Bipolar transistor manufacturing method

By applying a voltage to the ledge layer through a control electrode, the bipolar transistor achieves enhanced high-frequency characteristics and reliability, addressing the trade-off between ledge width and emitter capacitance.

JP7948333B2Active Publication Date: 2026-11-11NIPPON TELEGRAPH & TELEPHONE CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2024558490
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-11-14
Publication Date
2026-11-11
Estimated Expiration
2042-11-14

AI Technical Summary

Technical Problem

Existing technologies face challenges in improving the high-frequency characteristics of InP-based heterojunction bipolar transistors (HBTs) while maintaining long-term reliability, as thinning the ledge layer to suppress leakage current leads to increased emitter capacitance or leakage due to tunneling, and widening the ledge layer deteriorates high-frequency performance.

Method used

A control electrode is introduced to apply a voltage to the ledge layer, allowing for depletion control and minimizing the ledge width without increasing emitter capacitance, thereby enhancing high-frequency characteristics and reliability.

Benefits of technology

The control electrode enables improved high-frequency performance and reduced current gain variations, ensuring both high-frequency and long-term reliability of the bipolar transistor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007948333000001
    Figure 0007948333000001
  • Figure 0007948333000002
    Figure 0007948333000002
  • Figure 0007948333000003
    Figure 0007948333000003
Patent Text Reader

Abstract

This bipolar transistor comprises a collector layer (103) formed on a substrate (101), a base layer (104) formed on the collector layer (103), an emitter layer (105) formed on the base layer (104), and an emitter cap layer (106) formed on the emitter layer (105), includes a ledge layer (105a) in the emitter layer (105) around the emitter cap layer (106) so as to have a ledge structure, and is provided with a control electrode (107) which applies a voltage (electric field) to the ledge layer (105a).
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present invention relates to a bipolar transis Ta and a manufacturing method thereof. BACKGROUND ART

[0002] Heterojunction bipolar transistors (HBTs) using indium phosphide (InP)-based materials are excellent in high speed and high output performance, and are particularly suitable for front-end ICs for large-capacity optical communications and ICs for "Beyond 5G" wireless communications that require ultra-high frequency operation. For application deployment, it is required to maintain practical reliability and achieve intermittent high-speed operation of HBTs.

[0003] In particular, in order to improve the maximum oscillation frequency required for the above applications, it is effective to reduce the intrinsic collector capacitance and reduce the base resistance by miniaturizing the emitter. The base resistance is the sum of the intrinsic base resistance generated in the base layer directly below the emitter layer, the base access resistance generated in the base layer from the emitter end to the base electrode end, and the base electrode resistance generated at the base electrode. To reduce these, miniaturization of the element (reduction of the emitter width, reduction of the emitter-base electrode interval) is important.

[0004] However, it is extremely difficult to improve the high-frequency characteristics through the structural improvements described above while maintaining the reliability of HBTs with existing technologies.

[0005] A typical InP-based HBT will be described below using Figure 3 (Non-Patent Literature 1). This HBT comprises a substrate 301 made of InP doped with Fe to achieve high resistance, a sub-collector layer 302 made of InGaAs / InP doped with a high concentration of n-type impurities, a collector layer 303 made of InP doped with n-type impurities, a base layer 304 made of InGaAs doped with a high concentration of p-type impurities, and an emitter layer 305 made of InP doped with n-type impurities. Furthermore, an emitter cap layer 306 made of InGaAs doped with a high concentration of n-type impurities is formed on the emitter layer 305.

[0006] Furthermore, a collector electrode 321 is formed on the sub-collector layer 302 surrounding the collector layer 303, and a base electrode 322 is formed on the base layer 304 surrounding the emitter layer 305. The base electrode 322 is formed to surround the outer periphery of the emitter layer 305 in order to reduce base resistance. Additionally, an emitter electrode 323 is formed on the emitter cap layer 306.

[0007] Furthermore, in order to suppress the surface recombination current flowing through the surface of the outer base layer, which is the region between the emitter mesa portion above the base layer 304 and the base electrode 322, the emitter layer 305 is extended from the emitter mesa portion to form a ledge layer 305a, creating a ledge structure. In addition, a protective film 307 made of an insulating material is formed covering the sides of the emitter cap layer 306 and the upper surface of the ledge layer 305a.

