Method for manufacturing fiber-resin molded body
The method addresses thickness variations in fiber resin molded bodies by using protrusions to control resin flow and prevent leakage, ensuring consistent molding quality without heating.
Patent Information
- Application Number
- JP2021135338
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-08-23
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2041-08-23
AI Technical Summary
Existing methods for manufacturing fiber resin molded bodies face issues with thickness variations in plate-shaped bodies, leading to potential deformation, resin leakage, or insufficient clamping pressure due to inconsistent thickness.
A method involving injection molding with protrusions on the mold surface or plate-like body to prevent resin leakage and deformation by creating a damming effect, allowing for consistent molding despite thickness variations.
The method effectively prevents resin leakage and deformation, ensuring consistent molding quality without heating, even with varying plate thicknesses, by using protrusions to control resin flow and maintain contact with the plate.
Smart Images

Figure 0007567715000001 
Figure 0007567715000002 
Figure 0007567715000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for producing a fiber resin molding. [Background technology]
[0002] Conventionally, a known method for producing a fiber resin molded body is the technology described in Patent Document 1. Patent Document 1 discloses that a plate-like body (pre-board) containing vegetable fibers and a thermoplastic resin is heated, and then the softened plate-like body is pressed (cold pressed) with a molding die to form a substrate, and in a state where the substrate is pressed with the molding die, molten resin is injected through the molding space to form a fiber resin molded body (molded structure) in which the resin (resin molded body) is bonded to the substrate. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2020-157603 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the process disclosed in Patent Document 1, for example, in order to reduce manufacturing costs, the plate-shaped body is not heated (this is sometimes called a non-heating type) and the plate-shaped body in an unsoftened state is cold-pressed in a mold. In such a process, if there is variation in the thickness of each plate-shaped body, for example, if the plate-shaped body is relatively thick, excessive pressure from the mold may be applied to the plate-shaped body, causing destruction or deformation of the substrate to be molded. In addition, when compressing this plate-shaped body to a desired thickness, the mold clamping pressure may be insufficient. On the other hand, if the plate-shaped body is relatively thin, there is a possibility that the molten resin may leak from between the substrate and the mold when the resin is injected through the molding space.
[0005] The present disclosure is a technology that has been completed based on the above circumstances, and aims to provide a non-heating method for manufacturing a fiber resin molding that can deal with variations in plate thickness from one plate-shaped body to another. [Means for solving the problem]
[0006] The present disclosure relates to a method for manufacturing a fiber resin molding comprising a plate-like body containing at least fibers and resin and a resin structure provided on the plate-like body, the method including an injection molding process in which the plate-like body is sandwiched between a pair of molding dies and resin is injected through a recess provided on a molding surface of the molding dies facing the plate-like body to form the resin structure on the plate-like body, the method being characterized in that at least one of the opposing molding surfaces or the plate-like body is provided with a protrusion on a lateral portion of the recess, protruding toward the other opposing side.
[0007] According to this method for producing a fiber resin molding, even if the plate-like body is relatively thin at least in the portion where the recess is formed (i.e., the portion where the resin structure is formed) and a gap may occur between the plate-like body and the molding surface, the protrusions are arranged on the sides of the recess so as to protrude from at least one of the molding surface or the plate-like body, and the protrusions exhibit a blocking function, thereby preventing the resin from leaking and spreading through the gap between the recess and the plate-like body in the injection molding process. Since the protrusions prevent the resin from leaking and spreading, there is no problem even with press conditions that would cause a gap to occur between the plate-like body and the molding surface, and therefore there is no need to adopt press conditions that make the distance between the pair of molds smaller, and it becomes possible to avoid excessive compression of the plate-like body (particularly, it is possible to avoid a situation in which excessive press pressure is applied to a relatively thick plate-like body caused by plate thickness error, etc.).
[0008] In the injection molding step, the protrusion provided on the molding surface, shaped to conform to the groove-shaped recess, and protruding towards the opposing plate-like body may be brought into contact with the plate-like body.
[0009] According to this method for manufacturing a fiber resin molding, the protrusions can prevent the resin passing through the groove-like recesses from flowing sideways and leaking through the gap between the recesses and the plate-like body during the injection molding process. Depending on the thickness of the plate-like body, the protrusions can be made to bite into the plate-like body and in this state the resin can be injected through the groove-like recesses, further suppressing resin leakage from the gap between the recesses and the plate-like body.
[0010] In the injection molding step, the protrusion protruding in a pointed shape toward the plate-like body may be brought into contact with the plate-like body.
