Corrugated hose manufacturing system
The corrugated hose manufacturing system addresses uneven thickness issues by using a wall thickness adjustment mechanism to control parison thickness, ensuring uniformity and reliability in the corrugated hose production process.
Patent Information
- Application Number
- JP2021020611
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-02-12
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2041-02-12
AI Technical Summary
Existing corrugated hose manufacturing processes result in uneven thickness distribution due to the undulations of convex and concave portions, leading to potential damage and reduced product life.
A corrugated hose manufacturing system incorporating an extruder, corrugator, and a wall thickness adjustment mechanism, which includes a positioning mechanism connected to a core via a spindle, allowing for precise control of parison thickness through adjustments in the die core opening degree.
The system ensures uniform thickness distribution, enhancing the reliability and durability of the corrugated hose by preventing localized thinning and material wastage.
Smart Images

Figure 0007561053000001 
Figure 0007561053000002 
Figure 0007561053000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a manufacturing system for a corrugated hose. To In particular, a manufacturing system for forming a corrugated hose using an extruder and a corrugator. To It can be suitably used. [Background technology]
[0002] A technology is known in which a raw material resin is plasticized using an extruder to form a molten resin, the molten resin is extruded from a die of the extruder to form a cylindrical parison, and then the parison is processed in a corrugator to form a corrugated hose (corrugated tube).
[0003] For example, Patent Document 1 discloses a technique for providing thick and thin portions in a corrugated tube when the corrugated tube is molded from a resin raw material. Patent Document 1 also discloses a technique for changing the moving speed of a die provided in a corrugator, and a technique for adjusting the amount of resin passing through the die by a gear pump provided at the extrusion port of an extruder. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2014-218028 A Summary of the Invention [Problem to be solved by the invention]
[0005] For example, when forming a corrugated hose by vacuum forming, a corrugator performs a process in which the parison is sandwiched between mold blocks (metal dies) and the parison is brought into contact with the mold blocks by sucking the parison with a vacuum. The parison is processed into a shape corresponding to the shape of the inner wall of the mold block. For example, when the mold block has a bellows-shaped portion formed by alternating concave and convex portions, a corrugated hose having a bellows portion formed by alternating convex and concave portions is formed.
[0006] However, when a corrugated hose has such a bellows portion, the unevenness of the convex and concave portions tends to cause the parison thickness to vary from place to place. The portions where the parison is thin are prone to breakage, and this may shorten the product life of the corrugated hose. Therefore, there is a demand for a technology that can increase the uniformity of the parison thickness over the entire corrugated hose, thereby improving the reliability of the corrugated hose.
[0007] Other objects and novel features will become apparent from the description of this specification and the accompanying drawings. [Means for solving the problem]
[0008] A corrugated hose manufacturing system in one embodiment includes an extruder, a corrugator, and a wall thickness adjustment mechanism. The extruder includes a cylinder, a screw provided inside the cylinder, a raw material supply unit provided in the cylinder, a die connected to the cylinder downstream of the raw material supply unit, a die land integrated with the die and provided on the discharge outlet side of the die, and a cylindrical core whose outer periphery is covered by the die land. The corrugator includes an inlet section, a discharge section, and a mold block provided inside the corrugator and moving from the inlet section toward the discharge section. The wall thickness adjustment mechanism includes a positioning mechanism connected to the core via a spindle and capable of performing a positioning operation.
