Reinforced polymer material and method of manufacturing the same

Incorporating two-dimensional materials into reinforced polymeric materials addresses deformation issues, achieving a 46-90% reduction in molded article deformation and enhancing manufacturing precision.

JP7595566B2Active Publication Date: 2024-12-06PETROLIAM NASIONAL BHD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021512230
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-09-03
Filing Date
2019-08-30
Publication Date
2024-12-06
Estimated Expiration
2039-08-30

AI Technical Summary

Technical Problem

Reinforced polymeric materials used in composite components suffer from distortion and deformation during the curing process, necessitating time-consuming iterative mold and process adjustments to achieve desired dimensions.

Method used

Incorporating two-dimensional materials such as graphene or hexagonal boron nitride into the polymer matrix at specific volume percentages and aspect ratios, along with fiber reinforcement, to form a reinforced polymeric material that reduces deformation.

Benefits of technology

The incorporation of two-dimensional materials results in a reduction of deformation by 20-100%, specifically 46-90%, in molded articles, improving manufacturing efficiency and precision.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Disclosed herein is a reinforced polymeric material, in which a polymer matrix material is filled with a two-dimensional material having an average aspect ratio of 100 to 2000 and a fiber reinforcement material. The composition may also optionally include a curing agent. The material may be useful in providing molding materials with improved deformation characteristics.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an improved reinforced polymeric material and a method for making the improved reinforced polymeric material and its use in forming composite components, such as composite components requiring precision surfaces. [Background technology]

[0002] The listing or discussion of a prior-published document in this specification should in no way be taken as an admission that the document is part of the state of the art or is common general knowledge.

[0003] Reinforced polymer materials are often used in the manufacture of a variety of composite components. Reinforced polymer materials are "pre-impregnated" composite fibers, which have a thermoset or thermoplastic polymer matrix material, such as epoxy or polyamide, already present. These composite fibers are typically supplied in woven, non-woven or chopped strand mat form, with the polymer matrix material being used to bond the fibers together and (if required) to bond the fibers to other components during the manufacture of the final product.

[0004] Unfortunately, although the use of reinforced polymer materials seems like a very convenient way to manufacture composite components (e.g., to control the surface), the hardened materials tend to suffer from distortion and deformation, which can pose problems for proper assembly or bonding of the components.

[0005] To overcome the above problems, current processes follow an essentially iterative process of making the desired mold, then forming the desired product, and testing it for the above problems. If the tested product suffers from the above mentioned distortions, modifications are made to the mold and / or process, and the cycle is repeated. This process itself can take many cycles until something resembling a usable product with the desired cured dimensions is obtained. However, this iterative process is very time consuming, and in some cases, even requires a lay-up of material to accommodate the distortions. As a result, the full potential of the composite material is not realized.

[0006] It would therefore be desirable to provide a reinforced polymeric material that overcomes or mitigates the above-mentioned problems. Summary of the Invention

[0007] Surprisingly, it has been found that by adding a two-dimensional material to a polymer matrix, the deformation of such material is reduced. This is found, for example, in moulded articles made from such materials. Thus, in a first aspect of the present invention there is provided a reinforced polymer material comprising: A two-dimensional material comprising 0.002-6% by volume of the composition in a filled polymeric matrix material, the two-dimensional material having an average aspect ratio of 100-2000; In a filled polymer matrix material, a fiber reinforcement material is present at 20 to 75 volume percent of the composition; and The remainder is made up of a filled polymer matrix material and, optionally, a curing agent (if required).

