Method for separating resin-coated layer on inner surface of metal pipe
The method uses high-frequency induction heating with an inert gas atmosphere to thermally decompose and melt resin coating layers from metal tubes, addressing separation challenges and ensuring safe, complete recovery.
Patent Information
- Application Number
- JP2021003486
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-01-13
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2041-01-13
AI Technical Summary
Existing methods for separating resin coating layers from metal tubes face challenges such as resin breakage, re-adhesion, difficulty in small diameter tubes, and risk of ignition due to molten resin clogging, especially when contaminated with radioactive substances.
A method involving high-frequency induction heating with an inert gas atmosphere, where a coil heats the metal tube end, thermally decomposing and melting the resin while maintaining an inert gas flow to prevent re-adhesion and ignition, using a resin recovery container to collect the molten resin.
The method allows for easy and reliable separation of resin coating layers without tools, prevents re-adhesion, and avoids ignition risks, ensuring complete recovery of contaminants.
Smart Images

Figure 0007561474000001 
Figure 0007561474000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for separating a resin coating layer formed on the inner surface of a metal pipe from the inner surface. [Background technology]
[0002] For example, the present applicant has introduced a method for peeling off a resin coating layer formed on the inner surface of a metal pipe when replacing the resin coating layer, in which the resin coating layer is peeled off at one end of the metal pipe to create a gripping area, the gripping area is connected to a gripping and pulling means inserted into the metal pipe and the gripping area is reversed, the pipe body in the vicinity of the peeling front is heated by induction heating means so that the adhesive strength is temporarily reduced, the induction heating means is moved sequentially in the axial direction of the pipe to move the heating position sequentially while the gripping and pulling means is pulled out towards the other end of the metal pipe, and the resin coating layer is peeled off while being reversed (see Patent Document 1 below).
[0003] However, in the method described in Patent Document 1, the resin coating layer after peeling off is softened by heating and has reduced strength, and may break during the process due to the tensile force.
[0004] In addition, as another method for peeling off a resin coating layer formed on the inner surface of a metal pipe, the applicant has introduced a method including a first step of heating the interface between the metal pipe and the resin coating layer at a temperature equal to or higher than the thermal decomposition temperature of the resin constituting the resin coating layer while water-cooling the surface of the resin coating layer, thereby thermally decomposing the constituent resin near the interface, and a second step of peeling off and removing the resin coating layer from the inner surface of the metal pipe (see Patent Document 2 below).
[0005] However, in the method described in Patent Document 2, the resin coating layer may re-adhere to the inner surface of the metal pipe after the first step is completed, and it is extremely difficult to peel off the re-adhered resin in the second step.
[0006] In addition, it is extremely difficult to peel off a resin coating layer formed on the inner surface of a metal pipe having a small diameter (for example, an outer diameter of 27.2 to 114.3 mm) using fingers or a jig.
[0007] Incidentally, the resin coating layer formed on the inner surface of a metal pipe that has been used in a nuclear power controlled area may have its surface contaminated with radioactive materials, etc., and it is therefore necessary to reliably recover such contaminants together with the resin that constitutes the surface vicinity of the resin coating layer. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] JP 2000-210937 A [Patent Document 2] JP 2018-202797 A Summary of the Invention [Problem to be solved by the invention]
[0009] In view of the above circumstances, the present applicant has proposed a method for separating a resin coating layer formed on an inner surface of a metal pipe from the inner surface, which comprises the steps of: creating an inert gas atmosphere inside the metal pipe; positioning a coil constituting a high-frequency induction heating means so as to surround an upper end portion of the metal pipe, induction heating the upper end portion of the metal pipe; and, after the temperature of the outer surface of the metal pipe at the upper end portion exceeds the thermal decomposition temperature of the resin constituting the resin coating layer, continuing induction heating so that the temperature of the outer surface of the metal pipe opposite the center of the coil in the longitudinal direction is maintained at or above the thermal decomposition temperature. The present inventors have proposed a method for separating a resin coating layer on the inner surface of a metal pipe, which includes a step of moving the coil along the outer surface of the metal pipe to a position surrounding the lower end of the metal pipe, thereby sequentially thermally decomposing the constituent resin in the vicinity of the interface between the metal pipe and the resin coating layer from the upper end side to the lower end side of the metal pipe, and sequentially thermally melting the constituent resin other than in the vicinity of the interface from the upper end side to the lower end side of the metal pipe, and discharging the molten constituent resin from an opening on the lower end side of the metal pipe (see the specification of Patent Application No. 2019-133471).
