Granulator, kneading adjustment mechanism, and resin pellet manufacturing method

The kneading adjustment mechanism with movable members and protrusions on the screw enhances uniformity in resin pellet manufacturing by adjusting the gap between flow path surfaces, addressing the issue of inconsistent kneading in existing processes.

JP7578539B2Active Publication Date: 2024-11-06THE JAPAN STEEL WORKS LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021080412
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-05-11
Publication Date
2024-11-06
Estimated Expiration
2041-05-11

Smart Images

  • Figure 0007578539000001
    Figure 0007578539000001
  • Figure 0007578539000002
    Figure 0007578539000002
  • Figure 0007578539000003
    Figure 0007578539000003
Patent Text Reader

Abstract

To knead the molten resin more uniformly.SOLUTION: The kneading adjustment mechanism 80 has a pair of movable members 81, 82, each of which has a channel forming surface 85 forming part of a flow path 20 through which the kneaded molten resin is conveyed, and a screw 84 disposed between the channel forming surfaces 85 of the respective movable members 81, 82. At least one of the pair of movable members 81, 82 is operable to increase or decrease the gap between the flow path forming surface 85 and the screw 84, and at least one protrusion 86 is provided on the periphery of the screw 84.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an apparatus and method for producing resin pellets. [Background technology]

[0002] There are known devices and methods for producing resin pellets by cutting a molten resin while extruding it. For example, Patent Document 1 discloses an underwater cutting type granulator that cuts the molten resin extruded from a nozzle of a die head underwater. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-51617 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the production of resin pellets, it is desirable to knead the molten resin as uniformly as possible.

[0005] Other objects and novel features will become apparent from the description of this specification and the accompanying drawings. [Means for solving the problem]

[0006] According to one embodiment, the kneading adjustment mechanism includes a pair of movable members each having a flow path forming surface that forms a part of a flow path through which the kneaded molten resin is transported, and a screw disposed between the flow path forming surfaces of the movable members. At least one of the pair of movable members is operable to increase or decrease a gap between the flow path forming surface and the screw. In addition, at least one protrusion is provided on the outer periphery of the screw. Effect of the Invention

[0007] According to one embodiment, the molten resin is kneaded more uniformly. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a schematic diagram showing a configuration of a granulator according to one embodiment. [Diagram 2] FIG. 2 is a cross-sectional view showing the structure of a kneading processing section. [Diagram 3] FIG. 2 is a perspective view showing a structure of a kneading adjustment unit. [Figure 4A] 11 is a cross-sectional view showing a movable member rotated until the cross-sectional area of ​​the gate portion becomes a minimum. FIG. [Figure 4B] 11 is a cross-sectional view showing a movable member rotated until the cross-sectional area of ​​the gate portion becomes maximum. FIG. [Figure 5A] FIG. 4 is a perspective view showing a screw constituting the kneading adjusting mechanism. [Figure 5B] FIG. 5B is a cross-sectional view showing the screw shown in FIG. 5A and the movable members surrounding it. [Figure 6A] FIG. 13 is a perspective view showing a modified example of a screw constituting the kneading adjusting mechanism. [Figure 6B] FIG. 6B is a cross-sectional view showing the screw shown in FIG. 6A and the movable members around it. [Figure 7A] FIG. 13 is a perspective view showing another modified example of the screw constituting the kneading adjusting mechanism. [Figure 7B] FIG. 7B is a cross-sectional view showing the screw shown in FIG. 7A and the movable members around it. [Figure 8A] FIG. 13 is a perspective view showing another modified example of the screw constituting the kneading adjusting mechanism. [Figure 8B] FIG. 8B is a cross-sectional view showing the screw shown in FIG. 8A and the movable members surrounding it. [Figure 9A] FIG. 13 is a perspective view showing another modified example of the screw constituting the kneading adjusting mechanism. [Figure 9B] FIG. 9B is a cross-sectional view showing the screw shown in FIG. 9A and the movable members around it. [Figure 10] FIG. 13 is a diagram showing the results of a simulation. [Figure 11A] FIG. 11 is a perspective view showing a screw included in a granulator according to another embodiment. [Figure 11B] FIG. 11B is a cross-sectional view showing the screw shown in FIG. 11A and the movable members around it. [Figure 12A] FIG. 11 is a perspective view showing a screw included in a granulator according to another embodiment. [Figure 12B] FIG. 12B is a cross-sectional view showing the screw shown in FIG. 12A and the movable members around it. [Figure 13A] FIG. 11 is a perspective view showing a screw included in a granulator according to another embodiment. [Figure 13B] FIG. 13B is a cross-sectional view showing the screw shown in FIG. 13A and the movable members around it. [Figure 14A] FIG. 11 is a perspective view showing a screw included in a granulator according to another embodiment. [Figure 14B] FIG. 14B is a cross-sectional view showing the screw shown in FIG. 14A and the movable members around it. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment will be described in detail with reference to the drawings. In all drawings for explaining the embodiment, the same reference numerals are used to designate members and devices having the same or substantially the same functions, and repeated description will be omitted.

[0010] <Overall composition> Fig. 1 is a schematic diagram showing the configuration of a granulator according to one embodiment. Fig. 2 is a cross-sectional view showing the structure of a kneading section provided in the granulator shown in Fig. 1. The granulator 1A shown in Fig. 1 has a main motor 10, a reducer 11, a kneading section 12, a gear pump 13, a foreign matter removal section (screen changer) 14, a die head 15, and a cutting section (pelletizer, cutter unit) 16.