[0008] In an embodiment of the first aspect of the present invention: (a) the filled polymer matrix material may be a thermosetting material (e.g., selected from one or more of the group consisting of epoxy resins, polyesters, and vinyl esters; optionally, the epoxy resin may be selected from bisphenol-A diglycidyl ether resin); (b) the filled polymer matrix material may be a thermoplastic material (e.g., the filled polymer matrix material may be selected from one or more of the group consisting of polyethylene, polypropylene, polyamide, and polyetheretherketone; optionally, the thermoplastic material may be selected from one or more of the group consisting of high density polyethylene, medium density polyethylene, and low density polyethylene); (c) The two-dimensional material may be selected from one or more of the group consisting of graphene, graphene oxide, reduced graphene oxide, graphene nanoplatelets, graphene having 1-5 layers (e.g., 1-3 layers) (e.g., bilayer graphene), hexagonal boron nitride (hBN), molybdenum disulfide (MoS2), tungsten diselenide (WSe2), silicone, and germanene, including layered assemblies of mixtures of these materials (ISO / TS 80004-13). For example, the two-dimensional material may be selected from one or more of the group consisting of graphene, chemically modified graphene, reduced graphene oxide, and boron nitride, and optionally, the two-dimensional material is graphene; (d) the two-dimensional material may have an average aspect ratio of 180 to 500; (e) the reinforced polymeric material may comprise a two-dimensional material in a polymeric matrix that is between 0.05% and 1% by volume of the composition; (f) the fiber reinforcing material may be selected from one or more of the group consisting of glass, carbon fiber, Kevlar, and engineering reinforcing fiber (e.g., the transitional reinforcing material may be carbon fiber); (g) the reinforced polymeric material may comprise a fibrous reinforcement material that is between 50% and 70% by volume of the composition; (h) The curing agent may be selected from one or more of the group consisting of polyamines, aminoamides, and phenolic compounds.

[0009] In a second aspect of the present invention, there is provided a method of forming a moulded article from the reinforced polymeric material described in the first aspect of the present invention, and any technically prudent combination of embodiments thereof, the process comprising the steps of: (a) providing a reinforced polymeric material as described in the first aspect of the present invention, and any technically prudent combination of embodiments thereof, and laying up the material in a mould; and (b) curing the reinforced polymeric material in the mold to form a molded article.

[0010] In a third aspect of the present invention there is provided a prepreg material formed from the reinforced polymeric material described in the first aspect of the present invention, and any technically prudent combination of embodiments thereof.

[0011] In a fourth aspect of the invention there is provided a moulded article formed from the reinforced polymeric material as described in the first aspect of the invention, and any technically judicious combination of embodiments thereof, and / or a prepreg material as described in the third aspect of the invention. In an embodiment of this aspect, the resulting moulded article may exhibit a reduction in deformation of from 20 to 100%, such as from 45 to 99%, for example from 46 to 90%, compared to a moulded article formed from an otherwise identical reinforced polymeric material that does not include the two-dimensional material.

[0012] Further aspects and embodiments of the present invention are described in the following clauses.

[0013] 1. A reinforced polymer material comprising: a two-dimensional material that is 0.002-6% by volume of the composition in a filled polymer matrix material and has an average aspect ratio of 100-2000; A fiber-reinforced material that is 20 to 75 volume percent of the composition in a filled polymer matrix material; and the remainder consisting of a filled polymer matrix material and, optionally, a curing agent. A reinforced polymer material comprising:

[0014] 2. The reinforced polymer material of clause 1, wherein the filled polymer matrix material is a thermosetting material.

[0015] 3. The reinforced polymeric material of claim 2, wherein the thermosetting material is selected from one or more of the group consisting of epoxy resins, polyesters and vinyl esters.

[0016] 4. The reinforced polymeric material of clause 3, wherein the epoxy resin is a bisphenol-A diglycidyl ether resin.

[0017] 5. The reinforced polymer material of clause 1, wherein the filled polymer matrix material is a thermoplastic material.

[0018] 6. The reinforced polymeric material of claim 5, wherein the thermoplastic material is selected from one or more of the group consisting of polyethylene, polypropylene, polyamide and polyetheretherketone.

[0019] 7. The reinforced polymeric material of clause 6, wherein the thermoplastic is selected from one or more of the group consisting of high density polyethylene, medium density polyethylene and low density polyethylene.