[0010] According to this separation method, the constituent resin of the resin coating layer near the interface with the metal pipe is successively thermally decomposed from the upper end side to the lower end side of the metal pipe, while the constituent resin of the resin coating layer other than near the interface is successively thermally melted from the upper end side to the lower end side of the metal pipe, and the molten resin is separated from the inner surface of the metal pipe and flows toward the lower end, and is discharged from the opening at the lower end.
[0011] Here, the inert gas for creating an inert gas atmosphere inside the metal tube is supplied from the opening at the upper end of the metal tube, flows inside the metal tube from the upper end to the lower end, and is discharged from the opening at the lower end together with the molten resin.
[0012] However, when attempting to separate the resin coating layer formed on the inner surface of a small-diameter metal pipe, such as one with a nominal diameter of 50A or less, using the above-mentioned separation method, the molten resin may get stuck inside the metal pipe, blocking the pipe line and causing delays in subsequent processes. Furthermore, even if an inert gas is supplied under such a condition, the inert gas does not flow below the molten resin that is blocking the metal pipe, so there is a risk of ignition due to induction heating. Such ignition phenomena are likely to occur near the opening of the metal pipe through which the molten resin is discharged.
[0013] The present invention has been made based on the above circumstances. An object of the present invention is to provide a novel separation method capable of easily and reliably separating a resin coating layer formed on the inner surface of a metal pipe from the inner surface. Another object of the present invention is to provide a separation method which prevents the constituent resin of the resin coating layer, other than in the vicinity of the interface, from re-adhering to the inner surface of the metal pipe. It is still another object of the present invention to provide a method for separating a resin coating layer formed on an inner surface of a metal pipe from the inner surface without using fingers or a peeling tool. Yet another object of the present invention is to provide a separation method that can immediately eliminate the resin clogging inside a metal pipe, even if the pipe becomes clogged with molten resin, without causing a fire below the clogged part. Yet another object of the present invention is to provide a separation method capable of reliably recovering such contaminants together with the constituent resin of the resin coating layer when the surface of the resin coating layer is contaminated by radioactive substances or the like. [Means for solving the problem]
[0014] (1) A method for separating a resin coating layer on an inner surface of a metal pipe according to the present invention is a method for separating a resin coating layer formed on an inner surface of a metal pipe having openings at both ends from the inner surface, the method comprising the steps of: The metal tube is raised or tilted, and an opening on the upper end side of the metal tube is closed with a lid having an inert gas injection port; A resin recovery container having an inert gas inlet is connected to the lower end side of the metal pipe, an inert gas is injected into the interior of the metal pipe from the inert gas injection port, and an inert gas is introduced into the interior of the resin recovery container from the inert gas introduction port, thereby maintaining the interior of the metal pipe and the interior of the resin recovery container in an inert gas atmosphere; a coil constituting a high-frequency induction heating means is positioned so as to surround an upper end portion of the metal tube, and the upper end portion of the metal tube is induction-heated; After the outer surface temperature of the metal pipe at the upper end portion exceeds the thermal decomposition temperature of the constituent resin of the resin coating layer, the coil is moved to a position surrounding the lower end of the metal tube while continuing induction heating so that the temperature of the outer surface of the metal tube facing the longitudinal center of the coil is maintained at or above the thermal decomposition temperature, thereby thermally decomposing the constituent resin in the vicinity of the interface between the metal tube and the resin coating layer successively from the upper end to the lower end of the metal tube, and thermally melting the constituent resin other than in the vicinity of the interface successively from the upper end to the lower end of the metal tube, and causing the molten constituent resin to flow down and be discharged from an opening on the lower end of the metal tube.
[0015] According to this separation method, the constituent resin of the resin coating layer near the interface with the metal pipe is successively thermally decomposed from the upper end to the lower end of the metal pipe, while the constituent resin of the resin coating layer other than near the interface is successively thermally melted from the upper end to the lower end of the metal pipe, and the molten resin is separated (peeled off) from the inner surface of the metal pipe and flows toward the lower end, and is discharged from the opening on the lower end side, so that the constituent resin of the resin coating layer other than near the interface does not re-adhere to the inner surface of the metal pipe. Furthermore, the molten resin can be easily separated from the inner surface of the metal pipe without using fingers or a peeling tool.
