One-component chloroprene polymer composition
A chloroprene polymer composition with carboxyl groups, petroleum resin, alcohol, and metal compounds addresses heat resistance and contact retention issues, providing effective adhesion and extended open times without formaldehyde.
Patent Information
- Application Number
- JP2020207300
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-12-15
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2040-12-15
AI Technical Summary
Existing one-component chloroprene polymer compositions face issues with heat resistance and contact retention time, particularly when formaldehyde-free and using petroleum resins, leading to poor adhesive properties and short open times.
A one-component chloroprene polymer composition is formulated with a chloroprene polymer containing carboxyl groups, a petroleum resin, an alcohol, and specific metal compounds, balancing heat resistance and contact retention time without formaldehyde emission.
The composition achieves both practical heat resistance and extended contact retention time, ensuring excellent adhesive properties and improved workability while being formaldehyde-free.
Smart Images

Figure 0007571515000001 
Figure 0007571515000002 
Figure 0007571515000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a one-component chloroprene polymer composition containing a carboxyl group-containing chloroprene polymer, a petroleum resin, an alcohol, an organic solvent and a metal compound, and more specifically to a one-component chloroprene polymer composition which enables both heat resistance and contact retention time to be achieved, and which has excellent adhesive properties and is formaldehyde-free. [Background technology]
[0002] Due to their excellent initial adhesion and adhesive strength, adhesion to a wide range of substrates, chemical resistance, and aging resistance, solvent-based chloroprene polymers are used in many industrial fields, such as shoemaking, woodworking, construction, automobiles, home appliances, etc., and are being widely put to practical use industrially. On the other hand, general chloroprene adhesives have an issue with heat resistance due to a decrease in intermolecular cohesive force at temperatures above 60°C caused by decrystallization of chloroprene rubber.
[0003] As a countermeasure, a method is known that improves heat resistance by utilizing room temperature crosslinking of isocyanate. Since the crosslinking reaction between isocyanate and chloroprene rubber is very fast in this method, it is a two-component type in which isocyanate is added and applied just before the application of the adhesive. Since the two-component type has a short adhesive time, its popularity is limited.
[0004] On the other hand, one-component type compositions are known that form a heat-resistant chelate compound (decomposition temperature 250°C or higher) by blending an alkylphenol resin with a metal oxide, thereby compensating for the decrease in the cohesive force of chloroprene rubber. As a one-component type heat-resistant chloroprene polymer composition, a composition containing chloroprene rubber, an alkylphenol resin, and a metal oxide represented by magnesium oxide and zinc oxide has been proposed (see, for example, Patent Document 1). However, the composition proposed in Patent Document 1 has an environmental problem in that formaldehyde is gradually released from the alkylphenol resin, and there is a demand for an environmentally friendly formaldehyde-free one-component chloroprene polymer that does not use an alkylphenol resin.
[0005] Therefore, methods have been proposed that use petroleum resins modified with unsaturated polybasic acids or their anhydrides as an alternative to alkylphenol resins (see, for example, Patent Document 2), and that use petroleum resins with a softening point of 145°C or higher (see, for example, Patent Document 3).
[0006] Furthermore, solvent-based chloroprene polymers used industrially are required to have excellent adhesive contact properties (the property of instantly developing high adhesive strength by simply applying the adhesive to an adherend, drying it, and then lightly laminating the adherends together; this property is sometimes called self-adhesion) and excellent contact property retention time. In particular, if the contact property retention time is long, the drying time (open time) after applying the adhesive to the adherend surface can be extended, greatly improving workability. Furthermore, during actual application, the length of the open time can reduce variation in adhesive strength, which is extremely advantageous in terms of product quality.
[0007] The one-liquid type chloroprene polymer using the above-mentioned alkylphenol resin has a problem of short contact retention time in addition to formaldehyde.