[0020] 8. The reinforced polymer material according to any one of the preceding clauses, wherein the two-dimensional material is selected from one or more of the group consisting of graphene, graphene oxide, reduced graphene oxide, graphene nanoplatelets, graphene having 1 to 5 layers (e.g., 1 to 3 layers) (e.g., bilayer graphene), hexagonal boron nitride (hBN), molybdenum disulfide (MoS2), tungsten diselenide (WSe2), silicone, and germanene, including layered assemblies of mixtures of these materials (ISO / TS 80004-13).

[0021] 9. The reinforced polymer material of clause 8, wherein the two-dimensional material is selected from one or more of the group consisting of graphene, chemically modified graphene, reduced graphene oxide and boron nitride, optionally the two-dimensional material is graphene.

[0022] 10. The reinforced polymer material of any one of the preceding clauses, wherein the two-dimensional material has an average aspect ratio of 180 to 500.

[0023] 11. The reinforced polymer material of any one of the preceding clauses, wherein the reinforced polymer material comprises two-dimensional material in the polymer matrix that is between 0.05% and 1% by volume of the composition.

[0024] 12. A reinforced polymer material according to any one of the preceding clauses, wherein the fiber reinforcement material is selected from one or more of the group consisting of glass, carbon fiber, Kevlar and engineered reinforcement fibers.

[0025] 13. The reinforced polymer material according to clause 12, wherein the fibre reinforcement material is carbon fibre.

[0026] 14. The reinforced polymer material of any one of the preceding clauses, wherein the reinforced polymer material comprises a fiber reinforcement material that is 50% to 70% by volume of the composition.

[0027] 15. The reinforced polymeric material according to any one of the preceding clauses, wherein the curing agent is selected from one or more of the group consisting of polyamines, aminoamides and phenolic compounds.

[0028] 16. A method of forming a moulded product from a reinforced polymer material according to any one of clauses 1 to 15, comprising the steps of: (a) providing a reinforced polymer material as defined in any one of clauses 1 to 15 and laying up the material in a mould; and (b) curing the reinforced polymeric material in the mold to form a molded article. The present invention comprises:

[0029] 17. A prepreg material formed from the reinforced polymer material described in any one of clauses 1 to 15.

[0030] 18. A moulded article formed from a reinforced polymer material as described in any one of clauses 1 to 15 and / or a prepreg material as described in clause 17.

[0031] 19. A molded article according to clause 18, wherein the resulting molded article exhibits a reduction in deformation of 20-100%, such as 45-99%, such as 46-90%, compared to a molded article formed from an otherwise identical reinforced polymeric material that does not include the two-dimensional material. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0032] The present disclosure provides materials that overcome some or all of the aforementioned problems. Thus: a two-dimensional material comprising 0.002% to 6% by volume of the composition in a filled polymer matrix material, the two-dimensional material having an average aspect ratio of 100 to 2000; A fiber-reinforced material that is 20 to 75 volume percent of the composition in a filled polymer matrix material; and the remainder consisting of a filled polymer matrix material and, optionally, a curing agent. A reinforced polymeric material is disclosed comprising:

[0033] In the embodiments of the present specification, the term "comprising" may be interpreted as requiring the recited features, but not limiting the presence of other features. Alternatively, the term "comprising" may refer to the case where only the recited components / features are intended to be present (e.g., the term "comprising" may be replaced with the phrase "consists of" or "essentially consisting of"). It is expressly contemplated that both the broader and narrower interpretations may be applied to all aspects and embodiments of the present invention. In other words, the term "comprising" and its synonyms may be replaced with "consisting of" or "consisting essentially of" or their synonyms, and vice versa.

[0034] As used herein, "average aspect ratio" refers to the average lateral dimension of a material divided by the average thickness of the material. This ratio applies to two-dimensional materials, which are generally considered to be materials that are only one atom thick. However, as used herein, the term is intended to encompass materials that may be a few layers of atoms thick (e.g., 1-3 layers, 1-2 layers thick, etc., 1-5 layers thick). Any suitable two-dimensional material capable of reducing deformation, provided there is chemical compatibility with the other components, may be used to form the reinforced polymeric materials described herein. Suitable two-dimensional materials that may be mentioned herein include, but are not limited to, graphene, graphene oxide, reduced graphene oxide, graphene nanoplatelets, graphene having 1-5 layers (e.g., 1-3 layers) (e.g., bilayer graphene), hexagonal boron nitride (hBN), molybdenum disulfide (MoS2), tungsten diselenide (WSe2), silicone, and germanene, including layered assemblies of mixtures of these materials (ISO / TS 80004-13). In particular examples that may be mentioned herein, the two-dimensional material may be selected from one or more of the group consisting of graphene, chemically modified graphene, reduced graphene oxide, and boron nitride. For example, the two-dimensional material may be graphene.

