Manufacturing method of molded body

The method addresses the limitations of conventional molded body manufacturing by using a mold with a heating element and suppressors to control electromagnetic fields, enabling the production of molded articles from diverse materials with high melting points and preventing thermal issues, ensuring high accuracy and reduced cooling times.

JP7584133B2Active Publication Date: 2024-11-15MICRO AMS INC
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2021012024
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-28
Publication Date
2024-11-15
Estimated Expiration
2041-01-28

AI Technical Summary

Technical Problem

Conventional molded body manufacturing methods are limited to a narrow range of raw materials and struggle with the use of materials that require high molding temperatures or have self-heating properties, leading to issues like thermal runaway and sparking.

Method used

The method employs a mold with a heating element outside the cavity that generates heat through electromagnetic waves or alternating electric fields, using a transmission amount suppressor to control electromagnetic wave or electric field penetration, allowing for the use of various raw materials, including thermoplastic resins, thermosetting resins, low melting point metals, and nonmetals, by incorporating dielectricity-imparting substances like silicone rubber and fluororubber, and permeation amount suppressors made of metals and nonmetals to prevent thermal runaway.

Benefits of technology

This approach enables the production of molded articles using a wide variety of raw materials, including those with high melting points, while preventing thermal runaway and sparking, ensuring high dimensional accuracy and reducing cooling time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007584133000002
    Figure 0007584133000002
  • Figure 0007584133000003
    Figure 0007584133000003
  • Figure 0007584133000004
    Figure 0007584133000004
Patent Text Reader

Abstract

To provide a method for manufacturing a molded article that has a wide range of applicable raw material types.SOLUTION: A method for manufacturing a molded article irradiates at least a part of a mold with electromagnetic waves after introducing a raw material into a cavity 10 of the mold, or disposes at least a part of the mold in an alternating electric field, to mold the molded article in the cavity. The mold has, outside the cavity, a heating element 20c that generates heat by absorbing the electromagnetic waves or generates heat by being disposed in the alternating electric field. At least a part between the heating element and the cavity has a penetration-amount suppressing element which suppresses a penetration amount of the electromagnetic waves or alternating electric field into the cavity, or at least a part of the cavity is made of the penetration-amount suppressing element. The heating element generates heat, and the heat conducts to the raw material, which causes molding.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a molded article. [Background technology]

[0002] As a method for producing a molded body, for example, the method described in Patent Document 1 has been proposed. Patent Document 1 describes a molding method using an electromagnetic wave irradiation molding device, which is provided with a mold made of an insulating material and an electromagnetic wave irradiation means for irradiating specific electromagnetic waves including a wavelength range of 0.01 to 100 m, the mold being divided into a plurality of mold parts, a cavity for filling a thermoplastic resin to mold a molded product being formed between the mold parts, and a surface layer having a performance of absorbing the specific electromagnetic waves being formed on at least a part of the inner wall surface of the cavity, the electromagnetic wave irradiation molding method comprising a disposing step of disposing a thermoplastic resin in the cavity, a heating step of irradiating the thermoplastic resin disposed in the cavity with specific electromagnetic waves including a wavelength range of 0.01 to 100 m from the electromagnetic wave irradiation means through the mold, and a cooling step of cooling the thermoplastic resin to obtain a molded product (see claims 1 and 5). It is also described that in such a method, the thermoplastic resin generates heat by itself, the entire thermoplastic resin is heated more effectively, and the entire thermoplastic resin can be melted in a short time, so that molded products with large variations in thickness in each part and molded products with complex shapes can be stably molded with excellent appearance and dimensional accuracy (see paragraphs 0007 and 0008). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2012 / 173053 Summary of the Invention [Problem to be solved by the invention]

[0004] Conventional methods for producing a molded body tend to be limited to a narrow range of applicable raw materials. However, it is preferable that the method for producing a molded body is applicable to various types of raw materials.

[0005] An object of the present invention is to solve the above-mentioned problems, that is, to provide a method for producing a molded body that can be applied to a wide range of raw materials. [Means for solving the problem]

[0006] In order to solve the above problems, the present inventors have conducted extensive research and completed the present invention. The present invention relates to the following (1) to (10). (1) A method for producing a molded body, comprising: placing a raw material in a cavity of a mold; irradiating at least a part of the mold with electromagnetic waves; or placing at least a part of the mold in an alternating electric field; and molding the molded body in the cavity, The mold is A heating element that absorbs the electromagnetic waves to generate heat or generates heat when placed in an alternating electric field is provided outside the cavity, a transmission suppressor that suppresses the transmission of the electromagnetic wave or the alternating electric field into the cavity is provided at least partially between the heating element and the cavity, or at least a portion of the cavity is made of the transmission suppressor; The heating element generates heat, and the heat is conducted to the raw material to perform molding. A method for producing a molded body. (2) The method for producing a molded body according to (1) above, wherein the heating element covers the entire cavity. (3) The method for producing a molded article according to (1) or (2) above, wherein the transmission suppressor blocks the transmission of the electromagnetic wave or the alternating electric field into the cavity. (4) the cavity is made of the transmission suppressor, the heating element is a mold into which the cavity fits; At least a portion of the outer surface of the cavity is in contact with the inner surface of the heating element. A method for producing the molded article according to any one of the above (1) to (3). (5) The method for producing a molded body according to any one of (1) to (4) above, wherein the raw material is mainly composed of at least one selected from the group consisting of a thermoplastic resin, a thermosetting resin, a low-melting point metal, and a low-melting point nonmetal. (6) The method for producing a molded article according to any one of the above (1) to (5), wherein the raw material contains a fibrous material and / or a filler. (7) The method for producing a molded product according to any one of the above (1) to (6), wherein the heating element contains silicone rubber and / or fluororubber, and further contains 5 to 90 volume % of at least one selected from the group consisting of silicon carbide, ferrite, barium titanate, carbon black and graphite as a dielectric imparting substance. (8) The method for producing a molded article according to any one of the above (1) to (7), wherein the permeation amount suppressor contains a metal and / or a non-metal. (9) The method for producing a molded body according to the above (8), wherein the metal and / or the nonmetal is at least one selected from the group consisting of aluminum, iron, copper, an alloy containing these, and shielding glass. (10) The method for producing a molded article according to any one of (1) to (9) above, wherein the electromagnetic waves have a wavelength region within a range of 0.78 μm to 100 m. Effect of the Invention