[0008] In this HBT structure, the depleted ledge layer 305a suppresses the phenomenon where electrons injected from the emitter electrode 323 leak from the side of the emitter layer 305 and unintentionally recombine with holes in the base layer 304, thereby improving current gain and long-term reliability.

[0009] In the HBT structure described above, increasing the width of the ledge layer in plan view (ledge width) is usually effective in improving current gain and long-term reliability. On the other hand, increasing the ledge width leads to an increase in base access resistance and a deterioration of high-frequency characteristics due to an increase in collector capacitance, so there is essentially a trade-off between long-term reliability and high-frequency characteristics. [Prior art documents] [Non-patent literature]

[0010] [Non-Patent Document 1] K. KURISHIMA et al., "Performance of InP / InGaAs HBTs with a Thin Highly N-Type Doped Layer in the Emitter-Base Heterojunction Vicinity", The Institute of Electronics, Information and Communication Engineers Transactions on Electronics, vol. E95.C, no. 8, pp. 1310-1316, 2012. [Overview of the Initiative] [Problems that the invention aims to solve]

[0011] Another method to improve long-term reliability without increasing the ledge width is to thin the ledge layer. By thinning the ledge layer, ledge depletion progresses, further suppressing leakage current. However, in recent HBTs, the ledge layer has already been thinned to about 20 nm, and further thinning is limited as it may lead to an increase in emitter capacitance or, conversely, an increase in leakage current due to tunneling. Thus, conventional technology has presented a problem in that it is not easy to achieve both long-term reliability and improved high-frequency characteristics of bipolar transistors.

[0012] This invention was made to solve the above-mentioned problems and aims to improve the high-frequency characteristics of bipolar transistors while ensuring long-term reliability. [Means for solving the problem]

[0013] The bipolar transistor according to the present invention comprises a collector layer made of a compound semiconductor formed on a substrate, a base layer made of a compound semiconductor formed on the collector layer, an emitter layer made of a compound semiconductor formed on the base layer and having a smaller area than the base layer in a plan view, an emitter cap layer made of a compound semiconductor formed on the emitter layer and having a smaller area than the emitter layer in a plan view, a collector electrode connected to the collector layer, a base electrode formed on the base layer surrounding the emitter layer and spaced apart from the emitter layer, an emitter electrode formed on the emitter cap layer, and a control electrode that applies a voltage to the ledge layer formed by the emitter layer surrounding the emitter cap layer.

[0014] Furthermore, the method for manufacturing a bipolar transistor according to the present invention is a method for manufacturing a bipolar transistor, comprising: a first step of forming a collector formation layer made of a compound semiconductor on a substrate; a second step of forming a base formation layer made of a compound semiconductor on the collector formation layer; a third step of forming an emitter formation layer made of a compound semiconductor on the base formation layer; a fourth step of forming an emitter cap formation layer made of a compound semiconductor on the emitter formation layer; a fifth step of forming an emitter electrode on the emitter cap formation layer; a sixth step of patterning the emitter cap formation layer using the emitter electrode as a mask to form an emitter cap layer on the emitter formation layer; a seventh step of forming a control electrode after the emitter cap layer has been formed; an eighth step of patterning the emitter formation layer after the control electrode has been formed to form an emitter layer on the base formation layer; a ninth step of forming a base electrode on the base formation layer surrounding the emitter layer after the emitter layer has been formed; and a fifth step of patterning the base formation layer after the base electrode has been formed to form a base layer on the collector formation layer. 10The process involves forming a base layer, then patterning the collector layer to form the collector layer on the substrate (first step). 1 The process and the first process of forming the collector electrode 2 It includes a process. [Effects of the Invention]

[0015] As described above, according to the present invention, since a control electrode is provided to apply a voltage to the ledge layer, the high-frequency characteristics of the bipolar transistor can be improved while ensuring long-term reliability. [Brief explanation of the drawing]