[0011] <Main motor, reducer> The main motor 10 is a drive source for the kneading processing section 12. The rotational driving force output from the main motor 10 is input to a screw 70 of the kneading processing section 12 via a reducer 11, and rotates the screw 70. The reducer 11 reduces the speed of the rotational driving force output from the main motor 10 and increases the torque of the rotational driving force input to the screw 70.

[0012] <Mixing and kneading section> The kneading processing section 12 melts and transports the resin raw material by the rotating screw 70. The kneading processing section 12 also kneads and transports the molten resin raw material (molten resin) by the rotating screw 70.

[0013] 2, the kneading processing section 12 has a cylinder (barrel) 21 that forms a flow path (transport path) 20 through which the resin raw material and the molten resin are transported. A raw material hopper 22 is provided on one longitudinal end side of the cylinder 21. The raw material hopper 22 has an upper opening 22a and a lower opening 22b that is smaller than the upper opening 22a and communicates with the cylinder 21.

[0014] The resin raw material is fed into the raw material hopper 22 from the upper opening 22a. The resin raw material fed into the raw material hopper 22 falls into the cylinder 21 from the lower opening 22b. From another perspective, the resin raw material is supplied to the flow path 20 via the raw material hopper 22. In the following description, the upper opening 22a of the raw material hopper 22 may be referred to as the "feed port 22a," and the lower opening 22b of the raw material hopper 22 may be referred to as the "discharge port 22b."

[0015] The resin raw material supplied to the flow path 20 is transported from one end side to the other end side of the cylinder 21 where the raw material hopper 22 is provided. In other words, one end side (left side in FIG. 2) of the cylinder 21 where the raw material hopper 22 is provided is the upstream side of the flow path 20, and the other end side of the cylinder 21 (right side in FIG. 2) is the downstream side of the flow path 20.

[0016] The kneading processing section 12 includes at least a conveying section 30, a kneading section 40, a kneading adjustment section 50, a discharging section 60, and a screw 70, in addition to the cylinder 21 and the raw material hopper 22. The screw 70 is provided inside the cylinder 21 and supported so as to be freely rotatable. From another perspective, the screw 70 is provided so as to be freely rotatable within the flow path 20. As described above, the screw 70 is rotationally driven by the main motor 10.

[0017] Behind the screw 70 shown in FIG. 2, a similar screw 70 is provided (see FIG. 1). These two screws 70 are arranged in parallel to each other and are similarly rotated and driven by the main motor 10. In other words, the granulator 1A is equipped with two screws 70 parallel to each other and is generally called a "twin-screw granulator" or a "twin-screw extruder." In the following description, the two screws 70 equipped in the granulator 1A are collectively referred to as "screws 70." In addition, the description of the screw 70 shown in FIG. 2 also includes the description of the other screw 70 not shown in FIG. 2.

[0018] The conveying section 30, the kneading section 40, the kneading adjustment section 50, and the discharging section 60 are provided on the flow path 20. Furthermore, the conveying section 30, the kneading section 40, the kneading adjustment section 50, and the discharging section 60 are arranged in a line in this order along the flow path 20. In other words, the conveying section 30, the kneading section 40, the kneading adjustment section 50, and the discharging section 60 are arranged in a line in this order along the central axis X of the screw 70.

[0019] <Gear pump, foreign matter removal section> Referring again to Fig. 1, the gear pump 13 supplies (pumps) the molten resin kneaded by the kneading processing section 12 to the die head 15 through a foreign matter removal section (screen changer) 14. The gear pump 13 is driven by a motor 13a. The rotational driving force output from the motor 13a is input to the gear pump 13 via a reducer 13b. The foreign matter removal section 14 removes unnecessary components, residue, contaminants, etc. from the molten resin passing therethrough.

[0020] <Die head> The die head 15 is composed of a die holder, a die plate, a die plate cover, etc., and has a plurality of nozzles from which the molten resin is extruded. The molten resin that has passed through the foreign matter removal section 14 and is supplied to the die head 15 is extruded from the nozzles of the die head 15 and formed into a strand shape (string shape, rope shape).

[0021] <Cut section> The cutting unit 16 includes a cutting processing section that receives the strand-shaped molten resin extruded from the nozzle of the die head 15. The cutting processing section is provided on a flow path of water (pellet transport water) circulating in a resin pellet production system including the granulator 1A. During operation of the production system, the cutting processing section is filled with the pellet transport water. That is, the molten resin formed into a strand shape by the die head 15 is extruded into the water (pellet transport water).

[0022] A rotatable cutter head is provided in the cutting processing section of the cutting unit 16. A plurality of cutter blades are attached to the cutter head. The cutter head is driven by a motor 16a and cuts the strand-shaped molten resin extruded from the die head 15 to a predetermined length.

[0023] <Resin pellet manufacturing method> In the granulator 1A, resin pellets are produced, for example, by the following process. First, a resin raw material is supplied to the kneading processing section 12. More specifically, the resin raw material is charged into the raw material hopper 22. The resin raw material supplied to the kneading processing section 12 is, for example, a thermoplastic resin. More specifically, for example, a polyolefin resin having a bimodal structure is supplied to the kneading processing section 12. Additives and the like are added to the resin raw material as necessary.

