Aromatic amide polymer, its production method, and resin composition, prepreg, and molded article containing said aromatic amide polymer

A thermoplastic aromatic amide polymer with specific molecular properties addresses the limitations of existing epoxy resins, providing high heat resistance, thermal conductivity, and low thermal expansion, enabling film or sheet-shaped products and fiber-reinforced composites.

JP7587382B2Active Publication Date: 2024-11-20NIPPON STEEL CHEM & MATERIAL CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2020161065
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-09-25
Publication Date
2024-11-20
Estimated Expiration
2040-09-25

AI Technical Summary

Technical Problem

Existing epoxy resins, such as those based on bisphenol A or bisphenol F, suffer from issues like low heat resistance, high thermal expansion, poor thermal conductivity, and limited formability, making them unsuitable for film-like or sheet-like epoxy resin molded products and fiber-reinforced composite materials.

Method used

A thermoplastic aromatic amide polymer with a specific molecular structure and crystallinity, produced through methods involving bisphenol compounds and diglycidyl ether reactions, offering high heat resistance, thermal conductivity, and low thermal expansion properties.

Benefits of technology

The polymer enables the production of film or sheet-shaped epoxy resin cured products with excellent heat resistance, high thermal conductivity, and low thermal expansion, suitable for secondary processing and applications like multilayer printed wiring boards and fiber-reinforced composites.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007587382000001
    Figure 0007587382000001
  • Figure 0007587382000002
    Figure 0007587382000002
  • Figure 0007587382000003
    Figure 0007587382000003
Patent Text Reader

Abstract

To provide a polymer that is suitable for the preparation of a film-like or sheet-like epoxy resin composition or cured epoxy resin being excellent in high heat resistance, high thermal conductance, low thermal expansion and high toughness.SOLUTION: A crystalline, thermoplastic, aromatic amide polymer includes a unit represented by general formula (1), the proportion of which is 10-100 mol% (where A is an amide bond, R1, R2 independently represent a hydrogen atom, a C1-8 alkyl group, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and n is an integer selected from 1-3) and has a weight average molecular weight of 5,000 or more. There is also provided a method for producing the same.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a novel polymer containing an aromatic amide skeleton, a method for producing the same, a resin composition and a prepreg using the polymer, and molded articles obtained by molding them. [Background technology]

[0002] Up to now, high molecular weight epoxy resins, such as phenoxy resins, have been used as essential components of epoxy resins used to obtain film- or sheet-shaped epoxy resin molded products. Phenoxy resins with bisphenol A or bisphenol F as the main skeleton have been widely used, but they have problems with heat resistance, low thermal expansion, high thermal conductivity, and the like. For example, Patent Document 1 describes an adhesive-attached copper foil using a bisphenol A-type polymer epoxy resin, but the multilayer printed wiring board produced by this method has a disadvantage that it has inferior heat resistance and low thermal expansion compared to multilayer printed wiring boards produced by conventional techniques due to its low glass transition point. In addition, for example, Patent Document 2 discloses a phenoxy resin produced from bisphenol A and bisphenol S (4,4'-dihydroxydiphenyl sulfone) in order to provide a self-bonding insulated electric wire with excellent thermal adhesion and heat deformation resistance. However, this resin has a high viscosity compared to phenoxy resins with a similar molecular weight, and has problems with handling as a resin alone, and is still insufficient in terms of heat resistance. Furthermore, phenoxy resins are hardly soluble in common solvents such as toluene and methyl ethyl ketone, and have drawbacks in terms of handling. In addition, most of the phenoxy resins known to date are amorphous solids with no crystallinity, and have a problem in that their physical properties drop significantly above their glass transition point. Patent Document 3 also discloses an epoxy resin with an amide structure, and shows that it can be made into a three-dimensional cured product, but it does not have film properties.

[0003] Patent Document 4 discloses that an epoxy resin composition having an amide structure is formed into a sheet as a method for improving heat resistance. However, this gives a three-dimensionally cured product, which is poor in formability and lacks secondary processability. In addition, the molded product does not have crystallinity, and the effect of improving physical properties such as thermal conductivity and low thermal expansion is insufficient. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 7-202418 [Patent Document 2] Japanese Patent Application Publication No. 2-45575 [Patent Document 3] Japanese Patent Application Publication No. 2-282375 [Patent Document 4] JP 2010-195851 A Summary of the Invention [Problem to be solved by the invention]

[0005] An object of the present invention is to provide a polymer that can be suitably used for preparing a film- or sheet-shaped resin composition for use in a cured epoxy resin, or a fiber-reinforced composite material such as glass fiber or carbon fiber, and that has secondary processability after molding and is excellent in heat resistance, high thermal conductivity, and low thermal expansion; a method for producing the polymer; a resin composition and a prepreg that use the polymer; and molded products obtained by molding the polymer or the prepreg. [Means for solving the problem]

[0006] The present invention relates to a compound represented by the following general formula (1): [ka] (Wherein, A is an amide bond, R 1 , R 2each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and n represents a number from 1 to 3.) accounts for 10 to 100 mol % of the unit, and the weight average molecular weight is 5,000 or more.