[0011] According to this method for manufacturing a fiber resin molding, depending on the thickness of the plate-like body, it becomes easier for the protrusion to be embedded in the plate-like body, and leakage of resin from the gap between the recess and the plate-like body can be further suppressed.
[0012] In the injection molding step, the protrusions formed on the plate-like body and protruding toward the molding surface may be crushed by being brought into contact with the vicinity of the groove-shaped recesses.
[0013] According to this method for producing a fiber resin molding, the protrusions can prevent the resin passing through the groove-like recesses from flowing sideways through the gap between the recesses and the plate-like body and spreading out. In addition, even if the thickness of the plate-like body varies, the amount of crushing of the protrusions can be appropriately changed (for example, when the distance between a pair of molding dies for multiple plate-like bodies is constant, the thicker the thickness of any plate-like body, the greater the amount of crushing of the protrusions). This makes it possible to appropriately maintain the state in which the protrusions abut and are in close contact with the vicinity of the recesses.
[0014] The manufacturing method of the fiber resin molding includes an incision forming step of forming an incision in the plate-like body, and in the injection molding step, the plate-like body is sandwiched between a pair of molding dies in a manner that the incision is opened by folding the plate-like body, and resin injected through the recess may be filled into the opened incision.
[0015] According to this manufacturing method for a fiber resin molding, the shape of the opened cut portion (i.e., the shape of the folded plate-like body) can be fixed with resin, thereby providing a manufacturing method for a fiber resin molding that can fold a plate-like body at any part and fix the shape without heating it. Effect of the Invention
[0016] According to the present disclosure, it is possible to provide a non-heating method for producing a fiber resin molding that can deal with variations in plate thickness for each plate-shaped body. [Brief description of the drawings]
[0017] [Figure 1] FIG. 1 is a perspective view of a door trim according to a first embodiment, viewed from the front side; [Diagram 2] A perspective view of the door trim from the rear side [Diagram 3] FIG. 1 is a cross-sectional view showing a state in which a fiber mat is pressed by a press mold. [Figure 4] FIG. 13 is a perspective view showing a state in which a cut portion is formed in a pre-board; [Diagram 5] A cross-sectional view showing an embodiment in which a pre-board is arranged between an upper mold and a lower mold. [Figure 6] A cross-sectional view showing the state in which the upper mold is brought close to the lower mold and the pre-board is sandwiched between them. [Figure 7] Enlarged cross-sectional view of the cut area [Figure 8] Cross-sectional view of the first rib forming recess (cross-section taken along line IIX-IIX in Figure 7) [Figure 9] FIG. 11 is a cross-sectional view showing a state in which a resin is injected into a recess while a substrate is sandwiched. [Figure 10] Cross-sectional view near the first rib forming recess (cross-section at the same position as the cross-section in Figure 8) [Figure 11] FIG. 11 is a cross-sectional view showing a state in which the upper die is separated from the lower die to release the door trim. [Figure 12] Cross-sectional view of the vicinity of the first rib molding recess according to the second embodiment [Figure 13] 13 is a cross-sectional view showing a state in which a resin is injected into a recess while a substrate is sandwiched (a cross-section at the same position as the cross-section in FIG. 12). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] <Embodiment 1> A first embodiment of the present disclosure will be described with reference to Fig. 1 to Fig. 11. In this embodiment, a door trim (fiber resin molding) 100 will be described as a vehicle interior material attached to the door of an automobile (vehicle). Each figure will be described with the arrow direction F indicating the forward direction, the arrow direction B indicating the rearward direction, the arrow direction U indicating the upward direction (the front side of the door trim 100), the arrow direction D indicating the downward direction (the rear side of the door trim 100), the arrow direction L indicating the leftward direction, and the arrow direction R indicating the rightward direction.
[0019] As shown in FIG. 1 and FIG. 2, the door trim 100 includes a plate-shaped substrate (plate-shaped body) 1 and a plurality of resin structures 2 provided on the substrate. The substrate 1 includes fibers and resin, and is formed into a plate shape by binding intertwined fibers with resin as a binder. The fibers included in the substrate 1 are not particularly limited, but one or more fibers selected from the group of vegetable fibers, glass fibers, carbon fibers, etc. can be adopted. Among them, vegetable fibers are preferable, and kenaf fibers are preferable. By adopting such fibers as the fibers of the substrate 1, it is possible to improve the strength of the substrate 1 and contribute to the natural environment. The resin included in the substrate 1 is not particularly limited, but polyolefin-based thermoplastic resins such as polypropylene and polyethylene can be adopted from the viewpoints of improving processability and reducing manufacturing costs.
