Indication device
The liquid crystal display device addresses issues of aperture ratio and contrast by employing a structured design with conductive oxide semiconductor films and insulating layers, resulting in brighter and more contrasted reflective displays.
Patent Information
- Application Number
- JP2025137609
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2015-03-27
- Filing Date
- 2025-08-21
- Publication Date
- 2026-11-19
- Estimated Expiration
- 2036-03-15
AI Technical Summary
Existing liquid crystal display devices face challenges in achieving a high pixel aperture ratio, bright image display, and improved contrast, particularly in reflective displays using metal oxide semiconductors.
The liquid crystal display device incorporates a specific structure with first and second pixel electrodes, a transistor, capacitive elements, and multiple insulating films, utilizing conductive oxide semiconductor films to enhance pixel aperture ratio and image contrast, including textured surfaces and optimized insulating films to control resistivity and carrier density.
The solution results in a liquid crystal display device with increased aperture ratio, brighter images, and improved contrast, suitable for reflective displays, by optimizing the conductive oxide semiconductor films and insulating layers to enhance light reflection and diffusion.
Smart Images

Figure 0007954253000002 
Figure 0007954253000003 
Figure 0007954253000004
Abstract
Description
[Technical Field]
[0001] One aspect of the present invention relates to a liquid crystal display device, or an electronic device using the liquid crystal display device. In particular, the present invention relates to a reflective liquid crystal display device. Alternatively, one aspect of the present invention relates to a product, method, or manufacturing The present invention relates to a method, or one aspect of the present invention relates to a process, machine, manufacture, or This invention relates to a composition of matter. One aspect of the present invention relates to a semiconductor device, a table The present invention relates to display devices, electronic devices, methods for manufacturing them, or methods for driving them. [Background technology]
[0002] It is used in many flat panel displays, such as liquid crystal displays and light-emitting displays. The transistors being described are amorphous silicon, single-crystal silicon formed on a glass substrate. It is made of silicon semiconductors such as silicon or polycrystalline silicon. Transistors, which use semiconductors, are also used in integrated circuits (ICs), among other applications.
[0003] In recent years, metal oxides exhibiting semiconductor properties have been used in transistors instead of silicon semiconductors. The technology is attracting attention. In this specification, metal oxides exhibiting semiconductor properties are referred to as oxides. We will refer to them as semiconductors. For example, as oxide semiconductors, zinc oxide or In-Ga- A transistor was fabricated using a zinc oxide, and this transistor was used as a switch for the pixels of a display device. Technologies for use in chnothing elements and the like have been disclosed (see Patent Documents 1 and 2). [Prior art documents] [Patent Documents]
[0004] [Patent Document 1] Japanese Patent Publication No. 2007-123861 [Patent Document 2] Japanese Patent Publication No. 2007-96055 [Overview of the Initiative] [Problems that the invention aims to solve]
[0005] One aspect of the present invention provides a liquid crystal display device comprising a conductive oxide semiconductor film. This is one of the challenges. Alternatively, one aspect of the present invention provides a liquid crystal display device with an increased pixel aperture ratio. One of the objectives is to provide. Alternatively, one aspect of the present invention is that the contrast of the displayed image is One of the objectives is to provide a liquid crystal display device that is high-performance and produces bright images. One aspect of the invention aims to provide a novel liquid crystal display device and the like.
[0006] Furthermore, the description of these problems does not preclude the existence of other problems. One approach does not require that all of these issues be resolved. The title will become clear from the description in the specification, drawings, claims, etc. It is possible to extract other issues from the descriptions in the drawings, claims, etc. [Means for solving the problem]
[0007] One aspect of the present invention involves a first pixel electrode, a second pixel electrode, and the first pixel electrode electrically A connected transistor, a capacitive element electrically connected to the transistor, and a first insulation A liquid crystal display device having a film, a second insulating film, and a third insulating film, wherein a transistor It consists of a gate electrode, a gate insulating film provided in contact with the gate electrode, and a gate insulating film in contact with the gate insulating film. A first oxide semiconductor film is provided and is positioned to overlap with the gate electrode, and a first acid It has a source electrode and a drain electrode electrically connected to a semiconductor film, and the capacitive element One of the pair of electrodes includes a second oxide semiconductor film, and the first insulating film is a first oxide semiconductor The second insulating film is provided on the body film, and the second oxide semiconductor film is the second insulating film and the first insulating film. The third insulating film is provided on the second oxide semiconductor film so as to be sandwiched between the films, and the third insulating film is The second pixel electrode is provided on top of the end of the first pixel electrode, and the second pixel electrode is provided on the third insulating film. This is a liquid crystal display device characterized by the following features.
[0008] Furthermore, the third insulating film and the second pixel electrode are superimposed such that their edges generally coincide. The above-described liquid crystal display device is also one embodiment of the present invention.
[0009] Furthermore, it has a first colored film and a second colored film, the first colored film is on the first pixel electrode. The above-mentioned liquid crystal display device is also provided, and the second colored film is provided on the second pixel electrode. This is one aspect of the invention.
[0010] Furthermore, one aspect of the present invention includes a first pixel electrode, a second pixel electrode, a conductive film, and a first pixel A transistor electrically connected to an elementary electrode, and a capacitive element electrically connected to the transistor. A liquid crystal display device having a child, a first insulating film, a second insulating film, and a third insulating film. A transistor consists of a gate electrode, a gate insulating film provided in contact with the gate electrode, and A first oxide semiconductor is provided in contact with the electrode insulating film and in a position superimposed on the gate electrode. A body membrane, and source and drain electrodes electrically connected to the first oxide semiconductor film, The capacitive element has a pair of electrodes, one of which includes a second oxide semiconductor film, and the first insulating film is The second insulating film is provided on the first oxide semiconductor film, and the second oxide semiconductor film is provided on the first insulating film. A second oxide semiconductor film is provided so as to be sandwiched between the edge film and the second insulating film, The third insulating film has a region that overlaps with the second pixel electrode and the conductive film, and the conductive film overlaps with the first pixel This is a liquid crystal display device characterized by being electrically connected to electrodes.
[0011] Furthermore, the third insulating film is provided on the first and second pixel electrodes, and the conductive film is, The above-mentioned liquid crystal display device, provided on a third insulating film, is also one embodiment of the present invention.
[0012] Furthermore, the first pixel electrode and the third insulating film are provided on a conductive film, and the second pixel electrode is, The above-mentioned liquid crystal display device, provided on a third insulating film, is also one embodiment of the present invention.
[0013] Furthermore, the conductive film has a region that overlaps with the second pixel electrode via the third insulating film, as described above. A liquid crystal display device is also one aspect of the present invention.
[0014] Furthermore, the liquid crystal display device described above, in which the other electrode of a pair of capacitive elements includes a first pixel electrode, is also a liquid crystal display device. This is one aspect of the invention.
[0015] Furthermore, the transistor is positioned to overlap the first insulating film and the first oxide semiconductor film. The above-described liquid crystal display device having a second oxide semiconductor film is also one embodiment of the present invention. .
[0016] Furthermore, in the above liquid crystal display device, the first oxide semiconductor film and the second oxide semiconductor film In-M-Zn oxide (where M is Al, Ti, Ga, Y, Zr, La, Ce, Nd, Sn) It is preferable that (or represents Hf).
[0017] Furthermore, in the above liquid crystal display device, the first insulating film contains oxygen, and the second insulating film contains hydrogen It is preferable to include it.
[0018] Furthermore, an electric device having the above-mentioned liquid crystal display device, a switch, a speaker, a display unit or housing, Sub-devices are also an embodiment of the present invention. [Effects of the Invention]
[0019] According to one aspect of the present invention, a liquid crystal display device is provided that comprises a conductive oxide semiconductor film. This is possible. Alternatively, according to one aspect of the present invention, a liquid crystal display device with an increased aperture ratio is provided. This is possible. Alternatively, according to one aspect of the present invention, the contrast of the displayed image is high, and A liquid crystal display device that displays a bright image can be applied. Alternatively, according to one aspect of the present invention This allows us to provide novel liquid crystal display devices and the like.
[0020] Furthermore, the description of these effects does not preclude the existence of other effects. One embodiment does not necessarily have to possess all of these effects. Furthermore, other effects may be considered. This will become clear from the description in the specification, drawings, claims, etc., and the specification, drawings It is possible to extract effects other than those mentioned above from the descriptions in the surfaces, claims, etc. [Brief explanation of the drawing]
[0021] [Figure 1] A top view and a cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 2] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 3] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 4] A cross-sectional view showing one embodiment of a method for manufacturing a liquid crystal display device. [Figure 5] A cross-sectional view showing one embodiment of a method for manufacturing a liquid crystal display device. [Figure 6]A cross-sectional view showing one embodiment of a method for manufacturing a liquid crystal display device. [Figure 7] A cross-sectional view showing one embodiment of a method for manufacturing a liquid crystal display device. [Figure 8] A cross-sectional view showing one embodiment of a method for manufacturing a liquid crystal display device. [Figure 9] A top view and a cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 10] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 11] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 12] A top view and a cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 13] A top view showing one form of a liquid crystal display device and a circuit diagram showing one form of a pixel. [Figure 14] A top view showing one embodiment of a liquid crystal display device. [Figure 15] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 16] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 17] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 18] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 19] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 20] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 21] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 22] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 23] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 24] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 25] A cross-sectional view showing one embodiment of a liquid crystal display device. [Figure 26] High-resolution TEM image with Cs correction in cross-section of CAAC-OS, and schematic cross-sectional diagram of CAAC-OS. [Figure 27] High-resolution TEM image with Cs correction in the plane of CAAC-OS. [Figure 28] A diagram illustrating the XRD structural analysis of CAAC-OS and single-crystal oxide semiconductors. [Figure 29] A figure showing the electron diffraction pattern of CAAC-OS. [Figure 30] A diagram showing the changes in the crystalline structure of In-Ga-Zn oxide due to electron irradiation. [Figure 31] A diagram illustrating the CAAC-OS film deposition method. [Figure 32] A diagram illustrating the crystal structure of InMZnO4. [Figure 33] A diagram illustrating the CAAC-OS film deposition method. [Figure 34] A top view and cross-sectional view showing an example of a transistor. [Figure 35] A cross-sectional view showing an example of a transistor. [Figure 36] A diagram illustrating the band structure. [Figure 37] A cross-sectional view showing an example of a transistor. [Figure 38] A top view illustrating the configuration of the display device. [Figure 39] A top view illustrating the configuration of pixels arranged on a display device. [Figure 40] A cross-sectional diagram illustrating the cross-sectional configuration of a display device. [Figure 41] A cross-sectional view illustrating the cross-sectional configuration of the first display unit of the display device. [Figure 42] A cross-sectional diagram illustrating the cross-sectional configuration of the second display unit of the display device. [Figure 43] A cross-sectional diagram illustrating the cross-sectional configuration of a display device. [Figure 44] A cross-sectional view illustrating the cross-sectional configuration of the first display unit of the display device. [Figure 45] A cross-sectional diagram illustrating the cross-sectional configuration of the second display unit of the display device. [Figure 46] A diagram illustrating electronic devices. [Figure 47] A diagram illustrating electronic devices. [Figure 48] A figure showing the display results of a liquid crystal display device according to an embodiment. [Modes for carrying out the invention]
[0022] The embodiments of the present invention will be described in detail below with reference to the drawings. However, the present invention One aspect is not limited to the following description, and without departing from the spirit and scope of the present invention, It will be readily apparent to those skilled in the art that the form and details can be changed in various ways. Therefore, this One aspect of the invention is not limited to the description of the embodiments shown below. Furthermore, in the embodiments described below, the same part or a part having a similar function is The same reference numerals or hatch patterns are used in common across different drawings, and their repetition is prohibited. The explanation will be omitted.
[0023] In each figure described herein, the size, film thickness, or region of each component is clearly indicated. It may be exaggerated for clarity. Therefore, it is not necessarily limited to that scale. .
[0024] Furthermore, the ordinal numbers such as "1st," "2nd," etc. used in this specification are used to avoid mixing of constituent elements. This is a selection and not a numerical limit. Therefore, for example, "the first" This can be explained by substituting "the second" or "the third" as appropriate.
[0025] Furthermore, in this specification, the terms "membrane" and "layer" are interchangeable. It is possible to change the term. For example, the term "conductive layer" can be changed to the term "conductive film." It may be possible to change it. Or, for example, change the term "insulating film" to "insulating layer". In some cases, it may be possible to change the terminology to this.
[0026] In this specification, "ends generally coincide" means that the ends do not completely overlap, and the top This includes situations where one layer is located inside the lower layer, or where the upper layer is located outside the lower layer.
[0027] Furthermore, even when the term "semiconductor" is used in this specification, for example, if the conductivity is If the value is sufficiently low, it may have the properties of an "insulator". Also, "semiconductor" and " The term "insulator" has an ambiguous boundary and may not be strictly distinguishable in some cases. Therefore, this specification... The term "semiconductor" as used in this document may sometimes be replaced with "insulator." Similarly, this In some cases, the term "insulator" as used in specifications, etc., can be replaced with "semiconductor." In some cases, the term "insulator" as used in this specification may be replaced with "semi-insulator." .
[0028] Furthermore, even when the term "semiconductor" is used in this specification, for example, if the conductivity is If the value is sufficiently high, it may possess the properties of a "conductor." Also, "semiconductor" and " The term "conductor" has an ambiguous boundary and may not be strictly distinguishable in some cases. Therefore, this specification... The term "semiconductor" as used in this document may sometimes be replaced with "conductor." Similarly, this In some cases, the term "conductor" as used in specifications, etc., can be replaced with "semiconductor."
[0029] Note that the "source" and "drain" functions of a transistor are different for transistors with opposite polarities. When adopting this method, or when the direction of current changes during circuit operation, the configuration may be reversed. Therefore, in this specification, the terms "source" and "drain" are interchangeable. It may be used in this way.
[0030] In this specification, patterning refers to the process using photolithography. However, patterning is not limited to the photolithography process, but also applies to photolithography. Other processes besides the photolithography process can also be used. The scum will be removed after etching.
[0031] In this specification, a silicon oxidizride film is defined as having a composition that is more acidic than nitrogen. This refers to a membrane with a high element content, preferably containing 55 atomic% or more and 65 atomic% or less of oxygen, and 1 atomic% of nitrogen. Atomic percent to 20 atomic percent, silicon 25 atomic percent to 35 atomic percent, hydrogen 0.1 atomic percent This refers to substances that are included in a range of 10% to 10 atomic percent. A silicon nitride film is a film containing these substances. As a component, it refers to a membrane in which the nitrogen content is higher than the oxygen content, preferably with nitrogen content of 55 atomic percent or more. 5 atomic% or less, oxygen 1 atomic% to 20 atomic%, silicon 25 atomic% to 35 atomic% This refers to substances containing hydrogen in a concentration range of 0.1 atomic% to 10 atomic% or less.
[0032] (Embodiment 1) In this embodiment, a liquid crystal display device according to one aspect of the present invention will be described using Figures 1 to 8. I will reveal it.
[0033] <Example configuration of a liquid crystal display device> Figure 1(A) is a top view of a liquid crystal display device according to one embodiment of the present invention, and Figure 1(B) is a top view of Figure 1( This corresponds to the cross-sectional view of the section between the dashed lines A and B, and between the dashed lines C and D in A). Oh, in Figure 1(A), to avoid complexity, some of the components of the liquid crystal display device are shown. (Gate insulating film, etc.) are omitted in the illustration. Note that in the top view of the transistor, In subsequent drawings, as with Figure 1(A), some components may be omitted from the illustration. ru.
[0034] The dashed line AB in Figure 1(A) indicates the channel length direction of transistor 150. The dashed line CD indicates the channel width direction of transistor 150. In this context, the channel length direction of a transistor refers to the source (source region or source electrode) and Between the drain (drain region or drain electrode), the direction in which carriers move is This means that the channel width direction is perpendicular to the channel length direction in a plane horizontal to the substrate. It indicates direction.
[0035] The liquid crystal display device shown in Figures 1(A) and 1(B) includes a transistor containing a first oxide semiconductor film 110. It has a zista 150 and a capacitive element 160 which includes an insulating film between a pair of electrodes. In element 160, one of the pair of electrodes is a second oxide semiconductor film 111, and the pair of electrodes The other electrode is a conductive film 120.
[0036] The transistor 150 has a gate electrode 104 on the substrate 102 and a gate electrode 104 on the substrate 102. An insulating film 108 that functions as an insulating film, and a gate electrode 104 superimposed on the insulating film 108. A first oxide semiconductor film 110 at a certain position, and a source electrode 1 on the first oxide semiconductor film 110. It has 12a and drain electrode 112b. In other words, transistor 150 is first The oxide semiconductor film 110 and the gate insulating film provided in contact with the first oxide semiconductor film 110 An insulating film 108 that functions as a film, and a first oxide semiconductor provided in contact with the insulating film 108. A gate electrode 104 is provided at a position overlapping with the film 110, and the first oxide semiconductor film 110 It has a source electrode 112a and a drain electrode 112b that are electrically connected to it. The transistor 150 shown in Figures 1(A) and (B) is a so-called bottom-gate structure.
[0037] Furthermore, on transistor 150, more specifically, the first oxide semiconductor film 110, source power Insulating films 114, 116, 118, and 119 are formed on electrode 112a and drain electrode 112b. The insulating films 114, 116, and 118 are used as protective insulating films for transistor 150. It has the function of a planarizing film. The insulating film 119 has the function of a planarizing film. Also, insulating film 114 At 116, 118, and 119, an opening 143 is formed that reaches the drain electrode 112b. Therefore, a conductive film 120 is formed on the insulating film 119 so as to cover the opening 143. The conductive film 120 is electrically connected to the transistor 150. The conductive film 120 is on the liquid crystal surface. It functions as a pixel electrode in a display device.
[0038] Capacitive element 160 functions as one of a pair of electrodes on the insulating film 116. A second oxide semiconductor film 111 and a dielectric film that functions on the second oxide semiconductor film 111. Insulating films 118, 119 and a second oxide semiconductor film 111 via insulating films 118, 119 A conductive film 120 having the function of the other electrode of a pair of electrodes at superimposed positions, In other words, the conductive film 120 has the function of both a pixel electrode and a capacitive element electrode. ru.
[0039] The transistor 150, the capacitive element 160, and the conductive film 120 shown in Figures 1(A) and (B) Therefore, it is possible to constitute one pixel of a liquid crystal display device.
[0040] Furthermore, the insulating film 130 is provided on top of the edge of the conductive film 120, and on the insulating film 130 A conductive film 121 is provided. The conductive film 121 includes, for example, a transistor 150. It functions as a pixel electrode for a pixel and adjacent pixels.
[0041] The conductive film 120 and the conductive film 121 are insulated by the insulating film 130. This eliminates the gap between the conductive film 120 and the conductive film 121 in the upper surface shape. Having such a configuration, the liquid crystal display device according to one aspect of the present invention increases the aperture ratio of the pixels. This can be achieved. Furthermore, by increasing the aperture ratio of the pixels, the contrast of the displayed image is increased. Furthermore, it can be used as a reflective liquid crystal display device that produces bright images.
[0042] Furthermore, since the conductive film 121 is provided on the insulating film 130, the conductive film 121 and the common electrode The distance between (not shown in the diagram) and (hereinafter also referred to as the electrode distance) is defined as the distance between the conductive film 120 and the commo The distance between electrodes can be made shorter than the distance between electrodes of the N electrode. A liquid crystal display device according to one aspect of the present invention is a liquid crystal display device. A liquid crystal element is formed by pixel electrodes and a common electrode that sandwich a layer having crystals (not shown). The common electrode is then given a common potential at each pixel. Layers (for example, R (red), G (green), B (blue), or R, G, B, Y (yellow), etc.) are assigned to pixels. If present, shorten (or lengthen) the inter-electrode distance of pixels having a colored layer of a specific color. This allows you to adjust the color tone of the displayed image.
[0043] In Figure 1(B), the insulating film 130 and the conductive film 121 have edges that roughly coincide with each other. Although they are provided in an overlapping manner, they are not limited to this. As shown in Figure 2(A), The edge film 130 is provided only near the edge of the conductive film 120 so as to cover the edge of the conductive film 120. It may also be possible. Furthermore, the liquid crystal display device shown in Figures 1(A) and (B) has a conductive film 120 and a conductive Although the film 121 has a region where it overlaps via the insulating film 130, the conductive film 120 and the conductive film 1 21 does not need to have an overlapping region.
[0044] Furthermore, the surface of the insulating film 119 of the liquid crystal display device according to one aspect of the present invention is provided with irregularities. It is preferable that it is present. The irregularities on the surface of the insulating film 119 shown in Figure 2(B) are irregular in shape. This schematically represents the uneven structure, or so-called textured structure. Conductive film 120 and conductive film 1 Since 21 is provided on the insulating film 119, the texture structure of the insulating film 119 is the conductive film 1 This appears on the surfaces of 20 and the conductive film 121. As a result, light incident on these conductive films is diffusely reflected. Furthermore, conductive films 120 and 121 appear generally white macroscopically. By controlling the orientation of liquid crystals using poles, the contrast in reflective liquid crystal display devices can be improved. It can be improved. Furthermore, even if a textured structure is provided on the surface of the insulating film 130, stomach.
[0045] In a liquid crystal display device, the thickness of the insulating film 119 is adjusted according to the capacitance value required by the capacitive element 160. It can be adjusted as needed. Alternatively, a configuration without the insulating film 119 is also possible. Figure 3(A) An example of a cross-sectional view of a liquid crystal display device without an insulating film 119 is shown below. In Figure 3(A) The insulating film 118 functions as a dielectric film for the capacitive element 160.
[0046] Furthermore, the liquid crystal display device shown in Figure 3(A) has a second oxide semiconductor film 111 on an insulating film 116. a is provided. The second oxide semiconductor film 111a is formed simultaneously with the second oxide semiconductor film 111. By forming a film and etching it simultaneously, it is designed to overlap with the channel region of the transistor. It may be done. The second oxide semiconductor film 111a is, for example, the second oxide semiconductor film 1 Since film deposition, etching, and formation are performed simultaneously with 11, the same material is used. Therefore, the increase in process steps can be suppressed. However, the embodiments of the present invention One embodiment is not limited thereto. The second oxide semiconductor film 111a is the second oxide semiconductor The body membrane 111 may be formed by a different process.
[0047] The second oxide semiconductor film 111a is the first oxide which forms the channel region of the transistor 150. It has a region that overlaps with the oxide semiconductor film 110. Therefore, the second oxide semiconductor film 11 1a functions as the second gate electrode of transistor 150. Therefore, The second oxide semiconductor film 111a may be connected to the gate electrode 104. Or, The second oxide semiconductor film 111a is not connected to the gate electrode 104. Different signals or different potentials may be supplied. Transistor 1 shown in Figure 3(A) 50 is a so-called double-gate structure. With this configuration, transistor 15 The current driving capability of 0 can be improved. At this time, the gate of the second gate electrode The insulating films are insulating films 114 and 116.
[0048] Furthermore, transistor 150 has a second oxide semiconductor film 111a, and gate electrode 104 A configuration without this is also acceptable. The transistor 150 shown in Figure 3(B) is shown in Figure 3(A). Compared to the transistor 150 shown, it differs in that it does not have a gate electrode 104. Figure 3(B The transistor shown is a so-called top-gate structure, and the second oxide semiconductor film 111a is It functions as the first gate electrode.
[0049] Furthermore, the first oxide semiconductor film 110 functions as the channel region of the transistor 150. Furthermore, the second oxide semiconductor film 111 is one of the pair of electrodes of the capacitive element 160. Therefore, the second oxide semiconductor film 11 is better than the first oxide semiconductor film 110. The resistivity of 1 is low. Also, the first oxide semiconductor film 110 and the second oxide semiconductor film 111 are Preferably, they have the same metal element. The first oxide semiconductor film 110 and the second oxide semiconductor film By making the body film 111 a structure having the same metal element, the manufacturing equipment (for example, a film deposition apparatus, Since processing equipment (and other components) can be used in common, manufacturing costs can be reduced. .
[0050] Furthermore, even if wiring etc. formed separately with a metal film etc. is connected to the second oxide semiconductor film 111 Good. For example, when using the liquid crystal display shown in Figure 1 as the transistor and capacitive element of the pixel section... A metal film is formed to create a joint, routing, or gate wiring, and a second oxide semiconductor is applied to the metal film. A configuration that connects the body membrane 111 may also be used. The routing wiring or gate wiring, etc., may be made of metal. By forming it with a film, wiring resistance can be reduced, thereby suppressing signal delays and other issues. It is possible.
[0051] Furthermore, the insulating film 118 provided on the transistor 150 and used in the capacitive element 160 As such, an insulating film containing at least hydrogen is used. Also, the insulating film used in transistor 150 The insulating films 114 and 116 provided on the edge film 107 and the transistor 150 are as follows: An insulating film containing at least oxygen is used. Thus, transistor 150 and capacitive element 1 The insulating film used in 60, and the insulating film used on transistor 150 and capacitive element 160 By using an insulating film with the above configuration, the first oxide semiconductor of the transistor 150 Controlling the resistivity of the second oxide semiconductor film 111 of the conductive film 110 and the capacitive element 160. It is possible.
[0052] Furthermore, the insulating film used in the capacitive element 160, and the transistor 150 and the capacitive element 160 The insulating film used above has the following configuration, thereby the conductive film 120 and / or conductive film The flatness of 121 can be improved. Specifically, insulating films 114 and 116 are first oxidation The insulating film 118 is provided on the material semiconductor film 110, and the second oxide semiconductor film 111 is the insulating film. The second oxide semiconductor film 111 is provided so as to be sandwiched between 116 and the insulating film 118. This creates openings in the insulating films 114 and 116 at positions overlapping with the second oxide semiconductor film 111. The resistivity of the second oxide semiconductor film 111 can be controlled without providing such a structure. By doing so, in the liquid crystal display device shown in Figures 1(A) and (B), the conductive film 120 and the conductive The orientation of the liquid crystal formed on the film 121 can be improved.
[0053] In transistor 150, the first oxide semiconductor film 110 has a channel region and Because it is used in this way, it has a higher resistivity compared to the second oxide semiconductor film 111. On the other hand, the second Since the oxide semiconductor film 111 has the function of an electrode, the first oxide semiconductor film 110 and It has a lower resistivity in comparison.
[0054] Here, the resistivity of the first oxide semiconductor film 110 and the second oxide semiconductor film 111 is controlled. The method will be explained below.
[0055] <Method for controlling the resistivity of oxide semiconductor films> Acids that can be used in the first oxide semiconductor film 110 and the second oxide semiconductor film 111 The resistance of a semiconductor film depends on the oxygen vacancies and / or the concentration of impurities such as hydrogen and water within the film. It is a semiconductor material whose resistance can be controlled. Therefore, the first oxide semiconductor film 110 and a treatment to the second oxide semiconductor film 111 that increases the oxygen vacancy and / or impurity concentration, By selecting a treatment that reduces oxygen deficiency and / or impurity concentration, each acid The resistivity of the semiconductor film can be controlled.
