Memory and method for manufacturing the memory

By adjusting the thickness of the work function layer on memory fins, the solution addresses signal interference and stability issues in memory devices, ensuring high threshold voltages and reduced electron diffusion.

JP7575474B2Active Publication Date: 2024-10-29CHANGXIN MEMORY TECH INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022556269
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-08-06
Filing Date
2021-06-30
Publication Date
2024-10-29
Estimated Expiration
2041-06-30

AI Technical Summary

Technical Problem

The continuous shrinking of memory process nodes and narrowing of shallow trench partition structures leads to increased signal interference and reduced memory stability due to the close proximity of fins, causing electron diffusion and reduced retention times.

Method used

Adjusting the thickness of the work function layer on the sidewalls of memory fins to create a higher threshold voltage in opposing regions, thereby reducing the number of movable electrons and minimizing signal interference.

Benefits of technology

Enhances memory stability by reducing electron diffusion and signal interference between adjacent fins, maintaining high threshold voltages with minimal electron collection in the channel region.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007575474000001
    Figure 0007575474000001
  • Figure 0007575474000002
    Figure 0007575474000002
  • Figure 0007575474000003
    Figure 0007575474000003
Patent Text Reader

Abstract

An embodiment of the present application provides a memory and a method for manufacturing the memory. The memory includes first and second fins located on a substrate, a dielectric layer covering tops of the first fins and sidewall surfaces exposed by partition structures, and a work function layer located on the surface of the dielectric layer, wherein, in a direction parallel to an arrangement direction of the first fins and the second fins, the work function layer on opposing sidewalls of adjacent first fins has a first thickness, and the work function layer on a sidewall of the first fin facing the second fin has a second thickness, and the first thickness is greater than the second thickness.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application incorporates and claims priority to a Chinese patent application filed on August 6, 2020, bearing application number 202010784622.3 and entitled "Memory and Method for Manufacturing Memory", the entire contents of which are incorporated herein by reference.

[0002] SUMMARY OF THE DISCLOSURE The present embodiments relate to memories and methods of manufacturing memories. [Background technology]

[0003] A memory is a storage component for storing programs and various data information, and can be divided into a read only memory (ROM) and a random access memory (RAM) according to the type of use of the memory. One memory includes many storage units, and the storage units can store binary codes, which are converted from the storage information. A memory generally includes a capacitor and a transistor connected to the capacitor, the capacitor is for storing charges representing storage information, and the transistor is a switch for controlling the inflow and outflow of charges to the capacitor. Here, a source electrode, a drain electrode, and a gate electrode are formed in the transistor, and the gate electrode is connected to a word line. Summary of the Invention

[0004] An embodiment of the present application provides a memory, the memory comprising a substrate on which first fins and second fins are separated, at least two first fins are located between adjacent second fins, and a distance between adjacent first fins is smaller than a distance between the first fins and the second fins, a surface of the substrate has a partition structure, the partition structure includes a first partition structure and a second partition structure, the first partition structure is located between adjacent first fins, and the second partition structure is located between the first fins and the second fin, and a dielectric layer is formed by the tops of the first fins and the partition structure. the work function layer is located on the surface of the dielectric layer, and in a direction parallel to an arrangement direction of the first fin and the second fin, the work function layer on opposing sidewalls of at least two first fins has a first thickness, and the work function layer on a sidewall of the first fin facing the second fin has a second thickness, the first thickness being greater than the second thickness; and a conductive layer located on the surface of the work function layer.

[0005] The embodiment of the present application further provides a method for manufacturing a memory, the method including: providing a substrate on which first fins and second fins are separated, at least two first fins being located between adjacent second fins, and a distance between the adjacent first fins being smaller than a distance between the first fins and the second fins, a surface of the substrate having a partition structure, the partition structure including a first partition structure and a second partition structure, the first partition structure being located between the adjacent first fins, and the second partition structure being located between the first fins and the second fins, and forming a dielectric layer on tops of the first fins and sidewall surfaces exposed by the partition structure. the dielectric layer covering the top of the second fin and a sidewall surface exposed by the partition structure; forming a work function layer on a surface of the gate dielectric layer, wherein in a direction parallel to an arrangement direction of the first fin and the second fin, the work function layer on opposing sidewalls of at least two first fins has a first thickness, and the work function layer on a sidewall of the first fin toward the second fin has a second thickness, the first thickness being greater than the second thickness; and forming a conductive layer on a surface of the work function layer, wherein a work function value of the conductive layer is smaller than a work function value of the work function layer. Effect of the Invention