[0009] In one embodiment, the corrugated hose is molded by using a corrugated hose manufacturing system including an extruder, a corrugator, and a wall thickness adjustment mechanism. Here, the extruder includes a cylinder, a screw provided inside the cylinder, a raw material supply unit provided in the cylinder, a die connected to the cylinder downstream of the raw material supply unit, a die land integrated with the die and provided on the discharge outlet side of the die, and a cylindrical core whose outer periphery is covered by the die land. The corrugator includes an inlet section, a discharge section, and a mold block provided inside the corrugator and moving from the inlet section toward the discharge section. The wall thickness adjustment mechanism includes a positioning mechanism connected to the core via a spindle and capable of performing a positioning operation. Effect of the Invention
[0010] According to one embodiment, a highly reliable corrugated hose can be provided. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a schematic diagram showing a manufacturing system in a first embodiment. [Diagram 2] 4 is a plan view showing a forming process for processing a parison using the wall thickness adjustment mechanism in the first embodiment. FIG. [Diagram 3] 1 is a side view showing a corrugated hose in a first embodiment. [Figure 4] FIG. 1 is a cross-sectional view showing an ideal thickness. [Diagram 5] FIG. 11 is a cross-sectional view showing a problem in the study example. [Figure 6] FIG. 2 is a perspective view showing a die land and a core in the first embodiment. [Figure 7] FIG. 2 is a plan view showing a die land and a core in the first embodiment. [Figure 8] FIG. 2 is a plan view showing a combination of a die land and a core in the first embodiment. [Figure 9]4 is a flowchart showing a parison forming means and a corrugated hose molding means in the first embodiment. [Figure 10] 4 is a flowchart of a pre-processing according to the first embodiment. [Figure 11] 4 is a timing chart during a molding operation in the first embodiment. [Figure 12] 4 is a flowchart during a molding operation in the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, the embodiments will be described in detail with reference to the drawings. In all the drawings for explaining the embodiments, the same reference numerals are used for the members having the same functions, and the repeated explanations are omitted. In the following embodiments, the explanations of the same or similar parts will not be repeated as a rule unless it is particularly necessary.
[0013] Furthermore, in the drawings used in the embodiments, hatching may be omitted in order to make the drawings easier to understand.
[0014] (Embodiment 1) <Configuration of manufacturing system 100> A corrugated hose manufacturing system 100 according to the first embodiment will be described below with reference to FIGS.
[0015] 1 and 2, the manufacturing system 100 includes an extruder 200, a corrugator 300, and a wall thickness adjustment mechanism 50. By using the extruder 200, a cylindrical parison 41 is formed from a resin material, and by processing the parison 41 using the corrugator 300, a corrugated hose 42 is formed as a molded product.
[0016] The extruder 200 has a plasticizing section 10 and a head section 20 connected to the downstream side of the plasticizing section 10. The plasticizing section 10 includes a cylinder 11, a screw 12, a rotating mechanism 13, and a raw material supplying section 14. The screw 12 is provided inside the cylinder 11 and rotated by the driving of the rotating mechanism 13 connected to the upstream end of the cylinder 11. The raw material supplying section 14 is provided on the upstream side of the cylinder 11.
[0017] In FIG. 1, the plasticizing section 10 is exemplified as a single screw extruder, but the plasticizing section 10 may be a twin screw extruder or an extruder equipped with a plurality of screws, more than two screws.
[0018] The head unit 20 includes a die 21 connected to the downstream side of the cylinder 11, and a die land 22 integrated with the die 21 and provided on the discharge port side of the die 21. As shown in Fig. 2, the head unit 20 further includes a core 23, and the configurations and effects of the die land 22 and the core 23 will be described in detail later.
[0019] 1, in order to easily show the process of forming parison 41 from a raw material resin and processing parison 41 to form corrugated hose 42, the plasticizing unit 10, head unit 20 and corrugator 300 are illustrated as being arranged in the same direction. However, in reality, as shown in FIG. 2, the wall thickness adjustment mechanism 50, die 21 and corrugator 300 are arranged in the same direction, and the plasticizing unit 10 is arranged in a different direction.
[0020] 2, a crosshead die is applied to the die 21 of the head section 20, and the inflow direction of the molten resin 40 changes inside the die 21. The molten resin 40 that flows from the plasticizing section 10 into the die 21 flows in a spiral shape inside the die 21, and then the molten resin 40 is extruded as a parison 41 from between the die land 22 and the core 23.
[0021] 2, holes are provided inside the core 23 for allowing the air AR to flow along the extending direction of the core 23. The inner diameter of the formed parison 41 is expanded by the air AR.
[0022] 1, the corrugator 300 includes a main body 31, a mold block 32, an inlet section 33 which serves as an inlet path for the parison 41, and a discharge section 34 which serves as a discharge path for the corrugated hose 42. The mold block 32 moves from the inlet section 33 toward the discharge section 34.
