Divalent Platinum Complexes

JP7578827B2Active Publication Date: 2024-11-06GUANGDONG AGLAIA OPTOELECTRONICS MATERIALS
2 Cites 0 Cited by

Patent Information

Application Number
JP2023535593
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-12-30
Filing Date
2021-10-24
Publication Date
2024-11-06
Estimated Expiration
2041-10-24

AI Technical Summary

Technical Problem

Existing OLED materials face challenges with high production costs due to the use of expensive and contaminated rare earth metals like iridium, and there is a need for more efficient, stable, and cost-effective luminescent materials with improved energy utilization for singlet and triplet excitons.

Method used

A divalent platinum complex with ONCN tetradentate ligands is developed, featuring a specific structural formula that enhances thermal stability and photoelectric performance by incorporating functional groups to improve heavy atom effects and reduce intermolecular aggregation.

Benefits of technology

The platinum complex exhibits excellent thermal stability, high quantum efficiency, and extended device lifetime, enabling the production of high-efficiency green OLEDs with improved luminous efficiency and color purity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578827000018
    Figure 0007578827000018
  • Figure 0007578827000001
    Figure 0007578827000001
  • Figure 0007578827000002
    Figure 0007578827000002
Patent Text Reader

Abstract

The divalent platinum complex has the structure shown in formula (I). This complex has a bright green emission wavelength and can be applied to the field of OLED organic electroluminescent materials. Through structural design, the heavy atom effect of the phosphorescent material can be improved, spin coupling can be strengthened, and efficient T1-S0 conversion can be achieved, resulting in efficient luminous efficiency. Furthermore, the platinum complex molecule with the ONCN tetradentate ligand has advantages such as simple synthesis steps and easy coordination. It also has many modifiable sites, allowing for tuning of the PL emission wavelength and thermal stability. The increased steric hindrance of the carbazole group effectively reduces intermolecular aggregation, preventing the formation of exciplexes, further improving color purity and luminous efficiency. JPEG2023553155000019.jpg95170
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the field of OLED materials, and in particular to carbazole-containing divalent platinum complexes. [Background technology]

[0002] Organic Light-Emitting Diodes (OLEDs) have the advantages of self-luminescence, wide viewing angle, almost infinitely high contrast, low power consumption, extremely fast response speed, and potential flexibility and foldability, and have been widely studied and paid attention to in the last 20 years. Since their discovery in the laboratory by Chinese-American Professor Ching W. Tang in 1979, it was further discovered by SR Forrest et al. in 1998 that organometallic complexes can achieve series crossover (ISC) and long-life phosphorescence decay due to their strong spin-orbit coupling (SOC). Research has shown that phosphorescent materials can achieve an internal quantum efficiency of theoretically reaching 100% in OLEDs by fully utilizing the energy of singlet and triplet excitons during emission to improve the luminous efficiency of the complexes. In particular, Ir(I) complexes are luminescent materials that have been extensively studied and are currently widely used in the industry. However, rare earth metal Ir is expensive and highly polluting, which hinders their use in mass production. Therefore, the development of inexpensive metal complexes is desirable. Metal platinum complexes have attracted much attention from the scientific research industry in recent years due to their excellent material stability due to their planarity, high structural modification potential, and metal prices that are cheaper than iridium, and the industrialization process is also maturing. However, the industry is in dire need of simple, highly efficient, and long-life luminescent materials. The platinum complex molecule with the ONCN tetradentate ligand has simple synthesis steps, many modifiable sites, and has great room for improvement. Summary of the Invention [Problem to be solved by the invention]

[0003] In response to the above problems existing in the prior art, the present invention provides a luminescent material of platinum complex of ONCN tetradentate ligand containing functional group, which can improve the heavy atom effect of phosphorescent material and thereby improve the energy utilization rate for singlet and triplet excitons during emission. The functional group improves the thermal stability of the material by connecting different sites, providing the possibility of further industrialization of this type of material. This platinum complex exhibits excellent thermal stability, photoelectric performance, and device life when used in organic light-emitting diodes. [Means for solving the problem]

[0004] Such divalent platinum complexes have the structural formula shown in formula (I): JPEG0007578827000001.jpg95170

[0005] R1~R 24 One site of R1 to R6 in 10 and the remaining sites and A0 are independently selected from hydrogen, deuterium, halogen, substituted or unsubstituted alkyl having 1 to 20 carbon atoms, substituted or unsubstituted cycloalkyl having 3 to 20 ring carbon atoms, substituted or unsubstituted heteroalkyl having 1 to 20 carbon atoms, substituted or unsubstituted aralkyl having 7 to 30 carbon atoms, substituted or unsubstituted alkoxy having 1 to 20 carbon atoms, substituted or unsubstituted aryloxy having 6 to 30 carbon atoms, substituted or unsubstituted alkenyl having 2 to 20 carbon atoms, substituted or unsubstituted aryl having 6 to 30 carbon atoms, substituted or unsubstituted heteroaryl having 3 to 20 carbon atoms, substituted or unsubstituted alkylsilyl having 3 to 20 carbon atoms, substituted or unsubstituted arylsilyl having 6 to 20 carbon atoms, substituted or unsubstituted amino having 0 to 20 carbon atoms, acyl, carbonyl, carboxylic acid, ester, cyano, thio, sulfinyl, sulfonyl, phosphino, or adjacent R1 to R 24 are connected to each other by covalent bonds in a ring,

