Press-fit pin and method for manufacturing press-fit pin
A multilayer plating and heat treatment process for press-fit pins addresses the instability and wear issues of Sn-plated copper substrates, resulting in a stable and durable terminal with consistent electrical performance.
Patent Information
- Application Number
- JP2019033519
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-02-27
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2039-02-27
AI Technical Summary
Existing press-fit terminals with Sn-plated copper substrates have uneven contact surfaces leading to unstable electrical characteristics and poor wear resistance, limiting their use in precision electronic components.
A multilayer plating process involving Ni, Ni-Sn diffusion, Sn, and SnO coating layers, followed by heat treatment in an oxygen atmosphere, creates a flat and wear-resistant surface.
The resulting press-fit pin achieves stable electrical characteristics and improved wear resistance, ensuring consistent contact resistance and dimensional stability even with repeated use.
Smart Images

Figure 0007582638000001 
Figure 0007582638000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a press-fit pin, which is a type of press-fit terminal that has a high holding force on an IC board, etc., without soldering, by giving a spring property to the insertion part. More specifically, the present invention relates to a press-fit pin that has excellent abrasion resistance and electrical properties such as electrical conductivity and resistance value by forming a multilayer plating layer on the surface of a base body and performing heat treatment, and a method for manufacturing the press-fit pin. [Background technology]
[0002] In recent years, the use of solderless press-fit terminals has been increasing in the assembly process of devices using circuit boards. Press-fit terminals can be mounted using a simple press-fit method, simplifying the process. By eliminating the solder mounting process, it is possible to significantly reduce manufacturing costs, and by reducing harmful substances such as lead contained in the solder, it can be said to be an environmentally friendly mounting method.
[0003] A press-fit pin, which is one type of press-fit terminal, has a press-fit area created by plastic processing in part of it, and by processing the press-fit area to have spring properties (cross-sectional shape is N-type, M-type, H-type, etc.), the terminal can have a high retention force on the board just by pressing it into the through-hole of the IC board without soldering. In order to improve (or add) the wear resistance and electrical properties of the press-fit pin, the base material that forms the press-fit pin, such as copper, iron, or aluminum, is plated with Sn or the like.
[0004] Patent Document 1 states that the objective of the present invention is to provide a Pb-free Sn-plated copper substrate that is capable of stably forming a plating layer that is less susceptible to whisker formation even when an external stress is applied, and has excellent solderability (Patent Document 1: Objective) and states that the Sn-plated copper substrate 1 of the present invention comprises at least one plating film layer 5 having a thickness of 1.5 μm or more, the plating film layer 5 being formed by laminating an intermediate Sn plating layer 3IL and a Cu plating layer 4 in this order on a metal substrate 2 that is a pure copper plate, a copper alloy plate, or a copper-plated metal plate, and An outermost Sn plating layer 3OL having a layer thickness of 0.2 to 1.5 μm is provided on the plating film layer 5, with a total thickness including the plating film layer 5 being 3 μm or more, and at least either the grain boundaries 3g or the grain interiors 3c of the intermediate Sn plating layer 3IL and the outermost Sn plating layer 3OL have an Sn-Cu alloy phase 6 formed by diffusing Cu originating from at least one of the Cu plating layer 4 and the metal substrate 2 (Patent Document 1: Solution)." A Sn-plated copper substrate, a method for manufacturing the Sn-plated copper substrate, and a lead frame and a connector terminal using the same (Name of Invention) are disclosed. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2009-144210 A Summary of the Invention [Problem to be solved by the invention]
[0006] The Sn-plated copper substrate, the manufacturing method of the Sn-plated copper substrate, and the lead frame and connector terminal using the same (Patent Document 1: Title of the Invention) according to Patent Document 1 are technologies related to Sn-plated copper substrates used for semiconductor lead frames and connector terminals for electronic components. Specifically, it is a technology for laminating a Sn-plated layer and a Cu-plated layer in this order on a metal substrate such as a copper alloy plate, and further laminating a Sn-plated layer on the outermost layer. As can be seen from FIG. 1 of Patent Document 1, the plating surface is uneven and there is local variation. Considering that the intended use is a terminal, the unevenness of the contact surface causes contact resistance to occur only in the contact area, which makes the electrical characteristics unstable when considering use as a precision electronic component, and since the Sn-plated layer is formed on the outermost layer and is a metal, there is a limit to the wear resistance due to the material properties, so it cannot be said that it is sufficient (in terms of wear resistance).