[0016] In addition, by injecting inert gas into the inside of the metal tube through the inert gas inlet provided in the lid and introducing inert gas into the inside of the resin recovery container through the inert gas introduction port, even if molten resin clogs the inside of the metal tube and blocks the pipeline, the inside of the resin recovery container and the inside of the metal tube below the blocked location can be maintained in an inert gas atmosphere, thereby reliably preventing fire inside the metal tube below the blocked location and inside the resin recovery container.
[0017] In addition, since the opening at the upper end of the metal pipe is closed with a lid having an inert gas injection port and the injected inert gas and pyrolysis gas are not discharged from the opening, when the molten resin clogs the inside of the metal pipe and blocks the pipeline, the internal pressure of the metal pipe above the blocked part rises. As a result, the blocked state can be immediately resolved by forming pores (through holes) in the resin blocking the pipeline that allow the gas to pass through, crushing the resin (lumps), or flowing down the pipeline while maintaining the shape of the lumps and being discharged from the opening at the lower end.
[0018] It is also possible to preheat the metal tube in advance. For example, the method can be carried out after preheating in a heating furnace. When the coil is positioned to surround the upper end of the metal tube, the coil positioned to surround the lower end of the metal tube can be moved upward while preheating the metal tube by induction heating to a position surrounding the upper end of the metal tube. In these preheating steps, it is essential that the temperature of the outer surface of the metal tube does not exceed the thermal decomposition temperature of the constituent resin, and it is preferable that the temperature does not exceed the melting point of the constituent resin.
[0019] (2) In the method for separating a resin-coated layer on the inner surface of a metal pipe according to the present invention, it is preferable that the metal pipe and the resin recovery container are connected in an airtight manner. According to this separation method, it is possible to completely prevent air (oxygen) from flowing into the interior of the metal pipe and the resin recovery container through the connecting portion between them.
[0020] (3) In the method for separating a resin-coated inner surface layer of a metal pipe according to the present invention, it is preferable that the resin recovery container has a gas outlet communicating with a dust collector.
[0021] According to this separation method, pyrolysis gas, black smoke resulting from incomplete combustion, inert gas, etc., which are continuously discharged into the resin recovery container through the opening at the lower end of the metal tube, can be discharged outside the container from the gas exhaust port, and the black smoke resulting from incomplete combustion, etc. can be collected by a dust collector.
[0022] (4) In the method of the present invention for separating a resin coating layer on the inner surface of a metal pipe, it is preferable that a pressure gauge is attached to the lid and the resin coating layer is separated while monitoring the internal pressure of the metal pipe with the pressure gauge.
[0023] According to this separation method, the operator can grasp the internal state of the metal pipe (the occurrence and removal of clogging of the constituent resins) and can take appropriate measures as necessary.
[0024] (5) In the method for separating a resin-coated inner surface layer of a metal pipe according to the present invention, it is preferable that the specific gravity of the inert gas introduced into the resin recovery vessel from the inert gas inlet is greater than 1.0.
[0025] According to this separation method, the inert gas introduced into the resin recovery container from the inert gas inlet can be reliably retained inside the resin recovery container.
[0026] (6) In the method for separating a resin-coated layer on the inner surface of a metal pipe according to the present invention, it is preferable that the resin that constitutes the resin-coated layer is polyethylene.
