Alkyl Silicate

Alkyl silicates with specific structural units address the environmental stability issue of silicones by providing hydrolytic and thermal stability, enabling their use in various applications.

JP7584621B2Active Publication Date: 2024-11-15WACKER CHEMIE AG
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023504349
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-07-22
Publication Date
2024-11-15
Estimated Expiration
2040-07-22

AI Technical Summary

Technical Problem

Existing silicones are difficult to decompose in the environment due to Si-alkyl groups, limiting their practical applications, and there is a need for a material that can replace silicones with similar properties like glass transition temperature, surface tension, and hydrophobic behavior without permanent Si-C bonds.

Method used

Development of alkyl silicates represented by formula (I) with specific structural units and functional groups, ensuring hydrolytic stability and absence of Si-C bonds, allowing for low surface tension and hydrophobicity.

Benefits of technology

The alkyl silicates exhibit hydrolytic stability, low surface tension, and thermal stability, making them suitable for applications in textiles, cosmetics, and architectural protection, demonstrating hydrophobicity and ease of preparation.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

To provide an alkyl silicate that is stable to hydrolysis. The alkyl silicate is represented by the following formula (I): [SiO 4 / 2 ] a [(R x O)SiO 3 / 2 ] b [(R y O)SiO 3 / 2 ] b’ [(R x O)2SiO 2 / 2 ] c [(R x O)(R y O)SiO 2 / 2 ] c’ [(R y O)2SiO 2 / 2 ] c’’ [(R x O)3SiO 1 / 2 ] d [(R x O)2(R y O)SiO 1 / 2 ] d’ [(R x O)(R y O)2SiO 1 / 2 ] d’’ [(R y O)3SiO 1 / 2 ] d’’’ (I)
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a novel alkyl silicate represented by formula (I). [Background technology]

[0002] Silicones are a technologically very important class of products used in many technical fields and are distinguished from carbon-based polymers by their technologically important properties, such as low surface tension and low crystallinity. Silicones remain liquid over a wide temperature range and have a very low glass transition temperature.

[0003] However, silicones have the characteristic of being difficult to decompose in the environment because they have Si-alkyl groups. This characteristic has limited the applications of silicones. Therefore, there is a demand for alternative materials to conventional silicones that are theoretically possible to treat with water but have sufficient hydrolytic stability for practical use.

[0004] The object of the present invention is therefore to find a material that can replace silicone, which does not contain permanent Si-C bonds but has similar properties such as glass transition temperature, surface tension, density, hydrophobic behavior, etc.

[0005] Patent Document 1 discloses a compound of the general formula H 5 C 2 O-[(OC 2 H 5 ) 2 SiO] n-x [(OR) 2 SiO] x -C 2 H 5 In the formula, n is 3, 4 or 5, x is 1 to 6, and the groups R are the same or different groups selected from the group consisting of 2-phenylethyl, cinnamyl, thymyl, vanillyl, 5-formylphenyl, eugenyl, santalyl, santalidyl, menthyl, and isobutyl. These compounds are useful as fiber modifiers.

[0006] Non-Patent Document 1 discloses a compound of the formula [(BuO) 3 SiO] x Si(OH) y where Bu is tert-butyl, x is 2, and where Bu is 2-butyl, x is 2 or 3, and y is 4-x. These compounds have a low R y The mole fraction of =H can reach up to 50 mol%.

[0007] Patent Document 2 discloses a compound of the general formula R-[(OR) 2 SiO] x Disclosed is a method for preparing alkyl silicates represented by -OR, where x is 2, 3, or 4, and in each case, the radical R is an alkyl radical having 3 to 12 carbon atoms. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] Russian Patent Application Publication No. 2263115 [Patent Document 2] U.S. Patent No. 2,758,127 [Non-patent literature]

[0009] [Non-Patent Document 1] Abe et al., Bull. Soc. Chim. 1969, 42, 1118 Summary of the Invention

[0010] Thus, there remains a need to provide additional alkyl silicates, especially alkyl silicates that are hydrolytically stable.

[0011] This object is achieved by the novel alkylsilicates according to claims 1-7.