[0024] The resin raw material supplied to the kneading processing section 12 is transported from the upstream side to the downstream side of the flow path 20 by the rotating screw 70. The resin raw material (molten resin) transported within the flow path 20 is melted and kneaded during the transport. More specifically, the resin raw material (molten resin) is melted and kneaded while passing through the transport section 30, the kneading section 40, the kneading adjustment section 50, and the discharging section 60 in this order. Each step will be described in more detail below.

[0025] The resin raw material fed into the inlet 22a of the raw material hopper 22 shown in Fig. 2 is supplied to the conveying section 30. The resin raw material fed to the conveying section 30 is conveyed to the downstream side of the flow path 20 while being melted (melting process). Next, the resin raw material melted in the melting process (molten resin) is conveyed to the kneading section 40. The molten resin supplied to the kneading section 40 is conveyed further downstream of the flow path 20 while being kneaded (mixed) (kneading process).

[0026] In the melting process, the resin raw material is melted by heat generated mainly by the shearing action caused by the rotation of the screw 70. In the kneading process, the molten resin is kneaded (dispersively mixed and distributively mixed) mainly by the shearing action and elongation action caused by the rotation of the screw 70. The molten resin continues to generate heat during the kneading process. At least, the temperature of the molten resin during the kneading process is maintained within a predetermined temperature range by the heat generated. However, if necessary, the resin raw material and the molten resin may be heated by a heating means such as a heater, and the resin raw material and the molten resin may be cooled by a cooling means.

[0027] The molten resin kneaded in the kneading process is supplied (discharged) to the gear pump 13 shown in Fig. 1 through the kneading adjustment section 50 and the discharge section 60. In the kneading adjustment section 50, a process (kneading adjustment process) of adjusting the degree of kneading of the molten resin in the kneading process (degree of kneading) is performed. The kneading adjustment section 50 will be described later.

[0028] The molten resin supplied to the gear pump 13 is supplied (pressurized) to the die head 15 through the foreign matter removal section 14. In the foreign matter removal section 14, volatile components contained in the molten resin, catalyst residues, foreign matter mixed in from the outside, etc. are removed (foreign matter removal process).

[0029] The molten resin pressure-fed to the die head 15 is continuously extruded from a plurality of nozzles provided in the die head 15 (extrusion process). The molten resin passes through the nozzles of the die head 15 and is formed into a strand shape (string shape, rope shape).

[0030] The strand-like molten resin extruded from the nozzle of the die head 15 is cut to a predetermined length in the cutting processing section of the cutting unit 16 and solidified (cutting / solidifying process, pelletizing process). In other words, the molten resin extruded in the form of a strand is cut into pellets. As a result, resin pellets of a predetermined size (length and thickness) are produced.

[0031] As described above, the cutting processing section of the cutting unit 16 is filled with water (pellet transport water), and the molten resin is cut underwater (pellet transport water). This method of cutting the molten resin underwater is sometimes called "underwater cutting."

[0032] Depending on the characteristics of the resin raw material (especially the melting point), resin pellets may be produced without circulating pellet transport water. In this case, the molten resin extruded from the nozzle of the die head 15 is cut in a cutting processing section where there is no pellet transport water. In other words, the molten resin is extruded into the air and cut. This method of cutting the molten resin in the air is sometimes called "hot cut."

[0033] Returning to the description of the resin pellet manufacturing method of this embodiment in which underwater cutting is performed, the mixture (slurry) of resin pellets and pellet transport water sent out from the cutting processing section is separated into resin pellets and pellet transport water (dehydration process). Next, the resin pellets separated from the pellet transport water are sent to a storage container such as a pellet silo (transfer process). The resin pellets are sent to the pellet silo by, for example, an airflow generated by a blower.

[0034] In the resin pellet manufacturing method of this embodiment, resin pellets are manufactured through the above-mentioned steps. However, the resin pellet manufacturing method can be modified in various ways depending on the type and characteristics of the resin raw material and the resin pellets. For example, in another embodiment, a drying step is performed after the dehydration step. In the drying step, a centrifugal dehydrator or the like is used to remove moisture that was not completely removed in the dehydration step from the resin pellets. In still another embodiment, a sorting step is performed after the dehydration step and drying step to separate the resin pellets based on size.

[0035] <Mixing and kneading section> Next, the kneading processing section 12 of the granulator 1A will be described in more detail. As shown in Fig. 2, the kneading processing section 12 has a conveying section 30, a kneading section 40, a kneading adjustment section 50, and a discharge section 60 provided along the longitudinal direction of a cylinder 21 (flow path 20) and a screw 70. From another perspective, the cylinder 21 (flow path 20) and the screw 70 can be divided into the conveying section 30, the kneading section 40, the kneading adjustment section 50, and the discharge section 60 based on their functions.

[0036] As described above, the conveying section 30 is composed of the cylinder 21 and a part of the screw 70. In addition, the kneading section 40 is composed of the cylinder 21 and another part of the screw 70, the kneading adjustment section 50 is composed of another part of the screw 70, and the discharging section 60 is composed of the cylinder 21 and another part of the screw 70.

[0037] In the following description, a part of the cylinder 21 constituting the conveying section 30 may be referred to as the "upstream section," another part of the cylinder 21 constituting the kneading section 40 as the "midstream section," and another part of the cylinder 21 constituting the discharging section 60 as the "downstream section." However, such a distinction is made merely for the convenience of description.