[0027] (7) In the method for separating a resin coating layer on the inner surface of a metal pipe according to the present invention, it is preferable that 80 mass% or more of the resin coating layer formed on the inner surface of the metal pipe is discharged from an opening on the other end side of the metal pipe and recovered in the resin recovery container. Effect of the Invention
[0028] According to the separation method of the present invention, the resin coating layer formed on the inner surface of the metal pipe can be easily and reliably separated from the inner surface of the metal pipe. In addition, the resin coating layer can be separated without using fingers or a peeling tool, and the constituent resin of the resin coating layer other than in the vicinity of the interface does not re-adhere to the inner surface of the metal pipe. Furthermore, even if molten resin becomes lodged inside the metal pipe and blocks the pipeline, it is possible to reliably prevent fire inside the metal pipe below the blockage and inside the resin recovery container. Furthermore, even if the molten resin becomes clogged inside the metal pipe and blocks the pipe line, the blockage can be immediately resolved by, for example, discharging the resin from the opening on the lower end side. Furthermore, the resin constituting the vicinity of the surface of the resin coating layer can be discharged from the opening at the lower end of the metal pipe and reliably recovered. As a result, if the surface of the resin coating layer is contaminated with radioactive materials or the like, the contaminants such as radioactive materials can be recovered together with the discharged resin. [Brief description of the drawings]
[0029] [Figure 1] FIG. 1 is a schematic diagram showing one embodiment of the present invention, in which a coil constituting a high-frequency induction heating device is positioned so as to surround the outer surface of the upper end of a metal tube, and the upper end of the metal tube is induction heated. [Diagram 2] FIG. 2 is a schematic diagram showing one embodiment of the present invention, illustrating a state in which a coil constituting a high-frequency induction heating device has been moved (lowered) to a position surrounding the outer surface of the lower end of a metal pipe. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0030] The present invention will be described in detail below. The separation method of the present invention is a method for separating (peeling off) a resin coating layer formed (lining) on the inner surface of a metal pipe from the inner surface.
[0031] <Embodiment> 1 and 2 are schematic, partially cutaway views showing an embodiment of the separation method of the present invention. In FIG. 1 and FIG. 2, P1 is a metal tube arranged in an upright position. Both ends of the metal pipe P1 are open, and a resin coating layer L1 is formed on the inner surface of the metal pipe P1.
[0032] Examples of the metal pipe P1 include various steel pipes and copper pipes. The outer diameter of the metal pipe P1 is usually set to 27.2 to 114.3 mm, and a suitable example is set to 60.5 mm (nominal diameter 50A). The thickness of the metal tube P1 is usually 2.9 to 6.0 mm, and a suitable example is 3.9 mm.
[0033] Examples of resins constituting the resin coating layer L1 include thermoplastic resins such as polyolefins such as polyethylene and polypropylene, polyvinyl chloride, polyamide, and fluororesin, and the separation method of the present invention is particularly suitable as a method for separating a coating resin layer L1 made of polyethylene. The thickness of the resin coating layer L1 is usually 0.5 to 3 mm, and a suitable example is 2 mm.
[0034] The separation method of this embodiment is carried out using a blocking lid 10, a high-frequency induction heating device 20, a resin recovery container 30, a first inert gas supplying means 41, a second inert gas supplying means 42, and a dust collecting device 50.
[0035] The blocking lid 10 is an upper lid that blocks the opening at the upper end side of the metal pipe P1. An O-ring (not shown) is interposed between the blocking lid 10 and the metal tube P1, thereby ensuring airtightness between them. The blocking lid 10 is provided with an inert gas injection port 11 and is also fitted with a pressure gauge 13 for measuring the internal pressure of the metal tube P1.
[0036] The high-frequency induction heating device 20 includes a high-frequency power source 21 and a coil 23 that is movable (lifted and lowered) and surrounds the outer surface of the metal pipe P1. 1 and 2, reference numeral 25 denotes a radiation thermometer for measuring the outer surface temperature of metal tube P1 facing the center of coil in the longitudinal direction.
[0037] The resin recovery container 30 is connected to the lower end side of the metal pipe 11 in order to recover the constituent resin of the resin coating layer in a molten state. An O-ring (not shown) is interposed between the resin recovery container 30 and the metal pipe P1, thereby ensuring airtightness between them. The resin recovery container 30 is provided with an inert gas inlet 32 and a gas outlet 34 .
[0038] The first inert gas supply means 41 is connected to the injection port 11 (on the upper end side of the metal tube P1) of the block lid 10 in order to supply an inert gas into the inside of the metal tube P1. The inert gas supplied by the first inert gas supply means 41 may be any gas that can prevent the resin from igniting during induction heating, and nitrogen gas is preferably used.