[0007] According to the present invention, a method for producing a molded article that can be applied to a wide range of raw materials can be provided. [Brief description of the drawings]

[0008] [Figure 1] FIG. 2 is a schematic cross-sectional view illustrating a preferred embodiment of a cavity. [Diagram 2] FIG. 11 is a schematic cross-sectional view showing a molding die in which a permeation suppressor is present between a heating element and a cavity. [Diagram 3] 10 is a schematic cross-sectional view showing a molding die in which a permeation suppressor is present between the heating element and the cavity so as to cover the entire cavity. FIG. [Figure 4] 10 is a schematic cross-sectional view showing a molding die in which a heating element covers a cavity formed of a permeation suppressor. FIG. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing a case where the molding die described with reference to FIG. 4 is irradiated with electromagnetic waves. [Figure 6] 5 is a schematic cross-sectional view showing the case where the molding die described with reference to FIG. 4 is placed in an alternating electric field. [Figure 7] FIG. 2 is a schematic perspective view of a cavity used in the examples. [Figure 8] FIG. 2 is a schematic cross-sectional view of a cavity used in the examples. [Figure 9] 1 is a photograph showing the appearance of a cavity used in an example. [Figure 10] FIG. 2 is a schematic cross-sectional view showing a state in which raw material is placed in a cavity used in the examples. [Figure 11] This is a photograph of the appearance of a rubber mold. [Figure 12] FIG. 2 is a schematic cross-sectional view showing a state in which a cavity is fitted into a rubber mold. [Figure 13] 1 is a photograph showing the appearance of the cavity fitted into the center of the rubber mold. [Figure 14] FIG. 2 is a schematic perspective view of another molding die used in the examples. [Figure 15] FIG. 2 is a schematic cross-sectional view of another mold used in the examples. [Figure 16] FIG. 2 is a schematic cross-sectional view of a permeation suppressor. [Figure 17] 1 is a photograph showing that a permeation suppressor is fitted into the center of a heating element, and a cavity is formed inside the permeation suppressor. [Figure 18] 1 is a photograph of a molded body obtained in an example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] The present invention will now be described. The present invention is a method for producing a molded body, which involves placing a raw material into a cavity of a mold, irradiating at least a part of the mold with electromagnetic waves, or placing at least a part of the mold in an alternating electric field, and molding a molded body within the cavity, wherein the mold has a heating element outside the cavity that absorbs the electromagnetic waves and generates heat, or generates heat by being placed in the alternating electric field, and at least a part between the heating element and the cavity has a transmission amount suppressor that suppresses the amount of transmission of the electromagnetic waves or the alternating electric field into the cavity, or at least a part of the cavity is made of the transmission amount suppressor, and the heating element generates heat, which is conducted to the raw material to perform molding. Such a method for producing a molded article is hereinafter also referred to as the "production method of the present invention."

[0010] <Mold> The mold used in the production method of the present invention will now be described.

[0011] <Heater> The mold in the manufacturing method of the present invention has a heating element. The heating element may be one that generates heat by absorbing electromagnetic waves as described below, or one that generates heat when placed in an alternating electric field as described below.

[0012] The heating element is preferably made of rubber, resin, or ceramics to which a dielectric material has been added, and may be, for example, a fired ceramic material to which a dielectric material has been added.

[0013] The heating element is preferably made of silicone rubber and / or fluororubber containing a dielectric material.

[0014] The dielectric property imparting substance is a substance capable of imparting dielectric property, and is preferably a substance having a dielectric power factor (dielectric loss tangent, tan δ) of 0.01 or more.

[0015] The dielectric material is preferably at least one selected from the group consisting of silicon carbide, ferrite, barium titanate, carbon black and graphite.

[0016] The content of the dielectric property imparting substance in the heating element is preferably 5 to 90% by volume. It is also preferable that the heating element contains silicone rubber and / or fluororubber, and further contains 5 to 90 volume % of at least one selected from the group consisting of silicon carbide, ferrite, barium titanate, carbon black and graphite as a dielectric material. The content of the dielectric material in the heating element is more preferably 10 to 70% by volume, more preferably 13 to 50% by volume, and even more preferably 15 to 35% by volume. When the content of the dielectric material in the heating element is within such a range, the heating element is more likely to generate heat by absorbing electromagnetic waves as described below, or is more likely to generate heat by being placed in an alternating electric field as described below. In addition, the heating element is less likely to generate heat locally. In addition, sparks (for example, a discharge phenomenon) tend to be less likely to occur when the raw material is heated. In addition, the heating element is more likely to exhibit the required strength.

[0017] If the dielectric material is a powder, its average particle diameter (D 50 ) is preferably 3 to 800 μm, more preferably 4 to 500 μm, more preferably 5 to 300 μm, more preferably 6 to 100 μm, and even more preferably 7 to 50 μm. When the average particle size of the powdered dielectric property imparting substance is within such a range, it becomes easier to absorb electromagnetic waves and generate heat, as described later, or becomes easier to generate heat when placed in an alternating electric field, as described later. Also, the heating element becomes easier to exhibit the required strength. This average particle size is calculated from the particle size distribution based on weight obtained by sieving. 50 This means:

[0018] The mold has such a heating element outside the cavity.

[0019] <Cavity> The mold in the manufacturing method of the present invention has a cavity. The cavity is the part of the mold into which the raw material is poured, and in principle, a molded product having the same shape as the internal space of the cavity is obtained.

[0020] The structure of the cavity will be described with reference to the drawings. Fig. 1 is a schematic cross-sectional view of a cavity in a preferred embodiment. The cavity in the manufacturing method of the present invention is not limited to the embodiment shown in Fig. 1.

[0021] As shown in Fig. 1, the cavity 10 may be divided into a plurality of parts (two in Fig. 1) and may be constituted by a combination of a first mold part 11 and a second mold part 12. In the case of the embodiment shown in Fig. 1, an internal space 15 for filling a raw material is formed between the pair of the first mold part 11 and the second mold part 12. The internal space 15 in the cavity can be formed, for example, by transferring a master model of the molded body to be molded.