[0012] The present invention provides an alkylsilicate-containing organosilicon compound which contains at least 90% by weight, preferably at least 95% by weight, of an alkylsilicate represented by the following formula (I): [SiO 4 / 2 ] a [(R x O)SiO 3 / 2 ] b [(R y O)SiO 3 / 2 ] b’ [(R x O) 2 SiO 2 / 2 ] c [(R x O)(R y O)SiO 2 / 2 ] c’ [(R y O) 2 SiO 2 / 2 ] c’’ [(R x O) 3 SiO 1 / 2 ] d [(R x O) 2 (R y O)SiO 1 / 2 ] d’ [(R x O)(R y O) 2 SiO 1 / 2 ] d’’ [(R y O) 3 SiO 1 / 2 ] d’’’ (I) In the formula, the indices a, b, b', c, c', c'', d, d', d'', and d''' represent the average content of each structural unit in the compound and are each independently numbers in the range of 0 to 100,000, with the proviso that the sum of the indices is 2 or more. In addition, the group R x are each independently selected from groups satisfying at least one of the following conditions: (a)R x is a substituted or unsubstituted C branched at the α-carbon atom4 -C 20 It is a hydrocarbon group. (b)R x is a substituted or unsubstituted C branched at the β-carbon atom 5 -C 20 It is a hydrocarbon group. (c)R x is an unsubstituted or alkyl substituted cyclopentyl, cyclohexyl, or cycloheptyl group having a total of up to 9 carbon atoms. In this context, substituted in all cases means that the hydrocarbon group has at least one functional group selected from the group consisting of vinyl, ethynyl, amino, epoxy, thiol, and carbinol groups. In the formula, the group R y are each independently selected from the group consisting of: (i) hydrogen, (ii) a methyl group, and (iii) an ethyl group; However, all groups R in the alkyl silicate y The molar fraction of R is in the range of 0.1 to 20 mol%, preferably 1 to 15 mol%. y is (i) hydrogen, the molar fraction of which is not more than 9 mol %, preferably not more than 5 mol %, in which case all radicals R x and R y The molar amount is based on the total amount of However, the alkylsilicate-containing organosilicon compound does not contain a SiC bond group.

[0013] Alkyl silicates represented by the following formula (I) are preferred. [SiO 4 / 2 ] a [(R x O)SiO 3 / 2 ] b [(R y O)SiO 3 / 2 ] b’ [(R x O) 2 SiO 2 / 2 ] c [(R x O)(R y O)SiO 2 / 2 ]c’ [(R y O) 2 SiO 2 / 2 ] c’’ [(R x O) 3 SiO 1 / 2 ] d [(R x O) 2 (R y O)SiO 1 / 2 ] d’ [(R x O)(R y O) 2 SiO 1 / 2 ] d’’ [(R y O) 3 SiO 1 / 2 ] d’’’ (I) In the formula, the indices a, b, b', c, c', c'', d, d', d'', and d''' represent the average content of each structural unit in the compound and are each independently numbers in the range of 0 to 100,000, with the proviso that the sum of the indices is 2 or more. In addition, the group R x are each independently selected from groups satisfying at least one of the following conditions: (a)R x is a substituted or unsubstituted C branched at the α-carbon atom 4 -C 20 It is a hydrocarbon group. (b)R x is a substituted or unsubstituted C doubly branched at the β-carbon atom. 5 -C 20 It is a hydrocarbon group. (c)R x is an unsubstituted or alkyl substituted cyclopentyl, cyclohexyl, or cycloheptyl group having a total of up to 9 carbon atoms. In this context, substituted in all cases means that the hydrocarbon group has at least one functional group selected from the group consisting of vinyl, ethynyl, amino, epoxy, thiol, and carbinol groups. In the formula, the group R yare each independently selected from the group consisting of (i) hydrogen, (ii) a methyl group, and (iii) an ethyl group. However, all groups R in the silicate y The molar fraction of R is in the range of 0.1 to 20 mol%, preferably 1 to 15 mol%. y is (i) hydrogen is less than or equal to 9 mol %, preferably less than or equal to 5 mol %, wherein in each case all the groups R x and R y Based on the total molar amount of

[0014] "Branched" means that there are two carbon radicals on one carbon atom. "Doubly branched" means that there are three carbon radicals on one carbon atom.

[0015] Preferably, the group R y are each independently (ii) a methyl group or (iii) an ethyl group.

[0016] Preferably, the group R x are each independently selected from groups satisfying at least one of the following conditions: (a)R x is a substituted or unsubstituted C branched at the α-carbon atom 4 -C 10 A hydrocarbon group, especially a substituted or unsubstituted C 4 -C 10 It is an aliphatic hydrocarbon group. (b)R x is a substituted or unsubstituted C doubly branched at the β-carbon atom. 5 -C 10 A hydrocarbon group, especially a substituted or unsubstituted C doubly branched at the β-carbon atom 5 -C 10 It is an aliphatic hydrocarbon group. (c)R x is an unsubstituted or alkyl substituted cyclohexyl group having a total of up to 9 carbon atoms.

