Thermoelectric elements

The dual-layer resin structure in thermoelectric elements addresses the issue of thermal resistance and shear stress by optimizing bonding strength and conductivity, maintaining power generation performance and durability at high temperatures.

JP7587509B2Active Publication Date: 2024-11-20LG INNOTEK CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021543237
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-01-23
Filing Date
2020-01-23
Publication Date
2024-11-20
Estimated Expiration
2040-01-23

AI Technical Summary

Technical Problem

Thermoelectric elements experience reduced power generation performance and mechanical durability due to increased thermal resistance and shear stress at high temperatures, primarily caused by the thickness of the bonding layer between the substrate and electrode, which affects the soldering site.

Method used

A thermoelectric element design incorporating a dual-layer resin structure, where the first resin layer with higher electrical resistance and lower thermal conductivity is bonded to the first metal substrate, and a second resin layer with lower electrical resistance and higher thermal conductivity is bonded to the second metal substrate, ensuring adequate bonding strength and reducing thermal resistance.

Benefits of technology

The dual-layer resin structure effectively alleviates shear stress and maintains power generation performance by preventing thermal conductivity degradation, enhancing durability and efficiency at high temperatures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007587509000008
    Figure 0007587509000008
  • Figure 0007587509000009
    Figure 0007587509000009
  • Figure 0007587509000010
    Figure 0007587509000010
Patent Text Reader

Abstract

The thermoelectric element of the present invention comprises a first metal substrate, a first resin layer, a plurality of first electrodes, a plurality of P-type thermoelectric legs and a plurality of N-type thermoelectric legs, a plurality of second electrodes, a second resin layer and a second metal substrate, wherein the first metal substrate is a low temperature portion, the second metal substrate is a high temperature portion, the second resin layer comprises a first layer and a second layer disposed on the first layer, the first and second layers comprise a silicon (Si)-based resin, and the bonding strength of the first resin layer is higher than the bonding strength of the second resin layer.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a thermoelectric element, and more particularly to a junction structure of a thermoelectric element. [Background technology]

[0002] Thermoelectricity is a phenomenon that occurs due to the movement of electrons and holes inside a material, and refers to the direct energy conversion between heat and electricity.

[0003] A thermoelectric element is a general term for elements that utilize the thermoelectric phenomenon, and has a structure in which a P-type thermoelectric material and an N-type thermoelectric material are joined between metal electrodes to form a PN junction pair.

[0004] Thermoelectric elements can be classified into elements that use the temperature change of electrical resistance, elements that use the Seebeck effect, which is a phenomenon in which an electromotive force is generated due to a temperature difference, and elements that use the Peltier effect, which is a phenomenon in which heat absorption or heat generation occurs due to an electric current. Thermoelectric elements are widely used in home appliances, electronic components, communication components, etc. For example, thermoelectric elements can be used in cooling devices, heating devices, power generation devices, etc. Accordingly, the demand for thermoelectric performance of thermoelectric elements is increasing.

[0005] The thermoelectric element includes a substrate, an electrode, and a thermoelectric leg, and a plurality of thermoelectric legs are arranged in an array between an upper substrate and a lower substrate, a plurality of upper electrodes are arranged between the plurality of thermoelectric legs and the upper substrate, and a plurality of lower electrodes are arranged between the plurality of thermoelectric legs and the lower substrate. In this case, one of the upper substrate and the lower substrate may be a low temperature portion, and the other may be a high temperature portion. When the thermoelectric element is applied to a power generating device, the greater the temperature difference between the low temperature portion and the high temperature portion, the higher the power generating performance. Accordingly, the temperature of the high temperature portion may rise to 200°C or more. When the temperature of the high temperature portion rises to 200°C or more, a high mechanical shear stress is transferred between the leg and the solder due to the difference in thermal expansion coefficient between the substrate and the electrode on the high temperature portion side. In this case, in order to relieve the shear stress applied between the leg and the solder, a bonding layer between the substrate and the electrode may be formed to a certain thickness or more. However, as the bonding layer becomes thicker, the thermal resistance decreases, resulting in a problem of a decrease in the power generating performance of the thermoelectric element. Furthermore, when the substrate expands due to overheating on the joining side, there is a limit to how much the shear stress can be alleviated, which can cause cracks to form in the soldered portion. Summary of the Invention [Problem to be solved by the invention]

[0006] The technical problem to be solved by the present invention is to provide a junction structure for a thermoelectric element. [Means for solving the problem]

[0007] A thermoelectric element according to one embodiment of the present invention includes a first metal substrate, a first resin layer disposed on the first metal substrate, a plurality of first electrodes disposed on the first resin layer, a plurality of P-type thermoelectric legs and a plurality of N-type thermoelectric legs disposed on the plurality of first electrodes, a plurality of second electrodes disposed on the plurality of P-type thermoelectric legs and the plurality of N-type thermoelectric legs, a second resin layer disposed on the plurality of second electrodes, and a second metal substrate disposed on the second resin layer, wherein the first metal substrate is a low temperature portion and the second metal substrate is a high temperature portion, the second resin layer includes a first layer in direct contact with the plurality of second electrodes and a second layer disposed on the first layer and in direct contact with the second metal substrate, the first layer and the second layer include a silicon (Si)-based resin, and the bonding strength of the first resin layer may be higher than the bonding strength of the second resin layer.

[0008] At least one of the first metal substrate and the second metal substrate may include aluminum.

[0009] The thickness of the second resin layer may be greater than or equal to the thickness of the first resin layer.

[0010] The ratio of the thickness of the second resin layer to the thickness of the first resin layer may be 1-5.

[0011] The first layer can include polydimethylsiloxane (PDMS) and aluminum oxide, and the second layer can include polydimethylsiloxane (PDMS) and silver (Ag).

[0012] The first layer may have a lower thermal conductivity than the second layer.

[0013] The first layer may have a higher electrical resistance than the second layer.

[0014] The first layer may have a thermal conductivity of 1.5 to 3.5 W / mK, and the second layer may have a thermal conductivity of 6.0 to 10.0 W / mK.

[0015] The ratio of the thickness of the second layer to the thickness of the first layer may be between 0.2 and 2.5.

[0016] The substrate may further include a polyimide layer disposed between the first layer and the second layer, and the first layer and the second layer may include a polysiloxane resin.

[0017] The first and second layers have a resistance of 1 kgf / mm at a temperature of 150 to 200°C. 2 The bond strength may be as follows:

[0018] The substrate may further include a third layer between the first layer and the polyimide layer.

[0019] The insulating layer may further include a fourth layer between the second layer and the polyimide layer.

[0020] The thermal conductivity of each of the first to fourth layers may be greater as they are closer to the second metal substrate.

[0021] At least one of the first metal substrate and the second metal substrate may include copper (Cu). Effect of the Invention

[0022] According to the embodiment of the present invention, the thickness of the bonding layer between the substrate and the electrode is ensured, and the shear stress applied to the soldering portion of the leg is alleviated, thereby improving the durability of the thermoelectric element at high temperatures. In addition, the portion of the bonding layer that is bonded to the substrate is made of a material with excellent conductivity, thereby preventing a decrease in thermal conductivity as the thickness of the bonding layer increases, and maintaining the power generation performance of the thermoelectric element.

