Temperature control mold, resin container manufacturing device and manufacturing method
The temperature adjustment mold with adjustable intermediate molds addresses temperature imbalances in preforms, enabling precise temperature control and improved wall thickness distribution in container shaping.
Patent Information
- Application Number
- JP2023502448
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-02-25
- Filing Date
- 2022-02-22
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-02-22
AI Technical Summary
Conventional temperature adjustment methods using cylindrical heating pots fail to adequately address temperature imbalances in preforms, particularly in forming flat containers, and struggle to selectively heat predetermined portions for improved wall thickness distribution.
A temperature adjustment mold with adjustable intermediate molds that face the preform's outer surface, allowing selective heating and cooling in the circumferential direction to achieve desired temperature distributions.
The mold enables precise control of temperature distribution in preforms, enhancing the shaping of containers by reducing uneven temperatures and improving wall thickness uniformity.
Smart Images

Figure 0007571277000001 
Figure 0007571277000002 
Figure 0007571277000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a temperature adjusting mold, and an apparatus and method for manufacturing a resin container. [Background technology]
[0002] A hot parison type blow molding machine has been known as one of the conventional manufacturing devices for resin containers. The hot parison type blow molding machine is configured to blow mold a resin container by utilizing the heat retained during injection molding of a preform, and is advantageous in that it can manufacture a variety of resin containers with excellent aesthetic appearance compared to the cold parison type.
[0003] Generally, a preform immediately after injection molding has several low-temperature parts extending in the axial direction in the circumferential direction, causing temperature unevenness (temperature bias) in the circumferential direction. Therefore, in a hot parison blow molding cycle, a temperature adjustment process of the preform is performed between the injection molding process and the blow molding process in order to suppress temperature bias in the preform or to give the preform a desired temperature distribution suitable for shaping a container.
[0004] In this type of temperature adjustment process, for example, a cylindrical heating mold (heating pot mold) that houses the preform inside may be used to heat the preform from the outer periphery with radiant heat from the heating pot mold to adjust the temperature. In this case, temperature deviation of the preform is suppressed by arranging the cylindrical heating pot mold close to the low-temperature part of the preform. It has also been proposed to adjust the temperature of the preform using a temperature adjustment device in which pairs of heating blocks and cooling blocks are arranged alternately in the circumferential direction when molding a flat container (for example, Patent Document 1). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent No. 3595613 Summary of the Invention [Problem to be solved by the invention]
[0006] In conventional temperature control using a cylindrical heating pot mold, other than the low-temperature portion of the preform is also heated, so it may be difficult to eliminate temperature deviation appropriately and sufficiently. In addition, when molding a flat container, if the portion of the preform corresponding to the long side of the container can be selectively heated, the thickness distribution of the container can be improved. Therefore, there is a demand for a temperature control mold that can selectively heat a specific portion of the circumferential direction of the preform. [Means for solving the problem]
[0007] One aspect of the present invention is a temperature control mold for controlling the temperature of an injection-molded resin preform having a bottom. The temperature control mold has one or more control sections that face a part of the outer circumferential surface of the body of the preform and locally heat a predetermined portion of the preform in the circumferential direction. a lower die facing the bottom of the preform and supporting the lower end of the adjustment portion; and an upper die facing the neck of the preform and supporting the upper end of the adjustment portion. The adjustment portion is disposed so as to form a gap in the circumferential direction, and the attachment position is adjustable in the circumferential direction. The adjustment section is positioned by being sandwiched between the lower and upper dies. Effect of the Invention
[0008] According to one aspect of the present invention, it is possible to selectively heat a predetermined portion in the circumferential direction of a preform. [Brief description of the drawings]
[0009] [Figure 1] 1 is a diagram showing a schematic configuration of a blow molding device according to an embodiment of the present invention; [Diagram 2] FIG. 4 is a vertical cross-sectional view of the temperature adjustment unit. [Diagram 3] FIG. 2 is an exploded perspective view showing an example of the configuration of a temperature adjusting die of a temperature adjusting unit. [Figure 4] FIG. 13 is a diagram showing an example of an intermediate-stage arrangement of temperature adjustment units. [Diagram 5] 1 is a flow chart showing steps of a blow molding method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the embodiments, in order to make the description easier to understand, structures and elements other than the main parts of the present invention will be described in a simplified or omitted manner. In addition, in the drawings, the same elements are given the same reference numerals. Note that the shapes, dimensions, etc. of each element shown in the drawings are shown only for illustrative purposes, and do not represent the actual shapes, dimensions, etc.