[0056] Specifically, it is used in the second oxide semiconductor film 111 which functions as an electrode for the capacitive element 160. Plasma treatment is performed on an oxide semiconductor film to increase the oxygen vacancies in the oxide semiconductor film. , and / or by increasing impurities such as hydrogen and water in the oxide semiconductor film, It is possible to create oxide semiconductor films with high carrier density and low resistivity. A conductive film is formed by contacting a hydrogen-containing insulating film, and the hydrogen-containing insulating film, for example, insulating film 118 By diffusing hydrogen into the oxide semiconductor film, a high carrier density and low resistivity are achieved. It can be an oxide semiconductor film. The second oxide semiconductor film 111 is formed in the film as described above. Before the process of increasing the oxygen deficiency or diffusing hydrogen, the semiconductor is used It has the ability to function as a conductor after the process.
[0057] On the other hand, the first oxide semiconductor film 110 functions as the channel region of transistor 150. By providing insulating films 107, 114, and 116, the insulating films 106 and 1 containing hydrogen are provided. The configuration shall not come into contact with 18. At least one of the insulating films 107, 114, and 116 shall contain oxygen. By applying an insulating film, in other words, an insulating film capable of releasing oxygen, the first acid Oxygen can be supplied to the oxide semiconductor film 110. The first oxide semiconductor to which oxygen has been supplied The body membrane 110 becomes an oxide semiconductor film with high resistivity, as oxygen deficiencies in the membrane or at the interface are filled. For example, an insulating film capable of releasing oxygen is a silicon oxide film, or A silicon oxide nitride film can be used.
[0058] Furthermore, to obtain oxide semiconductor films with low resistivity, ion implantation and ion doping methods are used. Using methods such as plasma immersion ion implantation, hydrogen, boron, and ly N or nitrogen may be implanted into the oxide semiconductor film.
[0059] Furthermore, in order to obtain an oxide semiconductor film with low resistivity, the oxide semiconductor film is subjected to plasma treatment. It is permissible to do so. For example, typical plasma treatments include those using noble gases (He, Ne, A). Plasma using a gas containing one or more elements selected from r, Kr, Xe, hydrogen, and nitrogen Examples include plasma treatment. More specifically, plasma treatment in an Ar atmosphere, and mixing of Ar and hydrogen. Plasma treatment under a mixed gas atmosphere, plasma treatment under an ammonia atmosphere, Ar and ammonia Plasma treatment in a near-mixed gas atmosphere, or plasma treatment in a nitrogen atmosphere, etc. It can be listed.
[0060] As a result of the plasma treatment described above, the oxide semiconductor film has a lattice from which oxygen has been removed (or oxygen has been removed forms oxygen vacancies in the separated portion. The oxygen vacancies may become a factor that generates carriers . Furthermore, when hydrogen is supplied from an insulating film in the vicinity of the oxide semiconductor film, more specifically, in contact with the lower side or the upper side of the oxide semiconductor film, the oxygen vacancies and hydrogen bond to each other, which may generate electrons that are carriers .
[0061] On the other hand, an oxide semiconductor film in which oxygen vacancies are compensated and the hydrogen concentration is reduced can be referred to as a highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film. Here, the term "substantially intrinsic" means that the carrier density of the oxide semiconductor film is less than 8×10 11 / cm 3 , preferably less than 1×10 1 1 / cm 3 , more preferably less than 1×10 10 / cm 3 . A highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film has few carrier generation sources, and thus can have a low carrier density . Since the highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film has a low density of defect states, the density of trap states can be reduced . .
[0062] In addition, the highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film has an extremely low off-state current; even for an element with a channel width of 1×10 μm and a channel length of 10 μm, in the range where the voltage between the source electrode and the drain electrode (drain voltage) is from 1 V to 10 V, the off-state current can be a value lower than or equal to the measurement limit of a semiconductor parameter analyzer, that is, 1×10 6 -13 A or less . Accordingly, the above-described highly purified intrinsic or substantially highly purified intrinsic A first oxide semiconductor film 110a, which uses an oxide semiconductor film of a certain property, is used in the channel region. Transistor 150 exhibits minimal fluctuations in its electrical characteristics, resulting in a highly reliable transistor.
[0063] As the insulating film 118, for example, an insulating film containing hydrogen, or in other words, one that can release hydrogen. By using a suitable insulating film, typically a silicon nitride film, the second oxide semiconductor film 111 can be formed. Hydrogen can be supplied. An insulating film capable of releasing hydrogen includes... Hydrogen concentration is 1 × 10 22 atoms / cm 3 It is preferable that such an insulating film is By forming it in contact with the second oxide semiconductor film 111, it has an effect on the second oxide semiconductor film 111. In this way, hydrogen can be incorporated into the first oxide semiconductor film 110 and By changing the configuration of the insulating film in contact with the oxide semiconductor film 111, the oxide semiconductor film The resistivity can be controlled. Note that the insulating film 106 is made of the same material as insulating film 118. A material may be used. By using silicon nitride as the insulating film 106, from insulating film 107 The released oxygen is supplied to the gate electrode 104, which can suppress oxidation.
[0064] The hydrogen contained in the oxide semiconductor film reacts with the oxygen bonded to the metal atoms to form water. This forms an oxygen vacancy in the lattice (or the part from which oxygen has been removed). When hydrogen enters, electrons, which act as carriers, are sometimes generated. Also, some of the hydrogen In some cases, by bonding with oxygen atoms that bond with metal atoms, electrons, which act as carriers, can be generated. Therefore, the second oxide semiconductor film 111 is provided in contact with the insulating film containing hydrogen. This results in an oxide semiconductor film with a higher carrier density than the first oxide semiconductor film 110.
[0065] The first oxide semiconductor film 110 on which the channel region of transistor 150 is formed is hydrogen It is preferable that the first oxide semiconductor film 110 In this context, secondary ion mass spectrometry (SIMS) is used. The hydrogen concentration obtained by spectrometry is 2 × 10 20 atoms / cm 3 The following is preferably 5 × 10 19 atoms / cm 3 More preferably 1 × 10 19 atoms / cm 3 Below, 5 x 10 18 atoms / cm 3 Less than 1 × 10 1 8 atoms / cm 3 The following is more preferable: 5 x 10 17 atoms / cm 3 The following, Preferably 1 × 10 16 atoms / cm 3 The following applies:
[0066] On the other hand, the second oxide semiconductor film 111, which functions as an electrode for the capacitive element 160, is the first acid Oxide semiconductor film 110 has a higher hydrogen concentration and / or oxygen vacancy, and lower resistivity than oxide semiconductor film 110. It is a conductive film. The hydrogen concentration contained in the second oxide semiconductor film 111 is 8 × 10⁻⁶. 19 That's all. Preferably 1 × 10 20 atoms / cm 3 The above is more comfortable 5x10 20 That's all. Furthermore, compared to the first oxide semiconductor film 110, the second oxide semiconductor film 111 contains The hydrogen concentration is twice or more, preferably ten times or more. Also, the second oxide semiconductor film 1 The resistivity of 11 is 1 × 10⁻⁶ of the resistivity of the first oxide semiconductor film 110. -8 1×10 times more - 1 It is preferable that it be less than a multiple, typically 1 × 10⁻⁶. -3 Ωcm or more, 1 × 10 4 Ωcm not yet More preferably, the resistivity is 1 × 10⁻⁶. -3 Ωcm or more, 1 × 10 -1 It is less than Ωcm That's good.
[0067] Here, we will discuss the details of the other components of the liquid crystal display shown in Figures 1(A) and 1(B). Next, I will provide the following explanation.
[0068] <Circuit board> There are no major restrictions on the material of the substrate 102, but it should at least be able to withstand subsequent heat treatment. It must have heat resistance. For example, glass substrates, ceramic substrates, quartz substrates, etc. A fire substrate or the like may be used as substrate 102. Also, from silicon or silicon carbide Single-crystal semiconductor substrates, polycrystalline semiconductor substrates, compound semiconductor substrates such as silicon germanium SOI substrates and the like can also be applied, and semiconductor elements are provided on these substrates. The material may be used as the substrate 102. In addition, a glass substrate may be used as the substrate 102. In this case, the 6th generation (1500mm x 1850mm), the 7th generation (1870mm x 2200mm) m), 8th generation (2200mm x 2400mm), 9th generation (2400mm x 2800mm) m), by using large-area substrates such as the 10th generation (2950mm x 3400mm), A display device can be manufactured. Furthermore, a flexible substrate can be used as the substrate 102. The transistor 150, the capacitive element 160, etc., may be formed directly on the substrate.
[0069] In addition to these, various substrates can be used as substrate 102 to form transistors. This is possible. The type of circuit board is not limited to a specific one. As an example of such a circuit board... This includes plastic substrates, metal substrates, stainless steel substrates, and stainless steel wheels. Substrates having foil, tungsten substrates, substrates having tungsten foil, flexible substrates, Examples include laminated films, paper containing fibrous materials, or base films. Glass substrates. Examples include barium borosilicate glass, aluminoborosilicate glass, or soda glass. Examples include IMU glass. An example of a flexible substrate is polyethylene terephthalate (PE). T) Polyethylene naphthalate (PEN) and polyethersulfone (PES) are representative examples. These include plastics or flexible synthetic resins such as acrylic. Examples of films include polypropylene, polyester, polyvinyl fluoride, or poly Examples include polyvinyl chloride. Examples of base films include polyamide, polyimide, and inorganic vapor These include adhesive films or paper materials. In particular, semiconductor substrates, single crystal substrates, or SOI substrates. By manufacturing transistors using this method, variations in characteristics, size, or shape can be reduced. This allows for the manufacture of transistors with low current capacity, high current capability, and small size. When circuits are constructed using such transistors, the power consumption of the circuit can be reduced, or the circuit can be highly integrated. It is possible to achieve transformation.
[0070] Furthermore, a transistor is formed using one substrate, and then the transistor is transferred to another substrate. The transistor may be placed on one of the substrates on which the transistor is transposed. Examples include, in addition to the substrates on which the transistors described above can be formed, paper substrates, cellophane Fan substrates, stone substrates, wood substrates, fabric substrates (natural fibers (silk, cotton, linen), synthetic fibers (nylon)) , polyurethane, polyester) or regenerated fibers (acetate, cupro, rayon, These include recycled polyester, leather substrates, or rubber substrates. By using this method, it is possible to form transistors with good characteristics and transistors with low power consumption. This allows for the manufacture of durable devices, improved heat resistance, weight reduction, and thinner designs.
[0071] <First oxide semiconductor film and second oxide semiconductor film> The first oxide semiconductor film 110 and the second oxide semiconductor film 111 are at least indiu In (In), zinc (Zn), and M (Al, Ti, Ga, Y, Zr, La, Ce, Sn) It is preferable that the film includes an In-M-Zn oxide film containing a metal (such as Hf). Furthermore, in order to reduce variations in the electrical characteristics of transistors using the oxide semiconductor, Preferably, both include a stabilizer.
[0072] As stabilizers, metals such as gallium (Ga), sulfite, and sulfite are used, including the metals listed in M above. Zirconium (Sn), hafnium (Hf), aluminum (Al), or zirconium (Zr) These are some examples. Other stabilizers include lanthanides, such as lanthanum (La). , Cerium (Ce), Praseodymium (Pr), Neodymium (Nd), Samarium (Sm), Europium (Eu), Gadolinium (Gd), Terbium (Tb), Dysprosium ( Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium Examples include (Yb), lutetium (Lu), etc.
[0073] Oxide semiconductors constituting the first oxide semiconductor film 110 and the second oxide semiconductor film 111 For example, In-Ga-Zn oxides, In-Al-Zn oxides, In-Sn- Zn oxides, In-Hf-Zn oxides, In-La-Zn oxides, In-Ce-Z n-based oxides, In-Pr-Zn oxides, In-Nd-Zn oxides, In-Sm-Zn In-Eu-Zn oxides, In-Gd-Zn oxides, In-Tb-Zn oxides Oxides, In-Dy-Zn oxides, In-Ho-Zn oxides, In-Er-Zn acids In-Tm-Zn oxides, In-Yb-Zn oxides, In-Lu-Zn oxides In-Sn-Ga-Zn oxides, In-Hf-Ga-Zn oxides, In-Al- Ga-Zn oxides, In-Sn-Al-Zn oxides, In-Sn-Hf-Zn oxides In-Hf-Al-Zn oxides can be used.
[0074] In this context, In-Ga-Zn oxides are those that have In, Ga, and Zn as their main components. It means an oxide, and the ratio of In, Ga, and Zn is not specified. Other metal elements besides n may be present.
[0075] Furthermore, the first oxide semiconductor film 110 and the second oxide semiconductor film 111 are made of the above oxide They may have the same metal element. The first oxide semiconductor film 110 and the second oxide By using the same metal element for the semiconductor film 111, manufacturing costs can be reduced. For example, by using metal oxide targets with the same metal composition, manufacturing costs can be reduced. This can be achieved. Furthermore, by using a metal oxide target with the same metal composition, acid When processing a semiconductor film, the etching gas or etching solution is used in common. Yes, it is possible. However, the first oxide semiconductor film 110 and the second oxide semiconductor film 111 are identical. Even if they contain the same metal elements, their composition may differ. For example, transistors and capacitive elements During the manufacturing process, metal elements may detach from the film, resulting in a different metal composition.
[0076] Furthermore, when the first oxide semiconductor film 110 is an In-M-Zn oxide, the original In and M The ratio of offspring is preferably such that when the sum of In and M is taken as 100 atomic%, In is 2 Higher than 5 atomic%, M is less than 75 atomic%, and more preferably In is 34 The value must be higher than atomic%, and M must be less than 66 atomic%.
[0077] The first oxide semiconductor film 110 has an energy gap of 2 eV or more, preferably 2.5 The energy gap is eV or greater, more preferably 3eV or greater. Thus, acids with a wide energy gap. By using a synthetic semiconductor, the off-current of transistor 150 can be reduced.
[0078] The thickness of the first oxide semiconductor film 110 is 3 nm or more and 200 nm or less, preferably 3 nm. The wavelength should be 100 nm or less, and more preferably 3 nm to 50 nm.
[0079] The first oxide semiconductor film 110 is In-M-Zn oxide (where M is Al, Ga, Y, Zr, L). In the case of a, Ce, or Nd, sputtering is used to deposit In-M-Zn oxide films. The atomic ratio of the metal elements in the ring target is preferably such that In ≥ M and Zn ≥ M. The atomic ratio of metal elements in such a sputtering target is In:M:Zn= 1:1:1, In:M:Zn=1:1:1.2, In:M:Zn=3:1:2, In:M Examples include Zn=1:3:4 and In:M:Zn=1:3:6. The atomic ratio of the oxide semiconductor film 110 is as an error for the above sputtering process. This includes a variation of plus or minus 40% in the atomic ratio of metallic elements contained in the GET.
[0080] As the first oxide semiconductor film 110, an oxide semiconductor film with a low carrier density is used. For example, the first oxide semiconductor film 110 has a carrier density of 1 × 10⁻⁶ 17 pieces / cm 3 below, Preferably 1 × 10 15 pieces / cm 3 More preferably 1 × 10 13 pieces / cm 3 below , more preferably 1 × 10 11 pieces / cm 3 The following oxide semiconductor films are used.
[0081] Furthermore, this is not limited to the semiconductor characteristics and electrical characteristics (field effect) of the transistor as needed. A suitable composition should be used depending on the fruit mobility, threshold voltage, etc. To obtain the semiconductor characteristics of the transistor, the carrier density of the first oxide semiconductor film 110 The impurity concentration, defect density, atomic ratio of metal elements to oxygen, interatomic distance, density, etc., should be appropriate. It is preferable to do so.
[0082] In the first oxide semiconductor film 110, silicon and carbon, which are among the Group 14 elements, are included. When this occurs, oxygen vacancies increase in the first oxide semiconductor film 110, causing it to become n-type. Therefore, the concentration of silicon and carbon in the first oxide semiconductor film 110 (secondary ion mass) The concentration obtained by the analytical method is 2 × 10 18 atoms / cm 3 The following is preferably 2× 10 17 atoms / cm 3 The following applies:
[0083] Furthermore, in the first oxide semiconductor film 110, an a obtained by secondary ion mass spectrometry is obtained. The concentration of potassium metal or alkaline earth metal is 1 × 10⁻⁶ 18 atoms / cm 3 Below, good Mashiku is 2 x 10 16 atoms / cm 3 The following applies: Alkali metals and alkaline earth metals These molecules can generate carriers when bonded to oxide semiconductors, which can be used in the off-voltage phase of transistors. The flow may increase. For this reason, the alkali metal of the first oxide semiconductor film 110 Alternatively, it is preferable to reduce the concentration of alkaline earth metals.
[0084] Furthermore, if nitrogen is present in the first oxide semiconductor film 110, electrons, which are carriers, are generated. As a result, the carrier density increases, making it easier to convert to n-type semiconductors. Transistors using oxide semiconductors tend to exhibit normally-on characteristics. Therefore, the oxide semiconductor in question is prone to this. In the membrane, it is preferable that nitrogen is reduced as much as possible, for example, secondary ion mass The nitrogen concentration obtained by the analytical method is 5 × 10⁻⁶ 18 atoms / cm 3 The following is preferable It seems so.
[0085] Further, the first oxide semiconductor film 110 may have, for example, a non-single-crystal structure. The non-single-crystal structure is , for example, CAAC-OS (C Axis Aligned-Crystall ine Oxide Semiconductor) described later, a polycrystalline structure, a microcrystalline structure, or an amorphous structure. Among non-single-crystal structures, the amorphous structure has the highest density of defect states, and CA AC-OS has the lowest density of defect states.
[0086] The first oxide semiconductor film 110 may have, for example, an amorphous structure. An oxide semiconductor film with an amorphous structure has, for example, disordered atomic arrangement and no crystal component. Alternatively, an oxide film with an amorphous structure is, for example, a completely amorphous structure and has no crystal portion.
[0087] Note that the first oxide semiconductor film 110 may be a mixed film including two or more of a region with an amorphous structure, a region with a microcrystalline structure, a region with a polycrystalline structure, a region of CAAC-OS, and a region with a single-crystal structure. The mixed film may include, for example, two or more of any of the region with an amorphous structure, the region with a microcrystalline structure, the region with a polycrystalline structure , the region of CAAC-OS, and the region with a single-crystal structure. Further, the mixed film may have, for example, a stacked-layer structure of two or more of any of the region with an amorphous structure, the region with a microcrystalline structure, the region with a polycrystalline structure , the region of CAAC-OS, and the region with a single-crystal structure.
[0088] <Insulating Film> As the insulating films 106 and 107 functioning as the gate insulating films of the transistor 150, a silicon oxide film, a silicon oxynitride film, a silicon nitride oxide film, can be formed by a plasma CVD (CVD: Chemical Vapor Deposition) method, a spu ttering method, or the like. silicon nitride film, aluminum oxide film, hafnium oxide film, yttrium oxide film, zir conium oxide film, gallium oxide film, tantalum oxide film, magnesium oxide film, lanthanum oxide film , cerium oxide film, and neodymium oxide film, each of which may be used alone or as an insulating film containing one or more kinds thereof can be used. Note that a single-layer insulating film selected from the above materials may be used instead of a stacked structure of the insulating films 106 and 107 may be used.
[0089] The insulating film 106 functions as a blocking film that suppresses permeation of oxygen. For example , in the case where excess oxygen is supplied into the insulating films 107, 114, 116 and / or the first oxide semiconductor film 110 the insulating film 106 can suppress permeation of oxygen.
[0090] Note that the insulating film 107 in contact with the first oxide semiconductor film 110 which functions as a channel region of the transistor 150 is preferably an oxide insulating film, and more preferably has a region (oxygen excess region) containing oxygen in excess of the stoichiometric composition It is more preferable to have an excess oxygen region. In other words, the insulating film 107 is an insulating film which can release oxygen The insulating film 107 is an insulating film capable of releasing oxygen. Note that in order to provide the oxygen excess region in the insulating film 107, for example, the insulating film 107 may be formed in an oxygen atmosphere for example, the insulating film 107 may be formed in an oxygen atmosphere. Alternatively, oxygen may be introduced into the insulating film 107 after film formation to form an oxygen excess region oxygen may be introduced into the insulating film 107 after film formation to form an oxygen excess region. As a method for introducing oxygen, an ion implantation method, an ion doping method, a plasma immersion ion implantation method method, a plasma treatment, or the like can be used. , plasma treatment, or the like can be used.
[0091] Further, in the case where hafnium oxide is used for the insulating films 106 and 107, the following effects can be obtained Hafnium oxide has a higher relative dielectric constant than silicon oxide or silicon oxynitride. Therefore Therefore, compared to silicon oxide, the film thickness of insulating films 106 and 107 can be increased, This reduces leakage current due to the current flowing through the circuit. In other words, it reduces the off-current of the transistor. This makes it possible to realize a radiator. Furthermore, hafnium oxide, which has a crystalline structure, is amorphous. It has a higher dielectric constant compared to hafnium oxide with a structure. Therefore, the off-current is small. For a transistor, it is preferable to use hafnium oxide, which has a crystalline structure. Examples of crystal structures include monoclinic and cubic systems. However, the present invention One embodiment is not limited to these.
[0092] In this embodiment, a silicon nitride film is formed as the insulating film 106, and the insulating film 107 It forms a silicon oxide film. Compared to the silicon oxide film, the silicon nitride film has a relative dielectric constant. Because the rate is high and the thickness required to obtain capacitance equivalent to that of a silicon oxide film is large, The insulating film 108, which functions as the gate insulating film of the ZISTA 150, includes a silicon nitride film. This allows the insulating film to be physically made thicker. Therefore, the dielectric strength of transistor 150 By suppressing the pressure drop and further improving the dielectric strength, electrostatic discharge (ESD) breakdown of transistor 150 is prevented. It is possible.
[0093] <Gate electrode, source electrode, and drain electrode> It can be used for the gate electrode 104, source electrode 112a and drain electrode 112b. The materials used include aluminum, titanium, chromium, nickel, copper, yttrium, and zirconium. Metals such as nium, molybdenum, silver, tantalum, or tungsten, or materials mainly composed of these. The alloy can be used as a single-layer or multi-layer structure. For example, aluminum A two-layer structure in which a titanium film is laminated on a molybdenum film, and a two-layer structure in which a titanium film is laminated on a tungsten film , a two-layer structure in which a copper film is laminated on a molybdenum film, and on an alloy film containing molybdenum and tungsten a two-layer structure in which a copper film is laminated, and a copper film is laminated on a copper-magnesium-aluminum alloy film two-layer structure, a titanium film or titanium nitride film, and a titanium film or titanium nitride film overlaid thereon an aluminum film or a copper film is laminated, and a titanium film or a titanium nitride film is further formed thereon a three-layer structure, a molybdenum film or a molybdenum nitride film, and the molybdenum film or the molybdenum nitride film an aluminum film or a copper film is laminated overlaid on the ribden film, and a molybdenum film is further formed thereon or a three-layer structure in which a molybdenum nitride film is formed, and the like. Further, the source electrode 112a, and when the drain electrode 112b has a three-layer structure, titanium, titanium nitride are used for the first layer and the third layer , molybdenum, tungsten, an alloy containing molybdenum and tungsten, molybdenum and di an alloy containing ruconium, or a film made of molybdenum nitride is formed, and the second layer is made of copper, alumi num, gold or silver, or a film made of a low-resistance material such as an alloy of copper and manganese can be formed preferable. Note that indium tin oxide, indium oxide containing tungsten oxide, oxide indium zinc oxide containing tungsten, indium oxide containing titanium oxide, titanium oxide indium tin oxide containing tan, indium zinc oxide, indium added with silicon oxide A light-transmitting conductive material such as um tin oxide may be used. Further, the gate electrode 104, materials that can be used for the source electrode 112a and the drain electrode 112b are, for example, sp It can be formed by a puttering method.
[0094] <Conductive Film> Conductive films 120 and 121 function as pixel electrodes. For example, a material that is reflective in visible light can be used. Specifically, aluminum Aluminum, gold, platinum, silver, nickel, tungsten, chromium, molybdenum, iron, cobalt The use of metallic materials such as copper or palladium, or alloys containing these metallic materials, is possible. Yes, it is possible. Furthermore, lanthanum, neodymium, or germanium can be added to the above metal materials or alloys. It may be done. Also, aluminum-titanium alloys, aluminum-nickel alloys Aluminum and neodymium alloys, aluminum, nickel, and lanthanum alloys (Al Aluminum alloys such as Ni-La, silver alloys and copper alloys, and silver and palladium and copper alloy (Ag-Pd-Cu, also written as APC), silver and magnesium alloy It can be formed using alloys containing silver, such as gold. Alloys containing silver and copper have high heat resistance. Therefore, it is preferable. A film made of the above material can be used as a single layer or in a laminated form. Furthermore, By laminating a metal film or metal oxide film in contact with an aluminum alloy film, the aluminum alloy The oxidation of the gold film can be suppressed. Examples of materials for the metal film and metal oxide film include titanium. Examples include titanium dioxide.
[0095] <Protective insulating film> Insulating films 114, 116, and 118 function as protective insulating films for transistor 150. This involves using plasma CVD, sputtering, etc. to produce silicon oxide films and silicon oxide nitride films. Film, silicon nitride film, silicon nitride film, aluminum oxide film, hafnium oxide film, acid Yttrium oxide film, zirconium oxide film, gallium oxide film, tantalum oxide film, magnesium oxide film An insulating film containing one or more of the following: a cium film, a lanthanum oxide film, a cerium oxide film, and a neodymium oxide film. Each of these can be used.
[0096] Furthermore, the first oxide semiconductor film 110 functions as the channel region of the transistor 150. The insulating film 114 in contact with the material is preferably an oxide insulating film, and is capable of releasing oxygen. A stoichiometric insulating film is used. In other words, an insulating film that can release oxygen is a stoichiometric composition. This insulating film has a region containing an excess of oxygen (oxygen-rich region). To create an oxygen-rich region in 114, for example, the insulating film 114 can be formed in an oxygen atmosphere. Alternatively, oxygen can be introduced into the insulating film 114 after film formation to form an oxygen-rich region. Methods for introducing oxygen include ion implantation, ion doping, and plasma immersion. Ion implantation, plasma treatment, and other methods can be used.
[0097] By using an insulating film capable of releasing oxygen as the insulating film 114, the transient Oxygen is transferred to the first oxide semiconductor film 110 which functions as a channel region of 150. It becomes possible to reduce the amount of oxygen vacancies in the first oxide semiconductor film 110. For example, heating deoxygenation The surface temperature of the film, as measured by elution analysis (hereinafter referred to as TDS analysis), is 100°C. The amount of oxygen molecules released in the range of 700°C or 100°C to 500°C. , 1.0 × 10 18 molecules / cm 3 By using the above insulating film, the first oxide semiconductor film The amount of oxygen deficiency contained in 110 can be reduced.
