Persistent Current Switch

The PCS design with a high-conductivity splicing wire and soldered connection enhances quench resistance by shunting current and dissipating heat, addressing instability in superconducting magnets.

JP7558679B2Active Publication Date: 2024-10-01KK TOSHIBA
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020085691
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-05-15
Publication Date
2024-10-01
Estimated Expiration
2040-05-15

AI Technical Summary

Technical Problem

Persistent current switches (PCS) in superconducting magnets face high quenching risks due to insufficient cooling and heat dissipation in the lead wires, particularly in conduction cooling methods, leading to instability and phase transitions.

Method used

The PCS design incorporates a splicing wire with higher electrical conductivity than the lead wire, brazed with solder, and arranged along the longitudinal direction to shunt current and dissipate heat, enhancing quench resistance.

Benefits of technology

The design significantly increases quench tolerance by effectively suppressing transitions to a normal conducting state, improving stability and reducing quenching incidents.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007558679000001
    Figure 0007558679000001
  • Figure 0007558679000002
    Figure 0007558679000002
  • Figure 0007558679000003
    Figure 0007558679000003
Patent Text Reader

Abstract

To provide a permanent current switch with high quench resistance.SOLUTION: A permanent current switch 10 includes a main coil 21 that generates a magnetic field B, a non-inductive winding coil 11 that forms a closed circuit, a heater unit 12 that switches between the superconducting state and the normal conducting state of this non-inductive winding coil 11, and a splicing wire 18 (18a, 18b) that is electrically conductive along the longitudinal direction of a lead wire 17 (17a, 17b) from the non-inductive winding coil 11 and is electrically open at both ends.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] An embodiment of the present invention relates to a persistent current switch for a superconducting magnet. [Background technology]

[0002] A persistent current switch (PCS) generally consists of a coil made of superconducting wire wound in a non-inductive manner and a heater. The PCS uses the heater to control the temperature of the non-inductively wound coil, switching its superconducting / normal conducting phase transition and turning the closed circuit formed with the main coil on and off.

[0003] The material used for the non-inductive winding coil of the PCS is different from that used for the main coil of the superconducting magnet, which generally uses a superconductor such as NbTi and a stabilizer made of oxygen-free copper (Cu). In contrast, in the PCS, in order to maintain the switch function, a copper-nickel alloy (CuNi), which has a higher electrical resistance than Cu even at low temperatures, is generally used as the stabilizer.

[0004] The non-inductive winding coil of the PCS uses CuNi as a stabilizer, and as such has the property of slower thermal diffusion than the main coil of a general superconducting magnet, which uses Cu as a stabilizer. For this reason, when disturbances such as frictional heat between the windings occur, part of the current flowing through the NbTi superconductor may transfer to the CuNi stabilizer, and due to the slow thermal diffusion of Joule heat, an irreversible phase transition may occur from superconductivity to normal conductivity. Therefore, PCS has the property of being susceptible to quenching in response to slight disturbances.

[0005] The first known technique for stabilizing CuNi / NbTi superconducting wire is to coat the superconducting wire with an insulator such as MgO. According to this known technique, the equivalent thermal conductivity of the wire cross section of the CuNi / NbTi superconducting wire is improved, so that the minimum quench energy (MQE), which is an index of quench stability, increases by about 1000 times.

[0006] A second known technique involves winding a plurality of insulated wires of good thermal conductivity, thinner than the CuNi / NbTi superconducting wire, in a spiral shape around the superconducting wire. In both known techniques, a material with high thermal conductivity is placed along the entire length of the CuNi / NbTi superconducting wire, thereby dispersing heat generated by disturbances in the longitudinal direction of the superconducting wire. [Prior art documents] [Non-patent literature]

[0007] [Non-Patent Document 1] S. Yokohama, S. Yamamoto, S. Nakamura, T. Yamada, “Stabilization of CuNi / NbTi superconductors by MgO powder”, Cryogenics, 31(7), 1991, 521-523. [Patent documents]

[0008] [Patent Document 1] Japanese Patent Application Publication No. 10-116722 [Patent Document 2] Patent No. 3020140 Summary of the Invention [Problem to be solved by the invention]

[0009] There are two types of cooling methods for superconducting magnets: the conduction cooling method, which uses a GM refrigerator, and the immersion cooling method, which uses liquid helium. In the conduction cooling method, the main coil and PCS are cooled by supporting them on a heat transfer plate that is kept at a low temperature by a refrigerator. For this reason, the conduction cooling method is said to have lower cooling stability than the immersion cooling method.