[0007] The object of the present invention is to provide a press-fit pin that has stable electrical characteristics due to its flat surface (if the contact surface is uneven, contact resistance will be concentrated only in the contact area) and is also dimensionally stable (including dimensional reproducibility) due to its abrasion resistance.Furthermore, it provides a press-fit pin that can be heat-treated without flowing nitrogen or the like in a reflow furnace, thereby reducing production costs. [Means for solving the problem]
[0008] In order to solve the above problems, the invention described in claim 1 is a method for manufacturing a press-fit pin by forming a plating layer by performing a second plating process on a base body of the press-fit pin and then performing a predetermined heat treatment, the method comprising the steps of plating a Ni layer on the base body of the press-fit pin, S The process includes a step of plating the n-layer and a step of heat treating the coating at a temperature of 232°C to 350°C in an atmosphere containing oxygen. After the heat treatment, the thickness of the Sn layer is 0.03 μm to 5 μm. The present invention is characterized by being a method for manufacturing a press-fit pin. Effect of the Invention
[0012] The press-fit pin according to the present invention is a press-fit pin obtained by applying multi-layer plating to a base body of the press-fit pin and then performing a predetermined heat treatment. It has a Ni plating layer as a first layer, a Ni-Sn diffusion layer as a second layer, a Sn layer as a third layer, and a SnO coating layer as a fourth layer. Unlike the Sn-plated copper substrate and the manufacturing method of the Sn-plated copper substrate and the lead frame and connector terminal using the same according to Patent Document 1, the press-fit pin according to the present invention has a flat surface and is free of localized shape variations (unevenness), resulting in stable electrical characteristics.
[0013] Furthermore, the fourth layer is an SnO layer, which provides abrasion resistance and excellent dimensional stability. Since it is obtained by heat treatment in an O2 reflow furnace, it can be heat-treated at a lower cost than heat treatment in a reducing atmosphere such as Ar or N2, and the fourth layer becomes an SnO layer due to the oxidation of the surface, which provides superior abrasion resistance (than an Sn layer). Since press-fit pins are inserted and removed during use, abrasion resistance is particularly important. Even if the surface of the press-fit pin wears away due to repeated use, a new SnO layer can be formed by heat treatment again, so that the press-fit pin has excellent reproducibility in dimensional stability, which is a property directly related to the contact resistance value, taking into account its intended use as a press-fit pin. [Brief description of the drawings]
[0014] [Figure 1] 1 is a press-fit pin according to the present invention, and an enlarged partial cross-sectional view (plating layer structure) of the surface of the press-fit pin. [Diagram 2] 1A to 1C are diagrams for explaining a manufacturing process of a press-fit pin. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] <Surface plating layer structure of press-fit pins> An embodiment of a press-fit pin according to the present invention will be described in detail below with reference to Figures 1 and 2. Figure 1 is a partial enlarged cross-sectional view of a press-fit pin according to the present invention and the surface of the press-fit pin (plating layer structure).
[0016] The press-fit pin 10 according to the present invention is formed by plating the base body 20 of the press-fit pin 10, followed by a predetermined heat treatment. As shown in Fig. 1 (partially enlarged cross-sectional view), the press-fit pin 10 has, on the base body 20, a Ni plating layer 30 as a first layer, a Ni-Sn diffusion layer 40 as a second layer, a Sn plating layer 50 as a third layer, and a SnO coating layer 60 as a fourth layer. In this specification, the first layer, second layer, third layer, and fourth layer are defined as the first layer, second layer, third layer, and fourth layer counting from the side of the press-fit pin that is in direct contact with the base body 20.
