Submerged Arc Welding Flux

JP7578484B2Active Publication Date: 2024-11-06KOBE STEEL LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020213838
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-12-23
Publication Date
2024-11-06
Estimated Expiration
2040-12-23

AI Technical Summary

Technical Problem

Existing submerged arc welding methods for Cr-Mo steel face issues with wire breakage, increased manufacturing costs, unstable weld metal performance, and reduced toughness when using Al and N, especially during high-current welding, necessitating improved welding workability and mechanical performance.

Method used

A submerged arc welding flux composition containing specific amounts of Mn, Al, N, MgO, F, Ca, Al2O3, SiO2, CO2, C, Ni, and optional Na, K, Li, and Fe, optimized to enhance welding workability and mechanical performance, including components like AlN precipitation for strength and slag properties for stability.

Benefits of technology

The flux enables stable weld metal with excellent welding workability and mechanical performance, maintaining quality even under high-current conditions, ensuring high-temperature properties and low-temperature toughness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578484000001
    Figure 0007578484000001
  • Figure 0007578484000002
    Figure 0007578484000002
  • Figure 0007578484000003
    Figure 0007578484000003
Patent Text Reader

Abstract

To provide a submerged arc welding flux that excels in welding workability and is able to stably obtain a weld metal having excellent mechanical performance.SOLUTION: A submerged arc welding flux used in submerged arc welding of Cr-Mo steel sheet contains, based on the total mass of the flux: 0.01 mass% or more and 5.00 mass% or less of Mn; 0.50 mass% or more and 3.00 mass% or less of Al; more than 0 mass% and 0.50 mass% or less of N; 5.0 mass% or more and 40.0 mass% or less of MgO; 5.0 mass% or more and 12.0 mass% or less of F; 9.5 mass% or more and 21.5 mass% or less of Ca; 11.0 mass% or more and 23.0 mass% or less of Al2O3; 7.0 mass% or more and 20.0 mass% or less of a conversion value of SiO2 of Si and Si compound; 3.0 mass% or more and 10.0 mass% or less of CO2; as well as 1.00 mass% or less of C and 1.00 mass% or less of Ni.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Submerged arc welding method for cr-mo type low alloy steel

    JP1983058982A

  • Plating tank

    JP2000239816A

  • Bonded flux and wire for submerged arc welding

    JP2013039604A

  • Flux for one side submerged arc welding

    JP2013154363A

  • Baked flux for submerged arc welding for high-strength steel

    JP2020131221A