[0023] According to an embodiment of the present invention, by bonding the substrate and the electrode with an adhesive material, it is possible to effectively prevent mechanical shear stress from being transmitted to the soldering portion of the leg due to thermal expansion of the substrate.

[0024] According to the embodiment of the present invention, the thickness of the bonding layer between the substrate and the electrode is ensured, and the shear stress applied to the soldering portion of the leg is alleviated, thereby improving the durability of the thermoelectric element at high temperatures. In addition, the portion of the bonding layer that is bonded to the substrate is made of a material with excellent conductivity, thereby preventing a decrease in thermal conductivity as the thickness of the bonding layer increases, and maintaining the power generation performance of the thermoelectric element. [Brief description of the drawings]

[0025] [Figure 1] 1 is a cross-sectional view of a thermoelectric element according to a first embodiment of the present invention.

[0026] [Diagram 2] 2 is a top view of a first metal substrate included in a thermoelectric element according to a first embodiment of the present invention. FIG.

[0027] [Diagram 3] 2 is a side view of a first metal substrate included in the thermoelectric element according to the first embodiment of the present invention. FIG.

[0028] [Figure 4] FIG. 4 is a partially enlarged view of FIG.

[0029] [Diagram 5] 1 is a perspective view of a thermoelectric element according to a first embodiment of the present invention.

[0030] [Figure 6] FIG. 1 is an exploded perspective view of a thermoelectric element according to a first embodiment of the present invention.

[0031] [Figure 7] FIG. 2 is a partially enlarged view of a thermoelectric element according to the first embodiment of the present invention.

[0032] [Figure 8] 2 is a view illustrating a state in which a thermoelectric element according to a first embodiment of the present invention is generating electricity.

[0033] [Figure 9] FIG. 4 is a cross-sectional view of a thermoelectric element according to a second embodiment of the present invention.

[0034] [Figure 10] FIG. 10 is a partially enlarged view of FIG.

[0035] [Figure 11] 11 is a view illustrating a state in which power is applied to a thermoelectric element according to a second embodiment of the present invention.

[0036] [Figure 12] FIG. 11 is a cross-sectional view of a thermoelectric element according to a third embodiment of the present invention.

[0037] [Figure 13] FIG. 11 is a partially enlarged view of a thermoelectric element according to a third embodiment of the present invention.

[0038] [Figure 14] 13 is a view illustrating a state in which a thermoelectric element according to a third embodiment of the present invention is generating electricity.

[0039] [Figure 15] FIG. 11 is a cross-sectional view of a thermoelectric element according to a fourth embodiment of the present invention.

[0040] [Figure 16] FIG. 16 is a partially enlarged view of FIG.

[0041] [Figure 17] 13 is a view illustrating a state in which power is applied to a thermoelectric element according to a fourth embodiment of the present invention.

[0042] [Figure 18]13 is a graph showing the rate of resistance change versus the number of cycles in a temperature cycle test of a third embodiment and a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0043] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0044] However, the technical concept of the present invention is not limited to the described embodiments, but may be embodied in various different forms, and one or more of the components of the embodiments may be selectively combined or substituted within the scope of the technical concept of the present invention.

[0045] Furthermore, terms (including technical and scientific terms) used in the embodiments of the present invention may be interpreted in a manner that is commonly understood by a person having ordinary knowledge in the technical field to which the present invention belongs, unless otherwise clearly defined and described, and commonly used terms, such as terms defined in a dictionary, may be interpreted in light of the contextual meaning of the relevant art.

[0046] Furthermore, the terms used in the embodiments of the present invention are intended to describe the embodiments and are not intended to limit the present invention.

[0047] In this specification, the singular can include the plural unless otherwise specified in the context, and when it is stated that "A and (and) at least one (or more) of B and C" it can include one or more of all possible combinations of A, B, and C.

[0048] Additionally, terms such as first, second, A, B, (a), (b), etc. may be used to describe components of embodiments of the present invention.

[0049] Such terms are merely used to distinguish a component from other components, and are not intended to limit the nature, order, or sequence of the components.

[0050] Furthermore, when a component is described as being "coupled," "coupled," or "connected" to another component, it may include not only the case where the component is directly coupled, coupled, or connected to the other component, but also the case where the component is "coupled," "coupled," or "connected" by yet another component between the component and the other component.

[0051] In addition, when described as being formed or disposed "above or below" each component, "above" or "below" includes not only the case where two components are in direct contact with each other, but also the case where one or more other components are formed or disposed between the two components. In addition, when described as "above or below," it can include not only the upper direction but also the lower direction based on one component.

[0052] FIG. 1 is a cross-sectional view of a thermoelectric element according to the first embodiment of the present invention, FIG. 2 is a top view of a first metal substrate included in the thermoelectric element according to the first embodiment of the present invention, FIG. 3 is a side view of the first metal substrate included in the thermoelectric element according to the first embodiment of the present invention, FIG. 4 is an enlarged partial view of FIG. 3, FIG. 5 is an oblique view of the thermoelectric element according to the first embodiment of the present invention, and FIG. 6 is an exploded oblique view of the thermoelectric element according to the first embodiment of the present invention.

[0053] 1 to 6, the thermoelectric element includes a first metal substrate 110, a first resin layer 120, a plurality of first electrodes 130, a plurality of P-type thermoelectric legs 140, a plurality of N-type thermoelectric legs 150, a plurality of second electrodes 160, a second resin layer 170, a second metal substrate 180 and a sealing means 190.

[0054] The first metal substrate 110 is formed in a plate shape. The first metal substrate 110 is disposed facing the second metal substrate 180 at a distance. The first metal substrate 110 may be made of aluminum, an aluminum alloy, copper, or a copper alloy. In particular, the first metal substrate 110 may be made of aluminum. At this time, when a voltage is applied to the thermoelectric element, the first metal substrate 110 absorbs heat due to the Peltier effect and acts as a low temperature part, and the second metal substrate 180 releases heat and acts as a high temperature part.

[0055] Meanwhile, when different temperatures are applied to the first metal substrate 110, the electrons in the high temperature region move to the low temperature region due to the temperature difference, generating a thermoelectromotive force, which is called the Seebeck effect, and the resulting thermoelectromotive force generates electricity in the circuit of the thermoelectric element.

[0056] Here, the first metal substrate 110 may be in direct contact with the first resin layer 120. To this end, the first metal substrate 110 may have surface roughness formed on the entirety or part of the surface on which the first resin layer 120 is disposed, i.e., the surface of the first metal substrate 110 facing the first resin layer 120. This can prevent the first resin layer 120 from floating during thermocompression bonding between the first metal substrate 110 and the first resin layer 120. In this specification, surface roughness refers to unevenness and may be used interchangeably with surface roughness.

[0057] 2 to 4, the surface of the first metal substrate 110 on which the first resin layer 120 is disposed, i.e., the surface of the first metal substrate 110 facing the first resin layer 120, includes a first region 112 and a second region 114, and the second region 114 may be disposed inside the first region 112. That is, the first region 112 may be disposed within a predetermined distance from the edge of the first metal substrate 110 toward the central region, and the first region 112 may surround the second region 114.