[0006] Ar is selected from substituted or unsubstituted alkyl having 1 to 20 carbon atoms, substituted or unsubstituted cycloalkyl having 3 to 20 ring carbon atoms, substituted or unsubstituted heteroalkyl having 1 to 20 carbon atoms, substituted or unsubstituted aralkyl having 7 to 30 carbon atoms, substituted or unsubstituted alkoxy having 1 to 20 carbon atoms, substituted or unsubstituted aryloxy having 6 to 30 carbon atoms, substituted or unsubstituted alkenyl having 2 to 20 carbon atoms, substituted or unsubstituted aryl having 6 to 30 carbon atoms, substituted or unsubstituted heteroaryl having 3 to 20 carbon atoms, substituted or unsubstituted alkylsilyl having 3 to 20 carbon atoms, substituted or unsubstituted arylsilyl having 6 to 20 carbon atoms; The heteroatom in the heteroalkyl or heteroaryl is N, S, or O; The substitution means substitution with deuterium, halogen, amino, nitro, cyano, or C1 to C4 alkyl.

[0007] Preferably, R to R 24 One site of R1 to R6 in 10 The remaining sites and A0 are each independently selected from hydrogen, deuterium, halogen, alkoxy having 1 to 10 C atoms, cyano, styryl, aryloxy, diarylamine, saturated alkyl having 1 to 10 C atoms, unsaturated alkyl having 2 to 8 C atoms, substituted or unsubstituted aryl having 5 to 20 C atoms, substituted or unsubstituted heteroaryl having 5 to 20 C atoms, or adjacent R1 to R 24 are connected to each other in a ring by a covalent bond.

[0008] Ar is selected from substituted or unsubstituted bicyclic aryl or bicyclic heteroaryl derivatives having 6 to 30 carbon atoms, substituted or unsubstituted polycyclic aryl or polycyclic heteroaryl derivatives having 3 to 30 carbon atoms. More preferably,

[0009] One site of R1-R6 is R7-R 10 is connected to one site of R1 through a CC bond, 24 At the remaining sites, R 17 , R 19 is a C1-C4 group, the others are all hydrogen, and A0 is hydrogen. Ar is selected from substituted or unsubstituted aryl, heteroaryl, and benzoheteroaryl having 5 to 30 carbon atoms.

[0010] Preferably, R 17 , R 19 is isobutyl, Ar is selected from substituted or unsubstituted phenyl, 5- or 6-membered heteroaryl, and benzoheteroaryl, the heteroatom in the heteroaryl being N or O, and the substitution means being substituted by deuterium, halogen, or C1-C4 alkyl.

[0011] Examples of the platinum metal complex according to the present invention include, but are not limited to, the following structures.

[0012] JPEG0007578827000002.jpg255165JPEG0007578827000003.jpg255158JPEG0007578827000004.jpg55170

[0013] The precursor of the complex has the structure shown in formula (II) below: JPEG0007578827000005.jpg90170However, R1~R 24 , A0, and Ar are as described above. Use of the divalent platinum complexes according to the invention as phosphorescent dopant material in the light-emitting layer in an OLED. The present invention improves the material stability, device efficiency and service life through structural design. Such compounds have simple synthetic steps and are easily accessible for maturation. Such a structure has many modifiable sites, and the steric hindrance of the carbazole groups contained therein is increased, so that the aggregation effect between molecules can be effectively reduced. Such compounds can improve the molecular spatial arrangement, color purity, and luminous efficiency by connecting functional groups at different sites. Effect of the Invention

[0014] The divalent platinum complex according to the present invention has a bright green emission wavelength and can be applied to the field of OLED organic electroluminescent materials. The present invention can improve the heavy atom effect of the phosphorescent material through structural design, strengthen the spin coupling, and achieve efficient conversion of T1-S0, resulting in efficient luminous efficiency. In addition, the platinum complex molecule of the ONCN tetradentate ligand has the advantages of simple synthesis steps, easy coordination, and the like, and also has many modifiable sites, allowing the adjustment of PL emission wavelength and thermal stability. By increasing the steric hindrance of the contained carbazole group, the aggregation effect between molecules can be effectively reduced to avoid the formation of exciplexes, and the color purity and luminous efficiency can be further improved. The organometallic complex according to the present invention can be used to fabricate a green OLED device having high fluorescent quantum efficiency, excellent thermal stability, a low extinction constant, and high luminous efficiency. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1 is a structural diagram of an element according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] The invention will now be further defined with reference to the following figures and examples. All of the raw materials used below are commercially available products. Example 1: Synthesis of compounds of structure 1 (1a, see CN110872325A, 1d is custom made) JPEG0007578827000006.jpg65170 Synthesis of intermediate 1c