[0007] Moreover, it is desirable for the aromatic amide polymer to satisfy at least one of the following requirements: a) In the general formula (1), the benzene ring has a 1,4-phenylene structure, and R 1 , R 2 are all hydrogen atoms and n is 1. b) It has crystallinity, and the peak temperature of the endothermic curve accompanying the melting of the crystals in differential scanning calorimetry measured at a heating rate of 10°C / min is in the range of 100°C to 350°C. c) It is crystalline and the integrated value of the endothermic curve peak accompanying the melting of the crystals in differential scanning calorimetry measured at a heating rate of 10°C / min is 5 Joules / g or more.

[0008] The present invention also relates to a resin composition containing the above aromatic amide polymer, or a prepreg obtained by impregnating a fiber substrate with the aromatic amide polymer, and a molded product obtained by hot molding the same.

[0009] The process for producing an aromatic amide polymer of the present invention is any of the following processes. i) a compound represented by the following general formula (2): [ka] (Wherein, A is an amide bond, R 1 , R 2 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and n represents a number from 1 to 3, and [ka] (In the formula, m represents a number from 0 to 3, and R 3, R 4 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom; each X independently represents a direct bond, an oxygen atom, a sulfur atom, -SO-, -SO 2 -, -CO-, -COO-, -CONH-, -CH=N-, -CH=CH-, -CH=C(CH 3 )-, -CH 2 -, -CH(CH 3 )-, -C(CH 3 ) 2 -, -φ-, -CH 2 -φ-CH 2 -, -CH(CH 3 )-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-C(CH 3 ) 2 -, -CH 2 -φ-φ-CH 2 -, -CH(CH 3 )-φ-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-φ-C(CH 3 ) 2 13. A method for producing a bisphenol compound represented by the formula (I) wherein φ is a phenylene group,

[0010] ii) a compound represented by the following general formula (4): [ka] (In the formula, m, R 3 , R 4 and X are the same as in general formula (3), and a diglycidyl compound represented by the following general formula (5): [ka] (In the formula, A, R 1 , R 2 and n is the same as in general formula (2), Effect of the Invention

[0011] The polymer of the present invention has thermoplasticity and, when applied to a molding material, has secondary processability and preferably has crystallinity with a melting point of 100°C or higher, and is expected to have excellent characteristics such as high heat resistance, high thermal conductivity, and low thermal expansion, and can be suitably used in fields where it is utilized as film- or sheet-like molded products such as multilayer printed wiring boards, fiber-reinforced composite materials such as carbon fibers, adhesives, and coating materials. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The present invention will be described in detail below.

[0013] The polymer of the present invention contains the unit represented by the above general formula (1) in a ratio of 10 to 100 mol %, preferably 40 to 100 mol %, more preferably 60 to 100 mol %. If the ratio is less than this range, it is difficult to achieve the effects of the present invention, that is, high heat resistance, low thermal expansion, and high thermal conductivity.

[0014] An example of a unit other than the unit represented by general formula (1) that may be contained in the polymer of the present invention is a unit represented by the following general formula (6). Among these, in terms of ease of crystallization, a unit having a direct bond, an oxygen atom, or a methylene bond is preferably used. [ka] [In the formula, n represents a number from 0 to 3, and R 3 , R 4 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom; each X independently represents a direct bond, an oxygen atom, a sulfur atom, -SO-, -SO 2 -, -CO-, -COO-, -CONH-, -CH=N-, -CH=CH-, -CH=C(CH 3 )-, -CH 2 -, -CH(CH 3 )-, -C(CH 3) 2 -, -φ-, -CH 2 -φ-CH 2 -, -CH(CH 3 )-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-C(CH 3 ) 2 -, -CH 2 -φ-φ-CH 2 -, -CH(CH 3 )-φ-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-φ-C(CH 3 ) 2 - or 9,9-fluorenyl group, where φ represents a phenylene group.

[0015] The weight-average molecular weight of the polymer of the present invention is 5,000 or more. If the molecular weight is less than 5,000, when the resin composition using the polymer is applied and dried on a substrate such as copper foil, SUS foil, polyethylene terephthalate film, polyimide film, or glass plate, or when the resin composition is impregnated into a fiber substrate such as glass fiber or carbon fiber to form a composite material, problems such as insufficient strength or poor dimensional stability are likely to occur. In addition, if the molecular weight exceeds 200,000, even if the polymer is diluted and dissolved in a solvent, the solution viscosity becomes too high at a concentration of 40% by weight to 70% by weight that is generally used industrially, making it difficult to apply the polymer to a substrate or impregnate the fiber substrate. Therefore, the weight-average molecular weight of the polymer of the present invention is preferably 5,000 to 100,000, more preferably 10,000 to 60,000.

[0016] The polymer of the present invention preferably has a reduced viscosity in the range of 0.2 to 1.2 dL / g, more preferably 0.3 to 0.8 dL / g, as measured in N-methylpyrrolidone as a solvent at 30° C. If the reduced viscosity is lower than this range, the film properties are reduced, and if the reduced viscosity is higher than this range, the handleability is reduced.

