Manufacturing method of molded body
The method of overflow molding and burr removal addresses resin flow issues in compression molding, ensuring complete filling and stable production of molded bodies with removable burrs, enhancing manufacturing efficiency and quality.
Patent Information
- Application Number
- JP2020160483
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-25
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2040-09-25
AI Technical Summary
Existing compression molding methods face issues with resin flow reduction or decreased fluidity due to temperature drops, leading to incomplete filling and manufacturing defects, particularly when forming preforms without burrs.
A method involving a charging step, compression step, and burr removal step, where molten resin is overflowed between the female and male molds to ensure complete filling, and burrs are formed and then removed, even under conditions of reduced resin input or fluidity.
This approach stabilizes the manufacturing process by ensuring complete filling and allows for efficient production of molded bodies with burrs that can be easily removed, reducing defects and maintaining functional integrity.
Smart Images

Figure 0007568902000001 
Figure 0007568902000002 
Figure 0007568902000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a molded article. [Background technology]
[0002] Patent Document 1 discloses a technique for producing a preform by compression molding. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2008-173931 A Summary of the Invention [Problem to be solved by the invention]
[0004] In Patent Document 1, a preform is formed by compression molding so as not to produce burrs. However, when compression molding is performed so as not to produce burrs, if the amount of resin put into the female mold is slightly less for some reason, or if the ambient temperature drops and the fluidity of the molten resin decreases, there is a risk that the resin will not reach the opening end of the mouth of the preform, resulting in a manufacturing defect.
[0005] The present invention has been made in view of the above circumstances, and provides a method for producing a molded article, which is capable of stably producing a molded article. [Means for solving the problem]
[0006] According to the present invention, there is provided a method for manufacturing a molded body, comprising a pouring step, a compression step, and a burr removal step, in which molten resin is poured into a female mold cavity in the pouring step, a male mold core is inserted into the cavity, the molten resin is sandwiched between the female mold and the male mold, and the molten resin is compressed so that the molten resin overflows from the molding space between the cavity and the core to form a molded body with burrs, and the burr removal step removes the burrs from the molded body.
[0007] In the method of the present invention, compression molding is performed so that the molten resin overflows from the molding space between the female and male dies to form a burr. In this method, the compression molding conditions are set so that the molten resin overflows, so that even if the amount of molten resin input is slightly reduced or the environmental temperature drops and the fluidity of the molten resin decreases, the molding space is filled with molten resin, so the occurrence of manufacturing defects is suppressed and molded bodies can be manufactured stably. Burrs are formed on the molded body, but these burrs can be removed in a burr removal process.
[0008] Various embodiments of the present invention will be described below. The embodiments described below can be combined with each other. Preferably, in the method described above, the molten resin is a multi-layer resin sheet in a molten state. Preferably, in the above-described method, the multilayer resin sheet comprises a lower layer, an intermediate layer, and an upper layer in this order. Preferably, in the above-described method, the multilayer resin sheet is disposed so that the intermediate layer is parallel to a bottom surface of the cavity. Preferably, in the method described above, the molded body has a mouth portion provided with an engaging portion to which a discharge member can be attached, and a body portion continuing from the mouth portion, and the inner surface of the cavity is provided with a portion that determines the outer shape of the mouth portion and a portion that determines the outer shape of the body portion. Preferably, in the method described above, the male mold has a flange portion that protrudes radially beyond the core, and the flange portion is pressed against the female mold to form a thin-walled portion between the burr and the molded body, the thin-walled portion being thinner than the burr. Preferably, in the above-described method, the female mold is provided with an inclined surface continuing to the opening edge of the cavity, and the edge of the flange portion is pressed against the inclined surface. [Brief description of the drawings]
[0009] [Figure 1] 1 is a cross-sectional view of a state after molten resin 2 is poured into a cavity 1a of a female mold 1. FIG. [Diagram 2] 2 is a cross-sectional view showing a state after a core 5a of a male die 5 is pressed against molten resin 2 from the state shown in FIG. 1. FIG. [Diagram 3] 3 is a cross-sectional view of a state after the core 5a is further pressed against the molten resin 2 from the state of FIG. 2 to form a folded-back portion 3b2 in the intermediate layer 3b. [Figure 4] 4 is a cross-sectional view showing a state after the core 5a is further pressed against the molten resin 2 from the state shown in FIG. 3, and the molten resin 2 has reached the opening edge 1d of the cavity 1a of the female mold 1. FIG. [Diagram 5] 5 is a cross-sectional view of the state after core 5a is further pressed against molten resin 2 from the state of FIG. 4, and flange portion 5c is pressed against inclined surface 1e to form thin-walled portion 10 between flash 7 and molded body 8. FIG. [Figure 6] 1 is a cross-sectional view of a state after a female die 1 and a male die 5 have been removed from a molded body 8 with flash 7. FIG. [Figure 7] 4 is a cross-sectional view of a molded body 8 having burrs 7 after the burrs 7 have been removed. FIG. [Figure 8] 13 is a cross-sectional view of a state after burrs 7 have been removed from molded body 8 with burrs 7 without removing female die 1 and male die 5 from molded body 8 with burrs 7. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, embodiments of the present invention will be described. Various features shown in the following embodiments can be combined with each other. Also, each feature can be an invention independently.
