaining a non-defective product even if continuous casting is continued further has extremely decreased, and suggests that the casting conditions of injection filling, such as the injection speed and casting pressure, should be reviewed, and that cleaning and maintenance of the injection device 10, including the injection sleeve 11 and plunger tip 12, should be performed. Alternatively, it suggests that there is a high probability of fatal mechanical loss, such as a breakdown of the injection device 10, and that maintenance measures, such as part replacement, are required early. In this way, by using the discrimination process of counting the number of alarms, small changes in the casting quality and the injection unit can be predicted, and stable production can be continued by systematically readjusting the casting conditions and carrying out simple maintenance of the injection unit. In addition, it is possible to predict the occurrence of fatal machine losses such as failure of the injection unit, thereby ensuring preventive management such as arranging replacement parts in advance. Here, it is preferable that the reference number of times D1 is set in combination with the reference value A1 depending on the content of the required preventive control. For example, when the stabilization of the casting quality is given top priority, the reference value A1 is set strict and the reference number of times D1 is set low. If the discrimination result of the discrimination unit 35 is D1>E1, the continuous casting will continue, but the cast product will be temporarily stored as a product requiring inspection, and will be subjected to a new quality judgment after the discrimination result of the next shot is confirmed.
[0038] (Sliding resistance waveform: forward movement) The procedure for detecting the sliding resistance at the timing of the forward movement of the plunger tip 12 and performing preventive management will be described with reference to FIGS. Figure 5 shows the waveforms of the sliding resistance in the injection filling process. The control command value, waveform display, and calculation processing are the same as in Figure 3, so the differences from Figure 3 will be mainly explained. The horizontal axis of the waveform can be selected to represent either the position of the plunger tip 12 or the time elapsed since the start of injection. The standby position BE is the position of the plunger tip 12 where the molten metal is poured from the pouring port 15 into the injection sleeve 11. The injection completion position FE is the forward position where the plunger tip does not move forward any further after the injection filling process is completed. The vertical axis of the waveform is the control command value of the injection control device 20, and represents the sliding resistance between the plunger tip 12 and the injection sleeve 11 during forward movement. The difference from FIG. 3 is that it is expressed as the sliding resistance including the state in which the molten metal is present inside the injection sleeve 11 and the mold cavity 4 as the plunger tip 12 moves forward. As a result, small changes in the sliding resistance during the injection filling process represent slight changes in the quality of the casting related to the injection filling process, and preventive management can be performed by predicting changes in the casting quality. Furthermore, the accuracy of preventive management is increased by using the control command value of an electrically controlled hydraulic servo system.
[0039] As shown in Figure 5, the injection filling process generally involves a combination of an injection speed control range that combines low-speed injection and high-speed injection, and a casting pressure control range for high-pressure filling that increases the filling pressure to reliably compensate for the solidification shrinkage of the molten metal. The dashed line in the waveform shown in Fig. 5 is a waveform of sliding resistance (reference value waveform 401) when a good product is cast, which was collected in advance. In Fig. 5, it is shown by a single dashed line for ease of understanding, but it may be possible to accumulate waveform data when multiple good products are cast and show a range of good products including upper and lower limits. Alternatively, it may be possible to show the waveform data when a casting defect occurs as a limit value, and show this limit value or a safety range by multiplying the limit value by a safety factor to ensure that a good product is cast.
[0040] The detection section 402 is selected and set according to the purpose of detection, etc. For example, when casting defects related to the injection flow of the molten metal, such as air entrapment, wrinkles, and poor running, are problematic, two sections, low-speed injection and high-speed injection, are set. In addition, when it is desired to grasp the cooling and solidification process of the molten metal, such as blowholes and sink marks, it is preferable to set two ranges, high-speed injection and high-pressure filling. When it is desired to check all defects, including the inclusion of foreign matter, the entire range from the waiting position BE to the injection completion position FE may be set. In FIG. 5, the low-speed injection section, which is likely to show large fluctuations in sliding resistance and is likely to induce casting defects, is set as the detection section 402.
[0041] 5 is the waveform of the sliding resistance of the forward movement in one shot of actual casting during continuous operation (actual casting waveform 403). By displaying it overlaid on the reference value waveform 401, it becomes clear whether there is a deviation between the reference value waveform 401 and the actual casting waveform 403 and the degree of the deviation. The calculation unit 34 uses a technique such as binarization processing to digitize the sum of the areas of the deviation parts of the overwritten waveforms within the range of the detection section 402 set by the detection section setting unit 33 (the area surrounded by the shaded area in Figure 5) as deviation area 403a), and transmits the data to the discrimination unit 35. The discrimination unit 35 receives the data sent from the calculation unit 34, and compares it with a preset judgment reference area to discriminate the quality of the cast product of one actual casting shot and predict the quality of the cast product of the next shot. By continuously performing this flow of information processing during continuous operation, the quality discrimination and quality prediction of the cast product for each actual casting shot during continuous operation are continuously performed. This makes it possible to convert changes in the casting quality into data, and to predict changes in the casting quality from the next shot onwards and to predict the life until mechanical loss occurs.