[0017] The polymer of the present invention is essentially composed of the unit of general formula (1), and is not necessarily a two-dimensional polymer, and may have a branched structure. The branched structure can be formed by the reaction of the hydroxyl group of general formula (1) with the epoxy group, or when a trifunctional or higher epoxy resin and a curing agent are used in combination. It is necessary that the polymer having a branched structure also has thermoplasticity. Being thermoplastic improves the impact resistance of the molded product, and also enables secondary processing, such as molding the sheet into a different shape after molding the sheet.

[0018] The polymer of the present invention is preferably at least partially crystallized. The degree of crystallization can be grasped by differential scanning calorimetry. Specifically, the peak (endothermic peak) of the endothermic curve accompanying the melting of the crystals in differential scanning calorimetry measured at a heating rate of 10°C / min is measured, and the temperature is taken as the melting point, and the heat of fusion is calculated from the integral value of this endothermic peak curve. Here, the preferred heat of fusion is 5 joules / g (hereinafter sometimes written as "j / g") or more, preferably 10 j / g or more, and more preferably 30 j / g or more. If it is lower than this, the properties such as heat resistance, high thermal conductivity, and low thermal expansion based on the crystallinity are insufficient. In addition, the preferred melting point range is one in which the endothermic peak temperature is in the range of 100°C to 350°C when measured at a heating rate of 10°C / min using a differential scanning calorimetry device. If it is lower than this, the properties such as heat resistance and low thermal expansion based on the crystallinity are insufficient, and if it is higher than this, the handling property is reduced.

[0019] The degree of crystallinity of the polymer of the present invention can generally be adjusted by annealing at a temperature below the melting point. Annealing is preferably performed under conditions of a temperature 10°C to 100°C lower than the melting point for 5 minutes to 12 hours. In some cases, crystallization can be performed by adding a solvent or a low molecular weight epoxy.

[0020] Examples of the terminal group of the polymer of the present invention include an epoxy group, a hydroxyl group, a carboxylic acid, an amino group, a vinyl group, a mercapto group and an aromatic group, with an epoxy group being preferred.

[0021] The method for producing the polymer of the present invention may be a direct reaction between a dihydric phenol compound and epichlorohydrin, but is generally an addition polymerization reaction between a diglycidyl ether compound and a dihydric phenol compound. The polymer of the present invention may be produced by either method, but if the crystallinity of the polymer is low, it will be in a supercooled state and the crystallinity will not increase, and conversely, if the crystallinity is high, crystals will already precipitate in the low molecular weight state as the polymerization proceeds, and the molecular weight of the polymer will not increase. Therefore, it is necessary to select a desired polymerization method and polymerization conditions according to the properties of the target polymer. Each production method will be described below.

[0022] In the case of the direct reaction between a dihydric phenol compound and epichlorohydrin, a bisphenol compound represented by the above general formula (5) is used as the dihydric phenol compound, but the bisphenol compound of general formula (5) must account for 10 mol% or more of the total dihydric phenol compounds used. If it is less than 10 mol%, the effect of introducing an aromatic amide skeleton is insufficient, and it is difficult to obtain a molded product having excellent heat resistance, high thermal conductivity, and low thermal expansion.

[0023] In the case of a method using an addition polymerization reaction between a diglycidyl ether compound and a dihydric phenol compound, there is a method in which a dihydric phenol compound represented by the above general formula (3) or (5) is reacted with a diglycidyl ether compound represented by the above general formula (2) or (4). In this case, at least one of the dihydric phenol compound represented by the general formula (5) or the diglycidyl ether compound represented by the general formula (2) is essential.

[0024] In the general formulas (1) to (5), R 1 , R 2 , R 3 , R 4 R independently represents a substituent selected from a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and is preferably a hydrogen atom or a methyl group. 1 , R 2 , R 3, R 4 In the case where the carbon atom at the α-position is a secondary or tertiary carbon atom, the reactivity of the hydroxyl group is reduced, which is not preferred. In the general formulae (1) to (5), the linking positions of the benzene rings include the 1,4-position, the 1,3-position, and the 1,2-position, and the 1,4-position is particularly preferred. In the case of the 1,3-position and the 1,2-position, the crystallinity of the resulting polymer tends to be lower than that of the 1,4-position, and therefore the physical properties due to the crystallinity, such as heat resistance, high thermal conductivity, and low thermal expansion, tend to be lower.

[0025] In the general formula (3) or (4), each X group is independently a direct bond, an oxygen atom, a sulfur atom, -SO-, -SO 2 -, -CO-, -COO-, -CONH-, -CH=N-, -CH=CH-, -CH=C(CH 3 )-, -CH 2 -, -CH(CH 3 )-, -C(CH 3 ) 2 -, -φ-, -CH 2 -φ-CH 2 -, -CH(CH 3 )-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-C(CH 3 ) 2 -, -CH 2 -φ-φ-CH 2 -, -CH(CH 3 )-φ-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-φ-C(CH 3 ) 2 - or 9,9-fluorenyl group (φ represents a phenylene group), but preferably, the molecule is easily oriented for crystallization, has little steric hindrance, and is a symmetrical direct bond, an oxygen atom, -CO-, -COO-, -CH 2 -, -φ-.