[0038] In the following description, a part of the screw 70 constituting the conveying section 30 may be referred to as the "conveying screw section 70a," another part of the screw 70 constituting the kneading section 40 as the "front-stage kneading screw section 70b," another part of the screw 70 constituting the kneading adjustment section 50 as the "rear-stage kneading screw section 70c," and another part of the screw 70 constituting the discharging section 60 as the "discharging screw section 70d." These distinctions are merely made for the sake of convenience.

[0039] <Screw> The screw 70 has flights and protrusions provided on a shaft 71 extending from one end to the other end of the cylinder 21. More specifically, flights are provided on the outer periphery of the conveying screw section 70a, the front-stage kneading screw section 70b, and the discharging screw section 70d of the screw 70. In addition, protrusions are provided on the outer periphery of the rear-stage kneading screw section 70c of the screw 70.

[0040] The flights and protrusions provided on the screw 70 are formed by kneading disks, rotors, segments, etc. attached to the shaft 71, or are integrally molded with the shaft 71. The form (structure, shape, size, pitch, etc.) of the flights provided on the screw 70 is appropriately determined depending on the purpose of each flight, the type of resin, etc.

[0041] The flights provided on a part of the screw 70 in this embodiment (the conveying screw section 70a and the discharging screw section 70d) are intended mainly to convey the resin raw material and the molten resin, while the flights provided on the other part of the screw 70 in this embodiment (the front-stage kneading screw section 70b) are intended mainly to knead the molten resin.

[0042] In this embodiment, the flights provided on the conveying screw section 70a and the discharging screw section 70d are formed by helical blades integrally molded on the shaft 71. On the other hand, the flights provided on the front-stage kneading screw section 70b of the screw 70 are formed by a plurality of kneading disks or rotors attached to the shaft 71. The protrusions provided on the rear-stage kneading screw section 70c of the screw 70 will be described later.

[0043] <Mixing and adjusting section> 3 is a perspective view showing the structure of the kneading adjustment section 50. The kneading adjustment section 50 is provided on the flow path 20, downstream of the kneading section 40. The kneading adjustment section 50 forms a part of the flow path 20, and includes a kneading adjustment mechanism 80 that adjusts the degree of kneading of the molten resin.

[0044] The kneading adjustment mechanism 80 adjusts the degree of kneading of the molten resin by changing the cross-sectional area of ​​a portion of the flow path 20 formed by the kneading adjustment section 50. Furthermore, the kneading adjustment mechanism 80 itself kneads the molten resin.

[0045] The kneading adjustment mechanism 80 is composed of a pair of movable members 81, 82, a holding block 83, and a screw 84. However, the screw 84 constituting the kneading adjustment mechanism 80 is a part of the screw 70. More specifically, the screw 84 constituting the kneading adjustment mechanism 80 is the rear-stage kneading screw section 70c of the screw 70.

[0046] The movable members 81, 82 are metal rods that are rotatably held. Each of the movable members 81, 82 is disposed between the midstream and downstream portions of the cylinder 21, and is rotatably held by a holding block 83 that forms a part of the flow path 20. The holding block 83 is provided with an upper holding portion 83a that crosses above the flow path 20, and a lower holding portion 83b that crosses below the flow path 20. The upper holding portion 83a and the lower holding portion 83b cross the flow path 20 vertically, and extend parallel to each other.

[0047] The movable member 81 is inserted into the upper holding portion 83a, and the movable member 82 is inserted into the lower holding portion 83b. As a result, the movable member 81 vertically traverses above the flow path 20, and the movable member 82 vertically traverses below the flow path 20. In addition, a part of the outer circumferential surface of the movable member 81 is exposed to the flow path 20, and a part of the outer circumferential surface of the movable member 82 is also exposed to the flow path 20. From another perspective, the movable members 81 and 82, together with the holding block 83, form a part of the flow path 20.

[0048] On both longitudinal sides of each of the movable members 81, 82, gears that mesh with each other are formed around the entire circumference. Therefore, when at least one of the movable members rotates, both movable members rotate simultaneously in the opposite directions. For example, when the upper movable member 81 rotates clockwise, the lower movable member 82 rotates simultaneously counterclockwise. That is, the two movable members 81, 82 rotate in opposite directions in conjunction with each other. Then, the cross-sectional area of ​​a portion of the flow path 20 changes (increases or decreases) according to the rotation angle (amount of rotation) of the movable members 81, 82.

[0049] As described above, the kneading adjustment mechanism 80 is provided downstream of the kneading section 40. More specifically, the kneading adjustment mechanism 80 is provided between the midstream section and the downstream section of the cylinder 21. In other words, the kneading adjustment mechanism 80 is provided between the kneading section 40 and the discharge section 60. As a result, the cross-sectional area of ​​a portion (region) of the flow path 20 connecting the kneading section 40 and the discharge section 60 is changed by the kneading adjustment mechanism 80. In the following description, the portion (region) of the flow path 20 whose cross-sectional area is changed by the kneading adjustment mechanism 80 may be referred to as the "gate section G".