[0058] At this time, the surface roughness of the second region 114 is greater than the surface roughness of the first region 112, and the first resin layer 120 may be disposed on the second region 114. Here, the first resin layer 120 may be disposed so as to be spaced a predetermined distance from the boundary between the first region 112 and the second region 114. That is, although the first resin layer 120 is disposed on the second region 114, the edge of the first resin layer 120 may be located inside the second region 114. Accordingly, a part of the first resin layer 120, i.e., the epoxy resin 600 and a part of the inorganic filler 604 contained in the first resin layer 120, may be infiltrated into at least a part of the groove 400 formed by the surface roughness of the second region 114, and the adhesive strength between the first resin layer 120 and the first metal substrate 110 may be increased.

[0059] However, the surface roughness of the second region 114 may be larger than the size D50 of some particles of the inorganic filler contained in the first resin layer 120, and smaller than the size D50 of other particles. Here, the particle size D50 means a particle size corresponding to 50% of the weight percentage in a particle size distribution curve, that is, a particle size where the passing mass percentage is 50%, and may be mixed with the average particle size. For example, when the first resin layer 120 contains aluminum oxide and boron nitride as inorganic fillers, aluminum oxide does not affect the adhesive performance between the first resin layer 120 and the first metal substrate 110, but boron nitride has a smooth surface and may adversely affect the adhesive performance between the first resin layer 120 and the first metal substrate 110. Accordingly, if the surface roughness of the second region 114 is formed to be larger than the particle size D50 of the aluminum oxide contained in the first resin layer 120 but smaller than the particle size D50 of the boron nitride, then only aluminum oxide will be disposed in the grooves formed by the surface roughness of the second region 114, and boron nitride will be difficult to dispose of, so that the first resin layer 120 and the first metal substrate 110 can maintain a high bonding strength.

[0060] Such surface roughness can be measured using a surface roughness tester. The surface roughness tester uses a probe to measure a profile curve, and can calculate the surface roughness using the peak line, valley line, average line, and reference length of the profile curve. In this specification, surface roughness may refer to the arithmetic mean roughness (Ra) obtained by a center line average calculation method. The arithmetic mean roughness (Ra) can be obtained by the following Equation 1. Equation 1

[0061] JPEG0007587509000001.jpg1371

[0062] In other words, when the cross-sectional curve obtained by the probe of the surface roughness measuring instrument is extracted over a reference length L, and expressed as a function (f(x)) with the average line direction as the x-axis and the height direction as the y-axis, the value obtained by Equation 2 can be expressed in μm.

[0063] At this time, although not shown in the drawings, the first metal substrate 110 may have a surface roughness formed on the front surface thereof corresponding to the second region 114. In addition, the surface roughness formed on the first metal substrate 110 may be equally applied to the second metal substrate 180 described below.

[0064] The first resin layer 120 is disposed on the first metal substrate 110. The first resin layer 120 is formed to have an area smaller than that of the first metal substrate 110. Therefore, the first resin layer 120 may be disposed in an area spaced a predetermined distance from an edge of the first metal substrate 110.

[0065] The first resin layer 120 may be made of an epoxy resin composition containing an epoxy resin and an inorganic filler, or may be made of a silicone resin composition containing PDMS (polydimethylsiloxane).

[0066] Here, the inorganic filler may be contained in an amount of 68 to 88 vol% of the epoxy resin composition. If the inorganic filler is contained in an amount of less than 68 vol%, the thermal conductivity effect may be low, and if the inorganic filler is contained in an amount of more than 88 vol%, the adhesive strength between the resin layer and the metal substrate may be low, and the resin layer may be easily broken.

[0067] The epoxy resin may include an epoxy compound and a curing agent. At this time, the epoxy compound may be included in a volume ratio of 10 to 10 of the curing agent. Here, the epoxy compound may include at least one of a crystalline epoxy compound, a non-crystalline epoxy compound, and a silicon epoxy compound. The crystalline epoxy compound may include a mesogen structure. Mesogen is a basic unit of liquid crystal and includes a rigid structure. And, the non-crystalline epoxy compound may be a general non-crystalline epoxy compound having two or more epoxy groups in the molecule, for example, a glycidyl ether derived from bisphenol A or bisphenol F. Here, the curing agent may include at least one of an amine-based curing agent, a phenol-based curing agent, an acid anhydride-based curing agent, a polymercaptan-based curing agent, a polyaminoamide-based curing agent, an isocyanate-based curing agent, and a blocked isocyanate-based curing agent, and two or more types of curing agents may be mixed and used.

[0068] The inorganic filler may include aluminum oxide and nitride, and the nitride may be included in the inorganic filler at 55 to 95 wt%, more preferably 60 to 80 wt%. When the nitride is included in such a numerical range, the thermal conductivity and bonding strength can be increased. Here, the nitride may include at least one of boron nitride and aluminum nitride. Here, the boron nitride may be plate-like boron nitride or a boron nitride aggregate in which the plate-like boron nitride is solidified, and the surface of the boron nitride may be coated with a polymer resin. Here, any polymer resin may be used as long as it can be bonded to boron nitride or can coat the surface of boron nitride. The polymer resin may be selected from the group consisting of, for example, an acrylic polymer resin, an epoxy polymer resin, a urethane polymer resin, a polyamide polymer resin, a polyethylene polymer resin, an EVA (ethylene vinyl acetate copolymer) polymer resin, a polyester polymer resin, and a PVC (polyvinyl chloride) polymer resin. And, the polymer resin may be a polymer resin having the following unit 1.

[0069] Unit 1 is as follows:

[0070] Unit 1

[0071] JPEG0007587509000002.jpg73169

[0072] Here, R 1 , R 2 , R 3 and R 4 one of R is H and the rest are selected from the group consisting of C1-C3 alkyl, C2-C3 alkene, and C2-C3 alkyne; 5 can be a linear, branched, or cyclic divalent organic linker having 1 to 12 carbon atoms.

[0073] In one embodiment, R 1 , R 2 , R 3 and R 4 Among these, one of the remaining excluding H may be selected from C2-C3 alkenes, and the other and further other may be selected from C1-C3 alkyls. For example, the polymer resin according to the embodiment of the present invention may include the following unit 2.

[0074] Unit 2

[0075] JPEG0007587509000003.jpg55131

[0076] or the above R 1 , R 2 , R 3 and R 4 The remainders excluding H may be selected differently from the group consisting of C1-C3 alkyl, C2-C3 alkene, and C2-C3 alkyne.

[0077] In this way, when the polymer resin made of unit 1 or unit 2 is coated on boron nitride, the functional group can be easily formed, and when the functional group is formed on the boron nitride, the affinity with the resin can be increased.

[0078] In this manner, when the first resin layer 120 is disposed between the first metal substrate 110 and the plurality of first electrodes 130, heat transfer between the first metal substrate 110 and the plurality of first electrodes 130 is possible without a separate ceramic substrate, and a separate adhesive or physical fastening means is not required due to the adhesiveness of the first resin layer 120 itself. In particular, since the first resin layer 120 can be implemented with a significantly thinner thickness than an existing ceramic substrate, it is possible to improve the heat transfer performance between the plurality of first electrodes 130 and the first metal substrate 110 and reduce the overall size of the thermoelectric device.