[0011] 1. Manufacturing method of molded body A method for producing a molded article according to one embodiment of the present invention will be described with reference to FIGS.
[0012] As shown in FIG. 7, the molded body 8 to be manufactured by this method is a cylindrical body with a bottom. As shown in FIG. 1, the molded body 8 is formed by compression molding using a female mold 1 and a male mold 5. The female mold 1 has a cavity 1a. The cavity 1a has an inner shape that defines the outer shape of the molded body 8 to be manufactured. The male mold 5 has a core 5a. The core 5a is inserted into the cavity 1a of the female mold 1 during molding. The core 5a has an outer shape that defines the inner shape of the molded body 8. When the core 5a is inserted into the cavity 1a, a molding space 6 (shown in FIG. 5) having a shape corresponding to the shape of the molded body 8 is formed between the outer surface of the core 5a and the inner surface of the cavity 1a.
[0013] As shown in Fig. 1, the male die 5 has a core 5a protruding from a base 5b, and the base 5b has a flange portion 5c protruding radially beyond the core 5a. The female die 1 has an inclined surface 1e continuing to an opening edge 1d of the cavity 1a. The inclined surface 1e is inclined so as to spread radially outward in a direction away from the opening edge 1d of the cavity 1a.
[0014] 7, the molded body 8 includes, for example, a mouth portion 8b provided with an engagement portion 8a to which a discharge member (a member used for discharging the contents, such as a cap or a pump) can be attached, and a body portion 8c continuing from the mouth portion 8b. In this case, the inner surface of the cavity 1a is provided with a portion 1f that defines the outer surface shape of the mouth portion 8b, and a portion 1g that defines the outer surface shape of the body portion 8c.
[0015] The method of the present embodiment includes a feeding step, a compression step, and a burr removing step. Each step will be described below.
[0016] 1-1. Feeding process In the casting step, molten resin 2 is cast into a cavity 1a of a female mold 1, as shown in FIG.
[0017] The molten resin 2 is a thermoplastic resin in a molten state. The molten resin 2 may be in a block or sheet form. The molten resin 2 may have a single-layer structure or a multi-layer structure. The molten resin 2 is placed on the bottom surface 1b of the cavity 1a.
[0018] In this embodiment, the molten resin 2 is a multilayer resin sheet 3 in a molten state. The multilayer resin sheet 3 includes a lower layer 3a, an intermediate layer 3b, and an upper layer 3c in this order. The lower layer 3a, the intermediate layer 3b, and the upper layer 3c respectively become an outer layer 8f, an intermediate layer 8g, and an inner layer 8h of the molded body 8 to be manufactured (see FIG. 7). The lower layer 3a and the upper layer 3c are made of, for example, polyolefin (polyethylene, polypropylene, etc.), polyester, etc. The intermediate layer 3b is preferably a barrier layer having better gas barrier properties than the lower layer 3a and the upper layer 3c, and is made of, for example, a resin having excellent gas barrier properties such as EVOH or aromatic polyamide. The multilayer resin sheet 3 is preferably arranged so that the intermediate layer 3b is parallel to the bottom surface 1b. The number of layers of the multilayer resin sheet 3 may be 2 or 4 or more.
[0019] If the width (length in the left-right direction in FIG. 1) of the multilayer resin sheet 3 is W and the thickness (length in the up-down direction in FIG. 1) is T, the value of T / W is, for example, 0.1 to 0.95 (0.56 in FIG. 1), and preferably 0.3 to 0.8. Specifically, this value is, for example, 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, or 0.95, and may be within a range between any two of the numerical values exemplified here. If the depth (length perpendicular to the paper surface in FIG. 1) of the multilayer resin sheet 3 is D, then D / W is, for example, 0.5 to 1.5, and preferably 0.8 to 1.2. Specifically, this value may be, for example, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.1, 1.2, 1.3, 1.4, or 1.5, and may be within a range between any two of the numerical values exemplified here.
[0020] The molded body 8 produced by the method of this embodiment is, for example, a preform used in blow molding of containers and the like. In order to perform blow molding using a preform, it is necessary to produce a preform with a large wall thickness. By using a multilayer resin sheet 3 with a large T / W value, it becomes possible to produce a multilayer preform with a large wall thickness.