[0011] 1 is a diagram showing a schematic configuration of a blow molding apparatus 20 according to the present embodiment. The blow molding apparatus 20 according to the present embodiment is an apparatus of the hot parison type (also called one-stage type) that blow molds a container by utilizing the heat (internal heat) retained during injection molding without cooling the preform 10 to room temperature.
[0012] The blow molding apparatus 20 includes an injection molding section 21, a temperature adjustment section 22, a blow molding section 23, a removal section 24, and a conveying mechanism 26. The injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 are disposed at positions rotated a predetermined angle (e.g., 90 degrees) around the conveying mechanism 26.
[0013] (Transport mechanism 26) The conveying mechanism 26 includes a transfer plate 28 (not shown in FIG. 1) that moves so as to rotate around an axis perpendicular to the plane of the drawing in FIG. 1. At least one neck mold 27 (not shown in FIG. 1) that holds the neck of the preform 10 or a resin container (hereinafter simply referred to as a container) is arranged at each predetermined angle on the transfer plate 28. The conveying mechanism 26 conveys the preform 10 (or the container) whose neck is held by the neck mold 27 to the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 in this order by moving the transfer plate 28 by 90 degrees at a time. The conveying mechanism 26 further includes a lifting mechanism (vertical mold opening / closing mechanism) and a mold opening mechanism for the neck mold 27, and performs an operation of lifting and lowering the transfer plate 28 and an operation related to mold closing and mold opening (mold release) in the injection molding section 21, etc.
[0014] (Injection molding section 21) The injection molding section 21 includes an injection cavity mold and an injection core mold, both of which are not shown, and manufactures the preform 10 shown in Fig. 2. An injection device 25 that supplies a resin material, which is a raw material of the preform 10, is connected to the injection molding section 21.
[0015] In the injection molding section 21, the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26 are closed to form a mold space having a preform shape. Then, a resin material is poured from an injection device 25 into the mold space having the preform shape, whereby the preform 10 is manufactured in the injection molding section 21. For example, the overall shape of the preform 10 is a cylindrical shape with one end open and the other end closed at a bottom. A neck is formed at the end of the open side of the preform 10.
[0016] The material of the container and the preform 10 is a thermoplastic synthetic resin, and can be appropriately selected according to the application of the container. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexane dimethylene terephthalate), Tritan (Tritan (registered trademark): a copolyester manufactured by Eastman Chemical Co.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPSU (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), PLA (polylactic acid), and the like.
[0017] Incidentally, even when the injection molding section 21 is opened, the neck mold 27 of the transport mechanism 26 is not opened, but continues to hold and transport the preforms 10. The number of preforms 10 simultaneously molded in the injection molding section 21 (i.e., the number of containers that can be simultaneously molded by the blow molding device 20) can be set appropriately.
[0018] (Temperature adjustment section 22) The temperature adjustment section 22 includes a temperature adjustment mold 30 capable of housing the preform 10. The temperature adjustment section 22 uses the temperature adjustment mold 30 to equalize the temperature of the preform 10 manufactured in the injection molding section 21 and remove any temperature deviation, and adjusts the temperature of the preform 10 to a temperature suitable for blow molding (for example, about 90°C to 105°C) and a temperature distribution suitable for the container shape to be formed. The temperature adjustment section 22 also has a function of cooling the preform 10 in a high temperature state after injection molding. Although not particularly limited, the temperature adjustment section 22 may further include a mold member for temperature adjustment (temperature adjustment rod: not shown) inserted inside the preform 10.
[0019] Fig. 2 is a vertical cross-sectional view of the temperature adjusting section 22. Fig. 3 is an exploded perspective view showing an example of the configuration of a temperature adjusting die 30 of the temperature adjusting section 22.
[0020] The temperature control mold 30 is divided into at least three parts in the axial direction (vertical direction) of the preform 10, and includes, from the top, an upper mold 31, a middle mold 32, and a lower mold 33. The lower mold 33 is placed on a support table 34 fixed on the base 29, and an upper support plate 35 is disposed on the upper surface side of the upper mold 31. The support table 34 and the upper support plate 35 are connected by a plurality of pillars (not shown) extending along the axial direction of the preform 10. Therefore, the upper mold 31, the middle mold 32, and the lower mold 33 are sandwiched between the support table 34 and the upper support plate 35, and are fixed in a positioned state.