[0039] The second inert gas supplying means 42 is connected to the inert gas inlet 32 (at the lower end of the metal pipe P1) in order to supply an inert gas into the resin recovery container 30. The inert gas supplied by the second inert gas supply means 42 may be any gas capable of preventing the resin from igniting during induction heating, but from the viewpoint of ensuring that the gas is retained inside the resin recovery container 30 (and is not discharged from the gas exhaust port 34), it is preferable that the specific gravity of the gas be greater than 1.0, and argon gas (specific gravity = 1.38) can be suitably used.
[0040] The dust collector 50 is connected to the gas exhaust port 34 of the resin recovery container 30 in order to suck in and recover black smoke and the like resulting from incomplete combustion.
[0041] In the separation method of this embodiment, first, a blocking lid 10 is airtightly attached to an upright metal pipe P1 to block the opening at the upper end of the metal pipe P1, and a resin recovery container 30 is airtightly connected to the lower end of the metal pipe P1.
[0042] Next, an inert gas is injected into the inside of the metal pipe P1 through the injection port 11 of the blocking lid 10, and an inert gas is introduced into the inside of the resin recovery container 30 through the introduction port 32, thereby creating an inert gas atmosphere inside the metal pipe P1 and inside the resin recovery container 30.
[0043] Thereafter, as shown in FIG. 1, the coil 23 constituting the high-frequency induction heating device 20 is positioned so as to surround the outer surface of the upper end portion of the metal pipe P1, and the upper end portion of the metal pipe P1 is induction heated. After the temperature of the outer surface of the upper end of the metal pipe P1 exceeds the thermal decomposition temperature of the constituent resin of the resin coating layer L1 by induction heating, the coil 23 is moved (lowered) toward the lower end of the metal pipe P1.
[0044] Here, the thermal decomposition temperature of the constituent resin refers to the temperature at which the weight of the resin decreases by 5% when thermal analysis (TG / DTA) is performed under a nitrogen atmosphere, and the thermal decomposition temperature of polyethylene resin is 400 to 450°C.
[0045] In the induction heating by the high-frequency induction heating device 20, the frequency is preferably 2 to 30 kHz, and a suitable example is 20 kHz. The input power is preferably 5 to 120 kW, and a suitable example is 10 kW. The temperature rise rate of the outer surface at the upper end of the metal tube P1 is preferably 1° C. / sec or more, and a suitable example is 10° C. / sec.
[0046] The time from when induction heating of the upper end of the metal tube P1 starts to when the coil 23 starts to descend (stationary heating time) is usually 1 to 60 seconds, and a suitable example is 8 seconds.
[0047] If the stationary heating time is too short, the amount of heat supplied to the upper end of the metal pipe P1 will be insufficient to sufficiently raise the temperature of its outer surface, and the constituent resin of the resin coating layer L1 near the interface with the metal pipe P1 may not be sufficiently pyrolyzed. In such a case, it will be difficult to separate the resin coating layer L1 at the upper end of the metal pipe P1.
[0048] On the other hand, if the stationary heating time is too long, the amount of heat supplied to the upper end of the metal pipe P1 will be excessive, causing the outer surface temperature to become excessively high, and this may result in thermal decomposition of the constituent resin of the resin coating layer L1 other than in the vicinity of the interface.In such a case, it will be impossible to fully recover the constituent resin of the resin coating layer L1 formed on the upper end of the metal pipe P1.
[0049] After the stationary heating time has elapsed, the coil 23 is moved (lowered) along the outer surface of the metal tube P1 to a position surrounding the outer surface of the lower end of the metal tube P1, as shown in Figure 2, while continuing induction heating so that the temperature of the outer surface of the metal tube P1 facing the longitudinal center of the coil 23 is maintained at or above the thermal decomposition temperature of the constituent resin.
[0050] The outer surface temperature of the metal tube P1 facing the longitudinal center of the coil 23 can be controlled (maintained above the thermal decomposition temperature of the constituent resin) by appropriately adjusting the input power and the moving speed of the coil 23 (coil feed speed).
[0051] Here, the moving speed of the coil 23 (coil feed speed) differs depending on the input power, but is preferably 1 to 30 mm / sec, and a suitable example is 3 mm / sec.