[0022] The first mold part 11 or the second mold part 12 may have a vacuum hole to which a vacuum pump is connected for making the pressure inside the internal space 15 lower than atmospheric pressure (for example, a vacuum state).

[0023] 1, the first mold part 11 and the second mold part 12 are configured to be slidable relative to each other. When they slide toward each other, the volume of the internal space 15 decreases. Here, it is preferable that the second mold part 12 has a guide part 121 for allowing the first mold part 11 and the second mold part 12 to slide relatively to each other. When the first mold part 11 and the second mold part 12 approach each other, the volume of the internal space 15 decreases, and the raw material in the internal space 15 is pressed against the inner wall of the internal space 15.

[0024] In the embodiment shown in Figure 1, the internal space 15 is a space surrounded by the inner surfaces of the first mold portion 11 and the second mold portion that constitute the cavity, but in the manufacturing method of the present invention, the internal space 15 may be a space at least partially surrounded by the inner surface of the member that constitutes the cavity, and may be, for example, a space surrounded by the inner surface of the part that constitutes the cavity and the inner surface of the permeation amount suppressor.

[0025] <Permeation amount suppressor> The molding die in the manufacturing method of the present invention has a permeation suppressor at least partially between the heating element and the cavity as described above, or at least a portion of the cavity is made of the permeation suppressor.

[0026] The transmission suppressor may be made of a material capable of suppressing the transmission of the electromagnetic wave or alternating electric field into the cavity. Specifically, the material may be capable of suppressing the transmission of the electromagnetic wave or alternating electric field into the cavity to such an extent that the raw material in the cavity does not spark or go into thermal runaway. Thermal runaway refers to a phenomenon in which the temperature rises in a short period of time, making it difficult to control the temperature. The transmission suppressor is preferably made of a material capable of blocking the transmission of electromagnetic waves or alternating electric fields into the interior of the cavity.

[0027] The permeation inhibitor preferably comprises a metal and / or a non-metal. The metal and / or nonmetal content in the permeation suppressor is preferably 50% by mass or more, more preferably 65% ​​by mass or more, more preferably 80% by mass or more, even more preferably 95% by mass or more, and even more preferably substantially 100%. Here, "substantially" means that only unavoidable impurities that may be mixed in from raw materials or the manufacturing process are permitted to be included. Specifically, among metals, at least one selected from the group consisting of aluminum, iron, copper, and alloys containing these is preferable. The alloy containing aluminum, iron, and copper may be any alloy containing at least one of aluminum, iron, and copper, and an example of this is brass (copper-zinc alloy). Among non-metallic materials, shielding glass is preferable. These can suppress or block the amount of electromagnetic waves or alternating electric fields penetrating into the cavity.

[0028] <Mold structure> A case in which the molding die has a permeation suppressor at least partially between the heating element and the cavity as described above will be described with reference to Figs. 2 and 3. Figs. Fig. 2 is a schematic cross-sectional view showing molding die 1a in which permeation amount suppressor 30a is present between heating element 20a and cavity 10. Fig. 3 is a schematic cross-sectional view showing molding die 1b in which permeation amount suppressor 30b is present between heating element 20b and cavity 10 so as to cover the entire cavity 10. The embodiments shown in Figs. 2 and 3 are preferred examples, and the mold in the manufacturing method of the present invention is not limited to these.

[0029] In the molding die 1a shown in Fig. 2, the heating element 20a is present outside the cavity 10, and the permeation amount suppressor 30a is present therebetween. When at least a portion of this molding die 1a (a portion including at least a portion of the heating element 20a) is irradiated with electromagnetic waves, or when at least a portion of the molding die 1a (a portion including at least a portion of the heating element 20a) is placed in an alternating electric field, the heating element 20a generates heat. Even when only at least a portion of the heating element 20a in the molding die 1a is irradiated with electromagnetic waves, or when only at least a portion of the heating element 20a in the molding die 1a is placed in an alternating electric field, the heating element 20a generates heat. The heat is then conducted to the raw material present in the internal space 15 of the cavity 10 via the permeation suppressor 30a etc., and the heat melts or hardens the raw material, thereby forming the mold. Since the permeation suppressor 30a exists between the heating element 20a and the cavity 10, the amount of transmission of the electromagnetic wave or alternating electric field from the heating element 20a to the cavity 10 into the cavity 10 is suppressed or blocked.

[0030] In the molding die 1b shown in FIG. 3, the heating element 20b is present outside the cavity 10, and the permeation amount suppressor 30b is present between them. In the embodiment shown in FIG. 3, the permeation amount suppressor 30b covers the entire cavity 10, and the heating element 20b covers the entire permeation amount suppressor 30b (this is also true on the front and back sides in FIG. 3). That is, the heating element 20b covers the entire cavity 10. Here, the permeation amount suppressor 30b may be a mold into which the cavity 10 fits. The permeation amount suppressor 30b may be made of a plate (e.g., a mesh plate) or the like. The heating element 20b may be a mold into which the permeation amount suppressor 30b fits. When at least a part of such forming die 1b is irradiated with electromagnetic waves, or when at least a part of forming die 1b is placed in an alternating electric field, heating element 20b generates heat. The heat is then conducted to the raw material present in internal space 15 of cavity 10 via permeation suppressor 30b and the like, and the raw material is melted or hardened by the heat, thereby forming the material. Since permeation suppressor 30b is present between heating element 20b and cavity 10, the amount of transmission of the electromagnetic waves or alternating electric field into internal space 15 of cavity 10 is suppressed or blocked.

[0031] In the embodiment shown in Figures 2 and 3, the molding die (1a, 1b) may further have another portion between the cavity 10 and the permeation suppressor (30a, 30b), or between the permeation suppressor (30a, 30b) and the heating element (20a, 20b).

[0032] 2 or 3, the material of cavity 10 may be any material that does not soften under conditions in which the raw material in internal space 15 melts or hardens. For example, it may be a hardening resin material (thermosetting resin material, photosetting resin material, etc.), a cement material, a gypsum material, various heat-resistant nonmetallic materials, etc., and is preferably made of a rubber material. As the rubber material, various rubbers such as silicone rubber and fluororubber can be used.