[0021] The upper die 31 is a die facing (opposing) the outer peripheral surface of the preform 10 near the neck, and has a circular opening through which the preform 10 can be inserted. A heating member (not shown) such as a band heater (ring-shaped heater) is attached to the upper die 31, and the temperature of the upper die 31 can be adjusted to a predetermined temperature by the heating member. In addition, the upper die 31 abuts against the upper end of the middle die 32 to support the middle die 32.
[0022] The lower die 33 is a die facing (opposing) the outer peripheral surface of the bottom of the preform 10, and has a concave curved surface 33a on its upper surface that follows the shape of the bottom of the preform 10. A heating member (not shown) such as a band heater is attached to the lower die 33, and the temperature of the lower die 33 can be adjusted to a predetermined temperature by the heating member. The lower die 33 also abuts against the lower end of the middle die 32 to support the middle die 32.
[0023] The middle mold 32 is an example of an adjustment section (adjustment member) and is a mold that is disposed between the upper mold 31 and the lower mold 33 and faces (opposes) the outer circumferential surface of the body of the preform 10. The bottom surface of the upper mold 31 and the top surface of the middle mold 32, and the bottom surface of the middle mold 32 and the top surface of the lower mold 33 are engaged with each other in a spigot structure, for example, with a heat insulating member sandwiched therebetween.
[0024] As shown in Figures 2 and 3, the middle mold 32 is configured as a strip-shaped piece that is arc-shaped in plan view (at least the inner circumferential surface facing the preform 10 is arc-shaped) and has a constant axial length. Furthermore, the middle mold 32 may have a shape that has a constant radial thickness. For example, the middle mold 32 is a strip-shaped piece that is a quarter circle in plan view and can cover 1 / 4 of the outer periphery of the preform 10. Also, as shown in Figure 2, the middle mold 32 has a built-in heating member 32a such as a rod-shaped heater, and the middle mold 32 The temperature can be adjusted to a predetermined temperature by the heating member 32a.
[0025] One or more intermediate dies 32 are arranged in the circumferential direction of the preform so as to partially cover the outer peripheral surface of the body of the preform 10. In other words, in places where the intermediate dies 32 are not arranged, gaps are formed in the circumferential direction of the temperature control die 30. By partially arranging the intermediate dies 32 in the circumferential direction, the temperature of the body of the preform 10 is adjusted by the temperature control die 30 as follows.
[0026] First, in the portion facing the intermediate die 32 in the circumferential direction, the body of the preform 10 is heated by heat from the intermediate die 32. On the other hand, in the portion in the circumferential direction where the intermediate die 32 is not arranged, the body of the preform 10 is not heated and is naturally cooled by heat dissipation to the air. This makes it possible for the temperature control die 30 to selectively heat desired portions in the circumferential direction while preventing portions other than the desired portions from being excessively heated, making it easy to bring the temperature distribution in the circumferential direction of the preform 10 closer to the desired state.
[0027] FIG. 4 is a diagram showing an example of the arrangement of the middle mold 32 of the temperature adjustment unit 22. As shown in FIG. Fig. 4(A) shows an example in which one intermediate die 32 is arranged. In the case of Fig. 4(A), in a part of the circumferential direction of the preform 10 (located on the left side of the preform 10 in the figure, within a range of 90 degrees in the circumferential direction of the preform 10), the body part of the preform 10 is heated by the intermediate die 32. Also, in the range in the circumferential direction of the preform 10 where the intermediate die 32 is not arranged, the body part of the preform 10 is naturally cooled by heat dissipation to the air.
[0028] 4(B) shows an example in which two intermediate dies 32 are arranged facing each other with a gap in the circumferential direction so as to be point symmetrical. In the case of Fig. 4(B), the body of the preform 10 is heated by the intermediate dies 32 at two points in the circumferential direction of the preform 10 (located above and below the preform 10 in the figure, each within a range of 90 degrees in the circumferential direction of the preform 10). Meanwhile, in the range in the circumferential direction of the preform 10 where the intermediate dies 32 are not arranged, the body of the preform 10 is naturally cooled by heat dissipation to the air.