[0052] If the coil feed speed is too fast, the amount of heat supplied to the metal tube P1 from the moving coil 23 will be insufficient, and the outer surface temperature of the metal tube P1 cannot be maintained above the thermal decomposition temperature of the constituent resin, and the constituent resin of the resin coating layer L1 near the interface with the metal tube P1 may not be sufficiently thermally decomposed. In such a case, it will be difficult to separate the resin coating layer L1 from the inner surface of the metal tube P1.
[0053] On the other hand, if the coil feed speed is too slow, the amount of heat supplied from the moving coil 23 to the metal tube P1 becomes excessive, causing the outer surface temperature of the metal tube P1 to become excessively high, and even the constituent resin of the resin coating layer L1 other than in the vicinity of the interface with the metal tube P1 will be thermally decomposed. In such a case, the efficiency of recovering the resin coating layer L1 as resin will decrease.
[0054] The outer surface temperature of the metal tube P1 facing the longitudinal center of the moving coil 23 is set to be equal to or higher than the thermal decomposition temperature of the constituent resin of the resin coating layer L1, and preferably, is set to be equal to or higher than the thermal decomposition temperature of the constituent resin and equal to or lower than the thermal decomposition temperature of the constituent resin + 100°C. The actual temperature at the outer surface of the metal tube P1 opposite the longitudinal center of the coil 23 is measured by a radiation thermometer 25 which moves with the coil 23.
[0055] Here, if the thickness of the metal pipe P1 is about 15.9 mm or less, the interface temperature between the metal pipe P1 and the resin coating layer L1 during induction heating becomes approximately equal to the outer surface temperature of the metal pipe P1. Therefore, by maintaining the outer surface temperature of such metal pipe P1 at or above the thermal decomposition temperature of the constituent resin of the resin coating layer L1, the constituent resin in the vicinity of the interface with the metal pipe P1 can be thermally decomposed.
[0056] On the other hand, the thermal conductivity of the constituent resin of the resin coating layer L1 (e.g., polyethylene) is significantly smaller than the thermal conductivity of the constituent metal of the metal pipe P1 (e.g., a steel pipe). Therefore, even if the outer surface temperature of the metal pipe P1 is raised to a temperature above the thermal decomposition temperature of the constituent resin of the resin coating layer L1 (e.g., about the thermal decomposition temperature + 100°C), the constituent resin other than in the vicinity of the interface with the metal pipe P1 will exceed its melting temperature, but will not exceed its thermal decomposition temperature.
[0057] Therefore, by continuing induction heating while lowering the coil 23 so that the outer surface temperature of the metal tube P1 facing the longitudinal center of the coil 23 is maintained above the thermal decomposition temperature of the constituent resin, in particular above the thermal decomposition temperature of the constituent resin and below the thermal decomposition temperature + 100°C, the constituent resin of the resin coating layer L1 near the interface with the metal tube P1 is gradually thermally decomposed from the upper end toward the lower end of the metal tube P1, and the constituent resin other than near the interface which has not reached the thermal decomposition temperature is gradually thermally melted from the upper end toward the lower end of the metal tube P1. Here, the constituent resin of the resin coating layer L1 in the "near interface" with the metal pipe P1 refers to the constituent resin that is present within 0.3t, preferably within 0.1t, in the thickness direction from the interface with the metal pipe P1, where t is the thickness of the resin coating layer L1.
[0058] As the constituent resin in the vicinity of the interface with the metal pipe P1 is gradually thermally decomposed, the adhesive strength of the constituent resin in the areas other than the vicinity of the interface to the inner surface of the metal pipe P1 is lost. In addition, as the constituent resins other than those near the interface are successively thermally melted, the constituent resins flow down the inner surface of the metal pipe P1 due to their own weight, are discharged from the opening at the lower end of the metal pipe P1, and are stored in the resin recovery container 30. In the present invention, so long as the entire constituent resin other than in the vicinity of the interface has fluidity, a portion of the constituent resin other than in the vicinity of the interface (for example, the constituent resin in the vicinity of the surface) does not need to be thermally melted.