[0079] A plurality of first electrodes 130 are disposed on the first resin layer 120. A plurality of P-type thermoelectric legs 140 and a plurality of N-type thermoelectric legs 150 are disposed on the first electrodes 130. At this time, the first electrodes 130 are electrically connected to the P-type thermoelectric legs 140 and the N-type thermoelectric legs 150. Here, the first electrodes 130 may include at least one of copper (Cu), aluminum (Al), silver (Ag), and nickel (Ni).

[0080] The plurality of P-type thermoelectric legs 140 and the plurality of N-type thermoelectric legs 150 are disposed on the first electrode 130. At this time, the P-type thermoelectric legs 140 and the N-type thermoelectric legs 150 may be joined to the first electrode 130 by soldering.

[0081] In this case, the P-type thermoelectric leg 140 and the N-type thermoelectric leg 150 may be bismuth telluride (Bi-Te)-based thermoelectric legs containing bismuth (Bi) and tellurium (Te) as main raw materials. The P-type thermoelectric leg 140 may be a thermoelectric leg containing bismuth telluride (Bi-Te)-based main raw material material containing at least one of antimony (Sb), nickel (Ni), aluminum (Al), copper (Cu), silver (Ag), lead (Pb), boron (B), gallium (Ga), tellurium (Te), bismuth (Bi) and indium (In) at 99 to 99.999 wt% and a mixture containing Bi or Te at 0.001 to 1 wt% of the total weight, based on 100 wt% of the total weight. For example, the main raw material may be Bi-Se-Te, and Bi or Te may be further contained at 0.001 to 1 wt% of the total weight. The N-type thermoelectric leg 150 may be a thermoelectric leg containing 99 to 99.999 wt% of a bismuth telluride (Bi-Te)-based main raw material containing at least one of selenium (Se), nickel (Ni), aluminum (Al), copper (Cu), silver (Ag), lead (Pb), boron (B), gallium (Ga), tellurium (Te), bismuth (Bi), and indium (In) and 0.001 to 1 wt% of a mixture containing Bi or Te, based on a total weight of 100 wt%. For example, the main raw material may be Bi-Sb-Te, and Bi or Te may be further contained at 0.001 to 1 wt% of the total weight.

[0082] The P-type thermoelectric leg 140 and the N-type thermoelectric leg 150 may be formed in a bulk type or a stacked type. In general, the bulk type P-type thermoelectric leg 140 or the bulk type N-type thermoelectric leg 150 may be obtained by a process of heat-treating a thermoelectric material to produce an ingot, pulverizing and sieving the ingot to obtain a powder for the thermoelectric leg, sintering the powder, and cutting the sintered body. The stacked type P-type thermoelectric leg 140 or the stacked type N-type thermoelectric leg 150 may be obtained by a process of applying a paste containing a thermoelectric material onto a sheet-shaped substrate to form unit members, and then stacking and cutting the unit members.

[0083] In this case, the pair of P-type thermoelectric legs 140 and N-type thermoelectric legs 150 may have the same shape and volume or may have different shapes and volumes. For example, since the electrical conduction characteristics of the P-type thermoelectric legs 140 and the N-type thermoelectric legs 150 are different, the height or cross-sectional area of ​​the N-type thermoelectric legs 150 may be formed to be different from the height or cross-sectional area of ​​the P-type thermoelectric legs 140.

[0084] The performance of the thermoelectric device according to an embodiment of the present invention may be expressed by a thermoelectric figure of merit (ZT). The thermoelectric figure of merit (ZT) may be expressed as Equation 2.

[0085] JPEG0007587509000004.jpg14134

[0086] where α is the Seebeck coefficient [V / K], σ is the electrical conductivity [S / m], and α 2 σ is the power factor ([W / mK 2 ]), where T is temperature and k is thermal conductivity [W / mK]. k can be expressed as acpρ, and a is thermal diffusivity [cm 2 / S], cp is the specific heat [J / gK], and ρ is the density [g / cm 3 ].

[0087] To obtain the thermoelectric figure of merit of a thermoelectric element, a Z meter is used to measure the Z value (V / K), and the measured Z value can be used to calculate the thermoelectric figure of merit (ZT).

[0088] The P-type thermoelectric leg 140 or the N-type thermoelectric leg 150 may have a cylindrical shape, a polygonal column shape, an elliptical column shape, or the like. Alternatively, the P-type thermoelectric leg 140 or the N-type thermoelectric leg 150 may have a laminated structure. For example, the P-type thermoelectric leg or the N-type thermoelectric leg may be formed by laminating a plurality of structures in which a semiconductor material is applied to a sheet-like substrate, and then cutting the laminated structures. Accordingly, it is possible to prevent loss of material and improve electrical conductivity characteristics. Alternatively, the P-type thermoelectric leg 140 or the N-type thermoelectric leg 150 may be manufactured by a zone melting method or a powder sintering method. According to the zone melting method, an ingot is manufactured using a thermoelectric material, and then the ingot is slowly heated to refine the ingot so that the particles are rearranged in a single direction, and then slowly cooled to obtain a thermoelectric leg. According to the powder sintering method, an ingot is manufactured using a thermoelectric material, and then the ingot is crushed and sieved to obtain powder for the thermoelectric legs, which is then sintered to obtain the thermoelectric legs.

[0089] The plurality of second electrodes 160 are disposed on the plurality of P-type thermoelectric legs 140 and the plurality of N-type thermoelectric legs 150. At this time, the P-type thermoelectric legs 140 and the N-type thermoelectric legs 150 may be joined to the second electrodes 160 by soldering. At this time, if a shear stress is applied to the soldered portion, a crack may be formed in the soldered portion. Here, the second electrodes 160 may include at least one of copper (Cu), aluminum (Al), silver (Ag), and nickel (Ni).

[0090] The second resin layer 170 is disposed on the plurality of second electrodes 160. Then, the second metal substrate 180 is disposed on the second resin layer 170. The second resin layer 170 may be formed with an area smaller than that of the second metal substrate 180. Therefore, the second resin layer 170 may be disposed within a region spaced a predetermined distance from an edge of the second metal substrate 180.

[0091] In this case, the first resin layer 120 and the second resin layer 170 may be formed to have different sizes. For example, the volume, thickness or area of ​​one of the first resin layer 120 and the second resin layer 170 may be formed to be larger than the volume, thickness or area of ​​the other one. When the temperature of the second metal substrate 180 region is higher than the temperature of the first metal substrate 110 region in the Peltier or Seebeck element, the bonding strength between the second resin layer 170 and the plurality of second electrodes 160 or the second metal substrate 180 in direct contact therewith may be lower than the bonding strength between the first resin layer 120 and the plurality of first electrodes 130 or the first metal substrate 110 in direct contact therewith. The bonding strength between the first resin layer 120 and the plurality of first electrodes 130 or the first metal substrate 110 is 5 kgf / mm 2 It may be more than 10 kgf / mm 2 More preferably, 15 kgf / mm 2 In contrast, the bonding strength between the second resin layer 170 and the second electrodes 160 or the second metal substrate 180 is 1 kgf / mm 2 The bond strength may be as follows:

[0092] In this case, the thickness T2 of the second resin layer may be equal to or greater than the thickness T1 of the first resin layer. Preferably, the thickness T1 of the first resin layer 120 is about 40 μm, and the thickness T2 of the second resin layer 170 may be 40 to 200 μm. That is, the ratio of the thickness T2 of the second resin layer 170 to the thickness T1 of the first resin layer 120 may be 1 to 5.