[0042] Here, the judgment reference area is an area obtained by multiplying the area of the width indicated by the upper and lower limits of a good casting obtained by accumulating waveform data of a plurality of good castings by a safety factor. Alternatively, the waveform data when a casting defect occurs due to injection filling is set as a limit value, and this limit value or the limit value is multiplied by a safety factor to indicate an area indicating a safe range in which a good casting can be reliably obtained. In other words, by making a judgment at a time of minute change before the state in which the casting quality has already been affected by fluctuations in the injection speed or casting pressure, or before the state in which mechanical damage is suspected in the injection device such as the plunger tip 12 or the injection sleeve 11 due to thermal deformation of the injection sleeve or friction with molten metal residue, it is possible to prevent abnormal situations such as defective products being mixed in with good products or production being stopped.
[0043] In addition, the discrimination unit 35 can predict the quality of the cast product of the next actual casting shot using the data of the maximum value 403b of the deviation between the reference value waveform 401 and the actual casting waveform 403. For example, the waveform when a clear casting defect or mechanical loss occurs is set as the reference value waveform 401, and when it is detected that the maximum value 403b exceeds the maximum value of the reference value waveform 401, the discrimination unit 35 can instantly determine that an abnormality has occurred as a sudden event, and can prevent fatal mechanical loss such as production stoppage. Alternatively, the average value of the upper and lower limits of good casting obtained by accumulating data of multiple good castings is set as the reference average value 403c, and the number of times that the numerical value of the waveform of one actual casting shot exceeds the reference average value 403c can be counted, thereby making it possible to predict the tendency of change in the quality of the cast product and the life expectancy of mechanical loss.
[0044] Although the range of low speed injection has been described as the detection range 402, the same applies even if the range of the detection range is changed. Note that the entire range from low speed injection to high pressure filling may be judged together. Alternatively, each range may be classified and judged, and a judgment may be made with priority given to the form of casting defects, concerns about mechanical loss, etc.
[0045] (Process flow: forward movement) 6 shows a processing flow of the sliding resistance determination device 30 during the forward movement of the plunger tip 12. Note that the start is a state in which molten metal is poured into the injection sleeve 11 and the plunger tip 12 is waiting at the waiting position BE. When the injection filling process begins, the hydraulic cylinder 14 is driven by the injection control unit 20, and the plunger tip 12 moves forward at the set injection speed and casting pressure of low-speed injection, high-speed injection, or high-pressure filling.When the injection filling of the molten metal into the mold cavity 4 is completed, the forward movement of the plunger tip 12 stops at the injection completion position FE.
[0046] The control command value from the injection control unit 20 in the entire range from the start of injection (standby position BE) to the end of injection (injection completion position FE) is displayed as a waveform on the waveform display unit 32 via the signal input unit 31 (waveform measurement). The waveform of the detection section 302 set in the detection section setting unit 33 is extracted, and after a digitization process is performed in the calculation unit 34, a discrimination process is performed in the discrimination unit 35 (waveform analysis).
[0047] The discrimination unit 35 performs a two-stage discrimination process. In the first stage, the two waveforms, the reference value waveform 401 and the actual casting waveform 403, within the detection section 402 are compared to calculate, for example, the deviation area 403a (analysis result B2). The analysis result B2 is compared with a preset judgment reference area (reference value A2), and if A2≦B2, it is judged as "inspection required" and information on the discrimination result is sent to the alarm issuing unit 36. The alarm issuing unit 36 issues an alarm and at the same time starts counting the number of alarm signals from the discrimination unit 35. Note that inspection is required when the change in sliding resistance is so slight that it is difficult to clearly determine whether the quality of the casting is good or bad. The casting will be temporarily stored and will be re-evaluated for quality after the results of the next shot are confirmed. If the judgment result of the judgment unit 35 is A2>B2, the casting is judged as a non-defective product C2 and stored as a non-defective product, and continuous casting is continued.