[0010] By the way, as a result of investigating the location of quenches that occurred in conduction-cooled superconducting magnets, it was found that in many cases the origin of the quench was the lead wire of the non-inductive winding coil of the persistent current switch. This is thought to be because the lead wire of the non-inductive winding coil of the persistent current switch does not receive enough cold and heat from the heat transfer plate, and the quench resistance of the CuNi / NbTi superconducting wire due to disturbances is reduced.

[0011] The embodiments of the present invention have been made in consideration of the above circumstances, and an object of the present invention is to provide a persistent current switch with high quench resistance. [Means for solving the problem]

[0012] The persistent current switch comprises a non-inductive coil that forms a closed circuit with a main coil that generates a magnetic field, a heater section that switches the non-inductive coil between a superconducting state and a normal conducting state, and a splice wire that is electrically conductive along the longitudinal direction of a lead wire from the non-inductive coil and has both ends electrically open. The splice wire is a superconducting wire, and a stabilizer of the splice wire has a higher electrical conductivity than a stabilizer of the lead wire, or the lead wire and the splice wire are brazed and joined by solder. . Effect of the Invention

[0013] According to an embodiment of the present invention, a persistent current switch with high quench resistance is provided. [Brief description of the drawings]

[0014] [Figure 1] FIG. 2 is a circuit diagram of a persistent current switch according to an embodiment of the present invention. [Diagram 2] 4 is a cross-sectional view of a lead wire and a splice wire of the persistent current switch according to the embodiment. FIG. [Diagram 3] FIG. 2 is a perspective view of a persistent current switch according to an embodiment. [Figure 4] FIG. 2 is a cross-sectional view of a persistent current switch according to an embodiment. [Diagram 5] FIG. 4 is a wiring diagram of lead wires and splice wires in the persistent current switch according to the embodiment. [Figure 6] FIG. 13 is a perspective view showing another embodiment of the persistent current switch. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, an embodiment of the present invention will be described with reference to the accompanying drawings. Fig. 1 is a circuit diagram of a persistent current switch 10 according to an embodiment of the present invention. Thus, the persistent current switch 10 includes a non-inductive coil 11 that forms a closed circuit with a main coil 21 that generates a magnetic field B, a heater section 12 that switches the non-inductive coil 11 between a superconducting state and a normal conducting state, and splice wires 18 (18a, 18b) that are electrically conductive along the longitudinal direction of lead wires 17 (17a, 17b) from the non-inductive coil 11 and have both ends electrically open.

[0016] The main coil 21, the persistent current switch 10 and the structural members in contact with them are housed in a heat insulating container 22 since they must be isolated from the outside temperature and kept below the dividing temperature Tcs of the superconducting transition.

[0017] Superconducting electromagnet 20 cools a closed circuit consisting of main coil 21 and non-inductive winding coil 11 to make it superconducting, then circulates persistent current I to generate magnetic field B from main coil 21. The cooling method for making this closed circuit superconducting can be an immersion method using liquid helium or a heat conduction method using cold energy supplied from a cryogenic refrigerator.

[0018] When the cooling method is the thermal conduction method, the main coil 21 and the non-inductive winding coil 11 are supported by a support member (not shown) having high thermal conductivity, and receive cold heat from a cryogenic refrigerator. In either of the above-mentioned two cooling methods, an OFF / ON operation is performed using the persistent current switch 10 (PCS) at the start of circulating the persistent current I in the superconducting electromagnet 20. A general method is adopted for the method of starting the persistent current I involving the OFF / ON operation of the persistent current switch 10, and therefore a description thereof is omitted.

[0019] The main coil 21 is made of a superconducting wire wound in one direction, and generates a magnetic field B when a persistent current I flows through it. The non-inductive winding coil 11 of the persistent current switch 10 is made of two coils connected in series, each of which has a superconducting wire wound in the opposite direction, and does not generate an induced magnetic field even when the persistent current I flows through it.