[0017] Take a 2L three-neck flask, add 1a (60.0g, 101mmol), 1b (30.0g, 202mmol), Pd(PPh3)4 (5.90g, 5mmol), NaOH (8.2mg, 202mmol) and dioxane / water (1.2L / 240ml), and stir and react for 12h at 55℃ under nitrogen protection. After the reaction is completed, first, separate most of the solvent by rotation, add water, extract twice with DCM, mix with silica gel and dry by rotation, then load into a column and wash with (Hex:EA=10:1). 58g of white solid is obtained. Hydrogen spectrum data is as follows:

[0018] 1 HNMR(400MHz,CDCl3)δ8.69(s,1H),8.61(d,J=5.3Hz,1H),8.23(d,J=7.8Hz,1H),8.12-8.01(m,3H),7.91(d,J=1.4Hz,1H),7.85(d,J=1. 7Hz,1H),7.62(s,1H),7.55(s,3H),7.47-7.39(m,1H),7.30-7.26(m,1H),7.16(s,1H),7.06(d,J=8.1Hz,1H),3.92(s,3H),1.41(s,18H). Synthesis of intermediate 1e

[0019] Take a 250 mL single-neck flask and add 1c (8.0 g, 19.9 mmol), 1d (6.14 g, 21.4 mmol), and Pd 132 (0.303g, 0.42mmol), K2CO3 (5.9g, 42.7mmol), and THF / water (80ml / 16ml) are added, and the mixture is reacted at 70℃ for 12h under nitrogen protection. After the reaction is completed, most of the solvent is first separated by rotation, water is added, and the mixture is extracted twice with EA. The mixture is mixed with silica gel and dried by rotation, then loaded into a column and washed with (Hex:EA=6:1). 9.7g of white solid is obtained. Hydrogen spectrum data is as follows:

[0020] 1HNMR(400MHz,CDCl3)δ8.76(d,J=4.1Hz,2H),8.34-8.23(m,2H),8.20(d,J=7.8Hz,1H),8.13(d,J=7.8Hz,1H),8.10-8.01(m,3H),7.96(s,1 H),7.73-7.55(m,10H),7.55-7.38(m,5H),7.34(t,J=6.4Hz,1H),7.15(t,J=7.5Hz,1H),7.07(d,J=8.2Hz,1H),3.93(s,3H),1.44(s,18H). Synthesis of intermediate 1f

[0021] Take a 500ml one-neck flask, add 1e (8.5g, 11.06mmol), pyridine hydrochloride (90g), and 9mL of o-dichlorobenzene, and react at 200℃ for 6h under nitrogen protection. After the reaction is completed, extract twice with dichloromethane, mix with silica gel, dry by rotation, then load into a column and wash with (Hex:EA=6:1). The obtained crude product is slurried with methanol. 8.3g of pale yellow solid is obtained. Hydrogen spectrum data is as follows:

[0022] 1 HNMR(400MHz,CDCl3)δ8.74(d,J=4.8Hz,1H),8.64(s,1H),8.25(d,J=8.1Hz,1H),8 .17(dd,J=12.1,8.0Hz,2H),8.07(t,J=9.5Hz,3H),7.95(d,J=8.1Hz,1H),7.92(d, J=1.1Hz,1H),7.73-7.64(m,3H),7.64-7.57(m,5H),7.56-7.50(m,3H),7.50-7.39 (m,3H),7.39-7.28(m,2H),7.12-7.04(m,1H),6.97(t,J=7.0Hz,1H),1.43(s,18H). Synthesis of the compound shown in the final product structure 1

[0023] Take a 500ml one-neck flask, add 1f (2.0g, 2.65mmol), K2PtCl4 (1.32g, 3.18mmol), TBAB (85mg, 0.265mmol), and acetic acid (200mL), and react at 130℃ for 48h under nitrogen protection. After the reaction is completed, add excess deionized water to precipitate the solid, suction filter, dissolve the solid in dichloromethane, mix with silica gel and dry by rotation, then load into a column and wash with (DCM). 1.6g of yellow solid is obtained. Hydrogen spectrum data is as follows:

[0024] 1 HNMR(400MHz,CDCl3)δ8.89(d,J=5.9Hz,1H),8.21-8.01(m,3H),7.88(d,J=7.7Hz,1H),7.74-7.47(m,12H),7.47- 7.34(m,3H),7.34-7.28(m,3H),7.24(d,J=5.6Hz,2H),7.07(t,J=7.5Hz,1H),6.52(t,J=7.4Hz,1H),1.45(s,18H). Example 2: Synthesis of compound of structure 26 (26a is custom made) JPEG0007578827000007.jpg89170 Synthesis of intermediate 26b