[0016] [Figure 1A] Figure 1A is a cross-sectional view showing the configuration of a bipolar transistor according to an embodiment of the present invention. [Figure 1B] Figure 1B is a cross-sectional view showing the configuration of a bipolar transistor according to an embodiment of the present invention. [Figure 2A] Figure 2A is a cross-sectional view showing the state of a bipolar transistor during an intermediate step in the manufacturing process of a bipolar transistor according to an embodiment of the present invention. [Figure 2B] Figure 2B is a cross-sectional view showing the state of a bipolar transistor during an intermediate step in the manufacturing process of a bipolar transistor according to an embodiment of the present invention. [Figure 2C] Figure 2C is a cross-sectional view showing the state of a bipolar transistor during an intermediate step in the manufacturing process of a bipolar transistor according to an embodiment of the present invention. [Figure 2D] Figure 2D is a cross-sectional view showing the state of a bipolar transistor during an intermediate step in the manufacturing process of a bipolar transistor according to an embodiment of the present invention. [Figure 2E] Figure 2E is a cross-sectional view showing the state of a bipolar transistor during an intermediate step in the manufacturing process of a bipolar transistor according to an embodiment of the present invention. [Figure 2F]FIG. 2F is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2G] FIG. 2G is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2H] FIG. 2H is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2I] FIG. 2I is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2J] FIG. 2J is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2K] FIG. 2K is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2L] FIG. 2L is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2M] FIG. 2M is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2N] FIG. 2N is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2O] FIG. 2O is a cross-sectional view showing the state of the bipolar transistor in an intermediate step for explaining the method of manufacturing a bipolar transistor according to the embodiment of the present invention. [Figure 2P]Figure 2P is a cross-sectional view showing the state of a bipolar transistor during an intermediate step in the manufacturing process of a bipolar transistor according to an embodiment of the present invention. [Figure 3] Figure 3 is a cross-sectional view showing the configuration of a heterojunction bipolar transistor. [Modes for carrying out the invention]

[0017] Hereinafter, a bipolar transistor according to an embodiment of the present invention will be described with reference to Figures 1A and 1B. This bipolar transistor first comprises a collector layer 103 made of a compound semiconductor formed on a substrate 101, a base layer 104 made of a compound semiconductor formed on the collector layer 103, and an emitter layer 105 made of a compound semiconductor formed on the base layer 104, with an area smaller than that of the base layer 104 in a plan view.

[0018] In this embodiment, the collector layer 103 is formed on a subcollector layer 102 formed on the substrate 101. The emitter layer 105 is made of a different compound semiconductor than the base layer 104, and this bipolar transistor is a heterojunction bipolar transistor.

[0019] Furthermore, this heterojunction bipolar transistor is made of a compound semiconductor formed on the emitter layer 105 and includes an emitter cap layer 106 that is formed in an area smaller than the emitter layer 105 in a plan view. The stacked structure of the collector layer 103 and the base layer 104 forms a first mesa that is rectangular in a plan view, and the stacked structure of the emitter layer 105 and the emitter cap layer 106 forms a second mesa that is rectangular in a plan view. The second mesa has a smaller area than the first mesa in a plan view.

[0020] The element portion, including the collector layer 103, base layer 104, and emitter layer 105, has a rectangular (planar shape) in which the length in the first direction is longer than the length in the second direction perpendicular to the first direction when viewed from above. Figure 1A shows a cross-section of the plane perpendicular to the first direction, and Figure 1B shows a cross-section of the plane perpendicular to the second direction.

[0021] Furthermore, this heterojunction bipolar transistor includes a collector electrode 121 connected to the collector layer 103, a base electrode 122 formed on the base layer 104 surrounding the emitter layer 105 and spaced apart from the emitter layer 105, and an emitter electrode 123 formed on the emitter cap layer 106. The emitter electrode 123 is positioned directly above the emitter cap layer 106. The base electrode 122 is formed to surround the emitter layer 105 in a plan view. In addition, in the second direction of the element portion, the base electrode 122 has a connection portion with upper wiring (not shown).

