Methods for forming Josephson junctions in superconducting qubits

By forming Josephson junctions using a convex structure with oxide-sandwiched superconducting layers, the complexity and environmental sensitivity of traditional qubit fabrication are mitigated, enabling smaller, more coherent superconducting qubits for quantum computing.

JP7592083B2Active Publication Date: 2024-11-29INTERNATIONAL BUSINESS MACHINE CORPORATION
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2022527045
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-11-14
Filing Date
2020-11-13
Publication Date
2024-11-29
Estimated Expiration
2040-11-13

AI Technical Summary

Technical Problem

Traditional methods for forming superconducting qubits are complex, requiring many lithographic steps and result in qubits that are sensitive to far-field and near-field coupling with the external environment, leading to potential interference and size limitations.

Method used

A method involving a substrate with a convex structure and layers of superconducting material, where a portion of oxide material is sandwiched between layers to create a Josephson junction, eliminating the need for electron beam or light beam lithography and reducing environmental coupling.

Benefits of technology

This approach simplifies the fabrication process, reduces qubit size, and minimizes far-field and near-field coupling, resulting in more coherent and compact superconducting qubits suitable for two-dimensional lattice structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007592083000001
    Figure 0007592083000001
  • Figure 0007592083000002
    Figure 0007592083000002
  • Figure 0007592083000003
    Figure 0007592083000003
Patent Text Reader

Abstract

A method for forming a Josephson junction in a superconducting qubit includes providing a substrate having a convex structure with first and second surfaces that meet at an edge, depositing a first layer of superconducting material on the first surface, oxidizing the first layer to form a layer of oxide material on a surface of the first layer, and depositing a second layer of superconducting material on the second surface, wherein a portion of the second layer contacts a portion of the layer of oxide material at or near the edge such that a portion of the layer of oxide material is sandwiched between a portion of the first layer and a portion of the second layer at or near the edge, thereby defining a Josephson junction.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE The presently claimed embodiments of the invention relate to superconducting qubits, and more particularly to methods of forming Josephson junctions in superconducting qubits and superconducting qubit devices.

[0002] Quantum computing is based on reliable control of quantum bits (referred to throughout this specification as qubits). The basic operations required to realize quantum algorithms are a set of single-qubit operations and two-qubit operations that establish correlations between two separate quantum bits. The realization of high-fidelity two-qubit operations can be desirable both to reach error thresholds for quantum computing and to reach reliable quantum simulation.

[0003] A superconducting quantum processor (having one or more superconducting qubits) comprises a superconducting metal (e.g., Al, Nb, etc.) on an insulating substrate (e.g., Si or high resistivity Si, Al2O3, etc.). Superconducting quantum processors are generally planar two-dimensional lattice structures of individual qubits connected by couplers in various lattice symmetries (e.g., square lattice, hexagonal lattice, etc.) and readout structures disposed on a flip chip. The couplers may consist of capacitors, resonators, coils, or any microwave components that provide coupling between the qubits.

[0004] Conventional methods for fabricating superconducting qubits are based on standard Josephson junction fabrication using the Dolan or Manhattan methods to form the bridges. The above methods require many steps, including many lithography steps, and the resulting qubits can be relatively large and therefore sensitive to far-field and / or near-field coupling with the external environment. Summary of the Invention

[0005] An aspect of the invention is to provide a method of forming a Josephson junction in a superconducting qubit. The method includes providing a substrate having a convex structure with a first surface and a second surface where the convex structure meets at an edge, and depositing a first layer of superconducting material on the first surface of the substrate material. The method further includes oxidizing the first layer of superconducting material to form a layer of oxide material on a surface of the first layer of superconducting material, and depositing a second layer of superconducting material on the second surface of the substrate material. A portion of the second layer contacts a portion of the layer of oxide material at or near the edge such that at or near the edge, a portion of the layer of oxide material is sandwiched between a portion of the first layer of superconducting material and a portion of the second layer of superconducting material to define a Josephson junction.

[0006] Another aspect of the invention is to provide a qubit device. The qubit device includes a substrate having a convex structure having a first surface and a second surface that meet at an edge and form an angle therebetween. The qubit device further includes a first layer of superconducting material deposited on the first surface of the substrate material and a layer of oxide material on a surface of the first layer of superconducting material. The qubit device also includes a second layer of superconducting material on the second surface of the substrate material. A portion of the second layer contacts a portion of the layer of oxide material at or near the edge such that at or near the edge, a portion of the layer of oxide material is sandwiched between a portion of the first layer of superconducting material and a portion of the second layer of superconducting material to define a Josephson junction.