[0033] When the mold having the embodiment shown in FIG. 2 or FIG. 3 is used as the mold, the following embodiment of the manufacturing method of the present invention can be carried out. That is, A method for producing a molded body, comprising: placing a raw material in a cavity of a mold; irradiating at least a part of the mold with electromagnetic waves; or placing at least a part of the mold in an alternating electric field; and molding the molded body in the cavity, the method comprising the steps of: The mold is A heating element that absorbs the electromagnetic waves to generate heat or generates heat when placed in an alternating electric field is provided outside the cavity, A transmission suppressor that suppresses (preferably blocks) the amount of transmission of the electromagnetic wave or the alternating electric field into the cavity is provided at least partially between the heating element and the cavity, a method for producing a molded body, the heating element generating heat, and the heat being conducted to the raw material to perform molding; can be implemented.

[0034] Next, a case in which at least a portion of the cavity in the casting mold is made of a permeation suppressor will be described with reference to FIG. FIG. 4 is a schematic cross-sectional view showing a molding die 1c in which a heating element 20c covers a cavity 10 made of a permeation suppressor. 4 is a preferred embodiment, and the mold in the manufacturing method of the present invention is not limited to this embodiment. For example, only a part of the cavity may be made of the permeation suppressor.

[0035] In the casting mold 1c shown in Fig. 4, the cavity 10 is made of a permeation suppressor. In the embodiment shown in Fig. 4, the heating element 20c covers the entire cavity 10. In the preferred embodiment shown in Fig. 4, the heating element 20c is a mold into which the cavity 10 fits. Specifically, the heating element 20c shown in Fig. 4 has one mold part 201c and the other mold part 202c, which are configured to be slidable relative to each other. When the one mold part 201c and the other mold part 202c slide toward each other, the first mold part 11 and the second mold part 12 in the cavity 10 inside them approach each other. Here, at least a part of the outer surface of the cavity 10 (in principle, the entire outer surface) is in contact with the inner surface of the heating element 20c.

[0036] 4, the other mold part 202c has a vacuum hole 25 to which a vacuum pump is connected for making the inside of the heating element 20c lower than atmospheric pressure (for example, a vacuum state). When the inside of the heating element 20c is made lower than atmospheric pressure (for example, a vacuum state), the one mold part 201c and the other mold part 202c approach each other, and the first mold part 11 and the second mold part 12 in the cavity 10 therein approach each other.

[0037] When at least a part of forming die 1c as shown in Fig. 4 is irradiated with electromagnetic waves or when at least a part of forming die 1c is placed in an alternating electric field, heating element 20c generates heat. Even when only a part of the heating element in forming die 1c is irradiated with electromagnetic waves or when only a part of the heating element in forming die 1c is placed in an alternating electric field, heating element 20c generates heat. It is preferable to irradiate the entire outer surface of the heating element in the forming mold 1c with electromagnetic waves. The heat is then conducted to the raw material present in the internal space 15 of the cavity 10 made of the permeation suppressor, and the raw material is melted or hardened by the heat, thereby forming the mold. Here, since the cavity 10 is made of the permeation suppressor, the amount of transmission of the electromagnetic wave or alternating electric field into the internal space 15 of the cavity 10 is suppressed or blocked.

[0038] In the embodiment shown in FIG. 4, the molding die 1c may further have another portion between the cavity 10 and the heating element 20c.

[0039] When at least a portion of the cavity in the casting mold is made of the permeation suppressor, the heating element only needs to be present outside the cavity, and does not have to cover the entire cavity as shown in Fig. 4. Furthermore, the heating element does not have to be a mold into which the cavity fits.

[0040] When the cavity is made of a permeation inhibitor as shown in FIG. 4 and the permeation inhibitor contains a substance with a high melting point such as a metal and / or a non-metal (preferably 50% by mass or more, more preferably 65% ​​by mass or more, more preferably 80% by mass or more, more preferably 95% by mass or more, and even more preferably essentially 100%), the manufacturing method of the present invention can be carried out using raw materials that need to be treated at higher temperatures. Conventionally, when a cavity made of, for example, silicone rubber or fluororubber, or a mixture of silicone rubber or fluororubber with an added dielectric material (silicon carbide, ferrite, barium titanate, carbon black, graphite, etc.) is used, the cavity may soften when it becomes hot (for example, about 250°C or higher). In such cases, it has been difficult to manufacture a molded product using a raw material with a high melting point (for example, a raw material with a melting point of about 250°C or higher). This is because the cavity softens at the temperature at which the raw material melts or hardens. Examples of raw materials with high molding temperatures include PA66, PET, and PBT. In contrast, in the manufacturing method of the present invention, when the transmittance suppressor constituting the cavity contains a substance with a high melting point, such as at least one metal and / or nonmetal selected from the group consisting of aluminum, iron, copper, alloys containing these, and shielding glass (preferably containing 50 mass% or more, more preferably containing 65 mass% or more, more preferably containing 80 mass% or more, more preferably containing 95 mass% or more, and even more preferably containing substantially 100%), a molded body can be manufactured using a raw material with a high molding temperature.

[0041] 4, and when a portion of cavity 10 is made of a permeation suppressor, the material of the remaining portion of cavity 10 may be any material that does not soften under conditions in which the raw material in internal space 15 melts or hardens. For example, the material may be a curable resin material (thermosetting resin material, photocurable resin material, etc.), a cement material, a gypsum material, various heat-resistant nonmetallic materials, etc., and is preferably made of a rubber material. As the rubber material, various rubbers such as silicone rubber and fluororubber can be used.

[0042] When the mold having the above-mentioned embodiment shown in FIG. 4 is used as the mold, the following embodiment of the manufacturing method of the present invention can be carried out. That is, A method for producing a molded body, comprising: placing a raw material in a cavity of a mold; irradiating at least a part of the mold with electromagnetic waves; or placing at least a part of the mold in an alternating electric field; and molding the molded body in the cavity, the method comprising the steps of: The mold is A heating element that absorbs the electromagnetic waves to generate heat or generates heat when placed in an alternating electric field is provided outside the cavity, At least a part of the cavity is made of a transmission suppressor that suppresses (preferably blocks) the transmission amount of the electromagnetic wave or the alternating electric field into the cavity, a method for producing a molded body, the heating element generating heat, and the heat being conducted to the raw material to perform molding; can be implemented. In this embodiment, it is preferable that the heating element covers the entire cavity.