[0098] Furthermore, the insulating film 114 preferably has a low defect count, and typically, ESR measurement is used to determine its defect count. Furthermore, the spin density of the signal appearing at g=2.001 originates from the dangling bond of silicon. 3 x 10 17 spins / cm 3 The following is preferable. This is because the insulating film 114 If the defect density is high, oxygen will bond to the defects, resulting in acid formation in the insulating film 114. This is because the amount of transmission decreases. Also, the insulating film 114 and the first oxide semiconductor film 1 It is preferable that the amount of defects at the interface with 10 be small, and typically, this can be determined by ESR measurement. The g-value originating from defects in the first oxide semiconductor film 110 appears to be between 1.89 and 1.96. The signal spin density is 1 × 10 17 spins / cm 3 The following are below the detection limit. It is preferable.
[0099] Furthermore, in the insulating film 114, all of the oxygen that enters the insulating film 114 from the outside is absorbed by the insulating film 11 It may move to the outside of 4. Or, some of the oxygen that entered the insulating film 114 from the outside, It may also remain in the insulating film 114. In addition, when oxygen enters the insulating film 114 from the outside, Oxygen contained in the insulating film 114 moves to the outside of the insulating film 114, In some cases, oxygen movement may occur. The insulating film 114 is an acid that can permeate oxygen. When an insulating film is formed, oxygen is provided on the insulating film 114, and oxygen is released from the insulating film 116. This can be transferred to the first oxide semiconductor film 110 via the insulating film 114.
[0100] Furthermore, the insulating film 114 is formed using an oxide insulating film with a low nitrogen oxide energy density. This can be done. Note that the energy level density of the nitrogen oxide is the upper end of the valence band of the oxide semiconductor film. Energy (E V_OS) and the energy (E) at the lower end of the conduction band of the oxide semiconductor film. C_OS )and It may be formed between them. The above oxide insulating film has a low nitrogen oxide emission rate. Using silicon oxide nitride film, or aluminum oxide nitride film with low nitrogen oxide emission, etc. It is possible to be there.
[0101] Furthermore, silicon oxidnitride films with low nitrogen oxide emissions are analyzed by the temperature-controlled desorption gas analysis method. In other words, it is a membrane that releases more ammonia than nitrogen oxides, and typically ammonia The amount of molecules released is 1 × 10 18 molecules / cm 3 The above 5 x 10 19 molecules / cm 3 The following applies. The amount of ammonia released is when the surface temperature of the film is between 50°C and 650°C, preferably 50°C. The above refers to the amount released by heat treatment at 550°C or below.
[0102] Nitrogen oxides (NO x , x is greater than 0 and less than or equal to 2, preferably between 1 and 2), typically NO2 or NO forms an energy level in the insulating film 114, etc. This energy level is the first oxide It is located within the energy gap of the semiconductor film 110. Therefore, nitrogen oxides are located within the insulating film 1 When diffused to the interface between 14 and the first oxide semiconductor film 110, the energy level moves towards the insulating film 114 side. In some cases, electrons are trapped in the insulating film 114. And because it remains near the interface of the first oxide semiconductor film 110, the threshold voltage of the transistor It shifts the focus in a positive direction.
[0103] Furthermore, nitrogen oxides react with ammonia and oxygen during heat treatment. Insulating film 114 The nitrogen oxides contained in react with the ammonia contained in the insulating film 116 during the heat treatment. Therefore, nitrogen oxides contained in the insulating film 114 are reduced. Electrons are less likely to be trapped at the interface between the first oxide semiconductor film 110 and the first oxide semiconductor film 110.
[0104] By using the above oxide insulating film as the insulating film 114, the threshold voltage of the transistor can be adjusted. This makes it possible to reduce the shift and reduce fluctuations in the electrical characteristics of the transistor. can.
[0105] Furthermore, the heat treatment in the transistor manufacturing process typically involves temperatures below 400°C or below 375°C. By heat treatment at a temperature of 10°C or higher (preferably 340°C or higher and 360°C or lower), the insulating film 114 is 10 In spectra obtained by measurement at ESR below 0K, the g value is 2.037 or higher and 2.03 A first signal of 9 or less, a second signal with a g value of 2.001 or more and 2.003 or less, and A third signal is observed with a g value between 1.964 and 1.966. Note that the first signal The split width of the first and second signals, and the split width of the second and third signals. The split width is approximately 5 mT in the X-band ESR measurement. The g-value is 2.037. The first signal is 2.039 or less, and the second signal is 2.001 or more and 2.003 or less. The sum of the spin densities of the third signal, which has a g value between 1.964 and 1.966. The total is 1 x 10 18 spins / cm 3 It is less than 1 × 10⁻⁶. 17 spins / cm 3 The above 1 x 10 18 spins / cm 3 It is less than.
[0106] Furthermore, in ESR spectra below 100K, the g value must be between 2.037 and 2.039. The first signal, the second signal with a g value of 2.001 or more and 2.003 or less, and the g value of 1 A third signal between 0.964 and 1.966 indicates nitrogen oxides (NOx). x x is greater than 0 This corresponds to a signal caused by (2 or less, preferably 1 or more and 2 or less). Typical examples of nitrogen oxides are Examples include nitric oxide and nitrogen dioxide. That is, a g value of 2.037 or higher and 2.039 or lower. The first signal, the second signal with a g value of 2.001 or more and 2.003 or less, and the g value The smaller the sum of the spin densities of the third signal between 1.964 and 1.966, the less acid It can be said that the nitrogen oxide content in the oxide insulating film is low.
[0107] Furthermore, the above oxide insulating film has a nitrogen concentration of 6 × 10 as measured by SIMS. 20 atoms / cm 3 The following applies:
[0108] The substrate temperature is between 220°C and 350°C, and PEC is performed using silane and nitrous oxide. By forming the above oxide insulating film using the VD method, a dense and hard film is obtained. It can be formed.
[0109] The insulating film 116, which is formed in contact with the insulating film 114, contains oxygen that satisfies the stoichiometric composition. It is formed using an oxide insulating film containing more oxygen than the stoichiometric composition. Oxide insulating films, which contain a large amount of oxygen, lose some of their oxygen when heated. Oxide insulating films containing more oxygen than the required oxygen level are analyzed by thermal desorption gas spectroscopy (TDS): Thermal Desorption Spectroscopy (TOS) The converted oxygen release amount is 1.0 × 10 19 atoms / cm 3Preferably 3.0 ×10 20 atoms / cm 3 The above is an oxide insulating film. The surface temperature of the film is between 100°C and 700°C, or between 100°C and 500°C. A range is preferable.
[0110] Furthermore, it is preferable that the insulating film 116 has a low defect count, and typically, ESR measurement is used to determine this. Furthermore, the spin density of the signal appearing at g=2.001 originates from the dangling bond of silicon. is 1.5 × 10 18 spins / cm 3 Less than, and even 1 x 10 18 spins / cm 3 Below It is preferable that it be below. Note that the insulating film 116 is the first oxide compared to insulating film 114. Since it is far from the semiconductor film 110, it can have a higher defect density than the insulating film 114.
[0111] The thickness of the insulating film 114 is 5 nm or more and 150 nm or less, preferably 5 nm or more and 50 nm or less. The thickness of the insulating film 116 is preferably 10 nm or more and 30 nm or less. The wavelength can be 30 nm to 500 nm, preferably 150 nm to 400 nm. Cut.
[0112] Furthermore, insulating films 114 and 116 can be made of the same type of insulating material, thus providing insulation. In some cases, the interface between film 114 and insulating film 116 cannot be clearly identified. Therefore, in this implementation... In the diagram, the interface between insulating film 114 and insulating film 116 is shown with a dashed line. In the embodiment, a two-layer structure of insulating film 114 and insulating film 116 was described, but It is not limited to the above, but for example, a single-layer structure of insulating film 114, a single-layer structure of insulating film 116, or 3 A layered structure with more than one layer is also acceptable.
[0113] The insulating film 118 that functions as a dielectric film for the capacitive element 160 is a nitride insulating film. It is preferable. In particular, silicon nitride films have a higher dielectric constant compared to silicon oxide films, and acid Because the required film thickness to obtain capacitance equivalent to that of a silicon dioxide film is large, the induction of the capacitive element 160 By including a silicon nitride film as the insulating film 118 that functions as an electrostatic film, the insulating film is physically This allows for thicker film formation. Therefore, it suppresses the decrease in dielectric breakdown voltage of the capacitive element 160, and furthermore, By improving the dielectric strength, electrostatic discharge damage to the capacitive element 160 can be suppressed. The film 118 is the resistivity of the second oxide semiconductor film 111, which functions as an electrode for the capacitive element 160. It also has the function of reducing [something].
[0114] Furthermore, the insulating film 118 blocks oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc. It has the function of being able to do so. By providing an insulating film 118, the first oxide semiconductor film 110 The diffusion of oxygen from the outside, and the diffusion of oxygen contained in insulating films 114 and 116 to the outside, This prevents hydrogen, water, and other substances from entering the first oxide semiconductor film 110 from the outside. Oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc., which have a blocking effect. Instead of an oxide insulating film, an oxide insulating film having a blocking effect on oxygen, hydrogen, water, etc. is provided. It may be used. As an oxide insulating film having a blocking effect on oxygen, hydrogen, water, etc., Aluminum, aluminum oxide nitride, gallium oxide, gallium oxide nitride, yttrium oxide Examples include yttrium oxide nitride, hafnium oxide, and hafnium oxide nitride.
[0115] Examples of insulating films 119 that function as planarizing films include polyimide resin and acrylic resin. Polyamide resin, polyimideamide resin, benzocyclobutene resin, polyamide resin, epoxy resin Heat-resistant organic materials such as fats can be used.
[0116] The insulating film 130 can be made of the same material as the insulating film 119. The same material as the insulating film 106 may be used for film 130.
[0117] <Method for manufacturing liquid crystal display devices> Next, regarding an example of a method for manufacturing a liquid crystal display device shown in Figures 1(A) and 1(B), see Figures 4 to 1. I will explain using number 8.
[0118] First, the gate electrode 104 is formed on the substrate 102. Then, the substrate 102 and the gate An insulating film 108 containing insulating films 106 and 107 is formed on the electrode 104 (see Figure 4(A)). .
[0119] The substrate 102, gate electrode 104, and insulating films 106 and 107 are as described above. It can be formed by selecting from the listed materials. In this embodiment, substrate 1 For 02, a glass substrate is used, and for the gate electrode 104, tungsten is used as the conductive film. A film is used, and as the insulating film 106, a silicon nitride film capable of releasing hydrogen is used. As the insulating film 107, a silicon oxidizride film capable of releasing oxygen is used.
[0120] The gate electrode 104 is formed on the substrate 102 after the conductive film has been deposited, leaving a desired area of the conductive film intact. It can be formed by patterning and then etching away the unwanted areas.
[0121] Next, the first oxide semiconductor film 11 is placed on the insulating film 108 at a position where it overlaps with the gate electrode 104. It forms 0 (see Figure 4(B)).
[0122] The first oxide semiconductor film 110 can be shaped by selecting from the materials listed above. This can be achieved. In this embodiment, the first oxide semiconductor film 110 is In -Ga-Zn oxide film (using a metal oxide target with In:Ga:Zn = 1:1:1.2) Use.
[0123] Furthermore, the first oxide semiconductor film 110 is formed after the oxide semiconductor film is deposited on the insulating film 108. The oxide semiconductor film is patterned so that the desired region remains, and then the unwanted region is etched away. It can be formed by rubbing.
[0124] It is preferable to perform a heat treatment after forming the first oxide semiconductor film 110. This heat treatment is performed at 250°C. °C to 650°C, preferably 300°C to 500°C, more preferably 350°C or below. At temperatures below 450°C, in an inert gas atmosphere, or an atmosphere containing 10 ppm or more of an oxidizing gas, Alternatively, the process can be carried out under reduced pressure. Furthermore, the heat treatment should be performed under an inert gas atmosphere. After the procedure, an oxidizing gas is used to replenish the oxygen that has been removed from the first oxide semiconductor film 110. The procedure may be carried out in an atmosphere containing 0 ppm or more. The heat treatment here results in insulating film 106, 10 7. Remove impurities such as hydrogen and water from at least one of the first oxide semiconductor films 110. This can be done. Note that this heat treatment is performed before processing the first oxide semiconductor film 110 into island shapes. You can go.
[0125] Furthermore, the transistor 150, which has the first oxide semiconductor film 110 as its channel region, is stable. In order to impart certain electrical characteristics, the impurities in the first oxide semiconductor film 110 are reduced, and the first It is effective to make the oxide semiconductor film 110 intrinsic or substantially intrinsic.
[0126] Next, a conductive film is formed on the insulating film 108 and the first oxide semiconductor film 110, and the conductive film By patterning so that the desired area remains, and then etching away the unwanted areas, Source electrode 112a and drain electrode on insulating film 108 and first oxide semiconductor film 110 It forms pole 112b (see Figure 4(C)).
[0127] The source electrode 112a and the drain electrode 112b are selected from the materials listed above. It can be formed by selecting from. In this embodiment, the source electrode 112a, and The drain electrode 112b consists of a tungsten film, an aluminum film, and a titanium film. A three-layer laminated structure is used.
[0128] Furthermore, after the formation of the source electrode 112a and the drain electrode 112b, the first oxide semiconductor The surface of the body membrane 110 may be washed. For example, a cleaning solution such as phosphoric acid may be used. One example is the cleaning method used. By cleaning with a chemical solution such as phosphoric acid, the oxide semiconductor film 1 Impurities adhering to the surfaces of 10 (for example, source electrode 112a and drain electrode 112b) It can remove elements (etc.) contained in it. However, this cleaning is not always necessary. In some cases, cleaning may not be necessary.
[0129] Furthermore, the process of forming the source electrode 112a and the drain electrode 112b, and the cleaning process described above. In either or both of the steps, the source electrode 11 of the first oxide semiconductor film 110 The areas exposed from 2a and the drain electrode 112b may become thinner.
[0130] Next, insulating film 108, first oxide semiconductor film 110, source electrode 112a, and drain Insulating films 114 and 116 are formed on electrode 112b. Then, insulating films 114 and 116 The desired area is patterned, and then the unwanted area is etched to create an opening. Forms 141 (see Figure 4(D)).
[0131] Furthermore, after forming the insulating film 114, the insulating film 116 is formed continuously without exposure to the atmosphere. It is preferable to do so. After forming the insulating film 114, do not open it to the atmosphere, and control the flow rate, pressure, and high of the raw material gas. By adjusting the frequency power and substrate temperature to one or more units, the insulating film 116 is formed continuously, The concentration of impurities originating from atmospheric components at the interface between the edge film 114 and the insulating film 116 is reduced. In addition, the oxygen contained in the insulating films 114 and 116 is transferred to the first oxide semiconductor film 110. This makes it possible to move the first oxide semiconductor film 110, thereby reducing the amount of oxygen vacancies in the first oxide semiconductor film 110. This becomes possible.
[0132] Furthermore, in the process of forming the insulating film 116, the insulating film 114 is the first oxide semiconductor film 110 It serves as a protective film. Therefore, it reduces damage to the first oxide semiconductor film 110, The insulating film 116 can be formed using high-frequency power with high power density.
[0133] The insulating films 114 and 116 can be formed by selecting from the materials listed above. In this embodiment, the insulating films 114 and 116 are designed to release oxygen. A silicon oxide nitride film capable of this is used.
[0134] Furthermore, after forming the insulating films 114 and 116, a heat treatment (hereinafter referred to as the first heat treatment) is performed. It is preferable to perform the following. The first heat treatment removes nitrogen acid contained in the insulating films 114 and 116. The amount of oxidized material can be reduced by the first heat treatment. A portion of the contained oxygen is transferred to the first oxide semiconductor film 110, and the first oxide semiconductor film 1 The amount of oxygen deficiency contained in 10 can be reduced.
[0135] The temperature of the first heat treatment is typically less than 400°C, preferably less than 375°C, and Preferably, the temperature is 150°C to 350°C. The first heat treatment involves nitrogen, oxygen, and superdry Dry air (water content of 20 ppm or less, preferably 1 ppm or less, more preferably 10 ppm or less) The procedure should be carried out in an atmosphere of air (at ppb or less) or a noble gas (argon, helium, etc.). Furthermore, it is preferable that the above nitrogen, oxygen, ultra-dry air, or noble gases do not contain hydrogen, water, etc. The heat treatment involves an electric furnace, RTA (Rapid Thermal Annealing), etc. The following can be used.
[0136] The opening 141 is formed so that the drain electrode 112b is exposed. As a formation method, for example, a dry etching method can be used. However, for opening 1 The method for forming 41 is not limited to this, and may include wet etching or dry etching. A formation method combining the etching method and the wet etching method may also be used. Note that the opening 14 In the etching process for forming 1, the film thickness of the drain electrode 112b decreases. There is a match.
[0137] Next, a second oxide semiconductor film 111 is formed on the insulating film 116 so as to cover the opening 141. An oxide semiconductor film is formed (see Figures 5(A) and (B)).
[0138] Figure 5(A) shows the inside of the film deposition apparatus when forming an oxide semiconductor film on the insulating film 116. This is a schematic cross-sectional view. In Figure 5(A), a sputtering apparatus is used as the film deposition apparatus. A target 193 installed inside the sputtering apparatus, and a shape below the target 193 The resulting plasma 194 is schematically represented.
[0139] First, when forming an oxide semiconductor film, a plasma discharge is performed in an atmosphere containing oxygen gas. During this process, oxygen is added to the insulating film 116, which will be the surface on which the oxide semiconductor film is formed. Furthermore, when forming oxide semiconductor films, in addition to oxygen gas, an inert gas (for example, helium) is used. A mixture of gases (such as argon gas and xenon gas) may be used. For example, argon gas and Using oxygen gas, it is preferable to have a higher flow rate of oxygen gas than of argon gas. By increasing the flow rate of oxygen gas, oxygen can be suitably added to the insulating film 116. For example, one condition for forming an oxide semiconductor film is that oxygen gas makes up a large portion of the total deposition gas. The ratio should be 50% to 100%, preferably 80% to 100%. .
[0140] In Figure 5(A), the oxygen or excess oxygen added to the insulating film 116 is schematically represented. This is represented by a dashed arrow.
[0141] Furthermore, the substrate temperature for depositing oxide semiconductor films is preferably between room temperature and 340°C. Or, above room temperature and below 300°C, more preferably above 100°C and below 250°C, even more preferably The temperature is between 100°C and 200°C. By heating an oxide semiconductor film to form a film, oxidation occurs. The crystallinity of the semiconductor film can be improved. On the other hand, as the substrate 102, a large glass substrate When using a plate (for example, a 6th to 10th generation plate), the base when forming an oxide semiconductor film If the board temperature is set to 150°C or higher but less than 340°C, the substrate 102 will deform (warp or bend). ) In some cases, when using a large glass substrate, the formation of the oxide semiconductor film By keeping the substrate temperature between 100°C and 150°C during film formation, deformation of the glass substrate is suppressed. It is possible.
[0142] The oxide semiconductor film can be formed by selecting from the materials listed above. In this embodiment, an In-Ga-Zn metal oxide target (In:Ga:Zn=1:3 Using :6 [atomic ratio], an oxide semiconductor film is formed by sputtering.
[0143] Next, the oxide semiconductor is processed into a desired shape to form an island-shaped second oxide semiconductor film 1 Forms 11 (see Figure 5(C)).
[0144] The second oxide semiconductor film 111 is formed by depositing an oxide semiconductor film on the insulating film 116, and then the oxide The semiconductor film is patterned so that the desired region remains, and then the unwanted region is etched away. It can be formed by doing so.
[0145] Next, an insulating film 118 is formed on the insulating film 116 and the second oxide semiconductor film 111. See Figure 6(A).
[0146] The insulating film 118 contains either hydrogen or nitrogen, or both. For example, a silicon nitride film is preferable. Also, as the insulating film 118, for example For example, it can be formed using the sputtering method or the PECVD method. When depositing the edge film 118 by PECVD, the substrate temperature should be less than 400°C, preferably 375°C. The temperature is less than ℃, more preferably 180℃ or higher and 350℃ or lower. It is preferable to set the substrate temperature within the above-mentioned range, as this allows for the formation of a dense film. By setting the substrate temperature when depositing the insulating film 118 to the above range, the insulating film 114, 1 It is possible to transfer oxygen or excess oxygen in 16 to the first oxide semiconductor film 110. Yes.
[0147] Furthermore, after the formation of the insulating film 118, a heat treatment equivalent to the first heat treatment described above is performed (hereinafter, A second heat treatment may be performed. In this way, the second oxide semiconductor film 111 is formed. When forming an oxide semiconductor film, oxygen is added to the insulating film 116, and then the film is heated to a temperature of less than 400°C, preferably. Alternatively, the heat treatment is performed at a temperature of less than 375°C, more preferably between 180°C and 350°C. This process transfers oxygen or excess oxygen from the insulating film 116 into the first oxide semiconductor film 110. This allows for movement and the elimination of oxygen vacancies in the first oxide semiconductor film 110.
[0148] Here, the movement of oxygen into the first oxide semiconductor film 110 will be explained using Figure 7. The process is carried out. Figure 7 shows the substrate temperature (typically less than 375°C) when the insulating film 118 is deposited, or the insulating film. A second heat treatment (typically below 375°C) after the formation of film 118 removes the first oxide This is a model diagram representing oxygen moving into the semiconductor film 110. In Figure 7, the first oxide Oxygen (oxygen radical, oxygen atom, or oxygen molecule) moving into the semiconductor film 110 is indicated by a dashed line. The arrows indicate the process. Figures 7(A) and 7(B) show the results after the deposition of insulating film 118, respectively. This is a cross-sectional view corresponding to the dashed lines AB and CD shown in (A).
[0149] The first oxide semiconductor film 110 shown in Figure 7 is a film in contact with the first oxide semiconductor film 110 ( Here, oxygen moves from insulating film 107 and insulating film 114) to compensate for the oxygen deficiency. To be filled. In particular, in a liquid crystal display device according to one aspect of the present invention, the first oxide semiconductor film 110 During sputtering deposition of an oxide semiconductor film, oxygen gas is used to deposit acid into the insulating film 107. When an element is added, the insulating film 107 has an excess oxygen region. Also, the second oxide semiconductor film When forming an oxide semiconductor film 111 by sputtering, oxygen gas is used to form the insulating film 116 Because oxygen is added to it, the insulating film 116 has an excess oxygen region. The first oxide semiconductor film 110 sandwiched between insulating films having regions has oxygen vacancies suitably filled. ru.
[0150] Furthermore, an insulating film 106 is provided below the insulating film 107, and insulating films 114, 11 An insulating film 118 is provided above 6. The insulating films 106 and 118 have low oxygen permeability. By forming with a material such as silicon nitride, insulating films 107, 114, and 116 Because the oxygen contained within can be trapped on the first oxide semiconductor film 110 side, it is preferable. This makes it possible to transfer oxygen to the first oxide semiconductor film 110. 8 is the case where external impurities, such as water, alkali metals, alkaline earth metals, etc., are transient. This also has the effect of preventing diffusion into the first oxide semiconductor film 110 contained in STA 150.
[0151] Furthermore, the insulating film 118 contains either hydrogen or nitrogen, or both. Therefore, By forming the insulating film 118, the second oxide semiconductor film 111 in contact with the insulating film 118 is The addition of either hydrogen or nitrogen, or both, increases the carrier density. It can function as an oxide conductive film.
[0152] Furthermore, as the resistivity of the second oxide semiconductor film 111 decreases, Figures 5(C) and 6(A) show... The second oxide semiconductor film 111 shown is illustrated with a different hatching pattern.
[0153] The resistivity of the second oxide semiconductor film 111 is at least greater than that of the first oxide semiconductor film 110. It is also low, preferably 1 × 10 -3 Ωcm or more, 1 × 10 4 Less than Ωcm, more preferably , 1 x 10 -3 Ωcm or more, 1 × 10 -1 It should be less than Ωcm.
[0154] Next, the insulating film 118 is patterned so that the desired region remains, and then the unwanted region is removed. By cutting, an opening 142 is formed (see Figure 6(B)).
[0155] The opening 142 is formed so that the drain electrode 112b is exposed. As a formation method, for example, a dry etching method can be used. However, for opening 1 The method for forming 42 is not limited to this, and may include wet etching or dry etching. A formation method combining the etching method and the wet etching method may also be used. Note that the opening 14 In the etching process for forming 2, the film thickness of the drain electrode 112b decreases. There is a match.
[0156] Furthermore, if the process of forming the opening 142 is omitted from the process of forming the opening 141, Openings may be continuously formed in insulating films 114, 116, and 118. This makes it possible to reduce the manufacturing steps of the liquid crystal display device according to one aspect of the present invention, This can help reduce manufacturing costs.
[0157] Next, an insulating film 119 is formed on the insulating film 118, so that a desired region of the insulating film 119 remains. The pattern is applied, and then the unnecessary areas are etched to form the opening 143. A conductive film is formed on the insulating film 119 so as to cover the opening 143, and the desired area of the conductive film The conductive film 120 is created by patterning so that the desired area remains, and then etching away the unnecessary areas. It forms (see Figure 6(C)).
[0158] Furthermore, without performing the steps described above for forming openings 141 and 142, opening 143 is formed. In the process, openings may be continuously formed in the insulating films 114, 116, 118, and 119. i. By adopting such a process, the manufacturing process of the liquid crystal display device according to one embodiment of the present invention can be reduced. This makes it possible to reduce manufacturing costs.
[0159] The insulating film 119 and the conductive film 120 can be selected from the materials listed above. It can be formed. In this embodiment, acrylic resin is used as the insulating film 119. Furthermore, an Ag-Pd-Cu alloy is used as the conductive film 120.
[0160] Furthermore, a capacitive element 160 is fabricated in conjunction with the formation of the conductive film 120. The capacitive element 160 is The structure has a dielectric layer sandwiched between a pair of electrodes, and one of the pair of electrodes is a second oxide semiconductor The body film 111 is the other electrode of the pair, and the conductive film 120 is the other electrode. Also, insulating films 118, 11 9 functions as a dielectric layer for the capacitive element 160.
[0161] Next, an insulating film is formed on the insulating film 119 and the conductive film 120, and the desired region remains. The insulating film 130 is formed by turning and then etching away the unnecessary areas (Figure 8). (See (A)). The insulating film 130 is provided so as to cover the edges of the conductive film 120. However, the insulating film 130 is not present in the area between the pixel having the transistor 150 and the adjacent pixel having the transistor It has an opening for the inverter and the conductive film 121 to be electrically connected.
[0162] The insulating film 130 can be formed by selecting from the materials listed above. In this embodiment, acrylic resin is used as the insulating film 130.