[0022] Furthermore, this heterojunction bipolar transistor has a ledge structure, comprising a ledge layer 105a formed by the emitter layer 105 surrounding the emitter cap layer 106. In addition, this heterojunction bipolar transistor includes a control electrode 107 for applying a voltage (electric field) to the ledge layer 105a. The control electrode 107 is formed in isolation from the other electrodes.

[0023] Furthermore, in this embodiment, the heterojunction bipolar transistor includes a first insulating layer 108 formed in contact with the side surface of the emitter cap layer 106 and the surface of the ledge layer 105a. The control electrode 107 is formed on the ledge layer 105a via the first insulating layer 108. The first insulating layer 108 prevents the control electrode 107 from contacting the emitter cap layer 106. Here, the combined thickness of the first insulating layer 108 on the base layer 104 and the control electrode 107 is greater than that of the base electrode 122.

[0024] Furthermore, this heterojunction bipolar transistor may further include a second insulating layer 109 formed in contact with the side of the first insulating layer 108 on the side of the emitter cap layer 106 and the upper surface of the control electrode 107. The control electrode 107 and the second insulating layer 109 have portions that extend in the second direction of the element. In this extended portion, a contact hole 109a formed in the second insulating layer 109 enables connection between upper wiring (not shown) and the control electrode 107.

[0025] The substrate 101 can be made of InP that has been doped with Fe to increase its resistance, for example. The subcollector layer 102 can be made of InGaAs that has been doped with a high concentration of n-type impurities, for example. The subcollector layer 102 can also have a two-layer structure consisting of an InP layer on the substrate 101 side and an InGaAs layer formed on top of this layer.

[0026] The collector layer 103 can be made of, for example, InP doped with n-type impurities. The base layer 104 can be made of InGaSb doped with a high concentration of p-type impurities. The emitter layer 105 can be made of InP doped with a low concentration of n-type impurities. The emitter cap layer 106 can be made of InGaAs doped with a high concentration of n-type impurities.

[0027] In the bipolar transistor according to this embodiment, the potential of the ledge layer 105a can be controlled by the voltage applied to the control electrode 107. Typically, by applying a negative bias to the control electrode 107, depletion of the ledge layer 105a can be promoted, and ledge leakage current can be suppressed even when the ledge width is shortened. In other words, the ledge width can be miniaturized while maintaining current gain and reliability, and the high-frequency characteristics of the device can be improved.

[0028] Furthermore, in fine ledge structures, variations in current gain due to variations in ledge width between elements become a significant issue. In contrast, in a ledge structure (ledge layer 105a) equipped with control electrodes 107, the current gain variation between different elements can be reduced by adjusting the applied voltage to the control electrodes 107 of each element, and this is expected to reduce variations in the characteristics of the integrated circuit.

[0029] Next, the method for manufacturing a bipolar transistor according to the present invention will be described with reference to Figures 2A to 2P. Figures 2A to 2G, 2I, 2K, 2M, and 2O show cross-sections of a plane perpendicular to the first direction, while Figures 2H, 2J, 2L, 2N, and 2P show cross-sections of a plane perpendicular to the second direction.

[0030] The method for manufacturing a bipolar transistor described above is a method for manufacturing a bipolar transistor (heterojunction bipolar transistor) according to the embodiment described above. First, as shown in Figure 2A, a subcollector forming layer 202, a collector forming layer 203, a base forming layer 204, an emitter forming layer 205, and an emitter cap forming layer 206 are formed on a substrate 101 in the order described above (first step, second step, third step, fourth step).

[0031] For example, first, the subcollector formation layer 202 is formed by crystal growth (epitaxial growth) of InGaAs doped with a high concentration of n-type impurities. Next, the collector formation layer 203 is formed by crystal growth of InP doped with n-type impurities. Next, the base formation layer 204 is formed by crystal growth of InGaSb doped with a high concentration of p-type impurities. Next, the emitter formation layer 205 is formed by crystal growth of InP doped with a low concentration of n-type impurities. Next, the emitter cap formation layer 206 is formed by crystal growth of InGaAs doped with a high concentration of n-type impurities.