[0007] Yet another aspect of the invention is to provide a method of forming a Josephson junction in a superconducting qubit. The method includes providing a substrate, depositing a superconducting material on a surface of the substrate, and depositing a sacrificial material layer on the superconducting material. The method further includes removing a portion of the sacrificial material layer to reveal a portion of the surface of the substrate to define a qubit pocket, and etching the portion of the surface of the substrate to form a convex shape in the substrate, the convex shape having a first surface and a second surface that meet at an edge. The method also includes forming the Josephson junction at or near the edge without applying electron beam or light beam lithography to connect capacitor pads connected to the Josephson junction to a plurality of buses.

[0008] In one embodiment, forming the Josephson junction includes depositing a first layer of superconducting material on a first side of a convex feature in the substrate material, oxidizing the first layer of superconducting material to form a layer of oxide material on a surface of the first layer of superconducting material, and depositing a second layer of superconducting material on a second side of the convex feature in the substrate material, where a portion of the second layer contacts a portion of the layer of oxide material at or near the edge such that a portion of the layer of oxide material is sandwiched between a portion of the first layer of superconducting material and a portion of the second layer of superconducting material at or near the edge to define a Josephson junction.

[0009] In one embodiment, the method further includes defining a plurality of buses and a plurality of readout resonators using lithography and removing a portion of the superconducting material to form the plurality of buses and readout resonators on the substrate, In one embodiment, removing the portion of the sacrificial material layer includes applying a single lithography step.

[0010] The present disclosure, and its method of operation and function of the associated elements of construction and combination of parts and economy of manufacture will become more apparent from a consideration of the following description and appended claims, taken in conjunction with the accompanying drawings, all of which form a part of this specification, and in which like reference numerals indicate corresponding parts in the various views, It is to be expressly understood, however, that the drawings are for the purpose of illustration and description only and are not intended as a definition of the limits of the invention. [Brief description of the drawings]

[0011] [Figure 1] 1 is a schematic side view of a substrate having a layer of superconducting material deposited thereon, in accordance with an embodiment of the present invention; [Diagram 2] 2A shows a schematic top view of a substrate having a layer of superconducting material deposited thereon, with portions of the layer of superconducting material removed, in accordance with an embodiment of the present invention, and FIG. 2B shows a cross-sectional view of a substrate having a layer of superconducting material deposited thereon, taken along line 2B-2B shown in FIG. 2A, in accordance with an embodiment of the present invention. [Diagram 3] FIG. 3A shows a schematic top view of a substrate having a layer of superconducting material and a layer of sacrificial material deposited thereon with portions of the sacrificial material layer removed to reveal a portion of a surface of the substrate 100 defining a qubit pocket, in accordance with an embodiment of the present invention; and FIG. 3B shows a cross-sectional view along line 3B-3B shown in FIG. 3A of a substrate having a layer of superconducting material and a layer of sacrificial material deposited thereon with portions of the sacrificial material layer removed to reveal a portion of a surface of the substrate defining a qubit pocket, in accordance with an embodiment of the present invention. [Figure 4]4A is a schematic diagram showing a top view of a substrate having an exposed portion of its surface that defines a qubit pocket and an undercut when the exposed portion is etched, in accordance with an embodiment of the present invention; FIG. 4B is a cross-sectional view of a substrate having an exposed portion of its surface that defines a qubit pocket and an undercut when the exposed portion is etched, in accordance with an embodiment of the present invention; FIG. 4C is a cross-sectional view of a substrate having an exposed portion of its surface that defines a qubit pocket and an undercut when the exposed portion is etched, in accordance with an embodiment of the present invention; FIG. 4C is a cross-sectional view of a substrate having an exposed portion of its surface that defines a qubit pocket and an undercut when the exposed portion is etched, in accordance with an embodiment of the present invention; FIG. [Diagram 5] 2 is a cross-sectional view of a substrate showing a wedge-shaped structure according to an embodiment of the present invention. [Figure 6] 6A is a top view of a fabricated qubit device including a Josephson junction (JJ), a bus, and a resonator according to an embodiment of the invention, (B) is a cross-sectional view of a fabricated qubit device taken along line 6B-6B in FIG. 6A according to an embodiment of the invention, and (C) is a cross-sectional view of a fabricated qubit device taken along line 6C-6C in FIG. 6A according to an embodiment of the invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] In one embodiment, a method of forming a Josephson junction for a superconducting qubit device is provided herein. In one embodiment, the method includes providing a substrate 100 and depositing a layer 102 of superconducting material on a surface 100S of the substrate 100. FIG. 1 is a schematic side view of the substrate 100 having a layer 102 of superconducting material deposited thereon, according to an embodiment of the present invention. In one embodiment, the substrate 100 can be any non-conducting material, including but not limited to silicon (Si) and sapphire. In one embodiment, the superconducting material 102 can be any superconducting material, including but not limited to niobium (Nb), aluminum (Al), etc.