[0026] Examples of preferred dihydric phenol compounds represented by the general formula (3) include 4,4'-dihydroxybiphenyl, 4,4'-dihydroxydiphenyl ether, 1,4-bis(4-hydroxyphenoxy)benzene, 1,3-bis(4-hydroxyphenoxy)benzene, 4,4'-bis(4-hydroxyphenoxy)diphenyl ether, 4,4'-dihydroxybenzophenone, and 4,4'-dihydroxydiphenyl sulfide, and more preferably 4,4'-dihydroxybiphenyl and 4,4'-dihydroxybenzophenone. These dihydric phenol compounds can be used as a mixture.

[0027] In the case of the method by the addition polymerization reaction of a diglycidyl ether compound and a dihydric phenol compound, there is a method of reacting a diglycidyl ether compound represented by general formula (2) with a dihydric phenol compound represented by general formula (3), or a method of synthesizing by reacting a diglycidyl ether compound represented by general formula (4) with a dihydric phenol compound represented by general formula (5). This reaction can be carried out in the presence of a catalyst such as an amine, imidazole, triphenylphosphine, or phosphonium salt. The molar ratio of the diglycidyl ether compound to the dihydric phenol compound is usually in the range of 3:1 to 1:3 (glycidyl ether compound:dihydric phenol compound), preferably 2:1 to 1:2, and more preferably 1.1:1 to 1:1.1. The closer the molar ratio of the diglycidyl ether compound to the dihydric phenol compound is to 1, the higher the molecular weight of the obtained polymer will be.

[0028] This reaction can be carried out without using a solvent, but a solvent may be used. Examples of the solvent include aliphatic ketones such as acetone, methyl ethyl ketone, methyl isobutyl ketone, cyclohexanone, and cyclopentanone; aromatics such as benzene, toluene, ortho-xylene, meta-xylene, para-xylene, chlorobenzene, and dichlorobenzene; aliphatic amides such as N,N-dimethylformamide, N,N-dimethylacetamide, and N-methylpyrrolidone; ethers such as tetrahydrofuran, dioxane, diethylene glycol dimethyl ether, and triethylene glycol dimethyl ether; and dimethyl sulfoxide. Examples of preferred organic solvents include cyclopentanone, cyclohexanone, diethylene glycol dimethyl ether, N,N-dimethylacetamide, N-methylpyrrolidone, and dimethyl sulfoxide. Two or more of these organic solvents may be selected and used as a mixed solvent.

[0029] This reaction can be carried out after mixing fillers such as silica, alumina, carbon powder, carbon fiber powder, carbon nanofiber, and cellulose nanofiber. Furthermore, the reaction may be carried out after impregnating a fiber substrate such as glass fiber or carbon fiber with a mixture of a diglycidyl ether compound and a dihydric phenol compound with a catalyst, or a preliminary reaction product thereof. As a method of impregnation, the mixture or preliminary reaction product may be formed into a sheet or block shape, or a powdered product may be used. Furthermore, a solution or dispersion in a solvent may be used.

[0030] In this polymerization reaction, the diglycidyl ether compound and the dihydric phenol compound can each be used as a mixture of two or more kinds, but the diglycidyl ether compound and the dihydric phenol compound must be selected so that they are 10 mol % or more in the polymer obtained from the unit represented by general formula (1). If they are less than 10 mol %, the effect of introducing the aromatic amide skeleton is insufficient, and a molded product having heat resistance, low thermal expansion, and high thermal conductivity cannot be obtained, which is not preferable.

[0031] Such an aromatic amide polymer of the present invention can be made into a resin composition using components described later, or can be impregnated into a sheet-like fiber substrate to form a prepreg, as described later. Here, in the resin composition or prepreg of the present invention, if a polymer having a weight average molecular weight of 5,000 or more is used as the polymer of the present invention, the resin flow during molding is small and the circuit embedding property is often somewhat insufficient. In this case, in order to obtain sufficient circuit embedding property, another low molecular weight epoxy resin can be further added. In this case, the molecular weight of the low molecular weight epoxy resin is 3,000 or less, preferably 1,500 or less, more preferably 800 or less, in weight average molecular weight.

[0032] In this case, the blending ratio of the polymer of the present invention to the low molecular weight epoxy resin is preferably 10 to 90 parts by weight, more preferably 20 to 60 parts by weight, per 100 parts by weight of the polymer of the present invention. If the blending amount of the low molecular weight epoxy resin is less than this range, the improvement in the flowability of the resin during molding is small, whereas if the blending amount is more than this range, the heat resistance and moisture resistance of the cured product are reduced.