[0043] <Manufacturing method> In the manufacturing method of the present invention, first, raw material is placed in the cavity of the above-mentioned mold.

[0044] The raw material is not particularly limited as long as it is mainly composed of a substance that melts or hardens due to heat generated by the heating element and transmitted to the cavity via the transmission suppressor or the like.

[0045] The raw material is preferably composed mainly of at least one selected from the group consisting of thermoplastic resins, thermosetting resins, low-melting-point metals, and low-melting-point nonmetals.

[0046] Here, "main component" means a content of 50% by mass or more. This content is preferably 65% ​​by mass or more, more preferably 80% by mass or more, even more preferably 95% by mass or more, and even more preferably substantially 100%. Note that "substantially" means that only unavoidable impurities that may be mixed in from raw materials or the manufacturing process are permitted to be included. Unless otherwise specified, the "main component" in the production method of the present invention has the above meaning.

[0047] Examples of thermoplastic resins that can be used as raw materials include rubber-reinforced styrene-based resins such as ABS resin (acrylonitrile-butadiene-styrene resin), ASA resin (acrylate-styrene-acrylonitrile resin), and AES resin (acrylonitrile-ethylene-propylene-diene-styrene resin); styrene-based resins such as polystyrene, styrene-acrylonitrile copolymer, styrene-maleic anhydride copolymer, and (meth)acrylic acid ester-styrene copolymer; olefin-based resins such as polyethylene and polypropylene; acrylic resins; polycarbonate resin; and PBT resin (polybutylene terephthalate). Examples of the resin include polyester-based resins such as polyamide-based resins such as metaxylylenediamine polyamide resin, vinyl chloride-based resins, polyarylate resins, polyacetal resins, polyphenylene ether resins, PPS resin (polyphenylene sulfide resin), fluororesins, imide-based resins, ketone-based resins such as PEEK resin (polyether ether ketone resin), sulfone-based resins, urethane-based resins, polyvinyl acetate, polyethylene oxide, polyvinyl alcohol, polyvinyl ether, polyvinyl butyral, phenoxy resins, photosensitive resins, liquid crystal polymers, biodegradable plastics, and soft resins (elastomer resins). The thermoplastic resin may be a thermoplastic elastomer (styrene-based, olefin-based, vinyl chloride-based, vinyl acetate-based, urethane-based, polyester-based, etc.).

[0048] When a thermoplastic resin is used as a raw material, the raw material melts in the cavity due to the heat generated by the heating element. In addition, since the amount of electromagnetic waves or alternating electric fields penetrating into the internal space of the cavity is suppressed or blocked, self-heating does not occur in principle. Conventionally, when a raw material with strong self-heating behavior such as nylon-based resin is used, there are cases where the self-heating leads to thermal runaway. In the manufacturing method of the present invention, since the raw material does not self-heat in principle, a molded body can be manufactured using nylon-based resin as a raw material.

[0049] When a thermoplastic resin is used as a raw material, the thermoplastic resin may be in the form of particles or flakes. In this case, the average particle size is preferably 0.2 to 5 mm, more preferably 0.5 to 3 mm. The average particle size is determined by the D 50 This means:

[0050] A preform made of a thermoplastic resin can be used as the raw material. The preform is formed into a three-dimensional shape by some method using a thermoplastic resin, for example, a preform laminated into a three-dimensional shape by an additive manufacturing method. The additive manufacturing method here includes a method using various 3D printers (AM: Additive Manufacturing) that laminate thermoplastic resin extruded from a nozzle in a thread-like (linear) or granular form into a three-dimensional shape, a fused deposition modeling method (FDM: Fused Deposition Modeling), an extrusion molding method, an inkjet method, a granular material bonding method, etc.

[0051] Examples of thermosetting resins that can be used as raw materials include phenolic resins, epoxy resins, melamine resins, urea resins, unsaturated polyester resins, alkyd resins, polyurethanes, and thermosetting polyimides. When a thermosetting resin is used as the raw material, the raw material is cured by the heat generated by the heating element in the manufacturing method of the present invention to form a molded product.

[0052] Examples of low melting point metals that can be used as the raw material include alloys containing zinc, indium, gallium, tin, bismuth, lead, or the like as a main component. When a low-melting point metal is used as the raw material, the raw material is melted by the heat generated by the heating element in the production method of the present invention.

[0053] An example of a low-melting nonmetal that can be used as a raw material is glass. When a low-melting-point nonmetal is used as the raw material, the raw material is melted by the heat generated by the heating element in the production method of the present invention.

[0054] The raw material is mainly composed of a substance that melts or hardens by heat generated by a heating element and transmitted into the cavity via a transmission inhibitor or the like, such as at least one selected from the group consisting of thermoplastic resins, thermosetting resins, low-melting point metals, and low-melting point non-metals, and may contain other components such as high-melting point metals, high-melting point non-metals (ceramics, etc.), UV-curable resins, fibrous materials (CF (carbon fiber), GF (glass fiber), metal fibers (SUS fibers, etc.), glass fibers, etc.), softeners (plasticizers, oils, etc.), colorants (pigments, etc.), impact resistance modifiers (rubber components, etc.), antistatic agents, conductive materials, fillers (thermally conductive fillers, metallic fillers, etc.), flame retardants, heat-resistant resins, low heat storage resins, and sliding improvers.

[0055] Conventionally, when the raw material contains a fiber material or a filler such as CF or SUS fiber, sparks may occur starting from the fiber material when at least a part of the mold is irradiated with electromagnetic waves or when at least a part of the mold is placed in an alternating electric field. In contrast, in the manufacturing method of the present invention, sparks are unlikely to occur even when the raw material contains a fiber material or a filler.

[0056] In the manufacturing method of the present invention, after the above-mentioned raw material is placed in the cavity of the mold, at least a part of the mold is irradiated with electromagnetic waves or at least a part of the mold is placed in an alternating electric field.