[0020] The base material 1 includes a main body 10 which constitutes the majority of the base material, and bent portions 11 which are disposed on both the left and right sides of the main body 10 and are bent downward from the main body 10 in a crank shape. The bent portions 11 include a cutout portion 18 connected to the main body 10, an inclined portion 14 which is inclined downward as it goes outward in the left-right direction from the cutout portion 18, and a flange portion 16 which extends outward in the left-right direction from the inclined portion 14. The cutout portion 18 has a V-shaped groove which is cut in a V-shape from the front surface 1A side of the base material 1 in a cross-sectional view seen from the front side (or rear side) and extends in the front-rear direction. The upper side (front surface side) of the cutout portion 18 is provided with a linear filling portion 28 which is formed by filling the V-shaped groove of the cutout portion 18 with a thermoplastic resin such as polypropylene, and extends in the front-rear direction.
[0021] 2, on the back surface 1B side of the base material 1, there are provided an attachment boss 20 extending downward from the back surface of the main body portion 10, a first rib 23 extending in both left and right directions from the attachment boss 20 and linear as viewed from below, a second rib 25 extending in the front-rear direction on the back surface side of the cutout portion 18 and linear as viewed from below, and a plurality of plate-shaped retaining ribs 26 provided at regular intervals on the second rib 25. The filling portion 28, the attachment boss 20, the first rib 23, the second rib 25, and the retaining rib 26 are an example of a resin structure 2. Such a resin structure 2 is formed of, for example, polypropylene, which is a thermoplastic resin.
[0022] The mounting boss 20 has a cylindrical portion 21 with its height direction being the up-down direction, and a reinforcing rib 22 extending in both the front-rear direction and the rear-front direction from the upper end of the cylindrical portion 21. The mounting boss 20 is used as a portion for attaching other components such as a door pocket, ornament, arm rest, etc. The retaining rib 26 is in the form of a plate extending in the left-right and up-down plane, and stands so as to bridge the main body portion 10 and the bent portion 11 of the base material 1. The retaining rib 26 suppresses elastic deformation of the bent portion 11 in the up-down direction relative to the main body portion 10.
[0023] The first rib 23 is formed by cooling molten resin that has passed through a first rib molding recess 63 in an injection molding process described below. Similarly, the second rib 25 is formed by cooling molten resin that has passed through a second rib molding recess 64 in an injection molding process described below. The mounting boss 20 and the multiple retaining ribs 26 are connected via the first rib 23 and the second rib 25.
[0024] The mounting boss 20, the retaining rib 26, the first rib 23, and the second rib 25 each have a thin-film portion 29 on the base material 1 side (upper side) that spreads laterally (front-rear and left-right directions on the back surface 1B of the base material 1). The thickness (distance in the up-down direction) of the thin-film portion 29 is thinner than the thicknesses of the mounting boss 20, the retaining rib 26, the first rib 23, and the second rib 25. The thin-film portion 29 is provided on the front-rear and left-right sides of the mounting boss 20, on both the front and rear sides of the first rib 23, on the inner side (one side) of the retaining rib 26 in the left-right direction, and on the inner side (one side) of the second rib 25 in the left-right direction. The thin-film portion 29 is also one of the multiple resin structures 2.
[0025] Next, a description will be given of a manufacturing device for manufacturing the door trim 100. The manufacturing device for the door trim 100 is roughly divided into press dies 30 and 31 for manufacturing a pre-board (plate-like body) 1P by heating and pressing a mat-like fiber mat 1M in which vegetable fibers and resin fibers are intertwined, and a molding device 50 for molding the door trim 100 by sandwiching the pre-board 1P therebetween and injecting resin.
[0026] As shown in FIG. 3, the press dies 30, 31 (sometimes called press plates or hot plates) are provided with a lower die 31 and an upper die 30 disposed at a position facing the lower die 31. The upper die 30 is provided with a drive device (e.g., an electric motor, an air cylinder, a hydraulic cylinder, etc.) not shown, and is a movable die that can move in the vertical direction relative to the lower die 31. The press dies 30, 31 are provided with a heating device such as a heater, and can press the fiber mat 1M while heating it at an arbitrary temperature. Such a heater may be provided in only one of the press dies 30, 31. Note that the heating by the press dies 30, 31 is a process for melting the resin fibers of the fiber mat 1M and bonding it to the vegetable fibers to form the pre-board 1P, and is not a process for softening the pre-board 1P and molding it by bending it, for example, when performing the injection molding process described later (the injection molding process of this technology is performed without heating).