[0017] base Rx Examples include 2-butyl, 3-methyl-2-butyl, 3-methyl-2-pentyl, 3-pentyl, 2-hexyl, 3-hexyl, 2-heptyl, 2-octyl, 1-phenylethyl, 1-phenyl-1-propyl, 2,2-dimethyl-1-propyl, 1,1-dimethylethyl, 1,1-dimethylpropyl, cyclohexyl, and 3,3,5-trimethylcyclohexyl, cyclopentyl, and cycloheptyl.

[0018] base R x Preferred examples of the alkyl group include a 2-butyl group, a 3-methyl-2-butyl group, a 3-methyl-2-pentyl group, a 3-pentyl group, a 2-hexyl group, a 3-hexyl group, a 2-heptyl group, a 2-octyl group, a 1-phenylethyl group, a 1-phenyl-1-propyl group, a 2,2-dimethyl-1-propyl group, a 1,1-dimethylethyl group, a 1,1-dimethylpropyl group, a cyclohexyl group, and a 3,3,5-trimethylcyclohexyl group.

[0019] base R x Particularly preferred examples include a 2-butyl group, a 3-methyl-2-butyl group, a 3-methyl-2-pentyl group, a 3-pentyl group, a 2-hexyl group, a 3-hexyl group, a 2-heptyl group, a 2-octyl group, a 2,2-dimethyl-1-propyl group, a 1,1-dimethylethyl group, a 1,1-dimethylpropyl group, a cyclohexyl group, and a 3,3,5-trimethylcyclohexyl group.

[0020] Substituted group R x Examples include: -C(CH 3 ) 2 -CH 2 -NH 2 , -CH(CH 3 )-CH 2 -NH 2 , -CH(C 2 H 5 )-CH 2 -NH 2 , -C(CH 3 ) 2 -CH2 -NH-CH 2 -CH 2 -NH 2 , -CH(CH 3 )-CH 2 -NH-CH 2 -CH 2 -NH 2 , -CH(C 2 H 5 )-CH 2 -NH-CH 2 -CH 2 -NH 2 , -C(CH 3 ) 2 -CH=CH 2 , -CH(CH 3 )-CH=CH 2 , -CH(C 2 H 5 )-CH=CH 2 , -C(CH 3 ) 2 -C≡CH, -CH(CH 3 )-C≡CH,-CH(C 2 H 5 )-C≡CH, and glycidyl groups.

[0021] Preferably, the indices a, b, b', c, c', c'', d, d', d'', and d''' in formula (I) are each independently a number in the range of 0 to 500, preferably a number in the range of 0 to 100, more preferably a number in the range of 0 to 50, and particularly preferably a number in the range of 0 to 10, with the proviso that the sum of the indices is at least 2.

[0022] The silicate according to the present invention can be produced, for example, by hydrolysis of a compound represented by the general formula (II) (chlorosilane, alkoxychlorosilane or alkoxysilane). (R x O) m Cl 4-m Silicon(II) where m=0, 1, 2, 3 or 4, and optionally the formula Ry In the presence of an alcohol represented by OH or R x Compounds with OH and water (R y O) 4 The compound is obtained by alcoholysis of Si, and has the group R x are each independently represented by R x and the group R y are each selected from the group consisting of (i) hydrogen, (ii) a methyl group, and (iii) an ethyl group.

[0023] A further option for preparing the alkyl silicates of the invention is to react an oligomeric or polymeric methoxy or ethoxy silicate with an alcohol R, optionally in the presence of a catalyst. x OH, where the group R x is R in formula (I) x Examples of suitable catalysts are alkali metal hydroxides such as KOH, or sodium methoxide.

[0024] The compounds according to the invention are hydrophobic and have low surface tension as demonstrated by hydrophobicity tests. y is hydrogen and all groups R x and R y Based on the total molar amount of y Compounds containing are hydrophobic. The compound is furthermore hydrolytically and thermally stable: for example, at 140° C., no condensation of Si—OH groups to Si—O—Si was observed.

[0025] The compounds according to the invention are in particular y is 5 mol % or less of hydrogen, more preferably R y When is a methyl or ethyl group, it is stable and hydrophobic.