[0057] <Electromagnetic radiation> When the above-mentioned raw material is placed in the cavity of the mold, and then at least a part of the mold is irradiated with electromagnetic waves, the method is not particularly limited. It is sufficient that the electromagnetic waves can be irradiated with electromagnetic waves that can heat the heating element of the mold. The electromagnetic waves may be irradiated to at least the whole or part of the surface of the heating element.

[0058] The case where electromagnetic waves are irradiated onto the forming die will be described with reference to Fig. 5. Fig. 5 is a schematic cross-sectional view illustrating the case where electromagnetic waves are irradiated onto the forming die 1c described with reference to Fig. 4. In FIG. 5, raw material is placed in an internal space 15 present between a pair of a first mold part 11 and a second mold part 12 in the cavity 10. In addition, the vacuum hole 25 formed in the other mold portion 202c is connected to a vacuum pump 40, and by driving the vacuum pump 40, the pressure inside the heating element 20c can be made lower than atmospheric pressure (e.g., a vacuum state). Then, electromagnetic waves can be generated from electromagnetic wave generator 42 and irradiated onto forming die 1c.

[0059] It is preferable that the electromagnetic wave generator 42 is capable of generating electromagnetic waves having a wavelength range of 0.78 μm to 100 m. In other words, it is preferable that the wavelength range of the generated electromagnetic waves is within the range of 0.78 μm to 100 m. Furthermore, it is preferable that the electromagnetic wave generator 42 be capable of generating electromagnetic waves (near-infrared rays) including a wavelength range of 0.78 to 2 μm, electromagnetic waves (microwaves) including a wavelength range of 0.01 to 1 m, or electromagnetic waves (high frequency) including a wavelength range of 1 to 100 m. When generating near infrared radiation, the electromagnetic wave generator 42 may be a halogen lamp. When generating microwaves, the electromagnetic wave generator 42 may be a microwave oscillator. When generating high frequency waves, the electromagnetic wave generator 42 may be a high frequency oscillator.

[0060] <Placed in an alternating electric field> When placing at least a part of the mold in an alternating electric field after putting the above-mentioned raw material into the cavity of the mold, the method is not particularly limited. It is sufficient that the heating element of the mold can be made to generate heat by placing the mold in the alternating electric field. At least the whole or part of the heating element may be placed in the alternating electric field.

[0061] A case where the forming die is placed in an alternating electric field will be described with reference to Fig. 6. Fig. 6 is a schematic cross-sectional view illustrating a case where forming die 1c described with reference to Fig. 4 is placed in an alternating electric field. In FIG. 6, an internal space 15 existing between a pair of first and second mold parts 11 and 12 in a molding die 1c is filled with raw material. In addition, the vacuum hole 25 formed in the other mold portion 202c is connected to a vacuum pump 40, and by driving the vacuum pump 40, the pressure inside the heating element 20c can be made lower than atmospheric pressure (e.g., a vacuum state). Then, using dielectric heater 44, an alternating electric field can be applied to forming mold 1c by applying a high-frequency AC voltage to a pair of electrodes 441, 442. The frequency of the AC voltage from dielectric heater 44 is preferably a high-frequency electromagnetic wave having a wavelength range of 1 m to 100 m.

[0062] The production method of the present invention is applicable to a wide range of raw materials. In addition, conventionally known pellets can be used as raw materials, the dimensional accuracy of the molded body is higher than in the past, and the cooling time can be shorter than in the past. EXAMPLES

[0063] An embodiment of the present invention will be described below, but the present invention is not limited to the embodiment described below.

[0064] <Example 1> First, a mold was prepared. The mold had a cavity made of a permeation suppressor, and the cavity was fitted inside a rubber mold, which was a heating element, in the same manner as that shown in FIG.

[0065] The cavity in the mold was formed by processing an aluminum extrusion material (5052 material). FIG. 7 shows a schematic perspective view of the cavity, FIG. 8 shows a schematic cross-sectional view of the cavity, and FIG. 9 shows a photograph of the cavity's appearance. As shown in Fig. 7, cavity 50 has a structure formed by combining three parts: upper part 51, central part 52, and lower part 53. Moreover, a cross section of cavity 50 formed by fitting parts of upper part 51 and lower part 53 shown in Fig. 7 into central part 52 is as shown in Fig. 8. The dimensions of each part of cavity 50 are as shown in FIG. 8. That is, each of upper part 51, central part 52, and lower part 53 is approximately a square with a side of 30 mm when viewed from above. The thickness (maximum thickness) of upper part 51 and lower part 53 is 10 mm, and the thickness of the part that fits (enters) into central part 52 when upper part 51 and lower part 53 are fitted into central part 52 is 5 mm. The thickness of central part 52 (the length in the direction parallel to the thickness direction of upper part 51 and lower part 53) is 12 mm. Therefore, when upper part 51 and lower part 53 are fitted into central part 52, an approximately rectangular parallelepiped internal space 55 appears in central part 52, with a thickness of 2 mm and a base that is an approximately square with a side of 26 mm. 10, when raw material 57 is placed in internal space 55, raw material 57 is completely covered by upper portion 51, central portion 52, and lower portion 53. This blocks the transmission of electromagnetic waves and alternating electric fields into the cavity. Note that Figure 10 is a schematic cross-sectional view showing the state immediately after raw material 57 is placed in internal space 55. When raw material 57 is heated, the voids within raw material 57 decrease, and accordingly the distance between upper portion 51 and lower portion 52 decreases (i.e., upper portion 51 and lower portion 52 move closer to each other), and internal space 55 shrinks.

[0066] The rubber mold has a cavity fitted inside, as shown in the external photograph of Fig. 11. Fig. 11 also shows the same cavity as shown in Fig. 9 together with the rubber mold. Fig. 12 is a schematic cross-sectional view showing the state in which cavity 50 shown in Fig. 8 is fitted into rubber mold 59. Fig. 13 is an external photograph showing the state in which the cavity shown in Fig. 11 is fitted into the center of the rubber mold.

[0067] The rubber mold is made by mixing silicone with silicon carbide as a dielectric material, kneading it, hardening it, and then hollowing out the center so that the cavity can fit into it.