[0023] 2, a moving mechanism such as a rail 35 is provided inside the main body 31 of the corrugator 300, and the mold block 32 is mounted on the rail 35. The rail 35 rotates from the inlet portion 33 toward the discharge portion 34. The mold block 32 is moved by the movement of the rail 35. As the parison 41 flows toward the discharge portion 34, another molding portion of the mold block 32 can be assigned to the newly flowed parison 41.
[0024] The mold block 32 also includes a plurality of smooth molded portions 32a having a smooth surface, and a plurality of bellows molded portions 32b having a surface configured with a plurality of concave and convex portions arranged alternately. The surface of the smooth molded portions 32a is smoother than the undulations between the concave and convex portions of the bellows molded portions 32b. The parison 41 is processed so that the shape of the parison 41 corresponds to the shape of the plurality of smooth molded portions 32a or the bellows molded portions 32b.
[0025] 2, a thickness adjustment mechanism 50 is connected to the head portion 20. The thickness adjustment mechanism 50 has a positioning mechanism 51 that is connected to the core 23 via a spindle 52 and is capable of performing a positioning operation, a motor 53 that controls the positioning operation of the positioning mechanism 51, and a ball screw 54 that can support the positioning mechanism 51 while responding to the positioning operation of the positioning mechanism 51.
[0026] When the motor 53 is driven, the positioning mechanism 51 performs a positioning operation along the extension direction of the core 23 while being supported by the ball screw 54. The core 23 can move along the extension direction of the core 23 via the spindle 52 in response to the positioning operation of the positioning mechanism 51.
[0027] The manufacturing system 100 also includes a control unit CU configured by a computer, etc. The control unit CU is electrically connected to the extruder 200, the corrugator 300, and the wall thickness adjustment mechanism 50, and can control the operations thereof.
[0028] As described above, the rotation of the screw 12 is controlled by the rotation mechanism 13, the movement of the mold block 32 is controlled by a moving mechanism such as the rail 35, and the positioning operation of the positioning mechanism 51 is controlled by the motor 53. The rotation mechanism 13, the rail 35, and the motor 53 are electrically connected to the control unit CU, and their operations and controls are managed by the control unit CU. Therefore, hereinafter, various operations and controls performed by the extruder 200, the corrugator 300, and the wall thickness adjustment mechanism 50 may be described as being performed by the control unit CU.
[0029] <Configuration of corrugated hose 42> 3 shows an example of a corrugated hose 42 formed by a corrugator 300. The corrugated hose 42 includes a plurality of smooth portions 42a having a smooth surface, and a plurality of bellows portions 42b having a surface configured with a plurality of alternating projections and recesses. The surface of the smooth portions 42a is smoother than the undulations between the projections and recesses of the bellows portions 42b.
[0030] The smooth portion 42a is a portion that has been machined to correspond to the shape of the smooth molded portion 32a of the mold block 32, and the bellows portion 42b is a portion that has been machined to correspond to the shape of the bellows molded portion 32b of the mold block 32.
[0031] Also, here, the mold block 32 is configured with the smooth molded portion 32a and the bellows molded portion 32b, and the corrugated hose 42 includes the smooth portion 42a and the bellows portion 42b. However, the combination of the smooth portion 42a and the bellows portion 42b can be changed as appropriate by changing the combination of the smooth molded portion 32a and the bellows molded portion 32b. For example, it is also possible to mold a corrugated hose 42 whose entirety is configured with the bellows portion 42b.
[0032] <About the study example> 4 and 5 are enlarged views of a portion of the cross section of the corrugated hose 42. Fig. 4 shows a case where the corrugated hose 42 has an ideal thickness, and Fig. 5 shows problems with the corrugated hose 42 of an example studied by the present inventors.
[0033] It is ideal to mold a corrugated hose 42 in which the thickness of the convex and concave portions of the bellows portion 42b is uniform, as shown in Fig. 4. However, the inventors of the present application have found a problem that when the parison 41 is brought into contact with the mold block 32 by vacuum suction, the strength of the vacuum suction is likely to vary due to the unevenness of the convex and concave portions of the bellows portion 32b. When such variation occurs, for example, as shown in Fig. 5, the thickness of the convex portions of the bellows portion 42b becomes thinner than other portions.
