Manufacturing method of cast slab

The method optimizes slab production by setting light reduction areas, gradients, and cooling intensities to achieve consistent quality across varying slab sizes, addressing center segregation and defects, and enabling efficient production for diverse steel products.

JP7597281B1Active Publication Date: 2024-12-10JFE STEEL CORP
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2024552781
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2023-06-20
Filing Date
2024-06-04
Publication Date
2024-12-10
Estimated Expiration
2044-06-04

Smart Images

  • Figure 0007597281000002
    Figure 0007597281000002
  • Figure 0007597281000003
    Figure 0007597281000003
  • Figure 0007597281000004
    Figure 0007597281000004
Patent Text Reader

Abstract

Provided is a method for producing a slab capable of obtaining a slab of appropriate quality. The method for producing a slab of a predetermined size using a continuous casting machine. The method for producing a slab includes a soft reduction region setting step for setting a soft reduction region including a start point for soft reduction of the slab in the continuous casting machine and an end point for soft reduction, based on the conditions of cooling water for cooling the slab in the continuous casting machine, the withdrawal speed of the slab, and the solid phase ratio of the slab calculated using the composition of the slab; a reduction gradient setting step for setting a reduction gradient in the soft reduction region, based on the thickness, width, and withdrawal speed of the slab; a secondary cooling intensity setting step for setting a first strength zone and a second strength zone in which secondary cooling is performed at an intensity stronger than that of the first strength zone, as zones in which secondary cooling is performed in the soft reduction region, based on the solid phase ratio of the slab; and a continuous casting step for performing continuous casting using the set soft reduction region, reduction gradient, first strength zone, and second strength zone.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Method and apparatus for continuous casting and subsequent deformation of cast strands of steel, in particular cast strands having ingot size or blank steel size

    JP2004525767A

  • Continuous casting method of steel

    JP2015009264A

  • Secondary cooling control device for continuous casting machine, secondary cooling control method for continuous casting machine, and program

    JP2019048322A

  • Method for continuous steel casting

    WO2020203715A1

  • Continuous casting method

    JP1991090259A