[0025] Take a 250 mL single-neck flask and add 1c (8.0 g, 19.9 mmol), 26a (8.5 g, 21.4 mmol), and Pd 132 (0.303g, 0.42mmol), K2CO3 (5.9g, 42.7mmol), and THF / water (80ml / 16ml) were added, and the mixture was reacted at 70℃ for 12h under nitrogen protection. After the reaction was completed, most of the solvent was first separated by rotation, water was added, and the mixture was extracted twice with EA, mixed with silica gel and dried by rotation, then loaded into a column and washed with (Hex:EA=6:1). 11.08g of white solid was obtained. Hydrogen spectrum data was as follows:

[0026] 1HNMR(400MHz,Chloroform-d)δ8.67(d,J=4.5Hz,1H),8.22-8.17(m,3H),8.17-8.08(m,3H),7.95-7.86(m,4H),7.72(dd,J=6.8,2.4Hz, 1H),7.69-7.59(m,2H),7.53-7.27(m,10H),7.15(ddd,J=8.7,7.5,1.2Hz,1H),6.90(dd,J=7.7,1.2Hz,1H),3.90(s,3H),1.35(s,36H). Synthesis of intermediate 26c

[0027] Take a 500ml one-neck flask, add 26b (9.74g, 11.06mmol), pyridine hydrochloride (90g), and 9mL of o-dichlorobenzene, and react at 200℃ for 6h under nitrogen protection. After the reaction is completed, extract with dichloromethane twice, mix with silica gel and dry by rotation, then load into a column and wash with (Hex:EA=6:1). The obtained crude product is slurried with methanol. 8.3g of pale yellow solid is obtained. Hydrogen spectrum data is as follows:

[0028] 1 HNMR(400MHz,Chloroform-d)δ9.18-9.11(m,1H),8.26-8.09(m,5H),7.94(dd,J=8.2,1.2Hz,1H),7.74(d,J=2.1Hz,1H),7.68-7.62(m,3H) ,7.60-7.52(m,2H),7.51-7.44(m,3H),7.40-7.26(m,9H),7.17(d,J=6.7Hz,2H),7.09(ddd,J=8.4,7.5,1.2Hz,1H),1.36(d,J=2.9Hz,38H). Synthesis of the final product shown in Structure 26

[0029] Take a 500ml single-neck flask, add 26c (2.3g, 2.65mmol), K2PtCl4 (1.32g, 3.18mmol), TBAB (85mg, 0.265mmol), and acetic acid (200mL), and react at 130℃ for 48h under nitrogen protection. After the reaction is completed, add excess deionized water to precipitate the solid, suction filter, dissolve the solid in dichloromethane, mix with silica gel and dry by rotation, then load into a column and wash with (DCM). 1.8g of yellow solid is obtained. Hydrogen spectrum data is as follows:

[0030] 1 HNMR(400MHz,CDCl3)δ8.89(d,J=5.9Hz,1H),8.21-8.01(m,3H),7.88(d,J=7.7Hz,1H),7.74-7.47(m,12H),7.47- 7.34(m,3H),7.34-7.28(m,3H),7.24(d,J=5.6Hz,2H),7.07(t,J=7.5Hz,1H),6.52(t,J=7.4Hz,1H),1.45(s,18H).

[0031] Example 3: Synthesis of compound of structure 36 (36a is custom made) JPEG0007578827000008.jpg80170 Synthesis of intermediate 36c

[0032] In a dry 500mL two-neck flask, 36a (14.7g, 50mmol) was added with 36b (11.8g, 50mmol), toluene (120mL), ethanol (60mL), and 2mol / L potassium carbonate solution (60mL). The mixture was first sonicated for 5-10 minutes, and then rapidly stirred with nitrogen for 5 minutes. The catalyst tetrakis(triphenylphosphine)palladium (1.8g, 1.5mmol) was rapidly added and a large amount of nitrogen was transferred for 10 minutes. The mixture was heated to 100℃ and stirred for 12 hours. During the treatment, the mixture was first extracted, spun dry, and subjected to column chromatography with petroleum ether and dichloromethane to obtain 14.5g of white solid product with a yield of 90%. The hydrogen spectrum data was as follows:

[0033] 1 HNMR(400MHz,Chloroform-d)δ9.54(s,1H),8.37(dd,J=4.0,2.2Hz,1H),8.17-8.10(m,2H),7.94(dd,J=7.5,2.2Hz ,1H),7.56(s,1H),7.55-7.48(m,2H),7.46(dd,J=7.5,3.9Hz,1H),7.34(td,J=7.4,1.3Hz,1H),7.28-7.19(m,1H). Synthesis of intermediate 36d