[0163] Next, a conductive film that will become the conductive film 121 is applied to the insulating film 119, the conductive film 120, and the insulating film 130. Form the material, pattern it so that the desired area remains, and then etch away the unwanted areas. A conductive film 121 is formed (see Figure 8(B)).
[0164] The conductive film 121 can be formed by selecting from the materials listed above. In this embodiment, an Ag-Pd-Cu alloy is used as the conductive film 121.
[0165] By following the above steps, the liquid crystal display devices shown in Figures 1(A) and 1(B) can be manufactured. .
[0166] The configurations and methods described in this embodiment are similar to those described in other embodiments. They can be used in combination as appropriate.
[0167] (Embodiment 2) In this embodiment, regarding the liquid crystal display device according to one aspect of the present invention, the liquid crystal shown in Embodiment 1 is used. Modified examples of the display device will be explained with reference to Figures 9 to 11. The same symbols are used for parts that are the same as or have the same function as those shown in Figures 1 to 8. We will use numbers and omit the explanation of their repetition.
[0168] <Example configuration of a liquid crystal display device (modified)> Figure 9(A) is a top view of a liquid crystal display device according to one embodiment of the present invention, and Figure 9(B) is a top view of Figure 9( This corresponds to the cross-sectional view of the section between the dashed lines EF and GH in A). Oh, in Figure 9(A), to avoid complexity, some of the components of the liquid crystal display device are shown. The gate insulating film and other components are omitted from the illustration.
[0169] The liquid crystal display device shown in Figures 9(A) and (B) includes a transistor containing a first oxide semiconductor film 110. It has a zista 150 and a capacitive element 160 with an insulating film between a pair of electrodes. The configuration of the TA 150 and the capacitive element 160 is the same as that of the liquid crystal display device shown in Figures 1(A) and (B). Yes. Note that the dashed line EF in Figure 9(A) indicates the channel length direction of transistor 150. The dashed line GH indicates the channel width direction of transistor 150.
[0170] Furthermore, the structure of the conductive film 120a is the same as that of the conductive film 120 shown in Figures 1(A) and (B). The transistor 150, the capacitive element 160, and the conductive film 120a shown in Figures 9(A) and (B) Therefore, it is possible to constitute one pixel of a liquid crystal display device.
[0171] The conductive film 120b can be formed simultaneously using the same material as the conductive film 120a. The film 120b includes, for example, a pixel electrode of one pixel containing a transistor 150 and an adjacent pixel. It has the function of being a .
[0172] The liquid crystal display device described in this embodiment has an insulating film 130 which is a conductive film 120b and a conductive film 1 Having a region that overlaps with 22, the conductive film 122 is provided on the insulating film 130 and the conductive film 120a. The conductive film 122 is electrically connected to the conductive film 120a.
[0173] Furthermore, in the liquid crystal display device shown in Figure 9(B), the insulating film 130 is a conductive film 120a and a conductive film It is provided on the dielectric film 120b. Specifically, the insulating film 130 is provided on the edges of the conductive film 120a and the conductive film 120a. It is installed on top of the edge of the film 120b.
[0174] The conductive film 120a and the conductive film 122 are insulated by the insulating film 130. Therefore, in the upper surface shape, the gap between the conductive film 120a and the conductive film 122 can be eliminated. This configuration allows the liquid crystal display device according to one aspect of the present invention to achieve a pixel aperture ratio. It can be improved. Also, by increasing the aperture ratio of the pixels, the contrast of the displayed image can be increased. Furthermore, it can be used as a reflective liquid crystal display device that produces a bright display image.
[0175] Note that in Figures 9(A) and (B), conductive film 120b and conductive film 122 are insulated from insulating film 13 They are arranged so that their ends roughly coincide via 0. That is, in the upper surface shape The structure is configured such that there is no gap between the conductive film 120b and the conductive film 122, but is not limited to this. Furthermore, there may be a gap between the conductive film 120b and the conductive film 122. Also, Figure 10( As shown in A), the conductive film 120b and the conductive film 122 overlap via the insulating film 130. It may have a region.
[0176] Furthermore, as shown in Figure 10(B), the conductive film 122 is provided beneath the conductive film 120a. It is also possible. In the liquid crystal display device shown in Figure 10(B), the conductive film 120a and the insulating film 130 are conductive. The conductive film 120b is provided on film 122, and the conductive film 120b is provided on insulating film 130. The conductive film 120b can be formed simultaneously using the same material. Figure 10(B) Therefore, the upper surface shape is configured so that there is no gap between the conductive film 120b and the conductive film 122. However, as shown in Figure 11(A), conductive film 120b and conductive film 122 penetrate insulating film 130 It may have overlapping regions.
[0177] Furthermore, in the liquid crystal display device, the capacitance value required by the capacitive element 160 is adjusted according to the capacitance value of the insulating film 119. The film thickness can be adjusted as needed. Alternatively, the insulating film 119 may be omitted. (Figure) Figure 11(B) shows an example of a cross-sectional view of a liquid crystal display device without an insulating film 119. In this configuration, the insulating film 118 functions as the dielectric film of the capacitive element 160.
[0178] Furthermore, the resistance of the first oxide semiconductor film 110 and the second oxide semiconductor films 111 and 111a The resistance can be controlled by referring to the description in Embodiment 1.
[0179] The materials and manufacturing methods for each layer of the liquid crystal display device shown in this embodiment are described in the description of Embodiment 1. This can be taken into consideration. The materials and manufacturing methods of the conductive films 120a and 120b are the conductive films of Embodiment 1. Refer to 120. Also, the material and manufacturing method of the conductive film 122 are as follows: conductive film of Embodiment 1 You can refer to 121.
[0180] The configurations and methods described in this embodiment are similar to those described in other embodiments. They can be used in combination as appropriate.
[0181] (Embodiment 3) In this embodiment, regarding the liquid crystal display device according to one aspect of the present invention, the liquid crystal shown in Embodiment 1 is used. A modified example of the display device will be explained using Figure 12.
[0182] <Example configuration of a liquid crystal display device> Figure 12(A) is a top view of a liquid crystal display device according to one embodiment of the present invention, and Figure 12(B) is a top view of a liquid crystal display device according to one embodiment of the present invention. This corresponds to the cross-sectional view of the section between the dashed lines IJ and KL in 12(A). In addition, to avoid complexity, the configuration of the liquid crystal display device is shown in Figure 12(A). Some of the components (such as the colored film and gate insulating film) are omitted from the illustration.
[0183] The dashed line IJ in Figure 12(A) indicates the channel length direction of transistor 151. Furthermore, the dashed line KL indicates the channel width direction of transistor 151. In this book, the channel length direction of a transistor refers to the source (source region or source electrode). And the direction in which carriers move between the drain (drain region or drain electrode) This means that the channel width direction is perpendicular to the channel length direction in a plane horizontal to the substrate. It indicates the direction.
[0184] The liquid crystal display device shown in Figures 12(A) and (B) comprises a first oxide semiconductor film 110 and a second A transistor 151 containing an oxide semiconductor film 111a, and a capacitor containing an insulating film between a pair of electrodes. The device has an element 160. In the capacitive element 160, one of the pair of electrodes is a second acid The other electrode of the pair is a conductive film 120, and the other electrode is a semiconductor film 111.
[0185] Transistor 151 has a gate electrode 104 on the substrate 102 and a terminal on the gate electrode 104 An insulating film 108 that functions as a gate insulating film, and a gate electrode 104 on the insulating film 108 The first oxide semiconductor film 110 at the superimposed position and the source on the first oxide semiconductor film 110. Electrode 112a and drain electrode 112b, first oxide semiconductor film 110, source electrode 1 insulating film 114, which functions as a second gate insulating film on 12a and drain electrode 112b , 116 and the second oxide at a position superimposed on the first oxide semiconductor film 110 on the insulating film 116 It has a monocrystalline semiconductor film 111a. Note that the transistor 15 shown in Figures 12(A) and (B) 1 is a so-called double-gate structure.
[0186] Furthermore, on transistor 151, more specifically, the second oxide semiconductor film 111a, and the insulating Insulating films 118 and 119 are formed on the edge film 116. It functions as a protective insulating film for transistor 151. The insulating film 119 is a planarization film It has the function of a drain. In addition, the insulating films 114, 116, 118, and 119 have drains. An opening 143 is formed that reaches pole 112b, and an insulating film 119 covers the opening 143. A conductive film 120 is formed on top of it. That is, the conductive film 120 is electrically charged with the transistor 151. They are connected by air. The conductive film 120 functions, for example, as a pixel electrode in a liquid crystal display device. ru.
[0187] Capacitive element 160 functions as one of a pair of electrodes on the insulating film 116. A second oxide semiconductor film 111 and a dielectric film that functions on the second oxide semiconductor film 111. Insulating films 118, 119 and a second oxide semiconductor film 111 via insulating films 118, 119 A conductive film 120 having the function of the other electrode of a pair of electrodes at superimposed positions, In other words, the conductive film 120 has the function of both a pixel electrode and a capacitive element electrode. ru.
[0188] The transistor 151, the capacitive element 160, and the conductive film 120 are shown in Figures 12(A) and (B). This allows for the formation of a single pixel in a liquid crystal display device.
[0189] Furthermore, the insulating film 130 is provided on top of the edge of the conductive film 120, and on the insulating film 130 A conductive film 121 is provided. The conductive film 121 includes, for example, a transistor 151. It functions as a pixel electrode for a pixel and adjacent pixels.
[0190] The conductive film 120 and the conductive film 121 are insulated by the insulating film 130. This eliminates the gap between the conductive film 120 and the conductive film 121 in the upper surface shape. Having such a configuration, the liquid crystal display device according to one aspect of the present invention increases the aperture ratio of the pixels. This can be achieved. Furthermore, by increasing the aperture ratio of the pixels, the contrast of the displayed image is increased. Furthermore, it can be used as a reflective liquid crystal display device that produces bright images.
[0191] Furthermore, a colored film 170 is provided on the conductive film 120, and a colored film 171 is provided on the conductive film 121. A colored film is provided in contact with the conductive film, thereby improving the interaction of the pixel electrode in one pixel. This suppresses crosstalk, where incoming light passes through the colored film of adjacent pixels, improving the viewing experience of reflective liquid crystal displays. This reduces the dependence on field angle. Furthermore, by using this configuration, the base can be transmitted via the liquid crystal. Since it is no longer necessary to apply a colored film to the substrate facing the plate 102 (hereinafter also referred to as the opposing substrate), Therefore, the alignment accuracy required when bonding substrate 102 and the opposing substrate can be reduced. Yes, it is possible. Therefore, the yield in the manufacturing of liquid crystal display devices can be improved.
[0192] In Figure 12(B), the insulating film 130 covers the edge of the conductive film 120. Although provided only near the edges of the film 120, it is not limited to this. The insulating film 130 is an insulating film. Even if the edges of film 130 and conductive film 121 are superimposed on each other so that they generally coincide, Good. Also, the liquid crystal display device shown in Figures 12(A) and (B) has conductive film 120 and conductive film 12 Although 1 has a region that overlaps via the insulating film 130, conductive film 120 and conductive film 121 It is not necessary for them to have overlapping regions.
[0193] In a liquid crystal display device, the thickness of the insulating film 119 is adjusted according to the capacitance value required by the capacitive element 160. It can be adjusted as needed. Alternatively, the insulating film 119 may be omitted.
[0194] Furthermore, the liquid crystal display device shown in Figures 12(A) and (B) has a second oxide semiconductor on the insulating film 116. A body film 111a is provided. The second oxide semiconductor film 111a is the second oxide semiconductor film 1 By depositing and etching simultaneously with 11, the channel region of the transistor overlaps. It may be provided in such a way. The second oxide semiconductor film 111a is, for example, the second oxide Because the semiconductor film 111 is deposited, etched, and formed simultaneously, the same material It has [this property]. Therefore, it is possible to suppress the increase in process steps. However, this invention One embodiment is not limited thereto. The second oxide semiconductor film 111a is the second The oxide semiconductor film 111 may be formed by a different process.
[0195] The second oxide semiconductor film 111a is the first oxide which forms the channel region of transistor 151. It has a region that overlaps with the oxide semiconductor film 110. Therefore, the second oxide semiconductor film 11 1a functions as the second gate electrode of transistor 151. Therefore, The second oxide semiconductor film 111a may be connected to the gate electrode 104. Or, The second oxide semiconductor film 111a is not connected to the gate electrode 104. Different signals or different potentials may be supplied. With this configuration, This can improve the current drive capability of the transistor 151.
[0196] Furthermore, the first oxide semiconductor film 110 functions as the channel region of the transistor 151. Furthermore, the second oxide semiconductor film 111 is one of the pair of electrodes of the capacitive element 160. Therefore, the second oxide semiconductor film 11 is better than the first oxide semiconductor film 110. The resistivity of 1 is low. Also, the first oxide semiconductor film 110 and the second oxide semiconductor film 111 are Preferably, they have the same metal element. The first oxide semiconductor film 110 and the second oxide semiconductor film By making the body film 111 a structure having the same metal element, the manufacturing equipment (for example, a film deposition apparatus, Since processing equipment (and other components) can be used in common, manufacturing costs can be reduced. .
[0197] Furthermore, the insulating film 118 provided on the transistor 151 and used in the capacitive element 160 As such, an insulating film containing at least hydrogen is used. Also, the insulating film used in transistor 151 The insulating films 114 and 116 provided on the edge film 107 and transistor 151 are as follows: An insulating film containing at least oxygen is used. Thus, transistor 151 and capacitive element 1 The insulating film used in 60, and the insulating film used on transistor 151 and capacitive element 160 By using an insulating film with the above configuration, the first oxide semiconductor of transistor 151 Controlling the resistivity of the second oxide semiconductor film 111 of the conductive film 110 and the capacitive element 160. This is possible. The first oxide semiconductor film 110 and the second oxide semiconductor films 111, 11 The resistivity of 1a can be controlled by referring to the description in Embodiment 1. .
[0198] In transistor 151, the first oxide semiconductor film 110 has a channel region and Because it is used in this way, it has a higher resistivity compared to the second oxide semiconductor film 111. On the other hand, the second Since the oxide semiconductor films 111 and 111a have the function of electrodes, the first oxide semiconductor It has lower resistivity compared to film 110.
[0199] The materials and manufacturing methods for each layer of the liquid crystal display device shown in this embodiment are described in the description of Embodiment 1. This can be taken into consideration. Materials that can be used for the colored films 170 and 171 include metal materials and resins. Examples include resin materials containing lipids, pigments, or dyes.
[0200] The configurations and methods described in this embodiment are similar to those described in other embodiments. They can be used in combination as appropriate.
[0201] (Embodiment 4) In this embodiment, a liquid crystal display device 80, which is one aspect of the present invention, is shown in Figures 13 to 2. I will explain using number 5.
[0202] The liquid crystal display device 80 shown in Figure 13(A) comprises a pixel section 71, a scanning line driving circuit 74, and a signal Line drive circuit 76, and each of the lines arranged in parallel or approximately parallel, and driven by scan line drive circuit 74 m scan lines 77 whose potential is controlled, and each of them is arranged in parallel or approximately parallel, and the signal It has n signal lines 79 whose potential is controlled by a line drive circuit 76, and m, n are, and Both are integers greater than or equal to 1. Furthermore, the pixel section 71 consists of multiple pixels 7 arranged in a matrix. It has 0. Also, capacitive wiring is arranged parallel or substantially parallel to each other along the scan line 77. It has 75. In addition, the scan line drive circuit 74 and the signal line drive circuit 76 are collectively called the drive circuit section. There are cases like that.
[0203] Each scan line 77 is one of the pixels 70 arranged in m rows and n columns in the pixel section 71. It is electrically connected to n pixels 70 arranged in any row. Also, each signal line 79 Of the m rows and n columns of pixels 70, m pixels 70 located in any of the columns are charged. They are electrically connected. Also, each capacitance wiring 75 is connected to one of the pixels 70 arranged in m rows and n columns. It is electrically connected to n pixels 70 arranged in any row.
[0204] Figure 13(B) can be used for the pixels 70 of the liquid crystal display device 80 shown in Figure 13(A). This shows an example of a circuit configuration.
[0205] The pixel 70 shown in Figure 13(B) consists of a liquid crystal element 51, a transistor 50, and a capacitive element 55. It has, and
[0206] One of the pair of electrodes of the liquid crystal element 51 is connected to the transistor 50, and the potential is such that the pixel 70 It is set appropriately according to the specifications. The other of the pair of electrodes of the liquid crystal element 51 is a common wire (shown in the figure) It is connected to (not), and a common potential (common potential) is applied to each pixel. The orientation state of the liquid crystal in element 51 is controlled by the data written to transistor 50. It will be done.
[0207] Furthermore, the liquid crystal element 51 controls the transmission or non-transmission of light by the optical modulation effect of the liquid crystal. It is an element that... Note that the optical modulation effect of liquid crystals is due to the electric field applied to the liquid crystal (horizontal electric field, vertical electric field). It is controlled by an electric field in the direction or an electric field in the oblique direction. Liquid crystals include thermotropic liquid crystals, low molecular weight liquid crystals, polymer liquid crystals, polymer dispersed liquid crystals, and strong Dielectric liquid crystals, antiferroelectric liquid crystals, etc., can be used. These liquid crystal materials can be used depending on the conditions. Cholesteric phase, smectic phase, cubic phase, chiral nematic phase, isotropic phase This indicates things like this.
[0208] Furthermore, when employing a transverse electric field method, it is also possible to use a liquid crystal that exhibits a blue phase without using an alignment layer. The blue phase is one of the liquid crystal phases, and as the temperature of cholesteric liquid crystal is increased, the cholesteric phase This phase appears just before the transition from the blue phase to the isotropic phase. The blue phase only appears within a narrow temperature range. To improve the temperature range, a liquid crystal assembly containing several weight percent or more of chiral agent was mixed in. The resulting product is used in the liquid crystal layer. The liquid crystal composition containing a liquid crystal exhibiting a blue phase and a chiral agent is It has a short response speed and is optically isotropic. It also contains a liquid crystal exhibiting a blue phase and a chiral agent. The liquid crystal composition does not require alignment treatment and has low viewing angle dependence. Furthermore, it does not require an alignment layer. Since this is also good, rubbing treatment is unnecessary, thus eliminating the electrostatic discharge caused by rubbing treatment. This can prevent damage and reduce defects and breakage of liquid crystal display devices during the manufacturing process. ru.
[0209] The driving method for the liquid crystal display device 80 having liquid crystal elements 51 is TN (Twisted Nematic mode, IPS (In-Plane-Switching) mode, F FS (Fringe Field Switching) mode, ASM (Axiall y Symmetric aligned Micro-cell) mode, OCB(O (Pyral Compensated Birefringence) mode, FLC (Ferroelectric Liquid Crystal) mode, AFLC(A Using modes such as ntiFerroelectric Liquid Crystal It is possible.
[0210] Furthermore, as a driving method for the liquid crystal display device 80 having liquid crystal elements 51, MVA (Multi -Domain Vertical Alignment) mode, PVA (Patte Vertical Alignment (ASV) mode, etc. Directional mode can be used.
[0211] In the configuration of the pixel 70 shown in Figure 13(B), the source electrode and drain of the transistor 50 One end of the in electrode is electrically connected to the signal line 79, and the other end is connected to the pair of electrodes of the liquid crystal element 51. It is electrically connected to one side. Also, the gate electrode of transistor 50 is electrically connected to scan line 77. They are connected precisely. Transistor 50 has the function of controlling the writing of data to the data signal. To possess.
[0212] In the configuration of the pixel 70 shown in Figure 13(B), one of the pair of electrodes of the capacitive element 55 is A pair of capacitive elements 55 are connected to the source electrode and the other of the drain electrode of the transistor 50. The other electrode is electrically connected to the capacitive wiring 75. The potential value of the capacitive wiring 75 is, It is set appropriately according to the specifications of 70. The capacitive element 55 holds the written data. It functions as a capacity-generating resource.
[0213] <Example configuration of a liquid crystal display device> Next, the specific configuration of the liquid crystal display device 80 will be described. First, the liquid crystal display device 80 is Figure 14 shows a top view of the multiple pixels 70R, 70G, and 70B. In the top view, Only the configuration of the element substrate included in the liquid crystal display device 80 is shown. Also, Figure 14 Figure 15 shows a cross-sectional view of the liquid crystal display device 80 along the dashed line P1-P2. For example, pixel 70 R, 70G, and 70B are pixels that display red, green, and blue, respectively. This display is a liquid crystal display. Device 80 emits red, green, and blue light at positions where pixels 70R, 70G, and 70B overlap, respectively. This can be achieved by having selectively permeable colored films 340R, 340G, and 340B.
[0214] The liquid crystal display device 80 has pixels 70R, 70G, and 70B. It has a pixel electrode 320R and a transistor 50R, and the pixel 70G has a pixel electrode 320G and It has a transistor 50G, and the pixel 70B has a pixel electrode 320B and a transistor 50B. Transistor 50R is electrically connected to signal line 79R and scan line 77. Transistor 50G is electrically connected to signal line 79G and scan line 77. 0B is electrically connected to signal line 79B and scan line 77.
[0215] Furthermore, pixel 70R has a pair of electrodes consisting of pixel electrode 320R and oxide semiconductor film 311R. It has a capacitive element. Pixel 70G has a pixel electrode 320G and an oxide semiconductor film 311G. It has capacitive elements as a pair of electrodes. Pixel 70B has a pixel electrode 320B and an oxide semiconductor film 3 It has a capacitive element with 11B as a pair of electrodes. Oxide semiconductor films 311R, 311G, 3 11B is electrically connected to the capacitive wiring 75.
[0216] The liquid crystal display device 80 has at least three transistors (50R, Having 50G and 50B), an insulating film 318 covering the transistor and covering the insulating film 318 It has an insulating film 319 (see Figure 15). Pixel electrodes 320R, 320G, and 320B are insulated. It is provided on the film 319.
[0217] Furthermore, through the apertures of the insulating films 314, 316, 318, and 319, the pixel electrode 320R and The source or drain electrode of transistor 50R is electrically connected to the pixel electrode 32 The source or drain electrode of transistor 50G is electrically connected to the 0G, and the pixel is electrically connected. The source or drain electrode of the 320B electrode and the 50B transistor are electrically connected. Alignment films 335 are provided on the pixel electrodes 320R, 320G, and 320B.
[0218] The liquid crystal display device 80 has colored films 340R, 340G, and 340B on the substrate 303 side. Each colored film has an insulating film 344, a common electrode 345, and an alignment film 336 that overlap each other. For example, the liquid crystal element 51B in pixel 70B consists of a pixel electrode 320B and a common electrode 34 5 is composed of a liquid crystal layer 341 sandwiched between the pixel electrode 320B and the common electrode 345. The insulating film 344 may also have the function of a planarizing film. It is also acceptable to omit this configuration.
[0219] Furthermore, one end of the pixel electrode 320B is separated by the insulating film 330a. It is mounted on top of G, and the other end of the pixel electrode 320B has an insulating film 330b sandwiched between them. It is mounted on top of the pixel electrode 320R.
[0220] In Figure 15, insulating films 330a and 330b are the pixel electrodes 320R and 320G, respectively. Although it is provided only near the end so as to cover the end, it is not limited to this. As shown in Figure 16. Thus, the insulating film 330B covers the edges of the pixel electrodes 320R and 320G, and the insulating film 330 B and the end of the pixel electrode 320B may be positioned to roughly coincide. (See Figure 16 for example: Liquid crystal) In the display device 80, an aperture is provided in the insulating film 330B, and the pixel electrode 3 is connected through the aperture. The source or drain electrode of transistor 20B and transistor 50B are electrically connected.
[0221] Furthermore, in Figure 16, an insulating film 330B is provided below the pixel electrode 320B, and the pixel electrode 320R, Although the configuration does not include a 320G below it, this is not the only option. As shown in Figure 17, In the pixel 70R adjacent to pixel 70G, an insulating film 330R is provided beneath the pixel electrode 320R. Furthermore, in the pixel 70G adjacent to pixel 70R, an insulating film 330G is placed beneath the pixel electrode 320G. A feature may be provided. With this configuration, pixels 70R, 70G, and 70B are each In a liquid crystal display device having multiple pixels, the aperture ratio of pixels 70R, 70G, and 70B is uniformly increased. It is possible.
[0222] By the way, when there is an air gap between two adjacent pixel electrodes, at a position that overlaps with the air gap A structure may be formed. The liquid crystal display device shown in Figure 18 has a pixel electrode 320R and a pixel electrode 3 20G, pixel electrode 320G and pixel electrode 320B, and pixel electrode 320B and pixel electrode 320 There is a gap between R, and a structure 333 is located on the insulating film 318 at a position overlapping with the gap. As the structure 333, a material that blocks visible light can be used. For example, the structure 333 is made of a material that blocks visible light. It functions as a rack matrix. Structure 333 is used to support the lower layers below structure 333. When there are wires or other components present, this suppresses the reflection of ambient light by those wires, thereby improving the performance of reflective liquid crystal displays. It can improve trust.
[0223] Furthermore, as shown in Figure 19, multiple pixel electrodes in a liquid crystal display device are made using multiple materials. This configuration may be used. In Figure 19, the pixel electrodes 320R and 320G are made of the same material. They can be formed simultaneously. Also, the pixel electrode 320B is made of a different material than the pixel electrodes 320R and 320G. Materials are used. For example, APC is used for pixel electrodes 320R and 320G, and for pixel electrode 320B Aluminum can be used. Aluminum is suitable for the blue light wavelength range (e.g., 400 Because the reflectance in the range of 450 nm to 450 nm is higher than that of APC, the colored film 340B has It can be suitably used as the pixel electrode of pixel 70B. Also, the pixel electrode 320R, By changing the film thickness of 320G and the pixel electrode 320B, the thickness of the liquid crystal layer 341 of the liquid crystal element can be changed. This can be adjusted for each pixel. Depending on the wavelength of light passing through the liquid crystal layer 341, the liquid crystal layer 3 By changing the thickness of 41, it is possible to efficiently extract ambient light in a reflective liquid crystal display. Yes, it is possible. In Figure 19, the insulating film 330 is provided between adjacent pixels of different colors. The edges of the upper pixel electrodes (320G, 320R) and the insulating film 330 are roughly aligned. Furthermore, the insulating film 330 is entirely provided on the insulating film 319. It may be provided on the pixel electrode so as to cover the end of the pixel electrode. In Figure 20, insulating film 3 30 is provided so as to cover the end of the pixel electrode 320B. The ends of the pixel electrodes (320G, 320R) located on the insulating film 330 are at the edge of the insulating film 330. It may be located inside the section.
[0224] A liquid crystal display device according to one aspect of the present invention is provided with an insulating film between two adjacent pixel electrodes. In the top surface shape, the gap between two adjacent pixel electrodes can be eliminated. By having such a configuration, the aperture ratio of the pixels can be increased. According to one aspect of the present invention, The aperture ratio of the liquid crystal display device is 75% or more and less than 100%, preferably 90% or more and less than 100%. More preferably, it can be 98% or more but less than 100%.