[0026] Furthermore, the compounds according to the invention can be prepared in a simple manner, they have a silicone-like low surface tension and a low glass transition temperature, and can be used in particular in the fields where silicones are used, such as waterproofing, defoamers, textiles, cosmetics, building protection, and household products. EXAMPLES

[0027] (Measurement method) base R x and R y The mole fraction of H 2 -CH 3 Group, O.C. H 3 Group and -O H By integrating the group, 1 The composition of the ethyl silicate used and the composition of the product are determined by H-NMR spectroscopy. 29 Determined by Si-NMR spectroscopy. The surface tension γ was measured at 20° C. by the hanging drop method. The glass transition temperature was determined by differential thermal analysis. The dynamic viscosity η was measured at 20° C. using a rotational viscometer Stabinger SVM3000 from Anton Paar.

[0028] The hydrophobicity test was carried out as follows. The prepared alkyl silicate was applied twice to a cement-based gypsum board. After 2 hours, the alkyl silicate was dropped onto the applied gypsum board, and the change in the shape of the droplet was observed at room temperature after application. Evaluation criteria: 0 (droplets spread, no hydrophobicity), + (droplets become somewhat flat, good hydrophobic behavior), ++ (droplets do not change, very good hydrophobicity).

[0029] The silicate TES34 is 34% by weight of SiO 2 It is ethyl silicate having a content of 0.01% and is prepared by hydrolytic condensation of 850 g of tetraethoxysilicate with 38 g of water in the presence of ethanol and HCl.

[0030] Example 1: Preparation of an alkyl silicate containing 92 mol % 2,2-dimethyl-1-propyl groups and 8 mol % hydrogen groups 10.4 g (118 mmol) of 2,2-dimethyl-1-propanol was dissolved in 56 g of methyl tert-butyl ether and treated with 9.8 g of pyridine. This solution was added dropwise with stirring over 40 minutes to a solution containing 10.0 g (59.1 mmol) of silicon tetrachloride in 27 g of methyl tert-butyl ether, while maintaining the temperature in the range of -15°C to -5°C, and rinsed with 15 g of methyl tert-butyl ether. The reaction was allowed to react with stirring for an additional hour, warmed to room temperature, filtered, and the clear reaction solution was treated with a mixture of 9.8 g of pyridine and 1.04 g of water at room temperature. The mixture was left overnight, filtered again, and the solution was evaporated under reduced pressure to give the 2,2-dimethyl-1-propyl group (R x = 2,2-dimethyl-1-propyl group) 92 mol% and hydrogen group (R y 10.4 g of product are obtained, containing 8 mol % of =H. T g =-27℃

[0031] Example 2: Preparation of an alkyl silicate containing 92 mol % 2-butyl groups and 8 mol % hydrogen groups A solution containing 26.2 g (353 mmol) of 2-butanol, 29.2 g (369 mmol) of pyridine and 145 g of methyl tert-butyl ether is added dropwise with stirring over a period of 1 h to a solution containing 30.0 g (177 mmol) of silicon tetrachloride in 216 g of methyl tert-butyl ether solution, while keeping the temperature in the range of -15 ° C to -5 ° C, and stirred for a further 2.5 h without cooling. The reaction mixture is filtered and the MTBE is distilled off at standard pressure. The residue consists of a mixture of chloroalkoxysilanes, which is fractionally distilled under a reduced pressure of 13 to 15 mbar. Cl 2 Si[O(2-Bu)] 2 and ClSi[O(2-Bu)] 3The product fraction with a boiling point of 80-82 °C consisting of is diluted with methyl tert-butyl ether, treated with a mixture of 6.8 g of pyridine and 0.84 g of water, and stirred overnight. It is filtered, and the methyl tert-butyl ether is distilled off under reduced pressure. The residue is a 2-butyl group (R x = 2-butyl group) 92 mol% and hydrogen group (R y It consists of an alkyl silicate containing 8 mol% of (=H). T g =-124℃, η=48.6mPa·s, γ=17.4mN / m Heating the product at 140°C for 2 hours did not change the hydrogen group content. The prepared product was impregnated into cement-based gypsum board and showed water repellency (hydrophobicity), with a hydrophobicity value of +.