[0006] The technical solution according to the embodiment of the present application has at least the following advantages: The memory according to the embodiment of the present invention comprises a work function layer located on the surface of the dielectric layer, and in a direction parallel to the arrangement direction of the first fin and the second fin, the work function layer on the opposing sidewalls of at least two first fins has a first thickness, and the work function layer on the sidewall of the first fin facing the second fin has a second thickness, the first thickness being greater than the second thickness, and the thickness of the work function layer can adjust the threshold voltage in the opposing regions of the adjacent first fins and the region of the first fin facing the adjacent second fin, and the threshold voltage in the opposing regions of the two first fins is greater than the threshold voltage in the region of the first fin facing the second fin. In this way, the number of mobile electrons in the channel region between the adjacent first fins is smaller, and the stability of the memory is higher.

[0007] In addition, in the facing regions of the adjacent first fins along the direction of the substrate facing the first fins, the dielectric layer and the first partition structure surround the first filling region, and the work function layer fills the first filling region, i.e., the facing sidewalls of the two first fins share the work function layer, so that the threshold voltage of the first filling region is larger and the number of mobile electrons in the channel region between the adjacent first fins is smaller, thereby reducing the signal interference between the two first fins.

[0008] Here, the work function layer includes a first work function layer and a second work function layer, the first work function layer covers the entire surface of the dielectric layer, and the second work function layer is located on the first work function layer on the opposing sidewalls of at least two first fins. The thickness of the work function layer on the opposing sidewalls of the two first fins is the total thickness of the first work function layer and the second work function layer, and the total thickness of the first work function layer and the second work function layer is greater than the thickness of the work function layer on the sidewall of the first fin facing the second fin. Thus, the threshold voltage in the opposing regions of the adjacent first fins is greater, the number of mobile electrons in the channel region between the adjacent first fins is relatively small, and the signal interference between the adjacent first fins is also relatively small.

[0009] A method for manufacturing a memory according to an embodiment of the present invention includes forming a work function layer on a surface of a dielectric layer, and in a direction parallel to an arrangement direction of the first fin and the second fin, the work function layer on opposing sidewalls of at least two first fins has a first thickness, and the work function layer on a sidewall of the first fin toward the second fin has a second thickness, and the first thickness is greater than the second thickness. Thus, a threshold voltage in the opposing regions of the two first fins is greater than a threshold voltage in the region of the first fin toward the second fin, and the number of mobile electrons in a channel region between the two first fins is relatively small, thereby reducing signal interference between the two first fins and increasing memory stability. [Brief description of the drawings]

[0010] [Figure 1] FIG. [Diagram 2]2 is a schematic diagram of a cross-sectional structure of a memory taken along the A-A1 cross-sectional line direction of FIG. 1; [Diagram 3] 2 is a schematic diagram of a first cross-sectional structure of a memory taken along the A-A1 cross-sectional line direction in FIG. 1 according to a first embodiment of the present application; [Figure 4] 2 is a schematic diagram of a second cross-sectional structure of the memory taken along the A-A1 cross-sectional line direction in FIG. 1 according to the first embodiment of the present application; [Diagram 5] FIG. 11 is a schematic diagram showing a cross-sectional structure of a memory according to a second embodiment of the present application. [Figure 6] 2A to 2C are structural schematic diagrams corresponding to steps in a manufacturing method for manufacturing a memory according to an embodiment of the present application; [Figure 7] 2A to 2C are structural schematic diagrams corresponding to steps in a manufacturing method for manufacturing a memory according to an embodiment of the present application; [Figure 8] 2A to 2C are structural schematic diagrams corresponding to steps in a manufacturing method for manufacturing a memory according to an embodiment of the present application; [Figure 9] 2A to 2C are structural schematic diagrams corresponding to steps in a manufacturing method for manufacturing a memory according to an embodiment of the present application; [Figure 10] 5A to 5C are structural schematic diagrams corresponding to steps in another manufacturing method for manufacturing a memory according to an embodiment of the present application. [Figure 11] 5A to 5C are structural schematic diagrams corresponding to steps in another manufacturing method for manufacturing a memory according to an embodiment of the present application. [Figure 12] 5A to 5C are structural schematic diagrams corresponding to steps in another manufacturing method for manufacturing a memory according to an embodiment of the present application. [Figure 13] 5A to 5C are structural schematic diagrams corresponding to steps in another manufacturing method for manufacturing a memory according to an embodiment of the present application. [Figure 14] 5A to 5C are structural schematic diagrams corresponding to steps in another manufacturing method for manufacturing a memory according to an embodiment of the present application. [Figure 15] 5A to 5C are structural schematic diagrams corresponding to steps in another manufacturing method for manufacturing a memory according to an embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] One or more embodiments are illustratively illustrated by pictures in corresponding drawings, which are not intended to limit the embodiments, and unless otherwise specified, the figures in the drawings do not constitute a proportional limitation.