[0068] As described above, the molding die used in Example 1 is configured such that the rubber die acting as a heating element covers the entire cavity, the cavity fits inside the rubber die, and in principle, the entire outer surface of the cavity is in contact with the inner surface of the rubber die.

[0069] Here, two holes were formed in the rubber mold to connect the outside of the rubber mold with the cavity disposed inside it. An alumina sheath was inserted into one of the holes so that it was in contact with the outer surface of the internal cavity, and a fiber optic thermometer was inserted into the sheath to continuously measure the temperature of the outer surface of the cavity. The other hole is connected to a tube connected to a vacuum pump, and is configured so that the inside of the cavity can be reduced in pressure by driving the vacuum pump. This hole corresponds to the vacuum hole 25 shown in FIG.

[0070] Using the above-mentioned mold, the raw material was filled so as to fill the internal space within the cavity. Here, micropellets of Amilan CM1011G-30 (manufactured by Toray Industries, Inc.) which is a nylon resin, were used as the raw material. The particle size of the micropellets was about 0.8 to 1 mm.

[0071] The raw material was filled into the cavity, and the cavity was then closed. The cavity was then fitted inside a rubber mold, the rubber mold was then closed, and heat-resistant tape was applied to tightly seal the rubber mold so that it would not open.

[0072] After that, an optical fiber thermometer was inserted into the sheath tube to continuously measure the temperature of the outer surface of the cavity. A tube connected to a vacuum pump was connected to the other hole formed in the rubber mold.

[0073] The mold was then placed in a microwave molding device, and while a vacuum was being drawn with a vacuum pump so that the pressure inside the rubber mold was -95 kPa, the mold was irradiated with electromagnetic waves to perform molding.

[0074] The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1. The molding temperature and heating rate were adjusted while measuring with an optical fiber thermometer inserted in the sheath tube.

[0075] <Example 2> The raw material used was NS0031 (manufactured by SABIC Japan, LLC), a PC / ABS resin, which contains 15% by mass of SUS filler. Other than that, molding was carried out in the same manner as in Example 1. However, the molding temperature, heating rate, and holding time at the molding temperature during molding were changed according to the characteristics of the raw materials. The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1.

[0076] <Example 3> The raw material used was nylon resin PA6CF30 (manufactured by Toray Industries, Inc.), which contains 30% by mass of carbon fiber. Other than that, molding was carried out in the same manner as in Example 1. However, the molding temperature, heating rate, and holding time at the molding temperature during molding were changed according to the characteristics of the raw materials. The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1.

[0077] <Example 4> As a raw material, pellets of 1101G-30 (manufactured by Toray Industries, Inc.), which is a polyester resin (PBT resin), were used. The particle size of the pellets was about 0.8 to 1 mm. Other than that, molding was carried out in the same manner as in Example 1. However, the molding temperature, heating rate, and holding time at the molding temperature during molding were changed according to the characteristics of the raw materials. The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1.

[0078] <Example 5> The raw material used was metaxylylenediamine polyamide resin (MXD6 C-408 carbon long fiber grade). This raw material was in the form of pellets containing 40% by mass of carbon filler. Other than that, molding was carried out in the same manner as in Example 1. However, the molding temperature, heating rate, and holding time at the molding temperature during molding were changed according to the characteristics of the raw materials. The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1.

[0079] <Example 6> The raw material used was A630T-30V (manufactured by Toray Industries, Inc.), a carbon fiber reinforced PPS resin, containing 30% by mass of carbon fiber. Other than that, molding was carried out in the same manner as in Example 1. However, the molding temperature, heating rate, and holding time at the molding temperature during molding were changed according to the characteristics of the raw materials. The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1.

[0080] <Example 7> The raw material used was micropellets of VestaKeep 2000P (EVONIK Co., Ltd.), a PEEK resin (thermoplastic super engineering plastic). The particle size of the micropellets was about 0.8 to 1.0 mm. Other than that, molding was carried out in the same manner as in Example 1. However, the molding temperature, heating rate, and holding time at the molding temperature during molding were changed according to the characteristics of the raw materials. The molding temperature, heating rate, and holding time at the molding temperature during molding are shown in Table 1.

[0081] [Table 1]

[0082] In each of Examples 1 to 7, after molding was completed, the mold was removed from the microwave molding apparatus and cooled for 1 hour by blowing air on it using a fan while continuing to evacuate. As a result, molded bodies were obtained in all of Examples 1 to 7. Furthermore, no thermal runaway or sparks occurred due to self-heating of the raw materials during the production process.

[0083] In addition, in each of Examples 1 to 7, after molding was completed, the mold was removed from the microwave molding device, the vacuum was stopped, and only the cavity was removed from the rubber mold, and cooled by blowing air onto it using a fan. In this case, the mold was cooled after 5 minutes, and the molded body could be removed from the cavity. At this time, no problems such as deformation occurred in the molded body.

[0084] <Example 8> A molding die different from those used in Examples 1 to 7 was prepared. The molding die used in Example 8 has a rubber heating element on the outside of a rubber cavity, with a permeation inhibitor between them. The permeation inhibitor forms a mold into which the cavity can be in close contact, and can cover the entire cavity. The heating element forms a mold into which the permeation inhibitor fits, and can cover the entire permeation inhibitor. This mold is similar to the embodiment shown in FIG. 3, but differs from it in the structure of the cavity and the permeation suppressor.

[0085] The molding die used in Example 8 will be described with reference to Figures 14 to 17. Figure 14 is a schematic perspective view of the molding die used in Example 8, Figure 15 is a schematic cross-sectional view thereof, Figure 16 is a schematic cross-sectional view of the permeation suppressor, and Figure 17 is a photograph showing that the permeation suppressor is fitted into the center of the heating element and a cavity is formed inside the permeation suppressor.

[0086] As shown in Figs. 14 and 15, in the molding die 60 used in Example 8, the heating element 64 is made up of two sections, and the permeation suppressor 66 is fitted inside the heating element 64. Here, the heating element 64 is a rubber mold that is made by incorporating silicon carbide as a dielectric material into silicone, kneading and hardening it, and then hollowing out near the center so that the permeation suppressor 66 can be fitted inside. In principle, the entire outer surface of the permeation suppressor 66 is in contact with the inner surface of the rubber mold that serves as the heating element 64.