[0050] The gate portion G is located downstream of the kneading portion 40. Therefore, when the cross-sectional area of ​​the gate portion G is changed by the kneading adjustment mechanism 80, the pressure (back pressure) of the molten resin at the gate portion G changes. Specifically, when the cross-sectional area of ​​the gate portion G is reduced by the kneading adjustment mechanism 80, the pressure of the molten resin at the gate portion G increases. On the other hand, when the cross-sectional area of ​​the gate portion G is enlarged by the kneading adjustment mechanism 80, the pressure of the molten resin at the gate portion G decreases. Then, when the pressure of the molten resin at the gate portion G increases, the time during which the molten resin is kneaded at the kneading portion 40 becomes longer, and the degree of kneading becomes stronger (higher). On the other hand, when the pressure of the molten resin at the gate portion G decreases, the time during which the molten resin is kneaded at the kneading portion 40 becomes shorter, and the degree of kneading becomes weaker (lower). In other words, the kneading adjustment mechanism 80 controls the pressure of the molten resin at the gate portion G by partially changing the cross-sectional area of ​​the flow path 20, and adjusts the degree of kneading of the molten resin.

[0051] Fig. 4A is a cross-sectional view showing movable members 81 and 82 rotated until the cross-sectional area of ​​gate portion G becomes minimum. Fig. 4B is a cross-sectional view showing movable members 81 and 82 rotated until the cross-sectional area of ​​gate portion G becomes maximum.

[0052] The movable members 81 and 82 are provided with a flow path forming surface 85 that forms a part (gate portion G) of the flow path 20. The flow path forming surfaces 85 of the movable members 81 and 82 each have a curved shape following the outer shape of the screw 84 (rear-stage kneading screw portion 70c) and are disposed on both sides (upper and lower) in the radial direction of the screw 84. From another perspective, the screw 84 is disposed between the flow path forming surface 85 of the movable member 81 and the flow path forming surface 85 of the movable member 82.

[0053] The flow passage forming surface 85 of the movable member 81 forming the upper side of the gate portion G faces approximately the upper half of the screw 84, and the flow passage forming surface 85 of the movable member 82 forming the lower side of the gate portion G faces approximately the lower half of the screw 84. In other words, the flow passage forming surface 85 of the movable member 81 faces the upper side of the outer circumferential surface of the rear-stage kneading screw section 70c, and the flow passage forming surface 85 of the movable member 82 faces the lower side of the outer circumferential surface of the rear-stage kneading screw section 70c. However, the area on the screw 84 facing the flow passage forming surface 85 changes with the rotation of the screw 84. Also, depending on the rotation angle (amount of rotation) of the movable members 81 and 82, the flow passage forming surface 85 and the screw 84 may face each other parallel to each other or obliquely to each other.

[0054] 4B rotates counterclockwise, the flow path forming surface 85 of the movable member 81 approaches the screw 84. At the same time, the movable member 82 rotates clockwise, and the flow path forming surface 85 of the movable member 82 also approaches the screw 84. As a result, the gap (clearance) between the flow path forming surfaces 85 of the movable members 81 and 82 and the screw 84 decreases. In other words, the cross-sectional area of ​​the gate portion G decreases.

[0055] 4A rotates clockwise, the flow path forming surface 85 of the movable member 81 moves away from the screw 84. At the same time, the movable member 82 rotates counterclockwise, and the flow path forming surface 85 of the movable member 82 also moves away from the screw 84. As a result, the gap (clearance) between the flow path forming surfaces 85 of the movable members 81 and 82 and the screw 84 increases. In other words, the cross-sectional area of ​​the gate portion G increases.

[0056] As described above, the pair of movable members 81, 82 can operate to increase and decrease the gap (clearance) between the flow passage forming surface 85 and the screw 84. As the gap (clearance) between the flow passage forming surface 85 and the screw 84 increases and decreases, the cross-sectional area of ​​the gate portion G increases and decreases.

[0057] When the movable members 81 and 82 shown in FIG. 4B are rotated 50 degrees, they reach the state shown in FIG. 4A (fully closed state). The cross-sectional area of ​​the gate portion G is minimum when the movable members 81 and 82 are in the fully closed state. On the other hand, when the movable members 81 and 82 shown in FIG. 4A are rotated 50 degrees, they reach the state shown in FIG. 4B (fully open state). The cross-sectional area of ​​the gate portion G is maximum when the movable members 81 and 82 are in the fully open state. Furthermore, the cross-sectional area of ​​the gate portion G gradually decreases as the movable members 81 and 82 move from the fully open state to the fully closed state, and gradually increases as the movable members 81 and 82 move from the fully closed state to the fully open state.

[0058] It should be noted that the cross-sectional area of ​​the gate portion G can be increased or decreased by increasing or decreasing the gap (clearance) between at least one of the flow path forming surfaces 85 of the movable members 81, 82 and the screw 84. Also, the gap (clearance) between each of the flow path forming surfaces 85 and the screw 84 can be increased or decreased by raising or lowering the movable members 81, 82.

[0059] <Screw (rear mixing screw section)> Next, there will be described the shape of the screw 84 constituting the kneading adjustment mechanism 80. As already described, the screw 84 is a part of the screw 70 (the rear-stage kneading screw portion 70c).

[0060] The screw 84 has a shape capable of kneading the molten resin passing through the kneading adjustment section 50. More specifically, the screw 84 has a shape capable of dispersing and mixing the molten resin passing through the kneading adjustment section 50.