[0020] The ends of a pair of lead wires 27 (27a, 27b) of the main coil 21 are connected to the connecting member 16 (16a, 16b). The ends of a pair of lead wires 17 (17a, 17b) of the non-inductive winding coil 11 are also connected to the connecting member 16. In this manner, the main coil 21 and the persistent current switch 10 have their ends connected to each other at the connecting member 16 (16a, 16b) to form a closed circuit.

[0021] The heater portion 12 of the persistent current switch 10 has an electrical resistor 25 arranged in close proximity to the non-inductive winding coil 11, and a power controller 26 that supplies power to the electrical resistor 25 to generate heat and switch the non-inductive winding coil 11 from a superconducting state to a normal conducting state.

[0022] The splice wires 18 (18a, 18b) are electrically conductive along the longitudinal direction of the lead wires 17 (17a, 17b) from the non-inductive winding coil 11, and both ends are electrically open. By arranging the splice wires 18 in this manner, even if disturbance occurs in the lead wires 17 for some reason, the current is shunted and heat is dissipated via the splice wires 18, so that the transition (quenching) of the lead wires 17 from a superconducting state to a normal conducting state can be suppressed.

[0023] 2 is a cross-sectional view of the lead wires 17 (17a, 17b) and splice wires 18 (18a, 18b) of the persistent current switch 10 according to the embodiment. The superconducting wire of the non-inductive winding coil 11 wound around the bobbin 19 (FIG. 3) is surface-coated with an electrically insulating coating (not shown), but the lead wire 17 has this surface coating removed. The lead wire 17 is composed of a first superconductor 31 that switches between a superconducting state and a normal conducting state depending on the temperature, and a first stabilizing body 41 that maintains the normal conducting state regardless of the temperature.

[0024] The first superconductor 31 is exemplified by, but not limited to, a NbTi alloy, which is widely used in practice. Although the first superconductor 31 and the first stabilizer 41 are formed in a layered shape in a cross-sectional view, the first superconductor 31 and the first stabilizer 41 are not limited to such a structure, and may be formed, for example, in a sea-island shape.

[0025] Although not shown, the lead wire 27 (FIG. 1) of the main coil 21 also has a shape similar to the lead wire 17 (FIG. 2) of the persistent current switch 10 in a cross-sectional view. Like the first superconductor 31 of the non-inductive winding coil 11, the superconductor of the main coil 21 is also made of a NbTi alloy.

[0026] On the other hand, the stabilizer of the main coil 21 is made of oxygen-free copper, which has a small electric resistance, whereas the first stabilizer 41 of the non-inductive winding coil 11 is made of a copper alloy, which has a larger electric resistance than oxygen-free copper. The reason for making the electric resistance of the first stabilizer 41 large in this way is that the electric resistance of the non-inductive winding coil 11 needs to show a sufficiently large value when the persistent current switch 10 is turned off at the time of starting the circulation of the persistent current I.

[0027] Thus, oxygen-free copper is used for the stabilizer in the main coil 21, whereas a high-resistance copper-nickel alloy (CuNi) is used for the first stabilizer 41 in the non-inductive winding coil 11. A superconducting wire stabilized with CuNi is less stable than a superconducting wire stabilized with oxygen-free copper, and is more susceptible to quenching due to magnetic instability. For this reason, it can be said that the superconducting electromagnet 20 has a risk of quenching occurring in the persistent current switch 10 and its surroundings.

[0028] The diameter of the splice wire 18 (FIG. 2) is set to be equal to or smaller than the diameter of the lead wire 17. The splice wire 18 can also be made of a superconducting wire. In this case, the splice wire 18 is made of a second superconductor 32 that switches between a superconducting state and a normal conducting state depending on the temperature, and a second stabilizer 42 that maintains a normal conducting state regardless of the temperature. The first superconductor 31 and the second superconductor 32, and the first stabilizer 41 and the second stabilizer 42 can each be made of the same material. The splice wire 18 (FIG. 2) can also be made of a single wire of the second superconductor 32 only, without using the second stabilizer 42.

[0029] On the other hand, a material having a higher electrical conductivity than the first stabilizer 41 of the lead wire 17 may be selected for the second stabilizer 42 of the splice wire 18. Specifically, for the lead wire 17 whose first stabilizer 41 is made of a copper alloy (CuNi), the superconducting wire of the main coil 21 whose second stabilizer 42 is made of pure copper may be used as the splice wire 18.