[0027] FIG. 5 shows a cross section of the molding device 50 and the pre-board 1P at a position corresponding to the cross section of line XI-XI in FIG. 2. The molding device 50 has a pair of molding dies 51, 61. The pair of molding dies 51, 61 includes a lower die 61 and an upper die 51 arranged at a position opposite the lower die 61. The upper die 51 is a movable die that is equipped with a driving device (e.g., an electric motor, an air cylinder, a hydraulic cylinder, etc.) not shown and can move in the vertical direction relative to the lower die 61. FIGS. 6 to 10 show a state in which the pair of molding dies 51, 61 are closed by bringing the upper die 51 close to the lower die 61. The upper die 51 has a molding surface 51A that faces the lower die 61 and is recessed upward from the lower die 61 side. The lower die 61 has a molding surface 61A that faces the molding surface 51A of the upper die 51 and bulges toward the upper die 51 side. In the pair of molding dies 51, 61 in a closed state, the space between molding surface 51A of upper die 51 and molding surface 61A of lower die 61 is defined as a first molding space S1.
[0028] The pair of molding dies 51, 61, before closing (open state), place the pre-board 1P between the molding surfaces 51A and 61A, and close the upper die 51 close to the lower die 61, thereby sandwiching the pre-board 1P in the first molding space S1. When placing the pre-board 1P between the pair of molding dies 51, 61, the molding surface 51A is positioned so as to face the front surface 1PA of the pre-board 1P (the surface that will become the front surface 1A of the base material 1), and the molding surface 61A is positioned so as to face the back surface 1PB of the pre-board 1P (the surface that will become the back surface 1B of the base material 1).
[0029] An injection device 41 of, for example, a screw type is attached to the lower mold 61. The injection device 41 is capable of injecting a resin (for example, a thermoplastic resin such as polypropylene) constituting the resin structure 2 in a molten state toward the sprue 62. As shown in Figures 5 and 7, the lower mold 61 includes a sprue 62 that extends from the injection device 41 toward the molding surface 61A and penetrates the lower mold 61 in a tubular shape, a gate 69 provided at an outlet portion of the sprue 62 on the molding surface 61A, and a plurality of recesses 63, 64, 65 that are provided on the molding surface 61A and are recessed portions recessed toward the injection device 41 side (downward). The multiple recesses 63, 64, 65 include a first rib molding recess 63 extending in a groove-like manner from the gate 69 toward the inside in the left-right direction, a second rib molding recess 64 extending in a groove-like manner from the gate 69 toward the outside in the front-to-rear direction (toward the back of the paper in Figure 5) and perpendicular to the first rib molding recess 63, a mounting boss molding recess 65 provided midway through the first rib molding recess 63 (between the two first rib molding recesses 63 provided in the left-right direction), and multiple retaining rib molding recesses (not shown) provided midway through the second rib molding recess.
[0030] The sprue 62 is a flow path that allows the resin injected from the injection device 41 to flow toward the molding surface 61A. The gate 69 is provided at the portion where the first rib molding recess 63 and the second rib molding recess 64 are perpendicular to each other, and is a portion that divides the resin flowing from the sprue 62 into the first rib molding recess 63 and the second rib molding recess 64. The first rib molding recess 63 and the second rib molding recess 64 are flow paths that allow the resin flowing from the gate 69 to pass along the molding surface 61A, and are shallower than the mounting boss molding recess 65 and the holding rib molding recess, and are sometimes called runners. The first rib molding recess 63 is a flow path that allows the resin flowing from the gate 69 to pass inside in the left-right direction (the mounting boss molding recess 65 side). The second rib molding recess 64 is a flow path that allows the resin flowing from the gate 69 to pass outside in the front-rear direction (the holding rib molding recess side).
[0031] As shown in Figs. 5, 7 and 8, the molding surface 61A is provided with two protrusions 66 protruding toward the upper mold 51 side (the back surface 1PB side of the pre-board 1P facing the molding surface 61A when the pre-board 1P is sandwiched in the first molding space S1) at the side portions (front and rear portions) of the first rib molding recess 63. The protrusions 66 extend in the left-right direction along the groove-shaped first rib molding recess 63. The protrusions 66 protrude in a pointed shape from the molding surface 61A toward the back surface 1PB side of the pre-board 1P. The protrusions 66 are also provided on the side portions of the recesses other than the first rib molding recess 63 (the inner portion in the left-right direction of the second rib molding recess 64, the portion around the mounting boss molding recess 65, and the inner portion in the left-right direction of the holding rib molding recess).