[0017] The thickness of the Ni plating layer 30 as the first layer is preferably 0.03 μm to 5 μm, and the thickness of the Sn plating layer 50 as the third layer is preferably 0.03 μm to 5 μm. The Ni—Sn diffusion layer 40 as the second layer is sufficient if it exists, and the thickness of the SnO coating layer 60 as the fourth layer is preferably 8 Å (angstroms) or more.
[0018] <Press-fit pin manufacturing process (plating process, heat treatment process)> 2 is a diagram for explaining the manufacturing process of the press-fit pin 10 according to the present invention. As shown in FIG. 2, the manufacturing process of the press-fit pin 10 comprises a plating step and a heat treatment step. The plating method used in the plating step is generally electrolytic plating (electrical plating) since the press-fit pin 10 is a part used as a terminal, but electroless plating (chemical plating) may also be used. Furthermore, it goes without saying that any other plating method may be used for the plating method of the press-fit pin 10 according to the present invention, or a method similar to a plating method (e.g., vapor deposition, sputtering, etc.) may also be used.
[0019] In the plating process of the press-fit pin 10 according to the present invention, the press-fit pin 10 (base body 20) made of a material such as a copper alloy is subjected to a pre-plating base treatment, and then Ni plating is performed to form a first layer, which is then plated with Sn. This Sn-plated layer becomes the third layer after heat treatment (see FIG. 2).
[0020] The heat treatment process for the press-fit pin 10 according to the present invention is characterized in that the heat treatment is performed in the presence of oxygen without flowing nitrogen or the like (without performing the heat treatment in a reducing atmosphere). That is, the heat treatment is performed in an inexpensive O2 reflow furnace (heat treatment in the presence of Ar or N2 is costly). The heat treatment is performed in the presence of oxygen at a set temperature such that the temperature of the coating (plating layer: Ni plating layer 30 and Sn plating layer 50) is 232°C to 350°C.
[0021] The Ni-Sn diffusion layer 40, which is the second layer formed during the heat treatment, is formed by diffusing the Sn component into the first layer, Ni plating layer 30 (the melting point of Ni is 1455°C), by heat treating at a set temperature that brings the temperature of the coating (plated layer: Ni plating layer 30 and Sn plating layer 50) to a temperature equal to or higher than the melting point of Sn (232°C). The fourth layer, SnO coating 60, is formed by oxidizing the surface of the third layer, Sn plating layer 50, since the heat treatment is performed in an atmosphere containing sufficient oxygen (see FIG. 2). <Effect of press-fit pins>
[0022] The purpose of plating is decoration, corrosion prevention, surface hardening, imparting functionality (mechanical, electrical, magnetic, optical properties), etc. The press-fit pin 10 according to the present invention is a terminal part, and the plating film in the contact part must have a low and stable contact resistance value over a long period of time.
[0023] Specifically, the plated surface must be smooth and uniform so that unevenness does not form on the contact surface and contact resistance is not concentrated only in the contact areas. In other words, the plated film must be free of pinholes, cracks, etc., and the resistance value must not change by corroding the base metal (base body 20 in this invention). The hardness must be such that the contact resistance does not change as the surface wears away and the contact area changes with frequent use such as insertion and removal, i.e., it must be wear-resistant.
[0024] The press-fit pin 10 according to the present invention is obtained by applying multi-layer plating to a base body 20 of the press-fit pin 10, followed by a prescribed heat treatment. It comprises a Ni plating layer 30 as a first layer, a Ni-Sn diffusion layer 40 as a second layer, a Sn plating layer 50 as a third layer, and a SnO coating layer 60 as a fourth layer. The press-fit pin 10 has a flat surface (the plated surface is smooth and uniformly formed), so there is no local variation and the electrical characteristics are stable.