[0012] As can be seen from the background, memory has the problem of not being stable.

[0013] Through analysis, it has been found that the main factors causing the above problem include that as the memory process nodes are continually shrinking and the dimensions of the shallow trench partition structure in the active section are continually narrowing, the problem of electronic signal interference between adjacent storage capacitors becomes increasingly serious.

[0014] 1 is a top view of the memory, and FIG. 2 is a schematic diagram of a cross-sectional structure of the memory taken along the line A-A1 of FIG. 1, where the word lines extend in the direction of the line A-A1.

[0015] The analysis will be made with reference to FIGS. 1 and 2. FIG. 1 shows a plurality of active areas 101. FIG. 2 shows four fins 113 and a partition structure 114 between adjacent fins 113. The four fins in FIG. 2 correspond to a cross section of the four active areas 101 along the cross section line A-A1 in FIG. 1. Due to an etching loading effect, the depth of the partition structure between the active areas 101 with a relatively small interval is relatively small, that is, the depth of the partition structure 114 between two fins 113 is relatively small. When the word line 100 performs a read operation, it generates electrons e- in the channel region of the fin 113. For the two central fins 113, because the two central fins 113 are close to each other and the width and depth of the partition structure 114 between these two fins 113 are both small, the first diffusion path a through which the electrons e- diffuse from one fin 113 to another fin 113 is also relatively short, and the electrons e- can easily pass through from under the partition structure 114, which will cause signal interference between adjacent fins 113, i.e., signal interference between two adjacent storage capacitors b and c, and affect the electron retention time of the storage capacitors.

[0016] Further analysis shows that for the two central fins 113, the fins 113 include a first region facing each other and a second region toward the two end fins 113, and the number of diffusible electrons e- in the channel of the first region and the second region are approximately the same. If the number of diffusible electrons e- in the channel region of the first region can be reduced, the problem of electrons e- of the two central fins 113 diffusing each other can be improved.

[0017] In order to solve the above problem, the embodiment of the present application provides a memory and a method for manufacturing the memory. The thickness of the work function layer is adjusted to adjust the threshold voltage in the opposing regions of the two first fins and in the region of the first fin corresponding to the second fin. The thickness of the work function layer on the opposing sidewalls of the adjacent first fins is greater than the thickness of the work function layer on the sidewall of the first fin facing the second fin, so that the threshold voltage in the opposing regions of the adjacent first fins is greater than the threshold voltage in the region of the first fin facing the second fin. Therefore, in the process of the word line 100 performing a read, the threshold voltage in the opposing regions of the adjacent first fins is relatively large, and the number of electrons collected in the channel region is relatively small, i.e., the number of electrons that can diffuse is relatively small. Therefore, the number of electrons that diffuse between the two first fins is relatively small, the signal interference is small, and the stability of the memory is high.

[0018] In order to make the objectives, technical solutions and advantages of the embodiments of the present application clearer, the embodiments of the present application are described in detail below with reference to the drawings. However, as can be understood by those skilled in the art, many technical details are proposed in the embodiments of the present application to help readers to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solutions claimed for protection in the present application can be realized.

[0019] A first embodiment of the present application provides a memory. Figures 3 and 4 are structural schematic diagrams of the memory according to the first embodiment of the present application. Figure 3 is a first cross-sectional structural schematic diagram of the memory taken along the A-A1 cross-sectional line direction in Figure 1. Figure 4 is a second cross-sectional structural schematic diagram of the memory taken along the A-A1 cross-sectional line direction in Figure 1.