[0034] In order to solve these problems, the inventors of the present application tried to increase the overall thickness of the corrugated hose 42 by slowing down the speed of the corrugator 300 (the moving speed of the mold block 32) as a countermeasure in the study example shown in Fig. 4. As a result, the thickness of the convex part of the bellows part 42b became thicker, but it was found that if the moving speed of the mold block 32 becomes too slow compared to the inflow speed of the parison 41, the parison 41 may get into the gaps between the molding parts of the mold block 32, making it impossible to perform normal molding.
[0035] Furthermore, not only the thickness of the bellows portion 42b but also the overall thickness of the corrugated hose 42 increases, which causes problems in that the weight of the corrugated hose 42 increases, making it difficult to reduce the weight, and in that the cost of materials increases.
[0036] Another possible method is to increase the extrusion amount of the parison 41 and increase the thickness of the bellows portion 42b by changing the rotation speed of the screw 12 driven by the rotation mechanism 13 only when the bellows portion 42b is processed. However, since a time lag occurs between the timing when the rotation speed of the screw 12 is changed and the timing when the parison 41 is extruded, it is difficult to apply such a method.
[0037] Therefore, in order to solve the various problems found in the countermeasures of the example of FIG. 4, the inventors of the present application adopted a wall thickness adjustment mechanism 50 and investigated a method of adjusting the thickness of the parison 41 extruded from between the die land 22 and the core 23.
[0038] <Configuration of Head Unit 20> 6 to 8 show the structure of the head portion 20 in the vicinity of the discharge opening of the die 21. FIG.
[0039] 6 and 7, the die 21 includes a die land 22 that is integrated with the die 21 and provided on the discharge side of the die 21, and a core 23. The core 23 is cylindrical and extends in a direction toward the corrugator 300, and the outer periphery of the core 23 is covered with the die land 22.
[0040] The die land 22 includes a tip portion 22e located at the discharge port of the die 21. The core 23 includes an end portion 23i connected to the spindle 52 of the wall thickness adjustment mechanism 50, and an end portion (tip portion) 23e located on the opposite side to the end portion 23i and located at the discharge port of the die 21.
[0041] 6 and 7, the diameter of the core 23 becomes wider as it approaches the end 23e, and the inner diameter of the die land 22 is constant. The molten resin 40 passes between the die land 22 and the core 23, and is extruded as a parison 41 from between the die land 22 and the core 23 at the outlet of the die 21. Here, the core 23 can be moved as shown by the arrow in FIG. 7 by the positioning operation of the positioning mechanism 51 shown in FIG. 2. The movement of the core 23 changes the die core opening L1, which is the distance between the die land 22 and the core 23 at the outlet of the die 21. More specifically, the die core opening L1 is the length between the inner diameter of the die land 22 at the outlet of the die 21 and the diameter of the core 23.
[0042] 7, for example, when the die core opening L1 is decreased, the thickness of the parison 41 is decreased, and when the die core opening L1 is increased, the thickness of the parison 41 is increased. In this manner, by moving the core 23, it is possible to adjust the thickness of the parison 41 extruded between the die land 22 and the core 23.
[0043] 8, various combinations can be applied to the shape of the die land 22 and the shape of the core 23 at the outlet of the die 21. As such a combination, for example, the shape of the die land 22 and the shape of the core 23 can be a divergent type, a convergent type, or a straight type, respectively.
[0044] That is, a combination of the shape of the die land 22 and the shape of the core 23 is selected so that, at the outlet of the die 21, the inner diameter of the die land 22 changes as it approaches the tip 22e, the aperture of the core 23 changes as it approaches the end 23e, or both of them change as they approach the end 23e and the tip 22e. This allows the die core opening L1 to be changed when the core 23 moves, making it possible to adjust the thickness of the parison 41.
[0045] The parison forming means and the corrugated hose molding means included in the corrugated hose manufacturing system 100 according to the first embodiment will be described below with reference to Figs.