[0093] The second resin layer 170 may transfer heat generated in the P-type thermoelectric leg 140 and the N-type thermoelectric leg 150 to the second metal substrate 180, or transfer external heat acquired from the second metal substrate 180 to the P-type thermoelectric leg 140 and the N-type thermoelectric leg 150, and may prevent current from passing between the second metal substrate 180 and the second electrode 160. To this end, the second resin layer 170 may have a relatively high insulating property in a portion adjacent to the second electrode 160, and a relatively high thermal conductivity in a portion adjacent to the second metal substrate 180. In this specification, insulating property may mean electrical resistance. For example, high insulating property may be interpreted as high electrical resistance. In addition, the first metal substrate 110 and the second metal substrate 180 are illustrated as being integrally formed with the heat dissipation fins 115, 185, respectively, but are not limited thereto, and at least one of the first metal substrate 110 and the second metal substrate 180 may omit the heat dissipation fins or may not be integrally formed with the heat dissipation fins in consideration of thermal characteristics. In particular, the first metal substrate 110 may be in contact with a low temperature region without the first heat dissipation fins 115, and the second metal substrate 180 may be in contact with a high temperature region without being integrally formed with the second heat dissipation fins 185, and may be bonded with a separate heat dissipation fin and disposed therein.

[0094] FIG. 7 is a partially enlarged view of a thermoelectric element according to an embodiment of the present invention.

[0095] Referring to FIG. 7, the second resin layer 170 includes a first layer 171 and a second layer 172 .

[0096] The first layer 171 is in direct contact with the second electrode 160. The first layer 171 has an insulating property and serves to block the current flowing through the second electrode 160 from being transmitted to the second metal substrate 180. To this end, the first layer 171 may include a matrix resin and an insulating filler. Here, the matrix resin may include polydimethylsiloxane (PDMS). Also, the insulating filler may include ceramic powder such as aluminum oxide, aluminum nitride, boron nitride, etc. Preferably, the ceramic powder may be included at 50 to 99 wt %. More preferably, the aluminum oxide powder may be included at 50 to 99 wt %. In this case, the thermal conductivity of the first layer 171 may be 1.5 to 3.5 W / mK.

[0097] The second layer 172 is disposed on the first layer 171 and is in direct contact with the second metal substrate 180. The second layer 172 is in direct contact with the first layer 171. At this time, the second layer 172 has conductivity and transfers heat generated in the P-type thermoelectric leg 140 and the N-type thermoelectric leg 150 to the second metal substrate 180 and transfers external heat acquired from the second metal substrate 180 to the P-type thermoelectric leg 140 and the N-type thermoelectric leg 150.

[0098] The second layer 172 may include a matrix resin and a conductive filler. Here, the matrix resin may include a silicone resin, for example, polydimethylsiloxane (PDMS). At this time, the matrix resin applied to the second layer 172 is preferably the same as the matrix resin applied to the first layer 171. Also, the conductive filler may include a metal powder such as a silver (Ag)-based, gold (Au)-based, or aluminum (Al)-based metal powder. Preferably, the metal powder may be included at 50 to 99 wt %. More preferably, the silver (Ag)-based metal powder may be included at 50 to 99 wt %. At this time, the thermal conductivity of the second layer 172 may be 6.0 to 10.0 W / mK.

[0099] Here, the first layer 171 and the second layer 172 may have adhesive or adhesive properties.

[0100] The thickness t1 of the first layer 171 may be about 40 to 100 μm. If the thickness t1 of the first layer 171 is less than 40 μm, insulation is not ensured, which may lead to a risk of electrical conduction, and if the thickness t2 of the first layer 171 is greater than 40 μm, the thermal conductivity may decrease, which may degrade the power generation performance of the thermoelectric element. The thickness t2 of the second layer 172 may be 40 to 200 μm. That is, the ratio of the thickness t2 of the second layer 172 to the thickness t1 of the first layer 171 may be 0.2 to 2.5.

[0101] The second metal substrate 180 is disposed on the second resin layer 170 facing the first metal substrate 110. The second metal substrate 180 may be made of aluminum, an aluminum alloy, copper, or a copper alloy. In particular, the second metal substrate 180 may be made of aluminum. In this case, the second metal substrate 180 may be disposed in a high temperature region for power generation, or the second metal substrate 180 may be used as a high temperature part due to the Peltier effect by applying a current to the thermoelectric element.

[0102] In this case, the second metal substrate 180 may have a surface roughness formed on the entirety or part of the surface on which the second resin layer 170 is disposed, that is, the surface of the first metal substrate 180 facing the second resin layer 170 .

[0103] Here, the area of ​​the first metal substrate 110 and the second metal substrate 180 may be 40 mm×40 mm to 200 mm×200 mm, and the thickness may be 1 to 100 mm. In this case, the area or thickness of the first metal substrate 110 and the second metal substrate 180 may be the same or different from each other.

[0104] FIG. 8 is a diagram illustrating a state in which the thermoelectric device according to the first embodiment of the present invention is generating electricity.

[0105] Referring to FIG. 8, when the second metal substrate 180 of the thermoelectric element is placed in a high temperature region and the first metal substrate 110 is placed in a low temperature region, electricity is generated by the movement of electrons between a plurality of thermoelectric legs connected in series by the Seebeck effect. At this time, the second metal substrate 180 exposed to high temperature may expand in volume due to heat. At this time, the horizontal expansion of the second metal substrate 180 may apply a shear stress to the second resin layer 170. The shear stress may be transferred to the soldered portion of the second electrode 160, causing cracks in the soldered portion and reducing durability at high temperatures. At this time, the thermoelectric element according to the embodiment may ensure the thickness of the second resin layer 170, alleviating the shear stress transferred to the soldered joint portion and ensuring durability at high temperatures. At this time, the width of the second resin layer 170 may increase in the horizontal direction with respect to the second metal substrate 180 as it approaches the second metal substrate 180. Meanwhile, although not shown, the same can be applied to thermal expansion that occurs when the second metal substrate 180 operates at a high temperature due to the Peltier effect when a voltage is applied to the thermoelectric element.

[0106] 5 and 6 again, the sealing means 190 may be disposed on a side of the first resin layer 120 and a side of the second resin layer 170. That is, the sealing means 190 may be disposed between the first metal substrate 110 and the second metal substrate 180, and may be disposed to surround a side of the first resin layer 120, an outermost portion of the plurality of first electrodes 130, an outermost portion of the plurality of P-type thermoelectric legs 140 and the plurality of N-type thermoelectric legs 150, an outermost portion of the plurality of second electrodes 160, and a side of the second resin layer 170. Accordingly, the first resin layer 120, the plurality of first electrodes 130, the plurality of P-type thermoelectric legs 140, the plurality of N-type thermoelectric legs 150, the plurality of second electrodes 160, and the second resin layer may be sealed from external moisture, heat, contamination, and the like.