[0020] 3 and 4, in this embodiment, the memory includes a substrate 102, a first fin 103 and a second fin 104 that are separate and located on the substrate 102, a dielectric layer 108, a work function layer 109, and a conductive layer 110. At least two first fins 103 are located between adjacent second fins 104, and the spacing between the adjacent first fins 103 is smaller than the spacing between the first fins 103 and the second fins 104. The surface of the substrate 102 has a partition structure 105, and the partition structure 105 includes a first partition structure 106 and a second partition structure 107, and the first partition structure 106 is located between the adjacent first fins 103, and the second partition structure 107 is located between the first fins 103 and the second fins 104. The dielectric layer 108 covers the tops and sidewall surfaces of the first fins 103 exposed by the partition structures 105, and further covers the tops and sidewall surfaces of the second fins 104 exposed by the partition structures 105. The work function layer 109 is located on the surface of the dielectric layer 108, and in a direction parallel to the arrangement direction of the first fins 103 and the second fins 104, the work function layer 109 on the opposing sidewalls of at least two first fins 103 has a first thickness, and the work function layer 109 on the sidewall of the first fins 103 facing the second fins 104 has a second thickness, the first thickness being greater than the second thickness. The conductive layer 110 is located on the surface of the work function layer 109.

[0021] The memory according to this embodiment will be described in detail below with reference to the drawings.

[0022] In this embodiment, the arrangement direction of the first fins 103 and the second fins 104 is the same as the extension direction of the word lines 100 (see FIG. 1), that is, the same as the A-A1 cross-sectional line direction.

[0023] The material of the substrate 102 may include silicon, germanium, or other semiconductor material.

[0024] In this embodiment, the material of the first fin 103 and the second fin 104 is the same as the material of the substrate 102. In other embodiments, the material of the first fin and the second fin may be different from the material of the substrate.

[0025] The material of the partition structure 105 includes silicon dioxide, silicon nitride, silicon carbonitride, or other insulating materials. The first partition structure 106 can block the transmission of electrons between adjacent first fins 103, and the second partition structure 107 can block the transmission of electrons between the first fin 103 and the adjacent second fin 104.

[0026] Along the extension direction of the word line 100 (see FIG. 1), the width of the first partition structure 106 is smaller than the width of the second partition structure 107. In a direction perpendicular to the extension direction of the word line 100 (see FIG. 1), the depth of the first partition structure 106 is smaller than the depth of the second partition structure 107.

[0027] In this embodiment, the upper surface of the first partition structure 106 is higher than the upper surface of the second partition structure 107, and in other embodiments, the upper surface of the first partition structure may be flush with the second partition structure.

[0028] The dielectric layer 108 is the gate dielectric layer of the memory. The dielectric layer 108 further covers the top surface of the partition structure 105. In other embodiments, the dielectric layer may not cover the top surface of the partition structure.

[0029] The material of the dielectric layer 108 includes silicon dioxide or other high dielectric constant materials.

[0030] By adjusting the thickness of the work function layer 109 between the adjacent first fins 103, the threshold voltage of the facing region of the adjacent first fins 103 can be adjusted, and further, the number of electrons that can diffuse in the channel region between the adjacent first fins 103 can be adjusted. In this embodiment, the thickness of the work function layer 109 on the facing sidewalls of the adjacent first fins 103 is greater than the thickness of the work function layer 109 on the sidewall of the first fin 103 toward the second fin 104, so that the threshold voltage in the facing region of the adjacent first fin 103 is greater than the threshold voltage in the region of the first fin 103 toward the second fin 104. When the applied actuation voltage remains unchanged, the threshold voltage becomes larger, the number of electrons that can be actuated by the actuation voltage becomes smaller, and the number of electrons that can be collected in the channel region becomes smaller, thereby reducing the movement of electrons between the first fins 103 and reducing the problem of memory units interfering with each other.

