2-color molded product
The two-color molded product with a crystalline inner and high-fluidity polyester outer parts addresses durability and pattern clarity issues, ensuring robustness and precise design alignment.
Patent Information
- Application Number
- JP2020087931
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-05-20
- Publication Date
- 2024-11-20
- Estimated Expiration
- 2040-05-20
AI Technical Summary
Conventional two-color molded products face issues with durability, particularly when used as containers for medicinal liquids, due to cracking or damage from applied force or impact, and suffer from uneven patterns and poor alignment between resin parts.
A two-color molded product design using a crystalline synthetic resin for the inner part and a polyester with a spiral flow length of 200 mm or more at 200°C for the outer part, ensuring a clear decorative pattern and enhanced durability by controlling shrinkage and fluidity.
The design provides a two-color molded product with improved durability and clear decorative patterns, resisting cracking and impact, and maintaining design alignment.
Smart Images

Figure 0007587227000002 
Figure 0007587227000003 
Figure 0007587227000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a two-color molded product. [Background technology]
[0002] Conventionally, there is a so-called two-color molding method in which two types of molten molding resins differing in color, material, etc. are sequentially injection molded to produce a two-color molded product in which two different types of molded resin parts are joined (Patent Document 1). In addition, as a method for obtaining a decorated two-color molded product, there is a so-called simultaneous two-color molding and painting method in which a decorated sheet with a printed pattern or the like is sandwiched between a base sheet by closing the mold, and the molten molding resin is injection molded while the decorated sheet is bonded to the injection molded product at the same time.
[0003] Conventionally, a second cavity mold is used in which a decorative sheet is not supplied during secondary molding. For this reason, a decorative sheet can be attached to the surface of the primary molded resin part of a two-color molded product, but a decorative sheet cannot be attached to the surface of the secondary molded resin part. In order to form a pattern on the surface of the secondary molded resin part, the only option is to apply screen printing or the like to the surface of the secondary molded resin part of the two-color molded product in a separate process after the two-color molding process. A screen-printed pattern is far inferior to a pattern of a decorative sheet in terms of the number of colors and the precision of the pattern. In addition, it is extremely difficult to accurately align and screen print the pattern of the decorative sheet that is already attached to the surface of the molded resin part. Therefore, production efficiency is poor because a separate process is required in addition to the two-color molding process. Furthermore, the surface of the two-color molded product will have both the pattern of the decorative sheet and the pattern of the screen printing, which means that only two-color molded products with an unattractive appearance can be produced with unevenness in the number of colors and precision of the pattern. Furthermore, the pattern on the surface of the primary molded resin part and the pattern on the surface of the secondary molded resin part are not accurately aligned, so the only products that can be produced are those that are painted in two colors and look bad.
[0004] Therefore, in order to provide a two-color molded product with a good-looking pattern, the present inventor proposed a two-color molded product consisting of an inner part made of a crystalline plastic material and an outer part made of an amorphous plastic material (Patent No. 6608690). According to the invention of the two-color molded product previously proposed by the present inventor, the inner part is made of a high-shrinkage crystalline plastic material and the outer part is made of a low-shrinkage amorphous plastic material, so that the crystalline plastic of the inner part shrinks more than the amorphous plastic of the outer part when cooled. As a result, a small gap is formed between the material of the inner part and the material of the outer part, so that if a decorative pattern is applied to the material of the inner part, the decorative pattern of the material of the inner part can be clearly recognized due to the difference in refractive index between the material of the inner part and the material of the outer part. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2012-126079 A Summary of the Invention [Problem to be solved by the invention]
[0006] The two-color molded product proposed by the present inventor can be applied to various applications, and can be used, for example, as a container for storing medicinal liquids (liquid medicines such as eye drops, liquid quasi-drugs, liquid cosmetics, etc.). It is preferable that the two-color molded product storing such medicinal liquids has excellent durability. In this respect, the two-color molded product previously proposed by the present inventor can form an attractive pattern, but when used, for example, as a container for eye drops, cracks may occasionally occur on the outer part when too much force is continuously applied to the fastening due to opening and closing operations, or the outer part may occasionally be damaged when a large impact is temporarily applied, such as when the container is dropped while being carried, and there is room for improvement in terms of durability.