[0034] In a dry 500mL two-neck flask, 36c (14.5g, 50mmol) is added with 1a (28.7g, 50mmol), toluene (120mL), ethanol (60mL), and 2mol / L potassium carbonate solution (60mL). The mixture is first sonicated for 5-10 minutes, and then nitrogen is rapidly added for 5 minutes. The catalyst tetrakis(triphenylphosphine)palladium (1.8g, 1.5mmol) is rapidly added and a large amount of nitrogen is transferred for 10 minutes. The mixture is heated to 100℃ and stirred for 12 hours. During the process, the mixture is first extracted, spun dry, and subjected to column chromatography with petroleum ether and dichloromethane to obtain 10.2g of white solid product with a yield of 78%. The hydrogen spectrum data is as follows:

[0035] 1 HNMR(400MHz,Chloroform-d)δ9.54(s,1H),8.71(dd,J=4.1,2.2Hz,1H),8.19(t,J=2.0Hz,1H),8.17- 8.08(m,2H),8.02(dd,J=1.9,0.7Hz,1H),7.96-7.87(m,4H),7.80(ddd,J=8.5,1.9,1.2Hz,1H),7.67( t,J=8.6Hz,1H),7.57(d,J=8.3Hz,1H),7.54-7.48(m,2H),7.47-7.32(m,7H),7.24(ddd,J=7.9,7.3,1 .6Hz,1H),7.15(ddd,J=8.7,7.5,1.2Hz,1H),6.90(dd,J=7.7,1.2Hz,1H),3.90(s,3H),1.35(s,18H). Synthesis of intermediate 36f

[0036] In a 250ml three-neck flask, 36d (5.0g, 1.0eq), 36e (5.7g, 3.0eq), Cu (230mg, 0.5eq), CuI (688mg, 0.5eq), 1,10-phenanthroline (1.30g, 1.0eq), and cesium carbonate (7.06g, 3.0eq) were added, and 100ml of anhydrous xylene was used as the reaction solvent. Under nitrogen protection, the mixture was reacted at 160℃ oil bath temperature for 3d, and then cooled to room temperature. The reaction solution was directly filtered using EA as the eluent to remove inorganic salts, and then mixed with silica gel and subjected to column chromatography (chromatography solution hex:EA=8:1), and 3.9g of yellow fluorescent product spot was collected. Hydrogen spectrum data is as follows: 1 HNMR(400MHz,Chloroform-d)δ8.71(dd,J=4.1,2.2Hz,1H),8.24(dd,J=1.9,0.7Hz ,1H),8.22-8.08(m,5H),8.02(ddt,J=8.9,1.3,0.5Hz,1H),7.97-7.85(m,5H),7.8 4-7.77(m,2H),7.71-7.62(m,4H),7.59-7.53(m,1H),7.53-7.27(m,13H),7.15(dd d,J=8.7,7.5,1.2Hz,1H),6.90(dd,J=7.7,1.2Hz,1H),3.90(s,3H),1.35(s,18H). Synthesis of intermediate 36g

[0037] In a 100 ml single-neck flask, 36f (3.15 g), pyridine hydrochloride (30.0 g), and o-dichlorobenzene (3.0 ml) are added, and the mixture is reacted under nitrogen protection at an oil bath temperature of 200°C for 8 h, and then cooled to room temperature. The mixture is dissolved in a large amount of water and extracted three times with DCM. The organic phase is spun dry, mixed with silica gel, and subjected to column chromatography (chromatography solution hex:EA=10:1) to obtain 2.8 g of a pale yellow product. The hydrogen spectrum data is as follows: 1HNMR(400MHz,Chloroform-d)δ8.71(dd,J=4.1,2.2Hz,1H),8.24(dd,J=1.9,0.7Hz,1H),8.21-8.08(m,5H),8.06-7.97(m,2H),7 .97-7.77(m,6H),7.71-7.62(m,4H),7.59-7.53(m,1H),7.53-7.44(m,5H),7.44-7.20(m,8H),7.03-6.94(m,2H),1.35(s,18H). Synthesis of the final product shown in Structure 36

[0038] Take a 250ml one-neck flask, add 36g (105mg, 0.124mmol), K2PtCl4 (70mg, 0.167mmol), 18-crown-6 ether (6mg, 0.012mmol), and acetic acid (5mL), and react at 130℃ for 48h under nitrogen protection. After the reaction is completed, add excess deionized water to precipitate the solid, suction filter, dissolve the solid with dichloromethane, separate the solvent by rotation, mix with silica gel, then load into a column and wash with (Hex:DCM:EA=20:20:1). After passing through the column, recrystallize the product with dichloromethane:n-hexane=1:4. Obtain 85mg of red solid. Hydrogen spectrum data is as follows: 1 HNMR(400MHz,Chloroform-d)δ8.84(dd,J=5.4,2.3Hz,1H),8.21(d,J=1.8Hz,1H),8.17-7.99(m,5H),7.94(dd,J=8.1,1.2Hz,1H),7.81(t,J =1.2Hz,1H),7.76-7.62(m,6H),7.58-7.43(m,12H),7.42-7.26(m,8H),7.25-7.15(m,2H),7.09(ddd,J=8.5,7.5,1.2Hz,1H),1.35(s,18H).