[0225] Furthermore, in the upper surface shape, the boundary between two adjacent pixel electrodes separated by the insulating film 330, and It is preferable that the boundaries between the two pixel electrodes and the colored films that overlap them do not coincide. For example, as shown in Figure 22, the pixel electrode 320B is superimposed on the colored film 340R near its end. It is preferable to provide it in such a way.
[0226] Since the pixel electrode 320B and the adjacent pixel electrode 320R are on the insulating film 330, the insulating film 3 The distance between the pixel electrode 320R and the common electrode 345 on 30 is the distance between the pixel electrode 320B and the common electrode It is smaller than the distance to pole 345. Also, an insulating film 330 and an image near the side surface of pixel electrode 320B. pixel electrode 320R is positioned. From the above, the boundary between the pixel electrode 320B and the pixel electrode 320R near the boundary, the electric field applied between the pixel electrode 320B and the common electrode 345 is smaller than the electric field applied between the pixel elec trode 320R and the common electrode 345. Therefore, the electric field formed by the pixel electrode 32 0R also reaches a position overlapping the vicinity of the end portion of the pixel electrode 320B. For this reaso n, by providing the pixel electrode 320B such that the vicinity of its end portion overlaps the colored film 340R , light leakage from the pixel 70B in the display of the pixel 70R can be effectively suppressed. For the same reason, by providing the pixel electrode 320B such that the vicinity of its end portion overlaps the colored film 340G , light leakage from the pixel 70B in the display of the pixel 70G can be effectively suppressed.
[0227] For example, in FIG. 22, the width W of the pixel electrode 320R R , the width W of the pixel electrode 320G G are respectively 18 μm, and the width W of the pixel electrode 320B B1 is 21.5 μm. Also, APC the thicknesses of the pixel electrodes 320R and 320G formed using are each 100 nm, and the thickness of the pixel electrode 320B formed using aluminum is 300 nm. When the distance d1 between the surface of the pixel electrode 320R and the surface of the common electrode 345 is 2.2 μm, the pixel electrode the end portion of 320B is disposed 0.5 μm outward from the end portion of the colored film 340B, that is, the colored film the width W of 340B is set to 20.5 μm, whereby light leakage of the liquid crystal display device 80 is suppressed, B2 and consequently the color purity of display can be improved. Note that the end portions of the colored film 340B and the colored film 340 R and the end portions of the colored film 340B and the colored film 340G are respectively aligned with each other.
[0228] Furthermore, as shown in Figure 23, a colored film may be provided in contact with the pixel electrode. The color films 340R, 340G, and 340B are placed on the pixel electrodes 320R, 320G, and 320B, respectively. It may be provided in contact with the other. In this case, the alignment film 335 is a colored film 340R, 340G, 340B The orientation film 336 is provided on top of the common electrode 345. By doing so, the reflected light from the pixel electrode of one pixel (for example, pixel 70B) reaches the adjacent pixels ( For example, it suppresses crosstalk passing through the colored film of a 70G pixel, improving the visual clarity of a reflective liquid crystal display. This reduces dependence on field angle. Furthermore, it eliminates the need to apply a colored film to the substrate 303. Therefore, the alignment accuracy required when bonding substrate 302 and substrate 303 can be reduced. This allows for improved yield in the manufacturing of liquid crystal display devices.
[0229] In addition to the configuration shown in Figure 23, an overcoat film is provided on the colored film, and a conductive film is provided on the insulating film. A film may be provided. The liquid crystal display device shown in Figure 24 has colored films 340R, 340G, and 340B. On top of that, there is an overcoat film 337 and conductive films 325R, 325G, and 325B. The film 325R is formed through openings provided in the overcoat film 337 and the colored film 340R. It is electrically connected to the base electrode 320R. The conductive film 325G is the overcoat film 337 and It is electrically connected to the pixel electrode 320G through an opening provided in the colored film 340G. Film 325B is visible through openings provided in the overcoat film 337 and the colored film 340B. It is electrically connected to the base electrode 320B.
[0230] The conductive films 325R, 325G, and 325B are transparent conductive films, for example, common electric The same material as in pole 345 can be used. In the liquid crystal display device shown in Figure 24, For example, the liquid crystal element 51B in pixel 70B consists of a conductive film 325B and a common electrode 345, It is composed of a conductive film 325B and a liquid crystal layer 341 sandwiched between a common electrode 345. The film 325R, 325G, and 325B functions as pixel electrodes. Also, pixel electrode 3 20R, 320G, and 320B have the function of a reflective coating.
[0231] Transistors 50R, 50G, and 50B are the same as transistor 150 described in Embodiment 1. It can be manufactured using the same materials and forming methods as above. Also, transistor 50R, For 50G and 50B, the transistor 270 described in Embodiment 6 may be used.
[0232] As shown in Figure 25, transistors 50R, 50G, and 50B are second gate electrodes. It is preferable to have a pole. The second gate electrode is a semiconductor layer of the transistor and a pixel It can be placed between the electrodes, in a position that overlaps with the semiconductor layer. For example, the second gate electrode is It can be formed simultaneously using the same material as the oxide semiconductor film 311R. (See Figure 25) Compared to Figure 15, the liquid crystal display device 80 has transistors 50R, 50G, and 50B in the second... It differs in that it has an oxide semiconductor film 311a that functions as a gate electrode. Transistor 5 0R, 50G, and 50B have a second gate electrode, which reduces the distance between the semiconductor layer and the pixel electrode. When the potential of the pixel electrodes is close, the effect of changes in their potential on the transistor's characteristics is suppressed. This can be achieved. By providing pixel electrodes in positions that overlap with the transistors, the liquid crystal display device 80 The aperture ratio can be increased.
[0233] Each of the capacitive elements in pixels 70R, 70G, and 70B is the same as the capacitive element described in Embodiment 1. It can be manufactured using the same materials and forming methods as in 160. In the capacitance element, The insulating film 318 and insulating film 319 function as dielectric films.
[0234] The pixel electrodes 320R, 320G, and 320B are the conductive film 12 described in Embodiment 1. It can be manufactured using the same materials and forming methods as in 0. Also, the common electrode 345 and For example, a material that is translucent in visible light can be used. Specifically, The material used contains one element selected from ionium (In), zinc (Zn), and tin (Sn). This is good. Also, as the common electrode 345, for example, indium containing tungsten oxide can be used. Indium zinc oxide containing oxides, tungsten oxide, and indium acid containing titanium oxide Indium tin oxide containing titanium oxide, indium tin oxide (ITO:Indiu Indium tin oxide (m Tin Oxide), indium zinc oxide, indium tin oxide with added silicon dioxide A conductive material with light-transmitting properties, such as an oxide, can be used. Also, the common electrode 345 For example, it can be formed using the sputtering method.
[0235] For the insulating film 344, silicon oxide is produced by plasma CVD, sputtering, etc. Film, silicon oxide nitride film, silicon nitride oxide film, silicon nitride film, aluminum oxide film, Hafnium oxide film, yttrium oxide film, zirconium oxide film, gallium oxide film, t Lanthanum film, magnesium oxide film, lanthanum oxide film, cerium oxide film and neodymium oxide film An insulating film containing one or more of these elements can be used.
[0236] Note that the configurations and methods shown in this embodiment may differ from those shown in other embodiments. It can be used in appropriate combinations.
[0237] (Embodiment 5) In this embodiment, the invention is applied to the transistors and capacitive elements of a liquid crystal display device according to one aspect of the present invention. An example of a possible oxide semiconductor is described below.
[0238] The structure of oxide semiconductors will be described below.
[0239] In this specification, "parallel" means that two lines are positioned at an angle of -10° or more and 10° or less. This refers to a state in which it is in a certain condition. Therefore, it also includes cases where the angle is between -5° and 5°. Also, "abbreviated "Parallel" refers to a state where two straight lines are positioned at an angle between -30° and 30°. Furthermore, "perpendicular" refers to a state where two straight lines are positioned at an angle between 80° and 100°. This refers to the case where the angle is between 85° and 95°. Furthermore, "approximately perpendicular" means This refers to a state where two straight lines are positioned at an angle between 60° and 120°.
[0240] Furthermore, in this specification, if the crystal is trigonal or rhombohedral, it is listed as hexagonal. vinegar.
[0241] Oxide semiconductors are divided into single-crystal oxide semiconductors and other non-single-crystal oxide semiconductors. As a non-single-crystal oxide semiconductor, CAAC-OS (C Axis Aligned) is used. Crystalline Oxide Semiconductor, Polycrystalline Oxide Semiconductors, nc-OS (nanocrystalline oxide semiconductor) uctor), pseudo-amorphous oxide semiconductor (a-like OS: amorphous l Examples include amorphous oxide semiconductors (ike Oxide Semiconductor).
[0242] From another perspective, oxide semiconductors include amorphous oxide semiconductors and other crystalline oxides. They can be divided into semiconductors and crystalline oxide semiconductors. Crystalline oxide semiconductors include single-crystal oxide semiconductors and CAAC- Examples include OS, polycrystalline oxide semiconductors, and nc-OS.
[0243] Generally, an amorphous structure is defined as a structure that is not fixed in a metastable state and is isotropic. It is known that it does not have a heterogeneous structure. Also, the bond angles are flexible and short distance It can also be described as a structure that possesses deorderliness but lacks long-range orderliness.
[0244] Conversely, in the case of oxide semiconductors, which are inherently stable, they are perfectly amorphous (complete It cannot be called an oxide semiconductor (which is amorphous). Also, it is not isotropic. (For example, an oxide semiconductor having a periodic structure in a minute region) is subjected to complete amorphous oxidation. It cannot be called a physical semiconductor. However, a-like OS is a circumferential material in a minute region. Although it has a structural form, it also has voids (also called porous structures) and is therefore an unstable structure. In terms of physical properties, it can be said to be similar to an amorphous oxide semiconductor.
[0245] <caac-os> First, let me explain CAAC-OS.
[0246] CAAC-OS is an oxide having multiple c-axis oriented crystalline portions (also called pellets). It is a type of semiconductor.
[0247] Transmission Electron Microscope (TEM) A composite analysis image of the bright-field image and diffraction pattern of CAAC-OS (high-angle scope) is obtained. Also called a high-resolution TEM image, when observed, multiple pellets can be identified. On the other hand, in high-resolution TEM images, the boundaries between pellets, i.e., grain boundaries, and It is also said that it is not possible to clearly confirm the grain boundaries. Therefore, CAAC-OS is said to be at the grain boundaries. This means that a decrease in electron mobility caused by this phenomenon is less likely to occur.
[0248] The following describes CAAC-OS observed by TEM. Figure 26(A) The image shows a high-resolution TEM image of the cross-section of CAAC-OS observed from a direction approximately parallel to the sample surface. For observing high-resolution TEM images, spherical aberration correction is necessary. The n Corrector function was used. High-resolution TEM images using spherical aberration correction function were obtained. This is specifically called a Cs-corrected high-resolution TEM image. Acquisition of a Cs-corrected high-resolution TEM image can be done, for example, This is performed using an atomic-resolution analytical electron microscope such as the JEM-ARM200F manufactured by JEOL Ltd. It is possible.
[0249] Figure 26(B) shows an enlarged Cs-corrected high-resolution TEM image of region (1) in Figure 26(A). Figure 26(B) shows that the metal atoms in the pellet are arranged in layers. The arrangement of metal atoms in each layer is the plane (also called the surface to be formed) that forms the CAAC-OS film. Alternatively, it reflects the irregularities of the upper surface and is parallel to the surface or upper surface of the CAAC-OS that is formed on it.
[0250] As shown in Figure 26(B), CAAC-OS has a characteristic atomic arrangement. Figure 26(C Figures 26(B) and 26(C) show characteristic atomic arrangements indicated by auxiliary lines. ) Therefore, the size of a single pellet can be 1 nm or larger, or 3 nm or larger, It can be seen that the size of the gap created by the tilt between the toe and the pellet is approximately 0.8 nm. Therefore, pellets can also be called nanocrystals (nc). Furthermore, CAAC-OS is used in CANC (C-Axis Aligned nanocr It can also be called an oxide semiconductor containing ystals.
[0251] Here, based on the Cs-corrected high-resolution TEM image, the pellets of CAAC-OS on substrate 5120 are... The arrangement of the 5100 can be schematically represented as a structure resembling stacked bricks or blocks. This is the result (see Figure 26(D)). Between the pellets observed in Figure 26(C) The area where the inclination occurs corresponds to region 5161 shown in Figure 26(D).
[0252] Furthermore, Figure 27(A) shows the plane of CAAC-OS observed from a direction approximately perpendicular to the sample surface. The s-corrected high-resolution TEM images are shown. Regions (1), (2), and (3) of Figure 27(A) are shown. ) are enlarged Cs-corrected high-resolution TEM images, shown in Figure 27(B), Figure 27(C), and This is shown in Figure 27(D). From Figures 27(B), 27(C), and 27(D), the pellets are It can be confirmed that the metal atoms are arranged in a triangular, square, or hexagonal shape. However, no regularity is observed in the arrangement of metal atoms between different pellets.
[0253] Next, C was analyzed by X-ray diffraction (XRD). Let's discuss AAC-OS. For example, CAAC-OS having an InGaZnO4 crystal. When structural analysis of S is performed using the out-of-plane method, the result is as shown in Figure 28(A). In some cases, a peak may appear near a diffraction angle (2θ) of 31°. This peak is in InGa Since it is attributed to the (009) plane of the ZnO4 crystal, the CAAC-OS crystal is c-axis oriented. It can be confirmed that it possesses this property, and that the c-axis is oriented in a direction approximately perpendicular to the surface to be formed or the upper surface.
[0254] In addition, in the structural analysis using the out-of-plane method of CAAC-OS, 2θ is 31 In addition to the peak near °, a peak may also appear when 2θ is near 36°. The nearby peak indicates that some of the crystals in CAAC-OS do not exhibit c-axis orientation. This shows that a more preferable CAAC-OS is structured using the out-of-plane method. The analysis shows that 2θ shows a peak near 31°, but does not show a peak near 36°.
[0255] On the other hand, in the CAAC-OS, X-rays are incident from a direction approximately perpendicular to the c-axis in an in-plane configuration. Structural analysis using the ne method reveals a peak near 2θ = 56°. This peak corresponds to I It is attributed to the (110) plane of the nGaZnO4 crystal. In the case of CAAC-OS, 2θ is 5 The sample is fixed at approximately 6° and analyzed while rotating it around the normal vector of the sample surface as the axis (φ axis). Even after performing a (φ scan), no clear peak appears, as shown in Figure 28(B). In contrast, with a single-crystal oxide semiconductor of InGaZnO4, if 2θ is fixed to around 56°, then φ When scanned, it is attributed to a crystal plane equivalent to the (110) plane, as shown in Figure 28(C). Six peaks are observed. Therefore, structural analysis using XRD indicates that CAAC-OS is It can be confirmed that the orientation of the a-axis and b-axis is irregular.
[0256] Next, we will explain CAAC-OS analyzed by electron diffraction. For example, InGa For CAAC-OS containing ZnO4 crystals, a probe with a diameter of 300 nm is used parallel to the sample surface. When the electron beam is incident, a diffraction pattern like the one shown in Figure 29(A) (limited field transmitted electron wave) is produced. This diffraction pattern may appear. (Also called a diffraction pattern.) The spot originates from the (009) plane of the crystal. Therefore, electron diffraction also reveals The pellets contained in CAAC-OS have c-axis orientation, and the c-axis is on the surface to be formed or the upper surface. It can be seen that it is oriented in a nearly perpendicular direction. On the other hand, for the same sample, when the probe is directed perpendicular to the sample surface... Figure 29(B) shows the diffraction pattern when an electron beam with a diameter of 300 nm is incident on the surface. From 9(B), a ring-shaped diffraction pattern is observed. Therefore, electron diffraction also shows It can be seen that the a-axis and b-axis of the pellets contained in CAAC-OS do not have orientation. Note that the first ring in Figure 29(B) is the (010) plane of the InGaZnO4 crystal. This is thought to be caused by the nominal (100) plane, etc. Also, the second ring in Figure 29(B) This is thought to be caused by (110) planes, etc.
[0257] As mentioned above, CAAC-OS is a highly crystalline oxide semiconductor. Crystallinity may decrease due to entry of impurities, generation of defects, or the like; therefore, from a different perspective , a CAAC-OS can also be referred to as an oxide semiconductor with few impurities and few defects (such as oxygen vacancies).
[0258] Note that impurities are elements other than the main components of the oxide semiconductor, and include hydrogen, carbon, silicon, transition metal eleme nts, and the like. For example, an element such as silicon, which has a stronger bonding force with oxygen than the metal element included in the oxide semiconductor, deprives the oxide semiconductor of oxygen, thereby disturbing the atomic arrangement of the oxide semiconductor and becoming a factor that reduces crystallinity. In addition, heavy metals such as iron and nickel, argon, carbon dioxide, and the like have large atomic radii (or large molecular radii), and thus disturb the atomic arrangement of the oxide semiconductor and become a factor that reduces crystallinity.
[0259] In the case where an oxide semiconductor has impurities or defects, its characteristics might vary due to light, heat, or the like. For example, impurities contained in the oxide semiconductor might serve as carrier traps or might serve as carrie r generation sources. In addition, oxygen vacancies in the oxide semiconductor might serve as carrier traps or might serve as carrier generation sources by capturing hydrogen.
[0260] A CAAC-OS with few impurities and few oxygen vacancies is an oxide semiconductor with a low carrier densit y. Specifically, it is less than 8×10 11 / cm 3 , preferably less than 1×10 11 / cm 3 less , further preferably less than 1×10 10 / cm 3 , and can be an oxide semiconductor with a carrier density of 1×10 -9 / cm 3 or more . Such an oxide semiconductor is referred to as a highly purified These are called intrinsic or substantially high-purity intrinsic oxide semiconductors. CAAC-OS has an impurity concentration of It has a low defect level density. In other words, it can be said to be an oxide semiconductor with stable properties.
[0261] <nc-os> Next, I will explain nc-OS.
[0262] nc-OS allows for the identification of crystalline regions in high-resolution TEM images, and It has regions where a definite crystalline portion cannot be identified. The crystalline portion contained in nc-OS is They are often between 1 nm and 10 nm in size, or between 1 nm and 3 nm in size. Oh, an oxide semiconductor with a crystal size greater than 10 nm and less than 100 nm is microcrystalline acid It is sometimes called a monoxide semiconductor. nc-OS, for example, shows grain boundaries in high-resolution TEM images. In some cases, this cannot be clearly confirmed. Furthermore, nanocrystals are pellets in CAAC-OS. It may share the same origin. Therefore, below, the crystalline portion of nc-OS will be treated as a pellet. They may call.
[0263] nc-OS is used in minute regions (for example, regions between 1 nm and 10 nm, especially regions larger than 1 nm). It has periodicity in the atomic arrangement in the region of 3 nm or less. In addition, nc-OS has different properties. No regularity is observed in the crystal orientation between the letts. Therefore, no orientation is observed throughout the entire film. Therefore, depending on the analytical method, nc-OS may be a-like OS or amorphous oxide semiconductor. It can sometimes be indistinguishable from the body. For example, nc-OS has a larger diameter than pellets. When using X-rays, out-of-plane analysis shows peaks indicating crystal planes. Not detected. Also, for nc-OS, a probe diameter larger than the pellet (e.g., 50 When electron diffraction is performed using an electron beam (of a magnitude greater than nm), a diffraction pattern similar to a halo pattern is obtained. Observed. On the other hand, compared to nc-OS, the pellet size is close to or smaller than the pellet size. When nanobeam electron diffraction is performed using an electron beam with a lobe diameter, spots can be observed. When nanobeam electron diffraction is performed on nc-OS, a high-brightness pattern is observed, forming a circular (ring-shaped) pattern. In some cases, a region may be observed. Furthermore, multiple spots may be observed within a ring-shaped region. There are cases where this occurs.
[0264] Thus, since there is no regularity in the crystal orientation between pellets (nanocrystals), nc -OS has RANC (Random Aligned nanocrystals) Oxide semiconductors, or NANC (Non-Aligned nanocrystals), It can also be called an oxide semiconductor having s).
[0265] nc-OS is an oxide semiconductor with higher orderliness than amorphous oxide semiconductors. nc-OS has a lower defect level density than a-like OS and amorphous oxide semiconductors. However, nc-OS does not show any regularity in crystal orientation between different pellets. Therefore, nc-OS has a higher defect level density compared to CAAC-OS.
[0266] <a-like OS> a-like OS is an oxide having a structure between nc-OS and amorphous oxide semiconductors. It is a semiconductor.
[0267] a-like OS may exhibit porosity in high-resolution TEM images. Furthermore, In the high-resolution TEM image, there are regions where the crystalline portion can be clearly identified, and regions where the crystalline portion can be clearly identified. It has areas that cannot be done.
[0268] Due to its porous nature, a-like OS has an unstable structure. Below, a-lik This demonstrates that e OS has a less stable structure compared to CAAC-OS and nc-OS. Therefore, it shows the structural changes caused by electron irradiation.
[0269] The samples to be irradiated with electrons are a-like OS (referred to as sample A) and nc-OS. Prepare (referred to as Sample B) and CAAC-OS (referred to as Sample C). This sample is also an In-Ga-Zn oxide.
[0270] First, high-resolution cross-sectional TEM images are obtained for each sample. It can be seen that all of the materials contain crystalline parts.
[0271] The determination of which part should be considered a single crystal can be made as follows. The unit cell of the InGaZnO4 crystal has three In-O layers and a Ga-Zn-O layer. It is known to have a structure in which a total of nine layers, consisting of six layers, are stacked in layers along the c-axis. The spacing between these adjacent layers is approximately the same as the spacing between the grid planes of the (009) plane (also called the d value). Therefore, the value has been determined to be 0.29 nm from crystal structure analysis. The areas where the spacing is between 0.28 nm and 0.30 nm are considered to be the crystalline parts of InGaZnO4. It can be considered as such. Furthermore, the lattice patterns correspond to the ab-plane of the InGaZnO4 crystal.
[0272] Figure 30 shows an example of investigating the average size of the crystalline regions (22 to 45 locations) in each sample. However, the length of the lattice fringes mentioned above is used as the size of the crystal portion. From Figure 30, a-li It can be seen that the crystalline portion of keOS increases in proportion to the cumulative amount of electron irradiation. Specifically, as shown in (1) in Figure 30, the initial TEM observation is approximately 1.2 nm. The crystal region (also called the initial nucleus), which was initially a certain size, increased in size when the cumulative irradiation dose reached 4.2 × 10⁻⁶. 8 e - / n m 2 In this case, it can be seen that it has grown to a size of about 2.6 nm. On the other hand, nc-O S and CAAC-OS have a cumulative electron dose of 4.2 × 10⁻⁶ from the start of electron irradiation. 8 e - / nm 2 Within this range, it can be seen that there is no change in the size of the crystal portion. Specifically, As shown in (2) and (3) in Figure 30, regardless of the cumulative dose of electrons, nc-OS The crystal size of CAAC-OS is approximately 1.4 nm and 2.1 nm, respectively. It can be seen that this is the case.
[0273] Thus, in a-like OS, crystalline growth can be observed upon electron irradiation. Yes. On the other hand, in nc-OS and CAAC-OS, the growth of the crystal portion by electron irradiation is almost entirely... It can be seen that it cannot be seen. In other words, a-like OS is nc-OS and CAAC- Compared to an operating system, it appears to have an unstable structure.
[0274] Furthermore, because it is porous, a-like OS is compared to nc-OS and CAAC-OS. All of them are low-density structures. Specifically, the density of a-like OS is low compared to single-layer structures of the same composition. The density of the crystal will be between 78.6% and 92.3%. Also, the density of nc-OS and CAA The density of C-OS is between 92.3% and 100% of the density of a single crystal of the same composition. Oxide semiconductors with a crystal density of less than 78% are inherently difficult to deposit into film.
[0275] For example, in an oxide semiconductor satisfying In:Ga:Zn=1:1:1 [atomic ratio], The density of single-crystal InGaZnO₄ having a rhombohedral crystal structure is 6.357 g / cm 3 It becomes. There fore, for example, in an oxide semiconductor satisfying In:Ga:Zn=1:1:1 [atomic ratio] , the density of the a-like OS is 5.0 g / cm 3 or more and 5.9 g / cm 3 less than. Fur ther, for example, in an oxide semiconductor satisfying In:Ga:Zn=1:1:1 [atomic ratio] , the density of the nc-OS and the density of the CAAC-OS are 5.9 g / cm 3 or more and 6.3 g / cm 3 less than.
[0276] Note that a single crystal having the same composition may not exist. In that case, by combining single crystals with different compositions at any ratio, the density corresponding to a single crystal of the desired composition can be estimated. By combining single crystals with different compositions at any ratio, the density corresponding to a single crystal of the desired composition can be estimated. The density corresponding to the single crystal of the desired composition can be estimated using a weighted average with respect to the ratio of combining the single crystals having different compositions. However, it is preferable to estimate the density by combining as few types of single crystals as possible. It is preferable to estimate the density by combining as few types of single crystals as possible.
[0277] As described above, oxide semiconductors can have various structures, each having various characteristics. Note that the oxide semiconductor may be, for example, a stacked film including two or more of an amorphous oxide semiconductor, an a-like OS, and an nc-OS. , a stacked film including two or more of CAAC-OS.
[0278] <Method for Depositing CAAC-OS> Hereinafter, an example of a method for depositing a CAAC-OS will be described. Figure 31 is a schematic view inside a deposition chamber. The CAAC-OS can be deposited by a sputtering method.
[0279] As shown in Figure 31, the substrate 5220 and the target 5230 are positioned facing each other. There is a plasma 5240 between the substrate 5220 and the target 5230. Also, A heating mechanism 5260 is provided at the bottom of the substrate 5220. Although not shown, a target 5230 is bonded to the backing plate. The target is via the backing plate. Multiple magnets are positioned opposite the 5230. The sputtering method that uses magnetrons to increase the film deposition rate is called the magnetron sputtering method. It can be done.
[0280] The distance d between the substrate 5220 and the target 5230 (Target-substrate distance (TS distance) It is also called (separation). The distance is 0.01m or more and 1m or less, preferably 0.02m or more and 0.5m or less. The deposition chamber is mostly filled with deposition gas (e.g., oxygen, argon, or 5 volumes of oxygen). It is filled with a mixed gas containing a proportion of % or more, and the pressure is preferably between 0.01 Pa and 100 Pa. It is controlled to be between 0.1 Pa and 10 Pa. Here, target 5230 is above a certain level By applying voltage, discharge begins and plasma 5240 is confirmed. A high-density plasma region is formed in the vicinity of T5230 by a magnetic field. In this region, the film-forming gas is ionized, generating ion 5201. Ion 5201 is For example, the cation of oxygen (O + ) and the cation of argon (Ar + ) and so on.