[0030] It is well known that metals with high electrical conductivity also have high thermal conductivity. Therefore, since the second stabilizer 42 of the splice wire 18 has the above-mentioned characteristics, even if disturbance occurs in the lead wire 17 for some reason, the heat is diverted and dissipated via the splice wire 18, so that the transition (quench) of the lead wire 17 from the superconducting state to the normal conducting state can be effectively suppressed.

[0031] Also, the second superconductor 32 of the splice wire 18 may be made of a material having a higher critical current value than the first superconductor 31 of the lead wire 17. Specifically, when the first superconductor 31 is NbTi, it is considered to use MgB2 or Nb3Sn as the second superconductor 32.

[0032] Therefore, since the second superconductor 32 of the splice wire 18 has the above-mentioned characteristics, even if a disturbance occurs in the lead wire 17 for some reason, the current is diverted to the second superconductor 32 of the adjacent splice wire 18. This reduces Joule heat generated in the first stabilizer 41 of the lead wire 17, and effectively suppresses the transition (quench) of the lead wire 17 from a superconducting state to a normal conducting state.

[0033] The lead wire 17 and the splice wire 18 are brazed and joined with solder 35. For this joining, the insulating coating on the surface of both the lead wire 17 and the splice wire 18 is removed and they are entirely solder-plated. The splice wire 18 is then attached to the lead wire 17 and joined with solder 35 so as to completely fill the gap between them. Solder 35 with a high Sn content and high thermal conductivity is suitable.

[0034] After being brazed with solder 35, the lead wire 17 and the splice wire 18 are electrically insulated with insulating tape 36. This insulating tape 36 is preferably made of polyimide film having extreme cold resistance, or prepreg tape or other electrically insulating material. Here, the thermal conductivity of CuNi constituting the first stabilizing body 41 of the lead wire 17 is approximately 1 W / m / K at 4K.

[0035] In contrast, the thermal conductivity of the solder 35 (Sn64%-Pb) is 1200 W / m / K, which is about 1000 times that of the CuNi first stabilizer 41. By fully plating the lead wire 17 and the splice wire 18 with the solder 35 in this manner, even if disturbance occurs in the lead wire 17 for some reason, heat is dissipated via the solder 35, so that the transition (quench) of the lead wire 17 from the superconducting state to the normal conducting state can be effectively suppressed.

[0036] Fig. 3 is a perspective view of the persistent current switch 10 according to the embodiment, and Fig. 4 is a cross-sectional view thereof. Thus, the persistent current switch 10 includes the bobbin 19 around which the non-inductive winding coil 11 is wound, an insulating layer 37 for ensuring electrical insulation at the interface between the non-inductive winding coil 11 and the bobbin 19, an insulating plate 39 disposed on the inside of one of the flanges at both ends of the bobbin 19, and a heat transfer plate 38 in contact with the outer circumferential surface of the non-inductive winding coil 11 for transferring cold and heat from the refrigerator or refrigerant and heat from the electrical resistor 25 (Fig. 1).

[0037] 5 is a wiring diagram of the lead wire 17 and the splice wire 18 in the persistent current switch 10 according to the embodiment. As described above, in the persistent current switch 10, a guide groove 46 for guiding the lead wire 17 and the splice wire 18 is provided in the insulating plate 39 arranged on the flange side of the bobbin 19 (FIG. 4) around which the non-inductive winding coil 11 is wound. Also, the insulating plate 39 is provided with a reversing member 45 for reversing the winding direction of the superconducting wire of the non-inductive winding coil 11.

[0038] The guide groove 46 is deep enough that the lead wires 17 and the splice wires 18 are completely buried, and the guided lead wires 17 and splice wires 18 are fixed with resin. The lead wires of a typical coil are often arranged in positions where it is difficult to supply cold and heat, and are prone to becoming the starting point of a quench due to disturbance.

[0039] However, by fixing the lead wire 17 and splice wire 18 with resin in the guide groove 46 provided on the flange side of the bobbin 19, mechanical disturbances caused by movement of the lead wire can be prevented. In addition, the resin around the wire has heat capacity, which is expected to improve the thermal stability of the lead wire. Even if disturbances occur, the transition (quench) of the lead wire 17 from the superconducting state to the normal conducting state can be effectively suppressed.