[0013] The method further includes removing a portion of the superconducting material 102 to reveal a first portion 100A of the surface 100S of the substrate 100 for forming a plurality of buses 202 and read resonators 204 on the substrate. In one embodiment, removing the portion of the layer of superconducting material 102 may be performed by etching the portion of the layer of superconducting material 102 (e.g., using a chemical etch such as an acid etch).

[0014] Figure 2(A) shows a schematic top view of a substrate 100 having a layer of superconducting material 102 deposited thereon with some portions of the layer of superconducting material 102 removed, in accordance with an embodiment of the present invention. Figure 2(B) shows a cross-sectional view of the substrate having a layer of superconducting material 102 deposited thereon, in accordance with an embodiment of the present invention, taken along line 2B-2B shown in Figure 2(A).

[0015] The method further includes depositing a sacrificial material layer 302 over the layer of superconducting material 102 and over the exposed portion 100A of the surface 100S of the substrate 100. The method also includes applying electron beam or light beam lithography to expose a portion of the sacrificial material layer 302, and removing the exposed portion of the sacrificial material layer 302 to expose the portion 100B of the surface 100S of the substrate 100 to define the qubit pocket 304. In one embodiment, removing the exposed portion of the sacrificial material layer 302 includes applying a single lithography step.

[0016] Figure 3(A) shows a schematic top view of a substrate 100 having a layer of superconducting material 102 and a layer of sacrificial material 302 deposited thereon, with the layer of sacrificial material 302 having portions of the layer of sacrificial material 302 removed to reveal a portion 100B of a surface 100S of the substrate 100 defining a qubit pocket 304, in accordance with an embodiment of the present invention. Figure 3(B) shows a cross-sectional view of a substrate 100 having a layer of superconducting material 102 and a layer of sacrificial material 302 deposited thereon, with the layer of sacrificial material 302 having portions of the layer of sacrificial material 302 removed to reveal a portion 100B of a surface 100S of the substrate 100 defining a qubit pocket 304, in accordance with an embodiment of the present invention, taken along line 3B-3B shown in Figure 3(A).

[0017] In one embodiment, depositing the sacrificial material layer 302 on the layer of superconducting material 102 and on the exposed portion 100B of the substrate 100 includes depositing germanium (Ge) on the layer of superconducting material 102 and on the exposed portion 100B of the substrate 100.

[0018] As shown in Figure 3(A), in one embodiment, the exposed portion 102B of the surface 100S of the substrate 100 that defines the pocket 304 has two mirror-symmetric shapes 304A and 304B. As shown in Figure 3(A), the exposed portion 100B of the surface 100S of the substrate 100 has an H-shaped shape. The two mirror-symmetric shapes 304A and 304B face each other and form a relatively narrow strip 304C of the sacrificial material layer 302 at the midline of the two mirror-symmetric shapes 304A and 304B.

[0019] In one embodiment, the method further includes etching portion 100B of surface 100S of substrate 100 to form convex structures 402 in substrate 100 (shown in FIG. 4(C) and FIG. 5). In one embodiment, etching portion 100B includes etching using potassium hydroxide (KOH) or tetramethylammonium hydroxide (TMAH).

[0020] 4(A) shows a schematic top view of substrate 100 with exposed portion 100B of surface 100S of substrate 100 that defines the extent of qubit pocket 304 and undercut 404 upon etching of exposed portion 100B, in accordance with an embodiment of the present invention. In one embodiment, as shown in FIG. 4(A), the extent of undercut 404 formed by etching portion 100B is bounded by a dotted line.

[0021] Figure 4(B) is a cross-sectional view along line 4B-4B shown in Figure 4(A) of substrate 100 with exposed portion 100B of surface 100S of substrate 100 defining the extent of qubit pocket 304 and undercut 404 when etching exposed portion 100B, according to an embodiment of the present invention. Along the 4B-4B cross-sectional view shown in Figure 4(B), sacrificial material layer 302 runs on the top surface of surface 100S of substrate 100, forming a bridge structure 406 across void 408 formed after etching portion 100B of surface 100S of substrate 100.