[0031] In a direction parallel to the arrangement direction of the first fins 103 and the second fins 104, the work function layer 109 on the opposing sidewalls of at least two first fins 103 has a first thickness, and the work function layer 109 on the sidewall of the first fins 103 facing the second fin 104 has a second thickness, the first thickness being greater than the second thickness, and the thickness difference is 3 nm to 30 nm, and may further be 5-20 nm or 8-15 nm. By maintaining the thickness difference within a relatively large range, the difference between the threshold voltage in the opposing region of the adjacent first fins 103 and the threshold voltage of the region of the first fin 103 facing the second fin 104 can be maintained within a relatively large range. In this way, the number of diffusible electrons in the channel region between the first fins 103 is relatively small, and signal interference is relatively small.

[0032] Here, the first thickness may be 5-50 nm, for example 10 nm, 20 nm or 40 nm, and the second thickness may be 2-30 nm, for example 2 nm, 5 nm or 15 nm.

[0033] 3, in the direction in which the substrate 102 faces the first fin 103, the dielectric layer 108 and the first partition structure 106 surround a first filling region in the facing region of the adjacent first fin 103. In this embodiment, the dielectric layer 108 further covers the upper surface of the first partition structure 106, so that the dielectric layer 108 surrounds the first filling region, and the work function layer 109 fills the first filling region, and the width of the first filling region is 8-50 nm, and can also be 10-40 nm or 12-30 nm.

[0034] Compared to covering only the sidewalls of the first fin 103, filling the first filling region with the work function layer 109 is advantageous in further increasing the threshold voltage in the opposing regions of adjacent first fins 103, thereby reducing the number of diffusible electrons in the channel region between adjacent first fins 103 and reducing signal interference of the memory unit.

[0035] In another embodiment, referring to FIG. 4, adjacent first fins 103 have gaps between the work function layers 109 on opposing sidewalls.

[0036] The material of the work function layer 109 includes titanium nitride, cobalt, or nickel, which has a relatively high work function. The work function layer 109 may be made of a single material or may be made of a plurality of materials. In this embodiment, the material of the work function layer 109 is titanium nitride.

[0037] The work function of the work function layer 109 is larger than that of the conductive layer 110, the conductive layer 110 is a word line, and the material of the conductive layer includes tungsten or other conductive material.

[0038] In short, the thickness of the work function layer 109 on the opposing sidewalls of the adjacent first fins 103 in this embodiment is greater than the thickness of the work function layer 109 on the sidewall of the first fin 103 facing the adjacent second fin 104, so that the threshold voltage of the opposing regions of the adjacent first fins 103 is greater than the threshold voltage of the region of the first fin 103 facing the second fin 104. In this way, it is favorable to reduce the number of electrons collected in the channel region, which can be operated at the same operating voltage, thereby reducing the number of electrons moving by the channel region, and further reducing the signal interference between the adjacent first fins 103, and improving the stability of the memory.

[0039] The second embodiment of the present application provides a memory. The memory is almost the same as the above embodiment, but the main difference is that the work function layer includes a first work function layer and a second work function layer. Hereinafter, the memory according to the second embodiment of the present application will be described in detail with reference to the drawings. It should be noted that the same or corresponding parts as the above embodiment may refer to the detailed description in the above embodiment, and the description will be omitted here. FIG. 5 is a structural schematic diagram of the memory according to the second embodiment of the present application.

[0040] 5, the memory includes a substrate 202, a first fin 203 and a second fin 204 that are separate and located on the substrate 202, a partition structure 205 located on the surface of the substrate 202, a dielectric layer 208, a work function layer 209, and a conductive layer 210. The partition structure 205 includes a first partition structure 206 and a second partition structure 207, where the first partition structure 206 is located between adjacent first fins 203, and the second partition structure 207 is located between the first fin 203 and the second fin 204. The dielectric layer 208 covers the top of the first fin 203 and the sidewall surface exposed by the partition structure 205, and further covers the top of the second fin 204 and the sidewall surface exposed by the partition structure 205. The work function layer 209 is located on the surface of the dielectric layer 208. The conductive layer 210 is located on the surface of the work function layer 209.

[0041] In this embodiment, the work function layer 209 includes a first work function layer 211 covering the entire surface of the dielectric layer 208 and a second work function layer 212 located on the first work function layer 211 on opposing sidewalls of the at least two first fins 203.