[0040] FIG. 6 is a perspective view showing another embodiment of the persistent current switch 10. In this embodiment, the lead wire 17 and the splice wire 18 are characterized by having a twisted wire structure. In general, a transverse magnetic field perpendicular to the current reduces the non-uniformity of the current density in the filament. For this reason, if the filament diameter is made small, the superconducting wire becomes stable against the transverse magnetic field. However, if a longitudinal magnetic field parallel to the current is applied, the saturation region of the current distribution in the filament is likely to change depending on the magnitude and direction of the longitudinal magnetic field, resulting in spontaneous magnetic flux jumps and magnetic instability.

[0041] Therefore, by having the lead wire 17 and the splice wire 18 have a twisted wire structure, the directions of the current and the magnetic field can be shifted, and the magnetic instability of the superconducting wire against the vertical magnetic field can be alleviated. By adopting a twisted wire structure, it is possible to effectively suppress magnetic disturbance without compromising the ease of electrical connection of the lead wire 17. In addition, the thermal contact area with the lead wire 17 is increased, which has the effect of thermal stabilization.

[0042] According to at least one of the persistent current switches of the embodiments described above, the splice wire is provided along the longitudinal direction of the lead wire, thereby making it possible to increase the quench resistance.

[0043] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These embodiments can be implemented in various other forms, and various omissions, substitutions, modifications, and combinations can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope of the invention and its equivalents described in the claims, as well as in the scope and spirit of the invention. [Explanation of symbols]

[0044] 10... persistent current switch, 11... non-inductive wound coil, 12... heater portion, 16... connecting member, 17 (17a, 17b)... lead wire, 18 (18a, 18b)... splice wire, 19... bobbin, 20... superconducting electromagnet, 21... main coil, 22... insulated container, 25... electrical resistor, 26... power controller, 27 (27a, 27b)... lead wire, 31... first superconductor, 32... second superconductor, 35... solder, 36... insulating tape, 37... insulating layer, 38... heat transfer plate, 39... insulating plate, 41... first stabilizer, 42... second stabilizer, 42... stabilizer, 45... reversal member, 46... guide groove, B... magnetic field, I... circulating current.

Claims

1. A non-inductive winding coil that forms a closed circuit with a main coil that generates a magnetic field; A heater section for switching the non-inductive winding coil between a superconducting state and a normal conducting state; a splice wire electrically connected along a longitudinal direction of the lead wire from the non-inductive winding coil and having both ends electrically open, The splice wire is a superconducting wire, A persistent current switch, wherein the stabilizer of the splice wire has a higher electrical conductivity than the stabilizer of the lead wire.

2. A non-inductive winding coil that forms a closed circuit with a main coil that generates a magnetic field; A heater section for switching the non-inductive winding coil between a superconducting state and a normal conducting state; a splice wire electrically connected along a longitudinal direction of the lead wire from the non-inductive winding coil and having both ends electrically open, The lead wire and the splice wire are soldered together in this persistent current switch.

3. The persistent current switch according to claim 2, The splice wire is a persistent current switch that is a superconducting wire.

4. The persistent current switch according to claim 1 or 2, A persistent current switch, wherein the superconductor of the splice wire has a critical current value equal to or higher than that of the superconductor of the lead wire.

5. The persistent current switch according to claim 2, A persistent current switch, wherein the stabilizer of the splice wire has a higher electrical conductivity than the stabilizer of the lead wire.

6. The persistent current switch according to any one of claims 1 to 5, The superconducting wire of the non-inductive winding coil wound around the bobbin is surface-coated with an electrically insulating coating; A persistent current switch, wherein the lead wire is the superconducting wire from which the surface coating has been removed.

7. The persistent current switch according to claim 1, The lead wire and the splice wire are soldered together in this persistent current switch.

8. The persistent current switch according to any one of claims 1 to 7, A persistent current switch in which guide grooves for guiding the lead wire and the splice wire are provided on the flange side of the bobbin around which the non-inductive winding coil is wound, and the guide grooves are fixed with resin.

9. 9. The persistent current switch according to claim 1, The lead wire and the splice wire are a stranded wire structure.

Citation Information

Patent Citations

  • Permanent current switch

    JP1991074886A

  • Persistent current switch

    JP1993327041A

  • Superconducting conductor and permanent current switch

    JP1998116722A

  • Persistent current switch

    JP2007221013A

  • Persistent current switch device for refrigerator-cooled superconducting magnet

    JP3020140B2