[0029] Moreover, Fig. 4(C) shows an example in which two middle molds 32 are arranged adjacent to each other. In the case of Fig. 4(C), in the left half of the figure, the body part of the preform 10 is heated by the middle mold 32. On the other hand, in the right half of the figure, the body part of the preform 10 is naturally cooled by heat dissipation to the air.
[0030] 4 is merely an example, and the position of the intermediate mold 32 can be changed as appropriate depending on the temperature deviation state of the preform 10 and the specifications of the container to be shaped. For example, when two intermediate molds 32 are arranged circumferentially with a gap between them, the intermediate molds 32 may be arranged at positions shifted from point symmetrical positions. Also, three intermediate molds 32 may be arranged in the circumferential direction.
[0031] (Blow molding section 23) Returning to FIG. 1, the blow molding section 23 performs stretch blow molding on the preform 10 whose temperature has been adjusted in the temperature adjustment section 22, to manufacture a container. The blow molding section 23 includes a blow cavity mold, which is a pair of split molds corresponding to the shape of the container, a bottom mold, a stretching rod, and an air introduction member (blow core mold, neither of which are shown). The blow molding section 23 blow molds the preform 10 while stretching it. This allows the preform 10 to be shaped into the shape of the blow cavity mold to manufacture a container.
[0032] (Removal part 24) The removal section 24 is configured to release the neck of the container manufactured in the blow molding section 23 from the neck mold 27 and remove the container to the outside of the blow molding apparatus 20.
[0033] (Explanation of the blow molding method) Next, a blow molding method using the blow molding apparatus 20 of this embodiment will be described. 5 is a flow chart showing the steps of the blow molding method. In this embodiment, a mold adjustment step (S100) of adjusting a temperature adjusting mold 30 is performed before each of the steps (S101 to S104) of the blow molding method described below is performed.
[0034] (Step S100: Mold adjustment process) The die adjustment step is a step of adjusting the temperature adjusting die 30 of the temperature adjusting section 22 in accordance with the temperature deviation of the preform 10 and the shape of the container to be formed.
[0035] As an example, in order to suppress temperature deviation of the preform 10, the following work is performed in the mold adjustment process. In the following explanation, it is assumed that the adjustment is performed so as to reduce deviation in the temperature distribution of the preform 10 in the circumferential direction and in the wall thickness distribution of the container.
[0036] First, the blow molding apparatus 20 is test-operated to obtain information on the temperature distribution of the preform 10 or the wall thickness distribution of the container before adjustment.
[0037] For example, if there is a bias in the temperature distribution in the circumferential direction of the preform 10, the worker adjusts the position of the middle die 32 of the temperature adjustment die 30 so that it faces a low-temperature portion of the preform 10. This allows the middle die 32 to locally heat the portion of the preform 10 that has a low temperature during test operation in the circumferential direction, reducing the temperature bias in the circumferential direction of the preform 10.
[0038] Further, when adjusting the temperature adjusting mold 30 based on the distribution of wall thickness of the container manufactured in the test run, the following procedure may be carried out.
[0039] In one-stage blow molding, high-temperature parts of the preform 10 have a large amount of retained heat, and the preform 10 is more likely to be stretched. In other words, the thin-walled parts of the container correspond to the high-temperature parts of the preform 10. On the other hand, low-temperature parts of the preform 10 have less retained heat than the high-temperature parts of the preform 10, and the preform 10 is less likely to be stretched. In other words, the thick-walled parts of the container correspond to the low-temperature parts of the preform 10.
[0040] Therefore, when adjusting the temperature control mold 30 based on the thickness distribution of the container, the thinner parts of the container can be regarded as high temperature parts of the preform 10, and the thicker parts of the container can be regarded as low temperature parts of the preform 10, and the position of the middle mold 32 can be adjusted in the same manner as described above.
[0041] As another example, when adjusting the temperature control mold 30 according to the shape of the container to be formed, the worker adjusts the position of the middle mold 32 in the circumferential direction so that it faces a portion of the preform 10 where the stretch ratio is high in the circumferential direction. For example, when molding an eccentric container, the temperature control mold 30 is adjusted so that the middle mold 32 faces a corresponding portion on the major axis side of the container. This increases the heat retained by the preform 10 in the portion where the stretch ratio is high, making it easier to deform the preform 10 to fit the container shape, thereby improving the wall thickness distribution of the container.