[0008] Further, as chloroprene polymer compositions, there have been proposed a chloroprene polymer composition consisting of 100 parts by weight of a chloroprene polymer, 10 to 200 parts by weight of a tackifier resin, 1 to 15 parts by weight of a metal oxide or metal hydroxide, and an organic solvent (see, for example, Patent Document 4), a chloroprene rubber latex adhesive composition consisting of a chloroprene rubber latex, a tackifier resin emulsion, and a metal oxide emulsion (see, for example, Patent Document 5), and the like. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] Special Publication No. 54-7820 [Patent Document 2] Japanese Unexamined Patent Publication No. 49-128035 [Patent Document 3] Special Publication No. 56-39355 [Patent Document 4] Japanese Patent Application Publication No. 10-212465 [Patent Document 5] Japanese Patent Application Publication No. 10-237404 Summary of the Invention [Problem to be solved by the invention]
[0010] However, the one-liquid compositions proposed in Patent Documents 2 and 3 all have problems with heat resistance at a practical level. Also, the composition proposed in Patent Document 4 has excellent thixotropy, but may have problems with adhesion, contact properties, and contact retention time as an adhesive, while the composition proposed in Patent Document 5 is characterized by being a latex, that is, an emulsion, and is excellent in handleability, but may have problems with adhesion and heat resistance.
[0011] Therefore, an object of the present invention is to provide a one-liquid type chloroprene polymer composition which achieves both practical levels of heat resistance and contact retention time without using an alkylphenol resin which emits formaldehyde. [Means for solving the problem]
[0012] As a result of intensive research aimed at solving these problems, the present inventors have found that a one-component chloroprene polymer composition containing a specific chloroprene polymer, a petroleum resin, an alcohol, an organic solvent, and a specific metal compound can solve the above problems, and have completed the present invention.
[0013] That is, the present invention relates to a one-liquid chloroprene polymer composition comprising 100 parts by weight of a chloroprene polymer containing 0.005 to 1 weight% of carboxyl groups, 1 to 100 parts by weight of a petroleum resin, 5 to 20 parts by weight of an alcohol, 200 to 1,000 parts by weight of an organic solvent, and 0.5 to 15 parts by weight of one or more metal compounds selected from the group consisting of metal oxides and metal hydroxides.
[0014] The present invention will be described in detail below.
[0015] The one-component chloroprene polymer composition of the present invention contains a carboxyl group-containing chloroprene polymer, a petroleum resin, an alcohol, an organic solvent and a metal compound, and is formaldehyde-free and enables a practical level of both heat resistance and contact retention time to be achieved.
[0016] The carboxyl group-containing chloroprene polymer (hereinafter, sometimes referred to as carboxy-modified CR) constituting the one-component chloroprene polymer composition of the present invention is a chloroprene polymer containing a carboxyl group represented by the general formula -COOH in the molecule, and contains 0.005 to 1% by weight of the carboxyl group. If the carboxyl group content is less than 0.005% by weight, the resulting composition will have poor adhesion. On the other hand, if it exceeds 1% by weight, the stability of the resulting composition will be reduced.
[0017] The carboxy-modified CR is not particularly limited as long as it is a chloroprene polymer containing 0.005 to 1% by weight of carboxyl groups, and can be produced, for example, by a method of polymerizing a chloroprene monomer and a carboxyl group-containing vinyl monomer, or by a method of polymerizing a chloroprene monomer and a carboxyl group-containing vinyl monomer together with other copolymerizable ethylenically unsaturated monomers as necessary. Examples of the carboxyl group-containing vinyl monomer in this case include unsaturated fatty acids such as acrylic acid, methacrylic acid, 2-methacryloyloxyethyl succinic acid, 2-methacryloyloxyethyl hexahydrophthalic acid, fumaric acid, maleic anhydride, and crotonic acid, and among these, methacrylic acid is preferred because it has excellent copolymerizability with the chloroprene monomer.
[0018] The carboxy-modified CR may be a commercially available product, and examples thereof include Skyprene (registered trademark) 510 (carboxylic acid group content 0.2% by weight), Skyprene (registered trademark) 510L (carboxylic acid group content 0.2% by weight), Skyprene (registered trademark) 570 (carboxylic acid group content 0.2% by weight), Skyprene (registered trademark) 580 (carboxylic acid group content 0.1% by weight), and Skyprene (registered trademark) 580L (carboxylic acid group content 0.1% by weight), all of which are manufactured by Tosoh Corporation. Among these, Skyprene (registered trademark) 570 (carboxylic acid group content 0.2% by weight) is preferred because of its excellent heat resistance and initial strength. The carboxy-modified CR may also be a mixture of a chloroprene polymer containing a carboxyl group and a simple chloroprene polymer, and examples of the chloroprene polymer in this case include Skyprene (registered trademark) Y-30S, Skyprene (registered trademark) G-40S, and Skyprene (registered trademark) G-40T, all of which are manufactured by Tosoh Corporation.