[0107] Here, the sealing means 190 may include a sealing case 192 disposed at a predetermined distance from the side of the first resin layer 120, the outermost periphery of the plurality of first electrodes 130, the outermost periphery of the plurality of P-type thermoelectric legs 140 and the plurality of N-type thermoelectric legs 150, the outermost periphery of the plurality of second electrodes 160, and the side of the second resin layer 170, a sealant 194 disposed between the sealing case 192 and the second metal substrate 180, and a sealant 196 disposed between the sealing case 192 and the first metal substrate 110. In this manner, the sealing case 192 may contact the first metal substrate 110 and the second metal substrate 180 through the sealants 194 and 196. Accordingly, when the sealing case 192 directly contacts the first metal substrate 110 and the second metal substrate 180, heat conduction occurs through the sealing case 192, which may prevent a problem of a decrease in ΔT.

[0108] Here, the sealant (194, 196) may include at least one of epoxy resin and silicone resin, or may include a tape coated with at least one of epoxy resin and silicone resin on both sides. The sealant (194, 196) serves to make the gap between the sealing case (192) and the first metal substrate (110) and between the sealing case (192) and the second metal substrate (180) airtight, and may enhance the sealing effect of the first resin layer (120), the plurality of first electrodes (130), the plurality of P-type thermoelectric legs (140), the plurality of N-type thermoelectric legs (150), the plurality of second electrodes (160), and the second resin layer (170), and may be used in combination with a finishing material, a finishing layer, a waterproofing material, a waterproofing layer, etc.

[0109] Meanwhile, a guide groove G for leading out the wires W1 and W2 connected to the electrodes may be formed in the sealing case 192. For this purpose, the sealing case 192 may be an injection-molded product made of plastic or the like, and may be used together with a sealing cover.

[0110] Although the structure of the sealing means 190 is specifically illustrated, this is merely an example and the sealing means 190 may be modified in various ways.

[0111] Although not shown, insulation may further be included surrounding the sealing means 190. Alternatively, the sealing means 190 may include an insulating component.

[0112] FIG. 9 is a cross-sectional view of a thermoelectric element according to a second embodiment of the present invention, FIG. 10 is an enlarged partial view of FIG. 9, and FIG. 11 is a view showing the state in which power is applied to the thermoelectric element according to the second embodiment of the present invention.

[0113] According to another embodiment of the present invention, the second resin layer 200 may include a plurality of layers, which may be at least three layers and may be in direct contact with each other. In this case, the number of layers included in the second resin layer 200 may be variable.

[0114] 9 and 10, the second resin layer 200 includes first to fourth layers 201, 202, 203, and 204. At this time, the first to fourth layers 201, 202, 203, and 204 are made of different materials. Also, the first to fourth layers 201, 202, 203, and 204 may have different thermal conductivities. The first to fourth layers 201, 202, 203, and 204 are arranged in order of increasing thermal conductivity from the first metal substrate 110 to the second metal substrate 180.

[0115] The first to fourth layers 201, 202, 203, and 204 may include a matrix resin and a conductive filler or an insulating filler. Here, the matrix resin may include a silicone resin, for example, polydimethylsiloxane (PDMS). At this time, the content of the conductive filler or the insulating filler included in the first to fourth layers 201, 202, 203, and 204 may be different from each other.

[0116] 11, when the second metal substrate 180 of the thermoelectric element is placed in a high temperature region and the first metal substrate 110 is placed in a low temperature region, electricity is generated by the movement of electrons between a plurality of thermoelectric legs connected in series due to the Seebeck effect. At this time, the volume of the second metal substrate 180 exposed to high temperature may expand due to heat. At this time, a shear stress may be applied to the second resin layer 200 due to the horizontal expansion of the second metal substrate 180. At this time, the width of the second resin layer 200 may increase in the horizontal direction of the second metal substrate 180 from the first layer 211 to the fourth layer 214. Although not shown, the same can be applied to the thermal expansion that occurs when the second metal substrate 180 operates at a high temperature due to the Peltier effect when a voltage is applied to the thermoelectric element.

[0117] Hereinafter, the present invention will be described in more detail with reference to thermoelectric elements according to examples and comparative examples. These examples are presented only as examples to describe the present invention in more detail. Therefore, the present invention is not limited to these examples.

[0118] Both the thermoelectric element according to the comparative example and the thermoelectric element according to the example are measurement results in an environment where a temperature of 35°C was applied to the first metal substrate area and 200°C was applied to the second metal substrate area of ​​a 40mm x 40mm power generating thermoelectric element including a first metal substrate, a first resin layer, a plurality of first electrodes, a plurality of P-type thermoelectric legs, a plurality of N-type thermoelectric legs, a plurality of second electrodes, a second resin layer, and a second metal substrate as shown in FIG. 1. In the thermoelectric element according to the comparative example, the second resin layer was formed entirely of an insulating resin agent, and in the thermoelectric element according to the example, the second resin layer was made of a first layer and a second layer, the first layer having insulating properties, and the second layer having conductive properties. At this time, the thickness of the first layer was fixed at 40 μm, and the thickness of the second layer was changed to measure the power generation amount and the power generation amount reduction rate of the thermoelectric element.

[0119] [Table 1]

[0120] Referring to Table 1, it can be seen that the thermoelectric element according to the comparative example reduces the amount of power generation and increases the rate of decrease in the amount of power generation as the thickness of the second resin layer increases. On the other hand, the thermoelectric element according to the embodiment reduces the amount of power generation somewhat and increases the rate of decrease in the amount of power generation as the thickness of the second resin layer increases, but the decrease in the amount of power generation is significantly smaller than that of the comparative example. In other words, the thermoelectric element according to the embodiment can ensure sufficient power generation performance without a significant decrease in thermal conductivity even when the thickness of the second resin layer is increased to relieve thermal stress.

[0121] Another embodiment of the present invention will be described below with reference to Figures 12 to 14. The thermoelectric element according to this embodiment is substantially the same as the thermoelectric element of Figures 1 to 6 except for the second resin layer. Therefore, the same components as those in the thermoelectric element of Figures 1 to 6 are denoted by the same reference numerals and duplicated descriptions will be omitted.

[0122] FIG. 12 is a cross-sectional view of a thermoelectric element according to a third embodiment of the present invention, FIG. 13 is a partially enlarged view of a thermoelectric element according to the third embodiment of the present invention, and FIG. 14 is a view illustrating the state in which the thermoelectric element according to the third embodiment of the present invention is generating electricity.

[0123] 12 and 13, the second resin layer 210 includes a first layer 211, a second layer 212, and a polyimide layer 213. At this time, the first layer 211 and the second layer 212 may have adhesiveness. For example, the second resin layer may be a polyimide layer having adhesive layers formed on both sides thereof.

[0124] Here, the area of ​​the first metal substrate 110 and the second metal substrate 180 may be 40 mm×40 mm to 200 mm×200 mm, and the thickness may be 1 to 100 mm. In this case, the area or thickness of the first metal substrate 110 and the second metal substrate 180 may be the same or different from each other.