[0032] Example 3: Preparation of an alkyl silicate containing 85 mol % 2-butyl groups and 15 mol % ethyl groups Wacker(R) Silicate TES 40 WN(SiO 2 % by weight and about 60% by weight of ethyl groups, and is represented by the formula (I), in which R x =R y 150 g of ethyl (R = ethyl and relative ratio a:(b+b'):(c+c'+c''):(d+d'+d''+d''') = 1:19:42:38) is treated with 360 g of 2-butanol and 0.15 g of sodium methoxide. The resulting ethanol is slowly distilled off in a 40 cm packed column. After removing the excess 2-butanol, the residue is neutralized with ammonium chloride and filtered. The product is a 2-butyl group (R x = 2-butyl group) 85 mol% and ethyl group (R y = ethyl group) and consists of an alkyl silicate with a relative ratio of a:(b+b'):(c+c'+c''):(d+d'+d''+d''') = 1:16:42:40. T g =-130℃, η=23.2mPa·s, γ=22.3mN / m The prepared product was impregnated into cementitious gypsum board and showed very good water repellency (hydrophobicity), with a hydrophobicity value of ++. For comparison, the Wacker® Silicate TES 40 WN used has a hydrophobicity value of: 0. For comparison, a trimethylsiloxy-terminated polydimethylsiloxane having a viscosity of about 35 mPa·s has a hydrophobicity value of:++.

[0033] Example 4 Preparation of an alkyl silicate containing 75 mol % 2-butyl groups, 15 mol % 2,2-dimethyl-1-propyl groups, and 8 mol % ethyl groups Silicate TES34 [wherein R x and R y is ethyl, relative ratio a:(b+b'):(c+c'+c''):(d+d'+d''+d''')=0:3:23:74] is reacted with 153 g of 2-butanol as described in Example 3. The alkyl silicate formed contains 87 mol % 2-butyl groups and 13 mol % ethyl groups (R y = ethyl group). 21 g of this alkyl silicate is heated to 130-190 °C with 16.1 g of 2,2-dimethyl-1-propanol, and ethanol, 2-butanol, and finally excess 2,2-dimethyl-1-propanol are removed in a packed column. The residue is treated with ammonium chloride and filtered. The product is a 2-butyl group (R x = 2-butyl group) 75 mol%, 2,2-dimethyl-1-propyl group (R x = 2,2-dimethyl-1-propyl group) 15 mol%, and ethyl group (R y It is made of an alkyl silicate containing 8 mol% (ethyl group). T g =-134℃, η=6.65mPa·s, γ=19.4mN / m The hydrophobicity value is ++.

[0034] Example 5: Preparation of alkyl silicate containing 3,3,5-trimethylcyclohexyl group The flask is charged with 190.2 g (1.34 mol) of 3,3,5-trimethylcyclohexanol, 83.8 g (1.09 mol) of Wacker® Silicate TES 40 WN (containing 1.09 mol of ethoxy groups) and 81 mg of sodium methoxide. The ethanol formed during the reaction is distilled off and the bottom temperature rises to 200° C. in the course of the reaction. The excess 3,3,5-trimethylcyclohexanol is distilled off at 45 mbar, bottom temperature 135° C. and top temperature 110° C. The product is of formula I(R x = 3,3,5-trimethylcyclohexyl radical, R y = ethyl, R x :R y =99.8:0.2, relative ratio a:(b+b'):(c+c'+c''):(d+d'+d''+d''')=1:28:33:38), and it is obtained as a colorless liquid. T g =-43℃, η=2.46mPa s

[0035] Example 6 Hydrolytic stability 4.03 g of the product from Example 3 (containing 34.5 mmol of bound 2-butyl groups and 6.13 mmol of bound ethyl groups) was added to D 2 The biphasic mixture is stirred in a sealed flask at 23-25 ​​°C. The pH of the aqueous phase is 7.5. After 51 days, 1 As measured by H-NMR spectroscopy, 2 The contents of 2-butanol and ethanol in the O phase consist of 35 μmol of 2-butanol (approximately 1 mol % relative to bound butyl groups) and 4.77 μmol of ethanol (approximately 0.08 mol % relative to bound ethyl groups).

[0036] Example 7 Hydrolytic stability 4.97 g of the product from Example 5 is treated with 5.06 g (200 mmol) of water (pH 7.0) and the mixture is stirred at 23-25° C. for 19 days. The mixture is extracted with dichloromethane. The 3,3,5-trimethylcyclohexanol content is determined by gas chromatography using naphthalene as a standard. The 3,3,5-trimethylcyclohexanol content is 0.16%.