[0281] Target 5230 has a polycrystalline structure with multiple crystal grains, and in any of the crystal grains This includes the cleavage plane. As an example, Figure 32 shows the InMZn contained in target 5230. This shows the crystal structure of O4 (where element M is, for example, Al, Ga, Y, or Sn). Note that Figure 32 ( A) is the crystal structure of InMZnO4 when observed from a direction parallel to the b-axis. In ZnO4 crystals, the oxygen atoms have a negative charge, which causes two adjacent M-Zn atoms to form a Zn complex. -A repulsive force is generated between the O layers. Therefore, the InMZnO4 crystal has two adjacent M -The Zn-O layer has a cleavage plane.
[0282] Ions 5201 generated in the high-density plasma region are directed toward target 5230 by the electric field. It is accelerated and eventually collides with target 5230. At this time, from the cleavage plane, it becomes flat or pegged. The pellet 5200, which is a red-shaped sputtered particle, peels off (see Figure 31). Pellet 5 200 is the portion sandwiched between the two cleavage planes shown in Figure 32(A). Therefore, pellet 5 If we extract only 200, its cross-section will look like Figure 32(B), and its top surface will look like Figure 32(C). It can be seen that this will happen. Furthermore, pellet 5200 is affected by the impact of the collision of ion 5201. This can cause structural distortion.
[0283] Pellet 5200 is a flat plate or pellet having a triangular, for example, equilateral triangle plane. These are sputtered particles. Alternatively, pellet 5200 has a hexagonal, for example, regular hexagonal plane. The sputtered particles are flat or pellet-shaped. However, the shape of the pellet 5200 is not specified. This is not limited to triangles or hexagons; for example, it can also refer to shapes formed by combining multiple triangles. There is a quadrilateral (for example, a rhombus) formed by joining two triangles (for example, equilateral triangles). ) This can also happen.
[0284] The thickness of pellet 5200 is determined according to the type of film-forming gas used. For example, pellet 5200 has a thickness of 0.4 nm or more and 1 nm or less, preferably 0.6 nm or more and 0.8 nm or less. The following applies. Also, for example, pellet 5200 is preferably 1 nm or more and 100 nm or less in width. The wavelength is 2 nm to 50 nm, more preferably 3 nm to 30 nm. Ions 5201 are then collided with target 5230, which has In-M-Zn oxide. Then, a pellet 5 having three layers: an M-Zn-O layer, an In-O layer, and an M-Zn-O layer. 200 detaches. Furthermore, as pellet 5200 detaches, particles detach from target 5230. Particle 5203 is also ejected. Particle 5203 consists of one atom or an aggregate of several atoms. Therefore, particle 5203 is called an atomic particle. It's also possible.
[0285] As the pellet 5200 passes through the plasma 5240, its surface becomes negatively or positively charged. There are cases where this occurs. For example, when pellet 5200 is in plasma 5240 2- Negative charge This can result in the oxygen atoms on the surface of pellet 5200 becoming negatively charged. There is a combination. Also, when pellet 5200 passes through plasma 5240, plasma 52 It can grow by bonding with indium, element M, zinc, or oxygen in 40. .
[0286] The pellets 5200 and particles 5203 that have passed through the plasma 5240 are on the substrate 5220. It reaches the surface. Note that some of the particles 5203 have a small mass and can be removed by a vacuum pump, etc. It may be released into the environment.
[0287] Next, regarding the deposition of pellets 5200 and particles 5203 on the surface of substrate 5220 Let's explain using Figure 33.
[0288] First, the first pellet 5200 is deposited on the substrate 5220. The pellet 5200 is flat. Because of its shape, the pellet 52 is deposited with the flat side facing the surface of the substrate 5220. The charge on the surface of substrate 5220 of 00 is released through substrate 5220.
[0289] Next, the second pellet 5200 reaches the substrate 5220. At this point, it has already been deposited. The surface of the first pellet 5200, and the surface of the second pellet 5200, are charged. Therefore, a force of mutual repulsion is generated. As a result, the second pellet 5200 has already piled up. Avoiding the piled pellets 5200, place the flat side slightly away from the surface of the substrate 5220. They are deposited in that direction. By repeating this process, countless pellets 52 are deposited on the surface of the substrate 5220. 00 is deposited to the thickness of one layer. Also, between the pellets 5200, Areas where sediment has not been deposited will appear (see Figure 33(A)).
[0290] Next, the particle 5203, which has received energy from the plasma, reaches the surface of the substrate 5220. Particle 5203 can be deposited on active areas such as the surface of pellet 5200. No. Therefore, particle 5203 moves to an area where pellet 5200 has not accumulated, and the pellet It adheres to the side of the 5200. Particle 5203 receives energy from the plasma. As the bonding bonds become more active, they chemically connect with the pellet 5200 and the lateral growth portion 52 Forms O2 (see Figure 33(B)).
[0291] Furthermore, as the lateral growth section 5202 grows laterally (also called lateral growth), Connect the pellets 5200 together (see Figure 33(C)). In this way, the pellets 5200 Lateral growth section 5202 is formed until it fills the areas where sediment has not been deposited. This mechanism is The deposition mechanism of the Atomic Layer Deposition (ALD) method It is similar to zumu.
[0292] Therefore, even if the pellets 5200 are stacked facing different directions, Because particles 5203 fill the gaps between grains 5200 while growing laterally, clear grain boundaries are formed. It will not be accomplished. Also, the particles 5203 smoothly connect the pellets 5200. Therefore, a crystal structure different from both single crystals and polycrystalline structures is formed. In other words, minute crystal regions A crystal structure with strain is formed between the regions (pellets 5200). In this way, the crystal region Since the regions filling the gaps are distorted crystalline regions, it is inappropriate to refer to these regions as amorphous structures. It is unlikely to be a serious injury.
[0293] Next, new pellets 5200 are deposited with their flat side facing outwards (see Figure 33(D)). ). Then, particles 5203 pile up to fill the areas where pellets 5200 have not accumulated. By stacking, a lateral growth portion 5202 is formed (see Figure 33(E)). In this way, particle 520 3 adheres to the side of the pellet 5200, and the lateral growth portion 5202 grows laterally, Connect the pellets in the first layer (see Figure 33(F)). The mth layer (m is two or more layers) The film deposition continues until a number of layers are formed, resulting in a thin film structure with a laminate.
[0294] Furthermore, the way the pellets 5200 are deposited can also vary depending on the surface temperature of the substrate 5220. For example, if the surface temperature of substrate 5220 is high, the pellet 5200 will be on the surface of substrate 5220. Migration occurs across the surface. As a result, the pellets 5200 are separated by the particles 5203. Because the proportion of linked molecules increases, it becomes a more oriented CAAC-OS. The surface temperature of the substrate 5220 when depositing the OS film is between room temperature and 340°C, preferably at room temperature. Above 300°C or below, more preferably 100°C or above 250°C, even more preferably 100 The temperature range is between 200°C and 200°C. Therefore, substrate 5220 is a large-area substrate of the 8th generation or higher. Even when using this method, warping caused by the formation of the CAAC-OS film is almost nonexistent. I understand.
[0295] On the other hand, if the surface temperature of the substrate 5220 is low, the pellets 5200 will be on the surface of the substrate 5220. Irrigation becomes less likely. As a result, the 5200 pellets stack up on top of each other. This results in low orientation, such as nc-OS. In nc-OS, the pellet 5200 is negatively charged. As a result, the pellets 5200 may accumulate at regular intervals. Although it has low orientation, it possesses a slight regularity, making it comparable to amorphous oxide semiconductors. It will all have an intricate structure.
[0296] Furthermore, in CAAC-OS, the gaps between pellets become extremely small, Large pellets may form. The interior of one large pellet has a single-crystal structure. It has. For example, the pellet size is 10 nm to 200 nm when viewed from the top surface, 15 The wavelength may be between nm and 100 nm, or between 20 nm and 50 nm.
[0297] Based on the film deposition model described above, it is believed that the pellets will accumulate on the surface of the substrate. CAAC-OS can be deposited even when the surface to be formed does not have a crystalline structure. Therefore, the aforementioned film deposition model, which has a growth mechanism different from epitaxial growth, is highly valid. This can be seen. Also, since it is the film deposition model described above, CAAC-OS and nc-OS This demonstrates that uniform film deposition is possible even on large-area glass substrates. For example, Even if the structure of the substrate surface (the surface to be formed) is amorphous (for example, amorphous silicon oxide), It is possible to deposit CAAC-OS into a film.
[0298] Furthermore, even if the surface of the substrate to be formed has irregularities, the pellets will conform to that shape. It can be seen that they are arranged in a sequence.
[0299] Furthermore, based on the film deposition model described above, in order to deposit a highly crystalline CAAC-OS film, the following is required: It can be seen that this is how it should be done. First, in order to increase the mean free path, a higher vacuum state The film is deposited in this state. Next, in order to reduce damage near the substrate, the plasma energy is Weakening. Next, thermal energy is applied to the surface to be formed, and plasma damage occurs each time a film is deposited. It heals.
[0300] Furthermore, the aforementioned film deposition model is based on the In-M-Zn oxide having multiple crystal grains as the target. When a composite oxide has a polycrystalline structure, and one of the crystal grains contains a cleavage plane. Not limited to, for example, a mixture having indium oxide, an oxide of element M, and zinc oxide. This can also be applied when using an object as a target.
[0301] Because the target of the mixture does not have a cleavage plane, when sputtered, atoms are released from the target. The particles detach. During film formation, a strong plasma field region is formed near the target. Therefore, atomic particles detached from the target are bound together by the action of the strong electric field region of the plasma. They connect and grow laterally. For example, first, indium, which is an atomic particle, connects and grows laterally. -O layers form nanocrystals. Next, M-Zn-O layers are formed above and below to complement them. Combine. Thus, even when using a mixed target, it is possible to form pellets. It has properties. Therefore, even when using a mixed target, the above-mentioned film deposition model can be applied. It is possible.
[0302] However, if a strong electric field region of the plasma is not formed near the target, Only atomic particles detached from the substrate will be deposited on the substrate surface. In that case as well, on the substrate surface In some cases, atomic particles may grow laterally. However, this is because the orientation of atomic particles is not uniform. Furthermore, the crystal orientation in the resulting thin film is not uniform. That is, it becomes nc-OS, etc. .
[0303] (Embodiment 6) In this embodiment, a transistor with a different configuration from the transistor shown in Embodiment 1 is used. The configuration will be explained with reference to Figures 34 to 37.
[0304] <Transistor Configuration Example 1> Figure 34(A) is a top view of transistor 270, and Figure 34(B) is a top view of Figure 34(A). This corresponds to a cross-sectional view of the section between the dashed line X1 and X2 shown, and Figure 34(C) is Figure 34 This corresponds to the cross-sectional view of the section between the dashed line Y1 and Y2 shown in (A). The direction from X1 to X2 is referred to as the channel length direction, and the direction from Y1 to Y2 (marked with a dashed line) is referred to as the channel width direction. There are cases where this is the case.
[0305] Transistor 270 is connected to a conductive film 204 on substrate 202, which functions as the first gate electrode. And, the insulating film 206 on the substrate 202 and the conductive film 204, and the insulating film 207 on the insulating film 206 , an oxide semiconductor film 208 on an insulating film 207, and electrically connected to the oxide semiconductor film 208 A conductive film 212a that functions as a source electrode and an oxide semiconductor film 208 that is electrically connected A conductive film 212b that functions as a drain electrode, an oxide semiconductor film 208, and a conductive film 21 2a and insulating films 214 and 216 on conductive film 212b, and oxide semiconductor film on insulating film 216 It has 211b and an insulating film 218 provided on the oxide semiconductor film 211b.
[0306] Furthermore, in transistor 270, insulating film 214 and insulating film 216 are transistor It functions as a second gate insulating film of 270. Furthermore, the oxide semiconductor film 211a is Through the opening 252c provided in the insulating film 214 and insulating film 216, the conductive film 212b and The oxide semiconductor film 211a is used, for example, as a pixel electrode in a display device. It has the ability. Also, in transistor 270, the oxide semiconductor film 211b is a second gate It functions as a back electrode (also called a back gate electrode).
[0307] Furthermore, as shown in Figure 34(C), the oxide semiconductor film 211b consists of insulating films 206, 207, In the openings 252a and 252b provided in the insulating film 214 and insulating film 216, the first It is connected to the conductive film 204 which functions as a gate electrode. Therefore, the conductive film 220b and the oxide The semiconductor film 211b is given the same potential.
[0308] In this embodiment, openings 252a and 252b are provided, and an oxide semiconductor film 2 The example given illustrates a configuration for connecting 11b and the conductive film 204, but it is not limited to this. , forming only one of either opening 252a or opening 252b, and oxide semi A configuration that connects the conductive film 211b and the conductive film 204, or the opening 252a and the opening 252 Alternatively, b may be omitted, resulting in a configuration where the oxide semiconductor film 211b and the conductive film 204 are not connected. In the case of a configuration in which the oxide semiconductor film 211b and the conductive film 204 are not connected, the oxide semiconductor film 211b and the conductive film 204 can each be given different potentials.
[0309] Furthermore, as shown in Figure 34(B), the oxide semiconductor film 208 is the first gate electrode. The conductive film 204 functions as a second gate electrode, and the oxide semiconductor film 211b functions as a second gate electrode. They are positioned opposite each other and are sandwiched between two conductive films that function as gate electrodes. The length in the channel length direction of the oxide semiconductor film 211b which functions as the second gate electrode and The length in the channel width direction is the length in the channel length direction and the channel width of the oxide semiconductor film 208. Each of the oxide semiconductor films 208 is longer than the length in each direction, and the entire film is an insulating film 214 and an insulating film. It is covered by an oxide semiconductor film 211b via film 216. Also, as a second gate electrode The oxide semiconductor film 211b that functions and the conductive film 204 that functions as the first gate electrode are , insulating films 206, 207, insulating film 214 and the opening 252a provided in insulating film 216, Since it is connected at 252b, the side surface of the oxide semiconductor film 208 in the channel width direction is an absolute Oxide semiconductor film 2 functions as a second gate electrode via the edge film 214 and insulating film 216. It is opposite 11b.
[0310] In other words, in the channel width direction of transistor 270, as the first gate electrode The functional conductive film 204 and the oxide semiconductor film 211b, which functions as a second gate electrode, Insulators 206, 207 function as the first gate insulating film and as the second gate insulating film The functional insulating film 214 and insulating film 216 are connected at the openings provided therein, and Insulators 206 and 207 function as gate insulating films, and as a second gate insulating film The configuration surrounds the oxide semiconductor film 208 via functional insulating films 214 and 216. .
[0311] With this configuration, the oxide semiconductor film 208 contained in the transistor 270 The conductive film 204 functions as the first gate electrode and the second gate electrode functions The oxide semiconductor film 211b can be electrically enclosed by its electric field. Transistor 270 As shown, a channel region is formed by the electric fields of the first and second gate electrodes. The device structure of a transistor that electrically surrounds the oxide semiconductor film is called surround This can be called a d-channel (s-channel) structure.
[0312] Since transistor 270 has an s-channel structure, the first gate electrode is The conductive film 204 functions to effectively induce an electric field for channel formation in the oxide semiconductor. Because it can be applied to the body membrane 208, the current driving capability of the transistor 270 is improved. This makes it possible to obtain high on-current characteristics. Furthermore, it is possible to increase the on-current. Therefore, it becomes possible to miniaturize transistor 270. Also, transistor 270 , conductive film 204 which functions as the first gate electrode and acid which functions as the second gate electrode Because it has a structure surrounded by a semiconductor film 211b, the mechanical properties of the transistor 270 It can increase strength.
[0313] <Example of transistor configuration 2> Next, regarding a configuration example different from the transistor 270 shown in Figures 34(A), (B), and (C), This will be explained using Figures 35(A), 35(B), 35(C), and 35(D). Figures 35(A) and 35(B) are equivalent to Figure 34(B). Figure 35(C)(D) is a cross-sectional view of a modified example of transistor 270. This is a cross-sectional view of a modified version of transistor 270 shown in Figures 34(B) and 34(C).
[0314] The transistor 270A shown in Figures 35(A) and 35(B) is the same as the transistor shown in Figures 34(B) and 34(C). The oxide semiconductor film 208 of ZISTA 270 has a three-layer stacked structure. More specifically The oxide semiconductor film 208 of transistor 270A is an oxide semiconductor film 208a and It comprises an oxide semiconductor film 208b and an oxide semiconductor film 208c.
[0315] The transistor 270B shown in Figure 35(C)(D) is the same as the transistor shown in Figure 34(B)(C). The oxide semiconductor film 208 of ZISTA 270 has a two-layer stacked structure. More specifically The oxide semiconductor film 208 of transistor 270B is composed of oxide semiconductor film 208b and It has an oxide semiconductor film 208c and
[0316] The configuration of transistors 270, 270A, and 270B shown in this embodiment is as follows: Refer to the configuration of the liquid crystal display device described in 1. That is, the material and manufacturing method of the substrate 202. The method can be found in reference to the substrate 102. The material and method of preparing the conductive film 204 are as follows: gate electrode 104 You can refer to the following. The materials and manufacturing methods of insulating film 206 and insulating film 207 are as follows: insulating film 1 Refer to 06 and insulating film 107. The material and method of preparing the oxide semiconductor film 208 are as follows: The oxide semiconductor film 110 can be referenced. Oxide semiconductor film 211a and oxide semiconductor film 21 The materials and manufacturing method of 1b can be found in reference to the second oxide semiconductor film 111. Conductive film 212a The material and method of preparing the conductive film 212b are as follows: source electrode 112a and drain electrode 212b, respectively. Refer to pole 112b. Materials and fabrication of insulating film 214, insulating film 216 and insulating film 218. The methods can be described by referring to insulating film 114, insulating film 116, and insulating film 118, respectively.
[0317] Here, the band structure of the oxide semiconductor film 208 and the insulating film in contact with the oxide semiconductor film 208 The construction will be explained using Figure 36.
[0318] Figure 36(A) shows insulating film 207, oxide semiconductor films 208a, 208b, 208c, and This is an example of the band structure in the film thickness direction of a multilayer structure having an insulating film 214. Also, Figure 36(B ) has an insulating film 207, oxide semiconductor films 208b, 208c, and insulating film 214. This is an example of a band structure in the film thickness direction of a layered structure. Note that the band structure is shown for ease of understanding. The insulating film 207, oxide semiconductor films 208a, 208b, 208c, and insulating film 214 This shows the energy level (Ec) at the lower end of the guide.
[0319] Furthermore, Figure 36(A) shows that silicon oxide films are used as insulating films 207 and 214, and oxide semi-oxide films are used. The conductive film 208a has a metallic acid with an atomic ratio of metal elements of In:Ga:Zn = 1:1:1.2. Using an oxide semiconductor film formed with an oxide target, the oxide semiconductor film 208b is used. A metal oxide target with an atomic ratio of metal elements of In:Ga:Zn = 4:2:4.1 is used. Using an oxide semiconductor film formed by this process, the number of atoms of the metal element is determined as the oxide semiconductor film 208c. The oxidation formed using a metal oxide target with a ratio of In:Ga:Zn = 1:1:1.2 This is a band diagram of a configuration using a monocrystalline semiconductor film.
[0320] Furthermore, Figure 36(B) shows that silicon oxide films are used as insulating films 207 and 214, and oxide semi-oxide films are used. The conductive film 208b has a metallic acid with an atomic ratio of metal elements of In:Ga:Zn = 4:2:4.1. Using an oxide semiconductor film formed with an oxide target, the oxide semiconductor film 208c is used. A metal oxide target with an atomic ratio of metal elements of In:Ga:Zn = 1:1:1.2 is used. This is a band diagram of a configuration using an oxide semiconductor film formed by [processing].
[0321] As shown in Figures 36(A) and 36(B), the oxide semiconductor films 208a, 208b, and 208c Therefore, the energy levels at the lower end of the conduction band change smoothly. In other words, they change continuously. Alternatively, it can be said that they form a continuous bond. In order to have such a band structure, oxidation The interface between the monocrystalline semiconductor film 208a and the oxide semiconductor film 208b, or the oxide semiconductor film 208b At the interface between the oxide semiconductor film 208c, defect centers such as trap centers and recombination centers Assume that no impurities that would form a position exist.
[0322] To form a continuous junction on oxide semiconductor films 208a, 208b, and 208c, load Each film is deposited using a multi-chamber type film deposition apparatus (sputtering apparatus) equipped with a locking chamber. It is necessary to continuously stack the materials without exposing them to the atmosphere.
[0323] By using the configuration shown in Figures 36(A) and (B), the oxide semiconductor film 208b forms a well. Therefore, in the transistor using the above stacked structure, the channel region is an oxide semiconductor film 2 It can be seen that it is formed in 08b.
[0324] Furthermore, by providing oxide semiconductor films 208a and 208c, the oxide semiconductor film 208 The trap levels that may form on b can be moved away from the oxide semiconductor film 208b.
[0325] Furthermore, the trap level functions as a channel region in the conduction band of oxide semiconductor film 208b. As the energy levels at the edges (Ec) become further from the vacuum level, electrons tend to accumulate in the trap levels. Sometimes the number decreases. Electrons accumulate in the trap level, causing the negative energy to become fixed. This results in an electric charge, and the transistor's threshold voltage shifts to the positive direction. Therefore, , the trap level is more true than the energy level (Ec) of the lower end of the conduction band of the oxide semiconductor film 208b. It is preferable to configure it so that it approaches the empty level. By doing so, the trap level This makes it more difficult for electrons to accumulate, and it is possible to increase the on-current of the transistor. This can increase the field effect mobility.
[0326] Furthermore, oxide semiconductor films 208a and 208c are located below the conduction band than oxide semiconductor film 208b. The edge energy levels are close to the vacuum level, typically in the conduction band of oxide semiconductor film 208b. The energy levels at the edge and the energy levels at the lower edge of the conduction band of the oxide semiconductor films 208a and 208c. The difference from the position is 0.15 eV or more, or 0.5 eV or more and 2 eV or less, or 1 eV The following applies: that is, the electron affinity of the oxide semiconductor films 208a and 208c, and the oxide semiconductor The difference with the electron affinity of the body membrane 208b is 0.15 eV or greater, or 0.5 eV or greater, and 2 It is less than or equal to eV, or less than 1 eV.
[0327] With this configuration, the oxide semiconductor film 208b becomes the main current path. In other words, oxide semiconductor film 208b has the function of a channel region, and oxide semiconductor film 2 08a and 208c function as oxide insulating films. Also, oxide semiconductor film 208 a, 208c are metal elements that constitute the oxide semiconductor film 208b in which the channel region is formed. Since it is an oxide semiconductor film composed of one or more types, the oxide semiconductor film 208a and oxide The interface with the semiconductor film 208b, or the interface between the oxide semiconductor film 208b and the oxide semiconductor film 208c At the interface, interfacial scattering is less likely to occur. Therefore, at the interface, carrier movement is Because it is not inhibited, the field-effect mobility of the transistor increases.
[0328] Furthermore, the oxide semiconductor films 208a and 208c function as part of the channel region. To prevent this, materials with sufficiently low conductivity shall be used. Therefore, oxide semiconductors Films 208a and 208c are also called oxide insulating films, respectively, based on their physical properties and / or functions. It is possible to do so. In addition, the oxide semiconductor films 208a and 208c have electron affinity (vacuum level). The difference between the energy levels of the conduction band and the lower end of the conduction band is smaller than that of the oxide semiconductor film 208b, and the conduction band The lower energy level is the difference between the energy level at the lower end of the conduction band of the oxide semiconductor film 208b and ( A material having a band offset shall be used. Also, depending on the magnitude of the drain voltage In order to suppress the occurrence of a difference in threshold voltage, oxide semiconductor film 208a, 2 The energy level at the lower end of the conduction band of 08c is the same as the energy at the lower end of the conduction band of the oxide semiconductor film 208b. It is preferable to use a material that is closer to the vacuum level than the Ghee level. For example, an oxide semiconductor film 20 Energy levels at the lower end of the conduction band of 8b and the lower end of the conduction band of oxide semiconductor films 208a and 208c The difference from the energy level should be 0.2 eV or more, preferably 0.5 eV or more. It seems so.
[0329] Furthermore, the oxide semiconductor films 208a and 208c do not contain a spinel-type crystal structure within the film. It is preferable that the oxide semiconductor films 208a and 208c contain a spinel-type crystal structure. If included, at the interface between the spinel-type crystal structure and other regions, conductive films 212a, 21 In some cases, the constituent elements of 2b may diffuse into the oxide semiconductor film 208b. When conductive films 208a and 208c are CAAC-OS, the structure of conductive films 212a and 212b The blocking properties of constituent elements, such as copper, become higher, which is preferable.
[0330] The thickness of the oxide semiconductor films 208a and 208c is determined by the constituent elements of the conductive films 212a and 212b. A film thickness greater than or equal to that which can suppress diffusion into the oxide semiconductor film 208b, and provides insulation. The film thickness is set to a level that suppresses the supply of oxygen from film 214 to oxide semiconductor film 208b. For example, If the thickness of the oxide semiconductor films 208a and 208c is 10 nm or more, the conductive film 212a, This can suppress the diffusion of constituent elements of 212b into the oxide semiconductor film 208b. Furthermore, if the thickness of the oxide semiconductor films 208a and 208c is 100 nm or less, the insulating film 214 This allows for an effective supply of oxygen to the oxide semiconductor film 208b.
[0331] Furthermore, in this embodiment, the oxide semiconductor films 208a and 208c are made of metal elements. The atomic ratio was formed using a metal oxide target with In:Ga:Zn = 1:1:1.2. Although examples have been given of configurations using an oxide semiconductor film, the system is not limited to this. For example, acid For the ionized semiconductor films 208a and 208c, the ratio of In:Ga:Zn is 1:1:1 [atomic ratio]. In:Ga:Zn = 1:3:2 [atomic ratio], In:Ga:Zn = 1:3:4 [atomic ratio] ], or using a metal oxide target with an atomic ratio of In:Ga:Zn=1:3:6 The resulting oxide semiconductor film may also be used.
[0332] Furthermore, the oxide semiconductor films 208a and 208c are defined as In:Ga:Zn=1:1:1 [original When using a metal oxide target with a specific [number of particles ratio], the oxide semiconductor films 208a and 208c are as follows: In some cases, In:Ga:Zn = 1:β1 (0 < β1 ≤ 2):β2 (0 < β2 ≤ 3). Furthermore, as oxide semiconductor films 208a and 208c, In:Ga:Zn=1:3:4[original When using a metal oxide target with a specific [number of particles ratio], the oxide semiconductor films 208a and 208c are as follows: In some cases, In:Ga:Zn = 1:β3 (1≦β3≦5):β4 (2≦β4≦6). Furthermore, as oxide semiconductor films 208a and 208c, In:Ga:Zn=1:3:6[original When using a metal oxide target with a specific [number of particles ratio], the oxide semiconductor films 208a and 208c are as follows: In some cases, In:Ga:Zn = 1:β5 (1≦β5≦5):β6 (4≦β6≦8) .