[0125] The first layer 211 is in direct contact with the second electrode 160. More preferably, the first layer 211 may be a polysiloxan-based adhesive. At this time, the bonding strength of the first layer 211 decreases as the exposure temperature increases. That is, as the exposure temperature increases, the fluidity increases and the portion bonded to the second electrode 160 may fluidly deform. Therefore, even if a shear stress is applied to the first layer 211, the portion bonded to the second electrode 160 is fluidly pressed, thereby blocking the transfer of the shear stress to the second electrode 160. At this time, the first layer 211 has a bonding strength of 1 kgf / mm at a temperature of 150 to 200°C. 2 Preferably, the first layer 211 has a bonding strength of 0.5 kgf / mm at a temperature of 150 to 200° C. 2 More preferably, the first layer 211 has a bonding strength of 0.1 kgf / mm at a temperature of 150 to 200° C. 2 The bond strength may be as follows:

[0126] The second layer 212 is laminated at a distance from the first layer 211 and is in direct contact with the second metal substrate 180. More preferably, the second layer 212 may be a polysiloxan-based adhesive. At this time, the bonding strength of the second layer 212 decreases as the exposure temperature increases. That is, as the exposure temperature increases, the fluidity increases and the portion bonded to the second metal substrate 180 may fluidly deform. Therefore, even if the second metal substrate 180 expands at high temperatures, the portion bonded to the second metal substrate 180 may be fluidly pressed, thereby preventing shear stress from being applied from the second metal substrate 180. At this time, the second layer 212 has a compressive strength of 1 kgf / mm at a temperature of 150 to 200°C. 2 Preferably, the second layer 212 has a bonding strength of 0.5 kgf / mm at a temperature of 150 to 200° C. 2 More preferably, the second layer 212 has a bonding strength of 0.1 kgf / mm at a temperature of 150 to 200° C. 2 The bond strength may be as follows:

[0127] The bond strength of the second layer 212 may be the same as or greater than the bond strength of the first layer 211 .

[0128] The polyimide layer 213 is laminated between the first layer 211 and the second layer 212. At this time, one surface of the polyimide layer 213 contacts the upper surface of the first layer 211, and the other surface contacts the lower surface of the second layer 212. The polyimide layer 213 has insulating properties and blocks the current of the second electrode 160 from being transmitted to the second metal substrate 180. The polyimide layer 213 may be a polyimide-based material. At this time, an insulating layer containing other insulating materials may be disposed instead of the polyimide layer. Meanwhile, the thickness t1 of the polyimide layer 213 may be 1 to 500 μm. As the thickness t1 of the polyimide layer 213 increases, the thermal conductivity and thermoelectric breakdown voltage of the polyimide layer 213 decrease, so the risk of current flow decreases. On the other hand, as the thickness t1 of the polyimide layer 213 increases, the thermal conductivity decreases, so the power generation performance tends to decrease.

[0129] Table 2 below shows the dielectric breakdown voltage, thermal conductivity and thermal conductivity according to the thickness of the polyimide layer.

[0130] [Table 2]

[0131] From Table 2, the thickness of the polyimide layer 213 may be about 5 um. At this time, it can be seen that as the thickness of the polyimide layer increases, the dielectric breakdown voltage increases and the thermal conductivity and thermal conductivity decrease. At this time, the dielectric breakdown voltage required for the thermoelectric element is less than 1 kV, and when the polyimide layer is formed to a thickness of about 5 um, high thermal conductivity can be ensured without being damaged by overload.

[0132] Hereinafter, the present invention will be described in more detail with reference to Table 3 and FIG. 18 through thermoelectric elements according to examples and comparative examples. These examples are merely presented as examples to describe the present invention in more detail. Therefore, the present invention is not limited to these examples. Table 3 below shows the measurement results of the temperature cycle test of the examples and comparative examples, and FIG. 18 is a graph showing the resistance change rate versus the number of cycles in the temperature cycle test of the examples and comparative examples.

[0133] Both the thermoelectric element according to the comparative example and the thermoelectric element according to the embodiment are power-generating thermoelectric elements measuring 40 mm x 40 mm, including a first metal substrate, a first resin layer, a plurality of first electrodes, a plurality of P-type thermoelectric legs, a plurality of N-type thermoelectric legs, a plurality of second electrodes, a second resin layer, and a second metal substrate. The thermoelectric element according to the comparative example has the first resin layer and the second resin layer all of which are rated at 5 kgf / mm 2 The thermoelectric element according to the embodiment is formed of a resin having a bonding strength of 5 kgf / mm 2 It was formed using a resin agent having the above bonding strength, and the second resin layer was arranged using a polyimide film with a polysiloxane adhesive layer formed on both sides.

[0134] The temperature cycle test was performed a total of 5,000 cycles, with one cycle consisting of a heating step in which the temperature of the second metal substrate was changed from 50°C to 180°C and one cooling step in which the temperature was changed from 180°C to 50°C, while the temperature of the first metal substrate was maintained at 25°C. The heating rate in the heating step was 30°C / min, and the cooling rate in the cooling step was 22°C / min.

[0135] [Table 3]

[0136] 18, it was confirmed that the thermoelectric element according to the comparative example had a rapid increase in resistance and a rapid decrease in power generation from 0 to 200 cycles, and that the thermoelectric element was destroyed after 200 cycles. In contrast, the thermoelectric element according to the embodiment had a resistance change rate of within 5% over 5000 cycles, and the power generation amount increased. It was also confirmed that the thermoelectric element was not destroyed while maintaining 5000 cycles. In other words, it can be seen that the thermoelectric element according to the embodiment has stronger product durability against thermal changes and has excellent power generation performance at high temperatures compared to the thermoelectric element according to the comparative example.

[0137] Referring to FIG. 14, when the second metal substrate 180 of the thermoelectric element is placed in a high temperature region and the first metal substrate 110 is placed in a low temperature region, electricity is generated by the movement of electrons between a plurality of thermoelectric legs connected in series by the Seebeck effect. At this time, the volume of the second metal substrate 180 exposed to high temperature may expand due to heat. At this time, the horizontal expansion of the second metal substrate 180 may apply a shear stress to the second resin layer 210. The shear stress may be transferred to the soldering portion of the second electrode 160, causing cracks in the soldering portion and reducing durability at high temperatures. At this time, the thermoelectric element according to the embodiment is embodied such that the second resin layer 210 is fluidly pressed against the second metal substrate 180 even when the second metal substrate 180 expands at high temperatures, thereby mitigating the shear stress transferred to the soldering portion and ensuring the high temperature durability of the thermoelectric element. Although not shown, the same can be applied to thermal expansion that occurs when the second metal substrate 180 operates at a high temperature due to the Peltier effect when a voltage is applied to the thermoelectric element.

[0138] Hereinafter, a fourth embodiment of the present invention will be described with reference to Figures 15 to 17. The thermoelectric element according to this embodiment is substantially the same as the thermoelectric element in Figures 12 to 14 except for the second resin layer. Therefore, the same components as those in the thermoelectric elements in Figures 12 to 14 are denoted by the same reference numerals and duplicated descriptions will be omitted.

[0139] FIG. 15 is a cross-sectional view of a thermoelectric element according to a fourth embodiment of the present invention, FIG. 16 is an enlarged partial view of FIG. 15, and FIG. 17 is a view showing the state in which power is applied to the thermoelectric element according to the fourth embodiment of the present invention.

[0140] 15 and 16, the second resin layer 220 may include a plurality of layers and a polyimide layer. At this time, the number of layers is at least three, and the plurality of layers may be in contact with each other or with the polyimide layer 225. At this time, the number of layers included in the second resin layer 220 is variable.