[0032] The thickness, doping concentration, and composition of each layer described above are set to optimal values ​​to obtain the desired electrical performance. Furthermore, from the viewpoint of maximizing the effect of the fine ledge structure, it is desirable to make the emitter formation layer 205, which will be the emitter layer 105, as thin as is acceptable for the electrical properties. Specifically, the thickness of the emitter formation layer 205 is preferably around 10 nm to 20 nm. Each of the above layers can be formed by well-known methods such as metal-organic vapor deposition or molecular beam epitaxy.

[0033] Next, as shown in Figure 2B, the emitter electrode 123 is formed on the emitter cap forming layer 206 (fifth step). For example, a mask with an opening is formed in the area where the emitter electrode 123 is to be formed, and the metal constituting the emitter electrode 123 is deposited on top of this. For example, the metal can be deposited by sputtering or vacuum deposition. After this, the emitter electrode 123 can be formed by removing (lifting off) the mask.

[0034] Next, the emitter cap layer 206 is patterned using the emitter electrode 123 as a mask to form the emitter cap layer 106 on the emitter cap layer 205, as shown in Figure 2C (sixth step). For example, the emitter cap layer 106 can be formed by etching (wet etching or dry etching) the emitter cap layer 206 using the emitter electrode 123 as a mask.

[0035] As described above, after forming the emitter cap layer 106, a first insulating film 208 is formed on the emitter forming layer 205 including the emitter electrode 123 and the emitter cap layer 106, as shown in Figure 2D (first 3 (Process) A first insulating layer 108 is formed from the first insulating film 208. For example, the first insulating film 208 can be formed by depositing an insulating material such as SiN or Al2O3 by chemical vapor deposition (CVD) or atomic layer deposition (ALD). Insulating materials such as SiN and Al2O3 can form relatively good interfaces with InP-based compound semiconductors.

[0036] The thickness of the first insulating film 208, which forms the first insulating layer 108, affects the modulation efficiency of the ledge potential by the control electrode 107. Furthermore, since the thickness of the first insulating film 208 is proportional to the ledge width, it is desirable to form the first insulating film 208 as thinly as possible while obtaining the desired insulation, and a thickness of about 10 nm to 100 nm is preferable.

[0037] Next, as shown in Figure 2E, a control electrode forming layer 207 is formed on the first insulating film 208 around the emitter electrode 123 and on the first insulating film 208 above the emitter cap layer 106 (first 4 (Process). For example, the control electrode formation layer 207 can be formed by depositing the metal constituting the control electrode 107 by sputtering or vacuum deposition. With this type of highly perpendicular anisotropic deposition method, metal is not deposited on the sides (sides) of the mesa structure formed by the already formed emitter cap layer 106 and emitter electrode 123, and the metal is selectively deposited on the surface of the first insulating film 208 parallel to the plane of the substrate 101.

[0038] The material constituting the control electrode formation layer 207 can be any metal that functions as the control electrode 107, such as Pt or Pd, which have high work functions. By constructing the control electrode from this type of metal, the surface potential of the ledge layer 105a, which is made of a compound semiconductor such as InP, can be increased, and the ledge layer 105a can be depleted at a low voltage. The thickness of the control electrode formation layer 207, like the first insulating film 208, affects the ledge width, so a thinner layer is preferable.

[0039] Next, as shown in Figure 2F, the second insulating film 209 is formed by covering the exposed portion of the first insulating film 208 on the side of the mesa structure formed by the emitter cap layer 106 and the emitter electrode 123, and the control electrode formation layer 207 (first 5(Process). The second insulating film 209 can be made of, for example, SiO2. For example, by depositing SiO2 by chemical vapor deposition, the second insulating film 209 can also be formed on the lateral parts of the mesa structure. As will be described later, the second insulating film 209 is made of a different insulating material than the first insulating film 208, in order to etch the first insulating film 208 using the second insulating layer 109 formed from the second insulating film 209 as a mask.

[0040] Next, the second insulating film 209 is patterned (etched) to form the second insulating layer 109 as shown in Figures 2G and 2H (first 6 (Process). For example, by performing an etching process using dry etching with high perpendicular anisotropy, a sidewall-like second insulating layer 109 can be formed on the side of the mesa structure formed by the emitter cap layer 106 and the emitter electrode 123, as shown in Figure 2G. For example, the above etching process can be performed by reactive ion etching (ICP-RIE) using high-frequency inductively coupled plasma with fluorine gas.