[0035] As mentioned above, the two-dimensional material may have an average aspect ratio of 100-2000. In certain embodiments that may be mentioned herein, the two-dimensional material may have an average aspect ratio of 180-500, such as 150-750. For the avoidance of doubt, it is specifically intended that, for any numerical value, the lower and upper limits provided in the list of numerical ranges may be combined in any manner. For example, the two-dimensional material disclosed herein may have the following numerical range values: 100-2000, 180-500, 150-750, 100-180, 100-500, 100-750, 180-750, 180-2000, 500-750, 500-2000, and 750-2000.

[0036] As mentioned above, the two-dimensional material may comprise 0.002-6% by volume of the composition. In certain examples, the two-dimensional material may comprise 0.05-1% by volume of the composition, such as 0.1-0.5% by volume of the composition. As used herein, the volume percent of the composition refers to the total volume of the composition once formed.

[0037] As used herein, the term "filled polymer matrix material" is intended to refer to a polymer material that encapsulates (and is therefore filled by) other components. Any suitable polymer material may be used. For example, the polymer material may be a thermoplastic material or a thermoset material.

[0038] Examples of thermosetting materials that may be mentioned herein include, but are not limited to, epoxy resins, polyesters, vinyl esters, and combinations thereof. In certain embodiments that may be mentioned herein, the thermosetting material may be a bisphenol-A diglycidyl ether resin of an epoxy resin.

[0039] Examples of thermoplastic materials that may be mentioned herein include, but are not limited to, polyethylene, polypropylene, polyamide, polyetheretherketone, and combinations thereof. For example, the thermoplastic material may be selected from one or more of high density polyethylene, medium density polyethylene, and low density polyethylene.

[0040] As will be appreciated, when more than one polymeric material is used, the resulting polymer matrix is ​​a blend of selected polymeric materials, which may be used when specific properties are desired. In some embodiments, it is contemplated that the polymeric material may be a blend comprising both thermoplastic and thermoset materials.

[0041] Any suitable fiber reinforcement material may be used herein. For example, the fiber reinforcement material may be selected from the group including, but not limited to, glass, carbon fiber, Kevlar, engineering reinforcement fibers, and combinations thereof. In certain embodiments that may be mentioned herein, the fiber reinforcement material may be carbon fiber.

[0042] As noted above, the fibrous reinforcing material may be present in an amount of 20-75% by volume of the composition. Other examples of suitable ranges of the fibrous reinforcing material in the composition include 25-72% by volume of the composition, and 50-70% by volume of the composition.

[0043] In certain embodiments of the composition, the reinforced polymeric material may include a curing agent. As used herein, "curing agent" refers to a material capable of forming crosslinks between polymeric chains of the polymeric material. Any suitable curing agent may be used herein, provided that it is compatible with at least one of the polymeric materials forming the filled polymeric matrix material. Examples of suitable crosslinking agents that may be mentioned include, but are not limited to, polyamines, aminoamides, phenolic compounds, and combinations thereof. As will be appreciated by those skilled in the art, the amount of crosslinking agent (if any) required in the composition can be readily determined by those skilled in the art based on the polymeric materials used and the desired properties of the material to be subsequently cured.