[0141] The second resin layer 220 includes first to fourth layers 221, 222, 223, and 224, and at this time, the first to fourth layers 221, 222, 223, and 224 are made of different materials. Also, the first to fourth layers 221, 222, 223, and 224 may have different thermal conductivities. And, the first to fourth layers 221, 222, 223, and 224 are arranged in order of increasing thermal conductivity from the first metal substrate 110 to the second metal substrate 180. At this time, the first layer 221, which is in direct contact with the second electrode 160 and the second metal substrate 180, and the fourth layer 224 may have adhesiveness.

[0142] The polyimide layer 225 is disposed at any one of the first to fourth layers 221, 222, 223, and 224. In the drawing, the polyimide layer 225 is disposed between the second layer 222 and the third layer 223, but the polyimide layer 225 may be disposed at another position among the first to fourth layers 221, 222, 223, and 224. At this time, the polyimide layer 225 is made of an insulating material and blocks the current of the second electrode 160 from being transmitted to the second metal substrate 180. The polyimide layer 225 is more advantageous in blocking the current when it is disposed adjacent to the second electrode 160, but is not limited thereto. At this time, the polyimide layer 225 may be made of a polyimide-based material. The thickness of the polyimide layer 225 may be 1 to 500 μm, for example, the thickness of the polyimide layer 225 may be about 5 μm.

[0143] The thermoelectric element according to the embodiment of the present invention may be used in power generation devices, cooling devices, heating devices, etc. In particular, the thermoelectric element according to the embodiment of the present invention may be mainly applied to optical communication modules, sensors, medical devices, measuring devices, the aerospace industry, refrigerators, chillers, automobile ventilation seats, cup holders, washing machines, dryers, wine cellars, water purifiers, power supply devices for sensors, thermopiles, etc.

[0144] Here, an example of a medical device to which the thermoelectric element according to the embodiment of the present invention is applied is a PCR (Polymerase Chain Reaction) device. The PCR device is a device for amplifying DNA to determine the base sequence of the DNA, and requires precise temperature control and thermal cycling. For this purpose, a Peltier-based thermoelectric element can be applied.

[0145] Another example of a medical device to which the thermoelectric element according to the embodiment of the present invention is applied is a photodetector. Here, the photodetector may be an infrared / ultraviolet detector, a CCD (Charge Coupled Device) sensor, an X-ray detector, a TTRS (Thermoelectric Thermal Reference Source), etc. A Peltier-based thermoelectric element may be applied to cool the photodetector. As a result, it is possible to prevent changes in wavelength, a decrease in output, and a decrease in resolution caused by an increase in temperature inside the photodetector.

[0146] Further examples of applications of the thermoelectric device according to the embodiment of the present invention to medical devices include the immunoassay field, in vitro diagnostics field, general temperature control and cooling systems, physical therapy field, liquid chiller systems, blood / plasma temperature control field, etc. Accordingly, precise temperature control is possible.

[0147] Another example of a medical device to which the thermoelectric element according to the embodiment of the present invention is applied is an artificial heart, which can be used to supply power to the artificial heart.

[0148] Examples of applications of the thermoelectric element according to the embodiment of the present invention in the aerospace industry include star tracking systems, thermal imaging cameras, infrared / ultraviolet detectors, CCD sensors, Hubble Space Telescope, TTRS, etc. Accordingly, the temperature of the image sensor can be maintained.

[0149] Other examples of applications of thermoelectric devices according to embodiments of the present invention in the aerospace industry include cooling devices, heaters, and power generation devices.

[0150] In addition, the thermoelectric device according to the embodiment of the present invention may be applied to other industrial fields for power generation, cooling, and heating.

[0151] Although the present invention has been described above with reference to preferred embodiments, it will be understood by those skilled in the art that various modifications and variations of the present invention may be made without departing from the spirit and scope of the present invention as set forth in the following claims.

[0152] [Explanation of symbols] 110: First metal substrate 120: 1st resin layer 130: 1st electrode 140: P-type thermoelectric leg 150: N-type thermoelectric leg 160: 2nd electrode 180: Second metal substrate 190: Sealing means 170, 200, 210, 220: 2nd resin layer 171, 201, 211, 221: 1st layer 172, 202, 212, 222: Second layer 203, 223: 3rd layer 204, 224: 4th layer

Claims

1. A first metal substrate; a first resin layer disposed on the first metal substrate; a plurality of first electrodes disposed on the first resin layer; a plurality of P-type thermoelectric legs and a plurality of N-type thermoelectric legs disposed on the plurality of first electrodes; a plurality of second electrodes disposed on the plurality of P-type thermoelectric legs and the plurality of N-type thermoelectric legs; a second resin layer disposed on the plurality of second electrodes; and a second metal substrate disposed on the second resin layer; The first metal substrate is a low temperature part and the second metal substrate is a high temperature part, the second resin layer includes a first layer in direct contact with the second electrodes and a second layer disposed on the first layer in direct contact with the second metal substrate; the first layer and the second layer contain a silicon (Si)-based resin; The bonding strength of the first resin layer is higher than the bonding strength of the second resin layer, a ratio of a thickness of the second layer to a thickness of the first layer is between 0.2 and 2.5; the first layer includes polydimethylsiloxane (PDMS) and aluminum oxide; the second layer includes polydimethylsiloxane (PDMS) and silver (Ag); the thermal conductivity of the first layer is lower than the thermal conductivity of the second layer; or A thermoelectric element, wherein the first layer has a higher electrical resistance than the second layer.

2. The thermoelectric element of claim 1 , wherein at least one of the first metal substrate and the second metal substrate comprises aluminum.

3. The thermoelectric element according to claim 1 , wherein the thickness of the second resin layer is greater than or equal to the thickness of the first resin layer.

4. 4. The thermoelectric element according to claim 3, wherein a ratio of the thickness of the second resin layer to the thickness of the first resin layer is 1-5.

5. 2. The thermoelectric element according to claim 1, wherein the first layer has a thermal conductivity of 1.5 to 3.5 W / mK, and the second layer has a thermal conductivity of 6.0 to 10.0 W / mK.

6. The thermoelectric element according to claim 3 , further comprising a polyimide layer disposed between the first layer and the second layer, the first layer and the second layer comprising a polysiloxane-based resin.

7. The first layer and the second layer have a resistance of 1 kgf / mm at a temperature of 150 to 200° C. 2 The thermoelectric element according to claim 6 , having a bonding strength of:

8. The thermoelectric element of claim 6 , further comprising a third layer between the first layer and the polyimide layer.

9. The thermoelectric element of claim 8 , further comprising a fourth layer between the second layer and the polyimide layer.

10. The thermoelectric element according to claim 9 , wherein the thermal conductivity of each of the first to fourth layers increases toward the second metal substrate.

11. The thermoelectric element according to claim 2 , wherein at least one of the first metal substrate and the second metal substrate includes copper (Cu).

Citation Information

Patent Citations

  • Thermoelectric cooling device

    JP1994174329A

  • Peltier element system

    JP1996293627A

  • Temperature regulator and its manufacture

    JP2000214934A

  • Heat exchanger and method of manufacturing the same

    JP2006234362A