[0061] FIG. 5A is a perspective view of the screw 84. FIG. 5B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around the screw 84 shown in FIG. 5A. The cross section of the screw 84 shown in FIG. 5B is a cross section perpendicular to the central axis X. From the above description, it can be seen that the central axis X is the central axis of the screw 70 and also the central axis of the screw 84. In the following description, unless otherwise specified, the cross section of the screw 70 (screw 84) ​​means a cross section perpendicular to the central axis X. Note that the movable members 81 and 82 shown in FIG. 5B actually have a shape as shown in FIG. 3, and are shown in FIG. 5B as a schematic diagram.

[0062] At least one protrusion 86 is provided on the outer periphery of the screw 84. In this embodiment, six protrusions 86, each having a corner, are provided on the outer periphery of the screw 84. From another perspective, edges are provided at six points in the circumferential direction of the screw 84.

[0063] The six protrusions 86 provided on the screw 84 are disposed at equal intervals (60 degree intervals) in the circumferential direction (rotation direction) of the screw 84. Furthermore, each protrusion 86 extends parallel to the central axis X of the screw 84. As a result, the line segments connecting the vertices (tips) 86a of each protrusion 86 in the cross section of the screw 84 form a regular polygon (a regular hexagon). In other words, the screw 84 has a cross-sectional shape that is a regular hexagon.

[0064] The screw 84, which has protrusions 86 on its outer periphery, generates an elongational flow in the molten resin passing through the kneading adjustment section 50 (gate section G). Specifically, when the screw 84 rotates, the flow path forming surface 85 moves relatively closer to and away from the tip of the protrusions 86 of the screw 84. As a result, the flow path cross-sectional area changes continuously, and elongational deformation occurs in the molten resin.

[0065] From another perspective, by providing the protrusions 86 on the outer periphery of the screw 84, an elongation speed can be obtained in the kneading adjustment section 50. In other words, the molten resin kneaded (mixed) while passing through the kneading section 40 is also kneaded (mixed) while passing through the kneading adjustment section 50.

[0066] Here, if the cross-sectional area of ​​the flow passage is too small, the kneading may be excessive, whereas if the cross-sectional area of ​​the flow passage is too large, the kneading may be insufficient. In other words, if the clearance between the screw 84 and the flow passage forming surface 85 is too small, the kneading may be excessive. On the other hand, if the clearance between the screw 84 and the flow passage forming surface 85 is too large, the kneading may be insufficient.

[0067] Therefore, it is preferable that the ratio (b / a) of the minimum clearance a to the maximum clearance b shown in Fig. 5B is equal to or less than 4. In addition, it is preferable that the minimum clearance a when the movable members 81, 82 are in a fully closed state is equal to or less than 1 / 10 of the inner diameter d of the gate portion G.

[0068] 5B is the clearance between the protrusion 86 of the screw 84 and the flow passage forming surface 85. More specifically, it is the clearance between the tip of the protrusion 86 and the flow passage forming surface 85. Moreover, the maximum clearance b shown in FIG. 5B is the clearance between the flat portion between two adjacent protrusions 86 and the flow passage forming surface 85.

[0069] In this embodiment, six protrusions 86 are provided on the outer periphery of the screw 84. However, as long as at least one protrusion 86 is provided on the outer periphery of the screw 84, an elongational flow can be generated in the molten resin. Therefore, there is no limitation on the number, shape, arrangement, etc. of the protrusions 86 provided on the outer periphery of the screw 84. Therefore, some modified examples of the screw 84 will be described below.

[0070] <Variation 1> Fig. 6A is a perspective view showing a modified example of the screw 84. Fig. 6B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around it shown in Fig. 6A.

[0071] The screw 84 shown in Figures 6A and 6B has eight protrusions 86, each having a corner, on its outer periphery. These eight protrusions 86 are arranged at equal intervals (45 degree intervals) in the circumferential direction (rotation direction) of the screw 84. As a result, the line segments connecting the vertices 86a of the protrusions 86 in the cross section of the screw 84 form a regular polygon (regular octagon). In other words, the screw 84 shown in Figures 6A and 6B has a cross-sectional shape that is a regular octagon.

[0072] <Variation 2> Fig. 7A is a perspective view showing another modified example of the screw 84. Fig. 7B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around it shown in Fig. 7A.

[0073] Ten protrusions 86, each having a corner, are provided on the outer periphery of the screw 84 shown in Figures 7A and 7B. These ten protrusions 86 are arranged at equal intervals (36 degree intervals) in the circumferential direction (rotation direction) of the screw 84. As a result, the line segments connecting the vertices 86a of each protrusion 86 in the cross section of the screw 84 form a regular polygon (regular decagon). In other words, the screw 84 shown in Figures 7A and 7B has a cross-sectional shape that is a regular decagon.

[0074] <Variation 3> Fig. 8A is a perspective view showing another modified example of the screw 84. Fig. 8B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around it shown in Fig. 8A.

[0075] The screw 84 shown in Figures 8A and 8B has 12 projections 86, each having a corner, on its outer periphery. These 12 projections 86 are arranged at equal intervals (30 degree intervals) in the circumferential direction (rotation direction) of the screw 84. As a result, the line segments connecting the vertices 86a of the projections 86 in the cross section of the screw 84 form a regular polygon (regular dodecagon). In other words, the screw 84 shown in Figures 8A and 8B has a cross-sectional shape that is a regular dodecagon.