[0022] Figure 4(C) is a cross-sectional view along line 4C-4C shown in Figure 4(A) of substrate 100 with exposed portion 100B of surface 100S of substrate 100 that defines the extent of qubit pocket 304 and undercut 404 when etching exposed portion 100B, according to an embodiment of the present invention. Along the 4C-4C cross-sectional view shown in Figure 4(C), sacrificial material layer 302 forms a bridge structure 406 that runs over the top of surface 100S of substrate 100 and over the top of convex structure 402 that is formed after etching portion 100B of surface 100S of substrate 100.

[0023] In one embodiment, the convex structure 402 may have, for example, a wedge or triangular prism shape. In general, the convex structure 402 has a first face 402A and a second face 402B that meet at an edge 402C. The two faces 402A and 402B define an angle (e.g., an acute angle less than 90 degrees) at the edge 402C. In one embodiment, as shown in FIG. 4(C), a cross section of the convex structure along line 4C-4C has a triangular shape. In one embodiment, the first face 402A and the second face 402B are formed in a (111) crystal plane of the substrate 100.

[0024] 5 is a cross-sectional view of a substrate showing a wedge-shaped structure according to an embodiment of the present invention. In an embodiment, the method further includes depositing a first layer 502 of superconducting material on the first side 402A of the convex structure 402 in the substrate 100. In an embodiment, the first layer 502 of superconducting material can be deposited by using a first deposition, for example, as illustrated in FIG. 5. In an embodiment, the first layer 502 of superconducting material is also deposited in the first trench 510 and the second trench 512 formed during etching of the substrate 100.

[0025] The method further includes, after depositing the first layer of superconducting material 502, oxidizing the first layer of superconducting material 502 to form a layer of oxide material 504 on a surface of the first layer of superconducting material 502. The layer of oxide material 504 is formed where the first layer of superconducting material 502 is not in contact with the substrate 100. In particular, the end portion 502A of the first layer of superconducting material 502 near the edge 402C is also oxidized, and a portion 504A of the oxide layer 504 is formed on the end portion 502A of the first layer of superconducting material 502. Additionally, the oxide layer 504 is also formed at the bottom of the trenches 510 and 512 on the top surface of the first layer of superconducting material 502.

[0026] The method also includes depositing a second layer 506 of superconducting material on the second side 402B of the convex structure 402. In an embodiment, the second layer 506 of superconducting material may be deposited by using a second deposition, for example as illustrated in FIG. 5. The portion 506A of the second layer 506 of superconducting material is deposited in contact with the portion 504A of the layer 504 of oxide material at or near the edge 402C, such that the portion 504A of the layer of oxide material is sandwiched between the portion 502A of the first layer 502 of superconducting material and the portion 506A of the second layer 506 of superconducting material at or near the edge 402C to define a Josephson junction (JJ). In an embodiment, the layer 504 of oxide material is selected from the group consisting of aluminum oxide and niobium oxide. In one embodiment, a second layer of superconducting material 506 is also deposited within trenches 510 and 512 on the top surface of oxide layer 504 .

[0027] In one embodiment, the first layer of superconducting material 502 and the second layer of superconducting material 506 may be composed of the same or different superconducting materials. For example, in one embodiment, the first layer of superconducting material 502 and the second layer of superconducting material 506 may both be aluminum layers. In another embodiment, the first layer of superconducting material 502 may be an aluminum layer and the second layer of superconducting material may be a niobium layer. Additionally, the first layer of superconducting material 502 or the second layer of superconducting material 506 or both may be the same or different from the layer of superconducting material 102.

[0028] The method further includes removing the remaining sacrificial material layer (e.g., germanium) 302 to form Josephson junctions (JJs) and qubit device 600. Figure 6(A) is a top view of a formed qubit device 600 including Josephson junctions (JJs) and buses and resonators 202 and 204, according to an embodiment of the invention. Figure 6(B) is a cross-sectional view of a formed qubit device 600 taken along line 6B-6B shown in Figure 6(A), according to an embodiment of the invention. Figure 6(C) is a cross-sectional view of a formed qubit device 600 taken along line 6C-6C shown in Figure 6(A), according to an embodiment of the invention.