[0032] Next, a manufacturing method of the door trim 100 will be described. The manufacturing method of the door trim 100 is roughly divided into a pre-board molding process of molding the fiber mat 1M into a pre-board (plate-like body) 1P, a cut forming process of forming cut portions 18 in the pre-board 1P, and an injection molding process of sandwiching the pre-board 1P between a pair of molding dies 51, 61 and injecting resin through the multiple recesses 63, 64, 65 to form multiple resin structures 2 in the base material (plate-like body) 1, and each process is performed in this order.
[0033] As shown in FIG. 3, in the pre-board molding process, a mat-shaped fiber mat 1M containing fibers and a thermoplastic resin is heated and pressed by press dies 30 and 31. This compresses the fiber mat 1M, and the thermoplastic resin contained in the fiber mat 1M melts. The fiber mat 1M is then cooled and solidified, so that the thermoplastic resin is bonded to the fibers. Next, the cooled and solidified fiber mat 1M is cut into a predetermined size and shape using a cutting machine (not shown) to form a pre-board 1P. The fibers and thermoplastic resin constituting the fiber mat 1M are the same as those described as the fibers and resin contained in the base material 1.
[0034] As shown in Fig. 4, in the cut forming step, a plurality of cuts 18 extending linearly in the front-rear direction are formed on both the left and right sides of the pre-board 1P. The cuts 18 are formed by cutting from the front surface 1PA side of the pre-board 1P with a cutter or the like. The cuts 18 are deep enough not to penetrate to the back surface 1PB side of the pre-board 1P.
[0035] 5, in the injection molding process, the pre-board 1P is placed between the upper die 51 and the lower die 61. At this time, the pre-board 1P is placed so that the front surface 1PA on which the notches 18 are provided faces the molding surface 51A of the upper die 51, and the back surface 1PB faces the molding surface 61A of the lower die 61. In addition, the pre-board 1P is positioned so that the two notches 18 are located directly above the two second rib molding recesses 64.
[0036] Next, as shown in FIG. 6, the upper mold 51 is brought close to the lower mold 61 to close the mold, and the pre-board 1P is sandwiched between the molding surface 51A of the upper mold 51 and the molding surface 61A of the lower mold 61. As a result, the left and right portions 1PC of the pre-board 1P are folded toward the lower mold 61 from the cut portions 18 as starting points to form the folded portions 11, and the pre-board 1P is molded as the base material (plate-like body) 1. In the non-heating injection molding process in this embodiment, the pre-board 1P is not softened by heating, so the multiple cut portions 18 are torn along the front-rear direction (the back-to-front direction of the paper in FIG. 6) to form a continuous linear shape. Also, the cut portions 18 open as if stretched in the left-right direction, and the V-shaped shape in cross section spreads in the left-right direction.
[0037] In the injection molding process, the distance between the molding surface 51A of the upper mold 51 and the molding surface 61A of the lower mold 61 (sometimes referred to as the mold distance) is set based on a representative value (average value, median value, etc.) calculated from the thicknesses of a plurality of pre-boards 1P. For example, the mold distance is preferably equal to or greater than the representative value calculated from the thicknesses of a plurality of pre-boards 1P, more preferably equal to or greater than the maximum value of the error (variation) of the representative value, and even more preferably equal to the maximum value of the error of the representative value. For example, when the average value of the thicknesses of a certain number of pre-boards 1P is 2.5 mm and the error is ±0.3 mm (i.e., when the thicknesses of a certain number of pre-boards 1P vary in the range of 2.2 mm to 2.8 mm), the mold distance is preferably equal to or greater than 2.5 mm, more preferably equal to or greater than 2.8 mm, and even more preferably equal to 2.8 mm. The manufacturing method of the door trim 100 may include a process of measuring the representative value of the thicknesses of such a plurality of pre-boards before the injection molding process. In addition, there may be a small gap, either entirely or partially, between the molding surface 61A of the lower mold 61 and the back surface 1PB of the pre-board 1P (i.e., the back surface 1PB of the pre-board 1P may not be pressed by the molding surface 61A).