[0007] The present invention has been made in consideration of the above-mentioned improvements in the prior art, and an object of the present invention is to provide a two-color molded article having excellent durability. [Means for solving the problem]
[0008] The present invention relates to a two-color molded product consisting of an inner part of the primary injection molded product obtained by injection molding a first synthetic resin and a secondary injection molded product obtained by injection molding a second synthetic resin so as to cover the primary injection molded product, and the two-color molded product is composed of an inner part of the primary injection molded product and an outer part of the secondary injection molded product, the first synthetic resin being a crystalline synthetic resin and the second synthetic resin being a polyester having a spiral flow length of 200 mm or more at 200°C.
[0009] The spiral flow length is the flow length in Archimedes spiral flow when injection molding is performed using the following mold under the following measurement conditions. The mold used has a resin injection port at the center and an Archimedean spiral curved groove with constant groove spacing starting from the resin injection port. The spiral shape is 10 mm wide, 2 mm thick, and has a maximum flow length of 1,300 mm. The measurement conditions were: injection pressure 100 MPa, injection time 10 seconds, injection speed 50 mm / second, mold temperature 50°C, and molding temperature 200°C. The Archimedes spiral is a type of algebraic spiral, a curve expressed by the polar equation r=aθ (a is a constant) in polar coordinates (r, θ). The Archimedes spiral is a spiral in which the lines are spaced equally apart.
[0010] Generally, thermoplastic resins are in a solid state at temperatures below their melting point, but when heated above their melting point, they melt and become fluid. Representative methods for expressing the fluidity (viscosity) of thermoplastic resins when molten include melt flow rate, methods using measuring instruments such as capillary rheometers, and flow length evaluations using actual injection molding machines. Generally, melt viscosity characteristics show a tendency to depend on the molecular weight of the polymer, but in reinforced grades and elastomer-modified grades, the fluidity does not necessarily correlate with the molecular weight because it is affected by the content of the reinforcing material.
[0011] <Melt flow rate> Melt flow rate is an index of fluidity expressed by converting the amount of sample (between the marked lines) extruded from an orifice by applying a certain weight to a sample melted in a cylinder (heated barrel) into weight per 10 minutes (unit: g / 10 minutes). Under the same cylinder temperature and load conditions, a material with a higher melt flow rate has better fluidity, but since thermoplastic resins are generally non-Newtonian fluids in which the shear stress of the flow and the flow velocity gradient are not proportional, when the apparent shear rate changes significantly due to molding conditions or molded product shape, such as in injection molding, the relationship between the fluidity during molding and the melt flow rate may not match.
[0012] <Capillary rheometer> The capillary rheometer is a test method in which a sample molten in a cylinder is extruded through a capillary, similar to the melt flow rate. The difference from the melt flow rate is that it can be calculated as melt viscosity (unit: Pa·sec) instead of resin weight per unit time. However, melt viscosity depends on shear rate and temperature, so when using melt viscosity characteristics to judge fluidity, it is cumbersome to confirm the appropriate shear rate range according to the molding method and shape.
[0013] <Flow length> The flow length is a method of evaluating the fluidity of a material using an actual injection molding machine and mold. Since the flow length depends on the molding conditions and shape, the fluidity can be relatively judged by keeping the molding temperature, mold temperature, injection pressure, injection speed, and injection time constant. The flow length is also an index of fluidity that takes into account not only the melt viscosity but also the solidification characteristics of the material, making it more practical than the melt flow rate and capillary rheometer mentioned above. A long spiral flow length at 200°C indicates that the material has high fluidity at 200°C, which is a relatively low molding temperature for resins, and that it can be used under a wide range of molding conditions and is suitable for a variety of shapes.
[0014] In the present invention, the first synthetic resin of the inner part is a crystalline synthetic resin, and the second synthetic resin of the outer part is a polyester having a spiral flow length of 200 mm or more at 200°C, so that a two-color molded product with excellent durability can be provided, as described below.
[0015] Although it is called crystalline synthetic resin, not all parts are crystalline, but crystalline and non-crystalline parts are mixed. The proportion of the crystalline parts is called the crystallinity, and those with a relatively high degree of crystallinity are crystalline synthetic resins. Examples of crystalline synthetic resins include polyethylene, polypropylene, polyethylene terephthalate, polybutylene terephthalate, polyamide, polyacetal, polyphenylene sulfide, polyether ether ketone, and polytetrafluoroethylene.