[0029] As shown in Figures 6(A)-6(C), qubit device 600 includes substrate 100 having convex structure 402 having first and second faces 402A and 402B that meet at edge 402C and form an angle therebetween. Qubit device 600 also includes a first layer 502 of superconducting material deposited on first face 402A of convex structure 402 of substrate material 100. Qubit device 600 also includes a layer 504 of oxide material on a surface of first layer of superconducting material 502. Qubit device 600 also includes a second layer 506 of superconducting material on a second face of substrate material 402B. A portion 506A of the second layer 506 of superconducting material is deposited in contact with a portion 504A of the layer of oxide material 504 at or near the edge 402C, so as to sandwich a portion 504A of the layer of oxide material between a portion 502A of the first layer 502 of superconducting material and a portion 506A of the second layer 506 of superconducting material at or near the edge 402C to define a Josephson junction (JJ).

[0030] In one embodiment, as shown in Figures 6(A) and 6(B), the first layer of superconducting material 502 and the second layer of superconducting material 506 also deposited in the first trench 510 define a first capacitor pad 602 to electrically connect to the Josephson junction (JJ). As shown in Figures 6(A) and 6(B), the first layer of superconducting material 502 and the second layer of superconducting material 506 also deposited in the second trench 512 define a second capacitor pad 604 to electrically connect to the Josephson junction (JJ). In one embodiment, the Josephson junction (JJ) is formed at or near the edge 402C without applying electron beam or light beam lithography to connect the capacitor pads 602 and 604 to the Josephson junction (JJ) and to the plurality of buses 202 and / or the plurality of readout resonators 204. As described in the paragraphs above, the plurality of busses 202 and the plurality of read resonators 204 are defined using lithography and portions of the superconducting material layer 102 are removed to form the plurality of busses and read resonators 202 and 204 on the substrate 100. The spacing between the first capacitor pad 602 and the plurality of busses 202 and the read resonators 204 and the spacing between the second capacitor pad 604 and the plurality of busses 202 and the read resonators 204 define coupling capacitors for coupling microwave energy to the Josephson junctions (JJs).

[0031] In conventional methods, ion milling is used to open up the naturally formed oxide on the capacitor pad material to connect to the Josephson junction capacitor pad material. In conventional methods, this ion milling step is typically performed in situ, before junction metal deposition. In contrast, in some embodiments of the present invention, the capacitor pads 602 and 604 and the Josephson junctions (JJs) of the qubits are formed during the same step. As a result, the use of ion milling to open up the naturally formed oxide on the capacitor pad material to connect the Josephson junctions to the capacitor pads is not required. In fact, the ion milling step may damage the substrate 100 (e.g., silicon) in the exposed areas and thus adversely affect the coherence. Therefore, by using the present method according to some embodiments of the present invention, this problem may be avoided and thus the challenge may be overcome.

[0032] Additionally, methods according to some embodiments of the present invention allow for the fabrication of qubit device 600 that substantially reduces far-field and near-field coupling with the external environment. Additionally, the overall size of the resulting qubit device 600 is also reduced, thus providing a compact qubit device that reduces losses and allows for the fabrication of two-dimensional lattices of qubits with symmetry.

[0033] The description of various embodiments of the present invention is presented for illustrative purposes, but is not intended to be exhaustive or limited to the disclosed embodiments. Many modifications and variations will become apparent to those skilled in the art without departing from the scope and spirit of the described embodiments. The terms used in this specification are selected to best explain the principles of the embodiments, practical applications, or technical improvements to the technology found in the market, or to enable other skilled in the art to understand the embodiments disclosed herein.

Claims

1. 1. A method of forming a Josephson junction in a superconducting qubit, comprising the steps of: providing a substrate having a convex structure, the convex structure having a first surface and a second surface that meet at an edge; depositing a first layer of superconducting material on the first surface of the substrate; oxidizing the first layer of superconducting material to form a layer of oxide material on a surface of the first layer of superconducting material; depositing a second layer of the superconducting material on the second surface of the substrate; wherein the portion of the second layer contacts the portion of the layer of oxide material at or near the edge such that the portion of the layer of oxide material is sandwiched between a portion of the first layer of superconducting material and a portion of the second layer of superconducting material at or near the edge to define a Josephson junction.

2. depositing a superconducting material on a surface of the substrate; removing a portion of the superconducting material to expose a first portion of the surface of the substrate for forming a plurality of buses and a read resonator on the substrate; The method of claim 1 further comprising:

3. depositing a sacrificial material layer over the superconducting material and over the exposed first portion of the surface of the substrate; applying electron beam or optical beam lithography to expose a portion of the sacrificial material layer; removing the exposed portion of the sacrificial material layer to reveal a second portion of the surface of the substrate to define a qubit pocket; The method of claim 2 , further comprising:

4. 4. The method of claim 3, wherein depositing the sacrificial material layer over the superconducting material and over the exposed first portion of the substrate comprises depositing germanium (Ge) over the superconducting material and over the exposed first portion of the substrate.