[0038] As shown in Fig. 6 to Fig. 8, a pair of molding dies 51, 61 are closed to sandwich the pre-board 1P, and the protrusion 66 is brought into contact with the pre-board 1P from the rear surface 1PB side. The protrusion height of the protrusion 66 protruding from the molding surface 61A toward the pre-board 1P may be a value obtained by subtracting the thickness of the pre-board 1P corresponding to the minimum value of the error of the representative value from the mold distance, or may be a value obtained by subtracting the minimum value from the maximum value of the error of the representative value. For example, if the average value of the thickness of a certain number of pre-boards 1P is 2.5 mm, the error is ±0.3 mm, and the mold distance is 2.8 mm, the protrusion height of the protrusion 66 is set to 0.6 mm. When the protruding height of the protrusion 66 is of such a value, as shown in Figs. 6 to 8, when the thickness of the preboard 1P is relatively thick (for example, when the above average value is 2.5 mm and the thickness of the preboard 1P to be molded is 2.8 mm), the tip 66A of the protrusion 66 located on the upper mold 51 side can be thrust into and bit into the back surface 1PB of the preboard 1P. On the other hand, when the thickness of the preboard 1P is relatively thin (for example, when the above average value is 2.5 mm and the thickness of the preboard 1P to be molded is 2.2 mm), the tip 66A of the protrusion 66 can be abutted against the back surface 1PB of the preboard 1P. The space surrounded by the first rib molding recess 63, the protrusion 66, and the back surface 1PB of the preboard 1P is referred to as the second molding space S2.
[0039] Next, as shown in FIG. 9, the pre-board 1P (base material 1) is held between the pair of molding dies 51 and 61 without changing the mold distance, and molten resin is injected from the injection device 41 into the sprue 62. The resin injected into the sprue 62 flows into the first rib molding recess 63 and the second rib molding recess 64 from the gate 69. The resin passing through the first rib molding recess 63 fills the second molding space S2 (see FIG. 10) and reaches the mounting boss molding recess 65. Then, the resin fills the space surrounded by the mounting boss molding recess 65, the protrusion 66, and the back surface 1B of the base material 1. The resin passing through the second rib molding recess 64 reaches the holding rib molding recess and fills the space surrounded by the second rib molding recess 64, the holding rib molding recess, the protrusion 66, and the back surface 1B of the base material 1.
[0040] The resin that passes through the second rib molding recess 64 permeates the open cut portion 18 located directly above it from the back surface 1B side toward the front surface 1A side, filling the space between the cut portion 18 and the molding surface 51A of the upper mold 51 (the resin is filled into the open cut portion 18).
[0041] The injection of the resin is stopped, and the substrate 1 is kept sandwiched between the pair of molding dies 51, 61 for a predetermined period of time, and the injected resin is cooled and solidified, thereby forming multiple resin structures 2 on the front and back sides of the substrate 1. Specifically, as shown in Figures 9 and 10, when the injected resin solidifies, the resin filling the second molding space S2 is formed as the first rib 23 and the thin film portion 29, the resin filling the space surrounded by the mounting boss molding recess 65, the protrusion 66, and the back surface 1B of the substrate 1 is formed as the mounting boss 20 and the thin film portion 29 (see Figure 2), the resin filling the space surrounded by the second rib molding recess 64, the protrusion 66, and the back surface 1B of the substrate 1 is formed as the second rib 25 and the thin film portion 29, the resin filling the space surrounded by the holding rib molding recess, the protrusion 66, and the back surface 1B of the substrate 1 is formed as the holding rib 26 and the thin film portion 29, and the resin filling the space between the cut-out portion 18 and the molding surface 51A of the upper mold 51 is formed as the filling portion 28.
[0042] 11, upper die 51 is separated from lower die 61 to open the pair of molding dies 51, 61. Then, door trim 100 formed by forming resin structure 2 on base material 1 is released from pair of molding dies 51, 61. The cross section of door trim 100 shown in FIG. 11 corresponds to the cross section taken along line XI-XI in FIG.
[0043] Next, the effect of this embodiment will be described. In this embodiment, a method for manufacturing a door trim 100 including a base material 1 including at least fibers and resin and a resin structure 2 provided on the base material 1 is described, which includes an injection molding step of forming the resin structure 2 on the base material 1 by injecting resin through recesses 63, 64, and 65 provided on a molding surface 61A facing the pre-board 1P in a lower mold 61 while sandwiching the pre-board 1P between a pair of molding dies 51 and 61, and the molding surface 61A facing the pre-board 1P is provided with protrusions 66 protruding toward the pre-board 1P side at the side portions of the recesses 63, 64, and 65.
[0044] According to such a manufacturing method of the door trim 100, even if the plate thickness of the pre-board 1P is relatively thin at least in the portion where the recesses 63, 64, 65 are formed (i.e., the portion where the resin structure 2 is formed) and a gap may occur between the pre-board 1P and the molding surface 61A, the protrusions 66 are arranged protruding from the molding surface 61A at the side portions of the recesses 63, 64, 65, so that the protrusions 66 exhibit a blocking function and can suppress the resin from leaking and spreading through the gap between the side portions of the recesses 63, 64, 65 and the pre-board 1P in the injection molding process. Since the protrusions 66 suppress the resin from leaking and spreading in this way, there is no problem even if the press conditions cause a gap to occur between the pre-board 1P and the molding surface 61A, and therefore it is not necessary to adopt a condition for making the distance between the pair of molds 51, 61 smaller as the press conditions, and it becomes possible to avoid excessive compression of the pre-board 1P (particularly, it is possible to avoid a situation where excessive press pressure is applied to a relatively thick pre-board 1P caused by plate thickness error, etc.).