[0048] Furthermore, in the alarm issuing unit 36, the counted number of alarms E2 is compared with a preset reference number D2, and if D2≦E2, the alarm issuing unit 36 issues an abnormality determination G2 and takes measures to stop the continuous casting operation (second stage discrimination process). This abnormality judgment G2 indicates that the probability of obtaining a non-defective product even if continuous casting is continued further has dropped significantly, and suggests that the casting conditions for injection filling, such as the injection speed and casting pressure, should be reviewed, and that cleaning and maintenance of the injection device 10, including the injection sleeve 11 and plunger tip 12, should be performed. Alternatively, it suggests that there is a high probability of fatal mechanical loss, such as a breakdown of the injection device 10, and that maintenance measures, such as part replacement, are required early. In this way, by using the discrimination process of counting the number of alarms, small changes in the casting quality and the injection unit can be predicted, and stable production can be continued by systematically readjusting the casting conditions and carrying out simple maintenance of the injection unit. In addition, it is possible to predict the occurrence of fatal machine losses such as failure of the injection unit, thereby ensuring preventive management such as arranging replacement parts in advance. Here, it is preferable that the reference number of times D2 is set in combination with the reference value A2 depending on the content of the required preventive control. For example, when the stabilization of the casting quality is given top priority, the reference value A2 is set strict and the reference number of times D2 is set low. If the discrimination result of the discrimination unit 35 is D2>E2, the continuous casting is continued, but the cast product is temporarily stored as a product requiring inspection, and the quality is judged again after the discrimination result of the next shot is confirmed.
[0049] In addition to the above, the configurations given in the above embodiments can be selected or appropriately changed to other configurations without departing from the spirit of the present invention. [Explanation of symbols]
[0050] 1. Die casting machine 2 Fixed mold 3 Movable mold 4 Mold Cavity 10 Injection device 11 Injection sleeve 12 Plunger Tip 13 Plunger rod 14 Hydraulic cylinder 15 Pouring spout 20 Injection control device 30. Sliding resistance determination device 31 Signal input section 32 Waveform display section 33 Detection section setting section 34 Arithmetic section 35 Discrimination part 36 Alarm Transmission Unit 301, 401 Reference value waveform 302, 402 detection section 303, 403 Actual casting waveform 303a, 403a Deviation area between standard waveform and actual casting waveform 303b, 403b Maximum value of waveform during actual casting 303c, 403c Average value of reference waveform
Claims
1. A quality control method for a die-cast product, comprising: supplying molten metal into an inside of an injection sleeve at a standby position after a plunger tip disposed in the injection sleeve is moved backward; and completing injection and filling of the molten metal into a die cavity at an injection completion position after a forward movement of the plunger tip, comprising: A sliding resistance determination device is provided which sets a detection section within a moving range of the retraction operation of the plunger tip, continuously samples the sliding resistance between the plunger tip and the injection sleeve within the detection section, and compares the sliding resistance with a previously sampled sliding resistance during casting of a good product to determine whether the sliding resistance is good or bad for each shot during actual casting, The sliding resistance is obtained from a control command value of an electrically controlled hydraulic servo valve system that controls the retreating or advancing motion of the plunger tip; A quality control method for die-cast products, comprising determining whether the quality of an actual casting for each shot is good or bad based on the evaluation results of the sliding resistance determining device.
2. The quality control method for die-cast products according to claim 1 , wherein the detection section is set to a range from the injection completion position as a starting point to the standby position.
3. A quality control method for die-cast castings as described in claim 1 or 2, wherein the control command value of the electrically controlled hydraulic servo valve system is a current value.
4. The quality control method for die-cast products according to any one of claims 1 to 3, further comprising collecting the sliding resistance during forward movement of the plunger tip within a range from the standby position to the injection completion position.
5. The method for quality control of die-cast products according to any one of claims 1 to 4, wherein the sliding resistance discriminator displays the position of the plunger tip and the control command value in the detection section as waveforms, superimposes the non-defective product waveform during the casting of the non-defective product and the casting waveform during the actual casting to determine a total area of the deviating waveforms, and compares the total area with a predetermined judgment reference area to determine the quality of the actual casting for each shot.
6. The method for quality control of die-cast products according to any one of claims 1 to 5, wherein, when the quality of the actual casting is judged to be bad, the sliding resistance discriminator issues a warning alarm and starts accumulating the number of warning alarms, and when the number of warning alarms exceeds a preset accumulated number, the operation of the actual casting is stopped and a danger alarm is issued.
Citation Information
Patent Citations
Method for processing color photographic sensitive silver halide material
JP1985002952A
Method for detecting galling degree in injection plunger mechanism
JP1990303667A
Electro-hydraulic type system
JP1991003003A
Casting device in die casting machine
JP1991032460A
Method for detecting abnormality of sleeve / tip in die casting
JP1992279268A