[0037] Example 8 Hydrolytic stability The reaction of Example 7 is repeated using 220 mg of Tonsil® (acid-activated bleaching earth). The 3,3,5-trimethylcyclohexanol content is 0.67 mol %.

[0038] Example 9 Hydrolytic stability The reaction of Example 7 is repeated with 2.08 g of sodium acetate to obtain a pH of 8.8. The 3,3,5-trimethylcyclohexanol content is 0.29 mol%.

Claims

1. The following formula (I): [SiO 4/2 ] a [(R x O)SiO 3/2 ] b [(R y O)SiO 3/2 ] b’ [(R x O) 2 SiO 2/2 ] c [(R x O)(R y O)SiO 2/2 ] c’ [(R y O)2SiOO 2/2 ] c’’ [(R x O) 3 SiO 1/2 ] d [(R x O) 2 (R y O)SiO 1/2 ] d’ [(R x O)(R y O) 2 SiO 1/2 ] d’’ [(R y O) 3 SiO 1/2 ] d’’’ (I) (In the formula, the indices a, b, b', c, c', c'', d, d', d'', and d''' each independently represent the average content of each structural unit in the compound, and are numbers within the range of 0 to 100,000, provided that the sum of the indices is 2 or more; group R x are each independently selected from groups satisfying at least one of the following conditions: (a) R x is a substituted or unsubstituted C 4 -C 20 It is a hydrocarbon group. (b) R x is a substituted or unsubstituted C doubly branched at the β-carbon atom 5 -C 20 It is a hydrocarbon group. (c) R x is an unsubstituted or alkyl substituted cyclopentyl, cyclohexyl, or cycloheptyl group having a total of up to 9 carbon atoms. In the above conditions, the term "substituted" means that the hydrocarbon group has at least one functional group selected from the group consisting of a vinyl group, an ethynyl group, an amino group, an epoxy group, a thiol group, and a carbinol group; In the formula, the group R y are each independently selected from the group consisting of: (i) hydrogen, (ii) a methyl group, and (iii) an ethyl group; However, all groups R in the silicate y The mole fraction of R is in the range of 1 to 15 mol %. y (i) the molar fraction of hydrogen is not more than 9 mol %, and in each case all the groups R x and R y (based on the total molar amount of alkyl silicate).

2. The group R y and each independently is (ii) a methyl group or (iii) an ethyl group.

3. The group R x The alkyl silicate according to claim 1 or 2, wherein each of the groups is independently selected from groups satisfying any of the following conditions: (a) R x is a substituted or unsubstituted C 4 -C 10 It is an aliphatic hydrocarbon group. (b) R x is a substituted or unsubstituted C doubly branched at the β-carbon atom 5 -C 10 It is an aliphatic hydrocarbon group. (c) R x is an unsubstituted or alkyl substituted cyclohexyl group having a total of up to 9 carbon atoms.

4. The group R x is selected from the group consisting of a 2-butyl group, a 3-methyl-2-butyl group, a 3-methyl-2-pentyl group, a 3-pentyl group, a 2-hexyl group, a 3-hexyl group, a 2-heptyl group, a 2-octyl group, a 1-phenylethyl group, a 1-phenyl-1-propyl group, a 2,2-dimethyl-1-propyl group, a 1,1-dimethylethyl group, a 1,1-dimethylpropyl group, a cyclohexyl group, and a 3,3,5-trimethylcyclohexyl group.

5. The indices a, b, b', c, c', c'', d, d', d'', and d''' are each independently numbers in the range of 0 to 500, with the proviso that the sum of the indices is 2 or more. The alkylsilicate according to any one of claims 1 to 4.

6. The indices a, b, b', c, c', c'', d, d', d'', and d''' are each independently numbers in the range of 0 to 10, with the proviso that the sum of the indices is 2 or greater. The alkylsilicate according to any one of claims 1 to 5.

7. An alkylsilicate-containing organosilicon compound comprising 90% by weight or more, preferably 95% by weight or more, of the alkylsilicate according to any one of claims 1 to 6.

Citation Information

Patent Citations

  • Process for preparing composition containing 2-ethylhexyl silicate

    JP2017137485A

  • Process for preparing composition containing 2-propylheptyl silicate

    JP2017197521A

  • Modifying agents of textile materials - polyethoxysiloxanes comprising pharmacophore organooxysilyl ligands and method for their preparing

    RU2263115C1

  • Method of preparing silicon esters by reacting an alkoxysilanol with an alkoxysilamine

    US2758127A