[0021] 1-2. Compression process In the compression step, as shown in Figures 2 to 5, a core 5a of a male die 5 is inserted into the cavity 1a, the molten resin 2 is sandwiched between the female die 1 and the male die 5, and the molten resin 2 is compressed so that the molten resin 2 overflows from the molding space 6 between the cavity 1a and the core 5a, forming a molded body 8 with flash 7. Details of this step are as follows. The explanation will be given taking the case where the molten resin 2 is a multilayer resin sheet 3 as an example.
[0022] First, as shown in Fig. 2, the tip 5a1 of the core 5a is pressed against the multilayer resin sheet 3. Then, the area 3d of the multilayer resin sheet 3 where the tip 5a1 is pressed is recessed, and the molten resin 2 is extruded to the outside of the area 3d. At this time, the multilayer resin sheet 3 expands while maintaining its layered structure, and the end 3e of the multilayer resin sheet 3 comes into contact with the side surface 1c of the cavity 1a, resulting in the state shown in Fig. 2.
[0023] When the core 5a is pressed further in this state, the molten resin 2 of the multilayer resin sheet 3 is further extruded from the region 3d. The extruded molten resin 2 is then forced into the gap 9 between the side surface 5a2 of the core 5a and the side surface 1c of the cavity 1a, and moves toward the opening edge 1d of the cavity 1a, as shown in Fig. 3. Since the portion of the molten resin 2 in contact with the side surface 1c is less likely to move, the intermediate layer 3b is likely to have a folded-back portion 3b2 where the intermediate layer 3b is folded back at the crease 3b1, as shown in Fig. 3.
[0024] When the core 5a is pressed further in this state, the molten resin 2 in the multilayer resin sheet 3 is further extruded from the region 3d, and the extruded molten resin 2 moves toward the opening edge 1d of the cavity 1a, and the molten resin 2 reaches the opening edge 1d of the cavity 1a, resulting in the state shown in Fig. 4. In the conventional technology, the pressing of the core 5a is completed in this state, and a molded body without flash is taken out.
[0025] On the other hand, in this embodiment, the core 5a is further pressed in from the state shown in Fig. 4. Then, as shown in Fig. 5, the molten resin 2 overflows from the molding space 6, the overflowing portion becomes flash 7, and a molded body 8 is formed in the molding space 6, so that a molded body 8 with flash 7 is formed.
[0026] In conventional technology, if the amount of resin poured into the female mold was slightly less for some reason, or if the ambient temperature dropped and the fluidity of the resin decreased, production defects were likely to occur. However, in this embodiment, the compression molding conditions are set so that the molten resin 2 overflows, so that even if the amount of molten resin 2 poured is slightly less, or if the ambient temperature drops and the fluidity of the molten resin 2 decreases, the molding space 6 will be filled with molten resin 2, thereby suppressing the occurrence of production defects.
[0027] In addition, when the folded portion 3b2 is formed in the intermediate layer 3b, when the pressing of the core 5a is completed in the state of Fig. 4, the intermediate layer 3b does not reach the opening edge 1d, and as a result, the intermediate layer 8g may not be formed up to the opening end 8e (shown in Fig. 7) of the molded body 8, in which case there is a problem that the function (e.g., gas barrier function) of the intermediate layer 8g is not exhibited in the vicinity of the opening end 8e. On the other hand, in this embodiment, the core 5a is further pressed in from the state of Fig. 4, and at this time, the intermediate layer 3b moves toward the opening end 8e of the molded body 8, so that the occurrence of the problem that the intermediate layer 8g is not formed up to the opening end 8e of the molded body 8 is suppressed.
[0028] 5, the core 5a is pressed until the flange portion 5c is pressed against the female die 1, and a thin-walled portion 10 thinner than the flash 7 is formed between the flash 7 and the molded body 8 by pressing the flange portion 5c against the female die 1. The flash 7 can be separated from the molded body 8 by tearing the thin-walled portion 10.
[0029] Preferably, edge 5c1 of flange portion 5c is pressed against inclined surface 1e. When edge 5c1 is pressed against inclined surface 1e, the area of the contact surface is small, so that the pressure applied to molten resin 2 is large, making it easier to reduce the thickness of thin-walled portion 10.
[0030] 1-3. Burr removal process In the burr removing step, as shown in Figures 6 to 8, the burr 7 is removed from the molded body 8 having the burr 7. The removed burr 7 can be used for the production of recycled resin, etc.
[0031] This step may be performed after removing the female mold 1 and the male mold 5 from the molded body 8 with burrs 7, as shown in Figures 6 to 7, or may be performed without removing the female mold 1 and the male mold 5 from the molded body 8 with burrs 7, as shown in Figure 8.