[0025] The press-fit pin 10 has a SnO coating layer 60 as a fourth layer. The SnO oxide film is harder than the metal Sn, and therefore has wear resistance, and wear is less caused by repeated piercing and pulling, and has excellent dimensional stability. That is, the surface is oxidized to form the fourth layer as the SnO coating layer 60, and therefore the press-fit pin 10 has better wear resistance than metals. Even if the surface of the press-fit pin 10 wears due to repeated use, a new SnO layer 60 can be formed by heat treatment again, so that the press-fit pin 10 has excellent reproducibility in dimensional stability, which is a property directly related to the resistance value. Furthermore, the press-fit pin 10 is obtained by heat treatment in an atmosphere containing oxygen (heat treatment in an O2 reflow furnace), and therefore the heat treatment can be performed at a lower cost than heat treatment in a reducing atmosphere such as Ar or N2.
[0026] Regarding the conductivity of the plating film, it is required that the contact resistance value be small and stable over a long period of time, but the press-fit pin 10 according to the present invention is characterized in that it intentionally forms the SnO coating layer 60 as the fourth layer. In general, it can be said that it is rather undesirable for the contact resistance of the plating film to increase due to the influence of oxide films, sulfide films, organic films, etc. This is because the press-fit pin 10 having the SnO coating layer 60 formed as the fourth layer would seem to tend to have a larger contact resistance.
[0027] However, the press-fit pin 10 according to the present invention is based on the idea that better performance can be achieved by considering the improved wear resistance and dimensional stability, and even dimensional reproducibility (even if the surface of the press-fit pin wears away with repeated use, a new SnO layer can be formed by heat treatment again) due to the formation of the SnO coating layer 60, rather than the damage that tends to increase the contact resistance. In short, it is important to improve wear resistance so that the contact resistance does not change as the contact area changes due to wear on the surface (due to frequent use such as insertion and removal), and it can be said that an excellent balance is achieved with regard to electrical stability.
[0028] The press-fit pin 10 according to the present invention is characterized in that each plating film (first to fourth layers) is uniform (without cracks, pinholes, unevenness, etc.) and the thickness of each plating film can be accurately controlled by controlling the manufacturing conditions. This characteristic makes it possible to realize a press-fit pin 10 that is high in hardness, has excellent abrasion resistance, corrosion resistance, and also has excellent electrical properties. Furthermore, even if the material of the base body in the present invention is a material other than the copper alloy and the type of plating layer is different (in other words, even if the press-fit pin is composed of a plating layer other than Ni and Sn), it is possible to realize a press-fit pin that is excellent in abrasion resistance, corrosion resistance, and also has excellent electrical properties by controlling the manufacturing conditions.
[0029] <Press-fit pin change example> The press-fit pin according to the present invention is not limited to the above-described embodiments, and may include any of a base body, a Ni plating layer, a Ni-Sn diffusion layer, a Sn plating layer, a SnO coating layer, etc. The configuration and heat treatment conditions can be appropriately changed as necessary without departing from the spirit of the present invention. [Industrial Applicability]
[0030] The press-fit pin of the present invention has the excellent effects as described above, and can therefore be suitably used as a press-fit pin, which is one form of press-fit terminal that has a high holding force for IC boards, etc., even without soldering, by giving the insertion portion a spring property. [Explanation of symbols]
[0031] 10··Press-fit pin 20 Base body 30 Ni plating layer 40 Ni-Sn diffusion layer 50··Sn plating layer 60...SnO coating layer
Claims
[Claim 1] A method for manufacturing a press-fit pin, comprising the steps of: performing a second plating process on a base body of the press-fit pin to form a plating layer; and then performing a predetermined heat treatment on the base body. plating a Ni layer on a base body of the press-fit pin; plating a Sn layer on the Ni layer; The method includes a step of performing a heat treatment in an oxygen-containing atmosphere at a coating temperature of 232°C to 350°C, The method for producing a press-fit pin, wherein the Sn layer has a thickness of 0.03 μm to 5 μm after the heat treatment.
Citation Information
Patent Citations
Sn-PLATED COPPER SUBSTRATE, METHOD FOR MANUFACTURING Sn-PLATED COPPER SUBSTRATE, LEAD FRAME USING THE SAME, AND CONNECTOR TERMINAL
JP2009144210A
Surface treatment plated material and production method of the same, and electronic component
JP2014139345A
Press-fit terminal
JP2017021935A