[0039] Example 4: Synthesis of compound of structure 53 (53a is custom made) JPEG0007578827000009.jpg72170Synthesis of intermediate 53c:

[0040] In a dry 500mL two-neck flask, 53a (14.7g, 50mmol) is added with 53b (11.8g, 50mmol), toluene (120mL), ethanol (60mL), and 2mol / L potassium carbonate solution (60mL). The mixture is first ultrasonicated for 5-10 minutes, and then nitrogen is rapidly stirred for 5 minutes. The catalyst tetrakis(triphenylphosphine)palladium (1.8g, 1.5mmol) is rapidly added, and a large amount of nitrogen is transferred for 10 minutes. The mixture is heated to 100°C and stirred for 12 hours. During the treatment, the mixture is first extracted, the solvent is separated by rotation, and then column chromatography is performed with petroleum ether and dichloromethane to obtain 14.5g of white solid product with a yield of 90%. The hydrogen spectrum data is as follows:

[0041] 1 HNMR(400MHz,Chloroform-d)δ9.72(s,1H),8.37(dd,J=4.0,2.2Hz,1H),8.19-8.13(m,1H),8.13-8.06(m,1H),7.91(dd,J=7.4,2.3Hz,1 H),7.83(d,J=1.9Hz,1H),7.71(dd,J=8.1,2.0Hz,1H),7.55-7.42(m,2H),7.34(td,J=7.4,1.3Hz,1H),7.24(ddd,J=7.9,7.3,1.6Hz,1H). Synthesis of intermediate 53d

[0042] In a dry 500mL two-neck flask, 53c (14.5g, 50mmol) is added with 1a (28.7g, 50mmol), toluene (120mL), ethanol (60mL), and 2mol / L potassium carbonate solution (60mL). The mixture is first ultrasonicated for 5-10 minutes, and then nitrogen is rapidly stirred for 5 minutes. The catalyst tetrakis(triphenylphosphine)palladium (1.8g, 1.5mmol) is rapidly added, and a large amount of nitrogen is transferred for 10 minutes. The mixture is heated to 100℃ and stirred for 12 hours. During the process, the mixture is first extracted, the solvent is separated by rotation, and then column chromatography is performed with petroleum ether and dichloromethane to obtain 10.2g of white solid product with a yield of 78%. The hydrogen spectrum data is as follows:

[0043] 1 HNMR(400MHz,Chloroform-d)δ9.72(s,1H),8.71(dd,J=4.1,2.2Hz,1H),8.22 -8.06(m,5H),7.97-7.86(m,5H),7.84-7.74(m,2H),7.71-7.60(m,2H),7.55-7 .47(m,2H),7.45-7.30(m,6H),7.24(ddd,J=7.9,7.3,1.6Hz,1H),7.15(ddd,J =8.7,7.5,1.2Hz,1H),6.90(dd,J=7.7,1.2Hz,1H),3.90(s,3H),1.35(s,18H). Synthesis of intermediate 53f

[0044] In a 250ml three-neck flask, 53d (5.0g, 1.0eq), 53e (7.0g, 3.0eq), Cu (230mg, 0.5eq), CuI (688mg, 0.5eq), 1,10-phenanthroline (1.30g, 1.0eq), and cesium carbonate (7.06g, 3.0eq) were added, and 100ml of anhydrous xylene was used as the reaction solvent. Under nitrogen protection, the mixture was reacted at an oil bath temperature of 160°C for 3d, and then cooled to room temperature. The reaction solution was directly filtered out using EA as the eluent, and then mixed with silica gel and subjected to column chromatography (chromatography solution hex:EA=8:1), and 4.1g of yellow fluorescent product spots were collected. The hydrogen spectrum data was as follows: 1 HNMR(400MHz,Chloroform-d)δ8.71(dd,J=4.1,2.2Hz,1H),8.40-8.28(m,5H),8. 28-8.16(m,3H),8.11(d,J=2.2Hz,1H),7.97-7.85(m,5H),7.85-7.77(m,4H),7.67 (t,J=8.5Hz,1H),7.57-7.35(m,14H),7.31(ddd,J=7.9,7.2,1.6Hz,1H),7.15(dd d,J=8.7,7.5,1.2Hz,1H),6.90(dd,J=7.7,1.2Hz,1H),3.90(s,3H),1.35(s,18H). Synthesis of intermediate 53g