[0033] The low molecular weight epoxy resin is preferably aromatic and has an epoxy equivalent of 100 g / eq to 2,000 g / eq in order to ensure sufficient circuit embedding without deteriorating physical properties such as flexibility and heat resistance after curing. If the epoxy equivalent exceeds 2,000 g / eq, the effect of improving circuit embedding cannot be obtained sufficiently, and the crosslink density is likely to be low, making it difficult to obtain a heat-resistant cured film. If the epoxy equivalent is less than 100 g / eq, the crosslink density of the cured product is likely to be high, and thermoplasticity is impaired, resulting in a decrease in secondary processability of the molded product. For these reasons, the epoxy equivalent of the low molecular weight epoxy resin is preferably 130 g / eq to 1,500 g / eq, more preferably 150 g / eq to 1,000 g / eq. Preferred low molecular weight epoxy resins include epoxy resins obtained by reacting a dihydric phenol represented by the above general formula (3) with epichlorohydrin, and examples thereof include, but are not limited to, bisphenol A type epoxy resins, bisphenol F type epoxy resins, tetramethylbisphenol F type epoxy resins, tetrabromobisphenol A type epoxy resins, etc. These epoxy resins may be used alone or in combination of two or more kinds.

[0034] The weight-average molecular weight of the polymer of the present invention is 5,000 or more, but in order to impart more sufficient film properties, other high molecular weight epoxy resins can be further added.

[0035] In this case, the weight blending ratio of the polymer of the present invention to the high molecular weight epoxy resin is preferably in the range of 10 to 90 parts by weight, more preferably 20 to 60 parts by weight, per 100 parts by weight of the total amount of the polymer of the present invention and the high molecular weight epoxy resin. If the amount is less than this, the effects of adding the high molecular weight epoxy resin cannot be expected in terms of flexibility, heat resistance, low thermal expansion, and high thermal conductivity.

[0036] The preferred molecular weight of the high molecular weight epoxy resin is, in terms of weight average molecular weight, 5,000 to 100,000, more preferably 10,000 to 60,000. Examples of the high molecular weight epoxy resin include, but are not limited to, bisphenol A type epoxy resin, bisphenol F type epoxy resin, tetramethylbisphenol F type epoxy resin, and tetrabromobisphenol A type epoxy resin.

[0037] The resin composition or prepreg of the present invention advantageously contains an epoxy resin, a phenoxy resin, or a compound containing an epoxy group. Such a resin may be the polymer of the present invention. When the resin composition or prepreg of the present invention contains an epoxy resin or a compound containing an epoxy group, it is desirable to use a curing agent.

[0038] As the curing agent, all commonly known curing agents can be used. For example, dicyandiamide and its derivatives, imidazoles such as 2-methylimidazole and 2-ethyl-4-methylimidazole and their derivatives, divalent phenol compounds such as bisphenol A, bisphenol F, brominated bisphenol A, naphthalenediol, and dihydroxybiphenyl, novolac-type phenolic resins obtained by condensation reaction of phenols such as phenol, cresol, bisphenol A, naphthol, and naphthalenediol with aldehydes such as formaldehyde or ketones, and phenols such as phenol, cresol, bisphenol A, naphthol, and naphthalenediol with xylylene. Examples of the curing agent include, but are not limited to, commonly used epoxy resin curing agents, such as phenolic compounds such as aralkyl-type phenolic resins obtained by condensation reaction with propylene glycols, acid anhydride compounds such as phthalic anhydride, trimellitic anhydride, pyromellitic anhydride, maleic anhydride, and hexahydrophthalic anhydride, amine compounds such as polyamidoamines obtained by condensation reaction between acids such as diaminodiphenylmethane, triethylenetetramine, isophoronediamine, and dimer acid and polyamines, and hydrazides such as adipic acid dihydrazide and isophthalic acid dihydrazide. These curing agents may be used alone or in combination of two or more.

[0039] A solvent may be used in the resin composition or prepreg in the present invention to maintain a suitable viscosity when applied to a substrate. The solvent for adjusting viscosity is preferably one that does not remain when the solvent is dried at 80°C to 200°C, and specific examples thereof include toluene, xylene, methyl ethyl ketone, methyl isobutyl ketone, dioxane, ethanol, isopropyl alcohol, methyl cellosolve, ethyl cellosolve, cyclohexanone, N,N-dimethylformamide, N,N-dimethylacetamide, dimethyl sulfoxide, etc., but are not limited thereto. These solvents may be used alone or in combination of two or more.

[0040] To this resin composition or prepreg, silica, calcium carbonate, talc, aluminum hydroxide, mica, alumina, aluminum nitride, carbon powder, carbon fiber powder, carbon nanofiber, cellulose nanofiber, etc. may be added in order to impart heat resistance and flame retardancy, reduce the thermal expansion coefficient, increase the thermal conductivity, etc., and also, to improve adhesive strength, epoxy silane coupling agents, rubber components, etc. may be added to the extent that the physical properties of the molded product are not impaired.

[0041] This resin composition or prepreg may contain a curing accelerator as necessary. For example, various known curing accelerators such as amine-based, imidazole-based, triphenylphosphine, and phosphonium salt-based can be used, but are not limited to these. When a curing accelerator is used, the amount is preferably in the range of 0.01 wt% to 10 wt% based on the resin component. If the amount exceeds 10 wt%, it is not preferable because there is a concern that the storage stability may deteriorate.