[0333] Furthermore, the oxide semiconductor film 208 of transistor 270 and transistor 270A, The oxide semiconductor film 208c of 270B is shown in the drawing as conductive films 212a and 212 The oxide semiconductor film in the region that does not overlap with b becomes thinner; in other words, a part of the oxide semiconductor film becomes concave. The present invention is illustrated with examples of shapes having a part. However, the present invention is not limited to these examples. The oxide semiconductor film in regions that do not overlap with the films 212a and 212b does not need to have recesses. An example of this case is shown in Figures 37(A) and 37(B). Figures 37(A) and 37(B) show a transistor This is a cross-sectional view showing an example. Note that Figures 37(A) and 37(B) show the transistor 270B shown earlier. The oxide semiconductor film 208 has a structure that does not have recesses.
[0334] Furthermore, as shown in Figures 37(C) and 37(D), the thickness of the oxide semiconductor film 208c is pre-oxidized. It is formed thinner than the monocrystalline semiconductor film 208b, and further, the oxide semiconductor film 208c and insulating film 207 An insulating film 219 may be formed on top. In this case, the insulating film 219 may have an oxide semiconductor film 208 An opening is formed for c to come into contact with conductive film 212a and conductive film 212b. insulating film 219 This can be formed using the same materials and formation methods as the insulating film 214.
[0335] Furthermore, the transistor according to this embodiment can be freely combined with each of the above structures. It is possible to do so.
[0336] The configurations and methods shown in this embodiment can be appropriately combined with the configurations and methods shown in other embodiments. They can be used together.
[0337] (Embodiment 7) In this embodiment, the configuration of a display device according to one aspect of the present invention is shown with reference to Figures 38 to 45. I will explain while shining a light on it.
[0338] <Example of display device configuration 1.> Figure 38 is a top view illustrating the configuration of a display device according to one aspect of the present invention. Figure 39 is also an illustration of the present invention. This is a top view illustrating the pixel configuration of one embodiment of a display device.
[0339] Figure 40 shows the present invention in relation to the cutting lines Z1-Z2, Z3-Z4, and Z5-Z6 shown in Figure 38. This is a cross-sectional view illustrating the configuration of a cross-section of a display device according to one embodiment.
[0340] Figure 41(A) shows the cutting lines Z1-Z2, Z3-Z4, and Z5-Z6 shown in Figure 38. This is a cross-sectional view illustrating the cross-sectional configuration of the first display unit 700E of a display device according to one embodiment of the invention. Figure 41(B) is a cross-sectional view illustrating the structure of a transistor.
[0341] Figure 42 shows the present invention in relation to the cutting lines Z1-Z2, Z3-Z4, and Z5-Z6 shown in Figure 38. This is a cross-sectional view illustrating the cross-sectional configuration of the second display unit 500E of a display device according to one embodiment.
[0342] The display device described in this embodiment has pixels 702E and a substrate 710 (Figure 3). 8. See Figures 39 and 40). Note that sub-pixel 702EB, sub-pixel 702EG, or sub-pixel The 702ER pixel can be used as the 702E pixel.
[0343] The substrate 710 has a function to support the pixel 702E (see Figure 40).
[0344] Pixel 702E is the first display element 750EB and the area overlapping with the first display element 750EB. It comprises a second display element 550EB having a range (see Figures 39 and 40).
[0345] The first display element 750EB has a reflective film (first conductive film 751EB) that reflects ambient light and It also has a function to control the transmission of ambient light. The reflective film (first conductive film 751EB) is located at the opening 7 It is equipped with 51H.
[0346] The second display element 550EB is directed towards the region overlapping with the opening 751H and towards the opening 751H. It has the function of emitting light.
[0347] Furthermore, the first display element 750EB comprises a liquid crystal layer 753, a first conductive film 751EB and the It is equipped with two conductive films 752 (see Figure 41).
[0348] The second display element 550EB consists of a layer 553E containing a luminescent organic compound and a third conductive film 5 It comprises 51EB and a fourth conductive film 552 (see Figure 42).
[0349] The opening 751H is, for example, 5% to 35% of the area of the first conductive film 751EB. The area covered is between 15% and 25%.
[0350] The second display element 550EB emits light into an area that roughly overlaps with the aperture 751H. It is equipped with the function. Furthermore, the area whose shape roughly overlaps with the opening 751H is... It has a region that does not overlap with the region. And the area of the region that does not overlap with the opening 751H is The area of the overlapping region is 20% or less, preferably 10% or less.
[0351] Specifically, the area from which the light of the second display element 550EB is emitted is the area of the aperture 751H. An area of 0.5 times or more but less than 1.5 times, preferably an area of 0.8 times or more but less than 1.2 times, more Preferably, it has an area of 0.9 times or more and less than 1.1 times.
[0352] The above-described display device includes a sub-pixel 702EB and a substrate 710 that supports the sub-pixel 702EB. Furthermore, the sub-pixel 702EB uses a reflective film with an aperture 751H on the first conductive film 751EB. The first display element 750EB (for example, a reflective liquid crystal element) is positioned towards the aperture 751H. It comprises a second display element 550EB (for example, an organic EL element) that emits light, It can be done.
[0353] This allows it to be used as a reflective display device, for example, in environments with strong ambient light. This allows it to function as a self-illuminating display device, for example, in dimly lit environments. As a result, it provides a novel display device with reduced power consumption and superior convenience or reliability. It is possible.
[0354] Furthermore, an insulating film is provided between the two pixel electrodes in adjacent subpixels. Specifically This refers to the first conductive film 751EB on the sub-pixel 702EB and the second conductive film on the sub-pixel 702EG An insulating film 777 is provided between the conductive films 751EG. The first The conductive film 751EB and the first conductive film 751EG are insulated, and in the upper surface shape, The gap between the first conductive film 751EB and the first conductive film 751EG can be eliminated. By using such a configuration, the aperture ratio of the pixels in the first display unit 700E can be increased. Furthermore, by increasing the aperture ratio of the pixels, the contrast of the displayed image by the first display unit 700E is reduced. The stock can be increased, and the displayed image can be made brighter.
[0355] <Structure> A display device according to one aspect of the present invention comprises a first display unit 700E, a second display unit 500E and a connection It has a set layer 535 (see Figures 38 and 40).
[0356] 《First display unit 700E》 The first display unit 700E consists of a pixel unit, a wiring unit, a source driver circuit unit SD1, and a gate driver. It has a circuit section GD1 and a terminal section (see Figures 38 and 41).
[0357] Furthermore, the first display unit 700E consists of a substrate 710, a substrate 770, a structure KB1, and a liquid crystal layer 75 3. It has a sealing material 730 and an optical film 770P.
[0358] Substrate 770 has an area that overlaps with substrate 710.
[0359] The sealing material 730 has the function of bonding the substrates 710 and 770 together.
[0360] The liquid crystal layer 753 is disposed in the region surrounded by the substrate 710, the substrate 770, and the sealing material 730. It will be done.
[0361] Structure KB1 is placed between substrates 710 and 770. It has the function of forming a gap of a fixed distance between substrate 710 and substrate 770.
[0362] Pixel section The pixel section consists of pixel 702E, insulating film 771, insulating film 721A, insulating film 721B and insulating film 7 It is equipped with 28.
[0363] For example, multiple subpixels can be used for pixel 702E. Specifically, blue display Sub-pixel 702EB displays in green, sub-pixel 702EG displays in red 702ER and others can be used. Also, sub-pixels that display in white or yellow can be used. Sub-pixels, etc., can be used.
[0364] For example, make the area of pixels that display blue larger than the area of pixels that display other colors. This allows for a suitable display of white color.
[0365] 《Pixels》 The sub-pixel 702EB comprises the first display element 750EB, a colored film CFB1, and a pixel circuit. ru.
[0366] 《First display element 750EB》 For example, a display element having a function to control the reflection or transmission of light is the first display element 750 It can be used in EB. For example, a configuration combining a liquid crystal element and a polarizing plate or shutter A MEMS display element of the ter type can be used.
[0367] Specifically, IPS (In-Plane-Switching) mode, TN (Twi Sted Nematic) mode, FFS (Fringe Field Switch) ing) mode, ASM(Axially Symmetric aligned Mi cro-cell) mode, OCB (Optically Compensated B irefringence) mode, FLC (Ferroelectric Liqui d Crystal) mode, AFLC (AntiFerroelectric Liq. Liquid crystal elements that can be driven using driving methods such as uid Crystal mode. You can use it.
[0368] Also, for example, vertical orientation (VA) mode, specifically MVA (Multi-Domain) n Vertical Alignment) mode, PVA(Patterned V Using drive methods such as (Certical Alignment) mode and ASV mode A liquid crystal element that can be moved can be used.
[0369] For example, thermotropic liquid crystals, low molecular weight liquid crystals, polymer liquid crystals, polymer dispersed liquid crystals, ferroelectrics Liquid crystals, antiferroelectric liquid crystals, etc. can be used. Depending on the conditions, these liquid crystal materials can be used. Resteric phase, smectic phase, cubic phase, chiral nematic phase, isotropic phase, etc. The liquid crystal material shown can be used. Alternatively, the liquid crystal material showing the blue phase can be used. Cut.
[0370] For example, a liquid crystal layer 753 containing liquid crystal material can have an electric field applied to control the orientation of the liquid crystal material. It comprises a first conductive film 751EB and a second conductive film 752 arranged in a certain manner.
[0371] A conductive material can be used for the first conductive film 751EB.
[0372] For example, the material used in the wiring section is either the first conductive film 751EB or the second conductive film 752. It is possible to be there.
[0373] For example, if the first conductive film 751EB is made of a material that reflects light incident from the liquid crystal layer 753 side, This makes it possible to make the first display element 750EB a reflective liquid crystal element. This is possible. The first conductive film 751EB functions as a pixel electrode.
[0374] Furthermore, for example, a conductive film having irregularities on its surface may be used as the first conductive film 751EB. This allows for the reflection of incident light in various directions, resulting in a white display. .
[0375] For example, a material that is transparent to visible light and also conductive is used as the second conductive film 752 It can be used for this purpose.
[0376] For example, a conductive oxide or a conductive oxide containing indium is used for the second conductive film 752. It is possible to use a metal film thin enough to transmit light as the second conductive film 752. It is possible.
[0377] Specifically, indium oxide, indium tin oxide, indium zinc oxide, zinc oxide For example, zinc oxide with gallium added can be used for the second conductive film 752.
[0378] 《Opening 751H》 The first display unit 700F has an opening 751H in the first conductive film 751EB. Substrate 71 A portion of the light incident from 0 can pass through the aperture 751H and be emitted from the substrate 770. Cut.
[0379] 5% to 35%, preferably 15% to 25%, of the area of the first conductive film 751EB The area of the opening 751H is preferable at the bottom.
[0380] The shape of the opening 751H may be a polygon, square, ellipse, circle, or cross. It is possible.
[0381] 《First colored film》 The first colored film has an area that overlaps with the first display element 750EB and transmits light of a predetermined color. It has the function of [doing something]. The colored film can be used, for example, as a color filter.
[0382] For example, a colored film CFB1 that transmits blue light can be used for the sub-pixel 702EB. A colored film CFG1 that transmits green light can be used for the sub-pixel 702EG. A light-transmitting colored film can be used for the sub-pixel 702ER. Also, a film that transmits white light can be used. A colored film that transmits yellow light or a colored film that transmits yellow light is used as a sub-pixel for displaying various colors. It is possible.
[0383] 《Light blocking film BM》 The light-shielding film BM may be provided, which has an aperture in the region overlapping with the sub-pixel 702EB.
[0384] Materials that obstruct light transmission can be used in the light-shielding film BM. For example, it functions as a black matrix.
[0385] Pixel Circuit A transistor ME1 or a capacitive element C1, etc., can be used in the pixel circuit.
[0386] Transistor ME1 has a semiconductor film 718 and a region overlapping with the semiconductor film 718. It is equipped with a conductive film 704 (see Figure 41(B)). Also, transistor ME1 has a conductive film 712 It comprises A and a conductive film 712B.
[0387] Furthermore, the conductive film 712A has either the function of a source electrode or the function of a drain electrode. The film 712B has the function of either a source electrode or a drain electrode, and the other of the latter. Film 704 functions as a gate electrode, and insulating film 706 functions as a gate insulating film.
[0388] The semiconductor material used for the semiconductor film 718 is not particularly limited; for example, oxide semiconductors, silicon Examples include cellulose and germanium. Furthermore, regarding the crystallinity of semiconductor materials used in transistors... However, it is not particularly limited to amorphous semiconductors, crystalline semiconductors (microcrystalline semiconductors, polycrystalline semiconductors) Any of the following may be used: a solid, a single-crystal semiconductor, or a semiconductor having a crystalline region in part. Using semiconductors with properties is preferable because it can suppress the degradation of transistor characteristics.
[0389] Furthermore, semiconductor materials used in transistors include, for example, elements of Group 14 and compound semiconductors. Conductors or oxide semiconductors can be used as semiconductor layers. Typically, silicon-containing semiconductors... Conductors, semiconductors containing gallium arsenide, or oxide semiconductors containing indium can be applied.
[0390] In particular, applying oxide semiconductors to the semiconductors in which transistor channels are formed is It is preferable. In particular, it is preferable to use oxide semiconductors with a larger band gap than silicon. It seems so. A semiconductor material with a wider band gap and lower carrier density than silicon. Using this method is preferable because it reduces the current when the transistor is off.
[0391] For example, as a transistor using an oxide semiconductor, Embodiment 1 or Embodiment 6 The transistor described below can be used as transistor ME1.
[0392] Capacitive element C1 has a conductive film 712A and a conductive film having a region overlapping with the conductive film 712A. Prepare (see Figure 41(A)).
[0393] Furthermore, the conductive film 712A is electrically connected to the first conductive film 751EB.
[0394] Insulating film The insulating film 771 is disposed between the liquid crystal layer 753 and the colored films CFB1 and CFG1.
[0395] A material that has the function of suppressing the diffusion of impurities from the colored film CFB1, etc., to the liquid crystal layer 753. It can be used as the insulating film 771.
[0396] The insulating film 721B comprises a region that overlaps with the conductive film 704 and a region that overlaps with the semiconductor film 718. El.
[0397] The insulating film 721A is disposed between the semiconductor film 718 and the insulating film 721B (Figure 41) See A) and Figure 41(B).
[0398] 《Insulating Film 728》 The insulating film 728 is disposed between the insulating film 721B and the liquid crystal layer 753.
[0399] The insulating film 728 flattens steps caused by various structures overlapping with the insulating film 728. This makes it possible to make the thickness of the liquid crystal layer 753 uniform.
[0400] For example, insulating inorganic materials, insulating organic materials, or insulating materials including inorganic and organic materials The composite material can be used as the insulating film 728 (see Figure 41(A)).
[0401] Specifically, inorganic oxide films, inorganic nitride films, or inorganic oxynitride films, or derived from these. A laminated material formed by stacking multiple selected materials can be used as the insulating film 728.
[0402] Specifically, polyester, polyolefin, polyamide, polyimide, polycarbonate A combination of resins such as polysiloxane or acrylic resin, or a combination of resins selected from these. Laminated materials or composite materials can be used as the insulating film 728. Furthermore, photosensitive materials are also available. It may be formed using the following materials.
[0403] 《Insulating Film 777》 The insulating film 777 is provided so as to cover the end of one pixel electrode. Specifically, the first conductive It is provided so as to cover the edge of film 751EG (see Figures 39 and 40). Also, the first conductive It is provided so as to cover the end of the film 751ER (see Figure 39).
[0404] Source driver circuit section SD1 For example, an integrated circuit can be used in the source driver circuit section SD1. Specifically, Integrated circuits formed on a recon substrate can be used (see Figure 38).
[0405] For example, using the COG (Chip on glass) method, it is provided on the substrate 710. The source driver circuit section SD1 can be mounted on the pad. Specifically, an anisotropic conductive film is used. This allows integrated circuits to be mounted on the pads. The pads are electrically connected to the pixel circuits.
[0406] Gate driver circuit section GD1 For example, transistor ME2 can be used in the gate driver circuit GD1 (Figure 4). See 1(A) and Figure 41(B).
[0407] For example, the transistor described in Embodiment 1 or Embodiment 6 is the transistor ME It can be used in 2.
[0408] For example, it can be formed using the same process as the semiconductor film 718 on transistor ME1. A semiconductor film that can be used can be used in transistor ME2.
[0409] Furthermore, the same configuration as transistor ME1 can be used for transistor ME2. Furthermore, different configurations can be used for transistor ME2.
[0410] Conductive film 720 The conductive film 720 has a region that overlaps with the semiconductor film 718. In other words, the semiconductor film 718 This is placed between the conductive film 720 and the conductive film 704. This allows the transistor ME1 to Alternatively, the characteristics or reliability of transistor ME2 can be improved.
[0411] The conductive film 720 can be used as the second gate electrode of the transistor ME2. 720 can also be considered part of transistor ME1 or transistor ME2.
[0412] For example, a wiring that can supply the same potential as conductive film 704 and conductive film 720 electrically It can connect to
[0413] For example, the material used in the wiring section can be used for the conductive film 720. Specifically, conductive Conductive oxides containing indium, indium oxide, indium tin oxide, Indium zinc oxide, indium zinc gallium oxide, zinc oxide, gallium added Zinc oxide and the like can be used in the conductive film 720.
[0414] 《Wiring section, terminal section》 The wiring section includes a signal line 711. The terminal section also includes a connecting electrode 719 (Figure 41(A)). reference).
[0415] The signal line 711 is electrically connected to the connecting electrode 719. Also, a portion of the signal line 711 It can be used for the connecting electrode 719.
[0416] The connecting electrode 719 is connected to a flexible printed circuit board FP using, for example, a conductive member ACF1. It is electrically connected to C1.
[0417] Conductive materials can be used for the signal line 711 and the connecting electrode 719.
[0418] For example, inorganic conductive materials, organic conductive materials, metals, or conductive ceramics can be used to signal This can be a wire 711 or a connecting electrode 719.
[0419] Specifically, aluminum, gold, platinum, silver, copper, chromium, tantalum, titanium, molybdenum Gold selected from tungsten, nickel, iron, cobalt, palladium, or manganese. The group elements, etc., can be used in the signal line 711 or the connecting electrode 719. Alternatively, as described above. Alloys containing the aforementioned metal elements can be used for the signal line 711 or the connecting electrode 719. In particular, copper-manganese alloys are suitable for microfabrication using the wet etching method.
[0420] Specifically, a two-layer structure in which a titanium film is laminated on an aluminum film, and a titanium film on a titanium nitride film A two-layer structure in which a tungsten film is stacked on top of a titanium nitride film, a two-layer structure in which a tungsten film is stacked on top of a titanium nitride film, A two-layer structure in which a tungsten film is laminated on a tungsten film or a tungsten nitride film, and a titanium film and A three-layer structure is formed by laminating an aluminum film on top of the titanium film, and then forming another titanium film on top of that. The structure can be used for the signal line 711 or the connecting electrode 719.
[0421] Specifically, indium oxide, indium tin oxide, indium zinc oxide, zinc oxide A conductive oxide such as zinc oxide doped with gallium is used in the signal line 711 or connecting electrode 71 It can be used in 9.
[0422] Specifically, a film containing graphene or graphite is connected to the signal line 711 or the connecting electrode 7 It can be used in 19.
[0423] For example, by forming a film containing graphene oxide and reducing the film containing graphene oxide... This allows for the formation of a graphene-containing film. The reduction method involves applying heat. Examples include methods using reducing agents.
[0424] Specifically, conductive polymers can be used in the signal line 711 or the connecting electrode 719. .
[0425] Conductive material ACF1 For example, solder, conductive paste, or anisotropic conductive film may be used in the conductive member ACF1. It is possible.
[0426] Specifically, conductive particles and materials for dispersing the particles are used in the conductive member ACF1. It is possible.
[0427] For example, spheres with a size of 1 μm to 200 μm, preferably 3 μm to 150 μm. Particles having shapes such as cylindrical, columnar, or filler-like can be used.
[0428] For example, particles coated with a conductive material containing nickel or gold can be used. ru.
[0429] Specifically, particles containing polystyrene, acrylic resin, or titanium dioxide are used. It is possible.
[0430] For example, synthetic rubber, thermosetting resins, thermoplastic resins, etc., can be used as materials for dispersing particles. It is possible.
[0431] This allows the flexible printed circuit board FPC1 and the connecting electrode 719 to be electrically connected using particles. It can be connected to a target.
[0432] Circuit board 710 A translucent material can be used for the substrate 710. Furthermore, the thickness can be reduced using a polishing method. The modified material can be used for the substrate 710.
[0433] For example, a laminated material consisting of a base material 710A and an insulating film 710B is used as the substrate 710. 0B has the function of suppressing the diffusion of impurities contained in the substrate 710A or impurities from the outside. Prepare.
[0434] The substrate 710 is made of a material that has sufficient heat resistance to withstand the heat treatment during the manufacturing process. can.
[0435] For example, the 6th generation (1500mm x 1850mm), the 7th generation (1870mm x 220 0mm), 8th generation (2200mm x 2400mm), 9th generation (2400mm x 280 Based on large glass substrates such as 0mm, 10th generation (2950mm x 3400mm), etc. It can be used on plate 710. This makes it possible to manufacture large display devices.
[0436] The substrate 710 is made of organic materials, inorganic materials, or composite materials such as organic and inorganic materials. This is possible. For example, inorganic materials such as glass, ceramics, and metals can be used for the substrate 710. It is possible.
[0437] Specifically, alkali-free glass, soda-lime glass, potash glass, crystal glass, Quartz or sapphire can be used as the substrate 710. Specifically, inorganic oxides A film, an inorganic nitride film, or an inorganic oxynitride film can be used on the substrate 710. For example, , silicon oxide, silicon nitride, silicon oxide nitride, aluminum oxide, etc., on substrate 710 It can be used for this purpose. SUS or aluminum, etc., can be used for the substrate 710. ru.
[0438] For example, single-crystal semiconductor substrates made of silicon or silicon carbide, polycrystalline semiconductor substrates, silicon Compound semiconductor substrates such as congermanium, SOI substrates, etc. can be used for substrate 710. This allows semiconductor elements to be formed on the substrate 710.
[0439] For example, using organic materials such as resin, resin film, or plastic for the substrate 710. This can be done. Specifically, polyester, polyolefin, polyamide, polyimide, A resin film or resin plate such as carbonate or acrylic resin is used for the substrate 710. It is possible.
[0440] For example, a film of metal, thin glass, or inorganic material is laminated to a resin film, etc. The composite material can be used as the substrate 710. For example, fibrous or particulate metal, A composite material in which glass or inorganic materials are dispersed in a resin film is used as the substrate 710. This can be done. For example, by dispersing fibrous or particulate resin or organic material, etc., in an inorganic material. The composite material can be used in the substrate 710.
[0441] Furthermore, a single-layer material or a material with multiple layers can be used for the substrate 710. For example, a material in which a substrate and an insulating film that prevents the diffusion of impurities contained in the substrate are laminated together, It can be used in plate 710. Specifically, the diffusion of glass and impurities contained in the glass One or the following are selected from the silicon oxide layer, silicon nitride layer, or silicon oxidoxide-nitride layer to prevent the formation of a silicon oxide layer or A material in which multiple films are laminated can be used as the substrate 710. Alternatively, resin and resin can be used. A silicon oxide film, silicon nitride film, or silicon oxynitride film that prevents the diffusion of permeating impurities. Materials with such layers can be used for the substrate 710.
[0442] Specifically, polyester, polyolefin, polyamide, polyimide, polycarbonate A resin film, resin plate, or laminate such as acrylic resin is used for the substrate 710. It is possible.
[0443] Specifically, polyester, polyolefin, polyamide (nylon, aramid, etc.), Polyimide, polycarbonate, polyurethane, acrylic resin, epoxy resin or s A material containing a resin having roxane bonds can be used for the substrate 710.
[0444] Specifically, polyethylene terephthalate (PET), polyethylene naphthalate (P The substrate 710 must be made of EN, polyethersulfone (PES), or acrylic, etc. It is possible.
[0445] Furthermore, paper or wood can be used for the substrate 710.
[0446] For example, a flexible substrate can be used for the substrate 710.
[0447] Furthermore, a method is used in which transistors or capacitive elements are directly formed on a flexible substrate. It is possible to place transistors or capacitive elements on a heat-resistant substrate for the process. A method for forming and transposing a transistor or capacitive element, etc., formed on a flexible substrate. You can use it.
[0448] Circuit board 770 A translucent material can be used for the substrate 770.
[0449] For example, a material that can be used for substrate 710 can be used for substrate 770.
[0450] 《Sealant 730》 Inorganic materials, organic materials, or composite materials of inorganic and organic materials are used in the sealing material 730. It is possible.
[0451] For example, an organic material such as a heat-meltable resin or a curable resin may be used for the sealing material 730. It is possible.
[0452] For example, reaction-curing adhesives, photocuring adhesives, thermosetting adhesives, or / or anaerobic adhesives. Organic materials such as adhesives can be used in the sealant 730.
[0453] Specifically, epoxy resin, acrylic resin, silicone resin, phenolic resin, poly Mido resin, imide resin, PVC (polyvinyl chloride) resin, PVB (polyvinyl butyl Adhesives containing resins such as LA (Lar) resin and EVA (ethylene vinyl acetate) resin are used as sealants 730 It can be used for this purpose.
[0454] Optical film 770P The substrate 770 is sandwiched between the optical film and the liquid crystal layer 753. The optical film 770P is It includes an area that overlaps with the first display element 750EB.
[0455] For example, polarizing plates, phase difference plates, diffusion films, or light-gathering films are used with optical film 770. It can be used for P.
[0456] Furthermore, a hard coat layer to prevent scratches can be used on the optical film.
[0457] 《Second display unit 500E》 The second display unit 500E consists of a pixel unit, a wiring unit, a source driver circuit unit SD2, and a gate driver. It has a circuit section GD2 or a terminal section (see Figures 38 and 42).
[0458] Furthermore, the second display unit 500E consists of a substrate 510, an insulating film 570, a structure KB2, or a bonding layer. It has 530.
[0459] Furthermore, it has a colored film or insulating film 571.
[0460] Furthermore, it comprises insulating film 521A, insulating film 521B, and partition wall 528A or insulating film 528B. .
[0461] The insulating film 570 has a region that overlaps with the substrate 510.
[0462] The bonding layer 530 has the function of bonding the substrate 510 and the insulating film 570.
[0463] Structure KB2 is disposed between the substrate 510 and the insulating film 570. Structure KB2 is It has the function of forming a gap of a predetermined distance between the substrate 510 and the insulating film 570.
[0464] Pixel section The pixel section comprises pixels.
[0465] For example, multiple subpixels can be used for a single pixel. Specifically, a subpixel that displays blue can be used for a single pixel. Pixels, sub-pixels that display in green, sub-pixels that display in red, etc., can be used. Sub-pixels that display in white or sub-pixels that display in yellow can be used.