[0059] According to the separation method of this embodiment, the constituent resin of the resin coating layer L1 near the interface with the metal pipe P1 is successively thermally decomposed from the upper end side to the lower end side of the metal pipe P1, while the constituent resin of the resin coating layer L1 other than near the interface is successively thermally melted from the upper end side to the lower end side of the metal pipe P1, and the molten resin immediately flows down and is discharged from the opening. Therefore, without using fingers or a peeling tool, the constituent resin of the resin coating layer L1 other than near the interface can be easily and reliably separated from the inner surface of the metal pipe P1, and the constituent resin will not re-adhere. In addition, since the constituent resin of the resin coating layer L1 other than near the interface can be reliably recovered, if the surface of the resin coating layer L1 is contaminated with a radioactive substance, the radioactive substance can be reliably recovered together with the discharged resin.
[0060] In addition, when attempting to separate the resin coating layer L1 formed on the inner surface of a small-diameter metal pipe P1, such as a metal pipe P1 with a nominal diameter of 50A or less, it is conceivable that the molten resin may clog the inside of the metal pipe P1, blocking the pipeline, and the inert gas supplied by the first inert gas supply means 41 through the injection port 11 may not flow below the resin blocking the pipeline. However, in the separation method of this embodiment, not only is the inert gas injected into the inside of the metal pipe P1 from the injection port 11, but the inert gas is also introduced into the resin recovery container 30 through the introduction port 32 by the second inert gas supply means 42, and further introduced into the inside from the opening on the lower end side of the metal pipe P1. Therefore, even if the above-mentioned blockage occurs, the inside of the resin recovery container 30 and the inside of the metal pipe P1 below the blocked portion can be maintained in an inert gas atmosphere, and ignition can be reliably prevented inside the metal pipe P1 below the blocked portion and inside the resin recovery container 30.
[0061] In addition, the opening on the upper end of the metal pipe P1 is closed by a blocking lid 10 having an injection port 11, and the injected inert gas and pyrolysis gas are not discharged from the opening. Therefore, if molten resin clogs the inside of the metal pipe P1 and blocks the pipeline, the internal pressure of the metal pipe P1 above the blocked area will rise, and the resin (lump) blocking the pipeline will form small pores (through holes) that allow gas to pass through, or the resin (lump) will be crushed, or the resin will flow down the pipeline while maintaining the shape of the lump and be discharged from the opening on the lower end, thereby immediately resolving the blocked state.
[0062] In addition, when molten resin clogs the inside of the metal pipe P1 and blocks the pipeline, the pressure measured by the pressure gauge 13 rises, and when the blockage is resolved, the pressure returns to the level before the increase. This enables the operator to grasp the situation inside the metal pipe P1 (occurrence and resolution of the resin clog) and take appropriate measures as necessary. EXAMPLES
[0063] For a polyethylene-lined steel pipe having an outer diameter of 60.5 mm (nominal diameter 50A), a wall thickness of 3.9 mm and a length of 390 mm, on the inner surface of which a resin coating layer (L1) made of polyethylene and having a thickness of 1.7 mm or more was formed, the resin coating layer (L1) was separated from the inner surface of the steel pipe (P1) by the method of the above embodiment under the following conditions. When the inner surface of the steel pipe (P1) after the separation operation was observed, it was found that the resin coating layer (L1) had been completely removed. The recovery rate of the constituent resin of the resin coating layer was calculated from the weight of the (lining) steel pipe before and after the separation operation and the weight of the recovered resin.
[0064] (conditions) Inert gas: Nitrogen gas Induction heating frequency and input power: 20kHz, 10kW Fixed heating time at the top: 8 seconds -External surface temperature at the top end after the fixed heating time: 450℃ Coil feed speed: 3mm / sec The temperature of the outer surface of the metal tube facing the center of the length of the moving coil (23): 400 to 500°C
[0065] (result) Weight of lining steel pipe before separation operation (W1): 1812g Weight of steel pipe after separation (W2): 1713g Weight of recovered resin (W3): 90g Recovery rate (W3 / (W1-W2)) x 100: 91%
[0066] From the above results, it was found that the constituent resin (9%) near the interface of the polyethylene resin coating layer was thermally decomposed, and the constituent resin (91%) other than near the interface was recovered.
[0067] Although one embodiment of the present invention has been described above, the separation method of the present invention is not limited to this, and various modifications are possible. For example, in the above embodiment, the resin recovery container 30 is airtightly connected to the lower end side of the metal pipe 11, but by adjusting (increasing) the amount of inert gas supplied from the first inert gas supply means 41 and / or the second inert gas supply means 42 and making the internal pressure of the metal pipe P1 and the resin recovery container 30 somewhat higher than atmospheric pressure, it is possible to maintain an inert gas atmosphere inside the metal pipe P1 and the resin recovery container 30 without airtightly connecting them.