[0042] This resin composition can be obtained as a resin molded product by transfer molding, compression molding, or by casting a resin solution dissolved or dispersed in a solvent onto a metal foil, or by impregnating a sheet-like substrate such as glass fiber, carbon fiber, or aramid fiber with the resin solution to form a prepreg, and then press-molding the prepreg. In particular, when the resin composition of the present invention is an epoxy resin composition, it is preferable to adjust the viscosity to 15 Pa·s or less, preferably 10 Pa·s or less, using the solvent mentioned above, add an appropriate amount of curing agent so as to have a certain curing time, and optionally add a curing accelerator to make a varnish, which is applied to a substrate, volatilized at 100°C to 160°C to form a prepreg, and heated to form a molded product. EXAMPLES

[0043] The present invention will now be described in detail with reference to examples. The present invention is not limited to these examples, and various modifications and alterations are possible without departing from the gist of the present invention. The physical properties shown in the examples were evaluated according to the following methods.

[0044] (1) Hydrolyzable chlorine: 0.5 g of the sample epoxy resin A described below was dissolved in 30 ml of dioxane, 10 ml of 1N KOH was added, and the mixture was boiled under reflux for 30 minutes. The mixture was then cooled to room temperature, and 100 ml of 80% acetone water was added. The hydrolyzable chlorine was measured by potentiometric titration with a 0.002N AgNO3 aqueous solution. (2) Melting point and heat of fusion: The peak temperature of an endothermic curve obtained using a differential thermal analyzer at a heating rate of 10°C / min was taken as the melting point, and the integrated value of the endothermic peak was taken as the heat of fusion. (3) GPC measurement: Measurement was performed using a 515A model apparatus manufactured by Nihon Waters K.K. under the following conditions: columns: TSK-GEL2000 x 3 and TSK-GEL4000 x 1 (both manufactured by Tosoh Corporation), solvent: tetrahydrofuran, flow rate: 1 ml / min, temperature: 38°C, detector: RI. (4) Measurement of glass transition point and linear expansion coefficient: Measurement was performed using a thermomechanical measuring device, TMA120C, manufactured by Seiko Instruments Inc., at a heating rate of 10° C. / min. (5) Thermal conductivity: Measured by the transient hot wire method using a NETZSCH LFA447 thermal conductivity meter.

[0045] Reference example 1 (Synthesis of 4,4'-dihydroxybenzanilide) 300 g of 4,4'-dihydroxybenzophenone was dissolved in 900 mL of ethanol. Then, a solution of 147.6 g of hydroxylamine hydrochloride and 172.2 g of sodium acetate dissolved in 210 mL of distilled water was added, followed by 300 mL of ethanol. After heating at 75°C for 4 hours, the mixture was cooled to room temperature and filtered. The ethanol and water contained in the filtrate were evaporated and concentrated. The solution was then dropped into 2500 mL of distilled water, and the resulting white crystals were collected by filtration. These were then dried to obtain 284.0 g of white powder. This was 1It was confirmed to be 4,4'-dihydroxybenzophenone oxime by H-NMR measurement. 1200mL of acetic acid and 18.64g of toluenesulfonic acid monohydrate were added to 234.4g of the obtained 4,4-dihydroxybenzophenone oxime, and the reaction mixture was heated to 80°C and reacted for 3 hours, after which 1000mL of distilled water was added and the product was collected by filtration. After washing with distilled water and drying, 200.2g of pale yellow crystals were obtained (bisphenol compound A). The melting point was 273°C.

[0046] Reference example 2 50 g of 4,4'-dihydroxybenzanilide (bisphenol compound A) was dissolved in 550 g of epichlorohydrin and 500 mL of N-methylpyrrolidone (NMP), and 145 g of 12% aqueous sodium hydroxide solution was added dropwise to react at 75°C for 1.5 hours. Water and epichlorohydrin were distilled off from the reaction solution under reduced pressure, and insoluble matter was filtered off. The filtrate was then slowly added dropwise to a large amount of water while stirring. The precipitated solid was filtered, washed with water, and dried to obtain 70.0 g of white powdery epoxy resin (epoxy resin A). The melting point was 242°C. The epoxy equivalent was 174 g / eq, and the hydrolyzable chlorine was 670 ppm. The component ratios determined by GPC measurement of the obtained resin were as follows: R in the structure of general formula (2) 1 , R 2 Compounds with a hydrogen atom and n equal to 1 accounted for 93.6% of the compounds, and their dimers accounted for 6.4%.

[0047] Reference example 3 After dissolving 144 g of m-aminophenol in 900 mL of NMP, 120 mL of a tetrahydrofuran solution of 64 g of isophthaloyl chloride was added dropwise over 30 minutes. The mixture was then reacted at 80°C for 3 hours. The reaction solution was cooled to room temperature, then added dropwise to a large amount of water, and the precipitate was collected by filtration. After washing with distilled water and drying, 106.4 g of gray-white powdery crystals were obtained (bisphenol compound B). The melting point was 281.6°C. The product was analyzed by FD-MS, 1 H-NMR measurement confirmed that the compound was N,N'-bis(3-hydroxyphenyl)-1,3-benzenecarboxamide.