5. The method of claim 3 or 4, wherein the exposed second portion of the surface of the substrate has two mirror symmetric shapes.

6. The method of claim 5 , wherein the exposed second portion of the surface of the substrate has an H-shape.

7. 7. The method of claim 5 or 6, wherein the two mirror-symmetric shapes of the exposed second portion of the surface of the substrate are separated by a narrower strip of the sacrificial material layer at a midline of the two mirror-symmetric shapes.

8. Etching the exposed second portion of the surface of the substrate to form the raised structure in the substrate. The method of any one of claims 3 to 7, further comprising:

9. 9. The method of claim 8, wherein etching the exposed second portion of the surface of the substrate comprises etching using potassium hydroxide (KOH) or tetramethylammonium hydroxide (TMAH).

10. 10. The method of claim 8 or 9, further comprising removing a remaining sacrificial material layer to form the Josephson junction.

11. The method of claim 1 , wherein the first surface and the second surface are formed within a crystal plane of the substrate.

12. The method of claim 1 , wherein the substrate comprises silicon (Si).

13. 13. The method of claim 1, wherein the superconducting material is selected from the group consisting of aluminum (Al) and niobium (Nb).

14. 14. The method of claim 1, wherein the oxide material is selected from the group consisting of aluminum oxide and niobium oxide.

15. 1. A qubit device comprising: a substrate having a convex structure, the convex structure having a first surface and a second surface that meet at an edge and form an angle therebetween; a first layer of superconducting material deposited on the first surface of the substrate; a layer of oxide material on a surface of said first layer of superconducting material; a second layer of the superconducting material on the second surface of the substrate; and wherein a portion of the second layer contacts a portion of the layer of oxide material at or near the edge such that a portion of the layer of oxide material is sandwiched between a portion of the first layer of superconducting material and a portion of the second layer of superconducting material at or near the edge to define a Josephson junction.

16. The qubit device of claim 15 , wherein the substrate comprises silicon (Si).

17. 17. A qubit device according to any of claims 15 to 16, wherein the superconducting material is selected from the group consisting of aluminum (Al) and niobium (Nb).

18. 18. A qubit device according to any of claims 15 to 17, wherein the oxide material is selected from the group consisting of aluminium oxide and niobium oxide.

19. 1. A method of forming a Josephson junction in a superconducting qubit, comprising the steps of: Providing a substrate; depositing a superconducting material on a surface of the substrate; depositing a layer of sacrificial material on the superconducting material; removing a portion of the sacrificial material layer to reveal a portion of the surface of the substrate to define a qubit pocket; etching the portion of the surface of the substrate to form a convex feature in the substrate, the convex feature having a first surface and a second surface that meet at an edge; forming the Josephson junctions at or near the edges without applying electron beam or optical beam lithography to connect the capacitor pads connected to the Josephson junctions to a plurality of buses; A method comprising:

20. forming the Josephson junction depositing a first layer of superconducting material on the first surface of the convex feature in the substrate; oxidizing the first layer of superconducting material to form a layer of oxide material on a surface of the first layer of superconducting material; depositing a second layer of the superconducting material on the second surface of the convex feature in the substrate; 20. The method of claim 19, comprising: wherein the portion of the second layer contacts the portion of the layer of oxide material at or near the edge such that the portion of the layer of oxide material is sandwiched between a portion of the first layer of superconducting material and a portion of the second layer of superconducting material at or near the edge to define the Josephson junction.

21. defining the plurality of buses and a plurality of readout resonators using lithography; removing portions of the superconducting material to form the plurality of bus and read resonators on the substrate; 21. The method of claim 19 or 20, further comprising:

22. 22. The method of any of claims 19 to 21, wherein removing the portion of the sacrificial material layer comprises applying a single lithography step.

Citation Information

Patent Citations

  • Superconducting device and manufacture thereof

    JP1990234479A

  • Josephson device and manufacturing method thereof

    JP1993243627A

  • Magnetic field sensor device for direct magnetic field imaging and method of fabrication thereof

    WO2009004609A2

  • Shadow mask sidewall tunnel junction for quantum computing

    WO2018224876A1