[0076] <Variation 4> Fig. 9A is a perspective view showing another modified example of the screw 84. Fig. 9B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around it shown in Fig. 9A.

[0077] 24 protrusions 86, each having a corner, are provided on the outer periphery of the screw 84 shown in Figures 9A and 9B. These 24 protrusions 86 are arranged at equal intervals (15 degree intervals) in the circumferential direction (rotation direction) of the screw 84. As a result, the line segments connecting the vertices 86a of each protrusion 86 in the cross section of the screw 84 form a regular polygon (regular 24-sided polygon). In other words, the screw 84 shown in Figures 9A and 9B has a cross-sectional shape that is a regular 24-sided polygon.

[0078] <Simulation> Next, a simulation (flow analysis) performed to confirm the effect of this embodiment will be described. In this simulation, the elongation speed of molten resin with the same characteristics was calculated when a cylindrical screw with no protrusions on the outer periphery and a screw with protrusions on the outer periphery were rotated under the same conditions. From another perspective, the elongation speed of molten resin with the same characteristics was calculated when a screw with a circular cross-sectional shape and a screw with a regular polygonal cross-sectional shape were rotated under the same conditions.

[0079] It was assumed that each screw was rotated at the same speed in a cylinder under the same conditions. It was also assumed that each screw had the same or substantially the same outer diameter. For screws with a regular polygonal cross section, the diameter of a circle connecting the vertices of each protrusion was taken as the outer diameter of the screw.

[0080] The comparison results of the elongation speed calculated by this simulation are shown in Figure 10. The table in Figure 10 shows the ratio of the elongation speed obtained by each screw with a regular polygonal cross-sectional shape to the elongation speed obtained by a screw with a circular cross-sectional shape.

[0081] This simulation confirmed that in the granulator 1A of this embodiment, which has a screw 84 with a regular hexagonal cross-sectional shape, the molten resin is kneaded (mixed) not only in the kneading section 40 but also in the kneading adjustment section 50. From another perspective, the kneading adjustment section 50 (kneading adjustment mechanism 80) provided in the granulator 1A of this embodiment has a kneading function and a kneading degree adjustment function. Therefore, according to the granulator 1A of this embodiment, it is possible to knead the resin more uniformly. The granulator 1A of this embodiment, which has such an effect, is particularly suitable for kneading resins with different viscosities and dispersing fillers with strong cohesive force.

[0082] The invention made by the present inventor has been specifically described above based on the embodiment and examples, but the present invention is not limited to the above embodiment or examples, and it goes without saying that various modifications can be made without departing from the gist of the invention. For example, the screw 84 only needs to have at least one protrusion 86, and the cross-sectional shape is not limited to a regular polygon. Therefore, the screw 84 in the above embodiment can be replaced with the screw 84 shown in Figures 11 to 14, for example.

[0083] Fig. 11A is a perspective view of a screw 84 included in a granulator according to another embodiment. Fig. 11B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around the screw 84 shown in Fig. 11A.

[0084] 11A and 11B, eight protrusions 86 having a triangular cross-sectional shape are provided on the outer periphery of the screw 84. From another perspective, the screw 84 has a generally star-shaped cross-sectional shape. From yet another perspective, the outer periphery of the screw 84 has a plurality of peaks and valleys. Moreover, the peaks and valleys are arranged alternately in the circumferential direction.

[0085] Fig. 12A is a perspective view of a screw 84 included in a granulator according to still another embodiment. Fig. 12B is a cross-sectional view of the screw 84 and the movable members 81 and 82 around the screw 84 shown in Fig. 12A.

[0086] 12A and 12B, 24 protrusions 86 having a triangular (wedge-shaped) cross-sectional shape are provided on the outer periphery of the screw 84. The protrusions 86 on the screw 84 shown in Fig. 12A and 12B are sharper than the protrusions 86 on the screw 84 shown in Fig. 11A and 11B, and are arranged at a narrower pitch. From another perspective, the screw 84 has a plurality of thorns on its outer periphery.

[0087] Fig. 13A is a perspective view of a screw 84 included in a granulator according to still another embodiment, and Fig. 13B is a cross-sectional view of the screw 84 shown in Fig. 13A.

[0088] Four protrusions 86 are provided on the outer periphery of the screw 84 shown in Figures 13A and 13B. Furthermore, the outer periphery of the screw 84 connecting adjacent protrusions 86 is undulating (wavy). From another perspective, adjacent protrusions 86 are connected by curved surfaces. Note that in the screw 84 shown in Figures 13A and 13B as well, the line segments connecting the vertices 86a of the protrusions 86 in a cross section perpendicular to the central axis X form a regular polygon (regular quadrilateral).

[0089] Fig. 14A is a perspective view of a screw 84 included in a granulator according to still another embodiment. Fig. 14B is a cross-sectional view of the screw 84 shown in Fig. 14A.

[0090] Six protrusions 86 are provided on the outer periphery of the screw 84 shown in Figs. 14A and 14B. This screw 84 has a regular hexagonal cross-sectional shape, like the screw 84 shown in Figs. 5A and 5B. However, while the protrusions 86 provided on the screw 84 shown in Figs. 5A and 5B extend parallel to the central axis X, the protrusions 86 provided on the screw 84 shown in Figs. 14A and 14B extend in a direction intersecting the central axis X. From another perspective, the protrusions 86 provided on the screw 84 shown in Figs. 14A and 14B extend in a spiral shape with the central axis X as the rotation axis. Note that all of the protrusions 86 provided on the screw 84 shown in Figs. 6 to 13 extend parallel to the central axis X.