[0044] The reinforced polymeric materials disclosed herein may be formed by any suitable method. For example, the two-dimensional material may be dispersed in a suitable solvent (e.g., isopropanol) at a suitable concentration, e.g., 0.01-1 g, e.g., 0.05 g, per mL of solvent, and then sonicated for a suitable time (e.g., 30 minutes at 37 kHz). The resulting suspension may then be blended with the polymer matrix material and vented to remove the solvent (e.g., 250 g of resin for 0.5 g of two-dimensional material). The fiber reinforcement material may then be combined with the composition using any suitable method (e.g., a mechanical impregnation device) in an amount (determinable by one of skill in the art based on the desired use; and determined by volume percent) necessary to provide the desired reinforcement. If a hardener (or curing agent) is added to the composition, it may be added prior to combination with the fiber reinforcement material. Examples of the above procedures are provided in the Examples section below. Such materials (before curing and / or hardening) may be described as prepreg materials. The present invention therefore also relates to the formation of prepreg materials and the prepreg materials themselves, which are essentially reinforced polymeric materials as described herein above.

[0045] The reinforced polymeric materials disclosed herein may be used to form polymeric articles. An advantage associated with molded articles made using the reinforced polymeric materials described herein is that they exhibit reduced deformation compared to molded articles formed from otherwise identical reinforced polymeric materials that do not include two-dimensional materials. The reduced deformation may be 20-100%, such as 45-99%, for example 46-90%.

[0046] The molded articles described herein may be formed from the reinforced polymeric materials described above by a process including the following steps: (a) providing a reinforced polymeric material as described above and laying up the material in a mold; and (b) curing the reinforced polymeric material in the mold to form a molded article.

[0047] Further aspects and embodiments of the invention are described below in the examples and claims. EXAMPLES

[0048] Example 1 Preparation of reinforced polymer materials First, a 2-dimensional filler material such as graphene was blended with bisphenol-A diglycidyl ether (BADGE) resin at about 0.10% by volume with respect to the resin.

[0049] To prepare the two-dimensional filler material for blending, first, isopropanol was mixed with the two-dimensional filler material at a concentration of about 0.05 g filler / 1 ml isopropanol. The mixture was then sonicated at a frequency of 37 kHz for at least 30 minutes. After the preparation process, the filler and solvent mixture was blended with Bisphenol-A diglycidyl ether (BADGE) and vented at room temperature for more than 8 hours to form a blended resin. The amount of resin used was 250 g, with 0.5 g of graphene.

[0050] The blended resin was then mixed with 87.5 g of amine hardener and pre-impregnated into fiber reinforcements such as 0 / 90 NCF (656 gsm) carbon fiber (approximately 0.8-0.9 mm thick) with the aid of an in-house mechanical impregnation device to produce reinforced polymer materials as prepregs. The impregnation device consists of a resin bath, which draws in the "dry" fiber reinforcement fabric from one end, which is subsequently wound together on a pickup roller as a prepreg. The speed of impregnation is controlled at approximately 4 revolutions per minute with respect to the pickup roller. The overall composition has a fiber reinforcement content of approximately 60 vol.%, 0.10 vol.% graphene, and the remainder is composed of polymer matrix material and hardener.

[0051] Manufacturing L-bracket components for testing and analysis To measure the degree of deformation observed in the resulting cured reinforced polymer material, L-bracket components were fabricated using the prepreg reinforced polymer material and the internal bend angle was measured.

[0052] First, four layers of prepreg reinforced polymer material were cut and stacked into a right-angle mold with a radius of 3 mm. The mold and stacked layers were then vacuum bagged and cured at a temperature of 80° C. under vacuum for at least 6 hours. After curing, the stacked reinforced polymer layers were removed from the mold and an L-shaped bracket part was prepared. The L-shaped bracket had a width of about 35 mm, a length of about 70 mm on each side, and an inner diameter of 3 mm.

[0053] As a control, an L-bracket part made from reinforced neat prepreg resin (without any added filler material) was also fabricated using the method described above.

[0054] The angles of the L-brackets were measured using an angle ruler to compare the difference in deformation between the two sets of L-bracket parts when fully cured and when removed from the mold.

[0055] Overall, compared to neat reinforced resin (i.e., resin without filler material), L-brackets formed with the impregnated resin of the present invention exhibit increased resistance to deformation. Specifically, L-bracket components made from the reinforced polymeric material of the present invention exhibit a maximum 46% reduction in deformation, from 0.217° (neat) to 0.1° (filled).