[0041] Furthermore, in order to provide a connection between the upper wiring and the control electrode 107 at one end of the element portion in the first direction, as shown in Figure 2H, a mask pattern 231 is used to form a portion on the side wall-shaped second insulating layer 109 that extends in a direction parallel to the plane of the substrate 101.

[0042] Next, the control electrode 107 is formed by etching the control electrode formation layer 207, as shown in Figures 2I and 2J (Step 7). In the step of forming the control electrode 107, the emitter cap layer 106 has already been formed. Using the second insulating layer 109 (mask pattern 231) as a mask, the control electrode 107 can be formed by etching (patterning) the control electrode formation layer 207, for example, by reactive ion etching. Here, by adjusting the dry etching conditions and gas type, a slight undercut is introduced into the formed control electrode 107.

[0043] As described above, after forming the second insulating layer 109 and the control electrode 107, the first insulating film 208 is patterned to form the first insulating layer 108 on the side surface of the emitter cap layer 106, as shown in Figures 2K and 2L (first 7 (Process) Using the second insulating layer 109 (mask pattern 231) as a mask, the first insulating film 208 can be formed by etching it, for example, by reactive ion etching. This etching process also forms the first insulating layer 108 on the surface of the area that will become the ledge layer 105a of the emitter formation layer 205. The first insulating layer 108 is formed in contact with the side surface of the emitter cap layer 106 and also in contact with the surface of the area that will become the ledge layer 105a of the emitter formation layer 205. Here, by adjusting the dry etching conditions and gas type, a slight undercut is made in the first insulating layer 108 formed beneath the second insulating layer 109.

[0044] As described above, after forming the control electrode 107 and the first insulating layer 108, the emitter formation layer 205 is patterned to form the emitter layer 105 on the base formation layer 204, as shown in Figures 2M and 2N (step 8). The emitter formation layer 105 can be formed by wet etching (patterning) the emitter formation layer 205 using the mesa formed by the emitter electrode 123, the control electrode 107, the first insulating layer 108, and the second insulating layer 109 as masks. The emitter formation layer 205, which is made of InP, can be selectively etched using a hydrochloric acid-based etching solution without etching the base formation layer 204, which is made of InGaSb.

[0045] As described above, after forming the emitter layer 105, a base electrode 122 is formed on the base forming layer 204 surrounding the emitter layer 105, as shown in Figures 2O and 2P (9th step). For example, a mask with an opening is formed where the base electrode 122 is to be formed, and the metal constituting the base electrode 122 is deposited on top of this mask. For example, the metal can be deposited by sputtering or vacuum deposition. After this, the base electrode 122 can be formed by removing (lifting off) the mask.

[0046] The thickness of the base electrode 122 is formed to be thinner than the sum of the thickness of the control electrode 107 and the thickness of the first insulating layer 108. In other words, the combined thickness of the first insulating layer 108 on the base layer 104 and the control electrode 107 is formed to be thicker than the base electrode 122. As mentioned above, in etching using the second insulating layer 109 as a mask, by forming undercuts on the control electrode 107 and the first insulating layer 108, the second insulating layer 109 acts as a eaves, preventing the emitter electrode 123 and the control electrode 107 from coming into contact with the base electrode 122.

[0047] As described above, after forming the base electrode 122, the base forming layer 204 is patterned to form the base layer 104 on the collector forming layer 203 ( 10 (Process). Next, after forming the base layer 104, the collector formation layer 203 is patterned to form the collector layer 103 on the subcollector formation layer 202 (substrate 101) (1 1 Step 1) Forming a collector electrode 121 on the subcollector forming layer 202 (1 2 (Process). The subcollector forming layer 202 is patterned to form the subcollector layer 102. In addition, contact holes 109a are formed in the second insulating layer 109 in the portion of the control electrode 107 and the element portion of the second insulating layer 109 that extends in the second direction.