[0042] The thickness of the work function layer 209 on the opposing sidewalls of two adjacent first fins 203 is equal to the sum of the thicknesses of the first work function layer 211 and the second work function layer 212, which is greater than the thickness of the work function layer 209 on the sidewall of the first fin 203 facing the second fin 204, so that the threshold voltage of the opposing regions of the adjacent first fins 203 is greater than the threshold voltage of the region of the first fin 203 facing the second fin 204, and further, the number of diffusible electrons in the channel region between the adjacent first fins 203 is relatively small. Therefore, the signal interference between the two first fins 203 is small and the stability of the memory is high.

[0043] In this embodiment, the second work function layer 212 fills the opposing regions of the two first fins 203, i.e., the second work function layer 212 is an integral structure, not a separate two-layer work function layer covering different first fins 203. And there is no gap in the second work function layer 212. It should be noted that filling the opposing regions of the two first fins 203 further indicates that the thickness of the second work function layer 212 in a direction perpendicular to the surface of the substrate 202 meets a predetermined requirement. For example, the height difference between the top surface of the second work function layer 212 and the top surface of the first fin 203 is less than a predetermined height difference. In other embodiments, the second work function layer 212 may not fill the opposing regions of the two first fins 203.

[0044] In this embodiment, the material of the first work function layer 211 is the same as the material of the second work function layer 212. The same material can improve the bonding strength between the interfaces and further reduce the resistance. In other embodiments, the material of the first work function layer and the material of the second work function layer can be different.

[0045] In short, the thickness of the work function layer 209 between two adjacent first fins 203 is the total thickness of the first work function layer 211 and the second work function layer 212. The increase in thickness increases the threshold voltage of the region between the adjacent first fins 203. The number of diffusible electrons in the channel region between the adjacent first fins 203 is smaller, and the signal interference is smaller. A third embodiment of the present application provides a method for manufacturing a memory, which can be used to manufacture the memory according to the first embodiment. Figures 6 to 9 are structural schematic diagrams corresponding to each step in the method for manufacturing a memory according to the third embodiment of the present application.

[0046] Referring to FIG. 6 , a substrate 302 is provided, a first fin 303 and a second fin 304 are positioned and separated on the substrate 302, at least two first fins 303 are positioned between adjacent second fins 304, and the spacing between adjacent first fins 203 is smaller than the spacing between the second fins 304, the surface of the substrate 302 has a partition structure 305, and the partition structure 305 covers a portion of the sidewall of the first fins 303 and a portion of the sidewall of the second fins 304.

[0047] The width of the first partition structure 306 is smaller than the width of the second partition structure 307. Note that due to an etching loading effect, the larger the etching area, the larger the etching depth. Therefore, the depth of the first partition structure 306 is smaller than the depth of the second partition structure 307.

[0048] Referring to FIG. 7, a dielectric layer 308 is formed on the top and sidewall surfaces exposed by the partition structure 305 of the first fin 303, and the dielectric layer 308 covers the top and sidewall surfaces exposed by the partition structure 305 of the second fin 304.

[0049] In this embodiment, the dielectric layer 308 further covers the upper surfaces of the first partition structure 306 and the second partition structure 307. In other embodiments, the dielectric layer does not need to cover the upper surfaces of the first partition structure and the second partition structure.

[0050] Referring to Figure 8, a work function layer 309 is formed on a surface of a dielectric layer 308, and in a direction parallel to the arrangement direction of the first fin 303 and the second fin 304, the work function layer 309 on opposing sidewalls of at least two first fins 303 has a first thickness, and the work function layer 309 on the sidewall of the first fin 303 facing the second fin 304 has a second thickness, and the first thickness is greater than the second thickness.

[0051] Along the direction in which the substrate 302 faces the first fin 303, in the facing region of the adjacent first fin 303, the dielectric layer 308 and the first partition structure 306 surround the first filling region. In this embodiment, the dielectric layer 308 further covers the upper surface of the first partition structure 306, so that the dielectric layer 308 surrounds the first filling region. In this embodiment, the step of forming the work function layer 309 includes forming the work function layer 309 on the entire surface of the dielectric layer 308 and continuing until the first filling region is filled. By adjusting the coverage of the deposition thin film and making the deposition rate of the narrow groove region higher than that of the wide groove region, the formation of the work function layer 309 by a one-step process can be achieved, and the difficulty of manufacturing can be reduced.

[0052] It should be noted that the spacing between the two first fins 303 may be reduced to increase the filling rate of the work function layer 309 in the first heavy region.