[0091] In this specification, several examples of the shape of the screw 84 constituting the kneading adjustment mechanism 80 are shown. However, the shape of the screw 84 shown in this specification is merely one example. The shape, size, number, pitch, etc. of the protrusions 86 provided on the screw 84 constituting the kneading adjustment mechanism 80 can be appropriately changed according to the stress to be applied to the molten resin passing through the kneading adjustment section 50. For example, the protrusions 86 do not have to be sharp. The tip of the protrusions 86 may be, for example, an arc surface. When the tip of the protrusions 86 is an arc surface, the midpoint of the arc corresponds to the vertex 86a of the protrusions 86.

[0092] Granulators include at least twin screw granulators and single screw granulators, and twin screw granulators include at least continuous co-rotating intermeshing twin screw granulators and continuous counter-rotating non-intermeshing twin screw granulators. [Explanation of symbols]

[0093] 1A: Granulator 10: Main motor 11: Reducer 12: Mixing processing section 13: Gear pump 13a, 16a: Motor 13b: Reducer 14: Foreign matter removal section 15: Die head 16: Cutting section 20: Flow path 21: Cylinder 22: Raw material hopper 22a: Upper opening (inlet) 22b: Lower opening (exhaust port) 30: Transport section 40: Mixing section 50: Mixing and adjusting section 60: Emission part 70,84:Screw 70a: Conveying screw section 70b: Pre-mixing screw section 70c: Rear mixing screw section 70d: Discharge screw section 71: Shaft 80: Kneading adjustment mechanism 81, 82: Movable parts 83: Holding block 83a: Upper holding part 83b: Lower holding part 85: Flow path forming surface 86:Protrusion 86a: Vertex a: minimum clearance b: Maximum clearance d: inner diameter G: Gate section X: Central axis

Claims

1. a flow path through which the molten resin is transported; a kneading section that is provided on the flow path and kneads and transports the molten resin; A kneading adjustment unit is provided on the flow path and downstream of the kneading unit, the kneading adjustment unit includes a kneading adjustment mechanism including a pair of movable members each having a flow path forming surface that forms a part of the flow path, and a screw disposed between the flow path forming surfaces of the movable members; At least one of the pair of movable members is operable to increase or decrease a gap between the flow passage forming surface and the screw, A plurality of protrusions are provided on the outer periphery of the screw along the circumferential direction of the screw, Each of the protrusions is sharp and extends parallel to a central axis of the screw; A granulator, wherein vertices of all of the protrusions are present within a cross section of the screw perpendicular to the central axis, and line segments connecting each of the vertices within the cross section form a regular polygon.

2. A kneading adjustment mechanism provided on a flow path through which a kneaded molten resin is transported, A pair of movable members each having a flow path forming surface that forms a part of the flow path; a screw disposed between the flow passage forming surfaces of the movable members; At least one of the pair of movable members is operable to increase or decrease a gap between the flow passage forming surface and the screw, A plurality of protrusions are provided on the outer periphery of the screw along the circumferential direction of the screw, Each of the protrusions is sharp and extends parallel to a central axis of the screw; A kneading and adjusting mechanism, wherein vertices of all of the protrusions are present within one cross section of the screw perpendicular to the central axis, and line segments connecting the vertices within the cross section form a regular polygon.

3. The kneading and adjusting mechanism according to claim 2, A clearance between the apex of the protrusion and the flow path forming surface is a minimum clearance (a); When a clearance between a flat portion between two adjacent protrusions in the circumferential direction of the screw and the flow path forming surface is defined as a maximum clearance (b), A kneading adjusting mechanism, wherein a ratio (b / a) of the minimum clearance (a) to the maximum clearance (b) is 4 or less.

4. A method for producing resin pellets, comprising: a step (a) of kneading a molten resin; and a step (b) of adjusting a degree of kneading of the molten resin in the step (a), In the step (b), a cross-sectional area of ​​a flow path through which the molten resin kneaded in the step (a) is transported is changed by a kneading adjustment mechanism to increase or decrease a time during which the molten resin is kneaded in the step (a); The kneading adjustment mechanism used in the step (b) is A pair of movable members each having a flow path forming surface that forms a part of the flow path; a screw disposed between the flow passage forming surfaces of the movable members; At least one of the pair of movable members is operable to increase or decrease a gap between the flow passage forming surface and the screw, A plurality of protrusions are provided on the outer periphery of the screw along the circumferential direction of the screw, Each of the protrusions is sharp and extends parallel to a central axis of the screw; A method for producing resin pellets, wherein vertices of all of the protrusions are present within a cross section of the screw perpendicular to the central axis, and line segments connecting the vertices within the cross section form a regular polygon.

Citation Information

Patent Citations

  • Screw device for PE cast film production

    CN212795830U

  • Same-direction rotating type double screw kneader with kneading plate

    JP1985208209A

  • Twin screw kneading extruder for mixing titanium oxide

    JP1998109309A

  • Screw type kneading extruder

    JP2006240240A

  • Kneading adjusting mechanism, extruder, continuous kneader and method for adjusting degree of kneading

    JP2009113246A