[0048] Example 1 72 parts of 4,4'-diglycidyloxydiphenyl ether (epoxy resin B; Nippon Steel Chemical & Material, YSLV-80DE, epoxy equivalent 164g / eq., melting point 82°C) and 50 parts of 4,4'-dihydroxybenzanilide (bisphenol compound A) synthesized in Reference Example 1 were melt-mixed at 150°C, and 0.8 parts of triphenylphosphine was added and mixed, and then quickly cooled to obtain an epoxy resin composition. This was press-molded at 175°C for 5 minutes in a pressure molding machine to obtain a pale yellow, opaque, crystalline sheet-like molded product. Measurements were performed using a differential thermal analyzer at a heating rate of 10°C / min, and the melting point of the molded product was 211°C and the heat of fusion was 12 J / g. The physical property measurement results of the molded product are shown in Table 1. It was confirmed that the molded product was deformable by heating to 180°C and was a thermoplastic polymer. Although it did not completely dissolve in tetrahydrofuran (THF), the soluble portion was measured by GPC and found to have a weight average molecular weight of 8600. Based on the charge ratio during polymerization, the proportion of the unit of general formula (1) in the obtained polymer was 50.0 mol%.

[0049] Example 2 Epoxy resin B 75.4g, bisphenol compound A 30g, and 4,4'-dihydroxydiphenyl ether (bisphenol compound C) 20g were molded in the same manner as in Example 1 to obtain a pale yellow, opaque, crystalline sheet-like molded product. The melting point of the molded product was 206°C, and the heat of fusion was 7 J / g. The physical property measurement results of the molded product are shown in Table 1. The molded product was confirmed to be a thermoplastic polymer that could be deformed by heating to 180°C. Although it did not completely dissolve in THF, the soluble portion was measured by GPC and found to have a weight average molecular weight of 10,400. The ratio of the units of general formula (1) in the obtained polymer was 28.3 mol% based on the charge ratio during polymerization.

[0050] Example 3 Epoxy resin B (77.4 g), bisphenol compound A (20 parts), and bisphenol compound C (30 parts) were used for molding in the same manner as in Example 1 to obtain a yellow, opaque sheet-like molded product. The results of measuring the physical properties of the molded product are shown in Table 1. The molded product was confirmed to be a thermoplastic polymer that could be deformed by heating to 150°C. Although it did not completely dissolve in THF, the soluble portion was measured by GPC and found to have a weight average molecular weight of 12,800. Based on the charge ratio during polymerization, the proportion of the unit of general formula (1) in the obtained polymer was 18.5 mol%.

[0051] Example 4 86.1 g of epoxy resin A and 50 g of bisphenol compound C were molded in the same manner as in Example 1 to obtain a pale yellow, opaque, crystalline sheet-like molded product. The melting point of the molded product was 204°C, and the heat of fusion was 32 J / g. The physical property measurement results of the molded product are shown in Table 1. The molded product was confirmed to be a thermoplastic polymer, being deformable by heating to 180°C. Although it did not completely dissolve in THF, the soluble portion was measured by GPC and found to have a weight average molecular weight of 9200. The ratio of the units of general formula (1) in the obtained polymer was 50.0 mol% based on the charge ratio during polymerization.

[0052] Example 5 Epoxy resin B (74.4 g), bisphenol compound B (10 parts), and bisphenol compound C (40 parts) were used for molding in the same manner as in Example 1 to obtain a yellow, opaque sheet-like molded product. The results of measuring the physical properties of the molded product are shown in Table 1. The molded product was confirmed to be a thermoplastic polymer that could be deformed by heating to 150°C. Although it did not completely dissolve in THF, the soluble portion was measured by GPC and found to have a weight average molecular weight of 10,400. Based on the charge ratio during polymerization, the proportion of the unit of general formula (1) in the obtained polymer was 25.3 mol%.

[0053] Comparative Example 1 Molding was carried out in the same manner as in Example 1 using 81.2 g of epoxy resin B and 50 parts of bisphenol compound C to obtain a pale yellow, opaque, crystalline sheet-like molded product. The melting point of the molded product was 178°C, and the heat of fusion was 28 J / g. The results of measuring the physical properties of the molded product are shown in Table 1. The molded product was confirmed to be a thermoplastic polymer, being deformable by heating to 150°C. Although it did not completely dissolve in THF, the soluble portion was subjected to GPC measurement, and the weight average molecular weight was found to be 9700.

[0054] Comparative Example 2 85.1 g of epoxy resin A, 30 g of bisphenol compound B, and 20 g of phenol novolak (curing agent A: AICA Corporation, BRG-557; OH equivalent 104, softening point 83°C, bisphenol content 18.4%) were used and molded in the same manner as in Example 1 to obtain a pale yellow transparent sheet-like molded product. Measurement results of the physical properties of the molded product are shown in Table 1. It was confirmed that the molded product was deformable by heating to 180°C, and was a cured product that had thermoplasticity but rubber elasticity and no secondary processability. It was completely insoluble in THF.

[0055] Comparative Example 3 A bisphenol A-type phenoxy resin (YP-50; manufactured by Nippon Steel Chemical & Material Co., Ltd., weight average molecular weight 55,000) was used and molded in the same manner as in Example 1 to obtain a sheet-like molded product. The measurement results of the physical properties of the molded product are shown in Table 1.