[0068] Furthermore, in the above embodiment, the outer surface temperature of the metal pipe P1 is measured by the radiation thermometer 25, but the outer surface temperature of the metal pipe may be measured by a thermo tape, a contact thermometer, or the like. In the above embodiment, the metal pipe P1 is arranged in an upright state, but the metal pipe may be arranged in an inclined state. Here, the inclination angle (angle with respect to the horizontal plane) is preferably 30° or more. [Explanation of symbols]
[0069] P1 metal tube L1 resin coating layer 10 Occlusion lid 11 Inert gas inlet 13 Pressure gauge 20 High frequency induction heating device 21 High frequency power supply 23 Coil 25 Radiation thermometer 30 Resin collection container 32 Inert gas inlet 34 Gas exhaust port 41 First inert gas supply means 42 Second inert gas supply means 50 Dust collector
Claims
1. A method for separating a resin coating layer formed on an inner surface of a metal pipe having openings at both ends from the inner surface, comprising the steps of: The metal tube is raised or tilted, and an opening on the upper end side of the metal tube is closed with a lid having an inert gas injection port; A resin recovery container having an inert gas inlet is connected to the lower end side of the metal pipe, an inert gas is injected into the interior of the metal pipe from the inert gas injection port, and an inert gas is introduced into the interior of the resin recovery container from the inert gas introduction port, thereby maintaining the interior of the metal pipe and the interior of the resin recovery container in an inert gas atmosphere; a coil constituting a high-frequency induction heating means is positioned so as to surround an upper end portion of the metal tube, and the upper end portion of the metal tube is induction-heated; After the outer surface temperature of the metal pipe at the upper end portion exceeds the thermal decomposition temperature of the constituent resin of the resin coating layer, a step of: moving the coil to a position surrounding the lower end of the metal tube while continuing induction heating so that the temperature of the outer surface of the metal tube facing the longitudinal center of the coil is maintained at or above the thermal decomposition temperature, thereby thermally decomposing the constituent resin in the vicinity of the interface between the metal tube and the resin coating layer successively from the upper end to the lower end of the metal tube, and thermally melting the constituent resin other than in the vicinity of the interface successively from the upper end to the lower end of the metal tube, and causing the molten constituent resin to flow down and be discharged from an opening on the lower end of the metal tube.
2. 2. The method for separating a resin-coated layer on an inner surface of a metal pipe according to claim 1, further comprising the step of connecting said metal pipe and said resin recovery container in an airtight manner.
3. 3. The method for separating a resin-coated inner surface layer of a metal pipe according to claim 1, wherein the resin recovery container has a gas exhaust port communicating with a dust collector.
4. 4. The method for separating a resin coating layer on an inner surface of a metal pipe according to claim 1, further comprising the step of: attaching a pressure gauge to the lid; and performing a separation operation of the resin coating layer while monitoring the internal pressure of the metal pipe with the pressure gauge.
5. 5. The method for separating a resin-coated inner surface layer of a metal pipe according to claim 1, wherein the specific gravity of the inert gas introduced into the resin recovery container from the inert gas inlet is greater than 1.
0.
6. 6. The method for separating a resin-coated inner surface layer of a metal pipe according to claim 1, wherein a constituent resin of the resin-coated layer is polyethylene.
7. 7. The method for separating a resin coating layer on an inner surface of a metal pipe according to claim 1, wherein 80 mass % or more of the resin coating layer formed on the inner surface of the metal pipe is discharged from an opening on the lower end side of the metal pipe and recovered in the resin recovery container.
Citation Information
Patent Citations
Method and apparatus for rleasing coating plastic of plastic-coated steel tube
JP1996323750A
Method for separation of resin coating on metallic tube inner face
JP2000210937A
Method for separating heat-meltable plastic from waste, method for volume reducing treatment of waste, and apparatus for heat treatment of waste
JP2000225384A
Method for separating resin from resin-lined steel pipe, method for recycling, and recycled resin material
JP2001191330A
Peeling method of metal pipe inner surface resin coating layer
JP2018202797A