[0046] <Parison forming means> The parison forming means has steps S1 to S3 shown in FIG.
[0047] In step S1, raw material resin is fed from raw material supply unit 14 into cylinder 11. Thermoplastic resin can be used as raw material resin. Thermoplastic resin is, for example, polypropylene, polyethylene, polyamide, polyethylene terephthalate, or polyimide. The raw material in the first embodiment may be any of the above materials alone or a mixture containing two or more of these materials.
[0048] A heat source (not shown) is provided around the cylinder 11, and each region of the cylinder 11 is adjusted to a desired temperature by the heat source. The heat source may be any means capable of heating the thermoplastic resin to a temperature at which it can be melted. The cylinder 11 may also be provided with a liquid injection nozzle for injecting an additive, a filler, or a filler dispersion, and these may be injected into the resin being plasticized midway through the cylinder 11.
[0049] In step S2, the resin is kneaded and plasticized by the screw 12. As a result, molten resin 40 is formed as the plasticized resin.
[0050] In step S3, the parison 41 is formed. The plasticized molten resin 40 is extruded as a cylindrical parison 41 from between the die land 22 and the core 23. In this manner, the parison 41 in the first embodiment is formed. The parison 41 may have a multi-layer structure. For example, a plurality of extruders each form molten resin, and the molten resins are supplied to one die, thereby forming the parison 41 having a multi-layer structure.
[0051] In step S3, the control unit CU moves the core 23 by the positioning operation of the positioning mechanism 51, whereby the die core opening degree L1 changes, and the thickness of the parison 41 can be adjusted.
[0052] Therefore, the thickness of the parison 41 can be adjusted while the number of revolutions of the screw 12 driven by the rotation mechanism 13 is kept constant. There is almost no time lag between the timing at which the thickness of the parison 41 is changed and the timing at which the parison 41 is extruded. Therefore, the thickness of the parison 41 can be changed at a desired timing, such as when processing the parison 41 by the bellows molding section 32b. Therefore, it is possible to suppress the problem that the thickness of the convex part of the bellows part 42b becomes locally thin, as in the example of FIG. 4.
[0053] <Method of forming corrugated hose> The corrugated hose forming means has steps S4 to S6 shown in FIG.
[0054] In step S 4 , the cylindrical parison 41 is introduced into the corrugator 300 from the inlet portion 33 of the corrugator 300 .
[0055] In step S5, the parison 41 is processed by the mold block 32. A vacuum molding method is an example of a method for processing the parison 41. The vacuum molding method is a method in which the shape of the parison 41 corresponds to the shape of each molding part of the mold block 32 by sucking the parison 41 toward the mold block 32.
[0056] For example, in a state where the parison 41 is sandwiched between the pair of bellows molding parts 32b, the parison 41 is sucked by a vacuum to bring the parison 41 into contact with the pair of bellows molding parts 32b. This changes the shape of the parison 41, and the portions corresponding to the recesses of the bellows molding parts 32b are processed as protrusions of the bellows part 42b of the corrugated hose 42, and the portions corresponding to the protrusions of the bellows molding parts 32b are processed as recesses of the bellows part 42b of the corrugated hose 42.
[0057] In step S6, the processed parison 41 is discharged from the discharge portion 34 of the corrugator 300 as a cylindrical molded product, that is, a corrugated hose 42. In this manner, the corrugated hose 42 in the first embodiment is molded.
[0058] In step S5, when the thickness of the parison 41 is adjusted in step S3, the inflow speed of the parison 41 varies depending on the thickness of the parison 41. Here, the control unit CU can adjust the moving speed of the mold block 32 so as to approach the varied inflow speed of the parison 41.
[0059] FIG. 10 shows a pre-processing step in which first data regarding the variation in thickness of the parison 41, second data regarding the variation in the inflow speed of the parison 41, and third data regarding the variation in the die core opening L1 are stored in the control unit CU before the parison forming means and the corrugated hose molding means are performed.