[0019] The petroleum resin constituting the one-liquid chloroprene polymer composition of the present invention may be any petroleum resin as long as it belongs to the category of petroleum resins, and among them, since the one-liquid chloroprene polymer composition has an excellent balance between heat resistance and contact retention time, it is preferable that the petroleum resin has a softening point of 60 to 140°C, and particularly preferably 70 to 120°C. In addition, it is preferable that the weight average molecular weight (hereinafter sometimes referred to as Mw) is 300 to 5000, and particularly preferably 500 to 4000. In addition, examples of the petroleum resin include aliphatic petroleum resins, aromatic petroleum resins, and aliphatic / aromatic copolymer petroleum resins, and among these, aromatic petroleum resins and aliphatic / aromatic copolymer petroleum resins are preferable.
[0020] Examples of aromatic petroleum resins include resins obtained by homopolymerizing or copolymerizing a C9 fraction having a boiling point range of 140 to 280 ° C. among cracked oils obtained by thermal decomposition of petroleum as a raw material, and examples of aliphatic / aromatic copolymerized petroleum resins include resins obtained by copolymerizing a C5 fraction having a boiling point range of 20 to 110 ° C. obtained by thermal decomposition of petroleum as a raw material with the above-mentioned C9 fraction. In this case, components constituting the C5 fraction include, for example, monoolefinic unsaturated hydrocarbons having 4 to 6 carbon atoms such as 2-methyl-1-butene, 2-methyl-2-butene, 1-pentene, 2-pentene, and cyclopentene; linear dienes having 4 to 6 carbon atoms such as isoprene and piperylene; cyclopentadienes such as cyclopentadiene and methylcyclopentadiene; and aliphatic saturated hydrocarbons such as cyclopentane, 2-methylpentane, 3-methylpentane, and n-hexane. Examples of components constituting the C9 fraction include vinyl aromatic hydrocarbons having 8 to 10 carbon atoms, such as styrene and its alkyl derivatives such as α-methylstyrene and β-methylstyrene, vinyltoluene, indene and its alkyl derivatives, cyclic unsaturated hydrocarbons such as dicyclopentadiene and its derivatives, and saturated aromatics having 9 or more carbon atoms.
[0021] The amount of petroleum resin in the one-component chloroprene polymer composition of the present invention is 10 to 100 parts by weight of petroleum resin per 100 parts by weight of carboxy-modified CR, and is preferably 20 to 60 parts by weight, more preferably 30 to 50 parts by weight, since this results in a one-component chloroprene polymer composition having an excellent balance between heat resistance and contact property retention time. If the petroleum resin is less than 10 parts by weight, the resulting composition will have a short contact property retention time. On the other hand, if it exceeds 100 parts by weight, the resulting composition will have poor heat resistance.
[0022] The metal compound constituting the one-component chloroprene polymer composition of the present invention is one or more metal compounds selected from the group consisting of metal oxides and metal hydroxides, and examples thereof include metal oxides such as magnesium oxide, calcium oxide, cadmium oxide, lead oxide, zinc oxide, and titanium dioxide, and metal hydroxides such as magnesium hydroxide and calcium hydroxide. Among these, magnesium oxide and / or zinc oxide are preferred, as they result in a one-component chloroprene polymer composition having an excellent balance between heat resistance and contact retention time.
[0023] The amount of the metal compound in the one-liquid chloroprene polymer composition of the present invention is 0.5 to 15 parts by weight based on 100 parts by weight of the carboxy-modified CR. If the amount of the metal compound is less than 0.5 parts by weight, the resulting composition will have a short contact retention time. On the other hand, if the amount of the metal compound is more than 15 parts by weight, the resulting composition will have a very high viscosity and will be difficult to handle.