[0087] 14 to 16, the permeation amount suppressor 66 is composed of two parts, each of which has a rectangular main surface, and when they are fitted together, a space is created inside. The permeation amount suppressor 66 used in Example 8 was formed by processing an aluminum extrusion material (5052 material).

[0088] In the molded body 60 , the cavity 62 exists in intimate contact with the inside of the permeation suppressor 66 . In the cavity 62 of such a molding die 60 , a portion of the internal space 68 into which the raw material is placed is in contact with the inner surface of the permeation suppressor 66 .

[0089] Here, the cavity 62 was formed inside the permeation suppressor 66 using heat-resistant liquid rubber made of silicone rubber.

[0090] In Example 8, two holes were formed in the rubber mold serving as heating element 64 to connect the outside of the rubber mold with the outer surface of permeation amount suppressor 66 placed inside it, an alumina sheath tube was inserted into one of the holes and an optical fiber thermometer was inserted into the sheath tube to enable continuous measurement of the temperature of the outer surface of permeation amount suppressor 66, and the other hole was connected to a tube connected to a vacuum pump and the inside of cavity 62 could be reduced in pressure by driving the vacuum pump. This hole corresponds to vacuum hole 25 shown in FIG. 4.

[0091] Using the above-mentioned mold, the raw material was placed in the internal space of the cavity. The raw material used here was Kraft Alloy (manufactured by Nisshin Resin Co., Ltd.), a low melting point alloy with a melting point of 150° C. and containing mainly tin and bismuth.

[0092] 20.5 g of this raw material was filled into cavity 62, and the permeation amount suppressor 66 was then closed. The permeation amount suppressor 66 was then fitted inside a rubber mold serving as a heating element 64, the rubber mold was then closed, and heat-resistant tape was applied to tightly seal the rubber mold so that it would not open.

[0093] Thereafter, an optical fiber thermometer was inserted into the sheath tube so that the temperature of the outer surface of the permeation amount suppressor 66 could be continuously measured. In addition, a tube connected to a vacuum pump was attached to the other hole formed in the rubber mold.

[0094] The mold was then placed in a microwave molding device, and while a vacuum was being drawn with a vacuum pump so that the pressure inside the rubber mold was -95 kPa, the mold was irradiated with electromagnetic waves to perform molding. The molding temperature was 150°C, the heating rate was 10°C / min, and the holding time at the molding temperature was 60 seconds. The molding temperature and the heating rate were adjusted while measuring with an optical fiber thermometer inserted in the sheath tube.

[0095] After molding was completed, the mold was removed from the microwave molding apparatus and cooled for 1 hour by blowing air on it using a fan while continuing to evacuate. As a result, a green body was obtained as shown in Figure 18. No sparks were generated from the raw materials during the manufacturing process. [Explanation of symbols]

[0096] 1a, 1b, 1c mold 10 Cavity 11 1st mold section 12 Second mold section 121 Guide part 15. Interior Space 20a, 20b, 20c Heating elements 201c One side mold part 202c Other mold part 25 Vacuum hole 30a, 30b, permeation amount suppressor 40 Vacuum Pump 42 Electromagnetic Wave Generator 44 Dielectric Heater 441, 442 electrode 50 Cavity 51 Top 52 Central part 53 Lower 55 Interior Space 57 Raw materials 59 Rubber mold 60 mold 62 Cavity 64 Heating element 66 Permeation amount suppressor 68 Interior Space

Claims

1. A method for producing a molded body, comprising the steps of: placing a raw material into a cavity of a mold; maintaining a pressure inside the cavity lower than atmospheric pressure; irradiating at least a part of the mold with electromagnetic waves or placing at least a part of the mold in an alternating electric field; melting or hardening the raw material in the cavity to form a molded body; maintaining a pressure inside the cavity lower than atmospheric pressure until the molded body is cooled; and then removing the molded body from the cavity, The mold is A heating element that absorbs the electromagnetic waves to generate heat or generates heat when placed in an alternating electric field is provided outside the cavity, a transmission suppressor that suppresses the transmission of the electromagnetic wave or the alternating electric field into the cavity is provided at least partially between the heating element and the cavity, or at least a portion of the cavity is made of the transmission suppressor; the permeation amount suppressor is made of at least one metal selected from the group consisting of aluminum, iron, copper, and alloys containing these metals; The heating element generates heat, and the heat is conducted to the raw material to perform molding. A method for producing a molded body.

2. The method for producing a molded article according to claim 1 , wherein the heating element covers the entire cavity.

3. The method for producing a molded article according to claim 1 or 2, wherein the transmission suppressor blocks transmission of the electromagnetic wave or the alternating electric field into the cavity.

4. The cavity is made of the transmission suppressor, the heating element is a mold into which the cavity fits; At least a portion of the outer surface of the cavity is in contact with the inner surface of the heating element. A method for producing the molded article according to any one of claims 1 to 3.

5. The method for producing a molded product according to any one of claims 1 to 4, wherein the raw material is mainly composed of at least one selected from the group consisting of a thermoplastic resin, a thermosetting resin, a low-melting point metal, and a low-melting point nonmetal.

6. The method for producing a molded article according to any one of claims 1 to 5, wherein the raw material contains a fiber material and / or a filler.

7. the heating element contains silicone rubber and / or fluororubber, and further contains 5 to 90 volume % of at least one selected from the group consisting of silicon carbide, ferrite, barium titanate, carbon black, and graphite as a dielectric material; A method for producing the molded article according to any one of claims 1 to 6.

8. The method for producing a molded product according to any one of claims 1 to 7, wherein the wavelength region of the electromagnetic wave is within a range of 0.78 µm to 100 m.

Citation Information

Patent Citations

  • Method for manufacturing resin member, transfer mold, and transfer device

    JP2013119219A

  • A mold, a method for manufacturing a mold, and a method for manufacturing a plastic or composite material product using the mold.

    JP2013520335A

  • Resin block and its production method

    JP2018114723A

  • Curable composition for nanoimprint, and patterned substrate using the same

    JP2019192724A

  • Electromagnetic wave irradiation molding device and electromagnetic wave irradiation molding method

    WO2012173053A1