[0045] In a 100 ml single-neck flask, 53f (3.40 g), pyridine hydrochloride (30.0 g), and o-dichlorobenzene (3.0 ml) are added, and the mixture is reacted under nitrogen protection at an oil bath temperature of 200°C for 8 h, and then cooled to room temperature. The mixture is dissolved in a large amount of water and extracted three times with DCM. The organic phase is separated by rotation to remove the solvent, and mixed with silica gel. Column chromatography (chromatography solution hex:EA=10:1) is performed to obtain 2.9 g of a pale yellow product. The hydrogen spectrum data is as follows: 1 HNMR(400MHz,Chloroform-d)δ8.71(dd,J=4.1,2.2Hz,1H),8.40-8.28(m,5H),8.28-8.16(m,4H),8.11(d,J=2.2Hz,1H),7.99(dd,J =8.7,1.2Hz,1H),7.96-7.73(m,8H),7.67(t,J=8.5Hz,1H),7.56-7.37(m,13H),7.36-7.20(m,2H),7.03-6.94(m,2H),1.35(s,18H). Synthesis of the final product shown in structure 53

[0046] Take a 250ml one-neck flask, add 53g (115mg, 0.124mmol), K2PtCl4 (70mg, 0.167mmol), 18-crown-6 ether (6mg, 0.012mmol), and acetic acid (5mL), and react at 130℃ for 48h under nitrogen protection. After the reaction is completed, add excess deionized water to precipitate the solid, suction filter, dissolve the solid in dichloromethane, swirl dry, mix with silica gel and pass through a column (Hex:DCM:EA=20:20:1). After passing through the column, recrystallize the product with dichloromethane:n-hexane=1:4. Obtain 85mg of red solid. Hydrogen spectrum data is as follows: 1HNMR(400MHz,Chloroform-d)δ8.84(dd,J=6.0,1.8Hz,1H),8.40-8.28(m,5H),8.28-8.18(m,2H),8.15-8.10(m,1H),8.04-7.99(m,1H),7.94(dd, J=8.1,1.2Hz,1H),7.80-7.61(m,7H),7.59-7.42(m,13H),7.39-7.26(m, 5H),7.25-7.15(m,2H),7.09(ddd,J=8.5,7.5,1.2Hz,1H),1.35(s,18H).

[0047] Luminescent properties of the compound: JPEG0007578827000010.jpg65170

[0048] The following are examples of the use of the compounds according to the invention. How the device is made: First, a transparent conductive ITO glass substrate 10 (on which an anode 20 is to be applied) is washed in sequence with a detergent solution, deionized water, ethanol, acetone, and deionized water, and then treated with oxygen plasma for 300 seconds. Next, HATCN with a thickness of 3 nm is evaporated onto the ITO as a hole injection layer 30 . Next, the compound TAPC is evaporated to form a hole transport layer 40 having a thickness of 50 nm. Next, a 7 nm thick layer of guest complex (9%) and host TCTA (91%) is evaporated onto the hole transport layer as the light emitting layer 60 . Next, a 3 nm thick layer of guest complex (9%) and host TCTA (91%) is evaporated onto the hole transport layer as the light emitting layer 60 . Next, TmPyPb having a thickness of 50 nm is evaporated onto the light-emitting layer as a hole blocking layer 70 . Finally, 0.8 nm of LiF is evaporated as the electron injection layer 80 and 100 nm of Al is evaporated as the cathode 80 of the device. The structure of the device is shown in FIG. The structural formula of the compound used in the element is as follows: JPEG0007578827000011.jpg108170

[0049] Element results: 20mA / cm 2 The device performances of the organic electroluminescence devices in Comparative Example 1 and Comparative Example 2 at a current density of 1000 nm are listed in Table 1.

[0050] Table 1 JPEG0007578827000012.jpg82170

[0051] The organometallic complex according to the present invention maintains high quantum efficiency while slightly lowering the driving voltage of the device and improving the luminous efficiency. However, compared with the comparative example LT95, the life of the device according to the embodiment is qualitatively improved obviously. As can be seen from the data of this series of devices, when such a divalent platinum complex is used as a phosphorescent emitting ligand material, an OLED device with high luminous efficiency can be manufactured and a very long life can be achieved.

[0052] The above various embodiments are merely examples and do not limit the scope of protection of the present invention. The materials and structures in the present invention may be replaced with other materials and structures without departing from the spirit thereof. It should be understood that those skilled in the art can make many modifications and changes based on the concept of the present invention without exerting creative efforts. Therefore, any technical solution that those skilled in the art can obtain through analysis, reasoning or partial study based on the prior art is within the scope of protection limited by this application.