[0024] The alcohol constituting the one-component chloroprene polymer composition of the present invention suppresses an increase in viscosity of the chloroprene polymer composition over time and enables an extension of the pot life, and may be any alcohol as long as it belongs to the category of alcohol. Examples of the alcohol include isopropanol, 1-propanol, isobutanol, and 1-butanol. Among these, isopropanol is preferred because it is particularly excellent in extending the pot life.
[0025] The amount of alcohol in the one-liquid chloroprene polymer composition of the present invention is 5 to 20 parts by mass per 100 parts by weight of the carboxy-modified CR, since this has an excellent effect of suppressing the increase in viscosity of the chloroprene polymer composition. If the amount of alcohol is less than 5 parts by weight, the resulting composition will have a very high viscosity and poor handleability. On the other hand, if the amount of alcohol exceeds 20 parts by weight, precipitation of petroleum resins and the like will be observed, making it difficult to prepare a one-liquid composition.
[0026] In addition, the one-liquid chloroprene polymer composition of the present invention contains an organic solvent in addition to the alcohol because it is a one-liquid composition. The organic solvent may be any that dissolves carboxy-modified CR, petroleum resin, etc., and may include hydrocarbons, chlorinated hydrocarbons, ketones, esters, etc., and specific examples thereof include hydrocarbons such as benzene, toluene, xylene, cyclohexane, n-hexane, n-heptane, petroleum benzine, gasoline, and petroleum spirit; chlorinated hydrocarbons such as methylene chloride, chloroform, carbon tetrachloride, 1,1,1-trichloroethane, and dichloroethane; ketones such as acetone, methyl ethyl ketone, and methyl-n-propyl ketone; and esters such as propyl formate, ethyl acetate, n-propyl acetate, isopropyl acetate, and n-butyl acetate. The amount of the organic solvent is 200 to 1000 parts by weight relative to 100 parts by weight of the carboxy-modified CR. If the amount of the organic solvent is less than 200 parts by weight or more than 1000 parts by weight, the resulting composition will not have a suitable viscosity and will be difficult to handle.
[0027] The one-liquid chloroprene polymer composition of the present invention can be prepared by any method that allows preparation of the composition. Examples of the method include a method of preparing a solution by mixing alcohol, a petroleum resin, and a metal compound and dissolving the carboxy-modified CR therein; and a method of dissolving alcohol, the carboxy-modified CR, the petroleum resin, and the metal compound all at once. Any method can be used.
[0028] The one-liquid chloroprene polymer composition of the present invention is a formaldehyde-free adhesive composition having excellent heat resistance and contact retention time, and can be used as an adhesive, particularly as a heat-resistant adhesive. Effect of the Invention
[0029] According to the present invention, it is possible to provide a one-liquid type chloroprene polymer composition which has both heat resistance and contact retention time suitable for an adhesive and does not emit formaldehyde. EXAMPLES
[0030] The present invention will be described below with reference to examples, but the present invention is not limited to these.
[0031] The following raw materials were used: (1) Aliphatic / aromatic copolymer petroleum resin: (product name) Petrotack 100V (manufactured by Tosoh Corporation). (2) Aromatic copolymer petroleum resin: (trade name) Petcol LX (manufactured by Tosoh Corporation). (3) Alkylphenol resin: (trade name) Tamanol 521 (manufactured by Arakawa Chemical Industries, Ltd.). (4) Carboxy-modified CR: Skyprene (registered trademark) 570 (manufactured by Tosoh Corporation) (carboxyl group content: 0.2% by weight). (5) Chloroprene polymer: Skyprene (registered trademark) G-40S (manufactured by Tosoh Corporation). (6) MgO: (product name) Kyowamag 150 (manufactured by Kyowa Chemical Industry Co., Ltd.). (7) ZnO: manufactured by Sakai Chemical Industry Co., Ltd.
[0032] The analysis and evaluation methods are shown below.
[0033] (a) Measurement of weight average molecular weight (Mw) of petroleum resin Using polystyrene as the standard substance, measurements were performed by gel permeation chromatography in accordance with JIS K-0124 (1994). The measurement results are shown in Table 1.
[0034] (b) Measurement of the softening point of petroleum resin The measurements were performed according to JIS K-2531 (1960) (ring and ball method). The evaluation results are shown in Table 1.