[0060] Since the control unit CU holds the first to third data in advance, the control unit CU can control how much the thickness of the parison 41 and the inflow speed of the parison 41 will change depending on how much the control unit CU changes the die core opening L1.
[0061] First, in step S7, the user sets the outer diameter and thickness of the product in accordance with the requirements of the product (corrugated hose 42). In step S8, the cross-sectional area of the product is calculated based on these set values.
[0062] Meanwhile, in step S9, the user sets, for example, an extrusion amount and a product density as the operating conditions of the extruder 200. The extrusion amount is the weight of resin extruded from the extruder 200 per unit time. When the parison 41 is composed of multiple resin layers, the extrusion amount refers to the total weight from all the extruders 200. The product density is a value obtained by dividing the weight of the corrugated hose 42 per unit length by its volume.
[0063] It should be noted that there is no need to newly consider the values in steps S7 to S9 for the parison forming means and the corrugated hose molding means in the first embodiment, and existing set values and specifications can be used.
[0064] In step S10, a simulation is performed in advance based on the values in steps S7 to S9, thereby calculating first data regarding the variation in the thickness of the parison 41 and second data regarding the variation in the inflow speed of the parison 41.
[0065] In step S11, third data regarding the fluctuation of the die core opening degree L1 is calculated by performing a back calculation based on the result of step S10.
[0066] 11 is a timing chart (a timing chart during molding operation) when the parison 41 is processed by the smooth molding section 32a or the bellows molding section 32b. The "current position" shown in FIG. 11 indicates where in the mold block 32 the parison 41 being processed is located.
[0067] FIG. 12 is a flow chart showing a process in which the control unit CU detects the position of the mold block 32 and changes the die core opening L1 and the moving speed of the mold block 32 based on the result of the detection.
[0068] The main body 31 of the corrugator 300 originally has a function of detecting the position of the rail 35 on which the mold block 32 is mounted. The operation of the main body 31 (rail 35) is controlled by a control unit CU.
[0069] Therefore, first, in step S12, the control unit CU detects the position of the mold block 32. Next, in step S13, the control unit CU detects the position of the mold block 32 in which the parison 41 is being processed.
[0070] Depending on the result of step S13, it is determined whether the mold block 32 corresponding to the "current position" shown in Fig. 11 is the smooth molding portion 32a or the bellows molding portion 32b. In response to either of the determination results, the control unit CU adjusts the die core opening L1 used in step S3 and the moving speed of the mold block 32 used in step S5.
[0071] For example, when processing the parison 41 using the bellows molding section 32b, the control section CU makes the thickness of the parison 41 thicker and slows down the moving speed of the mold block 32 compared to when the parison 41 is processed using the smooth molding section 32a.
[0072] In the example of FIG. 4, the moving speed of the multiple mold blocks 32 was too slow compared to the inflow speed of the parison 41, causing problems such as the parison 41 getting into the gaps between the molding sections of the mold blocks 32.
[0073] In the first embodiment, the moving speed of the multiple mold blocks 32 can be adjusted so as to approach the fluctuating inflow speed of the parison 41. Therefore, the occurrence of the above problem can be suppressed.
[0074] Moreover, by changing the die core opening L1, the thickness of the parison 41 can be adjusted, and further, the thickness of the parison 41 can be changed at a desired timing, for example, when it is desired to form the bellows portion 42b.
[0075] As described above, according to the manufacturing system 100 in the first embodiment, the parison 41 is less likely to have variation in thickness, and therefore it is possible to improve the uniformity of the thickness throughout the corrugated hose 42. As a result, it is possible to provide a highly reliable corrugated hose 42.