[0042] Here, when assembling the temperature control mold 30, first the lower mold 33 is placed on the support stand 34. Next, the middle mold 32 is placed between the upper mold 31 and the lower mold 33, and columnar members (not shown) are placed between the upper mold 31 and the lower mold 33 in the places where the middle mold 32 is not placed. Then, an upper support plate 35 is placed from above the upper mold 31, and the upper support plate 35 and the support stand 34 are supported by pillars. (not shown) The temperature adjusting mold 30 is sandwiched between the upper mold 31 and the lower mold 33 and fixed in position. The columnar member may be removed from between the upper mold 31 and the lower mold 33. Once the above mold adjustment process is completed, the following steps of the blow molding cycle are carried out.
[0043] (Step S101: Injection molding process) In step S101, in the injection molding section 21, resin is injected from the injection device 25 into a preform-shaped mold space formed by the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26, and the preform 10 is manufactured.
[0044] In step S101, when the injection molding of the preform 10 is completed, the injection molding section 21 is opened and the preform 10 is released from the injection cavity mold and the injection core mold. Next, the transfer plate 28 of the transfer mechanism 26 moves so as to rotate by a predetermined angle, and the preform 10 held by the neck mold 27 is transferred to the temperature adjustment section 22.
[0045] (Step S102: Temperature adjustment process) Next, in the temperature adjusting section 22, temperature adjustment is performed to bring the temperature of the preform 10 close to a temperature suitable for the final blow.
[0046] 2, in the temperature adjustment step, the preform 10 is accommodated in a temperature adjustment mold 30. As a result, the temperature of the preform 10 after injection molding is adjusted by the temperature adjustment mold 30 so that the temperature distribution in the circumferential direction becomes a desired state.
[0047] After the temperature adjustment step, the transfer plate 28 of the conveying mechanism 26 moves so as to rotate by a predetermined angle, and the preform 10 after temperature adjustment held by the neck mold 27 is conveyed to the blow molding section 23 .
[0048] (Step S103: Blow molding process) Next, in the blow molding section 23, the container is blow molded. First, the blow cavity mold is closed to accommodate the preform 10 in the mold space, and the air introduction member (blow core) is lowered to bring the air introduction member into contact with the neck of the preform 10. Then, the stretch rod (vertical axis stretching member) is lowered to hold the bottom of the preform 10 from the inside, and while performing vertical axis stretching as necessary, blow air is supplied from the air introduction member to horizontally stretch the preform 10. As a result, the preform 10 is shaped by expanding so as to fit closely into the mold space of the blow cavity mold, and is blow molded into a container. Note that the bottom mold waits at a lower position where it does not come into contact with the bottom of the preform 10 before the blow cavity mold is closed, and quickly rises to the molding position before or after the mold is closed.
[0049] (Step S104: container removal process) When the blow molding is completed, the blow cavity mold and the bottom mold are opened, so that the container can be removed from the blow molding section 23. Next, the transfer plate 28 of the conveying mechanism 26 moves so as to rotate a predetermined angle, and the container is conveyed to the removal section 24. In the removal section 24, the neck of the container is released from the neck mold 27, and the container is removed to the outside of the blow molding apparatus 20.
[0050] This completes the series of steps in the blow molding cycle. Thereafter, the transfer plate 28 of the conveying mechanism 26 is moved so as to rotate by a predetermined angle, and the above steps S101 to S104 are repeated. When the blow molding apparatus 20 is in operation, four sets of containers are produced in parallel, with a time difference between each step.
[0051] The effects of this embodiment will be described below. The temperature adjusting mold 30 of this embodiment is configured to include one or more intermediate molds 32 that face part of the outer circumferential surface of the body of the preform 10 and locally heat a predetermined portion in the circumferential direction. In this embodiment, by adjusting the circumferential attachment position of the intermediate mold 32 so that it faces a low-temperature portion of the preform 10, it is possible to suppress uneven temperature distribution in the circumferential direction of the preform 10. In addition, when molding an eccentric container, by adjusting the circumferential mounting position of the middle mold 32 so that the middle mold 32 faces the area corresponding to the long diameter side of the container, the circumferential temperature distribution of the preform 10 can be made suitable for shaping the container, and the wall thickness distribution of the container can also be improved.