[0045] In the injection molding process, a protrusion 66 that is provided on the molding surface 61A, has a shape that conforms to the groove-like recesses 63, 64, and protrudes toward the opposing pre-board 1P side, is brought into contact with the pre-board 1P.
[0046] According to such a manufacturing method of the door trim 100, the resin passing through the groove-like recesses 63, 64 in the injection molding process can be prevented from flowing sideways and leaking and spreading through the gaps between the recesses 63, 64 and the pre-board 1P by the protrusions 66. Depending on the thickness of the pre-board 1P, the protrusions 66 can be caused to bite into the pre-board 1P and in this state the resin can be injected through the groove-like recesses 63, 64, so that leakage of the resin from the gaps between the recesses 63, 64 and the pre-board 1P can be further suppressed.
[0047] In the injection molding process, the projection 66 that projects in a pointed shape toward the pre-board 1P is brought into contact with the pre-board 1P.
[0048] According to such a manufacturing method for the door trim 100, depending on the thickness of the pre-board 1P, the protrusion 66 can be easily inserted into the pre-board 1P, and leakage of resin from the gaps between the recesses 63, 64 and the pre-board 1P can be further suppressed.
[0049] The manufacturing method of the door trim 100 includes a cut-out forming process for forming a cut-out portion 18 in the pre-board 1P, and in the injection molding process, the pre-board 1P is sandwiched between a pair of molding dies 51, 61 in a manner that the pre-board 1P is folded so as to open the cut-out portion 18, and resin is injected through the recess 64 to fill the opened cut-out portion 18.
[0050] According to such a manufacturing method of the door trim 100, the shape of the opened cutout portion 18 (i.e., the shape of the folded pre-board 1P) can be fixed with resin. This makes it possible to provide a manufacturing method of the door trim 100 that can fold any part of the pre-board 1P and fix the shape without heating it.
[0051] <Embodiment 2> Next, a second embodiment of the present disclosure will be described with reference to Figures 12 and 13. In this embodiment, the same components as those in the above embodiment are designated by the same reference numerals, and redundant descriptions of the structure, operation, and effects will be omitted.
[0052] As shown in Fig. 12, the pre-board 201P has a protrusion 219 that protrudes from its back surface 201PB toward the molding surface 261A of the lower die 261. The protrusion 219 has a ridge shape extending in the left-right direction (the direction toward the back of the paper) on the side (front-rear direction) of the facing portion 217 that faces the first rib forming recess 63. A lower end 219B of the protrusion 219 has a semi-cylindrical shape in cross section. The protrusions 219 are also provided on the side of portions of the pre-board 201P that face recesses other than the first rib forming recess 63 (the second rib forming recess 64, the mounting boss forming recess 65, and the holding rib forming recess).
[0053] The protrusions 219 are formed when the fiber mat 1M is hot-pressed by the press dies 30 and 31 in the pre-board molding process shown in Fig. 3. Specifically, a groove-like groove extending in one direction, such as the left-right direction, is formed in the lower die 31, and the shape of this groove is transferred to the back surface of the fiber mat 1M by pressing, thereby forming the protrusions 219 extending in one direction like ridges.
[0054] As shown in Fig. 13, in the injection molding process, the pre-board 201P is sandwiched between a pair of molding dies 51, 261, and the protrusion 219 is pressed (contacted) against the molding surface 261A of the lower die 261 to crush the lower end 219B of the protrusion 219. Then, without changing the mold distance in this state, molten resin is injected from the injection device 41 through the sprue 62 and gate 69 into the space between the recesses 63, 64, 65, the partially crushed protrusion 219, and the back surface 201PB of the pre-board 201P (the back surface 201B of the substrate 201). The space between the first rib molding recess 63, the partially crushed protrusion 219, and the back surface 201PB of the pre-board 201P is referred to as a second molding space S2.
[0055] When the resin that is injected through the recesses 63, 64, 65 and fills each space is cooled and solidified, the door trim 200 is manufactured, in which the resin structure 202, such as the thin film portion 229, the first rib 23, the second rib 25, the mounting boss 20, and the retaining rib 26, is formed on the base material 201.