[0016] Crystalline synthetic resins have the following characteristics: "They have a glass transition temperature and melting point. They are difficult to make transparent. Volume changes occur due to crystallization (large shrinkage during molding). It is difficult to achieve dimensional precision. They have excellent fatigue resistance. They have excellent mechanical strength. They have excellent chemical resistance. They have excellent sliding properties. They have a high reinforcing effect due to additives. They have excellent mechanical properties. They are suitable for functional parts. They have excellent rigidity and springiness." By constructing the inner part of the present invention from a crystalline synthetic resin, the following effects can be expected.
[0017] Crystalline synthetic resins shrink, reducing their volume, when they change from liquid to solid. The ratio of this shrinkage is called the shrinkage rate. In other words, it is a numerical value defined as: shrinkage rate = [(length before shrinkage) - (length after shrinkage)] / (length before shrinkage). Table 1 below shows the numerical values of the shrinkage rates of representative crystalline plastics.
[0018] [Table 1]
[0019] By making the inner part a high shrinkage material of crystalline synthetic resin, the crystalline synthetic resin of the inner part shrinks more than the second synthetic resin of the outer part when cooled. As a result, a small gap is formed between the material of the inner part and the material of the outer part, and if a decorative pattern is applied to the material of the inner part, the decorative pattern of the material of the inner part can be clearly recognized from the outside due to the refractive index difference between the material of the inner part and the material of the outer part. Therefore, as the crystalline synthetic resin of the inner part, polypropylene, high density polyethylene, polyacetal, and polybutylene terephthalate, which have a large shrinkage rate in Table 1, can be particularly preferably used. Note that the difference in shrinkage rate between the crystalline synthetic resin and the second synthetic resin (the value obtained by subtracting the shrinkage rate of the second synthetic resin from the shrinkage rate of the crystalline synthetic resin) is preferably 3 / 1000 or more. If this shrinkage rate difference is less than 3 / 1000, the difference in refractive index between the material of the inner part and the material of the outer part is small, so that the decorative pattern of the material of the inner part cannot be clearly recognized. In order to make it possible to more clearly see the decorative pattern of the inner material, it is preferable that the difference in shrinkage rate between the crystalline synthetic resin and the second synthetic resin is large, but judging from the materials that are actually available, the upper limit of the difference in shrinkage rate between the crystalline synthetic resin and the second synthetic resin is approximately 50 / 1000.
[0020] The second synthetic resin can be injection molded to cover the primary injection molded product at a temperature that does not melt the primary injection molded product, and a polyester having a spiral flow length of 200 mm or more at 200 ° C. can be used. The spiral flow length is more preferably 250 mm or more at 200 ° C., and even more preferably 300 mm or more at 200 ° C. The polyester is not particularly limited, but examples thereof include polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, etc., and blends thereof can also be used. Among them, polyethylene terephthalate is preferable. By adopting a polyester having a spiral flow length of 200 mm or more at 200 ° C. as the second synthetic resin for the outer part of the present invention, a two-color molded product having high fluidity, a wide range of molding conditions, adaptable to various shapes, and excellent durability can be provided. Effect of the Invention
[0021] According to the present invention, it is possible to provide a two-color molded article having excellent durability. [Brief description of the drawings]
[0022] [Figure 1] FIG. 1(a) is a longitudinal cross-sectional view of the inner part of one embodiment of a two-color molded product of the present invention, FIG. 1(b) is a longitudinal cross-sectional view of the outer part of one embodiment of a two-color molded product of the present invention, and FIG. 1(c) is a longitudinal cross-sectional view of one embodiment of a two-color molded product of the present invention. [Diagram 2] FIG. 2 is an external photograph showing the results of a compression test on a two-color molded product of an embodiment in which polyethylene terephthalate (spiral flow length at 200° C.: 320 mm) is used for the outer portion. [Diagram 3] FIG. 3 is an external photograph showing the results of a compression test on a two-color molded product of a comparative example in which acrylonitrile styrene was used for the outer portion. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] The present invention will be described in detail below based on the embodiments. Note that the embodiments described below are merely examples, and the present invention is not limited to the embodiments, and various changes and modifications are possible without departing from the technical scope of the present invention.