[0056] Example 2 To prepare a thermoplastic matrix with a two-dimensional filler material such as graphene, about 0.5 wt.% of graphene is mixed with HDPE, for example, 45 g of graphene and 8955 g of HDPE are mixed together for a total of 9 kg. The HDPE is in the form of pellets or powder, or a combination of pellets and powder. Mixing is carried out in a mixer with the material sealed in a bag. The mixed material is then fed into an extruder with a screw speed of about 600 rpm and a die temperature of 180°C to 220°C. The extruded material is chopped into pellets to form "filled pellets". The extrusion may be repeated to improve the dispersion of the filler within the pellets.

[0057] The filled pellets can be used to make thermoplastic fiber reinforced parts, for example in injection molding or extrusion processes, where the fiber reinforcement is added during the manufacturing process.

[0058] As in the thermosetting example (Example 1), the presence of two-dimensional fillers makes it possible to reduce deformation of the manufactured parts compared to unfilled parts.

Claims

1. 1. A reinforced polymer material comprising: a two-dimensional material in a filled polymer matrix material, the two-dimensional material being 0.05-0.5% by volume of the composition, the two-dimensional material being graphene having an average aspect ratio of 100-2000; In a filled polymer matrix material, a fiber reinforcement material that is 50-70% by volume of the composition; and the remainder consisting of the filled polymer matrix material and, if the filled polymer matrix material is a thermosetting material, a hardener; Consisting of A reinforced polymer material, wherein the fiber reinforcement material is carbon fiber.

2. The reinforced polymeric material of claim 1 , wherein the filled polymeric matrix material is a thermoset material.

3. The reinforced polymeric material of claim 2 , wherein the thermosetting material is selected from one or more of the group consisting of epoxy resins, polyesters, and vinyl esters.

4. 4. The reinforced polymeric material of claim 3, wherein the epoxy resin is a bisphenol-A diglycidyl ether resin.

5. The reinforced polymeric material of claim 1 , wherein the filled polymeric matrix material is a thermoplastic material.

6. The reinforced polymeric material of claim 5 , wherein the thermoplastic material is selected from one or more of the group consisting of polyethylene, polypropylene, polyamide, and polyetheretherketone.

7. 7. The reinforced polymeric material of claim 6, wherein the thermoplastic material is selected from one or more of the group consisting of high density polyethylene, medium density polyethylene, and low density polyethylene.

8. 10. The reinforced polymeric material of claim 1, wherein the two-dimensional material has an average aspect ratio of 180-500.

9. The reinforced polymeric material of claim 2 , wherein the curing agent is selected from one or more of the group consisting of polyamines, aminoamides, and phenolic compounds.

10. A prepreg material formed from the reinforced polymer material of claim 2.

11. A molded article formed from the reinforced polymeric material of claim 1.

12. A molded article formed from the prepreg material according to claim 10.

13. 12. The molded article of claim 11, wherein the resulting molded article exhibits a reduction in deformation of from 20 to 100%, such as from 45 to 99%, such as from 46 to 90%, compared to a molded article formed from an otherwise identical reinforced polymeric material that does not include the two-dimensional material.

14. 13. The molded article of claim 12, wherein the resulting molded article exhibits a reduction in deformation of from 20 to 100%, such as from 45 to 99%, such as from 46 to 90%, compared to a molded article formed from an otherwise identical reinforced polymeric material that does not include the two-dimensional material.

Citation Information

Patent Citations

  • Crystalline thermoplastic resin pillar reinforced with filaments and leaflet inorganic filler

    JP1994279615A

  • Polymer of high damping capacity

    JP2003128850A

  • Insulating layer composition for substrate, and prepreg and substrate using the same

    JP2013224424A

  • Resin composite material

    WO2013146213A1

  • Method of forming graphene nanoplatelets, graphene nanoplatelets so-obtained and composites comprising said nanoplatelets

    WO2018051095A1