[0056] [Table 1]

Claims

1. The following general formula (1): 【Chemistry 1】 (Wherein, A is an amide bond, R 1 , R 2 each independently represent a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and n represents a number from 1 to 3.) is present in a proportion of 10 to 100 mol %, has a weight average molecular weight of 5,000 or more, is crystalline, and exhibits a peak temperature in the endothermic curve accompanying melting of the crystals in a range of 100° C. to 350° C. as measured at a heating rate of 10° C. / min., and is a thermoplastic aromatic amide polymer in which the proportion of units represented by general formula (1) is in the range of 10 to 50.0 mol %.

2. In the general formula (1), the benzene ring has a 1,4-phenylene structure, and R 1 , R 2 2. The aromatic amide polymer according to claim 1, wherein each of the groups is a hydrogen atom, and n is 1.

3. An aromatic amide polymer according to claim 1 or 2, which contains a unit represented by the following general formula (6): 【Chemistry 2】 [In the formula, n represents a number from 0 to 3; R 3 and R 4 each independently represent a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom; and X each independently represents a direct bond, an oxygen atom, a sulfur atom, -SO-, -SO 2 -, -CO-, -COO-, -CONH-, -CH═N-, -CH═CH-, -CH═C(CH 3 )-, -CH 2 -, -CH(CH 3 )-, -C(CH 3 ) 2 -, -φ-, -CH 2 -φ-CH 2 -, -CH(CH 3 )-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-C(CH 3 ) 2 -, -CH 2 -φ-φ-φ-CH 2 -, -CH(CH )-φ-φ-CH(CH 3 )-, -C(CH 3 ) 2 -φ-φ-C(CH 3 ) 2 - or a 9,9-fluorenyl group, where φ represents a phenylene group.

4. The aromatic amide polymer according to any one of claims 1 to 3, which has crystallinity and has an integral value of an endothermic peak curve accompanying melting of crystals in differential scanning calorimetry measured at a heating rate of 10°C / min of 5 Joules / g or more.

5. A resin composition comprising the aromatic amide polymer according to any one of claims 1 to 4.

6. A resin molded product obtained by molding the resin composition according to claim 5.

7. A method for producing the aromatic amide polymer according to any one of claims 1 to 4, comprising the steps of: The following general formula (2): 【Chemistry 3】 (Wherein, A is an amide bond, R 1 , R 2 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and n represents a number from 1 to 3. 【Chemistry 4】 [In the formula, m represents a number from 0 to 3, and R 3 , R 4 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom; each X independently represents a direct bond, an oxygen atom, a sulfur atom, -SO-, -SO 2 -, -CO-, -COO-, -CONH-, -CH=N-, -CH=CH-, -CH=C(CH 3 ) -, -CH 2 -, -CH(CH 3 ) -, -C(CH 3 ) 2 -, -φ-, -CH 2 -φ-CH 2 -, -CH(CH 3 )-φ-CH(CH 3 ) -, -C(CH 3 ) 2 -φ-C(CH 3 ) 2 --, --CH 2 -φ-φ-CH 2 -, -CH(CH 3 )-φ-φ-CH(CH 3 ) -, -C(CH 3 ) 2 -φ-φ-C(CH 3 ) 2 13. A method for producing an aromatic amide polymer, comprising reacting a bisphenol compound represented by the formula (I) with a bisphenol compound represented by the formula (I):

8. A method for producing the aromatic amide polymer according to any one of claims 1 to 4, comprising the steps of: The following general formula (4): 【Chemistry 5】 [In the formula, m represents a number from 0 to 3, and R 3 , R 4 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom; each X independently represents a direct bond, an oxygen atom, a sulfur atom, -SO-, -SO 2 -, -CO-, -COO-, -CONH-, -CH=N-, -CH=CH-, -CH=C(CH 3 ) -, -CH 2 -, -CH(CH 3 ) -, -C(CH 3 ) 2 -, -φ-, -CH 2 -φ-CH 2 -, -CH(CH 3 )-φ-CH(CH 3 ) -, -C(CH 3 ) 2 -φ-C(CH 3 ) 2 --, --CH 2 -φ-φ-CH 2 -, -CH(CH 3 )-φ-φ-CH(CH 3 ) -, -C(CH 3 ) 2 -φ-φ-C(CH 3 ) 2 - or 9,9-fluorenyl group, where φ represents a phenylene group.], and a diglycidyl compound represented by the following general formula (5): 【Chemistry 6】 (Wherein, A is an amide bond, R 1 , R 2 each independently represents a hydrogen atom, an alkyl group having 1 to 8 carbon atoms, an aryl group, an alkoxy group, an aralkyl group, or a halogen atom, and n represents a number of 1 to 3.

9. A prepreg obtained by impregnating a sheet-like fiber substrate with the aromatic amide polymer according to any one of claims 1 to 4.

10. A molded product obtained by hot molding the prepreg of claim 9.

Citation Information

Patent Citations

  • Self-fusing insulating paint

    JP1990045575A

  • Improved epoxy compound of meso form

    JP1990232220A

  • Meso-type epoxy compound

    JP1990275872A

  • New diglycidyl ether

    JP1990282375A

  • Interlayer adhesive for multilayer printed wiring board, copper foil applied with adhesive and production of multilayer printed wiring board

    JP1995202418A