[0035] [Table 1]
[0036] (c) Preparation of adhesive test specimens Two pieces of No. 9 canvas (150mm x 60mm) are brushed with 230g / m2 adhesive on one side of each piece. 2 The adhesive was applied to the board and dried at 80°C for 5 minutes. After cooling at room temperature for 30 minutes, the adhesive was applied again with a brush at a rate of 90 g / m 2 The adhesive was applied to the canvas and dried at 80°C for 5 minutes. After leaving the canvas at room temperature for a certain period of time (open time, 0 to 90 minutes), the two pieces of canvas coated with the adhesive were pressed together with a hand roller. Finally, a test piece measuring 150 mm x 25 mm was cut out.
[0037] (d) Adhesive strength After leaving the test pieces at room temperature (23°C) for a certain period of time, the T-peel adhesion strength was measured at room temperature and at high temperature (80°C) using an Instron tensile tester (Toyo Baldwin, product name UTM-4-100) at a head speed of 100 mm / min. The peel strength 20 minutes after lamination was recorded as the initial strength, the peel strength 5 days after lamination as the normal strength, and the peel strength at 80°C as the heat resistance strength.
[0038] (e) Contact retention time Test pieces were prepared with open times (drying time after applying the adhesive to the adherend surface) of 0, 30, 60, and 90 minutes, and the peel strength was measured. The shortest open time when the test piece was prepared and the initial peel strength was less than 10N / 25mm was regarded as the contact retention time.
[0039] (f) Formaldehyde emission rate evaluation It complies with JISA1901 "Method of measuring emission of volatile organic compounds (VOC), formaldehyde and other carbonyl compounds from building materials - Small chamber method."
[0040] Example 1 The raw materials and solvent as compounding ingredients were placed in a bottle in the prescribed amounts shown in Table 2, and after sealing, the bottle was rotated and mixed on a ball mill stand at room temperature for 48 hours to prepare a one-component chloroprene polymer composition. The evaluation results of the obtained one-component chloroprene polymer composition are shown in Table 2.
[0041] Example 2 A one-liquid type chloroprene polymer composition was prepared in the same manner as in Example 1, except that Petrotac 100V was replaced with Petcol LX. The evaluation results of the obtained one-liquid type chloroprene polymer composition are shown in Table 2.
[0042] Example 3 Except for changing the amount of MgO to 0 part by weight and the amount of ZnO to 0.5 part by weight, a one-liquid type chloroprene polymer composition was prepared in the same manner as in Example 1. The evaluation results of the obtained one-liquid type chloroprene polymer composition are shown in Table 2.
[0043] Example 4 Except for changing the amounts of MgO to 12 parts by weight and ZnO to 3 parts by weight, a one-liquid type chloroprene polymer composition was prepared in the same manner as in Example 1. The evaluation results of the obtained one-liquid type chloroprene polymer composition are shown in Table 2.
[0044] Examples 5 and 6 A one-component chloroprene polymer composition was prepared in the same manner as in Example 1, except that the amount of Petrotac 100V was as shown in Table 2. The evaluation results of the obtained one-component chloroprene polymer composition are shown in Table 2.
[0045] [Table 2]
[0046] Examples 7 to 9 A one-component chloroprene polymer composition was prepared in the same manner as in Example 2, except that the carboxyl group-containing chloroprene polymer was a blend (as shown in Table 3) of a commercially available carboxy-modified CR (Skyprene (registered trademark) 570 (manufactured by Tosoh Corporation)) and a commercially available chloroprene polymer (Skyprene (registered trademark) G-40S (manufactured by Tosoh Corporation)). The evaluation results of the obtained one-component chloroprene polymer composition are shown in Table 3.
[0047] Examples 10 and 11 One-component chloroprene polymer compositions were prepared in the same manner as in Example 1, except that the amount of isopropanol used in Example 1 was changed to the amount shown in Table 3. The evaluation results of the obtained one-component chloroprene polymer compositions are shown in Table 3.
[0048] Example 12 A one-component chloroprene polymer composition was prepared in the same manner as in Example 1, except that 1-butanol was used instead of isopropanol. The evaluation results of the obtained one-component chloroprene polymer composition are shown in Table 3.