[0053] It should be noted that the formation of the work function layer may be completed in multiple steps, for example, by first forming a work function layer solely on the opposing sidewalls of the adjacent first fin, or by first forming a work function layer on the sidewall of the first fin facing the second fin.

[0054] Referring to FIG. 9, a conductive layer 310 is formed on the surface of the work function layer 309 , and the work function value of the conductive layer 310 is smaller than that of the work function layer 309 .

[0055] In short, by adjusting the process steps of manufacturing the work function layer 309, the thickness of the work function layer 309 on the opposing sidewalls of adjacent first fins 303 can be made larger than the thickness of the work function layer 309 on the sidewall of the first fin 303 facing the second fin 304, the threshold voltage of the opposing regions of adjacent first fins 303 can be made larger than the threshold voltage of the region of the first fin 303 facing the second fin 304, and further, the number of diffusible electrons in the channel region between adjacent first fins 303 is relatively small, resulting in small signal interference and high memory stability.

[0056] The fourth embodiment of the present application provides a method for manufacturing a memory. The method is used to manufacture a memory according to the second embodiment. The difference from the third embodiment is that in this embodiment, a first work function layer and a second work function layer are formed in the opposing regions of two first fins. FIGS. 10 to 15 are structural schematic diagrams corresponding to each step in the method for manufacturing a memory according to the fourth embodiment of the present application. For parts that are the same as or corresponding to the third embodiment, reference may be made to the corresponding descriptions in the above embodiments, and descriptions will be omitted below.

[0057] Referring to FIG. 10, a first work function layer 411 is formed on the surface of the dielectric layer 408 .

[0058] This embodiment provides a substrate 402, a first fin 403 located on the substrate, a second fin 404, a partition structure 405, a first partition structure 406, and a second partition structure 407. For detailed descriptions of the above structures, please refer to the third embodiment. For the method of forming the dielectric layer 408 according to this embodiment, please also refer to the third embodiment. Here, the description is omitted.

[0059] Referring to FIG. 11, a sacrificial layer 413 is formed on the surface of the first work function layer 411 .

[0060] Referring to FIG. 12, the sacrificial layer 413 in opposing regions of adjacent first fins 403 is removed.

[0061] Referring to FIG. 13, a second work function layer 412 is formed on the surface of the first work function layer 411 in the facing regions of the adjacent first fins 403. In this embodiment, the second work function layer 412 fills the facing regions of the two first fins 403. That is, the second work function layer 412 is a monolithic structure, not a separate two-layer work function layer covering different first fins 403. And there is no gap in the second work function layer 412. Note that filling the facing regions of the two first fins 403 further indicates that the thickness of the second work function layer 412 in a direction perpendicular to the surface of the substrate 402 meets a predetermined requirement. For example, the height difference between the top surface of the second work function layer 412 and the top surface of the first fin 403 is less than a predetermined height difference. In other embodiments, the second work function layer 412 may not fill the facing regions of the two first fins 403.

[0062] Referring to FIG. 14, the sacrificial layer 413 (see FIG. 13) in the area of ​​the first fin 403 facing the second fin 404 is removed.

[0063] Referring to FIG. 15, a conductive layer 410 is formed on the surface of the work function layer 409 .

[0064] In short, by adjusting the process steps of fabricating the work function layer 409, the first work function layer 411 and the second work function layer 412 can be formed on the opposing sidewalls of adjacent first fins 403. The total thickness of the first work function layer 411 and the second work function layer 412 is greater than the thickness of the first work function layer 411 on the sidewall of the first fin 403 facing the second fin 404, so that the threshold voltage of the opposing regions of the adjacent first fins 403 is greater than the threshold voltage of the region of the first fin 403 facing the second fin 404, and further, the number of diffusible electrons in the channel region between the adjacent first fins 403 is relatively small, resulting in small signal interference and high memory stability.

[0065] As can be understood by those skilled in the art, the above embodiments are specific examples for realizing the present application, and various changes in form and details can be made in actual application without departing from the spirit and scope of the present application. Since those skilled in the art can make respective changes and modifications without departing from the spirit and scope of the present application, the protection scope of the present application shall be in accordance with the scope defined in the claims.

