Surface-treated copper foil, copper-clad laminates and printed wiring boards
JP7579704B2Active Publication Date: 2024-11-08JX NIPPON MINING & METALS CORP
View PDF 0 Cites 0 Cited by
Patent Information
- Application Number
- JP2020516355
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-07-19
- Filing Date
- 2019-04-22
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2039-04-22
Smart Images

Figure 00000020_0000 
Figure 00000020_0001 
Figure 00000021_0000
Abstract
The surface-treated copper foil 1 has a copper foil 2 and a first surface-treated layer 3 formed on one side of the copper foil 2. In an XPS depth profile, the first surface-treated layer 3 of the surface-treated copper foil 1 has a Ni concentration of 0.1 to 15.0 atm% relative to the total amount of C, N, O, Zn, Cr, Ni, Co, Si, and Cu elements when sputtered for 1 minute at a sputtering rate of 2.5 nm / min (SiO2 equivalent). The copper-clad laminate 10 includes the surface-treated copper foil 1 and an insulating substrate 11 bonded to the first surface-treated layer 3 of the surface-treated copper foil 1.
Need to check novelty before this filing date? Find Prior Art