[0052] In this embodiment, the preform 10 is not heated in the area where the middle die 32 is not arranged, and is naturally cooled by heat dissipation to the air. Therefore, it is possible to prevent excessive heating of the parts of the preform 10 that do not require heating in the circumferential direction, and it becomes easier to appropriately control the temperature distribution in the circumferential direction of the preform 10. Furthermore, compared to a configuration in which the entire circumferential direction is heated, it is possible to reduce energy consumption in the temperature adjustment die 30.
[0053] Here, when the material of the preform 10 is polyethylene (PE) or high density polyethylene (HDPE), the temperature suitable for blow molding is close to the melting point. Moreover, compared with PET and the like, these materials do not have strain hardening characteristics, and it is known that it is difficult to adjust the wall thickness during blow molding. The strain hardening characteristic refers to a characteristic in which the weakest part of the preform (usually the hottest part) first reaches the yield point during the blow process, and then the weakest part begins to stretch, increasing its strength through molecular orientation until the wall thickness becomes uniform. Therefore, when blow molding a PE or HDPE preform, temperature adjustment before blowing is very important, but according to this embodiment, it is easy to adjust the temperature of the preform suitable for molding a PE or HDPE container.
[0054] The present invention is not limited to the above-described embodiment, and various improvements and design changes may be made without departing from the spirit of the present invention.
[0055] In the above embodiment, the circumferential length of the intermediate mold 32 is in the range of 90 degrees (a quarter circle in a plan view) of the circumferential length of the preform 10, but the circumferential length of the intermediate mold 32 can be changed as appropriate. For example, an intermediate mold 32 having a circumferential length corresponding to the circumferential length of the preform 10 in the range of 45 degrees to 180 degrees (preferably in the range of 60 degrees to 120 degrees) may be used. In addition, the circumferential temperature distribution of the preform 10 may be adjusted by selecting and using one or more (for example, one to four) intermediate molds 32 from a plurality of types of intermediate molds 32 having different circumferential lengths. In this case, a plurality of intermediate molds 32 having different circumferential lengths may be used in combination.
[0056] In the above embodiment, the preform 10 having a circular cross section is used, but a preform having a cross section other than a circular cross section may be used. For example, when manufacturing a flat container, a preform having a substantially rectangular cross section may be used.
[0057] In addition, the embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]
[0058] Reference Signs List 10: preform, 20: blow molding device, 21: injection molding section, 22: temperature control section, 23: blow molding section, 30: temperature control mold, 31: upper mold, 32: middle mold, 33: lower mold
Claims
1. A temperature control mold for controlling the temperature of an injection-molded resin preform having a bottom, One or more adjustment units facing a part of an outer peripheral surface of a body portion of the preform and locally heating a predetermined portion in a circumferential direction of the preform; A lower die facing the bottom of the preform and supporting a lower end of the adjustment portion; An upper mold facing the neck portion of the preform and supporting an upper end of the adjustment portion, The adjustment portion is arranged so as to form a gap in the circumferential direction, and an attachment position of the adjustment portion is adjustable in the circumferential direction, The adjustment section is positioned by being sandwiched between the lower die and the upper die. Mold for temperature adjustment.
2. The adjustment portion is disposed in a plurality of positions with gaps in the circumferential direction. The temperature regulating mold according to claim 1 .
3. an injection molding unit that injection molds a resin preform having a bottom; A temperature adjusting unit that adjusts a circumferential temperature distribution of the preform containing the heat retained during injection molding by using the temperature adjusting die according to claim 1 or 2; a blow molding section for producing a resin container by blow molding the temperature-controlled preform; A resin container manufacturing apparatus comprising:
4. An injection molding process of injection molding a resin preform having a bottom; A temperature adjustment process of adjusting a circumferential temperature distribution of the preform containing the heat retained during injection molding using the temperature adjustment mold according to claim 1 or 2; a blow molding step of producing a resin container by blow molding the temperature-controlled preform; A method for manufacturing a resin container having the above structure.
Citation Information
Patent Citations
Temperature controlling method of parison
JP1982089929A
Submarine cable detection method
JP1994102358A
Molding apparatus
JP1994285965A
PREFORM TEMPERATURE CONTROLLER AND BLOW MOLDING METHOD USING THE SAME
JP3595613B2