Claims

1. A memory, a substrate on which first fins and second fins are provided, at least two of the first fins being located between adjacent ones of the second fins, a distance between adjacent ones of the first fins being smaller than a distance between the first fin and the second fin; a surface of the substrate has a partition structure, the partition structure including a first partition structure and a second partition structure, the first partition structure being located between adjacent ones of the first fins and the second partition structure being located between the first fin and the second fin, a depth of the first partition structure being smaller than a depth of the second partition structure in a direction perpendicular to an extension direction of a word line; and a dielectric layer covering a top of the first fin and a sidewall surface exposed by the partition structure, and further covering a top of the second fin and a sidewall surface exposed by the partition structure; a work function layer including a first work function layer covering an entire surface of the dielectric layer and a second work function layer located on the first work function layer on opposing sidewalls of the at least two first fins and filling opposing regions of the at least two first fins, wherein in a direction parallel to an arrangement direction of the first fins and the second fins, a sum of thicknesses of the first work function layer and the second work function layer on the opposing sidewalls of the at least two first fins is a first thickness, and the first work function layer on a sidewall of the first fin facing the second fin has a second thickness, and the first thickness is greater than the second thickness; a conductive layer located on a surface of the work function layer.

2. In a direction in which the substrate faces the first fin, the dielectric layer and the first partition structure surround a first filling region within an opposing region of the adjacent first fins, and the work function layer fills the first filling region. The memory of claim 1 .

3. a gap between the work function layers on opposing sidewalls of the at least two first fins; The memory of claim 1 .

4. The material of the first work function layer is the same as the material of the second work function layer. The memory of claim 1 .

5. The first thickness is 5-50 nm and the second thickness is 2-30 nm. The memory of claim 1 .

6. The difference between the first thickness and the second thickness is between 3 nm and 30 nm. The memory of claim 1 .

7. The work function of the work function layer is greater than the work function of the conductive layer. The memory of claim 1 .

8. The material of the work function layer includes titanium nitride, cobalt, or nickel. The memory of claim 7.

9. A method for manufacturing a memory, comprising the steps of: providing a substrate, on which first fins and second fins are separated, at least two of the first fins being located between adjacent ones of the second fins, a distance between adjacent ones of the first fins being smaller than a distance between the first fins and the second fins, a surface of the substrate having a partition structure, the partition structure including a first partition structure and a second partition structure, the first partition structure being located between adjacent ones of the first fins, the second partition structure being located between the first fins and the second fins, and a depth of the first partition structure being smaller than a depth of the second partition structure in a direction perpendicular to an extension direction of a word line; forming a dielectric layer on a top of the first fin and a sidewall surface exposed by the partition structure, the dielectric layer covering a top of the second fin and a sidewall surface exposed by the partition structure; forming a work function layer on a surface of the dielectric layer, the work function layer including forming a first work function layer on an entire surface of the dielectric layer, and forming a second work function layer located on the first work function layer on opposing sidewalls of the at least two first fins and filling opposing regions of the at least two first fins, wherein in a direction parallel to an arrangement direction of the first fin and the second fin, a sum of thicknesses of the first work function layer and the second work function layer on opposing sidewalls of the at least two first fins is a first thickness, and the first work function layer on a sidewall of the first fin facing the second fin has a second thickness, and the first thickness is greater than the second thickness; forming a conductive layer on a surface of the work function layer, the work function value of the conductive layer being less than the work function value of the work function layer; A method for manufacturing a memory, wherein forming the second work function layer includes forming a sacrificial layer on a surface of the first work function layer, removing the sacrificial layer in opposing regions of adjacent first fins, forming the second work function layer on a surface of the first work function layer in opposing regions of adjacent first fins, and removing the sacrificial layer in a region of the first fin facing the second fin.

10. In a direction in which the substrate faces the first fin, the dielectric layer and the first partition structure surround a first filling region in an opposing region of the adjacent first fin, and forming the work function layer includes forming the work function layer on an entire surface of the dielectric layer and continuing until the first filling region is filled. A method for manufacturing the memory according to claim 9.

Citation Information

Patent Citations

  • Semiconductor device

    CN109427789A

  • Semiconductor structure and forming method thereof

    CN111200019A

  • Semiconductor device having buried channel array

    US20150263113A1

  • Semiconductor device including a gate insulation pattern and a gate electrode pattern

    US20190067278A1

  • Asymmetric finfet in memory device, method of fabricating same and semiconductor device

    WO2019091493A1