[0048] In the above, we have described in detail the npn-type InP / GaAsSb-based HBT on an InP substrate, which is promising for realizing ultra-high-speed integrated circuits. However, similar effects are also effective for other HBTs, specifically InP / InGaAs-based HBTs and InP-based HBTs formed on SiC heat dissipation substrates.

[0049] As described above, according to the present invention, since a control electrode is provided to apply a voltage to the ledge layer, it becomes possible to improve the high-frequency characteristics of the bipolar transistor while ensuring long-term reliability.

[0050] It should be noted that the present invention is not limited to the embodiments described above, and it is clear that many modifications and combinations can be implemented within the technical concept of the present invention by those with ordinary skill in the art. [Explanation of symbols]

[0051] 101...Substrate, 102...Subcollector layer, 103...Collector layer, 104...Base layer, 105...Emitter layer, 105a...Ledge layer, 106...Emitter cap layer, 107...Control electrode, 108...First insulating layer, 109...Second insulating layer, 109a...Contact hole, 121...Collector electrode, 122...Base electrode, 123...Emitter electrode.

Claims

1. A collector layer made of a compound semiconductor formed on a substrate, A base layer made of a compound semiconductor formed on the collector layer, An emitter layer made of a compound semiconductor formed on the base layer, having a smaller area than the base layer in a plan view, An emitter cap layer, which is made of a compound semiconductor formed on the emitter layer and has a smaller area than the emitter layer in a plan view, A collector electrode connected to the collector layer, A base electrode formed on the base layer surrounding the emitter layer and spaced apart from the emitter layer, An emitter electrode formed on the emitter cap layer, A control electrode that applies a voltage to the ledge layer formed by the emitter layer around the emitter cap layer, A method for manufacturing a bipolar transistor, comprising the control electrode being formed in an insulated manner from other electrodes, A first step is to form a collector formation layer made of a compound semiconductor on the substrate, A second step involves forming a base layer made of a compound semiconductor on the collector formation layer, A third step involves forming an emitter formation layer made of a compound semiconductor on the base formation layer, A fourth step involves forming an emitter cap formation layer made of a compound semiconductor on the emitter formation layer, A fifth step involves forming the emitter electrode on the emitter cap forming layer, A sixth step involves patterning the emitter cap forming layer using the emitter electrode as a mask to form the emitter cap layer on top of the emitter forming layer, A seventh step is to form the control electrode after forming the emitter cap layer, An eighth step is to form the emitter layer on the base layer by patterning the emitter layer after forming the control electrode, A ninth step is to form the base electrode on the base forming layer surrounding the emitter layer after the emitter layer has been formed, A tenth step involves forming the base electrode, then patterning the base forming layer to form the base layer on top of the collector forming layer, An eleventh step involves forming the base layer, then patterning the collector forming layer to form the collector layer on the substrate, The 12th step of forming the collector electrode and A method for manufacturing a bipolar transistor equipped with [a specific feature].

2. In the method for manufacturing a bipolar transistor according to claim 1, A thirteenth step involves forming the emitter cap layer, followed by forming a first insulating film on the emitter forming layer including the emitter electrode and the emitter cap layer, A 14th step is to form a control electrode forming layer on the first insulating film around the emitter electrode and on the first insulating film above the emitter cap layer, A 15th step of forming a second insulating film by covering the exposed portion of the first insulating film and the control electrode forming layer, A 16th step involves patterning the second insulating film to form a second insulating layer on the side of the emitter electrode and the emitter cap layer, The process includes a 17th step of forming the second insulating layer and then patterning the first insulating film to form a first insulating layer that is in contact with the side surface of the emitter cap layer and the surface of the ledge layer, The seventh step involves forming the control electrode by patterning the control electrode formation layer using the second insulating layer as a mask. The eighth step involves forming the emitter layer by patterning the emitter formation layer using the first insulating layer as a mask. A method for manufacturing a bipolar transistor characterized by the following:

3. In the method for manufacturing a bipolar transistor according to claim 2, A method for manufacturing a bipolar transistor, characterized in that the combined thickness of the first insulating layer on the base layer and the control electrode is formed to be thicker than the base electrode.

Citation Information

Patent Citations

  • Heterojunction bipolar transistor