[0466] For example, make the area of pixels that display blue larger than the area of pixels that display other colors. This allows for a suitable display of white color.
[0467] 《Pixels》 Each pixel comprises a second display element 550EB, a colored film CFB2, and a pixel circuit.
[0468] 《Second display element 550EB》 The second display element 550EB is directed towards the region overlapping with the opening 751H and towards the opening 751H. It has the function of emitting light.
[0469] The second display element 550EB has a light-emitting region that roughly overlaps with the aperture 751H. Prepare the area (see Figure 39).
[0470] Various light-emitting elements can be used for the second display element 550EB. For example, organic Electroluminescent element, inorganic electroluminescent element, or light-emitting diode The dots and other elements can be used in the second display element 550EB.
[0471] For example, a third conductive film 551EB and a fourth conductive film having a region that overlaps with the third conductive film. 552 and the luminescent material placed between the third conductive film 551EB and the fourth conductive film 552 The layer 553E containing an organic compound can be used in the second display element 550EB. (See Figure 42)
[0472] For example, a laminate that is stacked to emit white light, with a layer containing a luminescent organic compound. It can be used in 553E. Specifically, it includes a luminescent material that emits blue light. A layer containing organic compounds and materials other than fluorescent materials that emit green and / or red light. A laminate formed by stacking the layer containing the luminescent organic compound can be used in layer 553E. Cut.
[0473] For example, if the material used in the wiring section is the third conductive film 551EB or the fourth conductive film 552 It is possible to be there.
[0474] For example, a material that is reflective to visible light and also conductive is used as the third conductive film 551 It can be used in EB.
[0475] For example, a material that is transparent to visible light and also conductive is used as the fourth conductive film 552 It can be used for this purpose.
[0476] Specifically, conductive oxides or conductive oxides containing indium, indium oxide, Indium tin oxide, indium zinc oxide, zinc oxide, zinc oxide with added gallium, etc. This can be used for the fourth conductive film 552.
[0477] Alternatively, a thin metal film that allows light to pass through can be used as the fourth conductive film 552.
[0478] 《The second colored film》 The second colored film covers the opening 751H of the first conductive film 751EB and the second display element 550 It is placed between EBs.
[0479] The second colored film includes an area that overlaps with the opening 751H and the second display element 550EB. It has the function of transmitting light of a predetermined color. For example, it transmits light that passes through the colored film CFB1. This allows the colored film to be used as the colored film CFB2. A portion of the light emitted by B is transmitted through the colored film CFB2, aperture 751H, and colored film CFB1. It can then be removed from the display device.
[0480] For example, a material that can be used for colored film CFB1 can be used for colored film CFB2. Cut.
[0481] Pixel Circuit Transistors such as ME3 can be used in pixel circuits.
[0482] For example, a configuration that can be used for transistor ME1 can be used for transistor ME3. It is possible.
[0483] For example, the transistor described in Embodiment 1 or Embodiment 6 is the transistor ME It can be used in 3.
[0484] Insulating film An insulating film 571 is provided between the colored film CFB2 and the bonding layer 530.
[0485] The insulating film 521B includes regions that overlap with the conductive film 504 and regions that overlap with the semiconductor film.
[0486] The insulating film 521A is placed between the semiconductor film and the insulating film 521B (see Figure 42).
[0487] 《Insulating film 528B》 The insulating film 528B flattens steps caused by various structures overlapping with the insulating film 528B. It is possible.
[0488] For example, a material that can be used for insulating film 728 can be used for insulating film 528B. ru.
[0489] 《Bulkhead 528A》 The partition wall 528A has an opening in the region that overlaps with the second display element 550EB. For example, A material with edge properties can be used for the partition wall 528A. This allows the second display element 5 50EB can be isolated from other adjacent components. Alternatively, it can be installed in partition wall 528A. The shape of the second display element can be determined using the shape of the opening.
[0490] For example, a material that can be used for insulating film 528B can be used for partition wall 528A. ru.
[0491] Source driver circuit section SD2 For example, an integrated circuit can be used in the source driver circuit section SD2. Specifically, Integrated circuits formed on a recon substrate can be used (see Figure 38).
[0492] For example, using the COG (Chip on glass) method, a substrate 510 is provided The source driver circuit section SD2 can be mounted on the pad. Specifically, using an anisotropic conductive film The pads can be used to mount integrated circuits. The pads are electrically connected to the pixel circuits.
[0493] 《Gate driver circuit section GD2》 For example, transistor ME4 can be used in the gate driver circuit GD2 (Figure 4). (See 2).
[0494] For example, the transistor described in Embodiment 1 or Embodiment 6 is the transistor ME It can be used in 4.
[0495] For example, a semiconductor film that can be formed using the same process as the semiconductor film of transistor ME3 The conductive film can be used in transistor ME4.
[0496] Furthermore, the same configuration as transistor ME3 can be used for transistor ME4. Furthermore, different configurations can be used for the ME4 transistor.
[0497] Conductive film 520 The conductive film 520 has a region that overlaps with the semiconductor film. In other words, the semiconductor film overlaps with the conductive film 52. It is placed between 0 and the conductive film 504. This allows the transistor ME3 or the transistor This can improve the reliability of the STAME4.
[0498] The conductive film 520 can be used as the second gate electrode of the transistor ME4. 520 can also be considered part of transistor ME3 or transistor ME4.
[0499] For example, a wiring that can supply the same potential as conductive film 504 and conductive film 520 electrically It can connect to
[0500] For example, the material used in the wiring section can be used for the conductive film 520. Specifically, conductive Conductive oxides containing indium, indium oxide, indium tin oxide, Indium zinc oxide, indium zinc gallium oxide, zinc oxide, gallium added Zinc oxide and the like can be used in the conductive film 520.
[0501] 《Wiring section, terminal section》 The wiring section includes signal lines. The terminal section also includes connecting electrodes 519 (see Figure 42).
[0502] The signal line is electrically connected to the connecting electrode 519. Additionally, a portion of the signal line is connected to the connecting electrode 519. It can be used in 9.
[0503] The connecting electrode 519 is connected to a flexible printed circuit board FP using, for example, a conductive member ACF2. It is electrically connected to C2.
[0504] Materials that can be used for the signal line 711 or connecting electrode 719 are used for the signal line or connecting electrode It can be used in pole 519.
[0505] Conductive material ACF2 Materials that can be used in conductive member ACF1 can also be used in conductive member ACF2. .
[0506] Circuit board 510 The substrate 510 can be made of a material that has sufficient heat resistance to withstand the heat treatment during the manufacturing process. Cut.
[0507] For example, a laminated material consisting of a base material 510A and an insulating film 510B is used as the substrate 510. 0B has the function of suppressing the diffusion of impurities contained in the substrate 510A or impurities from the outside. Prepare.
[0508] For example, a material that can be used for substrate 710 can be used for substrate 510. Oh, a light-shielding material can also be used for the substrate 510.
[0509] 《Insulating film 570》 For example, a single-layer material or a material with multiple layers can be used as the insulating film 570. For example, a material with a laminated insulating film to prevent the diffusion of impurities can be used as the insulating film 570. This is possible. Specifically, a silicon oxide layer that prevents the diffusion of impurities that permeate the resin and other materials. One or more films selected from silicon nitride layers or silicon oxidizide layers are laminated. The material can be used in the insulating film 570.
[0510] 《Joining layer 530》 Inorganic materials, organic materials, or composite materials of inorganic and organic materials are used in the bonding layer 530. It is possible.
[0511] For example, a material that can be used for the sealing material 730 can be used for the bonding layer 530. ru.
[0512] 《Adhesive layer 535》 Inorganic materials, organic materials, or composite materials of inorganic and organic materials are used in the adhesive layer 535. It is possible.
[0513] For example, a material that can be used in the bonding layer 530 can be used in the adhesive layer 535. .
[0514] <Example of display device configuration 2.> Another configuration of a display device according to one aspect of the present invention is shown in Figures 38, 39, or 43 to 44. I will explain this while referring to item 5.
[0515] Figure 43 shows the present invention in relation to the cutting lines Z1-Z2, Z3-Z4, and Z5-Z6 shown in Figure 38. This is a cross-sectional view illustrating the configuration of a cross-section of a display device according to one embodiment.
[0516] Figure 44(A) shows the cutting lines Z1-Z2, Z3-Z4, and Z5-Z6 shown in Figure 38. This is a cross-sectional view illustrating the cross-sectional configuration of the first display unit 700F of a display device according to one embodiment of the invention. Figure 44(B) is a cross-sectional view illustrating the structure of a transistor.
[0517] Figure 45 shows the present invention in relation to the cutting lines Z1-Z2, Z3-Z4, and Z5-Z6 shown in Figure 38. This is a cross-sectional view illustrating the cross-sectional configuration of the second display unit 500F of a display device according to one embodiment.
[0518] This section provides a detailed explanation of a configuration that differs from the display device described above, and also describes a similar configuration. Where applicable, refer to the explanation above.
[0519] 《First display unit 700F》 The first display unit 700F is provided with a flat first conductive film 751FB, and the optical film The features include the inclusion of the 770PF and the fact that the structure KB1 is provided on the substrate 770, top The fact that it includes the rifling transistors MF1 and MF2 is as shown in Figure 41. This differs from the first display unit 700E, which will be explained next.
[0520] For example, a polarizing plate containing a dichroic dye can be used in the optical film 770PF.
[0521] 《Second display unit 500F》 In the second display unit 500F, the colored film CFB2 is not provided, and the color is blue, green or red. It is equipped with a second display element 550FB that emits light of color, etc., and a top gate type transistor The second point, which will be explained with reference to Figure 42, is that it includes transistor MF1 and transistor MF2. The display unit is different from the 500E.
[0522] A second display element 550 that emits a different color from the second display element located in other subpixels. FB is used as a sub-pixel. For example, a second display element 550FB that emits blue light is used. A second display element is used for one sub-pixel and emits green or red light to the other sub-pixels. .
[0523] Specifically, the second layer comprises a layer 553F containing a luminescent organic compound that emits blue light. The display element is used as one of the sub-pixels. It also contains a light-emitting organic compound that emits green light. A second display element comprising a layer or a layer containing a luminescent organic compound that emits red light, It is used as a sub-pixel.
[0524] Furthermore, a vapor deposition method using a shadow mask is used to form a layer containing a luminescent organic compound. Alternatively, an inkjet method can be used. This allows the second subpixels to be placed in other subpixels. A second display element 550FB that emits a different color from the first display element is used as a sub-pixel. It is possible.
[0525] Transistor MF1 Transistor MF1 has a conductive film 704 that overlaps with insulating film 710B, and insulating film 7 The device comprises a semiconductor film 718 having a region disposed between 10B and the conductive film 704. Furthermore, the conductive film 704 also functions as a gate electrode (Figure 44(B)).
[0526] The semiconductor film 718 has a first region 718A and a second region 7 that do not overlap with the conductive film 704. 18B and the conductive film 704 overlapping between the first region 718A and the second region 718B It has three regions 718C.
[0527] Transistor MF1 has an insulating film 706 between the third region 718C and the conductive film 704. It is equipped with a gate insulating film.
[0528] The first region 718A and the second region 718B have lower resistance compared to the third region 718C. It is transformed and possesses the functionality of either the source area or the drain area.
[0529] For example, the method for controlling the resistivity of the oxide semiconductor film, as described later, is the first method of the semiconductor film 718. It can be used in a method for forming region 718A and a second region 718B. Specifically Plasma treatment using gases containing noble gases can be applied to this. For example, conductive film 7 When 04 is used as a mask, a part of the shape of the third region 718C is the shape of the edge of the conductive film 704. It can be self-consistent.
[0530] Transistor MF1 has a conductive film 712A in contact with the first region 718A, and a second region 7 It comprises a conductive film 712B in contact with 18B. The conductive film 712A and conductive film 712B are It functions as either a source electrode or a drain electrode.
[0531] A transistor that can be formed using the same process as transistor MF1 is used for transistor MF2. It is possible to be there.
[0532] <Method for controlling the resistivity of oxide semiconductor films> This section describes a method for controlling the resistivity of oxide semiconductor films.
[0533] An oxide semiconductor film having a predetermined resistivity is provided as the conductive film 720, the first region 718A or the It can be used in region 718B of 2. A method for controlling the resistivity of an oxide semiconductor film is practical You can refer to the method for controlling the resistivity of the second oxide semiconductor film 111 described in Embodiment 1.
[0534] Furthermore, the oxidation film has a higher hydrogen concentration and / or oxygen vacancy than semiconductor film 718, and has lower resistivity. A monocrystalline semiconductor film is used for the conductive film 720.
[0535] Furthermore, the hydrogen concentration in the conductive film 720 is twice that of the hydrogen concentration in the semiconductor film 718. Preferably, the ratio is 10 times or more.
[0536] Furthermore, the resistivity of the conductive film 720 is 1 × 10⁻⁶ of the resistivity of the semiconductor film 718. -8 more than 1×1 0 -1 It is less than double.
[0537] Specifically, the resistivity of conductive film 720 is 1 × 10⁻⁶. -3 Ωcm or more, 1 × 10 4 Less than Ωcm Preferably, 1 × 10 -3 Ωcm or more, 1 × 10 -1 It is less than Ωcm.
[0538] This embodiment can be appropriately combined with other embodiments shown herein. ru.
[0539] (Embodiment 8) In this embodiment, an electronic device having a liquid crystal display device according to one aspect of the present invention is shown in Figure 46. This will be explained using Figure 47.
[0540] The display module 8000 shown in Figure 46 consists of an upper cover 8001 and a lower cover 8002. In between, the touch panel 8004 connected to the FPC8003 and the FPC8005 are connected. The display panel 8006, frame 8009, printed circuit board 8010, and battery 8011 To possess.
[0541] A display device according to one aspect of the present invention can be used, for example, as a display panel 8006.
[0542] The upper cover 8001 and the lower cover 8002 are the touch panel 8004 and the display panel. The shape and dimensions can be appropriately modified to match the size of the 8006.
[0543] The touch panel 8004 is a display panel using either a resistive or capacitive touch panel. It can be used superimposed on 8006. Also, the opposing substrate (sealing substrate) of the display panel 8006 It is also possible to give the board a touch panel function. It is also possible to install a light sensor in each pixel of 006 to create an optical touch panel.
[0544] Frame 8009 provides protection for the display panel 8006, as well as the movement of the printed circuit board 8010. It has the function of an electromagnetic shield to block electromagnetic waves generated by the operation. The 8009 may also function as a heat sink.
[0545] The printed circuit board 8010 contains power supply circuits and signals for outputting video and clock signals. It has a power processing circuit. The power supply that provides power to the power supply circuit is an external commercial power supply. Alternatively, a separate power source, the battery 8011, may also be used. This can be omitted when using commercial power.
[0546] Furthermore, the display module 8000 includes components such as polarizing plates, phase difference plates, and prism sheets. They may also be provided.
[0547] Figures 47(A) through 47(H) show electronic devices. These electronic devices are enclosed in a casing. Body 5000, display unit 5001, speaker 5003, LED lamp 5004, operation keys 50 05 (including power switch or operation switch), connection terminal 5006, sensor 5007 ( Force, displacement, position, velocity, acceleration, angular velocity, rotational speed, distance, light, liquid, magnetism, temperature, chemical substances , sound, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration, odor It may have a microphone 5008 (or a device that includes a function to measure infrared rays), etc. can.
[0548] Figure 47(A) shows a mobile computer, and in addition to the above, it has a switch 5009 It may have an infrared port 5010, etc. Figure 47(B) shows a portable recording device. A strip-type image playback device (for example, a DVD player), and in addition to those mentioned above, see Table 2. It may have a display unit 5002, a recording medium reading unit 5011, etc. Figure 47(C) is a Go It is a group-type display, and in addition to the above, it includes a second display unit 5002 and a support unit 5012 It can have earphones 5013, etc. Figure 47(D) is a portable gaming machine, and above In addition to those described above, it may also have a recording medium reading unit 5011, etc. Figure 47(E) It is a digital camera with a television receiving function, and in addition to the above, it has an antenna 5014, It may have a shutter button 5015, an image receiving unit 5016, etc. Figure 47(F) is a portable It is a band-type gaming machine, and in addition to the above, it also has a second display unit 5002 and a recording medium reading unit 5011. , etc. Figure 47(G) is a portable television receiver, and the above-mentioned In addition, it may have a charger 5017 capable of transmitting and receiving signals, etc. Figure 47(H ) is a wristwatch-type information terminal, and in addition to the above, it includes band 5018, clasp 5019 It has, etc. The display unit 5001 mounted on the housing 5000 which also serves as the bezel is non-rectangular. It has a shaped display area. The display unit 5001 has an icon 5305 that represents the time, and other Icon 5306 and others can be displayed.
[0549] The electronic devices shown in Figures 47(A) to 47(H) can have a variety of functions. For example, a function that displays various information (still images, videos, text images, etc.) on the display unit, Panel functions, calendar, date or time display functions, various software ( A function that controls processing by program, wireless communication function, and various functions using wireless communication function. Functions to connect to computer networks, and to transmit various data using wireless communication functions or The function of receiving data, reading programs or data recorded on the recording medium and displaying them on the display unit. It can have a display function, etc. Furthermore, in electronic devices having multiple display units In this system, one display unit primarily displays image information, and another display unit primarily displays text information. A function to display a three-dimensional image by displaying images that take parallax into account on multiple display units. It can have functions such as displaying an image. Furthermore, in electronic equipment having an image receiving unit... It has functions for taking still images, recording videos, and automatically or manually correcting the captured images. Functions to take pictures, functions to save the captured images to a recording medium (external or built into the camera), and the captured images It can have a function to display an image on the display unit, etc. Note that Figures 47(A) to 47( The functions that electronic devices shown in H) may have are not limited to these, and may have a variety of functions. It is possible.
[0550] The electronic device of this embodiment is characterized by having a display unit for displaying some kind of information. A liquid crystal display device according to one aspect of the present invention can be applied to the display unit.
[0551] The configuration shown in this embodiment may be used in appropriate combination with the configurations shown in other embodiments. It is possible. [Examples]
[0552] In this embodiment, a liquid crystal display device according to one aspect of the present invention was fabricated and the display was verified. Let me explain. The cross-sectional configuration of pixels 70R and 70G of the liquid crystal display device corresponds to Figure 21, and The cross-sectional configuration of component 70B corresponds to Figure 22.
[0553] First, Table 1 shows the specifications of the liquid crystal display device manufactured in this embodiment.
[0554] [Table 1]
[0555] The liquid crystal display device fabricated in this embodiment is an active matrix reflective liquid crystal display device, color This is a display, and CAAC-IGZO was used for the FET on the backplane side. The manufactured liquid crystal display device has a reflectivity of 25.1% and an NTSC ratio of 37%.
[0556] An example of the display of the liquid crystal display device is shown in Figure 48. From Figure 48, a liquid crystal display device according to one aspect of the present invention is shown. This allows for high-contrast display while maintaining a high aperture ratio.
[0557] The configuration shown in this embodiment can be used in appropriate combination with the configurations shown in other embodiments. Cut. [Explanation of Symbols]
[0558] 50 transistors 50B transistor 50G Transistor 50R Transistor 51 Liquid crystal elements 51B Liquid Crystal Element 55 Capacitive elements 70 pixels 70B pixels 70G pixels 70R pixels 71 pixel section 74 Scan line drive circuit 75 Capacitance wiring 76 Signal Line Drive Circuit 77 scan lines 79 Signal Line 79B signal line 79G signal line 79R signal line 80 LCD display device 102 circuit boards 104 Guard gate 106 Insulating film 107 Insulating Film 108 Insulating Film 110 Oxide semiconductor film 110a Oxide semiconductor film 111 Oxide semiconductor film 111a Oxide semiconductor film 112a Source electrode 112b Drain electrode 114 Insulating Film 116 Insulating film 118 Insulating Film 119 Insulating film 120 Conductive film 120a conductive film 120b Conductive film 121 Conductive film 122 Conductive film 130 insulating film 141 Aperture 142 Aperture 143 Aperture 150 transistors 151 transistors 160 Capacitive elements 170 Colored film 171 Colored film 193 Target 194 Plasma 202 circuit boards 204 Conductive film 206 Insulating film 207 Insulating film 208 Oxide Semiconductor Film 208a Oxide Semiconductor Film 208b oxide semiconductor film 208c oxide semiconductor film 211a Oxide semiconductor film 211b Oxide semiconductor film 212a Conductive film 212b Conductive film 214 Insulating film 216 Insulating film 218 Insulating film 219 Insulating film 220b Conductive film 252a opening 252b opening 252c opening 270 transistors 270A Transistor 270B transistor 302 circuit board 303 circuit board 311a Oxide semiconductor film 311B Oxide Semiconductor Film 311G Oxide Semiconductor Film 311R Oxide Semiconductor Film 314 Insulating Film 316 Insulating film 318 Insulating film 319 Insulating film 320B Pixel Electrode 320G pixel electrode 320R pixel electrode 325B Conductive film 325G conductive film 325R conductive film 330 insulating film 330a insulating film 330b insulating film 330B insulating film 330G insulating film 330R insulating film 333 Structure 335 Orientation film 336 Orientation film 337 Overcoat film 340B Colored film 340G colored film 340R colored film 341 Liquid crystal layer 344 Insulating Film 345 Common Electrode 500E display 500F display section 504 Conductive film 510 circuit board 510A base material 510B insulating film 519 Connecting electrodes 520 Conductive film 521A Insulating Film 521B Insulating Film 528A Bulkhead 528B insulating film 530 Bonding layer 535 Adhesive layer 550EB display element 550FB display element 551EB Conductive film 552 Conductive film 553E layer 553F layer 570 Insulating film 571 Insulating film 700E display 700F display section 702E pixels 702EB subpixels 702EG sub-pixel 702ER sub-pixel 704 Conductive film 706 Insulating film 710 circuit board 710A base material 710B insulating film 711 signal line 712A Conductive film 712B Conductive film 718 Semiconductor film 718A area 718B area 718C area 719 Connecting electrodes 720 Conductive film 721A Insulating Film 721B insulating film 728 Insulating film 730 Sealant 750EB display element 751EB Conductive film 751EG conductive film 751ER conductive film 751FB conductive film 751H opening 752 Conductive film 753 Liquid crystal layer 770 circuit boards 770P Optical Film 770 PHIO Optical Film 771 Insulating Film 777 Insulator 5000 cabinets 5001 Display section 5002 Display section 5003 Speaker 5004 LED Lamp 5005 Operation Keys 5006 Connection terminal 5007 Sensor 5008 Microphone 5009 Switch 5010 Infrared Port 5011 Recording medium reading unit 5012 Support part 5013 Earphones 5014 Antenna 5015 Shutter button 5016 Image receiving unit 5017 charger 5018 Band 5019 Clasp 5100 pellets 5120 circuit board 5161 area 5200 pellets 5201 Aeon 5202 Lateral growth part 5203 particles 5220 circuit board 5230 Target 5240 Plasma 5260 Heating mechanism 5305 Icons 5306 Icons 8000 Display Module 8001 Top cover 8002 Lower cover 8003 FPC 8004 Touch Panel 8005 FPC 8006 Display Panel 8009 Frame 8010 Printed Circuit Board 8011 Battery
Claims
1. A first pixel having a transistor, a capacitive element, and a first pixel electrode, A second pixel adjacent to the first pixel and having a second pixel electrode, The first pixel is, A first oxide semiconductor film having a channel formation region of the transistor, A first insulating film having a region in contact with the upper surface of the first oxide semiconductor film, A first conductive layer having a region in contact with the upper surface of the first insulating film and a region in contact with the upper surface of the first oxide semiconductor film, A second conductive layer having a region in contact with the upper surface of the first insulating film and a region in contact with the upper surface of the first oxide semiconductor film, A second oxide semiconductor film having a region that functions as one electrode of the capacitive element, A second insulating film is located above the first oxide semiconductor film, above the first conductive layer, above the second conductive layer, and above the second oxide semiconductor film. A third insulating film located above the second insulating film and having the function of a planarizing film, A fourth insulating film above the third insulating film, A fourth conductive layer is provided above the fourth insulating film and has a region overlapping with the first pixel electrode and a region overlapping with the second pixel electrode, The first pixel electrode is provided above the third insulating film and is electrically connected to the first oxide semiconductor film via the first conductive layer. The fourth insulating film has a region covering the end of the first pixel electrode and a region covering the end of the second pixel electrode, In a plan view, the first pixel electrode does not have a region that overlaps with the first oxide semiconductor film, and has a region that overlaps with the second oxide semiconductor film. A display device in which, in a plan view, the second pixel electrode has a region that overlaps with the second conductive layer and a region that overlaps with the third conductive layer which functions as the gate electrode of the transistor.
2. A first pixel having a transistor, a capacitive element, and a first pixel electrode, A second pixel adjacent to the first pixel and having a second pixel electrode, The first pixel is, A first oxide semiconductor film having a channel formation region of the transistor, A first insulating film having a region in contact with the upper surface of the first oxide semiconductor film, a first conductive layer having a region in contact with the upper surface of the first insulating film and a region in contact with the upper surface of the first oxide semiconductor film, A second conductive layer having a region in contact with the upper surface of the first insulating film and a region in contact with the upper surface of the first oxide semiconductor film, A second oxide semiconductor film having a region that functions as one electrode of the capacitive element, A second insulating film is located above the first oxide semiconductor film, above the first conductive layer, above the second conductive layer, and above the second oxide semiconductor film. A third insulating film located above the second insulating film and having the function of a planarizing film, A fourth insulating film above the third insulating film, A fourth conductive layer is provided above the fourth insulating film and has a region overlapping with the first pixel electrode and a region overlapping with the second pixel electrode, The first pixel electrode is provided above the third insulating film and is electrically connected to the first oxide semiconductor film via the first conductive layer. The fourth insulating film has a region covering the end of the first pixel electrode and a region covering the end of the second pixel electrode, In a plan view, the first pixel electrode does not have a region that overlaps with the first oxide semiconductor film, and has a region that overlaps with the second oxide semiconductor film. In a plan view, the second pixel electrode has a region that overlaps with the second conductive layer and a region that overlaps with the third conductive layer which functions as the gate electrode of the transistor. In a plan view, the second oxide semiconductor film has a region in which the length in the first direction is greater than the length of the first oxide semiconductor film in the first direction. The first direction is the direction of extension of the source line, in the display device.
3. In claim 1 or 2, The second insulating film is a display device having silicon oxide.
4. In any one of claims 1 to 3, A display device wherein each of the first oxide semiconductor film and the second oxide semiconductor film comprises In, Ga, and Zn.
Citation Information
Patent Citations
Substrate for light valve
JP1993216071A
Liquid crystal display device
JP1994160875A
Liquid crystal panel and projection type display device
JP1998123564A
Liquid crystal display device and its manufacture
JP1998170954A
Semiconductor device and method for manufacturing the same
JP2007096055A