[0076] Although the present invention has been specifically described based on the above embodiment, the present invention is not limited to the above embodiment and can be modified in various ways without departing from the spirit of the present invention. [Explanation of symbols]
[0077] 10 Plasticization Section 11 Cylinders 12 Screw 13 Rotation mechanism 14 Raw material supply department 20 Head section 21 Die 22 Dyland 22e Tip of die land 23 Cores 23i Core End 23e Core end (tip) 31 Main unit 32 Mold Block 32a Smooth molded part 32b Bellows molding part 33 Inlet 34 Discharge section 35 Rail 40 Molten Resin 41 Parison 42 Corrugated hose 42a Smooth part 42b Bellows section 50 Thickness adjustment mechanism 51 Positioning mechanism 52 Spindle 53 Motor 54 Ball screw 100 Manufacturing System 200 Extruder 300 Corrugator AR Air CU control unit L1 Dicore opening
Claims
1. A corrugated hose manufacturing system including an extruder, a corrugator, and a wall thickness adjustment mechanism, The extruder comprises: A cylinder; A screw provided inside the cylinder; A raw material supply unit provided in the cylinder; a die connected to the cylinder downstream of the raw material supply unit; a die land that is integrated with the die and is provided on the outlet side of the die; a cylindrical core whose outer periphery is covered with the die land; having The corrugator comprises: An inlet portion; A discharge section; a mold block disposed inside the corrugator and moving from the inlet portion toward the outlet portion; having the wall thickness adjustment mechanism has a positioning mechanism that is connected to the core via a spindle and is capable of performing a positioning operation; A parison forming means; A corrugated hose forming means; a control unit electrically connected to the extruder, the corrugator, and the wall thickness adjustment mechanism and capable of controlling the operations of these; Further comprising: The parison forming means is (a1) a step of feeding a raw material resin from the raw material supply part into the inside of the cylinder; (a2) plasticizing the resin by the screw; (a3) extruding the plasticized resin as a cylindrical parison from between the die land and the core at a discharge port of the die; having The corrugated hose forming means includes: (b1) introducing the parison into the corrugator from the inlet portion; (b2) processing the parison by contacting the parison with the mold block and causing the shape of the parison to correspond to the shape of the mold block; (b3) discharging the processed parison from the discharge section as a corrugated hose; having The mold block includes at least a bellows-shaped portion having a surface with alternating concave and convex portions; The corrugated hose includes a bellows portion processed by the bellows molding portion, In the step (a3), the control unit adjusts a thickness of the parison extruded between the die land and the core by moving the core through a positioning operation of the positioning mechanism; In the process (b2), when the thickness of the parison is adjusted, an inflow speed of the parison fluctuates, and the control unit adjusts the moving speed of the mold block so as to approach the fluctuated inflow speed of the parison.
2. 2. The corrugated hose manufacturing system according to claim 1, the die land includes a first end located at an outlet of the die; the core includes a second end located at an outlet of the die; an inner diameter of the die land varies toward the first end, a diameter of the core varies toward the second end, or both vary toward the first end and the second end; A corrugated hose manufacturing system, in which when the core moves, the thickness of the parison is adjusted by changing a die core opening, which is the distance between the die land at the die outlet and the core.
3. 3. The corrugated hose manufacturing system according to claim 2, (c) before the parison forming means and the corrugated hose forming means are performed, First data relating to a variation in thickness of the parison; second data relating to a variation in inflow velocity of the parison in response to a variation in thickness of the parison; third data relating to a variation in the die core opening in response to a variation in the thickness of the parison and a variation in the inflow velocity of the parison; The corrugated hose manufacturing system further comprises a step of recording the above in the control unit.
4. 2. The corrugated hose manufacturing system according to claim 1, The control unit of the system for manufacturing a corrugated hose is capable of detecting a position of the mold block while the parison is being processed.
5. 5. The corrugated hose manufacturing system according to claim 4, the mold block includes a smooth molded portion having a surface smoother than the undulations between the concave portion and the convex portion; a control unit that, when processing the parison by the bellows molding unit, increases the thickness of the parison and slows the moving speed of the mold block compared to when the parison is processed by the smooth molding unit.
6. 2. The corrugated hose manufacturing system according to claim 1, The (b2) step is performed by sucking the parison toward the mold block.
Citation Information
Patent Citations
Method and apparatus for manufacturing resin tube
JP2006069180A
Parison marking method and wall thickness adjusting apparatus
JP2006123410A
Corrugated tube and method for manufacturing the same
JP2010260241A
Corrugate tube manufacturing apparatus and method
JP2014218028A
Apparatus for manufacturing foamed resin tube and foamed resin tube
WO2018124213A1