Claims

1. A divalent platinum complex having a structure represented by formula (I): In the formula, R 1 ~R 24 R in 1 ~R 6 One of the sites is R 7 ~R 10 Connected to one of the sites with a C-C bond, Remaining sites and A 0 are each independently selected from hydrogen, deuterium, halogen, a substituted or unsubstituted alkyl group having 1 to 20 carbon atoms, a substituted or unsubstituted cycloalkyl group having 3 to 20 ring carbon atoms, a substituted or unsubstituted heteroalkyl group having 1 to 20 carbon atoms, a substituted or unsubstituted aralkyl group having 7 to 30 carbon atoms, a substituted or unsubstituted alkoxy group having 1 to 20 carbon atoms, a substituted or unsubstituted aryloxy group having 6 to 30 carbon atoms, a substituted or unsubstituted alkenyl group having 2 to 20 carbon atoms, a substituted or unsubstituted aryl group having 6 to 30 carbon atoms, a substituted or unsubstituted heteroaryl group having 3 to 20 carbon atoms, a substituted or unsubstituted alkylsilyl group having 3 to 20 carbon atoms, a substituted or unsubstituted arylsilyl group having 6 to 20 carbon atoms, a substituted or unsubstituted amino group having 0 to 20 carbon atoms, an acyl group, a carboxylic acid, an ester group, a cyano group, a sulfinyl group, a sulfonyl group, and a phosphino group, or an adjacent R 1 ~R 24 are connected to each other by covalent bonds in a ring, Ar is selected from the group consisting of substituted or unsubstituted alkyl groups having 1 to 20 carbon atoms, substituted or unsubstituted cycloalkyl groups having 3 to 20 ring carbon atoms, substituted or unsubstituted heteroalkyl groups having 1 to 20 carbon atoms, substituted or unsubstituted aralkyl groups having 7 to 30 carbon atoms, substituted or unsubstituted alkoxy groups having 1 to 20 carbon atoms, substituted or unsubstituted aryloxy groups having 6 to 30 carbon atoms, substituted or unsubstituted alkenyl groups having 2 to 20 carbon atoms, substituted or unsubstituted aryl groups having 6 to 30 carbon atoms, substituted or unsubstituted heteroaryl groups having 3 to 20 carbon atoms, substituted or unsubstituted alkylsilyl groups having 3 to 20 carbon atoms, and substituted or unsubstituted arylsilyl groups having 6 to 20 carbon atoms; the heteroatom in the heteroalkyl or heteroaryl group is N, S, or O; the substitution is by deuterium, halogen, amino, nitro, cyano or C1-C4 alkyl; A divalent platinum complex comprising:

2. R 1 ~R 24 R in 1 ~R 6 One of the sites is R 7 ~R 10 A is connected to one of the sites by a C-C bond, and the remaining sites and A 0 are each independently selected from hydrogen, deuterium, halogen, an alkoxy group having 1 to 10 C atoms, a cyano group, a styryl group, an aryloxy group, a diarylamine group, a saturated alkyl group having 1 to 10 C atoms, an unsaturated alkyl group having 2 to 8 C atoms, a substituted or unsubstituted aryl group having 5 to 20 C atoms, and a substituted or unsubstituted heteroaryl group having 5 to 20 C atoms, or R 1 ~R 24 are connected to each other by a covalent bond in a ring; 2. The divalent platinum complex according to claim 1 .

3. Ar is selected from substituted or unsubstituted bicyclic aryl or heteroaryl derivatives having 6 to 30 carbon atoms, and substituted or unsubstituted polycyclic aryl or heteroaryl derivatives having 3 to 30 carbon atoms; 3. The divalent platinum complex according to claim 2 .

4. R 1 ~R 24 R in 1 ~R 6 One of the sites is R 7 ~R 10 is connected to one site of the aryl group by a C-C bond, and at the remaining site, R 17 , and R 19 is a C1-C4 group, the others are all hydrogen, and A 0 is hydrogen, 4. The divalent platinum complex according to claim 3.

5. Ar is selected from the group consisting of substituted or unsubstituted aryl groups having 5 to 30 carbon atoms, heteroaryl groups, and benzoheteroaryl groups; 5. The divalent platinum complex according to claim 4.

6. R 17 , and R 19 is an isobutyl group, Ar is selected from the group consisting of a substituted or unsubstituted phenyl group, a 5- or 6-membered heteroaryl group, and a benzoheteroaryl group, the heteroatom in the heteroaryl group being N or O, and the substitution being by deuterium, halogen, or a C1-C4 alkyl group; 6. The divalent platinum complex according to claim 5 .

7. 2. The divalent platinum complex of claim 1, having any one of the following structures:

8. A precursor of the divalent platinum complex according to any one of claims 1 to 7, having a structure represented by the following formula (II): In the formula, R 1 ~R 24 , A 0 and Ar is as defined above. A precursor of a divalent platinum complex.

9. Use of a divalent platinum complex according to any one of claims 1 to 7 as phosphorescent dopant material in an emissive layer in an OLED.

Citation Information

Patent Citations

  • Organometallic compound, and organic light-emitting device and diagnostic composition that include the same

    JP2018002722A

  • Organic light-emitting materials based on tetradentate platinum ONCN complexes, their synthesis methods and use in organic light-emitting diodes