[0049] [Table 3]
[0050] Comparative Example 1 A chloroprene polymer composition was prepared in the same manner as in Example 1, except that a resol-type alkylphenol resin was used instead of the petroleum resin Petrotac 100V. The evaluation results of the obtained chloroprene polymer composition are shown in Table 4.
[0051] When resol-type alkylphenol resin was used, the contact retention time was short and formaldehyde emission was observed.
[0052] Comparative Example 2 Except for not using the petroleum resin Petrotac 100V, a chloroprene polymer composition was prepared in the same manner as in Example 1. The evaluation results of the obtained chloroprene polymer composition are shown in Table 4.
[0053] The resulting chloroprene polymer composition had a significantly reduced adhesive strength and did not reach a practical level.
[0054] Comparative Example 3 Except for changing the blend amount of the petroleum resin Petrotac 100V to 110 parts by weight, a chloroprene polymer composition was prepared in the same manner as in Example 1. The evaluation results of the obtained chloroprene polymer composition are shown in Table 4.
[0055] The resulting chloroprene polymer composition had a reduced adhesive strength and did not reach a practical level.
[0056] Comparative Example 4 Except for not using isopropanol, a chloroprene polymer composition was prepared in the same manner as in Example 1. The viscosity of the resulting chloroprene polymer composition after preparation was 100,000 mPa s or more, and it was not possible to coat it, so that it was not possible to prepare a test piece and therefore no evaluation was performed.
[0057] Comparative Example 5 Except for changing the blending amount of isopropanol to 30 parts by weight, a chloroprene polymer composition was prepared in the same manner as in Example 1. The viscosity of the obtained chloroprene polymer composition after preparation was 100,000 mPa s or more, and it was not possible to coat it, so that it was not possible to prepare a test piece and therefore no evaluation was performed.
[0058] Comparative Example 6 Except for not using MgO and ZnO, a chloroprene polymer composition was prepared in the same manner as in Example 1. The evaluation results of the obtained chloroprene polymer composition are shown in Table 4.
[0059] The resulting chloroprene polymer composition had a significantly reduced adhesive strength and did not reach a practical level.
[0060] Comparative Example 7 Except for changing the blending amount of MgO to 16 parts by weight and the blending amount of ZnO to 4 parts by weight, a chloroprene polymer composition was prepared in the same manner as in Example 1. The viscosity of the obtained chloroprene polymer composition after preparation was 100,000 mPa s or more, and it was not possible to coat it, so that it was not possible to prepare a test piece and therefore no evaluation was performed.
[0061] [Table 4] [Industrial Applicability]
[0062] According to the present invention, it is possible to produce a one-component chloroprene polymer which is both heat resistant and has a long contact retention time and is also formaldehyde-free. The polymer has extremely high industrial value as an adhesive which can improve the working environment and reduce costs when used in shoemaking, woodworking, construction, automobiles, home appliances, and the like.
Claims
1. A formaldehyde-free one-liquid chloroprene polymer composition comprising 100 parts by weight of a chloroprene polymer containing 0.005 to 1% by weight of a carboxyl group, 1 to 100 parts by weight of a petroleum resin, 5 to 20 parts by weight of an alcohol, 200 to 1,000 parts by weight of an organic solvent, and 0.5 to 15 parts by weight of one or more metal compounds selected from the group consisting of metal oxides and metal hydroxides.
2. The formaldehyde-free one-liquid chloroprene polymer composition according to claim 1, characterized in that the petroleum resin is an aromatic petroleum resin or an aromatic / aliphatic copolymer petroleum resin having a softening point of 60 to 140°C and a weight average molecular weight of 300 to 5000.
3. 3. The formaldehyde-free one-liquid chloroprene polymer composition according to claim 1, wherein the metal compound is magnesium oxide and / or zinc oxide.
4. 4. The formaldehyde-free one-liquid chloroprene polymer composition according to claim 1, wherein the alcohol is isopropanol and / or 1-butanol.
Citation Information
Patent Citations
JP1974128035A
Compensation circuit for pin cushion distortion at left and right
JP1979007820A
Hydraulic circuit device of liquiddtype torque converter fitted with clutch directly connected
JP1981039355A
Chloroprene-based adhesive of one-pack type