[0032] Furthermore, the removal of the flash 7 may be performed before or after a post-process is performed on the molded body 8. For example, when the molded body 8 is a preform used for blow molding, an example of the post-process is blow molding. This blow molding may be performed without reheating the molded body 8, or may be performed after reheating the molded body 8.
[0033] In one example, the female die 1 is removed from the molded body 8, and the molded body 8 is placed in a cavity of a split mold for a container with the molded body 8 attached to the male die 5. In this state, air is blown into the molded body 8 through an air flow path built into the male die 5 to perform blow molding. With this method, the blow molded body can be efficiently manufactured. In this case, the burrs may be removed before or after the female die 1 is removed.
[0034] In addition, when the engaging portion 8a is caught by the female mold 1 and the female mold 1 cannot be removed when the molded body 8 is attached to the male mold 5, the female mold 1 may be configured so that a portion including the portion 1f that defines the outer shape of the mouth portion 8b and a portion including the portion 1g that defines the outer shape of the body portion 8c are separable from each other, and blow molding may be performed with the portion 1g removed from the molded body 8 and the portion 1f attached to the molded body 8. The portion 1f may be an integral structure or a split mold. When the portion 1f is an integral structure, the male mold 5 can be removed from the molded body 8 after blow molding, and then the portion 1f can be removed from the molded body 8. When the portion 1f is a split mold, the portion 1f can be removed from the molded body 8 before removing the male mold 5 from the molded body 8 after blow molding.
[0035] Through the above steps, a molded body 8 from which burrs 7 have been removed can be obtained. The volume V1 of the resin constituting the molded body 8 is smaller than the volume V2 of the molten resin 2 poured into the female die 1 by the amount of the burrs 7. Therefore, V2 / V1>1. Furthermore, since an excessive amount of burrs 7 leads to an increase in manufacturing costs, it is preferable that V2 / V1<2. V2 / V1 is preferably 1.05 to 1.5, specifically, for example, 1.05, 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, or 1.95, and may be within a range between any two of the numerical values exemplified here.
[0036] 2. Other embodiments The above method can be used to manufacture containers that can be formed only by compression molding, such as coffee portions, and can also be used to manufacture bottomed cylindrical objects other than containers, such as caps. [Explanation of symbols]
[0037] 1: Female type 1a: Cavity 1b: Bottom 1c: Side 1d: Opening edge 1e: Inclined surface 1f: part 1g: part 2: Molten resin 3: Multi-layer resin sheet 3a: Lower layer 3b: Middle layer 3b1: crease 3b2: Folding part 3c: Upper layer 3d: area 3e :edge 5: Male type 5a: Core 5a1: Tip 5a2: Side 5b: Bass 5c: Flange part 5c1: Edge 6: Molding space 7: Bali 8: Formed body 8a: Engaging part 8b: Mouth part 8c: Barrel part 8d: Bottom part 8e: Open end 8f: Lower layer 8g: Intermediate layer 8h: Upper layer 9: Gap 10: Thin part
Claims
1. A method for producing a molded body, comprising the steps of: The method includes a feeding step, a compression step, and a burr removal step, In the injection step, molten resin is injected into a cavity of a female mold, In the compression step, a male core is inserted into the cavity, the molten resin is sandwiched between the female and male dies, and the molten resin is compressed so that the molten resin overflows from a molding space between the cavity and the core, thereby forming a molded body with flash; The male die includes a flange portion that protrudes radially beyond the core, The flange portion is pressed against the female die to form a thin-walled portion between the flash and the molded body that is thinner than the flash, In the burr removing step, the burrs are removed from the compact.
2. 2. The method of claim 1 , The method, wherein the molten resin is a multilayer resin sheet in a molten state.
3. 3. The method of claim 2, The multilayer resin sheet comprises a lower layer, an intermediate layer, and an upper layer in this order.
4. 4. The method of claim 3, The multilayer resin sheet is positioned such that the intermediate layer is parallel to a bottom surface of the cavity.
5. The method according to any one of claims 1 to 4, The molded body includes a mouth portion provided with an engagement portion to which a discharge member can be attached, and a body portion connected to the mouth portion, The method of claim 1, wherein an inner surface of the cavity has a portion that defines an outer surface shape of the mouth portion and a portion that defines an outer surface shape of the body portion.
6. The method according to any one of claims 1 to 5, The female mold is provided with an inclined surface that is continuous with an opening edge of the cavity, An edge of the flange portion is pressed against the inclined surface.
Citation Information
Patent Citations
Compression molding equipment for compressing and molding preform for blow molding
JP2003159739A
Thermoforming mold for optical lens made of thermoplastic material and its process
JP2005511367A
Preform compression-molding method
JP2008173931A
Method for molding thermoplastic resin-made single wall structure
JP2011031500A
Apparatus and method for forming a concave object
WO2020121190A1