[0024] The two-color molded product of the present invention can be obtained by injection molding using first and second fixed molds and a movable mold. Figure 1(a) is a diagram showing a vertical cross section of an inner part 1 obtained by performing a first injection molding using a crystalline synthetic resin in a first cavity defined by a first fixed mold and a movable mold. Then, the first injection molding part is moved together with the movable mold, and a second injection molding is performed using a polyester having a spiral flow length of 200 mm or more at 200°C in a second cavity defined by a second fixed mold and a movable mold, and a two-color molded product 3 in which the outer part 2 and the inner part 1 are integrated can be obtained as shown in Figure 1(c).
[0025] As shown in FIG. 1(a), a radially protruding undercut portion 4 is formed at the lower end of the inner portion 1, so that the outer portion 2 is held in the undercut portion 4 of the inner portion 1 as shown in FIG. 1(c), thereby enabling a good fitting state to be maintained.
[0026] <Compression test> A compression test was carried out to evaluate the strength of the two-color molded article of the present invention. As an example, polypropylene was used for the inner part 1 and easily moldable polyethylene terephthalate (spiral flow length at 200°C: 320 mm) was used for the outer part 2, and injection molding was performed as described in paragraph 0024 to prepare a two-color molded product with a predetermined decorative pattern on the outside of the inner part 1.
[0027] As a comparative example, a two-color molded product was prepared using polypropylene for the inner part 1 and acrylonitrile styrene for the outer part 2, and by performing injection molding as described in paragraph 0024, a predetermined decorative pattern was applied to the outside of the inner part 1.
[0028] A load of 180 N was applied to the two-color molded products of the examples and comparative examples using a tensile compression tester ("TRAPEZIUM LITE X" manufactured by Shimadzu Corporation) at a speed of 100 mm / min to check the state of damage to the caps. As a result, the photographs shown in Figures 2 and 3 were obtained.
[0029] As shown in Fig. 3, in the two-color molded product of the comparative example in which acrylonitrile styrene was used for the outer part, numerous cracks in the form of white stripes were observed in the diagonal and horizontal directions in the outer part which appears gray. However, as shown in Fig. 2, in the two-color molded product of the example in which polyethylene terephthalate (spiral flow length at 200°C is 320 mm) was used for the outer part, no cracks like those shown in Fig. 3 were observed. In this way, it was confirmed that the two-color molded product of the present invention has remarkably high durability. [Industrial Applicability]
[0030] As described above, the two-color molded article of the present invention is useful as a container or a part of a container (for example, a lid) for storing cosmetics, medicines, foodstuffs, and various other contents. [Explanation of symbols]
[0031] 1 Inner part 2 Outer part 3 Two-color molded product 4 Undercut section
Claims
1. The two-color molded product is composed of an inner part of the primary injection molded product obtained by injection molding a first synthetic resin, and a secondary injection molded product obtained by injection molding a second synthetic resin so as to cover the primary injection molded product, and is composed of an outer part of the secondary injection molded product, wherein the first synthetic resin is a crystalline synthetic resin, and the second synthetic resin is a polyester having a spiral flow length of 200 mm or more at 200°C during injection molding using the following mold and measurement conditions, and the difference in shrinkage rate between the crystalline synthetic resin and the second synthetic resin is 3 / 1000 or more and 50 / 1000 or less. The mold used had a resin injection port at the center and an Archimedes spiral curved groove with constant groove spacing starting from the resin injection port. The spiral shape was 10 mm wide, 2 mm thick, and had a maximum flow length of 1,300 mm. The measurement conditions were an injection pressure of 100 MPa, an injection time of 10 seconds, an injection speed of 50 mm / second, a mold temperature of 50°C, and a molding temperature of 200°C.
2. 2. The two-color molded product according to claim 1, wherein the crystalline synthetic resin is any one of polyethylene, polypropylene, polyethylene terephthalate, polybutylene terephthalate, polyamide, polyacetal, polyphenylene sulfide, polyether ether ketone and polytetrafluoroethylene.
3. 3. The two-color molded article according to claim 1, wherein the polyester comprises polyethylene terephthalate.
4. 4. The two-color molded article according to claim 1, wherein the secondary injection molded article is transparent.
5. 5. The two-color molded product according to claim 1, wherein a decorative pattern is applied to the outside of the primary injection molded product.
Citation Information
Patent Citations
Injection molding composite vessel and its manufacturing method
JP2009263006A
Thermoplastic polyester resin composition
JP2011032295A
Synthetic-resin multiple container and manufacturing method for the same
JP2012025402A
Mold for two color molding and method of molding two color molding
JP2012126079A
JPP6608690B