[0056] According to such a manufacturing method of the door trim 200, the resin passing through the groove-like recesses 63, 64 can be prevented from flowing laterally through the gap between the recesses 63, 64 and the pre-board 1P and leaking and spreading, by the protrusion 219. Even if the thickness of the pre-board 201P varies, the amount of crushing of the protrusion 219 can be appropriately changed (for example, when the distance between the pair of molding dies 51, 261 for a plurality of pre-boards 201P is constant, the thicker the thickness of any pre-board 201P, the greater the amount of crushing of the protrusion 219). This makes it possible to suitably maintain the state in which the protrusion 219 abuts against the vicinity of the recesses 63, 64 and is in close contact with them.
[0057] <Other embodiments> The present disclosure is not limited to the embodiments described above and in the drawings, and for example, the following embodiments are also included within the technical scope of the present disclosure. Furthermore, in addition to the embodiments described below, various modifications can be made without departing from the spirit of the present disclosure.
[0058] (1) In the above embodiment, the protrusion is provided on either the forming surface or the pre-board, but this is not limited thereto. For example, the protrusion may be provided on both the forming surface and the pre-board.
[0059] (2) In addition to the above embodiment, the shape of the cutout can be changed as appropriate. For example, the cutout may extend in a straight line from one end of the pre-board to the other end. The cutout may also penetrate to the back side of the pre-board.
[0060] (3) In the injection molding step, the pre-board may be pressed by a pair of molds, i.e., the molding surface of the upper mold may contact and press against the front surface of the pre-board, and the molding surface of the lower mold may contact and press against the back surface of the pre-board.
[0061] (4) The manufacturing method of the fiber resin molding exemplified in the above embodiment can be applied not only to manufacturing door trim as a fiber resin molding but also to manufacturing other vehicle interior materials such as pillar garnish, instrument panel, roof lining, etc. The manufacturing method of the fiber resin molding exemplified in the above embodiment can be applied not only to vehicles but also to manufacturing fiber resin moldings to be mounted on various vehicles. For example, the manufacturing method of the fiber resin molding can be applied to fiber resin moldings to be mounted on vehicles such as trains and recreational vehicles as ground vehicles, airplanes and helicopters as flying vehicles, and ships and submarines as marine and underwater vehicles. [Explanation of symbols]
[0062] 1,201...Base material (plate-shaped body), 1P,201...Preboard (plate-shaped body), 2,202...Resin structure, 11...Bending portion, 18...Notch portion, 20...Mounting boss, 41...Injection device, 51,61,261...Molding die, 61,261...Lower die, 61A,261A...Molding surface of lower die, 63,64,65...Recess, 66,219...Protrusion, 100,200...Door trim (fiber resin molded body)
Claims
1. A method for producing a fiber resin molding comprising a plate-like body including at least fibers and a resin, and a resin structure provided on the plate-like body, comprising: a plate-shaped body manufacturing process in which a mat-shaped fiber mat in which plant fibers and resin fibers are entangled is heated and pressed by a press mold to bond the resin fibers contained in the fiber mat to the plant fibers, and then the fiber mat is cooled and solidified, and cut into a predetermined size and shape to manufacture the plate-shaped body; a cut forming step of forming a cut portion in the plate-like body; an injection molding step of sandwiching the plate-like body between a pair of molds in an unheated state and injecting a resin through a recess provided on a molding surface of the mold facing the plate-like body to form the resin structure on the plate-like body, The molding surface is provided with a protrusion that protrudes in a pointed shape toward the plate-like body at a side portion of the recess, Furthermore, in the injection molding process, the plate-like body is bent in the non-heated state so as to open the cut portion, and the plate-like body is sandwiched between a pair of molding dies, and resin injected through the recess is filled into the opened cut portion.
2. In the cut forming step, a plurality of the cuts extending linearly are formed in a linear arrangement at predetermined intervals and to a depth that does not penetrate to the back surface side of the plate-like body, In the injection molding process, in the non-heated state, the plate-like body is bent so as to open the cut portions, and is sandwiched between the pair of molds, so that the plurality of cut portions are torn and connected to form a single straight line, and the resin injected to pass through the recesses is filled into the single straight line of the cut portions. The method for producing a fiber resin molding according to claim 1 .
Citation Information
Patent Citations
Producing fiber-reinforced component, comprises pressing partially base component, which is at least partially formed from fibers by means of tool, and providing plastic, which is inserted into cavity by cavity of tool in one portion
DE102012009006A1
Injection molding apparatus and injection molding method
JP2005186482A
Method for forming skin to core material and molding machine suitable therefor
JP2005231282A
Resin leak preventing structure
JP2006218666A
Molded structure
JP2020157603A